Method for cleaning oxide scale attached to water beam in heating furnace
By adjusting the position of the billet in the steel rolling heating furnace, it scratches the iron oxide adhesion on the water beam, the billet deflection and friction problems caused by the iron oxide adhesion are solved, and rapid and no shutdown is achieved, and production is improved Efficiency and safety.
Patent Information
- Application Number
- CN202411358084.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-27
- Publication Date
- 2024-11-29
AI Technical Summary
In the steel rolling heating furnace, the iron oxide sheet adheres to the water beam, causing the billet to move poorly, causing deflection and friction, affecting the smooth discharge of the furnace and poses safety hazards.
By adjusting the position of the billet, the iron oxide sheet attachment is placed in the intermediate vacancy between the two billets, the steel billet is used to scratch the iron oxide sheet, and the attachment is removed. The cleaning process does not require additional tools and is carried out using the maintenance time of the furnace.
It realizes fast and simple cleaning of iron oxide sheet, shortens processing time, reduces operation difficulty and cost, and ensures the continuity and efficiency of rolled steel production.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of hot-rolled strip technology, and in particular to a method for cleaning iron oxide scale attached to a water beam in a heating furnace. Background Art
[0002] The steel rolling heating furnace is generally a walking beam heating furnace. The heating temperature of the steel billet in the steel rolling heating furnace is generally around 1200℃. There will be oxidation and burning before the billet leaves the furnace, and there will be iron oxide scale falling off, which is mainly concentrated in the soaking section of the heating furnace, and there will generally be some falloff near the soaking section of the second heating furnace. Due to excessive heating temperature or long hot stop time and untimely cooling, oxidation and burning in the high temperature section will greatly increase, and part of the iron scale or the billet itself will even melt. At this time, the iron oxide scale will adhere to the water beam in the heating furnace, and will become dense and difficult to fall off under the pressure of the billet above under high temperature.
[0003] When the amount of iron oxide scale attached to the water beam increases to a certain extent, it will affect the movement of the steel billet in the heating furnace, lift the steel billet to cause it to bend in a bow shape, and cause part of the steel billet to deflect due to friction from the protruding iron sheet deposits when it moves forward. After the steel billet is out of the furnace, it is easy to hit the guard plates on both sides of the transport roller due to its incorrect position, resulting in it being unable to enter the rolling mill for rolling normally. It needs to be adjusted when it is out of the furnace, affecting the rhythm of steel tapping. When the deflection is serious, the steel billet will scrape the furnace walls on both sides of the furnace, and the steel billet may even be unable to come out of the furnace, causing safety hazards in production. Summary of the invention
[0004] In order to overcome the shortcomings of the prior art, the present invention provides a method for cleaning iron oxide scale attached to a water beam in a heating furnace. The method comprises the following steps: adjusting the position arrangement of the steel billets in pouring steel, placing the iron oxide scale attachments in the middle space between two steel billets that are translated left and right, adjusting the height of the movable beam, raising the height of the iron oxide scale attachments above the lower edge of the steel billets, and translating the movable beam left and right to cause scratches between the steel billets and the iron oxide scale attachments. The iron oxide scale attachments are subjected to force on the sides to be scratched off, and the iron oxide scale attachments are directly cleaned with the steel billets. The cleaning is quick and convenient, the processing time is shortened, no other processing tools are required to intervene in the processing, the cleaning cost is saved, the machine does not need to be shut down for processing, and subsequent production is not affected.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] A method for cleaning iron oxide scale attached to a water beam in a heating furnace, the cleaning method comprising the following steps:
[0007] S1. Before cleaning, conduct on-site inspection to observe the condition of the oxidized iron scale, determine the location of the oxidized iron scale attached to the water beam and the volume of the oxidized iron scale;
[0008] S2. When loading steel, the billets are placed side by side, leaving a space of 3000-4000mm between the two billets;
[0009] S3. Normal steel pouring, so that the scale attachment on the water beam is in the empty space between the two steel billets, and the distance between the scale attachment and the steel billet is kept less than the translation stroke of a movable beam;
[0010] S4. The oxidized iron scale is attached to the fixed beam. The movable beam is manually raised to a height 15 to 25 mm higher than the fixed beam. The movable beam is translated left and right. The steel billet on the movable beam is moved left and right. The oxidized iron scale attached to the fixed beam is scratched by the moving steel billet until the oxidized iron scale falls off.
[0011] S5. The oxidized iron scale attachment is on the movable beam. The lifting height of the movable beam is manually controlled. The movable beam is lifted to a height 15 to 25 mm lower than the fixed beam. The movable beam is translated left and right. The oxidized iron scale attachment on the movable beam is scratched with the steel billet on the fixed beam until the oxidized iron scale attachment falls off.
[0012] S6. After the oxidized iron scale falls off, check the water seal groove below. If the volume of the oxidized iron scale that falls into the water seal groove is larger than 3cm×3cm, clean it out of the water seal groove manually in time.
[0013] Furthermore, the iron oxide scale cleaning is performed during the maintenance time of the production line without stopping the furnace.
[0014] Furthermore, in the step S4, steel billets are provided on both sides of the oxidized iron scale attachments on the fixed beam, and the movable beam is translated left and right, and the steel billets on both sides scratch the oxidized iron scale attachments alternately and reciprocally.
[0015] Furthermore, in the step S5, steel billets are provided on both sides of the iron oxide scale attachments on the movable beam, the movable beam is translated left and right, and the iron oxide scale attachments on the movable beam alternately and reciprocally scrape against the lower edge of the steel billet.
[0016] Furthermore, in step S6, the detached iron oxide scale with a volume less than 3 cm×3 cm is directly cleaned by using a scraper in the water seal tank.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] 1. The oxidized iron scale attachments on the water beam can be cleaned directly by scraping the steel billet against the oxidized iron scale attachments. No auxiliary cleaning tools are needed, which reduces the difficulty of operation. The cleaning operation is simple and convenient, reduces the workload of operators, improves cleaning efficiency, shortens cleaning time, and reduces cleaning costs.
[0019] 2. During the maintenance of the production line, the furnace can be cleaned when there is no need to load steel. No additional shutdown is required during the cleaning process, ensuring that the heating furnace is in working condition at any time, ensuring continuous production of steel rolling, improving steel rolling production efficiency, increasing output, and increasing production profits. DETAILED DESCRIPTION
[0020] The specific embodiments of the present invention are further described below:
[0021] A method for cleaning iron oxide scale attached to a water beam in a heating furnace, the cleaning method comprising the following steps:
[0022] S1. Before cleaning, conduct on-site inspection to observe the condition of the oxidized iron scale, determine the location of the oxidized iron scale attached to the water beam and the volume of the oxidized iron scale;
[0023] S2. When loading steel, the billets are placed side by side, leaving a space of 3000-4000mm between the two billets;
[0024] S3. Normal steel pouring, so that the scale attachment on the water beam is in the empty space between the two steel billets, and the distance between the scale attachment and the steel billet is kept less than the translation stroke of a movable beam;
[0025] S4. The oxidized iron scale is attached to the fixed beam. The movable beam is manually raised to a height 15 to 25 mm higher than the fixed beam. The movable beam is translated left and right. The steel billet on the movable beam is moved left and right. The oxidized iron scale attached to the fixed beam is scratched by the moving steel billet until the oxidized iron scale falls off.
[0026] S5. The oxidized iron scale attachment is on the movable beam. The lifting height of the movable beam is manually controlled. The movable beam is lifted to a height 15 to 25 mm lower than the fixed beam. The movable beam is translated left and right. The oxidized iron scale attachment on the movable beam is scratched with the steel billet on the fixed beam until the oxidized iron scale attachment falls off.
[0027] S6. After the oxidized iron scale falls off, check the water seal groove below. If the volume of the oxidized iron scale that falls into the water seal groove is larger than 3cm×3cm, clean it out of the water seal groove manually in time.
[0028] Furthermore, the iron oxide scale cleaning is performed during the maintenance time of the production line without stopping the furnace.
[0029] Furthermore, in the step S4, steel billets are provided on both sides of the oxidized iron scale attachments on the fixed beam, and the movable beam is translated left and right, and the steel billets on both sides scratch the oxidized iron scale attachments alternately and reciprocally.
[0030] Furthermore, in the step S5, steel billets are provided on both sides of the iron oxide scale attachments on the movable beam, the movable beam is translated left and right, and the iron oxide scale attachments on the movable beam alternately and reciprocally scrape against the lower edge of the steel billet.
[0031] Furthermore, in step S6, the detached iron oxide scale with a volume less than 3 cm×3 cm is directly cleaned by using a scraper in the water seal tank.
[0032] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solutions and concepts of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
[0033] The following examples are implemented on the premise of the technical solution of the present invention, and provide detailed implementation methods and specific operating processes, but the protection scope of the present invention is not limited to the following examples. The methods used in the following examples are conventional methods unless otherwise specified.
[0034] [Example]
[0035] The steel billet in the heating furnace was tilted in the furnace. After on-site inspection, it was observed that there was an oxidized iron scale attachment on the second movable beam at the junction of the second heating and the equalizing heat. The attachment had a volume diameter of 500mm and a height of 60mm.
[0036] During the maintenance time of the production line, the furnace temperature was controlled at 900℃. Four selected steel billets were loaded in the furnace. The positions of the steel billets and the iron oxide scale attachments were observed in the discharge furnace. The iron oxide scale attachments were placed in the empty space between the two steel billets for translation to the left and right. The distance between the iron oxide scale attachments and the steel billets was smaller than the left and right translation distance of the movable beam.
[0037] Manually adjust the lifting height of the movable beam to make it 20mm lower than the fixed beam. The movable beam with the oxidized iron scale attachment above is higher than the bottom edge of the fixed beam billet.
[0038] The movable beam translates left and right, and the oxidized iron scale attachments on the movable beam translates left and right. During the movement, the oxidized iron scale attachments on the movable beam scrape against the bottom edges of the unmoved steel billets on the fixed beams on the left and right sides, and the sides of the iron scale package fall off due to the force.
[0039] After the iron oxide scale attachment falls off, check the water seal groove below. The volume inside the water seal groove is greater than 10cm 3 The oxidized iron scale should be cleaned up manually in time, and the size should be less than or equal to 10cm. 3 The iron oxide scale is directly cleaned by the scraper plate in the water seal tank.
Claims
1. A method for cleaning iron oxide scale attached to the water beam in a heating furnace, characterized in that: The cleaning method comprises the following steps: S1. Before cleaning, conduct on-site inspection to observe the condition of the oxidized iron scale, determine the location of the oxidized iron scale attached to the water beam and the volume of the oxidized iron scale; S2. When loading steel, the billets are placed side by side, leaving a space of 3000-4000mm between the two billets; S3. Normal steel pouring, so that the scale attachment on the water beam is in the empty space between the two steel billets, and the distance between the scale attachment and the steel billet is kept less than the translation stroke of a movable beam; S4. The oxidized iron scale is attached to the fixed beam. The movable beam is manually raised to a height 15 to 25 mm higher than the fixed beam. The movable beam is translated left and right. The steel billet on the movable beam is moved left and right. The oxidized iron scale attached to the fixed beam is scratched by the moving steel billet until the oxidized iron scale falls off. S5. The oxidized iron scale attachment is on the movable beam. The lifting height of the movable beam is manually controlled. The movable beam is lifted to a height 15 to 25 mm lower than the fixed beam. The movable beam is translated left and right. The oxidized iron scale attachment on the movable beam is scratched with the steel billet on the fixed beam until the oxidized iron scale attachment falls off. S6. After the oxidized iron scale falls off, check the water seal groove below. If the volume of the oxidized iron scale that falls into the water seal groove is larger than 3cm×3cm, clean it out of the water seal groove manually in time.
2. The method for cleaning the iron oxide scale attached to the water beam in the heating furnace according to claim 1 is characterized in that: The iron oxide scale cleaning is performed during the maintenance time of the production line without stopping the furnace.
3. The method for cleaning the iron oxide scale attached to the water beam in the heating furnace according to claim 1 is characterized in that: In the step S4, steel billets are provided on both sides of the oxidized iron scale attachments on the fixed beam, and the movable beam is translated left and right, and the steel billets on both sides scratch the oxidized iron scale attachments alternately and reciprocally.
4. The method for cleaning the iron oxide scale attached to the water beam in the heating furnace according to claim 1, characterized in that: In the step S5, steel billets are arranged on both sides of the iron oxide scale attachment on the movable beam, the movable beam is translated left and right, and the iron oxide scale attachment on the movable beam scrapes against the lower edge of the steel billet alternately and reciprocally.
5. The method for cleaning the iron oxide scale attached to the water beam in the heating furnace according to claim 1, characterized in that: In the step S6, the shed iron oxide scale with a volume less than 3 cm×3 cm is directly cleaned by using a scraper in the water seal tank.