In-situ repair method and display panel
Through the in-situ repair method, the adsorption device is used to remove the defective components in the Micro-LED display panel and supplement the replacement components, which solves the problems of substrate damage and solder splash in the prior art, and improves the repair yield and reliability of the display panel. .
Patent Information
- Application Number
- CN202411333233.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-11-29
Smart Images

Figure CN119050218A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to an in-situ repair method and a display panel. Background Art
[0002] Micro Light Emitting Diode (Micro-LED) display has the characteristics of high brightness, high contrast, and wide color gamut, and is considered to be the ultimate display technology. Currently, common Micro-LED display panels are composed of millions of micron-sized LEDs. How to accurately transfer a large number of Micro-LEDs to the driving backplane is the current main bottleneck. This transfer technology is called Micro-LED mass transfer.
[0003] Micro LED display manufacturing technology is still immature and has not yet achieved mass production; mass transfer is one of the main bottlenecks. Currently, a variety of transfer schemes have been proposed, including wafer bonding technology, fluid self-assembly technology, stamp transfer and laser transfer. Among them, stamp transfer and laser transfer are the two most widely used technologies, but the industry's current yield level of one-time bonding is <99.99%, which cannot meet mass production requirements.
[0004] Since the transfer bonding process will result in a certain yield loss, post-bonding repair is an essential process and is also the main bottleneck for improving product yield. The modification solutions for Micro-LED display panels include redundant repair and in-situ repair. In the redundant repair solution, the redundant circuit design itself will be limited by the pixel density (Pixels Per Inch, PPI) of the substrate. In-situ repair is considered a better solution. It can remove the LED at the defective point and replace the new LED at the original position. Its technical solution is not limited by the product PPI, there is no chromaticity shift problem, and its application range is wider.
[0005] However, in the process of removing the defective LED, the fallen LED is easy to fall back to the substrate (i.e., the driving backplane), and the chips that fall back to the substrate need to be cleaned, especially the chips that fall back to the active area (AA) area are easy to cause substrate crushing during repair and rebonding. Summary of the invention
[0006] In view of this, the purpose of the present application is to provide an in-situ repair method and a display panel to reduce substrate damage and improve the display panel repair yield.
[0007] In a first aspect, the present application provides an in-situ repair method, the method comprising:
[0008] Providing a substrate with light-emitting elements welded thereon, wherein the light-emitting elements include defective elements and qualified elements, and the positions of the defective elements are used as bad point positions;
[0009] performing a separation process on the defective component to release the welding between the defective component and the substrate;
[0010] After attaching an adsorption device to the side of the substrate where the light-emitting element is welded, the adsorption device is removed to remove the defective element and retain the qualified element;
[0011] A replacement element is added at the position of the bad point.
[0012] In a second aspect, an embodiment of the present application further provides a display panel, comprising a substrate having a light-emitting element welded thereto, wherein the light-emitting element is repaired using the method described.
[0013] The embodiments of the present application provide an in-situ repair method and a display panel, and provide a substrate with light-emitting elements welded thereto, wherein the light-emitting elements include defective elements and qualified elements, and the positions of the defective elements are used as bad point positions, and the defective elements are subjected to a detachment process to release the welding between the defective elements and the substrate, and the adsorption device is attached to the side of the substrate with the light-emitting elements welded thereto and then removed, because the welding between the defective elements and the substrate is released, it is easy to remove the defective elements by adsorption but not easy to remove the qualified elements by adsorption, so that the defective elements are removed by the adsorption device and the qualified elements are retained, and then a replacement element can be added at the bad point position, and the defective elements are removed by adsorption, thereby reducing the damage to the substrate caused by the defective elements falling back onto the substrate, and the removal process does not cause solder splashing, thereby ensuring the reliability of the substrate. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0015] Figure 1 A schematic diagram of removing a light-emitting element provided in an embodiment of the present application;
[0016] Figure 2 A top view of a display panel during a light emitting element removal process provided by an embodiment of the present application;
[0017] Figure 3 A schematic diagram of a backfill bonding process provided in an embodiment of the present application;
[0018] Figure 4A schematic diagram of another method of removing a light-emitting element provided in an embodiment of the present application;
[0019] Figure 5 A flowchart of an in-situ repair method provided in an embodiment of the present application;
[0020] Figure 6-Figure 14 A schematic diagram of the structure of a substrate and a light-emitting element thereon during an in-situ repair process provided in an embodiment of the present application. DETAILED DESCRIPTION
[0021] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below with reference to the accompanying drawings.
[0022] In the following description, many specific details are set forth to facilitate a full understanding of the present application, but the present application may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present application. Therefore, the present application is not limited to the specific embodiments disclosed below.
[0023] Secondly, the present application is described in detail with reference to the schematic diagram. When describing the embodiments of the present application in detail, for the sake of convenience, the cross-sectional diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present application. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.
[0024] As described in the background technology, in the process of removing the defective LED, the detached LED is easy to fall back to the substrate (i.e., the driving backplane), and the chips that fall back to the substrate need to be cleaned, especially the chips that fall back in the active area (AA) area are easy to cause substrate crushing during repair and rebonding.
[0025] At present, it is possible to add LED blowing and suction while removing the LED to recycle the LED, so that the LED can be recycled in a directional manner. Figure 1 As shown, it is a schematic diagram of removing a light-emitting element provided by an embodiment of the present application. At present, a high-energy laser is used to act on the light-emitting element 200 to produce an impact effect. The positive and negative electrodes 210 / 220 of the light-emitting element are in contact with the back plate electrodes 110 / 120. After the high-energy laser heats the solder, the instantaneous high temperature generated causes the material to vaporize and form high temperature and high pressure locally, thereby pushing the light-emitting element 200 to fly away. The direction of the light-emitting element 200 falling off is random and it is easy to fall back to the substrate. Reference Figure 2 FIG. 1 is a top view of a display panel during a light emitting element removal process provided in an embodiment of the present application. The light emitting element 200 falls back onto the substrate 100. Figure 3As shown, it is a schematic diagram of a backfill bonding process provided in an embodiment of the present application. The backfill substrate 300 is fixed with a replacement element 400 to supplement the original position of the removed light-emitting element. However, the light-emitting element 200 remaining on the substrate 100 is likely to cause damage to the substrate.
[0026] refer to Figure 4 As shown, it is a schematic diagram of another method of removing a light-emitting element provided in an embodiment of the present application. By setting an air suction device in one direction and a blowing device in another direction, the detached light-emitting element can be removed in a direction. However, laser removal will cause the solder to melt. While this large-flow air suction and blowing method increases the success rate of light-emitting element recovery, it will also cause the solder 230 to splash and scatter onto the substrate, which may easily cause problems such as device short circuit.
[0027] Based on the above technical problems, the embodiments of the present application provide an in-situ repair method and a display panel, providing a substrate with light-emitting elements welded thereto, the light-emitting elements including defective elements and qualified elements, the position of the defective elements being used as the bad point position, the defective elements being detached to release the welding between the defective elements and the substrate, the adsorption device being attached to the side of the substrate with the light-emitting elements welded thereto and then being removed, since the welding between the defective elements and the substrate is released, it is easy to remove the defective elements by adsorption but not easy to remove the qualified elements by adsorption, so that the defective elements are removed by the adsorption device and the qualified elements are retained, and then substitute elements can be added at the bad point position, and the defective elements are removed by adsorption, thereby reducing the damage to the substrate caused by the defective elements falling back onto the substrate, and the removal process will not cause solder splashing, thereby ensuring the reliability of the substrate.
[0028] In order to better understand the technical solution and technical effects of the present application, specific embodiments will be described in detail below with reference to the accompanying drawings.
[0029] refer to Figure 5 FIG. 1 is a flowchart of an in-situ repair method provided in an embodiment of the present application, referring to Figure 6-Figure 14 A schematic diagram of the structure of a substrate and a light-emitting element thereon during an in-situ repair process provided in an embodiment of the present application, wherein Fig.14 is a top view of the substrate, Figure 6-Figure 13 is a longitudinal cross-sectional view of the substrate at a defective component, the method may include:
[0030] S101, provide a substrate with light-emitting components soldered on it, the light-emitting components include defective components and qualified components, the location of the defective components is taken as the bad point location, refer to Figure 6 shown.
[0031] In the embodiment of the present application, the substrate 100 welded with the light emitting element 200 can be used as the substrate to be repaired, and the substrate 100 can be a driving substrate, which can be provided with a driving circuit, and the positive and negative electrodes of the light emitting element 200 can be welded to the driving circuit on the substrate 100. Specifically, the surface of the substrate 100 can have substrate electrodes 110 / 120, and the positive and negative electrodes 210 / 220 of the light emitting element 200 are respectively aligned with the substrate electrodes 110 / 120, and the two are connected by welding, for example, by solder welding, or by eutectic welding and the like.
[0032] The light-emitting elements 200 may be arranged in an array on the substrate 100, including red light-emitting elements, green light-emitting elements, and blue light-emitting elements. The light-emitting elements 200 may be, for example, micro-light-emitting diodes (Micro-LEDs). The yield of the light-emitting elements 200 needs to be improved, and may include defective elements and qualified elements, wherein defective elements are elements that cannot meet the application requirements, that is, elements whose test results are test failures, and elements whose luminous intensity cannot meet the requirements, such as no light, too high or too low luminous intensity, etc. The position where the light-emitting element 200 is located is a bad point position, which needs to be repaired, and qualified elements are elements that can meet the actual application requirements, that is, elements whose test results are test passing.
[0033] S102, perform separation processing on the defective component to release the welding between the defective component and the substrate, refer to Figure 1 shown.
[0034] The defective component is separated from the substrate 100 to release the welding between the defective component and the substrate. Figure 1 Specifically, laser can be used to align the defective component to separate it. The laser and the defective component produce an impact effect. The positive and negative electrodes of the defective component are in contact with the back plate electrodes, and the middle is suspended. The instantaneous high temperature generated by the high-energy laser causes the material to vaporize and form high temperature and high pressure locally, thereby pushing the defective component to fly away. The defective component may fall back onto the substrate and show a random distribution characteristic.
[0035] In a specific implementation, UV pulse laser can be used to align the defective components to remove the defective components.
[0036] S103, after attaching an adsorption device to the side of the substrate where the light emitting element is welded, remove the adsorption device to remove defective elements through the adsorption device and retain qualified elements, refer to Figure 7-Figure 12 shown.
[0037] In an embodiment of the present application, the substrate and the adsorption device can be aligned and pressed together, the adsorption device can remove the defective components, and the adsorption device can provide adsorption force. Since the welding between the defective components and the substrate is released, the defective components rely on electrostatic force to contact the substrate, and the bonding force is relatively weak, while the qualified components are effectively bonded to the substrate through welding. Therefore, it is easy to adsorb and remove the defective components but not easy to adsorb and remove the qualified components, so that the defective components are removed by the adsorption device and the qualified components are retained.
[0038] The adsorption force of the adsorption device can be evenly distributed at various positions, or a larger adsorption force can be set in the central area of the adsorption device, that is, the adsorption force in the central area of the adsorption device is greater than the adsorption force in the edge area. This is because there is a temperature difference from the center to the edge of the substrate, and the low edge temperature leads to a relatively weak bonding strength between the substrate and the light-emitting element. In addition, there may be warping in the edge area, and the center area is concave relative to the edge area. The larger adsorption force in the center area can enhance the success rate of removing defective components in the center area.
[0039] As a possible implementation, the adsorption device may include a substrate 500 and an adhesive layer 510 on the substrate, and the adhesive layer 510 is used to face the substrate 100 when the substrate is attached to the adsorption device to adsorb defective components. That is, the adsorption device may be a sticky adsorption plate, and the adhesive layer 510 provides an adsorption force to pick up defective components, and remove the defective components by physical contact, thereby avoiding solder splashing and low recycling yield problems in the blowing and suction scheme, and avoiding the light-emitting components that fall back during re-bonding and damage the circuit to cause secondary defects.
[0040] The material of the adhesive layer 510 must have the characteristics of high adhesion and durability, not easy to age, not easy to fall off, anti-static, moisture-proof, friction-resistant, non-toxic, rust-free, pollution-free, easy to clean, etc. The adhesive layer 510 can be a pressure-sensitive adhesive type material, for example, it can be at least one of a rubber-type pressure-sensitive adhesive, an acrylate-type pressure-sensitive adhesive, and a silicone pressure-sensitive adhesive.
[0041] The adhesive layer 510 can be coated on the substrate 500, and after curing, an adsorption device including the substrate 500 and the adhesive layer 510 can be obtained. At this time, the defective components adsorbed on the adhesive layer 510 can be removed, and the adhesive layer can be cleaned to achieve the reuse of the adhesive layer 510. The adhesive layer 510 can be cleaned by water spraying and then air-dried for reuse. The adhesive layer 510 can also be set on the substrate 500 by film pasting. At this time, the adhesive layer 510 can be removed, and a new adhesive layer 510 can be set on the substrate to achieve the reuse of the substrate, and the used adhesive layer 510 can be removed by film tearing.
[0042] The substrate 500 may be a carrier, and the adhesive layer 510 is disposed on the surface of the substrate to form an adsorption carrier. Figure 7As shown; alternatively, the substrate can be a roller, and the adhesive layer is arranged on the surface of the substrate to form an adsorption roller, and the adsorption roller can be rolled and adhered to the substrate, which is not illustrated here.
[0043] The thickness of the adhesive layer 510 may be greater than the thickness of the defective component, so that the adsorption force of the adhesive layer on the defective component can smoothly realize the picking up of the defective component.
[0044] The adhesive layer 510 may have a uniform thickness. Figure 7 As shown; the adhesive layer 510 may also have a greater thickness in the central region, that is, the thickness of the adhesive layer 510 in the central region is greater than the thickness of the edge region, reference Figure 8 As shown, this can match the shape of the substrate where the edge area is warped and the center area is concave relative to the edge area, balance the poor pickup caused by the substrate warping, and ensure the success rate of picking up the defective components in the center area. The thickness of the center area of the adhesive layer 510 gradually decreases in the direction from the center point of the adhesive layer to the outside to match the concave shape of the center area; the thickness of the edge area of the adhesive layer 510 gradually decreases in the direction from the center point of the adhesive layer to the outside to match the gradually warped shape of the edge area.
[0045] When the adsorption force of the adsorption device is relatively uniform, the adsorption force of the adhesive layer is also relatively uniform, and the degree of solidification at each position of the adhesive layer can be kept consistent; when the adsorption force of the adsorption device is uneven, the degree of solidification at different positions of the adhesive layer can be used to achieve the adsorption force corresponding to each position. For example, the degree of solidification in the edge area of the adhesive layer is greater than that in the central area, so that the adsorption force in the edge area is smaller than that in the central area, so as to cope with the shape of the substrate being warped in the edge area and the central area being concave relative to the edge area, thereby ensuring the success rate of picking up defective components in the central area.
[0046] As another possible implementation, the adsorption device may include a magnetic adsorption device 600. In this solution, before the defective component is separated, a magnetic material 700 may be disposed on the side of the defective component away from the substrate. Fig. 9 As shown, the defective components that fall back to the substrate also carry magnetic material 700, see Fig.10 As shown, after the defective components are separated, the defective components can be picked up by utilizing the adsorption force between the magnetic device and the magnetic material. Fig.11 and Fig.12 shown.
[0047] The magnetic material is arranged on the side of the defective component away from the substrate. Specifically, a colloid material is formed on the side of the defective component away from the substrate through a dispensing process or an inkjet printing process. The colloid material may include a magnetic material and an organic solvent, and then the colloid material is solidified so that the magnetic material forms a good coating effect on the defective component. The organic solvent may be, for example, a resin, and the magnetic material may be a magnetic metal material.
[0048] The magnetic device 600 may have a uniform thickness. Fig.11 As shown; the magnetic device 600 may also have a greater thickness in the central area, that is, the thickness of the magnetic device 600 in the central area is greater than the thickness of the edge area, reference Fig.12 As shown, this can match the shape of the substrate where the edge area is warped and the center area is concave relative to the edge area, and has a larger adsorption force in the center area and a smaller adsorption force in the edge area, thereby ensuring the success rate of picking up defective components in the center area. The thickness of the center area of the magnetic suction device 600 gradually decreases in the direction from the center point of the magnetic suction device to the outside to match the concave shape of the center area; the thickness of the edge area of the magnetic suction device 600 gradually decreases in the direction from the center point of the magnetic suction device to the outside to match the gradually warped shape of the edge area.
[0049] S104, add replacement components at the location of the bad point, refer to Fig.13 and Fig.14 shown.
[0050] After the defective component is removed, a replacement component 400 can be added to the defective pixel position, thereby replacing the defective component with the replacement component 400, that is, the in-situ replenishment of the light-emitting component is realized, and the defective pixel position is repaired. Fig.14 The substitute component 400 can have the function that the defective component originally has, and both are used to emit light of the same color, and the light-emitting parameters of the substitute component 400 can usually meet actual requirements.
[0051] Specifically, a repair substrate 300 may be attached to the side of the substrate 100 on which the light emitting element 200 is welded, and a replacement element 400 is provided on the repair substrate 300 to weld the replacement element 400 at the position of the bad point. Fig.13As shown, the replacement component 400 can be connected to the substrate electrode 110 / 120 by bonding, and specifically, the electrodes 410 / 420 of the replacement component 400 are connected to the substrate electrodes 110 / 120 by welding. The replacement component 400 can be connected to the substrate 100 by welding. The backfill substrate 300 can be a COC (Chip on Carrier) carrier, on which a chip is mounted. The backfill substrate 300 can also be called a packaging substrate or packaging carrier, which can be attached to the substrate 100 by a packaging device 40A.
[0052] The embodiment of the present application provides an in-situ repair method, providing a substrate with light-emitting elements welded thereon, the light-emitting elements including defective elements and qualified elements, the position of the defective elements being used as the bad point position, the defective elements being detached to release the welding between the defective elements and the substrate, the adsorption device being attached to the side of the substrate with the light-emitting elements welded thereon and then being removed, since the welding between the defective elements and the substrate is released, it is easy to remove the defective elements by adsorption but not easy to remove the qualified elements by adsorption, so that the defective elements are removed by the adsorption device and the qualified elements are retained, and then a replacement element can be added at the bad point position, and the defective elements are removed by adsorption, thereby reducing the damage to the substrate caused by the defective elements falling back onto the substrate, and the removal process will not cause solder splashing, thereby ensuring the reliability of the substrate.
[0053] An embodiment of the present application also provides a display panel, which includes a substrate with light-emitting elements soldered thereto, at least one light-emitting element being repaired using the aforementioned in-situ repair method, and the solder splashing around the repaired light-emitting element is significantly reduced.
[0054] Each embodiment in this specification is described in a progressive manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the device embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.
[0055] The above is only a preferred implementation of the present application. Although the present application has been disclosed as a preferred embodiment, it is not intended to limit the present application. Any technician familiar with the art can use the above disclosed methods and technical contents to make many possible changes and modifications to the technical solution of the present application without departing from the scope of the technical solution of the present application, or modify it into an equivalent embodiment of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present application without departing from the content of the technical solution of the present application still falls within the scope of protection of the technical solution of the present application.
Claims
1. An in-situ repair method, characterized in that: The method comprises: Providing a substrate with light-emitting elements soldered thereon, wherein the light-emitting elements include defective elements and qualified elements, and the locations of the defective elements are used as bad pixel locations; performing a separation process on the defective component to release the welding between the defective component and the substrate; After attaching an adsorption device to the side of the substrate where the light emitting element is welded, removing the adsorption device, so as to remove the defective element through the adsorption device and retain the qualified element; A replacement element is added at the position of the bad point.
2. The method according to claim 1, characterized in that The adsorption force of the central area of the adsorption device is greater than the adsorption force of the edge area.
3. The method according to claim 1 or 2, characterized in that The adsorption device includes a substrate and an adhesive layer on the substrate, and the adhesive layer is used to face the substrate when the substrate is attached to the adsorption device, so as to adsorb the defective component.
4. The method according to claim 3, characterized in that The thickness of the adhesive layer in the central area is greater than that in the edge area.
5. The method according to claim 4, characterized in that The thickness of the central area of the bonding layer gradually decreases in a direction from the central point of the bonding layer to the outside, and / or the thickness of the edge area of the bonding layer gradually decreases in a direction from the central point of the bonding layer to the outside.
6. The method according to claim 3, characterized in that The curing degree of the edge area of the adhesive layer is greater than that of the central area, so that the adsorption force of the edge area is smaller than that of the central area.
7. The method according to claim 3, characterized in that The method further comprises: removing defective components adsorbed on the adhesive layer and cleaning the adhesive layer to achieve reuse of the adhesive layer; or The adhesive layer is removed and a new adhesive layer is provided on the substrate to achieve the reuse of the substrate.
8. The method according to claim 3, characterized in that The thickness of the adhesive layer is greater than the thickness of the defective component.
9. The method according to claim 1 or 2, characterized in that The adsorption device includes a magnetic device. Before the defective component is separated, the method further includes: A magnetic material is provided on a side of the defective component facing away from the substrate.
10. The method according to claim 9, characterized in that The thickness of the magnetic attraction device in the central area is greater than that in the edge area.
11. The method according to claim 10, characterized in that The thickness of the central region of the magnetic device gradually decreases in a direction outward from the center point of the magnetic device, and / or the thickness of the edge region of the magnetic device gradually decreases in a direction outward from the center point of the magnetic device.
12. The method according to claim 9, characterized in that The step of providing a magnetic material on a side of the defective component facing away from the substrate comprises: forming a colloidal material on a side of the defective component facing away from the substrate by a dispensing process or an inkjet printing process, wherein the colloidal material includes a magnetic material and an organic solvent; The colloidal material is solidified.
13. The method according to claim 1 or 2, characterized in that The step of separating the defective components includes: The defective component is aligned with a laser to release the welding between the defective component and the substrate.
14. The method according to claim 1 or 2, characterized in that The method of supplementing a replacement element at the position of the bad point includes: A repair substrate is attached to the side of the substrate on which the light emitting element is welded. A replacement element is provided on the repair substrate so as to weld the replacement element at the position of the bad point.
15. A display panel, characterized in that: The invention comprises a substrate having a light-emitting element welded thereto, wherein the light-emitting element is repaired by the method according to any one of claims 1 to 14.
Citation Information
Patent Citations
Repair method of micro light-emitting unit and display device
CN116598394A
Chip removal device and method
CN118057627A
Chip component removing method and chip component removing device
JP2022121826A
Micro LED Display Manufacturing Method
KR102288309B1
KR20210091640A