Landfill leachate filtering material and preparation method thereof

By constructing a chitosan micro-nano network on the wood cellulose skeleton and loading hydrotalcite, it forms an efficient waste leachate filter material, and solves the problems of high difficulty and cost of waste leachate in the prior art, and realizes the impurities Efficient removal significantly improves the wastewater treatment effect.

CN119056414APending Publication Date: 2024-12-03SHANGHAI JIFAN ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411398089.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-09
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The waste leachate is difficult to handle, the existing filtering adsorbents are costly and have low removal efficiency, especially for difficult degradation of organic matter and metal ions, resulting in environmental pollution.

Method used

Using wood cellulose as the skeleton, a chitosan micro-nano network with fiber orientation is constructed, and a sheet-like hydrotalcite is constructed on it to form a garbage leachate filter material, and ultrasonic shearing is carried out through NaClO2 solution delignin and glutaraldehyde. Prepare through the same steps, combining the hydrothermal reaction of divalent salts and trivalent salts to form an efficient filtering adsorption material.

Benefits of technology

It improves the adsorption performance and removal efficiency of impurities, reduces the migration resistance of impurities, enhances the removal ability of impurities in wastewater, and significantly improves the wastewater treatment effect.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a garbage leachate filtering material which is characterized in that wood cellulose is used as a framework of the garbage leachate filtering material, a chitosan micro-nano network with fiber orientation is constructed in a fiber pore channel structure of the framework, and flaky hydrotalcite-like compounds are constructed on the chitosan micro-nano network. According to the landfill leachate filtering material provided by the invention, the wood, the chitosan and the hydrotalcite are organically combined, so that the advantages of various materials are fully played, the advantages of the materials are made up of each other, the treatment effect is improved, and a novel and efficient filtering and adsorbing material is explored.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of garbage disposal, and in particular to a garbage leachate filtering material and a preparation method thereof. Background Art

[0002] Landfill leachate is a high-concentration organic wastewater with complex components. Its water quality and quantity vary greatly over time, making it extremely difficult to treat. If landfill leachate is not properly treated, it will often cause serious secondary pollution to the environment, mainly manifested in the pollution of groundwater and surface water bodies and the pollution of the atmosphere by gas during the landfill process. In addition, its pollution of groundwater bodies is difficult to detect and lasting. The properties of landfill leachate are related to the composition of the landfill, the operating conditions during landfilling, the degradation rate of the landfill, the degree of stabilization of the landfill, and the local natural and social conditions. It generally has the following characteristics: (1) There are many types of organic pollutants and the water quality is complex. Generally speaking, the organic matter in landfill leachate can be divided into low molecular weight fatty acids, medium molecular weight fulvic acid substances, and high molecular weight carbohydrate substances and humus. Among them, low molecular weight fatty acid organic matter is easier to biodegrade, while fulvic acid organic matter is difficult to biodegrade; (2) Since anaerobic landfill technology is currently used, NH4 + After the landfill enters the methanogenic stage, the concentration of -N continues to rise due to the anaerobic hydrolysis and fermentation of nitrogen-containing biodegradable organic components. After reaching the peak value, it lasts for a long time until the landfill is finally closed. Even when the landfill is stable, it can still reach a fairly high concentration. + -N content usually accounts for 85%-90% of TN, and NH4 + -N is not present in the form of free ammonia in the leachate; (3) High content of inorganic salts and metals. Leachate contains more than 10 kinds of metal ions and high concentrations of Cl-, SO4 2- In order to find an effective method to treat landfill leachate, a large number of domestic and foreign scholars have been conducting research and exploration, and believe that the filtration adsorption process in the physical and chemical treatment method is a low-cost leachate pretreatment method with good removal effect on metal ions and difficult-to-degrade organic matter. The key to the filtration adsorption method is the filtration adsorbent. Finding a cheap and efficient filtration adsorbent has become a concern of current environmentalists. Summary of the invention

[0003] Technical problem to be solved: The purpose of the present invention is to provide a landfill leachate filter material, which adopts an organic combination of wood, chitosan and hydrotalcite to give full play to the advantages of various materials, complement each other's strengths and weaknesses, improve the treatment effect, and explore a new type of efficient filtering and adsorption material.

[0004] Technical solution: A landfill leachate filter material, which uses wood cellulose as a skeleton, constructs a chitosan micro-nano network with fiber orientation in the fiber pore structure of the skeleton, and constructs a flaky hydrotalcite-like substance on the chitosan micro-nano network. The preparation method of the above-mentioned landfill leachate filter material comprises the following steps: S1. Select wood with a thickness of 1.5-2.5cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 4-5, and react in a water bath to obtain delignified wood; S2. The delignified wood was added to the chitosan solution, the chitosan solution was pressurized to penetrate into the wood, and then the glutaraldehyde solution was added dropwise, and after ultrasonic shearing, unidirectional freeze drying was performed to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Add the divalent salt and the mixed trivalent salt into deionized water and stir to dissolve to obtain a mixed salt solution; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, stirred and dissolved to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is between 9.0 and 9.5. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution, perform a hydrothermal reaction, and obtain the landfill leachate filter material. Preferably, the temperature of the water bath reaction in step S1 is 90-100° C. and the time is 2-3 h. Preferably, the concentration of the chitosan solution in step S2 is 0.8-2wt%, and the concentration of the glutaraldehyde solution is 1-2wt%. Preferably, the temperature of the unidirectional freeze drying in step S2 is -80 to -40°C, and the time is 10-20h. Preferably, in step S4, the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.5-1 mol / L. Preferably, the molar ratio of sodium hydroxide to sodium carbonate in step S5 is 1:0.8-1.2. Preferably, the temperature of the hydrothermal reaction in step S6 is 80-100° C. and the time is 10-30 hours. Beneficial effects: The landfill leachate filter material of the present invention has the following advantages: 1. In the present invention, chitosan is compounded with delignified wood, and chitosan can enter the micropores of wood. The hydroxyl groups in its molecular chain can form hydrogen bond crosslinking points with the hydroxyl groups on the surface of cellulose. The internal directional porous structure helps the migration of impurities in wastewater within the hydrogel, reduces the migration resistance of impurities, and enhances the adsorption performance of impurities; 2. In the present invention, hydrotalcite-like substances are selected to be loaded on chitosan. Compared with ordinary hydrotalcite, the MgAl-Sc hydrotalcite in the present invention has a larger specific surface area and pore volume, and has more abundant oxygen vacancies on the surface. These favorable conditions can provide more active sites for the MgAl-Sc hydrotalcite adsorbent, thereby being more conducive to improving its adsorption of impurities in wastewater. It can be seen that the doping of an appropriate amount of rare earth elements can significantly improve the removal efficiency of the adsorbent for wastewater. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a wood with a thickness of 1.8 cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 4, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and obtain delignified wood; S2. The delignified wood was added to a 0.8wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -80°C for 10h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.5 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:0.8, stirred and dissolved to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 100°C for 10 hours to obtain a landfill leachate filter material. Example 2 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a wood with a thickness of 2 cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 100 ° C, the time is 2h, and delignified wood is obtained; S2. The delignified wood was added to a 2 wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 2 wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -40 ° C for 20 h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 1 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1.2, stirred and dissolved to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH value of the solution is 9.0. After the mixed salt solution is completed, adjust the pH value to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 80°C for 30 hours to obtain a landfill leachate filter material. Example 3 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a wood with a thickness of 2 cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 4, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and obtain delignified wood; S2. The delignified wood was added to a 1 wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1.2 wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -60 ° C for 12 h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.6 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:0.9, stirred and dissolved to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 95°C for 15 hours to obtain a landfill leachate filter material. Example 4 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a wood with a thickness of 2.2 cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 95 ° C, the time is 2h, and delignified wood is obtained; S2. The delignified wood was added to a 1.5wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1.5wt% glutaraldehyde solution was added dropwise, and after ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -50°C for 18h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.8 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1.1, stirred and dissolved to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 85°C for 25 hours to obtain a landfill leachate filter material. Example 5 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a 2 cm thick piece of wood, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and delignified wood is obtained; S2. The delignified wood was added to a 1.2wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1.0wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -55°C for 15h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.7 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1, and stirred to dissolve to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 90°C for 20 hours to obtain a landfill leachate filter material. Comparative Example 1 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a 2 cm thick piece of wood, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and delignified wood is obtained; S2. Add the delignified wood to a 1.2wt% chitosan solution, pressurize the chitosan solution to make it penetrate into the wood, then drop a 1.0wt% glutaraldehyde solution, and after ultrasonic shearing, perform unidirectional freeze drying at a temperature of -55°C for 15 hours to obtain a landfill leachate filter material. Comparative Example 2 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a wood with a thickness of 2 cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and obtain delignified wood; S2. The delignified wood was added to a 1.2wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1.0wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -55°C for 15h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.7 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1, and stirred to dissolve to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 90°C for 20 hours to obtain a landfill leachate filter material. Comparative Example 3 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a wood with a thickness of 2 cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and obtain delignified wood; S2. The delignified wood was added to a 1.2wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1.0wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, unidirectional freeze drying was performed at a temperature of -55°C for 15h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and lanthanum nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.7 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1, and stirred to dissolve to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 90°C for 20 hours to obtain a landfill leachate filter material. Comparative Example 4 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a 2 cm thick piece of wood, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and delignified wood is obtained; S2. The delignified wood is added to deionized water and fully soaked so that the delignified wood is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.7 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1, and stirred to dissolve to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S2 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 90°C for 20 hours to obtain a landfill leachate filter material. Comparative Example 5 A method for preparing a landfill leachate filter material, the method comprising the following steps: S1. Select a 2 cm thick piece of wood, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 5, react in a water bath, the water bath reaction temperature is 90 ° C, the time is 3h, and delignified wood is obtained; S2. The delignified wood was added to a 1.2wt% chitosan solution, pressurized to allow the chitosan solution to penetrate into the wood, and then a 1.0wt% glutaraldehyde solution was added dropwise. After ultrasonic shearing, freeze drying (non-unidirectional freezing) was performed directly. The unidirectional freeze drying temperature was -60°C for 10h to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Adding a divalent salt and a mixed trivalent salt to deionized water, stirring and dissolving, to obtain a mixed salt solution, wherein the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.7 mol / L; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, the molar ratio of sodium hydroxide and sodium carbonate was 1:1, and stirred to dissolve to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is 9.0. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution and perform a hydrothermal reaction at a temperature of 90°C for 20 hours to obtain a landfill leachate filter material. The materials in Examples 1-5 and Comparative Examples 1-5 were subjected to a filtration test. The specific method was as follows: 30 g of the adsorption material was weighed and placed in a G3 sand core funnel, and 90 mL of leachate was added in sequence. The filtrate was sampled and the water quality indicators in the filtrate were tested. The leachate used in the experiment was collected from a garbage treatment plant. The main water quality indicators were: COD concentration of 33562 mg / L, ammonia concentration of 1896 mg / L, copper ion concentration of 0.365 mg / L, and turbidity of 1298 mg / L (the water quality indicators of the following water samples were selected from the water quality indicators collected after 20 minutes of filtration). COD removal rate / % Ammonia removal rate / % Copper ion removal rate / % Turbidity removal rate / % Example 1 66.9 76.9 85.9 89.6 Example 2 64.4 75.6 86.3 88.5 Example 3 65.8 77.0 84.2 87.2 Example 4 66.8 74.6 83.8 86.9 Example 5 67.2 75.9 84.5 85.4 Comparative Example 1 56.3 62.3 74.3 83.6 Comparative Example 2 65.6 66.9 80.3 86.3 Comparative Example 3 65.3 68.3 81.1 87.1 Comparative Example 4 52.3 54.5 78.9 82.3 Comparative Example 5 58.9 69.3 86.1 83.4 Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

Claims

1. A landfill leachate filter material, characterized in that: The garbage filtrate filter material uses wood cellulose as a skeleton, constructs a chitosan micro-nano network with fiber orientation in the fiber pore structure of the skeleton, and constructs a sheet-like hydrotalcite on the chitosan micro-nano network.

2. The method for preparing the landfill leachate filter material according to claim 1, characterized in that: The preparation method comprises the following steps: S1. Select wood with a thickness of 1.5-2.5cm, immerse the wood in a NaClO2 solution, adjust the pH of the solution to 4-5, and react in a water bath to obtain delignified wood; S2. The delignified wood was added to the chitosan solution, the chitosan solution was pressurized to penetrate into the wood, and then the glutaraldehyde solution was added dropwise, and after ultrasonic shearing, unidirectional freeze drying was performed to obtain a chitosan / porous wood composite porous material; S3. The chitosan / porous wood composite porous material is added to deionized water and fully immersed so that the chitosan / porous wood composite material is immersed in water; S4. Add the divalent salt and the mixed trivalent salt into deionized water and stir to dissolve to obtain a mixed salt solution; S5. The sodium hydroxide and sodium carbonate were mixed and added to deionized water, stirred and dissolved to obtain a mixed alkaline solution; S6. Alternately add the mixed salt solution and the mixed alkali solution to the aqueous solution in step S3 to ensure that the pH of the solution is between 9.0 and 9.

5. After the mixed salt solution is completed, adjust the pH to 9.5 with the mixed alkali solution, perform a hydrothermal reaction, and obtain the landfill leachate filter material.

3. The method for preparing the landfill leachate filter material according to claim 1, characterized in that: The temperature of the water bath reaction in step S1 is 90-100° C. and the reaction time is 2-3 hours.

4. The method for preparing the landfill leachate filter material according to claim 1, characterized in that: In step S2, the concentration of the chitosan solution is 0.8-2 wt %, and the concentration of the glutaraldehyde solution is 1-2 wt %.

5. The method for preparing the landfill leachate filter material according to claim 1, characterized in that: The temperature of the one-way freeze drying in step S2 is -80 to -40°C and the time is 10 to 20 hours.

6. The method for preparing the landfill leachate filter material according to claim 1, characterized in that: In step S4, the divalent salt is magnesium nitrate hexahydrate, and the mixed trivalent salt is a mixture of aluminum nitrate nonahydrate and scandium nitrate hexahydrate, wherein the molar ratio of the divalent salt to the trivalent salt is 2:1, and the concentration of the trivalent salt in the mixed salt solution is 0.5-1 mol / L.

7. The method for preparing the landfill leachate filter material according to claim 1, characterized in that: The molar ratio of sodium hydroxide to sodium carbonate in step S5 is 1:0.8-1.

2.