Ceramic matrix composite small-curvature component shape correction tool and shape correction method

By designing the small curvature component scheduling tooling of ceramic matrix composite materials, using the alternating use of base and crimping parts and zigzag design, the problems of uneven deformation of parts and bulky molds in traditional scheduling methods are solved, and ceramic composite parts are realized efficient, uniform deposition and precise calibration.

CN119057943APending Publication Date: 2024-12-03XIAN XINGUI CERAMIC COMPOSITE MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411078024.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the traditional method of proofreading small curvature components of ceramic matrix composites, single-sided molds cause uneven deformation of parts, double-sided molds are bulky and cumbersome to operate, making it difficult to meet the accuracy and performance requirements.

Method used

Design a ceramic matrix composite small curvature component proofing tooling, including base and crimping components. The base is a rectangular structure that runs through the upper and lower ends. The curvature of the two end surfaces is consistent with the component to be proofed, and it is improved by multiple reinforcement ribs and zigzag designs. Strength and fit, and improve gas permeability through weight-reducing holes, deposition is carried out using alternating crimps.

Benefits of technology

It effectively avoids new deformation of parts during the deposition process, improves deposition uniformity and accuracy, reduces production costs, and simplifies operations. It is suitable for flat-panel thin-walled parts of ceramic composite materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119057943A_ABST
    Figure CN119057943A_ABST
Patent Text Reader

Abstract

The invention provides a tool and a method for correcting a small-curvature component made of a ceramic matrix composite. The tool and the method mainly solve the technical problems that an existing single-face mold correcting tool is prone to causing new deformation of a part, a double-face mold correcting tool is heavy, the correcting process is tedious and the like. The shape correcting tool comprises a base and a crimping assembly, the base comprises two cross beams and two vertical beams; the two ends of the two cross beams in the length direction are connected through the two vertical beams to form a vertically-through cuboid structure. The upper end face and the lower end face of the cuboid structure are both use molded surfaces, the curvature of the upper end face is consistent with that of the A face of the to-be-shaped component, and the curvature of the lower end face is consistent with that of the B face of the to-be-shaped component; a plurality of reinforcing ribs are arranged between the two cross beams; the crimping assembly comprises a first crimping part for crimping the B surface of the to-be-corrected component and a second crimping part for crimping the A surface of the to-be-corrected component; and the contact surfaces of the first crimping part and the second crimping part with the to-be-shaped component are consistent with the curvature of the corresponding surface of the to-be-shaped component.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of ceramic matrix composite material parts preparation, and in particular to a ceramic matrix composite material small curvature component shaping tool and a shaping method. Background Art

[0002] Ceramic-based composites have excellent properties such as high temperature resistance, oxidation resistance, ablation resistance, low density, high specific strength, high specific modulus, and insensitivity to cracks. They are the main candidate materials for the fuselage, cabin, wing surface, rudder surface, and large windward surface of warheads of near-space / hypersonic aircraft. With the continuous expansion of service environment and application scope, the performance requirements and dimensional accuracy requirements of ceramic-based composites are becoming more and more stringent. In the preparation process, the smaller the deformation of each part and the better the deposition effect, the better the accuracy and performance of the assembled product will be. It can be seen that the degree of deformation and deposition effect of the parts before assembly determine the quality of the entire product.

[0003] During the CVI deposition process, ceramic matrix composite small curvature components (i.e. flat thin-walled parts) generally need to be calibrated by calibrating tooling. The traditional calibrating method is to use a single-sided or double-sided mold for calibrating. This type of mold has a high degree of fit with the component to be calibrated and has a good dimensional effect, but it also has the following disadvantages:

[0004] (1) When using a single-sided mold for profiling, the mating surface between the part and the mold is basically completely blocked, resulting in a poor CVI deposition effect on the blocked side, while a good CVI deposition effect on the non-bonded side. After deposition, the densification on the front and back surfaces of the part is uneven, which easily leads to density differences and new deformation of the part.

[0005] (2) When using a double-sided mold for calibration, the calibration mold is relatively heavy, which increases the difficulty of the calibration process. Summary of the invention

[0006] The purpose of the present invention is to provide a profiling tool and profiling method for small-curvature components of ceramic-based composite materials, mainly to solve the technical problems that the existing single-sided mold profiling tool is easy to cause new deformation of parts, the double-sided mold profiling tool is relatively bulky, and the profiling process is cumbersome.

[0007] To achieve the above purpose, the technical solution of the present invention is as follows:

[0008] A ceramic matrix composite material small curvature component shaping tool is used to shape a small curvature thin-walled component, and one surface of the component to be shaped is defined as surface A, and the other surface is defined as surface B. The special features of the tool are:

[0009] Including base and crimping assembly;

[0010] The base comprises two horizontal beams and two vertical beams; the two horizontal beams are arranged in parallel and their lengths are greater than those of the vertical beams; the two ends of the two horizontal beams in the length direction are respectively connected by two vertical beams to form a rectangular parallelepiped structure that penetrates from top to bottom; the upper end face and the lower end face of the rectangular parallelepiped structure are both use profiles, wherein the upper end face has the same curvature as the surface A of the component to be shaped, and the lower end face has the same curvature as the surface B of the component to be shaped;

[0011] A plurality of reinforcing ribs are arranged between the two beams, and the two ends of each reinforcing rib are respectively installed on the inner walls of the two beams, and the curvatures of the upper end face and the lower end face of the reinforcing rib are respectively consistent with the curvatures of the A face and the B face of the component to be calibrated;

[0012] The crimping assembly includes at least one first crimping part for crimping the B surface of the component to be shaped, and at least one second crimping part for crimping the A surface of the component to be shaped; the contact surfaces of the first crimping part, the second crimping part and the component to be shaped are respectively consistent with the curvature of the corresponding surface of the component to be shaped.

[0013] Furthermore, the first crimping part includes a first pressure strip and a second pressure strip, and the two ends of the first pressure strip and the second pressure strip are respectively connected by bolts to form a rectangular frame, which is used to be mounted on the outside of the rectangular structure; a plurality of first protrusions are evenly distributed on the inner side surface of the first pressure strip, and when the A surface of the component to be shaped contacts with the upper end surface of the base, the first protrusions are used to be crimped on the B surface of the component to be shaped, and the crimping surface has the same curvature as the B surface of the component to be shaped; the inner side surface of the second pressure strip has the same curvature as the lower end surface of the base.

[0014] Furthermore, the second crimping piece includes a third pressure strip and a fourth pressure strip, and the two ends of the third pressure strip and the fourth pressure strip are respectively connected by bolts to form a rectangular frame, which is used to be mounted on the outside of the rectangular structure; the inner side surface of the third pressure strip is evenly distributed with a plurality of second protrusions, and when the B surface of the component to be shaped contacts with the lower end surface of the base, the second protrusions are used to be crimped on the A surface of the component to be shaped, and the crimping surface has the same curvature as the A surface of the component to be shaped; the inner side surface of the fourth pressure strip has the same curvature as the upper end surface of the base.

[0015] Further, the upper and lower end surfaces of each of the cross beams, and the upper and lower end surfaces of the reinforcing ribs are respectively serrated, and the serrations at the corresponding positions of the upper and lower end surfaces of the cross beams, and the serrations at the corresponding positions of the upper and lower end surfaces of the reinforcing ribs are respectively arranged alternately, and the width of each serration is greater than the gap between two adjacent serrations;

[0016] The outer end faces of all the saw teeth located at the same end of the corresponding cross beam and the corresponding reinforcing rib are all in the same curved surface, and the curvature of the curved surface is consistent with the curvature of the corresponding surface of the component to be shaped.

[0017] Furthermore, it also includes two oblique beams arranged in an eight-shaped shape, one end of the two oblique beams is respectively connected to the middle part of one of the vertical beams, and the other end is respectively connected to the two horizontal beams;

[0018] The upper and lower end surfaces of one of the vertical beams are respectively provided with a third protrusion, and the inner side of the third protrusion is provided with a triangular groove for positioning the head of the component to be calibrated;

[0019] The upper and lower end faces of the inclined beam are respectively provided with a fourth protrusion, the outer end face of the fourth protrusion and the bottom of the triangular groove and the outer end faces of all the saw teeth on the same side are all in the same curved surface, and the curved surface has the same curvature as the corresponding surface of the component to be shaped.

[0020] Furthermore, it also includes a plurality of positioning protrusions arranged on the outer end surfaces of the serrations at the upper and lower ends of each beam, with intervals provided between adjacent positioning protrusions, and the number of positioning protrusions being less than the number of serrations on the corresponding beam; the inner side surface of the positioning protrusion is used to locate the outer contour of the component to be shaped, and is adapted to the structure corresponding to the outer contour.

[0021] Furthermore, the fourth protrusion and all the serrations are rectangular teeth or trapezoidal teeth, and have a height of 3-10 mm.

[0022] Furthermore, each of the cross beams, vertical beams and reinforcing ribs is provided with a weight-reducing hole, which can reduce the weight of the tooling and increase the gas passing rate, thereby improving the deposition efficiency.

[0023] At the same time, the present invention also provides a method for shaping a ceramic matrix composite material component with small curvature, comprising the following steps:

[0024] Step 1, preparing the ceramic matrix composite material small curvature component profiling tooling according to the size of the component to be profiling and the curvatures of its A surface and B surface;

[0025] Step 2: Place the A surface of the component to be shaped on the upper end surface of the base, and crimp the first crimping piece to the B surface of the component to be shaped, thereby achieving installation of the component to be shaped and the base;

[0026] Step 3: Place the installed component to be shaped together with the base and the first crimping part into a deposition furnace, complete a deposition according to the preset requirements, then take it out of the furnace and disassemble the first crimping part, and remove the component to be shaped from the base;

[0027] Step 4: Place the B surface of the component to be shaped on the lower end surface of the base, and crimp the second crimping piece to the A surface of the component to be shaped, thereby achieving installation of the component to be shaped and the base;

[0028] Step 5: Place the installed component to be shaped together with the base and the second crimping part into a deposition furnace, complete another deposition according to preset requirements, then take it out of the furnace and disassemble the second crimping part, and remove the component to be shaped from the base;

[0029] Step 6: Repeat steps 2 to 5 until the density of the component to be shaped reaches the expected value, thereby completing the shaping of the ceramic matrix composite material component with small curvature.

[0030] Further, step 2 is specifically as follows: placing the A surface of the component to be shaped on the upper end surface of the base, so that the head of the component to be shaped abuts in the triangular groove, and the side abuts against the inner side surface of the corresponding positioning protrusion, and pre-positioning is completed; then the inner side surface of the first pressure strip of the first crimping member is crimped to the B surface of the component to be shaped, and the inner side surface of the second pressure strip is crimped to the lower end surface of the base, and boron nitride powder is applied to the outer side of the bolt and then the bolt is tightened, thereby realizing the installation of the component to be shaped and the base;

[0031] Step 4 specifically includes placing the B surface of the component to be shaped on the lower end surface of the base, so that the head of the component to be shaped abuts against the triangular groove, and the side abuts against the inner side surface of the corresponding positioning protrusion to complete the pre-positioning; then the inner side surface of the third pressure strip of the second crimping piece is crimped to the A surface of the component to be shaped, and the inner side surface of the fourth pressure strip is crimped to the upper end surface of the base, and boron nitride powder is applied to the outside of the bolt and then the bolt is tightened to achieve the installation of the component to be shaped and the base.

[0032] Compared with the prior art, the present invention has the following beneficial effects:

[0033] 1. The shaping tool for small-curvature components of ceramic-based composite materials provided by the present invention designs the base to be a rectangular structure that runs through from top to bottom, and the upper end face and the lower end face of the rectangular structure are both use surfaces, and the curvatures of the two use surfaces are respectively consistent with the curvatures of the A surface and the B surface of the component to be shaped, and a plurality of reinforcing ribs are added to ensure the strength of the shaping tool, so that the entire shaping tool is in fit except for the contact with the component to be shaped, and the component to be shaped is connected to the base through a crimping assembly. This design can effectively prevent the component to be shaped from undergoing new deformation during the deposition process; at the same time, the non-contact areas between the shaping tool and the component to be shaped are both hollow designs, which ensures smooth airflow while making the overall weight of the shaping tool lighter, which is convenient for carrying operations in and out of the furnace.

[0034] 2. The ceramic-based composite material small-curvature component profiling tool provided by the present invention is an integrated dual-purpose tool, and the upper and lower surfaces can be used alternately. There is no need to prepare two sets of profiling tools, front and back, as with traditional profiling tools. While ensuring the uniformity of deposition on the front and back surfaces of ceramic composite parts, the production cost is reduced.

[0035] 3. The shaping tool for small-curvature components of ceramic-based composite materials provided by the present invention has a plurality of first protrusions (i.e., serrated) evenly distributed on the inner side surface of the first pressure strip, a plurality of second protrusions (i.e., serrated) evenly distributed on the inner side surface of the third pressure strip, and the upper and lower end surfaces of each beam and the upper and lower end surfaces of the reinforcing ribs are all serrated. By designing the contact surfaces of the shaping tool and the component to be shaped to be serrated, and the serrations on the upper and lower surfaces are staggered, different parts of the component to be shaped contact with the shaping tool during alternating deposition, so that no part of the component to be shaped will affect the deposition effect due to long-term contact with the shaping tool, thereby improving the deposition quality of the component to be shaped.

[0036] 4. The ceramic-based composite material small-curvature component profiling tool provided by the present invention has a third protrusion on one of the vertical beams for positioning the head of the component to be shaped; in addition, multiple positioning protrusions are provided on the outer end faces of the serrations on the upper and lower end faces of each cross beam for positioning the outer contour of the component to be shaped. The positioning method is simple and accurate, and can achieve the purpose of accurately profiling the parts.

[0037] 5. The shaping tool for small-curvature components of ceramic-based composite materials provided by the present invention is provided with weight-reducing holes on the crossbeam, vertical beam and reinforcing ribs respectively. The weight-reducing holes can not only reduce the overall weight of the shaping tool, but also allow the deposition gas to flow out to the side of the component to be shaped that contacts the base, thereby making both surfaces of the component to be shaped have a good deposition effect and improving the uniformity of deposition.

[0038] 6. The ceramic-based composite material small-curvature component shaping tool provided by the present invention has a simple connection method, is easy to disassemble, is convenient to operate, is not easily damaged, and can be reused many times.

[0039] 7. The ceramic-based composite material small-curvature component profiling tool provided by the present invention is suitable for ceramic-based composite material flat plates and thin-walled parts with small curvature. It has a wide range of applications and can prepare the base and the corresponding molding profile according to the different sizes and profiles of the components to be shaped. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 It is a structural schematic diagram of an embodiment of the present invention;

[0041] Figure 2 The structure of the base in the embodiment of the present invention is shown in FIG. Figure 1 ;

[0042] Figure 3 The structure of the base in the embodiment of the present invention is shown in FIG. Figure 2 ;

[0043] Figure 4 It is a schematic structural diagram of a first crimping member in an embodiment of the present invention;

[0044] Figure 5 It is a schematic structural diagram of a second crimping member in an embodiment of the present invention;

[0045] Figure 6 It is a structural schematic diagram of the component to be calibrated being installed on the upper surface of the base in an embodiment of the present invention;

[0046] Figure 7 It is a schematic structural diagram of the structure in which the component to be calibrated is installed on the lower surface of the base in an embodiment of the present invention.

[0047] The reference numerals are as follows:

[0048] 1-component to be shaped, 2-base, 3-crossbeam, 4-vertical beam, 41-third protrusion, 42-triangular groove, 5-reinforcement rib, 6-first crimping piece, 61-first pressure strip, 611-first protrusion, 62-second pressure strip, 7-second crimping piece, 71-third pressure strip, 711-second protrusion, 72-fourth pressure strip, 8-inclined beam, 81-fourth protrusion, 9-positioning protrusion. DETAILED DESCRIPTION

[0049] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.

[0050] like Figure 1 As shown, this embodiment provides a ceramic-based composite material small curvature component shaping tool, including a base 2 and a crimping assembly, the shaping tool is used to shape small curvature thin-walled components, and one of the surfaces of the component to be shaped 1 is defined as surface A, and the other surface is defined as surface B, and both surface A and surface B have small curvatures.

[0051] Combination Figure 2 and Figure 3 As shown, the base 2 includes two horizontal beams 3 and two vertical beams 4, and the thickness of the horizontal beams 3 and the vertical beams 4 is generally 6 to 20 mm. The two horizontal beams 3 are arranged in parallel, and the length is greater than the length of the vertical beams 4. The two ends of the two horizontal beams 3 in the length direction are respectively connected by two vertical beams 4 to form a rectangular structure that penetrates from top to bottom. The upper end face and the lower end face of the rectangular structure are both use molding surfaces, wherein the upper end face is consistent with the curvature of the A surface of the component 1 to be calibrated, and the lower end face is consistent with the curvature of the B surface of the component 1 to be calibrated, so as to ensure that the component 1 to be calibrated will not be deformed during the deposition process.

[0052] A plurality of reinforcing ribs 5 are arranged between the two cross beams 3, and the two ends of each reinforcing rib 5 are respectively installed on the inner walls of the two cross beams 3, and are used to support the component to be shaped 1; the curvatures of the upper and lower end surfaces of the reinforcing rib 5 are respectively consistent with the curvatures of the A surface and the B surface of the component to be shaped 1. The number and width of the reinforcing ribs 5 can be determined according to the size and specific shape of the component to be shaped 1, which can strengthen the strength of the base 2 on the one hand, and improve the supporting effect of the middle area of ​​the component to be shaped 1 on the other hand.

[0053] In this embodiment, the width of the reinforcing rib 5 is 12 mm, the thickness of the horizontal beam 3 and the vertical beam 4 is 10 mm, the width of the saw teeth is 10 mm, and the width between two adjacent saw teeth is 8 mm.

[0054] Each cross beam 3, vertical beam 4 and reinforcing rib 5 is respectively provided with a weight-reducing hole. On the one hand, the weight of the shaping tool base 2 is reduced. On the other hand, a part of the deposition airflow can flow out through the weight-reducing hole to the bottom surface of the component to be shaped 1 (the contact surface with the shaping tool base 2), so that both surfaces of the component to be shaped 1 can have a better deposition effect, thereby controlling the deformation of the parts and improving the uniformity of the part deposition.

[0055] The crimping assembly includes three first crimping parts 6 for crimping the B surface of the component 1 to be calibrated, and three second crimping parts 7 for crimping the A surface of the component 1 to be calibrated; the contact surfaces of the first crimping parts 6, the second crimping parts 7 and the component 1 to be calibrated are respectively consistent with the curvature of the corresponding surfaces of the component 1 to be calibrated.

[0056] like Figure 4 As shown, each first crimping member 6 includes a first pressure strip 61 and a second pressure strip 62, and the two ends of the first pressure strip 61 and the second pressure strip 62 are respectively connected by bolts to form a rectangular frame, which is used to be mounted on the outside of the rectangular structure. The inner side surface of the first pressure strip 61 is evenly distributed with a plurality of first protrusions 611. When the A surface of the component 1 to be shaped contacts the upper end surface of the base 2, the first protrusions 611 are used to be crimped on the B surface of the component 1 to be shaped, and the crimping surface has the same curvature as the B surface of the component 1 to be shaped. The inner side surface of the second pressure strip 62 contacts the lower end surface of the base 2, and the curvatures of the two are the same, and there is no need to process it into a serrated shape.

[0057] like Figure 5 As shown, each second crimping member 7 includes a third pressure strip 71 and a fourth pressure strip 72, and the two ends of the third pressure strip 71 and the fourth pressure strip 72 are respectively connected by bolts to form a rectangular frame, which is used to be sleeved on the outside of the rectangular structure. The inner side surface of the third pressure strip 71 is evenly distributed with a plurality of second protrusions 711. When the B surface of the component 1 to be shaped contacts the lower end surface of the base 2, the second protrusions 711 are used to be crimped on the A surface of the component 1 to be shaped, and the crimping surface has the same curvature as the A surface of the component 1 to be shaped. The inner side surface of the fourth pressure strip 72 contacts the upper end surface of the base 2, and the curvatures of the two are consistent, so it is not necessary to process it into a serrated shape.

[0058] The upper and lower end faces of each cross beam 3 and the upper and lower end faces of the reinforcing rib 5 are respectively serrated, and the serrations at the corresponding positions of the upper and lower end faces of the cross beam 3 and the upper and lower end faces of the reinforcing rib 5 are arranged alternately, and the width of each serration is greater than the gap between two adjacent serrations. All serrations are rectangular teeth or trapezoidal teeth, and the height is 3 to 10 mm.

[0059] The outer end faces of all saw teeth located at the same end of the corresponding crossbeam 3 and the corresponding reinforcing rib 5 (i.e. the end of the saw teeth away from the corresponding crossbeam 3 or reinforcing rib 5) are all in the same curved surface, and the curved surface has the same curvature as the corresponding surface of the component 1 to be shaped.

[0060] like Figure 3 As shown, this embodiment further includes two oblique beams 8 arranged in an eight-shaped pattern, one end of each of the two oblique beams 8 is connected to the middle of one of the vertical beams 4, and the other end is connected to the two cross beams 3. The upper and lower end surfaces of one of the vertical beams 4 are respectively provided with a third protrusion 41, and the inner side of the third protrusion 41 is provided with a triangular groove 42 for positioning the head of the component 1 to be calibrated.

[0061] The upper and lower end surfaces of the inclined beam 8 are respectively provided with fourth protrusions 81, which are rectangular teeth or trapezoidal teeth with a height of 3 to 10 mm. The outer end surface of the fourth protrusion 81 and the bottom of the triangular groove 42 and the outer end surfaces of all the saw teeth on the same side are all in the same curved surface, and the curvature of the curved surface is consistent with the curvature of the corresponding surface of the component 1 to be calibrated.

[0062] In order to accurately position the part to be shaped in the width direction, the present embodiment further includes 2 to 8 positioning protrusions 9 arranged at intervals on the outer end faces of the saw teeth at the upper and lower ends of each beam 3 (i.e., the end of the saw teeth away from the beam), and the number of positioning protrusions 9 is less than the number of saw teeth on the corresponding beam 3. The width of the positioning protrusion 9 is less than the width of the corresponding saw teeth, and the thickness is less than the thickness of the corresponding saw teeth (i.e., the positioning protrusion 9 and the corresponding saw teeth form a step structure), so the inner side surface of the positioning protrusion 9 can be used to locate the outer contour of the component 1 to be shaped, and is adapted to the structure corresponding to the outer contour.

[0063] The shaping tooling of this embodiment is made of high-strength fine graphite, that is, the base 2, the first pressure strip 61, the second pressure strip 62, the third pressure strip 71, the fourth pressure strip 72, the inclined beam 8, etc. are all made of high-strength fine graphite.

[0064] Combination Figures 1 to 7 This embodiment also provides a method for calibrating a ceramic matrix composite material component with a small curvature, comprising the following steps:

[0065] Step 1: According to the size of the component 1 to be shaped and the curvatures of its A and B surfaces, a corresponding ceramic-based composite material small-curvature component shaping tool (i.e., the shaping tool described in this embodiment) is prepared in advance.

[0066] Step 2: Place the A surface of the component to be shaped 1 on the upper end surface of the base 2, and crimp the first crimping member 6 to the B surface of the component to be shaped 1, so as to achieve the installation of the component to be shaped 1 and the base 2 ( Figure 6 shown).

[0067] Specifically, place the A surface of the component 1 to be shaped on the upper end surface of the base 2 (at this time, the B surface is exposed to the outside), so that the head of the component 1 to be shaped abuts against the triangular groove 42, and the side abuts against the inner side surface of the corresponding positioning protrusion 9, thereby completing the pre-positioning; then crimp the inner side surface of the first pressure strip 61 of each group of first crimping parts 6 to the B surface of the component 1 to be shaped, and crimp the inner side surface of the second pressure strip 62 to the lower end surface of the base 2, and apply BN powder to the connection between the bolts and the nuts, so that the bolts and nuts can be easily disassembled after being taken out of the furnace; then tighten the bolts, and when the second pressure strip 62 coincides with the limiting groove on the cross beam 3 of the base 2, connect them in place (generally, each group of first pressure strips 61 and second pressure strips 62 corresponds to the position of the corresponding reinforcing ribs 5), thereby realizing the installation of the component 1 to be shaped and the base 2.

[0068] Step 3: Place the installed component to be shaped 1 together with the base 2 and the first crimping part 6 into the deposition furnace, lean it against the chemical vapor deposition furnace, complete a deposition according to the preset requirements, then take it out of the furnace and disassemble the first crimping part 6, remove the component to be shaped 1 from the base 2, and use an air gun, brush or other tools to clean the scum on the surface of the component to be shaped 1 and the surface of the shaping tooling.

[0069] Step 4: Place the B surface of the component to be shaped 1 on the lower end surface of the base 2, and crimp the second crimping piece 7 to the A surface of the component to be shaped 1, so as to achieve the installation of the component to be shaped 1 and the base 2 ( Figure 7 shown).

[0070] Specifically, the base 2 is turned over, and the B surface of the component 1 to be shaped is placed on the lower end surface of the base 2 (at this time, the A surface is exposed to the outside), so that the head of the component 1 to be shaped is abutted in the triangular groove 42, and the side is abutted against the inner side surface of the corresponding positioning protrusion 9, and the pre-positioning is completed. Then the inner side surface of the third pressure strip 71 of each group of second crimping parts 7 is crimped to the A surface of the component 1 to be shaped, and the inner side surface of the fourth pressure strip 72 is crimped to the upper end surface of the base 2, and BN powder is applied to the connection between the bolt and the nut to avoid the adhesion of the bolt after chemical vapor deposition, so that the bolt and the nut can be easily disassembled after being taken out of the furnace; then tighten the bolt, and when the fourth pressure strip 72 coincides with the limiting groove on the cross beam 3 of the base 2, connect it in place (generally, each group of the third pressure strip 71 and the fourth pressure strip 72 corresponds to the position of the corresponding reinforcing rib 5), thereby realizing the installation of the component 1 to be shaped and the base 2.

[0071] Step 5: Place the installed component to be shaped 1 together with the base 2 and the second crimping part 7 into the deposition furnace, complete another deposition according to the preset requirements, then take it out of the furnace and remove the second crimping part 7, remove the component to be shaped 1 from the base 2, and use an air gun, brush or other tools to clean the scum on the surface of the component to be shaped 1 and the surface of the shaping tooling.

[0072] Step 6, repeating steps 2 to 5, re-installing the surface after each deposition, until the density of the component 1 to be shaped reaches the expected value, thereby completing the shaping of the small curvature component of the ceramic matrix composite material.

[0073] The preferred implementation modes of the present invention are introduced above. Those skilled in the art may make various modifications or additions to the described specific embodiments or replace them in a similar manner. As long as they do not deviate from the structure of the present invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.

Claims

1. A ceramic matrix composite material small curvature component shaping tool, used for shaping small curvature thin-walled components, defining one surface of the component to be shaped (1) as surface A and the other surface as surface B; characterized in that: It comprises a base (2) and a crimping assembly; The base (2) comprises two horizontal beams (3) and two vertical beams (4); the two horizontal beams (3) are arranged in parallel and have a length greater than that of the vertical beams (4); the two ends of the two horizontal beams (3) in the length direction are respectively connected by two vertical beams (4) to form a rectangular parallelepiped structure that is connected from top to bottom; the upper end face and the lower end face of the rectangular parallelepiped structure are both use profiles, wherein the upper end face has the same curvature as the A surface of the component to be shaped (1), and the lower end face has the same curvature as the B surface of the component to be shaped (1); A plurality of reinforcing ribs (5) are provided between the two cross beams (3), and the two ends of each reinforcing rib (5) are respectively mounted on the inner walls of the two cross beams (3), and the curvatures of the upper end surface and the lower end surface of the reinforcing rib (5) are respectively consistent with the curvatures of the A surface and the B surface of the component to be shaped (1); The crimping assembly comprises at least one first crimping piece (6) for crimping the B surface of the component to be calibrated (1), and at least one second crimping piece (7) for crimping the A surface of the component to be calibrated (1); the contact surfaces of the first crimping piece (6), the second crimping piece (7) and the component to be calibrated (1) are respectively consistent with the curvature of the corresponding surface of the component to be calibrated (1).

2. The ceramic matrix composite material small curvature component shaping tool according to claim 1, characterized in that: The first crimping member (6) comprises a first pressure strip (61) and a second pressure strip (62), the two ends of which are respectively connected by bolts to form a rectangular frame, which is used to be sleeved on the outer side of the rectangular structure; the inner side surface of the first pressure strip (61) is evenly distributed with a plurality of first protrusions (611), and when the A surface of the component to be shaped (1) contacts the upper end surface of the base (2), the first protrusions (611) are used to be crimped on the B surface of the component to be shaped (1), and the crimping surface has the same curvature as the B surface of the component to be shaped (1); the inner side surface of the second pressure strip (62) has the same curvature as the lower end surface of the base (2).

3. The ceramic matrix composite material small curvature component shaping tool according to claim 1, characterized in that: The second crimping member (7) comprises a third pressure strip (71) and a fourth pressure strip (72), the two ends of which are respectively connected by bolts to form a rectangular frame, which is used to be sleeved on the outer side of the rectangular structure; the inner side surface of the third pressure strip (71) is evenly distributed with a plurality of second protrusions (711), and when the B surface of the component to be shaped (1) contacts the lower end surface of the base (2), the second protrusions (711) are used to be crimped onto the A surface of the component to be shaped (1), and the crimping surface has the same curvature as the A surface of the component to be shaped (1); the inner side surface of the fourth pressure strip (72) has the same curvature as the upper end surface of the base (2).

4. The ceramic matrix composite material small curvature component shaping tool according to claim 1, 2 or 3, characterized in that: The upper and lower end surfaces of each of the cross beams (3) and the upper and lower end surfaces of the reinforcing ribs (5) are respectively serrated, the serrations at the corresponding positions of the upper and lower end surfaces of the cross beams (3) and the serrations at the corresponding positions of the upper and lower end surfaces of the reinforcing ribs (5) are respectively arranged in a staggered manner, and the width of each serration is greater than the gap between two adjacent serrations; The outer end faces of all the saw teeth located at the same end of the corresponding cross beam (3) and the corresponding reinforcing rib (5) are all located within the same curved surface, and the curvature of the curved surface is consistent with the curvature of the corresponding surface of the component to be shaped (1).

5. The ceramic matrix composite material small curvature component shaping tool according to claim 4, characterized in that: It also includes two oblique beams (8) arranged in an eight-shaped pattern, one end of the two oblique beams (8) is respectively connected to the middle of one of the vertical beams (4), and the other end is respectively connected to the two horizontal beams (3); The upper and lower end surfaces of one of the vertical beams (4) are respectively provided with a third protrusion (41), and the inner side of the third protrusion (41) is provided with a triangular groove (42) for positioning the head of the component to be calibrated (1); The upper and lower end surfaces of the inclined beam (8) are respectively provided with fourth protrusions (81); the outer end surface of the fourth protrusion (81) and the bottom of the triangular groove (42), as well as the outer end surfaces of all saw teeth on the same side, are all located in the same curved surface, and the curvature of the curved surface is consistent with the curvature of the corresponding surface of the component to be shaped (1).

6. The ceramic matrix composite material small curvature component shaping tool according to claim 5, characterized in that: It also includes a plurality of positioning protrusions (9) arranged on the outer end surfaces of the saw teeth at the upper and lower ends of each crossbeam (3), with intervals between adjacent positioning protrusions (9), and the number of positioning protrusions (9) is less than the number of saw teeth on the corresponding crossbeam (3); the inner side surface of the positioning protrusion (9) is used to locate the outer contour of the component (1) to be calibrated, and is adapted to the structure corresponding to the outer contour.

7. The ceramic matrix composite material small curvature component shaping tool according to claim 6, characterized in that: The fourth protrusion (81) and all the saw teeth are rectangular teeth or trapezoidal teeth, and the height is 3-10 mm.

8. The ceramic matrix composite material small curvature component shaping tool according to claim 1, characterized in that: Each of the cross beam (3), vertical beam (4) and reinforcing rib (5) is respectively provided with a weight-reducing hole.

9. A method for shaping a small-curvature component of a ceramic-based composite material, characterized in that: The following steps are involved: Step 1: prepare a shaping tool for a ceramic-based composite material component with small curvature as claimed in any one of claims 1 to 8 according to the size of the component to be shaped (1) and the curvatures of its A surface and B surface; Step 2: Place the A surface of the component to be shaped (1) on the upper end surface of the base (2), and crimp the first crimping piece (6) to the B surface of the component to be shaped (1), thereby achieving the installation of the component to be shaped (1) and the base (2); Step 3, placing the installed component to be shaped (1) together with the base (2) and the first crimping part (6) into a deposition furnace, completing a deposition according to preset requirements, then taking it out of the furnace and disassembling the first crimping part (6), and removing the component to be shaped (1) from the base (2); Step 4: Place the B surface of the component to be shaped (1) on the lower end surface of the base (2), and crimp the second crimping piece (7) to the A surface of the component to be shaped (1), thereby achieving the installation of the component to be shaped (1) and the base (2); Step 5: Place the installed component to be shaped (1) together with the base (2) and the second crimping part (7) into a deposition furnace, complete another deposition according to preset requirements, then take it out of the furnace and disassemble the second crimping part (7), and remove the component to be shaped (1) from the base (2); Step 6, repeating steps 2 to 5 until the density of the component to be shaped (1) reaches the expected value, thereby completing the shaping of the ceramic matrix composite material component with small curvature.

10. The method for shaping a ceramic matrix composite material component with small curvature according to claim 9, characterized in that: Step 2 specifically comprises placing the A surface of the component to be shaped (1) on the upper end surface of the base (2), so that the head of the component to be shaped (1) abuts against the inside of the triangular groove (42), and the side abuts against the inner side surface of the corresponding positioning protrusion (9), thereby completing the pre-positioning; then the inner side surface of the first pressure strip (61) of the first crimping member (6) is crimped against the B surface of the component to be shaped (1), and the inner side surface of the second pressure strip (62) is crimped against the lower end surface of the base (2), and the bolts are tightened, thereby achieving the installation of the component to be shaped (1) and the base (2); Step 4 specifically comprises placing the B surface of the component to be shaped (1) on the lower end surface of the base (2), so that the head of the component to be shaped (1) abuts against the inside of the triangular groove (42), and the side abuts against the inner side surface of the corresponding positioning protrusion (9), thereby completing the pre-positioning; then the inner side surface of the third pressure strip (71) of the second crimping member (7) is crimped against the A surface of the component to be shaped (1), and the inner side surface of the fourth pressure strip (72) is crimped against the upper end surface of the base (2), and the bolts are tightened, thereby realizing the installation of the component to be shaped (1) and the base (2).