Tray thermal forming curling equipment and method

Through the mold heating of the pallet thermoforming curling equipment and the cooperation of the press plate top plate, the closed semicircular curling of the outer edge of the blister pallet is realized, solving the problems of sharp edges and insufficient strength in the prior art, protecting the human body and packaging. Improve product quality and production efficiency.

CN119058067APending Publication Date: 2024-12-03HONEST MOULD &PLASTICS CO (SHENZHEN) LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411323875.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-23
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The outer edges of existing blister pallets are sharp and sharp, making it difficult to achieve closed semicircular curling, which has the potential to cut the human body and the outer seal packaging film, and the curling structure is insufficient.

Method used

A pallet thermoforming and curling equipment is designed, and the edge-curling is heated by molds, including hot molds and cold molds. Through the cooperation of the press plate and the top plate, a closed semicircular curling edge of the outer edge of the pallet is realized.

Benefits of technology

Effectively protect the human body and the outer seal packaging film from sharp edges, enhance the overall load-bearing capacity of the pallet, reduce production costs and energy consumption, and improve product quality and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119058067A_ABST
    Figure CN119058067A_ABST
Patent Text Reader

Abstract

The equipment comprises a workbench, a crimping die, a pressing plate, a top plate, a control box and a start-stop switch, the crimping die comprises a hot die and a cold forming die, the crimping die further comprises a pressing plate air cylinder, a top plate air cylinder, a hot die heating mechanism and a cold die refrigerating mechanism; a tray product is pressed into the hemming die through the pressing plate, the product is deformed in the descending process through the structure and temperature control of the hot die and the cold forming die, and hemming and shaping are achieved. According to the produced curled plastic uptake tray, curled edges are bent to be close to right angles, the modeling effect is good, the human body and an outer sealing packaging film can be protected against damage, the bearing capacity of products is improved, reasonable stacking intervals of the products are formed, and the curled plastic uptake tray is suitable for curled edge forming of plastic uptake forming tray type food packaging boxes made of PET, PVC, PP, PS and other materials.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of blister tray production, and in particular to a tray thermoforming curling device and method. Background Art

[0002] Blister trays are mainly made of various plastic materials such as PET, PVC, PP, PS, etc., produced through blister and punching processes. They are used for separation, shockproofing, and as a foil. The products packaged in them can include toys, stationery, food, handicrafts, cosmetics, and other fields.

[0003] At present, the outer edges of most blister trays on the market are directly punched out with a blade, which is sharp and pointed, and there is a hidden danger of cutting the human body and the outer packaging film. Especially for food packaging, cutting the outer packaging film is likely to affect the shelf life and appearance of the packaged product.

[0004] It is understood that there is also a process for curling the outer edge of the blister tray, but it is impossible to achieve a closed semi-circular curling in which the outer edge is bent downward, then inward and curled upward again. Instead, it is an open curling that curls downward. Such a curling structure has insufficient strength, and there is still a risk of sharp edges cutting the human body and the outer packaging film.

[0005] Therefore, it is necessary to develop a production equipment that can curl the sharp and pointed parts of the outer edge of the blister tray into a closed semicircular curled edge, so that the human body and the outer packaging film are prevented from contacting, thereby protecting the human body from injury and reducing the impact of damage to the outer packaging film. Summary of the invention

[0006] The purpose of the present invention is to provide a tray thermoforming curling device and method to address the defects of the prior art, which realizes the closed semicircular curling of the blister tray by heating the mold to solve the problems raised in the background technology.

[0007] In order to achieve the above object, the present invention proposes the following technical solutions: The pallet hot forming curling equipment comprises a workbench, a curling mold, a pressing plate, a top plate, a control box and a start-stop switch, wherein the curling mold comprises a hot mold and a cold forming mold, wherein the cold forming mold is fixedly mounted on the workbench, wherein the hot mold is fixedly mounted above the cold forming mold, wherein the pressing plate is arranged above the hot mold, wherein a pressing plate cylinder is arranged above the pressing plate, wherein the pressing plate cylinder is fixedly mounted on the workbench through a column, wherein the pressing plate cylinder can control the pressing plate to move downward and upward, wherein the pressing plate is used to press the pallet product downward into the curling mold for curling forming, wherein the top plate is mounted inside the cold forming mold and is provided with a top plate cylinder, wherein the pressing plate cylinder can control the pressing plate to move downward and upward The top plate moves upward and downward, and the top plate is used to push the pallet product after curling forming upward; the hot mold is provided with a heating mechanism, and the cold forming mold is provided with a refrigeration mechanism. The control box is connected with the heating mechanism and the refrigeration mechanism, and is used to set the temperature parameters of the heating mechanism and the refrigeration mechanism. The control box is also connected with the pressure plate cylinder and the top plate cylinder, and is used to set the speed parameters of the pressure plate cylinder and the top plate cylinder. The start-stop switch is installed on the side of the workbench and is connected with the control box, and is used to control the opening and closing of the pallet thermoforming and curling equipment. The pallet thermoforming and curling equipment is also provided with a power supply device.

[0008] Furthermore, the hot mold is a hollow square structure, the middle of which can allow the pallet product to pass through, a sloped opening is provided on the upper part of the inner wall, the inner wall is a vertical surface, and mounting feet are provided at the four corners below; the cold forming mold is a box-shaped structure, which can accommodate the pallet product inside, a curling forming groove is provided on the inner side of the upper part, and mounting columns are provided at the four corners of the upper surface; the mounting feet of the hot mold are connected to the mounting columns of the cold forming mold for installation and fixation.

[0009] Furthermore, the top plate is a concave structure, and the inner side surface is an arc-shaped protective wall, which is used to adapt to the bottom shape of the pallet product to support the pallet product; the bottom surface of the top plate is provided with a cylinder mounting position 1 and a push rod hole 1, and the bottom surface of the cold forming mold is provided with a cylinder mounting position 2 and a push rod hole 2. The cylinder mounting position 1 and the cylinder mounting position 2 are aligned during installation and are used to install the top plate cylinder; the push rod hole 1 and the push rod hole 2 are centrally aligned during installation and are used to install the push rod, and the push rod is used to lift the top plate upward or pull it back downward through the action of the push rod cylinder; the bottom surface of the cold forming mold is also provided with a mounting hole, which is used to fix the cold forming mold on the workbench.

[0010] Furthermore, the curling forming groove of the cold forming die is a continuous groove extending around the inner edge of the upper part of the cold forming die, and is used to curl the outer edge of the pallet product. According to needs, the curling of the pallet product includes three shapes: 1 / 3 semicircle, semicircle, and 2 / 3 semicircle, which are completed by setting the curling forming groove accordingly.

[0011] Furthermore, the pressure plate cylinder provided on the pressure plate has an air pressure of 5-8kg and is controlled by a solenoid valve; the bottom plate of the pressure plate in contact with the pallet product is made of an insulating plate material.

[0012] Furthermore, the top plate cylinder provided on the top plate has an air pressure of 5-8kg.

[0013] Furthermore, the heating mechanism of the hot mold is a heating tube arranged on the outside of the upper half of the hot mold, which is used to heat the hot mold, and its working temperature is controlled by a temperature control meter and a thyristor; the refrigeration mechanism includes a water circulation pipeline arranged around the outside of the cold forming mold, and an industrial water chiller, and the industrial water chiller is used to control the working temperature of the cold forming mold.

[0014] In order to achieve the curling of the pallet product, the dimensions of the pressing plate, hot mold, cold forming mold and the pallet product need to be matched. Taking the long side of the pallet product when viewed from above as an example, the outer width of the pallet product before curling is recorded as a, and the outer width of the pallet product after curling is recorded as b; the bottom plate of the pressing plate that contacts the upper surface of the pallet product has a width of b, and the periphery of the bottom plate of the pressing plate is also provided with a skirt, which is made of soft plastic material, and the width of the skirt on both sides plus the width of the bottom plate is a; the upper edge width of the upper slope opening of the hot mold is a, the lower edge width is b, and the inner wall width is b; the inner wall width of the cold forming mold plus the width of the curling forming groove is b, and the lower edge of the inner wall of the hot mold is aligned with the outer edge of the curling forming groove of the cold forming mold; the relationship between the short side of the pallet product when viewed from above and the dimensions of the pressing plate, hot mold and cold forming mold is similar.

[0015] Based on the tray thermoforming and curling equipment, the present invention provides a tray thermoforming and curling method, comprising the following steps: S1. Start the heating mechanism and cooling mechanism of the tray thermoforming and curling equipment to make the hot mold and the cold forming mold reach the predetermined high temperature and low temperature range respectively; S2. The operator puts the pallet product to be curled into the curling mold so that the upper edge of the pallet product contacts the upper edge of the hot mold, that is, the upper edge of the slope opening; S3. Press the start switch, the pressure plate cylinder pushes the pressure plate downward, and the bottom plate of the pressure plate stops after it touches the upper edge of the pallet product; the pressure plate pushes the pallet product downward into the hot film, and uses the high temperature of the inner wall of the hot mold to heat and bend the part to be curled, until the pallet product is pushed into the cold forming mold, and the curled bottom of its upper edge touches the curling forming groove. S4, the pressing plate continues to press down, and in the process of continuous downward movement, it enters the curling forming groove and curls inward to form a curling shape, until the bottom of the tray product is supported by the top plate, and then pauses, and the curling is cooled and formed by the low temperature of the inner wall of the cold forming mold; S5, after the pallet product is curled and shaped, the pressure plate returns to the upper initial position, the top plate cylinder is activated to lift the top plate, and the pallet product is pushed above the curling mold, and the operator takes it out.

[0016] Wherein, step S3 specifically includes the following steps: S31, the pressing plate pushes the pallet product downward, during which the outer edge of the pallet product contacts the inner wall of the hot film and becomes soft due to the heat. Since the outer skirt of the pressing plate bottom plate presses the outer edge of the pallet product, the outer edge bends downward while the width of the ramp opening gradually decreases, until the pallet product is pushed to the first set position in the hot mold, that is, the upper edge of the pallet product is aligned with the lower edge of the hot mold ramp opening, and then pauses; the pressing plate bottom skirt is compressed and contracted during the downward process, and is compressed when it is aligned with the lower edge of the hot mold ramp opening; S32, the pressing plate continues to push the tray product downward until the tray product is pushed to the second set position in the hot mold, and then pauses; S33, the pressing plate continues to push the pallet product downward until the pallet product is pushed to the third set position in the hot mold, that is, the pallet product enters the cold forming mold, and the curled bottom of its upper edge contacts the curling forming groove, and pauses.

[0017] During the implementation of the above-mentioned tray thermoforming curling method, the temperature of the hot mold is controlled between 70° and 110°, and the temperature of the cold forming mold is controlled between 1° and 10°.

[0018] The angle between the inclined surface of the hot mold slope opening and the vertical surface is 30° to 60°.

[0019] In the above step S3, the pressing plate moves down three times, each time for 1-4 seconds, and the tray product pauses in the hot mold three times, each time for 0.1-2 seconds.

[0020] In the above operation, the principle of the curling of the pallet product is: the curling of the pallet product should be able to eventually form a predetermined shape. The difficulty lies in the first bend of the curling, which should be able to form a right angle. The smaller the radius of the bending angle, the better. At the same time, the part to be curled needs to be fully heated and softened, so that it can smoothly curl along the bottom curved surface of the groove when the outer edge enters the curling forming groove, and finally cool and shape. Through the mold structure design and operation method design of the present invention, the outer edge of the pallet product can be effectively bent downward due to the high temperature of the inner wall of the heated mold, the slope of the hot mold slope opening, the downward pressure of the pressing plate, and the effect of the outer skirt of the pressing plate floor; through three times of pressing down and pausing, because the pallet product itself has a certain elasticity, the bent part of the outer edge of the pallet product is close to the inner wall of the hot mold, and the bending angle becomes smaller and smaller, close to a right angle; when the outer edge of the pallet product contacts the curling forming groove, it has been fully heated.

[0021] Compared with the prior art, the present invention has the following beneficial effects: 1. After the pallet is curled, the human body and the outer packaging film are protected from the sharp outer edges and are not easily damaged, which will not cause the packaged products to deteriorate or affect their appearance. 2. The outer edges of the pallet are curled into a semicircle, which also increases the overall load-bearing capacity of the pallet; 3. Through the shaping of the curling die and the control of the production process parameters, the pallet products are curled into 1 / 3 semicircle, half circle, and 2 / 3 semicircle, forming the different stacking spacing required by the product on the terminal packaging production line, making the product smoother to use on the automatic packaging production line of downstream customers; 4. The present invention is applicable to all blister-formed tray-type food packaging boxes made of PET, PVC, PP, and PS materials; 5. The automatic production equipment and method for vacuum forming, punching and curling provided by the present invention produce curling products with lower labor cost than traditional processes, which is only 1 / 10 of the traditional process, lower energy consumption, 90% electricity saving, higher quality and fewer defective products; 6. The design of the sloped opening of the hot mold, the vertical inner wall, the outer skirt of the pressure plate floor, and the design of the pallet product being pressed down and paused three times in the hot mold make the bending angle of the outer edge of the pallet product small, close to a right angle, and have a good molding effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 This is a schematic diagram of the structure of the tray thermoforming equipment of the present invention; Figure 2 It is a schematic diagram of the hot mold structure; Figure 3 It is a schematic diagram of the structure of the heat mold from another angle; Figure 4 It is a schematic diagram of the cold forming die structure; Figure 5 This is a schematic diagram of the cold forming die structure from another angle; Figure 6 is a schematic diagram of the top plate structure; Figure 7 This is a schematic diagram of the pallet product structure; Figure 8 Schematic diagram of three types of curling edges for pallet products; Fig. 9 It is a cross-sectional view of the curling die during curling forming; Fig.10 for Fig. 9 Middle A is a partial enlarged view; Fig.11 It is a schematic diagram of the structural relationship between the pressing plate, the curling die, the pallet product and the top plate; Fig.12 Schematic diagram of the curling forming process.

[0023] Explanations in the figure: 1. Workbench; 2. Curling mold; 3. Press plate; 31. Bottom plate; 32. Skirt; 4. Top plate; 41. Arc-shaped wall guard; 42. Cylinder installation position one; 43. Push rod hole one; 5. Control box; 6. Start-stop switch; 7. Hot mold; 71. Sloped opening; 72. Mounting foot; 8. Cold forming mold; 81. Mounting column; 82. Curling forming groove; 83. Cylinder installation position two; 84. Push rod hole two; 85. Mounting hole; 9. Press plate cylinder; 10. Top plate cylinder; 11. Pallet product; 111. Curling; 12. Power supply unit; P1-4, positioning point. DETAILED DESCRIPTION

[0024] The present invention is further described below through the accompanying drawings and embodiments, but they are not intended to limit the present invention.

[0025] like Figure 1 As shown, the present invention provides a pallet hot forming curling device, including a workbench 1, a curling mold 2, a pressing plate 3, a top plate 4, a control box 5 and a start-stop switch 6. The curling mold 2 includes a hot mold 7 and a cold forming mold 8. The cold forming mold 8 is fixedly installed on the workbench 1, and the hot mold 7 is fixedly installed above the cold forming mold 8. The pressing plate 3 is arranged above the hot mold 7. A pressing plate cylinder 9 is arranged above the pressing plate 3. The pressing plate cylinder 3 is fixedly installed on the workbench 1 through a column. The pressing plate cylinder 9 can control the pressing plate 3 to move downward and upward. The pressing plate 3 is used to press the pallet product 11 downward into the curling mold 2 for curling forming. The top plate 4 is installed inside the cold forming mold 2 and is provided with a top plate cylinder 10, can control the upward and downward movement of the top plate 4, the top plate 4 is used to push the pallet product after curling forming upward 11; the hot mold 7 is provided with a heating mechanism, the cold forming mold 8 is provided with a refrigeration mechanism, the control box 5 is connected with the heating mechanism and the refrigeration mechanism, and is used to set the temperature parameters of the heating mechanism and the refrigeration mechanism, the control box 5 is also connected with the pressing plate cylinder 9 and the top plate cylinder 10, and is used to set the speed parameters of the pressing plate cylinder 9 and the top plate cylinder 10, the start-stop switch 6 is installed on the side of the workbench 1, and is connected with the control box 5, and is used to control the opening and closing of the pallet thermoforming and curling equipment, and the pallet thermoforming and curling equipment is also provided with a power supply device 12.

[0026] Combination Figure 1-5 As shown, the hot mold 7 is a hollow square structure, the middle of which can allow the pallet product to pass through, a slope opening 71 is provided on the upper part of the inner wall, the inner wall is a vertical surface, and mounting feet 72 are provided at the four corners below; the cold forming mold 8 is a box-shaped structure, which can accommodate the pallet product inside, a curling forming groove 82 is provided on the inner side of the upper part, and mounting columns 81 are provided at the four corners of the upper surface; the mounting feet 72 of the hot mold are connected to the mounting columns 81 of the cold forming mold for installation and fixation.

[0027] Combination Figure 1 , Figure 5 , Figure 6As shown, the top plate 4 is a concave structure, and the inner side surface is an arc-shaped protective wall 41, which is used to adapt to the bottom shape of the pallet product to support the pallet product; the bottom surface of the top plate 4 is provided with a cylinder mounting position 42 and a push rod hole 43; the bottom surface of the cold forming mold 8 is provided with a cylinder mounting position 83 and a push rod hole 84, and the cylinder mounting position 42 and the cylinder mounting position 83 are aligned when the top plate 4 is installed inside the cold forming mold 8, and are used to install the top plate cylinder 10; the push rod hole 43 and the push rod hole 84 are aligned in the center during installation, and are used to install the push rod, and the push rod 4 is used to lift the top plate 4 upward or pull it back downward through the action of the push rod cylinder 10; the bottom surface of the cold forming mold 8 is also provided with a mounting hole 85, which is used to fix the cold forming mold 8 on the workbench 1.

[0028] like Figure 7 As shown, the upper outer edge of the tray product 11 forms a curling edge 111 after the curling is formed. Figure 7-8 As shown, the pallet product curling edge 111 includes three shapes: 1 / 3 semicircle, half circle, and 2 / 3 semicircle, corresponding to Figure 8 (a), (b), and (c) in . Figure 4-5 , Figure 9-10 The curling groove 82 of the cold forming die 8 is a continuous groove extending around the inner edge of the upper portion of the cold forming die 8, and is used to curl the outer edge of the pallet product. Figure 8 As shown, according to needs, the curling forming groove is set to three shapes of 1 / 3 semicircle, semicircle, and 2 / 3 semicircle.

[0029] In this embodiment, the pressure plate cylinder 9 arranged above the pressure plate 3 is controlled by a solenoid valve, the air pressure is set to 6kg, and the bottom plate is made of insulating board material; the air pressure of the top plate cylinder arranged below the top plate 4 is 5kg. A heating pipe is arranged on the outer side of the upper half of the hot mold 7, and its working temperature is controlled by a temperature control meter and a thyristor; a water circulation pipeline is arranged around the outside of the cold forming mold 8, and the temperature is controlled by the industrial chiller.

[0030] like Fig.11 As shown, and see Figure 9-10 Taking the long side of the pallet product 11 when viewed from above as an example, the outer width of the pallet product 11 before curling is recorded as a, and the outer width of the pallet product 11 after curling is completed is recorded as b; the bottom plate 31 at the bottom of the pressing plate 3 that contacts the upper surface of the pallet product has a width of b, and a skirt 32 is also provided on the periphery of the bottom plate 31 of the pressing plate 3. The skirt 32 is made of soft plastic material, and the width of the skirt 32 on both sides plus the width of the bottom plate 31 is a; the upper edge width of the upper slope opening 71 of the hot mold 7 is a, the lower edge width is b, and the inner wall width is b; the inner wall width of the cold forming mold 8 plus the curling forming groove width is b, and the lower edge of the inner wall of the hot mold 7 is aligned with the outer edge of the curling forming groove of the cold forming mold 8; the size relationship between the short side of the pallet product 11 and the pressing plate 3, the hot film 7, and the cold forming mold 8 when viewed from above is similar.

[0031] See also Fig.11 Based on the tray thermoforming and curling equipment, the present invention provides a tray thermoforming and curling method, comprising the following steps: S1. Start the heating mechanism and cooling mechanism of the tray thermoforming and curling equipment to make the hot mold and the cold forming mold reach the predetermined high temperature and low temperature range respectively; S2. The operator puts the pallet product to be curled into the curling mold so that the upper edge of the pallet product contacts the upper edge of the hot mold, that is, the upper edge of the slope opening; S3. Press the start switch, the pressure plate cylinder pushes the pressure plate downward, and the bottom plate of the pressure plate stops after it touches the upper edge of the pallet product; the pressure plate pushes the pallet product downward into the hot film, and uses the high temperature of the inner wall of the hot mold to heat and bend the part to be curled, until the pallet product is pushed into the cold forming mold, and the curled bottom of its upper edge touches the curling forming groove. S4, the pressing plate continues to press down, and in the process of continuous downward movement, it enters the curling forming groove and curls inward to form a curling shape, until the bottom of the tray product is supported by the top plate, and then pauses, and the curling is cooled and formed by the low temperature of the inner wall of the cold forming mold; S5, after the pallet product is curled and shaped, the pressure plate returns to the upper initial position, the top plate cylinder is activated to lift the top plate, and the pallet product is pushed above the curling mold, and the operator takes it out.

[0032] See also Fig.11 , Fig.12 , step S3 specifically includes the following steps: S31, the pressing plate pushes the pallet product downward, during which the outer edge of the pallet product contacts the inner wall of the hot film and becomes soft due to the heat. Since the outer skirt of the pressing plate bottom plate presses the outer edge of the pallet product, the outer edge bends downward while the width of the ramp opening gradually decreases, until the pallet product is pushed to the first set position P1 in the hot mold, that is, the upper edge of the pallet product is aligned with the lower edge of the hot mold ramp opening, and then pauses; the pressing plate bottom skirt is compressed and shrunk during the downward process, and is compressed when it is aligned with the lower edge of the hot mold ramp opening; S32, the pressing plate continues to push the tray product downward until the tray product is pushed to the second set position P2 in the hot mold, and then pauses; S33, the pressing plate continues to push the pallet product downward until the pallet product is pushed to the third set position P3 in the hot mold, that is, the pallet product enters the cold forming mold, and the curled bottom of its upper edge contacts the curling forming groove, and pauses.

[0033] In this embodiment, the temperature of the hot mold is controlled at about 105°, and the temperature of the cold forming mold is controlled at about 5°. The inner wall depth of the hot mold is 100 mm, the vertical height of the hot mold slope opening is 10 mm, the third pause position is half the depth of the hot mold, and the angle between the inclined surface of the hot mold slope opening and the vertical surface is 45°. In step S3, the three downward times of the pressing plate are 1 second, 1 second, and 4 seconds respectively, and the pallet product pauses three times in the hot mold for 0.5 seconds, 0.5 seconds, and 1 second respectively.

[0034] See also Fig.12 When the outer edge of the pallet product stops at point P1, it is ready to start curling; in the process of descending from point P1 to point P2, the outer edge of the pallet product is bent downward due to the high temperature of the inner wall of the heating mold, the slope of the slope opening of the heating mold, the pressure of the pressing plate, and the effect of the outer skirt of the pressing plate floor; at point P2, the radius of the bending angle is still relatively large, so it pauses at this time. Due to the heat, the bending part will continue to soften and the bending angle will become smaller; it continues to descend to point P3 and pauses. During the process, the part that has been bent downward becomes flatter and more vertical. During the pause, since the pallet product itself has a certain elasticity, the bent part of the outer edge of the pallet product is close to the inner wall of the heating mold, and the bending angle becomes smaller and smaller, approaching a right angle; when the outer edge of the pallet product contacts the curling forming groove, it has been fully heated and the curling is successfully completed.

[0035] The above description is only a preferred example of the present invention and is not any formal or substantial limitation to the present invention. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. Any equivalent changes and modifications made to the above examples based on the essential technology of the present invention should also be regarded as the protection scope of the present invention.

Claims

1. Equipment and method for thermoforming and curling of trays, characterized in that: It includes a workbench, a curling mold, a pressing plate, a top plate, a control box and a start-stop switch. The curling mold includes a hot mold and a cold forming mold. The cold forming mold is fixedly installed on the workbench, and the hot mold is fixedly installed above the cold forming mold. The pressing plate is arranged above the hot mold. A pressing plate cylinder is arranged above the pressing plate. The pressing plate cylinder is fixedly installed on the workbench through a column. The pressing plate cylinder can control the pressing plate to move downward and upward. The pressing plate is used to press the pallet product downward into the curling mold for curling forming. The top plate is installed inside the cold forming mold and is provided with a top plate cylinder to control the top plate to move upward. and downward, the top plate is used to push the pallet product after curling forming upward; the hot mold is provided with a heating mechanism, and the cold forming mold is provided with a refrigeration mechanism, the control box is connected with the heating mechanism and the refrigeration mechanism, and is used to set the temperature parameters of the heating mechanism and the refrigeration mechanism, the control box is also connected with the pressure plate cylinder and the top plate cylinder, and is used to set the speed parameters of the pressure plate cylinder and the top plate cylinder, the start-stop switch is installed on the side of the workbench, and is connected with the control box, and is used to control the opening and closing of the pallet thermoforming and curling equipment, and the pallet thermoforming and curling equipment is also provided with a power supply device.

2. The tray thermoforming curling equipment according to claim 1, characterized in that: The hot mold is a hollow square structure, the middle of which can allow the pallet product to pass through, a slope opening is provided on the upper part of the inner wall, the inner wall is a vertical surface, and mounting feet are provided at the four corners below; the cold forming mold is a box-shaped structure, which can accommodate the pallet product inside, a curling forming groove is provided on the inner side of the upper part, and mounting columns are provided at the four corners of the upper surface; the mounting feet of the hot mold are connected to the mounting columns of the cold forming mold for installation and fixation.

3. The tray thermoforming curling equipment according to claim 1, characterized in that: The top plate is a concave structure, and the inner side is an arc-shaped protective wall, which is used to adapt to the bottom shape of the pallet product to support the pallet product; the bottom surface of the top plate is provided with a cylinder mounting position 1 and a push rod hole 1, and the bottom surface of the cold forming mold is provided with a cylinder mounting position 2 and a push rod hole 2. The cylinder mounting position 1 and the cylinder mounting position 2 are aligned during installation and are used to install the top plate cylinder; the push rod hole 1 and the push rod hole 2 are centrally aligned during installation and are used to install the push rod, and the push rod is used to lift the top plate upward or pull it back downward through the action of the push rod cylinder; the bottom surface of the cold forming mold is also provided with a mounting hole, which is used to fix the cold forming mold on the workbench.

4. The tray thermoforming curling equipment according to claim 1, characterized in that: The curling forming groove of the cold forming die is a continuous groove extending around the upper inner edge of the cold forming die, which is used to curl the outer edge of the pallet product; the curling of the pallet product includes three shapes: 1 / 3 semicircle, semicircle, and 2 / 3 semicircle, and the curling forming groove is correspondingly set to three shapes: 1 / 3 semicircle, semicircle, and 2 / 3 semicircle.

5. The tray thermoforming curling equipment according to claim 1, characterized in that: The pressure plate cylinder provided on the pressure plate has an air pressure of 5-8kg and is controlled by a solenoid valve; the bottom plate of the pressure plate in contact with the pallet product is made of insulating board material; the top plate cylinder provided on the top plate has an air pressure of 5-8kg.

6. The tray thermoforming and curling equipment according to claim 1, characterized in that: The heating mechanism of the hot mold is a heating tube arranged on the outside of the upper half of the hot mold, which is used to heat the hot mold, and its working temperature is controlled by a temperature controller and a thyristor; the refrigeration mechanism includes a water circulation pipeline arranged around the outside of the cold forming mold, and an industrial water chiller, and the industrial water chiller is used to control the working temperature of the cold forming mold.

7. The tray thermoforming curling equipment according to claim 2, characterized in that: Taking the long side of the pallet product when viewed from above as an example, the outer width of the pallet product before curling is recorded as a, and the outer width of the pallet product after curling is completed is recorded as b; the bottom plate of the pressure plate that contacts the upper surface of the pallet product has a width of b, and the periphery of the bottom plate of the pressure plate is also provided with a skirt, and the skirt is made of soft plastic material, and the width of the skirts on both sides plus the width of the bottom plate is a; the upper edge width of the upper slope opening of the hot mold is a, the lower edge width is b, and the inner wall width is b; the inner wall width of the cold forming mold plus the curling forming groove width is b, and the lower edge of the inner wall of the hot mold is aligned with the outer edge of the curling forming groove of the cold forming mold; the dimensional relationship between the short side of the pallet product when viewed from above and the pressure plate, hot mold, and cold forming mold is similar.

8. The method for thermoforming and curling a pallet according to claim 7, comprising the following steps: S1. Start the heating mechanism and cooling mechanism of the tray thermoforming and curling equipment to make the hot mold and the cold forming mold reach the predetermined high temperature and low temperature range respectively; S2. The operator puts the pallet product to be curled into the curling mold so that the upper edge of the pallet product contacts the upper edge of the hot mold, that is, the upper edge of the slope opening; S3. Press the start switch, the pressure plate cylinder pushes the pressure plate downward, and the bottom plate of the pressure plate stops after it touches the upper edge of the pallet product; the pressure plate pushes the pallet product downward into the hot film, and uses the high temperature of the inner wall of the hot mold to heat and bend the part to be curled, until the pallet product is pushed into the cold forming mold, and the curled bottom of its upper edge touches the curling forming groove. S4, the pressing plate continues to press down, and in the process of continuous downward movement, it enters the curling forming groove and curls inward to form a curling shape, until the bottom of the tray product is supported by the top plate, and then pauses, and the curling is cooled and formed by the low temperature of the inner wall of the cold forming mold; S5, after the pallet product is curled and shaped, the pressure plate returns to the upper initial position, the top plate cylinder is activated to lift the top plate, and the pallet product is pushed above the curling mold, and the operator takes it out.

9. The method for thermoforming and curling a tray according to claim 8, wherein step S3 specifically comprises the following steps: S31, the pressing plate pushes the pallet product downward, during which the outer edge of the pallet product contacts the inner wall of the hot film and becomes soft due to the heat. Since the outer skirt of the pressing plate bottom plate presses the outer edge of the pallet product, the outer edge bends downward while the width of the ramp opening gradually decreases, until the pallet product is pushed to the first set position in the hot mold, that is, the upper edge of the pallet product is aligned with the lower edge of the hot mold ramp opening, and then pauses; the pressing plate bottom skirt is compressed and contracted during the downward process, and is compressed when it is aligned with the lower edge of the hot mold ramp opening; S32, the pressing plate continues to push the tray product downward until the tray product is pushed to the second set position in the hot mold, and then pauses; S33, the pressing plate continues to push the pallet product downward until the pallet product is pushed to the third set position in the hot mold, that is, the pallet product enters the cold forming mold, and the curled bottom of its upper edge contacts the curling forming groove, and pauses.

10. The method for thermoforming and curling a tray according to claim 9, characterized in that: The temperature of the hot mold is controlled between 70° and 110°, and the temperature of the cold forming mold is controlled between 1° and 10°; the angle between the inclined surface of the slope opening of the hot mold and the vertical surface is 30° to 60°; in step S3, the pressing plate moves down three times, each time for 1-4 seconds, and the pallet product pauses in the hot mold three times, each time for 0.1-2 seconds.