Blockage removal composition and application thereof

A plugging-removing composition with oxidant, activator, stabilizer, and complexing agent effectively addresses polymer gel blockages in high-temperature and high-salt environments, achieving efficient unblocking rates.

CN119060706AActive Publication Date: 2024-12-03CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310648593.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-02
Publication Date
2024-12-03
Estimated Expiration
2043-06-02

AI Technical Summary

Technical Problem

Existing technologies lack an effective unblocking agent for polymer gel in high-temperature and high-salt environments, leading to pipeline blockages, well pollution, excessive injection pressure, and failure of plugging agents in oil reservoirs.

Method used

A plugging-removing composition comprising an oxidant, an activator, a stabilizer, and a complexing agent, with optional solvent, designed to operate effectively at temperatures up to 110°C and mineralization levels of 0 to 218000 mg/L.

Benefits of technology

The composition achieves unblocking rates of 87.33% to 98.73% for polymer gels under harsh conditions, demonstrating high temperature and salt resistance, and is suitable for popularization and use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119060706A_ABST
    Figure CN119060706A_ABST
Patent Text Reader

Abstract

The invention provides a blocking removal composition and application thereof. The blocking removal composition mainly comprises an oxidizing agent, an activating agent, a stabilizing agent and a complexing agent, and further comprises a solvent. The unblocking composition provided by the invention has a good unblocking effect on the polymer gel: at 110 DEG C, the 10-day unblocking rate of the unblocking composition on the polymer gel prepared from polyacrylamide, a phenolic aldehyde crosslinking system and simulated mineralized water with the mineralization degree of 218000 mg / L is 87.33-98.73%, and the highest 10-day unblocking rate reaches 98% or above; and effective plug removal of the polymer gel can be realized at a high temperature of 110 DEG C and a degree of mineralization of 0-218000 mg / L.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of polymer gel blockage removal, and in particular relates to a blockage removal composition and application thereof. Background Art

[0002] In order to effectively ease the pressure of oil supply and demand and ensure the increase and stability of old oil fields, polymer water plugging technology has been industrialized in Daqing, Shengli and other oil fields. The application of gel can significantly reduce the permeability of fractures and high seepage zones, making the seepage process more effective, and effectively solving the problems of high water content and low recovery rate in oil wells. This technology plays an important role in improving the ultimate recovery rate of oil fields, maintaining stable production of oil fields, and improving the development effect of oil fields in the high water content period. However, with the increase in the number of water plugging, the production problems of new oil fields have become more prominent. The application of gel may cause blockage of injection pipelines, pollution around the well caused by water plugging of fixed pipe strings, excessive injection pressure, failure to inject plugging agents, and even invasion of porous formations to cause formation damage.

[0003] At present, 117 horizontal wells in clastic oil reservoirs have been plugged with water in multiple rounds, accounting for nearly 40%. If the pipe string is not used for water plugging, there will be problems such as pollution around the well, too high injection pressure, and failure to inject the plugging agent. As the formation conditions become increasingly harsh, it is of great significance to develop corresponding high-performance heat-resistant and salt-resistant plugging removers. In recent years, research and application have been carried out in the fields of physical plugging removal, chemical plugging removal, and biological plugging removal at home and abroad, and certain results have been achieved. However, the current research mainly focuses on the degradation of polymer molecules and the reduction of solution viscosity. Although it can better solve the blockage problems caused by polymer entanglement and gelation, there is little research on the unblocking of polymer gels and the unblocking of polymer gels under harsh formation conditions. Various existing unblocking technologies have certain limitations:

[0004] ① The application scope of physical plugging removal technology is limited and cannot be used in deep well areas;

[0005] ② Biological plugging removal technology is only applicable to specific oil reservoirs due to the specificity of gelatinase. In addition, gelatinase is not heat-resistant enough, and its activity at high temperatures will be greatly reduced, resulting in poor plugging removal effect.

[0006] ③Chemical declogging technology currently has insufficient heat and salt resistance (90℃ / 100,000 mineralization degrees). It decomposes quickly under high temperature (110℃) conditions and cannot effectively dredge. Under high mineralization conditions, the solubility of the declogging agent is poor and may even produce precipitation, causing blockage.

[0007] As can be seen from the above, the existing physical plugging removal technology, biological plugging removal technology and chemical plugging removal technology are unable to achieve polymer gel plugging removal in the harsh formation environment of high temperature and high salt. Therefore, it is urgent to develop a high temperature (110℃) and high salt (21.8×10 4The polymer gel plugging remover with a concentration of 100 mg / L provides a solution for the plugging removal of high-temperature and high-salinity oil reservoirs. It solves the problems of pipeline blockage, pollution around the well, excessive injection pressure, and failure of plugging agent injection after water plugging in high-temperature and high-salinity oil reservoirs, improves the seepage capacity of the plugged layer, and achieves increased and stable production of oil fields. Summary of the invention

[0008] In order to solve the problem in the prior art that there is a lack of an effective unblocking agent for polymer gel in a high temperature and high salt environment, the purpose of the present invention is to provide a polymer gel unblocking agent, which can be used in high temperature (110°C) and high salt (21.8×10 4 mg / L) environment to achieve efficient deblocking of polymer gel.

[0009] In order to achieve the above object, the present invention provides a plugging-removing composition, which includes an oxidant, an activator, a stabilizer and a complexing agent.

[0010] In a specific embodiment of the present invention, the plugging removal composition further comprises a solvent.

[0011] In a specific embodiment of the present invention, based on the mass of the declogging composition as 100%, the declogging composition includes 6wt% to 12wt% oxidant, 0.3wt% to 0.6wt% activator, 0.5wt% to 1wt% stabilizer, 3wt% complexing agent and the remainder solvent.

[0012] In one embodiment of the present invention, the oxidant is a persulfate;

[0013] Preferably, the oxidant is selected from at least one of ammonium persulfate, potassium persulfate and sodium persulfate.

[0014] In a specific embodiment of the present invention, the activator is sodium bisulfate.

[0015] In a specific embodiment of the present invention, the stabilizer is sodium sulfamate and / or sodium carbonate;

[0016] Preferably, the stabilizer is a mixture of sodium sulfamate and sodium carbonate;

[0017] Preferably, the mass ratio of the sodium carbonate to sodium sulfamate is 2:1.

[0018] In a specific embodiment of the present invention, the complexing agent is an organic polyphosphate complexing agent;

[0019] Preferably, the complexing agent is selected from at least one of polyaminopolyethermethylenephosphonic acid (PAPEMP), hydroxyethylidene diphosphonic acid (HEDP) and 2-phosphonobutane-1,2,4-tricarboxylic acid (PBTCA).

[0020] In one embodiment of the present invention, the solvent is water or mineralized water;

[0021] Preferably, the mineralization degree of the solvent is 0 to 218000 mg / L.

[0022] The application of the blockage-removing composition of the present invention in polymer gel blockage removal, in particular, as a polymer gel blockage-removing agent.

[0023] In one embodiment of the present invention, the applied temperature is not less than 110°C; and / or

[0024] The applied mineralization range is 0 to 218000 mg / L.

[0025] Beneficial effects of the present invention:

[0026] In view of the problem that there is a lack of an unblocking agent that can effectively unblock polymer gel in a high temperature and high salt environment in the prior art, the present invention provides an unblocking composition and its application. The unblocking composition provided by the present invention mainly includes an oxidant, an activator, a stabilizer and a complexing agent, and secondly also includes a solvent. The unblocking composition has good high temperature resistance and salt resistance, and has a strong unblocking ability for polymer gel: at 110°C, the unblocking composition has a 10-day unblocking rate of 87.33% to 98.73% for polymer gel prepared by polyacrylamide, phenolic cross-linking system (specifically a mixture of phenol and hexamethylenetetramine with a mass ratio of 1:1) and simulated mineralized water with a mineralization of 218100.55 mg / L after constant temperature aging at 110°C for 24 hours, and the highest 10-day unblocking rate is more than 98%, which can achieve effective unblocking of polymer gel under the conditions of 110°C and a mineralization of 0 to 218100.55 mg / L. In addition, the plugging-removing composition provided by the present invention has readily available raw materials, a simple preparation method, and is suitable for popularization and use. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 From left to right, the blocking removal performance of the polymer gel by the blocking removal compositions prepared in Example 1, Example 3, Example 2 and Example 4 is shown in the polymer gel blocking removal performance evaluation when the experimental time is 24 hours. DETAILED DESCRIPTION

[0028] The present invention will be further described below in conjunction with examples, but the examples of the present invention are only exemplary descriptions, and the implementation methods do not constitute limitations of the present invention under any circumstances.

[0029] Preparation of plugging-removing composition

[0030] The simulated mineralized water used in Examples 1 to 8 has a total mineralization of 218100.55 mg / L, of which K ++Na + 71634.37mg / L, Ca 2+ 11272.5mg / L, Mg 2+ 1161.84 mg / L, Cl - 133658mg / L, SO 4 2- 150 mg / L, HCO 3 - 33.84 mg / L, I - 10mg / L, Br - It is 180mg / L.

[0031] In Examples 1, 2, 5, 6 and Comparative Example 4, polyaminopolyethermethylenephosphonic acid (PAPEMP) was purchased from Shandong Taihe Science and Technology Co., Ltd.;

[0032] In Examples 7 and 8, 2-phosphobutane-1,2,4-tricarboxylic acid (PBTCA): purchased from Shandong Taihe Science and Technology Co., Ltd., CAS No. 37971-36-1;

[0033] In Examples 3 and 4, hydroxyethylidene diphosphoric acid (HEDP) was purchased from Shandong Taihe Science and Technology Co., Ltd., CAS No. 2809-21-4.

[0034] Example 1

[0035] Weigh 6 g of sodium persulfate, 0.3 g of sodium bisulfate, 0.5 g of a stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of polyaminopolyethermethylenephosphonic acid (PAPEMP) and 90.2 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L, mix them, and stir at a speed of 300 rpm for 5 min to obtain a plugging-removing composition.

[0036] Example 2

[0037] 12 g of sodium persulfate, 0.3 g of sodium bisulfate, 0.5 g of a stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of polyaminopolyethermethylenephosphonic acid (PAPEMP) and 84.2 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a speed of 300 rpm for 5 min to obtain a plugging-removing composition.

[0038] Example 3

[0039] Weigh 6 g of ammonium persulfate, 0.6 g of sodium bisulfate, 0.5 g of stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of hydroxyethylidene diphosphoric acid (HEDP) and 89.9 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L, mix them, and stir at a speed of 300 rpm for 5 min to obtain a plugging removal composition.

[0040] Example 4

[0041] 12 g of potassium persulfate, 0.6 g of sodium bisulfate, 0.5 g of stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of hydroxyethylidene diphosphoric acid (HEDP) and 83.9 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a speed of 300 rpm for 5 min to obtain a plugging-removing composition.

[0042] Example 5

[0043] Weigh 6 g of ammonium persulfate, 0.3 g of sodium bisulfate, 1 g of stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of polyaminopolyethermethylenephosphonic acid (PAPEMP) and 89.7 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L, mix them, and stir at a speed of 300 rpm for 5 min to obtain a plugging removal composition.

[0044] Example 6

[0045] 12 g of potassium persulfate, 0.3 g of sodium bisulfate, 1 g of stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of polyaminopolyethermethylenephosphonic acid (PAPEMP) and 83.7 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a speed of 300 rpm for 5 min to obtain a plugging removal composition.

[0046] Example 7

[0047] 6 g of sodium persulfate, 0.6 g of sodium bisulfate, 1 g of stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of 2-phosphobutane-1,2,4-tricarboxylic acid (PBTCA) and 89.4 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a speed of 300 rpm for 5 min to obtain a plugging removal composition.

[0048] Example 8

[0049] 12 g of sodium persulfate, 0.6 g of sodium bisulfate, 1 g of a stabilizer (a mixture of sodium carbonate and sodium aminosulfonate in a mass ratio of 2:1), 3 g of 2-phosphobutane-1,2,4-tricarboxylic acid (PBTCA) and 83.4 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a speed of 300 rpm for 5 min to obtain a plugging removal composition.

[0050] Comparative Example 1

[0051] Weigh 6 g of sodium persulfate, 0.3 g of sodium bisulfate and 93.7 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L, mix them, and stir them at a speed of 300 rpm for 5 minutes to obtain a plugging-removing composition.

[0052] Comparative Example 2

[0053] 12 g of sodium persulfate, 0.3 g of sodium bisulfate and 87.7 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a rotation speed of 300 rpm for 5 minutes to obtain a plugging-removing composition.

[0054] Comparative Example 3

[0055] 6 g of sodium persulfate, 0.3 g of sodium bisulfate, 0.5 g of stabilizer (sodium carbonate: sodium aminosulfonate = 2:1) and 93.2 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a speed of 300 rpm for 5 minutes to obtain a plugging-removing composition.

[0056] Comparative Example 4

[0057] 6 g of sodium persulfate, 0.3 g of sodium bisulfate, 3 g of polyaminopolyethermethylenephosphonic acid (PAPEMP) and 90.7 g of simulated mineralized water with a mineralization degree of 218100.55 mg / L were weighed and mixed, and stirred at a rotation speed of 300 rpm for 5 minutes to obtain a plugging-removing composition.

[0058] Evaluation of the plugging removal performance of polymer gel in plugging removal composition

[0059] The polymer jelly was prepared according to the following method, and then the deblocking composition was used to deblock the aged polymer jelly, and the deblocking rate was calculated to evaluate the deblocking performance of the deblocking composition prepared in Examples 1 to 8 and Comparative Examples 1 to 4 on the polymer jelly. The specific experimental steps are as follows:

[0060] The simulated mineral water used in this experiment has a total mineralization of 218100.55 mg / L, of which K + +Na + 71634.37mg / L, Ca 2+ 11272.5mg / L, Mg 2+1161.84 mg / L, Cl - 133658mg / L, SO 4 2- 150 mg / L, HCO 3 - 33.84 mg / L, I - 10mg / L, Br - It is 180mg / L.

[0061] ⅰ Preparation of polymer gel

[0062] 1) Weigh 0.5 g of polyacrylamide (molecular weight of 6 million to 8 million), 0.4 g of phenol, 0.4 g of hexamethylenetetramine and 98.7 g of simulated mineralized water and mix them evenly to obtain a polymer gel solution;

[0063] 2) 10 g of the polymer gel solution was injected into a thick-walled pressure-resistant screw-mouth bottle and aged at 110° C. for 24 h to obtain a polymer gel;

[0064] According to the above method, 12 portions of polymer jelly (10 g each) were prepared and set aside.

[0065] ii. Deblocking the polymer gel using a deblocking composition

[0066] 1) Weigh 10 g of each of the blocking-removing compositions prepared in Examples 1 to 8 and Comparative Examples 1 to 4, and then add them to the 12 portions of polymer jelly prepared in step i (add 10 g of the blocking-removing composition to each portion of polymer jelly);

[0067] 2) 12 groups of polymer gels added with the plugging-removing composition were placed at 110° C. for constant temperature reaction for 10 days. During the reaction period, the gels were taken out for observation every 24 hours. After the experiment, the remaining mass of the polymer gels in each group was weighed;

[0068] The unblocking rate of the unblocking composition for the polymer jelly is measured by the mass of the dissolved polymer jelly. The calculation formula of the unblocking rate is formula (1):

[0069] K=(m 0 -m t ) / m 0 ×100% Formula (1)

[0070] Where, K is the blocking rate;

[0071] m t —The quality of the polymer jelly after the reaction;

[0072] m 0 —The mass of the polymer jelly before reaction.

[0073] The data of the unblocking rate are shown in Table 1. The unblocking situation when the experimental time is 24 hours is as follows: Figure 1 shown.

[0074] Table 1. Unblocking rate of unblocking composition for polymer gel at 110°C and 218100.55 mg / L salinity

[0075] Serial number 10-day unblocking rate / % Example 1 95.66 Example 2 95.73 Example 3 87.33 Example 4 88.90 Example 5 96.53 Example 6 95.83 Example 7 98.32 Example 8 98.73 Comparative Example 1 47.52 Comparative Example 2 45.86 Comparative Example 3 73.21 Comparative Example 4 67.42

[0076] Analysis of the data in Table 1 shows that: under the conditions of a temperature of 110°C and a mineralization of 218100.55 mg / L, the blocking removal rates of the blocking removal compositions prepared in Examples 1 to 8 as blocking removal agents for polymer gel are 87.33% to 98.73%, and the blocking removal effects are relatively good; the blocking removal rates of the blocking removal compositions prepared in Comparative Examples 1 to 4 as blocking removal agents for polymer gel are 45.86% to 73.21%, and the blocking removal effects are relatively poor. Combining the formulas of Example 1 and Example 2 and the data on the polymer gel unblocking rate, it can be seen that: when the concentration of the oxidant in the unblocking composition reaches 6wt%, continuing to increase the concentration of the oxidant will not significantly increase the polymer gel unblocking rate; Combining the formulas of Examples 1 and 5, Examples 2 and 6 and the data on the polymer gel unblocking rate, it can be seen that: when the concentration of the oxidant in the unblocking composition is 6wt% to 12wt% and the concentration of the activator is 0.3wt%, increasing the concentration of the stabilizer alone has basically no effect on the unblocking effect of the unblocking composition, and the polymer gel unblocking rate does not show a significant improvement; Combining the formulas of Example 1 and Example 3 and the data on the polymer gel unblocking rate, it can be seen that: when the concentration of the oxidant in the unblocking composition is 6wt%, the concentration of the stabilizer is 0.5wt%, and the concentration of the complexing agent is 3wt%, the concentration of the activator reaches 0.3wt%. %, if the concentration of the activator is further increased, the blocking removal rate will decrease. The inventors believe that the higher the concentration of the activator, the faster the decomposition of the oxidant, resulting in a decrease in the blocking removal rate. Combining the formulas and blocking removal rate data of Example 7 and Example 3, Example 8 and Example 4, it can be seen that when the concentration of the oxidant in the blocking removal composition is 6wt% to 12wt%, the concentration of the activator is 0.6wt%, and the concentration of the complexing agent is 3wt%, increasing the concentration of the stabilizer alone can significantly improve the blocking removal performance of the blocking removal composition for polymer jelly. Combining the formulas and blocking removal rate data of Example 3 and Example 8, it can be seen that when the concentration of the activator in the blocking removal composition is 0.6wt% and the concentration of the complexing agent is 3wt%, increasing the concentrations of the oxidant and the stabilizer at the same time can significantly improve the blocking removal performance of the polymer jelly of the blocking removal composition. Comparing Examples 1 and 2 with Comparative Examples 1 and 2, it can be seen that the unblocking rate of the unblocking composition for polymer gel without adding stabilizer and complexing agent drops to less than 50%. This may be due to the rapid decomposition and consumption of the oxidant under the dual effects of high temperature and activator; at the same time, the oxidant and activator generate precipitation at high temperature, which affects the unblocking reaction and leads to a poor final unblocking rate. By comparing Example 1, Comparative Example 1 and Comparative Example 3, it can be found that the addition of stabilizer increases the unblocking rate of the unblocking agent for polymer gel by about 25.69%. It can be seen that the stabilizer improves the temperature resistance of the unblocking composition and slows down the decomposition rate of the oxidant, thereby improving the unblocking rate of the unblocking composition. On this basis, the addition of complexing agent further improves the solubility of the unblocking composition, and the unblocking rate of the unblocking composition is further improved to 95.66%.Similarly, it can be found from Comparative Example 1, Comparative Example 1, and Comparative Example 4 that the solubility of the blocking-removing composition is improved after the complexing agent is added, so the blocking-removing rate is increased by about 20%. On this basis, the stabilizer is added to improve the temperature resistance of the oxidant and slow down the decomposition rate of the oxidant, so the blocking-removing rate is further increased by about 28%. It can be seen that the addition of stabilizers and complexing agents can effectively improve the blocking-removing effect of the blocking-removing composition, and the four agents of stabilizer, complexing agent, oxidant, and activator are synergistically enhanced to further improve the blocking-removing effect of the blocking-removing composition.

[0077] Figure 1 The dissolution of the polymer gel by the blocking-removing compositions prepared in Example 1, Example 3, Example 2, and Example 4 at 110°C and a salinity of 218100.55 mg / L for 24 hours is shown from left to right. It can be seen that Figure 1 There is a slight difference in the color depth of the containers from left to right in the figure, that is, when the experimental time is 24h, the unblocking degree of the unblocking composition prepared in Examples 1 to 4 on the polymer jelly is inconsistent. Combining the formulas of the unblocking compositions of Examples 1 to 4, it can be seen that in the unblocking composition, when the amount of the complexing agent and the stabilizer remains unchanged, the mass ratio of the oxidant to the activator is different, and the unblocking effect of the unblocking composition on the polymer jelly is also different. This shows that the mass ratio between the oxidant and the activator affects the unblocking performance of the unblocking composition on the polymer jelly.

[0078] Based on the above table 1, Figure 1 The analysis shows that in the blockage-removing composition provided by the present invention, the respective contents of the oxidant, activator, stabilizer and complexing agent and the mass relationship between the components will affect the blockage-removing performance of the blockage-removing composition. The four agents of stabilizer, complexing agent, oxidant and activator are synergistic, which can further improve the blockage-removing effect of the blockage-removing composition. Within the scope of the blockage-removing composition formula provided by the present invention, effective blockage removal can be achieved for polymer gel at 110°C and a mineralization of 0 to 218100.55 mg / L.

[0079] Although the present invention has been described with reference to specific embodiments, it will be appreciated by those skilled in the art that various changes may be made without departing from the true spirit and scope of the present invention. In addition, the subject matter, spirit and scope of the present invention may be varied to accommodate specific situations, materials, material combinations and methods. All of these changes are included within the scope of the claims of the present invention.

Claims

1. A plugging-removing composition comprising an oxidant, an activator, a stabilizer and a complexing agent.

2. The plugging-removing composition according to claim 1, characterized in that: The plugging-removing composition further includes a solvent.

3. The plugging-removing composition according to claim 2, characterized in that: Taking the mass of the declogging composition as 100%, the declogging composition includes 6wt% to 12wt% of an oxidant, 0.3wt% to 0.6wt% of an activator, 0.5wt% to 1wt% of a stabilizer, 3wt% of a complexing agent and the remainder of a solvent.

4. The plugging-removing composition according to any one of claims 1 to 3, characterized in that: The oxidizing agent is persulfate.

5. The plugging-removing composition according to any one of claims 1 to 4, characterized in that: The activator is sodium bisulfate.

6. The plugging-removing composition according to any one of claims 1 to 5, characterized in that: The stabilizer is sodium sulfamate and / or sodium carbonate.

7. The plugging-removing composition according to any one of claims 1 to 6, characterized in that: The complexing agent is an organic polyphosphorus complexing agent; Preferably, the complexing agent is selected from at least one of polyaminopolyether methylene phosphoric acid, hydroxyethylene diphosphoric acid and 2-phosphonobutane-1,2,4-tricarboxylic acid.

8. The plugging-removing composition according to claim 2 or 3, characterized in that: The solvent is water or mineralized water.

9. Use of the plugging-removing composition according to any one of claims 1 to 8 in polymer jelly plugging removal, in particular as a polymer jelly plugging remover.

10. The use according to claim 9, characterized in that: The temperature of the application is not less than 110°C; and / or The applied mineralization range is 0 to 218000 mg / L.

Citation Information

Patent Citations

  • Anti-salt anti-high-temperature high-intensity gel blocking agent

    CN105131921A

  • Medium-high temperature oil reservoir phenolic gel self-degradation temporary plugging agent and preparation method thereof

    CN111574977A

  • High-efficiency blockage removal system for polymer flooding injection well as well as preparation method and application of high-efficiency blockage removal system

    CN111607371A

  • Capsule blocking remover and composite blocking removal method

    CN116023919A