Method for removing olefin from reformate

By introducing hydrogenation additives into the reforming oil and carrying out hydrogenation reaction, the problems of serious losses and high costs in the olefin removal process in the prior art are solved, and the high efficiency and low loss of olefin removal effect is achieved. in the petrochemical field.

CN119060757AActive Publication Date: 2024-12-03CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202310648965.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-02
Publication Date
2024-12-03
Estimated Expiration
2043-06-02

AI Technical Summary

Technical Problem

The prior art has the problem of serious and high cost of aromatic hydrocarbon loss in the olefin removal process in the reforming oil, making it difficult to achieve efficient removal and maintain low aromatic hydrocarbon loss.

Method used

The hydrogenation reaction and catalyst are carried out by introducing hydrogenation additives, such as norbornene, C2-C6 olefin groups, substituting norbornene, styrene, 1-butene, cyclopentene and dicyclopentene, etc., in the reforming oil. Contact, selective hydrogenation reaction is carried out to remove olefins. The reaction conditions include a reaction temperature of 10°C to 200°C, a hydrogen pressure of 0.1 MPa to 10 MPa, and a mass space velocity of 0.1 h-1 to 50 h-1.

Benefits of technology

It has achieved efficient removal of olefins in reforming oil, with few side reactions, low aromatic loss rate, mild reaction process and low cost, and is suitable for petrochemical field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004264365610000031
    Figure BDA0004264365610000031
  • Figure BDA0004264365610000071
    Figure BDA0004264365610000071
  • Figure BDA0004264365610000072
    Figure BDA0004264365610000072
Patent Text Reader

Abstract

The invention relates to a method for removing olefin from reformate, which comprises the following steps: contacting the reformate, a hydrogenation additive and a hydrogenation catalyst to carry out olefin hydrogenation reaction, wherein the hydrogenation auxiliary agent is selected from one or a combination of more of norbornene, C2-C6 alkylene substituted norbornene, styrene, 1-butene, cyclopentene and dicyclopentadiene. According to the method for removing the olefin from the reformate, the hydrogenation additive is introduced into the reaction system, selective hydrogenation of the olefin in the reformate is promoted so as to remove the olefin, the whole reaction process has few side reactions, the olefin removal rate is high, the loss rate of aromatic hydrocarbon is low, and efficient removal of the olefin in the reformate is realized; the method is simple and easy to implement, low in cost and mild in reaction process, has important significance in the petrochemical field and has wide industrial application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of petrochemical engineering, and in particular to a method for removing olefins from reformed oil. Background Art

[0002] Reformate can be used to produce aromatic chemicals such as BTX (benzene, toluene and xylene). However, reformate contains a small amount of olefins, which need to be removed for purification and separation. Therefore, the continuous removal of olefins from reformate is of great significance to the chemical industry.

[0003] Since reformed oil is prone to hydrogenation of aromatic hydrocarbons at high temperatures, it is particularly important to remove olefins from reformed oil at low temperatures and with high efficiency. Existing technologies mainly start with the development of new catalysts. For example, patent CN1045305C uses non-precious metal (such as Co-Mo or Ni-Mo / Al2O3) or precious metal (Pt, Pd / Al2O3) catalysts to selectively hydrogenate and remove olefins from reformed oil. Non-precious metal catalysts have high reaction temperatures (generally around 300-330°C) and cause large aromatic hydrocarbon losses. Precious metal catalysts are expensive.

[0004] Based on the current situation that the de-olefination of reforming oil causes serious aromatic losses and high costs, how to develop a method for removing olefins from reforming oil that can efficiently remove olefins with low aromatic losses is a technical problem that needs to be solved urgently.

[0005] It should be noted that the information disclosed in the aforementioned background technology section is only used to enhance the background understanding of the present invention, and therefore it may include information that does not constitute the prior art known to ordinary technicians in the field. Summary of the invention

[0006] The invention provides a method for removing olefins from reformed oil, aiming at efficiently removing olefins from reformed oil and keeping low aromatics loss.

[0007] The present invention relates to a method for removing olefins from reformed oil, which comprises: contacting reformed oil, a hydrogenation aid and a hydrogenation catalyst to carry out a hydrogenation reaction of olefins; wherein the hydrogenation aid is selected from a combination of one or more of norbornene, C2-C6 olefin-substituted norbornene, styrene, 1-butene, cyclopentene and dicyclopentadiene.

[0008] Optionally, the C2-C6 olefin-substituted norbornene is selected from a combination of one or more of vinyl norbornene, propenyl norbornene and butenyl norbornene.

[0009] Optionally, the mass ratio of the hydrogenation aid to the reformed oil is 1:(1-1000); preferably, the mass ratio of the hydrogenation aid to the reformed oil is 1:(1-100).

[0010] Optionally, the hydrogenation catalyst comprises an active component and a carrier; the active component is selected from a combination of one or more of Ni, Mo, W, Co, Pd, Pt and Rh; the carrier is selected from a combination of one or more of SiO2, C, Al2O3 and molecular sieves.

[0011] Optionally, the active component is selected from a combination of one or more of Ni, Pd and Pt, and the carrier is selected from a combination of one or more of SiO2, C and Al2O3.

[0012] Optionally, the hydrogenation reaction is carried out in a fixed bed reactor.

[0013] Optionally, the conditions of the hydrogenation reaction include: reaction temperature of 10°C to 200°C, hydrogen pressure of 0.1MPa to 10MPa, mass space velocity of 0.1h -1 ~50h -1 , the volume ratio of hydrogen to oil is 10 to 1000.

[0014] Optionally, contacting the reformed oil, the hydrogenation aid and the hydrogenation catalyst comprises: dissolving the hydrogenation aid in the reformed oil, and then feeding the reformed oil into the fixed bed reactor to contact with the hydrogenation catalyst, and introducing hydrogen.

[0015] Optionally, the hydrogenation reaction is carried out in a high-pressure reactor.

[0016] Optionally, the conditions of the hydrogenation reaction include: reaction temperature of 10°C to 200°C, hydrogen pressure of 0.1MPa to 10MPa, reaction time of 0.1h to 10h, stirring speed of 400r / min to 1000r / min, and a mass ratio of the hydrogenation catalyst to the reforming oil of 1:(1 to 500).

[0017] Beneficial effects:

[0018] The method for removing olefins from reformed oil of the present invention promotes the selective hydrogenation of olefins in the reformed oil to remove olefins by introducing a hydrogenation aid into the reaction system. The whole reaction process has few side reactions, a high olefin removal rate and a low aromatic loss rate, thereby achieving efficient removal of olefins from the reformed oil. The method is simple and easy to operate, low in cost, and has a mild reaction process. It is of great significance to the petrochemical field and has broad prospects for industrial application. DETAILED DESCRIPTION

[0019] The present invention is further described in detail below through examples. Through these examples, the features and advantages of the present invention will become clearer and more specific.

[0020] The word “exemplary” is used exclusively herein to mean “serving as an example, example, or illustration.” Any embodiment described herein as “exemplary” is not necessarily to be construed as preferred or advantageous over other embodiments.

[0021] In addition, the technical features involved in different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.

[0022] The present invention relates to a method for removing olefins from reformed oil, which comprises: contacting reformed oil, a hydrogenation aid and a hydrogenation catalyst to carry out a hydrogenation reaction of olefins; wherein the hydrogenation aid is selected from a combination of one or more of norbornene, C2-C6 olefin-substituted norbornene, styrene, 1-butene, cyclopentene and dicyclopentadiene.

[0023] It should be noted that, firstly, in the method for deolefination of reformed oil of the present invention, the reformed oil, a hydrogenation aid and a hydrogenation catalyst are contacted to carry out a hydrogenation reaction of olefins. By introducing the hydrogenation aid into the reaction system for deolefination of reformed oil, the selective hydrogenation of olefins in the reformed oil is promoted. After the hydrogenation reaction of olefins, the olefins in the reformed oil can be removed at a high olefin removal rate, and the aromatics loss rate is low, thereby achieving efficient removal of olefins in the reformed oil and providing a guarantee for the subsequent utilization of the reformed oil.

[0024] Secondly, the reformed oil and the hydrogenation aid can be simultaneously introduced into the reaction system of the hydrogenation reaction, contacted with the hydrogenation catalyst, and hydrogen is introduced at the same time to carry out the hydrogenation reaction; or, the reformed oil and the hydrogenation aid can be mixed first, and the mixed material is introduced into the reaction system as a raw material, contacted with the hydrogenation catalyst, and hydrogen is introduced at the same time to carry out the hydrogenation reaction.

[0025] According to a specific embodiment of the method of the present invention, the C2-C6 olefin-substituted norbornene is selected from a combination of one or more of vinyl norbornene, propenyl norbornene and butenyl norbornene.

[0026] It should be noted that in the C2-C6 olefin-substituted norbornene, the C2-C6 olefin group may be a straight-chain hydrocarbon group, and the connection position and connection mode of the olefin group may be similar to the vinyl norbornene shown in the following formula (1), and the olefin group may be connected to the 5-position C of the norbornene. The hydrogenation aid may be a C2-C4 olefin-substituted norbornene, which may be a pentenyl norbornene or a hexenyl norbornene. Preferably, it is a combination of one or more of norbornene, vinyl norbornene, propenyl norbornene and dicyclopentadiene.

[0027]

[0028] According to another specific embodiment of the method of the present invention, the mass ratio of the hydrogenation aid to the reformed oil is 1:(1-1000).

[0029] As a preferred embodiment of the method of the present invention, the mass ratio of the hydrogenation aid to the reformed oil is 1:(1-100).

[0030] It should be noted that in the method for deolefination of reformed oil of the present invention, the reformed oil and a hydrogenation aid are contacted with a hydrogenation catalyst to carry out a hydrogenation reaction of the olefins. The olefins to be hydrogenated include olefins in the reformed oil and a combination of one or more of norbornene, C2 to C6 olefin-substituted norbornene, styrene, 1-butene, cyclopentene and dicyclopentadiene as a hydrogenation aid.

[0031] The reformed oil product after olefin removal by the method of the present invention contains a small amount of hydrogenation product of the hydrogenation aid. Since the amount of the hydrogenation aid is very small, the reformed oil product after olefin removal can be used directly without separation and purification when the purity requirement is not high. For example, when the product is used as an oil product for combustion, separation and purification are not required. Alternatively, if there are certain requirements for purity when using it, such as when the reformed oil product after olefin removal is used to prepare aromatic products, the method of the present invention can also include a separation and purification step after the hydrogenation reaction to separate the product after hydrogenation of the hydrogenation aid. The separation and purification method can adopt conventional methods in the field, such as distillation, rectification, chemical purification, etc., which are not limited by the present invention.

[0032] It should be noted that when the mass ratio of the hydrogenation aid to the reformed oil is within the above preferred numerical range, the olefins in the reformed oil can be removed at a higher olefin removal rate through the hydrogenation reaction of the olefins. In addition, specifically, the mass ratio of the hydrogenation aid to the reformed oil can also be 1:20, 1:50, 1:60, 1:80, 1:90, 1:150, 1:200, 1:220, 1:250, 1:300, 1:400, 1:500, 1:600, 1:700, 1:800, 1:900, etc.

[0033] According to a specific embodiment of the method of the present invention, the hydrogenation catalyst comprises an active component and a carrier; the active component is selected from a combination of one or more of Ni, Mo, W, Co, Pd, Pt and Rh; the carrier is selected from a combination of one or more of SiO2, C, Al2O3 and molecular sieves.

[0034] It should be noted that the method of the present invention, in the reaction system of removing olefins by hydrogenation reaction of reformed oil, by adding a hydrogenation aid to increase the removal rate of olefins in the reformed oil and maintaining a low aromatic loss rate, has a wide range of applicability. The catalyst based on the above-mentioned active components and carriers can be used in the method of the present invention to effectively remove olefins in the reformed oil.

[0035] As a preferred embodiment of the method of the present invention, the active component is selected from a combination of one or more of Ni, Pd and Pt, and the carrier is selected from a combination of one or more of SiO2, C and Al2O3.

[0036] It should be noted that, when the method for removing olefins from reformed oil of the present invention is carried out based on the catalyst composed of the above-mentioned preferred active components and carrier, the catalyst and the hydrogenation aid can better play a synergistic role to better remove olefins from the reformed oil.

[0037] According to a specific embodiment of the method of the present invention, the hydrogenation reaction is carried out in a fixed bed reactor.

[0038] It should be noted that the method for deolefination of reformed oil of the present invention has a wide range of applicability and can be well carried out in a variety of reactors.

[0039] According to the embodiment of the method of the present invention carried out in a fixed bed reactor, the conditions of the hydrogenation reaction include: a reaction temperature of 10°C to 200°C, a hydrogen pressure of 0.1MPa to 10MPa, a mass space velocity of 0.1h -1 ~50h -1 , the volume ratio of hydrogen to oil is 10 to 1000.

[0040] It should be noted that when the method of the present invention is carried out in a fixed bed reactor, the reformed oil can be mixed with a hydrogenation aid and then fed into the fixed bed reactor. Under the above reaction conditions, olefins in the reformed oil can be removed at a higher removal rate, and the aromatic loss rate is low. The reaction temperature can specifically be 20°C, 40°C, 60°C, 70°C, 75°C, 80°C, 90°C, 100°C, 103°C, 110°C, 116°C, 124°C, 136°C, 141°C, 159°C, 168°C, 180°C, 190°C, etc. Optionally, the reaction temperature is 40°C to 160°C. The hydrogen pressure can be 0.2MPa, 0.7MPa, 1MPa, 2MPa, 3.5MPa, 4MPa, 5MPa, 6MPa, 7MPa, 8MPa, 9MPa, 10MPa, etc., and optionally, the hydrogen pressure is 2MPa to 7MPa. The mass space velocity can be 0.1h -1 , 0.5h -1 , 1h -1 , 2h -1, 4h -1 , 10h -1 , 25h -1 , 37h -1 , 45h -1 , 50h -1 The volume ratio of hydrogen to oil can be 100, 220, 350, 490, 550, 760, 880, 1000, 1600, 2000, etc.

[0041] According to an embodiment of the method of the present invention carried out in a fixed bed reactor, contacting the reformed oil, the hydrogenation aid and the hydrogenation catalyst comprises: dissolving the hydrogenation aid in the reformed oil, then feeding the reformed oil into the fixed bed reactor to contact with the hydrogenation catalyst, and introducing hydrogen.

[0042] It should be noted that when the method of the present invention is carried out in a fixed bed reactor, the hydrogenation aid is first dissolved in the reformed oil, and then fed into the fixed bed reactor to contact with the hydrogenation catalyst for hydrogenation reaction, so that the entire reaction can be carried out more stably and continuously, and a high olefin removal rate can be better achieved while maintaining a low aromatic loss rate.

[0043] According to another specific embodiment of the method of the present invention, the hydrogenation reaction is carried out in a high-pressure reactor.

[0044] It should be noted that, as can be seen from the above, the method of the present invention can be carried out in a fixed bed reactor or a high-pressure reactor, and can well complete the removal of olefins in the reformed oil. However, the method of deolefination of reformed oil of the present invention is not limited to a certain fixed reactor. As long as it is in the reaction process of hydrogenation deolefination of reformed oil, the method of introducing the hydrogenation aid falls within the protection scope of the present invention.

[0045] According to an embodiment of the method of the present invention carried out in a high-pressure reactor, the conditions of the hydrogenation reaction include: a reaction temperature of 10°C to 200°C, a hydrogen pressure of 0.1MPa to 10MPa, a reaction time of 0.1h to 10h, a stirring speed of 400r / min to 1000r / min, and a mass ratio of the hydrogenation catalyst to the reformed oil of 1:(1 to 500).

[0046] It should be noted that when the method of the present invention is carried out in a high-pressure reactor, the reformed oil can be first mixed with a hydrogenation aid, and then placed in a high-pressure reactor, and a hydrogenation catalyst is added to the high-pressure reactor. In a hydrogen atmosphere, the reformed oil is contacted with the hydrogenation catalyst to carry out a selective hydrogenation reaction. When the method of the present invention is carried out in a high-pressure reactor and under the above reaction conditions, olefins in the reformed oil can be removed at a higher removal rate, and a low aromatic loss rate is maintained.

[0047] It should be noted that when the method of the present invention is carried out in a high pressure reactor, specifically, the reaction temperature can be 20°C, 40°C, 60°C, 70°C, 75°C, 80°C, 90°C, 100°C, 103°C, 110°C, 116°C, 124°C, 136°C, 141°C, 159°C, 168°C, 180°C, 190°C, etc. Optionally, the reaction temperature is 40°C to 160°C. The hydrogen pressure can be 0.2MPa, 0.7MPa, 1MPa, 2MPa, 3.5MPa, 4MPa, 5MPa, 6MPa, 7MPa, 8MPa, 9MPa, 10MPa, etc., preferably 2MPa to 7MPa. The reaction time can be 0.1h, 0.5h, 1h, 2h, 4h, 10h, etc., and optionally, 0.5h to 4h. The stirring speed may be 400 r / min, 500 r / min, 670 r / min, 800 r / min, 950 r / min, 1000 r / min, etc. The mass ratio of the hydrogenation catalyst to the reformed oil may be 1:10, 1:20, 1:25, 1:30, 1:35, 1:40, 1:45, 1:50, 1:60, 1:70, 1:80, 1:90, 1:100, 1:150, 1:200, 1:220, 1:250, 1:280, 1:300, 1:350, 1:400, etc.

[0048] In summary, in the method for deolefination of reformed oil of the present invention, in the reaction system of hydrogenating and removing olefins from reformed oil, by adding the hydrogenation aid, the selective removal of olefins in the reformed oil is better promoted, the selective hydrogenation and deolefination reaction in the reformed oil is better completed, and the aromatic components in the reformed oil are well retained. The method of the present invention has mild reaction conditions and low cost. It is applicable to various reactors such as fixed bed reactors or high-pressure reactor reactors, has wide applicability, and has a significant breakthrough significance for scientific research and development and actual production in the petrochemical field.

[0049] The present invention is further described in detail by the following examples, but the present invention is not limited thereto. The reagents used in the following examples can be commercial products unless otherwise specified.

[0050] The 20% Ni / SiO2 catalyst used in the following examples can be synthesized by the method disclosed in patent ZL201811408739.0; the Raney Ni catalyst is from Macklin, and its product number is N858485 on the Inokai reagent platform, with a purity of ≥99% and a Ni mass content of ≥47%; the 0.5% Pd / C catalyst is from Alfa, and its product number is 038289 on the Inokai reagent platform; the 3% Co-11% Mo / γ-Al2O3 catalyst is from Alfa, and its product number is 045579 on the Inokai reagent platform. The bromine index of the reformed oil before the reaction in the following examples is 0.6 mg Br / 100 g oil.

[0051] The calculation method is described in the following examples:

[0052]

[0053]

[0054] It should be noted that in the calculation formula of olefin removal rate, the olefin concentration at the end of the reaction refers to the concentration of olefins in the reformate after the reaction is completed, and the olefin concentration before the reaction refers to the concentration of olefins in the reformate before the reaction. In the calculation formula of aromatic loss rate, the aromatic concentration at the end of the reaction refers to the concentration of aromatics in the reformate after the reaction is completed, and the aromatic concentration before the reaction refers to the concentration of aromatics in the reformate before the reaction. The concentration of olefins or aromatics in the reformate before or after the reaction can be measured by chromatography.

[0055] 20% Ni / SiO2 catalyst preparation example:

[0056] Weigh 290g Ni(NO3)2·6H2O and 773g silica sol (solid content 30%) and dissolve them in deionized water to prepare a solution a with a concentration of 1.0mol / L in terms of Ni ions; prepare a 1.0mol / L sodium hydroxide solution b; keep solution a in a stirring state and slowly add solution b to solution a until the pH value of the system reaches 10.5. After the addition is complete, continue stirring for 1h, then stop stirring and let stand for aging for 8h. Then filter and wash the precipitate to neutrality, dry the filter cake in a forced air drying oven at 110°C for 12h, and then calcine in a muffle furnace at 500°C for 3h to obtain a nickel-silicon composite oxide. Finally, the above nickel-silicon composite oxide is reduced by hydrogen to obtain a 20% Ni / SiO2 catalyst.

[0057] Example 1

[0058] Add 20.0g reformed oil, 0.1g vinyl norbornene and 0.1g 20% ​​Ni / SiO2 catalyst to a 100mL reactor, tighten the reactor and replace the gas in the reactor with 3MPa hydrogen. Start stirring at 60℃, the stirring speed is 600r / min, and the reaction time is 0.5h. Finally, the olefin removal rate is 99.7% and the aromatic loss rate is 0.2%.

[0059] Example 2

[0060] Add 20.0g reformed oil, 0.2g propenyl norbornene and 0.3g Raney Ni catalyst to a 100mL reactor, tighten the reactor and replace the gas in the reactor with 5MPa hydrogen. Start stirring at 100℃, the stirring speed is 600r / min, and the reaction time is 2h. Finally, the olefin removal rate is 99.8% and the aromatic loss rate is 0.3%.

[0061] Example 3

[0062] Add 20.0g reformed oil, 0.1g dicyclopentadiene and 0.1g 0.5% Pd / C catalyst to a 100mL reactor, tighten the reactor and replace the gas in the reactor with 4MPa hydrogen. Start stirring at 60℃, the stirring speed is 600r / min, and the reaction time is 1h. Finally, the olefin removal rate is 99.5% and the aromatic loss rate is 0.1%.

[0063] Example 4

[0064] 3g of 20% Ni / SiO2 catalyst was used in a fixed bed reactor to carry out deolefination reaction of reformed oil. Norbornene was dissolved in the reformed oil and the mass fraction of norbornene was 2%. The reaction temperature was 60°C, the hydrogen pressure was 3MPa, and the reaction mass space velocity was 10h -1 , hydrogen to oil volume ratio was 800. Finally, the catalyst was operated continuously for 1000 h, and the catalytic activity did not decrease significantly, the olefin removal rate was 99.8%, and the aromatic loss rate was 0.2%.

[0065] Example 5

[0066] Add 20.0g reformed oil, 0.1g dicyclopentadiene and 0.1g 3% Co-11% Mo / γ-Al2O3 catalyst to a 100mL reactor, tighten the reactor and replace the gas in the reactor with 4MPa hydrogen. Start stirring at 60℃, the stirring speed is 600r / min, and the reaction time is 1h. Finally, the olefin removal rate is 95.4% and the aromatic loss rate is 0.1%.

[0067] Example 6

[0068] Add 20.0g reformed oil, 0.1g cyclopentene and 0.1g 20% ​​Ni / SiO2 catalyst to a 100mL reactor, tighten the reactor and replace the gas in the reactor with 3MPa hydrogen. Start stirring at 60℃, the stirring speed is 600r / min, and the reaction time is 0.5h. Finally, the olefin removal rate is 97.6% and the aromatic loss rate is 0.2%.

[0069] Comparative Example 1

[0070] Add 20.0g reformed oil and 0.1g 20% ​​Ni / SiO2 catalyst to a 100mL reactor, tighten the reactor and replace the gas in the reactor with 3MPa hydrogen. Start stirring at 60℃, the stirring speed is 600r / min, and the reaction time is 0.5h. Finally, the olefin removal rate is 69.5% and the aromatic loss rate is 0.1%.

[0071] From the above results, it can be seen that the methods for removing olefins from reformed oil of Examples 1 to 6 of the present invention have the characteristics of mild reaction process, low cost and low aromatic loss rate. Under the same reaction conditions, compared with Comparative Example 1 without adding hydrogenation aid (vinyl norbornene), the olefin removal rate of Example 1 is improved, which indicates that the introduction of hydrogenation aid (vinyl norbornene) in the reaction system promotes the removal of olefins in reformed oil.

[0072] In summary, the present invention promotes the removal of olefins by introducing a hydrogenation aid into the reaction system for deolefination of reformed oil, and is expected to be widely used in the future.

[0073] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "install", "connect" and "connect" should be understood in a broad sense. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0074] The present application has been described above in conjunction with preferred embodiments, but these embodiments are only exemplary and serve only as an illustration. On this basis, various replacements and improvements may be made to the present application, all of which fall within the scope of protection of the present application.

Claims

1. A method for removing olefins from reformed oil, characterized in that: The method includes: The reformed oil, the hydrogenation aid and the hydrogenation catalyst are contacted to carry out the hydrogenation reaction of the olefins; The hydrogenation aid is selected from one or more combinations of norbornene, C2-C6 olefin-substituted norbornene, styrene, 1-butene, cyclopentene and dicyclopentadiene.

2. The method according to claim 1, characterized in that The C2-C6 olefin-substituted norbornene is selected from one or more combinations of vinyl norbornene, propenyl norbornene and butenyl norbornene.

3. The method according to claim 1, characterized in that The mass ratio of the hydrogenation aid to the reformed oil is 1:(1-1000); Preferably, the mass ratio of the hydrogenation aid to the reformed oil is 1:(1-100).

4. The method according to claim 1, characterized in that: The hydrogenation catalyst comprises an active component and a carrier; The active component is selected from one or more combinations of Ni, Mo, W, Co, Pd, Pt and Rh; The carrier is selected from one or more combinations of SiO2, C, Al2O3 and molecular sieves.

5. The method according to claim 4, characterized in that The active component is selected from one or more combinations of Ni, Pd and Pt, and the carrier is selected from one or more combinations of SiO2, C and Al2O3.

6. The method according to any one of claims 1 to 5, characterized in that: The hydrogenation reaction is carried out in a fixed bed reactor.

7. The method according to claim 6, characterized in that The conditions of the hydrogenation reaction include: The reaction temperature is 10℃~200℃, the hydrogen pressure is 0.1MPa~10MPa, and the mass space velocity is 0.1h -1 ~50h -1 , the volume ratio of hydrogen to oil is 10 to 1000.

8. The method according to claim 6, characterized in that Contacting the reformate, the hydrogenation aid and the hydrogenation catalyst comprises: The hydrogenation aid is dissolved in the reformed oil, and then fed into the fixed bed reactor to contact with the hydrogenation catalyst, and hydrogen is introduced.

9. The method according to any one of claims 1 to 5, characterized in that: The hydrogenation reaction is carried out in a high-pressure reactor.

10. The method according to claim 9, characterized in that The conditions of the hydrogenation reaction include: The reaction temperature is 10°C to 200°C, the hydrogen pressure is 0.1MPa to 10MPa, the reaction time is 0.1h to 10h, the stirring speed is 400r / min to 1000r / min, and the mass ratio of the hydrogenation catalyst to the reformed oil is 1:(1 to 500).

Citation Information

Patent Citations

  • Saturation hydrogenating process for removing olefines from reforming produced oil

    CN1045305C

  • Nickel-silicon composite oxide and preparation method thereof, catalyst containing nickel-silicon composite oxide and applications of catalyst

    CN111215072A

  • Catalyst for liquid-phase hydrogenation olefin removal of attapulgite-based reformate, as well as preparation method and application of catalyst

    CN106268792A

  • Non-noble metal catalyst for selective hydrogenation olefin removal of reformate as well as preparation method and application thereof

    CN110841650A

  • Cytalyst for reformed formation oil selective hydrogen removing olefin

    CN1448474A