Detection method for rapidly detecting glue failure of dimming film

The peel test of the dimming film sample is solved by peeling tester, which has solved the problem of long and incomplete detection time in the prior art, and has achieved rapid and accurate glue opening inspection, which has improved the service life and yield rate of the product.

CN119064262APending Publication Date: 2024-12-03SHANGHAI MEMBRANE NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411007297.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The prior art cannot quickly and effectively detect the problem of dimming film glue opening, resulting in long, cumbersome and incomplete detection time, affecting the service life and yield of the product.

Method used

The peeling tester is used to carry out peeling tests on the dimming film to cut samples. When the test is stopped, the uniformity is observed. If the unevenness is less than 0.2mm, the glue will not be opened. If it is greater than or equal to 0.2mm or the conductive film and the liquid crystal layer are completely peeled off, the glue will be opened. The machine generates shear force and quickly determines the glue opening situation.

Benefits of technology

It realizes fast, simple and repeatable dimming film glue opening inspection, provides a method to quickly judge the glue opening performance, and improves the service life and yield of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119064262A_ABST
    Figure CN119064262A_ABST
Patent Text Reader

Abstract

The invention discloses a detection method for rapidly detecting glue failure of a dimming film. The detection method comprises the following steps: S1, cutting the dimming film into a rectangular sample; s2, carrying out a stripping test on the rectangular sample by adopting a stripping test machine; s3, in the testing process, stopping the stripping testing machine for N seconds; s4, continuing to operate the stripping tester until complete stripping is realized; s5, observing the uniformity of the light adjusting film at the stop position, and if the light adjusting film at the stop position is uniform or non-uniform smaller than 0.2 mm occurs, judging that the light adjusting film does not have glue failure; and if the dimming film at the stop position is not uniform and is greater than or equal to 0.2 mm or the conductive film is completely stripped from the liquid crystal layer within the stop time, judging that the dimming film is unglued.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of detection of debonding of dimming films, and more specifically, to a method for quickly detecting debonding of dimming films. Background Art

[0002] PDLC film includes a liquid crystal-plastic core layer and two transparent conductive film surface layers, and the two transparent conductive film surface layers are arranged on both sides of the liquid crystal-plastic core layer. PDLC film can be used to make a series of derivative products such as dimming glass, magic glass, electro-induced liquid crystal fogging glass, Smart Glass, etc. PDLC film and its derivative products are a new type of material. Such products can adjust the incident light between transmission and scattering by controlling the on and off of the applied voltage, thereby controlling the product to change between a transparent state and a fogging state (frosted glass state). It has a double-layer function of transparency and concealment and has an increasingly wide range of applications. During the long-term use and transportation of PDLC film and its derivative products, the liquid crystal-plastic core layer and the transparent conductive film layer of the PDLC film layer will have a debonding phenomenon, and long strips or dots will appear on the edge, with a width of about 2mm; one side is white, and the other side is reflective; it is translucent or even fogged when powered on; in the long-term use and storage and transportation process, it will further expand to the inside. This defect seriously affects the service life and appearance of the product, and this kind of debonding is currently inevitable.

[0003] In order to detect the debonding of the dimming film, a method for detecting the debonding performance of a polymer dispersed liquid crystal film is disclosed in the prior art. The method uses a wet heat aging method to accelerate the change of the performance of the polymer dispersed liquid crystal film, accelerate the aging of the glue layer and the penetration of moisture, and then check the debonding phenomenon of the polymer dispersed liquid crystal film according to the specified conditions to judge the weather resistance of the polymer dispersed liquid crystal film in a wet heat environment. The method uses a steady-state wet heat box to place the polymer dispersed liquid crystal film sample or its derivative in the steady-state wet heat box for aging treatment; after the aging treatment is completed, the polymer dispersed liquid crystal film sample is taken out, and the debonding length and width dimensions of the edge of the polymer dispersed liquid crystal film sample are manually measured; the aging treatment time is 45-50 hours, the aging treatment temperature is 55℃-65℃, and the aging treatment humidity is 90%-99%. This method can partially detect the debonding problem of the polymer dispersed liquid crystal film, but it cannot completely detect the debonding problem, and it takes a long time. During the experiment, it is also necessary to do a comparative test of the liquid crystal film and the dimming glass samples simultaneously, which is cumbersome and the conditions are harsh. Therefore, it is not suitable for testing the debonding of polymer dispersed liquid crystal films. With the in-depth development and wide application of polymer dispersed liquid crystal films and their derivative products such as dimming glass, manufacturers and users are paying more and more attention to the severity of their debonding. Therefore, a method that can quickly detect the debonding performance of polymer dispersed liquid crystal films is needed, so that manufacturers can verify the debonding problem of the formula in advance when designing the formula, improve the formula, ensure that the formula put into use has no debonding problem, and the products produced have no debonding risk in subsequent processing, thereby improving the product yield and reducing costs and corporate product risks. Summary of the invention

[0004] In view of the above-mentioned defects in the prior art, the present invention provides a method for quickly detecting debonding of a dimming film.

[0005] The technical solution adopted by the present invention to solve the technical problem is to construct a method for quickly detecting the debonding of the dimming film, and the detection method comprises the following steps:

[0006] S1. Cut the dimming film into rectangular samples;

[0007] S2, performing a peel test on the rectangular sample using a peel tester;

[0008] S3. During the test, stop the peel tester for N seconds;

[0009] S4, continue to operate the peel tester until it is completely peeled off;

[0010] S5. Observe the uniformity of the dimming film at the stopping point. If the dimming film at the stopping point is uniform or has an unevenness less than 0.2 mm, it is judged that the dimming film will not debond. If the dimming film at the stopping point has an unevenness greater than or equal to 0.2 mm or the conductive film and the liquid crystal layer are completely separated during the stopping time, it is judged that the dimming film will debond.

[0011] In the method for quickly detecting debonding of the dimming film of the present invention, the width of the rectangular sample is 10 mm-200 mm, and the length of the rectangular sample is 50 mm-500 mm.

[0012] In the method for quickly detecting debonding of the dimming film of the present invention, the width of the rectangular sample is 25 mm, and the length of the rectangular sample is 250 mm.

[0013] In the method for quickly detecting debonding of the dimming film of the present invention, stopping the peeling tester for N seconds is specifically:

[0014] Stop the peel tester for 10-3600 seconds.

[0015] In the method for quickly detecting debonding of the dimming film of the present invention, stopping the peeling tester for N seconds is specifically:

[0016] Stop the peel tester for 120 seconds.

[0017] In the method for quickly detecting debonding of the dimming film of the present invention, the peeling tester is a 90° peeling tester or a 180° peeling tester.

[0018] The implementation of the detection method of the invention for rapid detection of debonding of the dimming film has the following beneficial effects: when implementing the detection method of the invention, the dimming film is first cut into rectangular samples, and the rectangular samples are fixed on a peeling tester for peeling test. When the peeling is performed to a small part or half, the peeling tester is stopped for N seconds. Then the peeling tester is continued to run until it is completely peeled. Finally, the uniformity of the dimming film at the stop is observed. If the dimming film at the stop is uniform or has an unevenness less than 0.2 mm, it is judged that the dimming film will not debond; if the dimming film at the stop has an unevenness greater than or equal to 0.2 mm or the conductive film and the liquid crystal layer are completely peeled off during the stop time, it is judged that the dimming film will debond. The present invention adopts a peeling tester, and the machine keeps the dimming film in a peeled state, so that the liquid crystal layer and the conductive film generate shear force, thereby obtaining reliable results, which has the advantages of being simple, fast, and repeatable. The present invention quickly judges the debonding performance of the polymer dispersed liquid crystal film based on the debonding condition of the polymer dispersed liquid crystal film (liquid crystal layer), and provides a reference basis for the use and storage of the polymer dispersed liquid crystal film. In order to take targeted measures to increase the service life of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention will be further described below with reference to the accompanying drawings and embodiments, in which:

[0020] Figure 1 It is a schematic diagram of the process of the method for quickly detecting debonding of the dimming film of the present invention. DETAILED DESCRIPTION

[0021] In order to make the objectives, technical solutions and advantages of the present invention more clear, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings.

[0022] like Figure 1 As shown, in the first embodiment of the method for quickly detecting the debonding of the dimming film of the present invention, the detection method includes the following steps:

[0023] S1. Cut the dimming film into rectangular samples;

[0024] S2, performing a peel test on the rectangular sample using a peel tester;

[0025] S3. During the test, stop the peel tester for N seconds;

[0026] S4, continue to operate the peel tester until it is completely peeled off;

[0027] S5. Observe the uniformity of the dimming film at the stopping point. If the dimming film at the stopping point is uniform or has an unevenness less than 0.2 mm, it is judged that the dimming film will not debond. If the dimming film at the stopping point has an unevenness greater than or equal to 0.2 mm or the conductive film and the liquid crystal layer are completely separated during the stopping time, it is judged that the dimming film will debond.

[0028] It can be understood that observing the uniformity of the dimming film at the stop point is to observe the uniformity of the liquid crystal layer (the debonding condition of the liquid crystal layer) after the conductive film is peeled off.

[0029] When implementing the detection method of the present invention, first cut the dimming film into rectangular samples, fix the rectangular samples on a peeling tester for peeling test, and stop the peeling tester for N seconds when the peeling is carried out to a small part or half. Then continue to run the peeling tester until it is completely peeled. Finally, observe the uniformity of the dimming film at the stop point. If the dimming film at the stop point is uniform or has an unevenness less than 0.2mm, it is judged that the dimming film will not be debonded; if the dimming film at the stop point has an unevenness greater than or equal to 0.2mm or the conductive film and the liquid crystal layer are completely peeled off during the stop time, it is judged that the dimming film will be debonded. The present invention adopts a peeling tester, and the machine keeps the dimming film in a peeled state, so that the liquid crystal layer and the conductive film generate shear force, thereby obtaining reliable results, which has the advantages of being simple, fast, and repeatable. The present invention quickly judges the debonding performance of the polymer dispersed liquid crystal film based on the debonding condition of the polymer dispersed liquid crystal film (liquid crystal layer), and provides a reference basis for the use and storage of the polymer dispersed liquid crystal film. So as to take targeted measures to improve the service life of the product.

[0030] In the present application, the width of the rectangular sample is 10 mm-200 mm, and the length of the rectangular sample is 50 mm-500 mm.

[0031] Preferably, the width of the rectangular sample is 25 mm, and the length of the rectangular sample is 250 mm.

[0032] In the present application, stopping the peel tester for N seconds specifically means: stopping the peel tester for 10-3600 seconds.

[0033] Preferably, the peel tester is stopped for 120 seconds.

[0034] Specifically, the peel tester is a 90° peel tester or a 180° peel tester.

[0035] In addition, in the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", "stacked" and the like should be understood in a broad sense, for example, it can be fixedly connected, detachably connected, or integrated; it can be directly connected, or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0036] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for quickly detecting debonding of a dimming film, characterized in that: The detection method comprises the following steps: S1. Cut the dimming film into rectangular samples; S2, performing a peel test on the rectangular sample using a peel tester; S3. During the test, stop the peel tester for N seconds; S4, continue to operate the peel tester until it is completely peeled off; S5. Observe the uniformity of the dimming film at the stopping point. If the dimming film at the stopping point is uniform or has an unevenness less than 0.2 mm, it is judged that the dimming film will not debond. If the dimming film at the stopping point has an unevenness greater than or equal to 0.2 mm or the conductive film and the liquid crystal layer are completely separated during the stopping time, it is judged that the dimming film will debond.

2. The method for rapidly detecting debonding of a dimming film according to claim 1, characterized in that: The width of the rectangular sample is 10 mm-200 mm, and the length of the rectangular sample is 50 mm-500 mm.

3. The method for rapidly detecting debonding of a dimming film according to claim 1, characterized in that: The width of the rectangular sample is 25 mm, and the length of the rectangular sample is 250 mm.

4. The method for rapidly detecting debonding of a dimming film according to claim 1, characterized in that: The specific method of stopping the peel tester for N seconds is: Stop the peel tester for 10-3600 seconds.

5. The method for rapidly detecting debonding of a dimming film according to claim 1, characterized in that: The specific method of stopping the peel tester for N seconds is: Stop the peel tester for 120 seconds.

6. The method for rapidly detecting debonding of a dimming film according to claim 1, characterized in that: The peel tester is a 90° peel tester or a 180° peel tester.