Glasses and glasses leg core

By using a linear temple core formed by shape memory resin and combined with extrusion forming technology, the problems of high manufacturing cost and difficulty in user adjustment of existing glasses are solved, and the convenience and manufacturing of users can be achieved by adjusting the fit by themselves Reduced costs.

CN119065147APending Publication Date: 2024-12-03JINS HLDG INC
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410683019.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-30
Filing Date
2024-05-29
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The existing glasses temple parts using shape memory resin are expensive to manufacture and it is difficult for users to adjust the fit by themselves, especially the design of the temple parts being pre-bent is not suitable for users with different face shapes and ear shapes.

Method used

A linear temple core formed of shape memory resin is used to bend it through heat treatment and fit the shape of the user's face or ear, and the residual stress is reduced through extrusion forming technology and manufacturing costs are reduced.

Benefits of technology

It realizes that the user can easily adjust the fit of temples while reducing the manufacturing cost of glasses, and avoids bending and restoration through appropriate glass transition temperature range, improving the durability and fit comfort of temples.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119065147A_ABST
    Figure CN119065147A_ABST
Patent Text Reader

Abstract

The invention relates to a pair of glasses and glasses leg cores. The invention provides a pair of eyeglasses, which uses shape memory resin and reduces manufacturing cost while enabling a user to easily adjust fitting degree of temple parts. The eyeglasses according to the present invention comprise: a front frame; a pair of end pieces disposed at both ends of the front frame; the pair of temples are respectively connected with the pair of end pieces; and a pair of linear temples extending in the longitudinal direction of the pair of temples and connected thereto, the pair of linear temples including a linear temple core formed of a shape memory resin in the longitudinal direction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a pair of glasses and a temple core. Background Art

[0002] It has long been known that there are glasses using shape memory resin for temples (for example, Patent Document 1), glasses having ear pads using shape memory resin (for example, Patent Document 2), and glasses using shape memory resin for temple caps into which metal temples having core rods are inserted (for example, Patent Document 3).

[0003] [Background Technology Literature]

[0004] [Patent Document]

[0005] [Patent Document 1] Japanese Utility Model Application Laid-Open No. 1-157316

[0006] [Patent Document 2] Japanese Patent Application Laid-Open No. 8-15654

[0007] [Patent Document 3] Japanese Patent Publication No. 2003-43426 Summary of the invention

[0008] [Problems to be solved by the invention]

[0009] Here, in the glasses using shape memory resin in patent documents 1 to 3, since the relatively expensive shape memory resin is used to manufacture the entire temple including the temple portion of the prescribed shape, or to manufacture the parts covering the temple portion, the manufacturing cost of the glasses increases. In addition, patent document 1 discloses a pair of glasses that can be adjusted by an ordinary user (wearer of the glasses) by himself without having to adjust it in a glasses store, etc., and the temple portion at the front end of the temple is bent to a prescribed angle in the initial state of shape memory. Since the temple portion of the glasses commonly sold is also bent to a prescribed angle in most cases, it is not necessarily easy for users with different face sizes, shapes, ear shapes, etc. to fit the temple portion bent to a prescribed angle to themselves by hand.

[0010] Therefore, an object of the present invention is to provide glasses using shape memory resin, which allows the user to easily adjust the fit of the temple portion while reducing the manufacturing cost.

[0011] [Technical means to solve the problem]

[0012] A pair of glasses according to one aspect of the present invention comprises: a front frame; a pair of temples arranged at both ends of the front frame; a pair of temples respectively connected to the pair of temples; and a pair of temples extending along the long side direction of the pair of temples and connected to the pair of temples and being straight, and the pair of temples comprise a straight temple core formed of shape memory resin along the long side direction.

[0013] [Effects of the invention]

[0014] According to the present invention, it is possible to provide eyeglasses that allow a user to easily adjust the degree of fit of the temple portion and that reduce the manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 1 is a perspective view showing an example of the glasses 100 according to the embodiment of the present invention as seen from the front.

[0016] Figure 2 This is a diagram showing an example of a temple core A obtained by extrusion molding.

[0017] Figure 3 This is a diagram showing an example of a temple core B obtained by injection molding.

[0018] Figure 4 The diagram is for confirming the deformation states of temple cores A and B having a glass transition temperature of 65°C in the initial state, after storage at 90°C for 5 minutes, and after storage at 90°C for 15 minutes.

[0019] Figure 5 The diagram is for confirming the deformation states of temple cores A and B having a glass transition temperature of 75°C in the initial state, after storage at 90°C for 5 minutes, and after storage at 90°C for 15 minutes.

[0020] Figure 6 This is a diagram showing an example of a temple core bent at 30 degrees.

[0021] Figure 7 3 is a diagram showing the results of confirming the angle of the bending recovery of each temple core in Experiment A.

[0022] Figure 8 3 is a diagram showing the cores of each temple in which the bending recovery in Experiment A was visually confirmed.

[0023] Fig. 9 1 and 2 are diagrams showing the results of confirming the angles of the bending recovery of the temple cores in Experiment B.

[0024] Fig.10 3 is a diagram showing the cores of each temple in which the bending recovery in Experiment B was visually confirmed.

[0025] Fig.113 is a diagram showing the results of confirming the angle of the bending recovery of each temple core in Experiment C.

[0026] Fig.12 3 is a diagram showing the cores of each temple in which the bending recovery in Experiment C was visually confirmed.

[0027] Fig.13 This is a graph showing the experimental results of applying a heat load of 70°C for 24 hours to temple cores A and B having a glass transition temperature of 75°C.

[0028] Fig.14 The diagram shows an example of the temple portion of glasses before and after deformation. DETAILED DESCRIPTION

[0029] Hereinafter, with reference to the accompanying drawings, the embodiments of the present invention will be described in detail. However, the embodiments described below are merely examples and are not intended to exclude the application of various changes or technologies that are not explicitly described below. In other words, the present invention can be implemented with various changes without departing from its main purpose. In addition, in the following description of the drawings, the same or similar parts are indicated by the same or similar symbols. The drawings are schematic and may not be consistent with actual dimensions or ratios. The drawings may also contain parts with different dimensional relationships or ratios.

[0031] <Glasses>

[0032] Figure 1 1 is a perspective view showing an example of the glasses 100 according to the embodiment when viewed from the front. Figure 1 As shown, the glasses 100 are an example of glasses, and include a pair of lenses 110 for vision correction, and a frame 120. In addition, in this embodiment, although the lenses 110 are described as a pair of lenses, they are not necessarily a pair. In addition, in this embodiment, although the lenses 110 are described as a component of the glasses 100, the lenses 110 themselves are not necessarily a necessary component of the glasses 100. In addition, as the glasses of the present invention, in addition to vision correction glasses, there are also sunglasses or protective glasses.

[0033] The frame 120 includes, for example, a front frame 140, a pair of temples 180 rotatably connected to both ends of the left and right sides of the front frame 140, and a pair of temples 160 attached to the rear side of the pair of temples 180. The pair of temples 160 each include a temple core 170. In addition, the frame 120 holds a pair of lenses 110, and keeps the lenses 110 and the front frame 140 in an appropriate posture relative to the user's eyes and head.

[0034] The front frame 140 supports a pair of lenses 110. The temple 180 and the temple 160 are pressed against the user's temple to clamp the site. The temple core 170 contained in the temple 160 is formed of a shape memory resin and is formed into a straight line along the long side direction of the temple 180 during manufacturing.

[0035] In addition, as a method of bending the temple 160 of the present invention, for example, the temple 160 is immersed in hot water, and then the user or the like bends the temple core 170 of the shape memory resin so that the temple core 170 fits the shape of the user's face or ear. In this way, since the temple core 170 fits the upper part and the back of the user's ear, the glasses 100 are appropriately prevented from falling off.

[0036] In the following description, for the sake of convenience, Figure 1 The long side direction of the front frame 140 shown is defined as the "left-right direction". In addition, when the glasses 100 are worn, the left side viewed by the user is defined as the "left side", and the right side viewed by the user is defined as the "right side". Furthermore, the short side direction of the front frame 140 is defined as the "upper and lower directions", the upper direction of the head is defined as the "upper direction", and the lower direction of the head is defined as the "lower direction". In addition, the thickness direction of the front frame 140 is defined as the "front-back direction", the front frame 140 side is defined as the "front", and the temple 160 side is defined as the "rear".

[0037] In addition, the glasses 100 according to the present embodiment are formed symmetrically around the nose bridge (middle bridge) 142. Therefore, in the following description, the left and right sides of the symmetrical structure are not distinguished, and only the structure located on either side of the drawing is marked and described.

[0038] The front frame 140 is, for example, a plate-shaped structure extending in the left-right direction, and is curved to protrude forward along the user's face. In addition, the front frame 140 includes: a nose bridge 142 located in the center; a pair of nose pads 144 installed on the left and right sides of the back of the nose bridge 142; a pair of frames 146 formed at the left and right ends of the nose bridge 142; a pair of eyeglass heads 147 formed and arranged at each end of the pair of eyeglass frames 146; and a pair of first hinge parts (not shown) installed on the back of the pair of eyeglass heads 147.

[0039] The nose bridge 142 connects the left and right parts of the front frame 140 (glasses 100). The nose bridge 142 is, for example, a curved plate-shaped member and may be formed of resin or the like.

[0040] The nose pad 144 supports the front frame 140 by clamping the user's nose from both sides, and maintains the height of the front frame 140 relative to the user's eyes. In addition, the nose pad 144 is, for example, a cling type having a resin pad and a metal support. In addition, the posture of the front frame 140 relative to the user's nose and eyes (for example, the distance between the corneal vertices) can be finely adjusted by the deformation of the pad and the support.

[0041] The lens frame 146 holds the lens 110. The lens frame 146 is, for example, an annular member formed along the shape of the lens 110 and is formed of resin or the like.

[0042] A first hinge portion (not shown) is formed on the head 147. The head 147 is, for example, a curved plate-like member and is formed of resin or the like.

[0043] The first hinge portion functions as an example of a connecting portion, and is combined with a second hinge portion (not shown) formed on the side of the temple 180 and having a plate-like shape, so that the temple 180 is rotatably connected to the front frame 140. That is, the first hinge portion and the second hinge portion constitute a hinge.

[0044] The temple 180 is a substantially straight member or a slightly curved member that fits the temple. The temple 180 is connected to the front frame 140 in a manner that allows rotation within a range from a folded position where the angle between the temple 180 and the front frame 140 is the smallest to an open position where the angle between the temple 180 and the front frame 140 is the largest.

[0045] The temple 160 is in a straight line shape extending along the long side direction of the temple 180 and connected thereto. The temple 160 contains a temple core 170 formed of a shape memory resin and in a straight line along the long side direction. The temple 160 is formed of a cylindrical elastic member, such as an elastomer, preferably with water resistance and heat resistance. The temple core 170 can be inserted into the cylindrical cavity inside the temple 160, or the temple core 170 can be covered by the elastic member of the temple 160.

[0046] The temple core 170 is, for example, a shape memory resin with thermoplastic polyurethane as its main component. After being deformed in a rubber state by heat above the glass transition temperature (Tg) (for example, after being immersed in hot water for a specified period of time, taken out and deformed), the deformed shape is maintained by cooling, and the temple core 170 has the following property, namely, when heat is applied again, it will return to its original shape.

[0047] It is known that resin products are subject to time-dependent deformation (deterioration) caused by the strain remaining inside the molded product during the usual molding process, i.e., the so-called residual stress. In addition, there are shape memory resins with various glass transition temperatures. In order to prevent the bending recovery of the temple core 170 during the use of the glasses 100, which may lead to a poor wearing feeling, it is necessary to find a range of glass transition temperatures suitable for maintaining the fitting state of the temple 160.

[0048] Therefore, the inventors conducted the following experiments on the temple core 170 of the present invention. First, various comparisons were made between a temple core obtained by extrusion molding and a temple core obtained by injection molding regarding the manufacturing method of the temple core 170 .

[0049] Figure 2 This is a diagram showing an example of a temple core A obtained by extrusion molding. Figure 2 The temple core A shown is manufactured in a target shape of, for example, a quadrangular prism of 2 mm in width×3 mm in length×65 mm in length.

[0050] Figure 3 This is a diagram showing an example of a temple core B obtained by injection molding. Figure 3 The temple core B shown is manufactured into, for example, a quadrangular prism shape with one end being 2 mm wide by 3 mm long and the other end being 1.6 mm wide by 2.6 mm long, and having a length of 65 mm.

[0051] in addition, Figure 2 The temple core A obtained by extrusion molding shown in FIG. Figure 3 Although the temple core B obtained by injection molding shown in the figure is the same temple core in terms of the target shape, the actual measured values ​​of each temple core may contain some errors. The difference in shape between the two ends of the temple core B is caused by the inclination when the temple core B is pulled out of the mold during injection molding. It is more ideal to make the temple core B as close to the temple core A as possible. In this experiment, "SMP" (Shape Memory Polymer) of SMPTECHNOLOGIES Co., Ltd. is used as the material of the temple core A and the temple core B.

[0052] (Heat load test)

[0053] In this experiment, it is assumed that when the product is used, the temple core 170 is heated for a predetermined time and then bent multiple times, and the deformation of the molded product itself when the heat load is applied is confirmed to simulate the observation of the change over time. Specifically, the temple core A and the temple core B, whose glass transition temperatures are 65°C and 75°C, are stored in a constant temperature machine at 90°C for a fixed time, and the change is visually confirmed. 90°C is assumed to be the normal temperature of hot water heated by a household electric kettle, assuming that the temple 160 (temple core 170) is immersed in hot water to deform it.

[0054] Figure 4 The diagram is used to confirm the deformation state of the temple cores A and B having a glass transition temperature of 65°C in the initial state, after being stored at 90°C for 5 minutes, and after being stored at 90°C for 15 minutes. The storage time of 5 minutes and 15 minutes is set based on the assumption that the temple part is immersed in 90°C for 15 seconds to 45 seconds for bonding (bending) about 20 times as the product usage, and is calculated as 15 seconds × 20 times ÷ 60 seconds = 5 minutes and 45 seconds × 20 times ÷ 60 seconds = 15 minutes.

[0055] exist Figure 4 In the example shown, the temple core A (extrusion molded product) having a glass transition temperature of 65°C hardly deforms after storage at 90°C for 5 minutes and 90°C for 15 minutes compared to the initial state after manufacturing. The length of the temple core A slightly shortens as the storage time increases, but this is not a problem at a practical level.

[0056] exist Figure 4 In the example shown, the temple core B (injection molded product) with a glass transition temperature of 65°C shrinks to about half its length after storage at 90°C for 5 minutes and 90°C for 15 minutes compared to the state after manufacturing. In addition, the temple core B to which the heat load is applied also deforms in shape from a straight line, such as the end portion being slightly warped.

[0057] The reason why the temple core B with a glass transition temperature of 65°C shrinks or deforms is that residual stress is likely to remain during injection molding. It is believed that in injection molding, when the shape memory resin material is poured into the mold and cooled and solidified, uneven pressure is applied to the resin, so residual stress remains in the molded temple core B. Therefore, it is believed that the injection-molded temple core B shrinks or deforms due to the residual stress after heat loading.

[0058] On the other hand, the reason why it is believed that the temple core A is hardly deformed is that, unlike injection molding, extrusion molding does not involve the step of applying pressure to the resin inside the mold and then cooling and solidifying it, so residual stress is not likely to remain inside the resin during molding.

[0059] Figure 5 This is a diagram for confirming the deformation state of temple core A and temple core B with a glass transition temperature of 75°C in the initial state, after being stored at 90°C for 5 minutes, and after being stored at 90°C for 15 minutes. Figure 5 In the example shown, the temple core A (extrusion molded product) with a glass transition temperature of 75°C hardly deforms after storage at 90°C for 5 minutes and 90°C for 15 minutes compared to the initial state after manufacturing. As the storage time increases, the length of the temple core A decreases slightly, but the shrinkage is smaller than that of the temple core A with a glass transition temperature of 65°C.

[0060] exist Figure 5 In the example shown, regarding the temple core B (injection molded product) with a glass transition temperature of 75°C, similarly to the temple core B with a glass transition temperature of 65°C, compared with the state after manufacturing, its length is shrunk after storage at 90°C for 5 minutes and after storage at 90°C for 15 minutes, and deformation such as slight warping of the ends occurs.

[0061] According to the results of the above heat load test, the temple core B as an injection molded product shrinks or deforms from the initial state due to the heat load conditions, regardless of whether it is a temple core with a glass transition temperature of 65°C or a temple core with a glass transition temperature of 75°C, and therefore may not be suitable for practical use. On the other hand, the temple core A as an extruded product has better deformation resistance than the temple core B as an injection molded product, regardless of whether it is a glass transition temperature of 65°C or a glass transition temperature of 75°C, and shrinks slightly even after the heat load is applied, so there is no problem in terms of practical use. In addition, the temple core A with a glass transition temperature of 75°C shrinks less than the temple core A with a glass transition temperature of 65°C, so it can be said that it is more suitable for practical use.

[0062] (30 degree bending recovery test)

[0063] In this experiment, in order to find the appropriate range of glass transition temperature, the following experiment was conducted, that is, the temple core 170 that was bent under heat and then cooled to maintain the bent state was confirmed whether it would bend back to its original shape due to the heat load of the assumed temperature (body temperature or midsummer temperature, etc.). The temple core used for the experiment was made by extrusion molding, and after heat treatment, it was bent 30 degrees from the approximate center position of the temple core using a specified tool. The reason for the 30-degree bend is that the temples of glasses usually sold are bent about 30 to 35 degrees based on the long side direction of the temple wire.

[0064] Figure 6 : is a diagram showing an example of a temple core bent at 30 degrees. The temple core used in the experiment is as follows Figure 6It is shown bent at 30 degrees and has glass transition temperatures of 45°C, 55°C, 65°C, and 75°C.

[0065] Two temple cores were prepared for each of the glass transition temperatures, and a bending recovery test was performed on each temple core under the following experimental conditions.

[0066] Experiment A: Each temple core was stored in a constant temperature machine at 40°C for 8 hours, and the bending recovery was confirmed by visual inspection and angle measurement.

[0067] Experiment B: Each temple core was stored in a constant temperature machine at 40°C for 24 hours, and the bending recovery was confirmed by visual inspection and angle measurement.

[0068] Experiment C: After each temple core was stored in a thermostat at 36°C for 8 hours, it was taken out of the thermostat once and the bend was confirmed to have recovered by visual inspection and angle measurement. Then it was put back into the thermostat and stored in the thermostat for 16 hours (i.e., after a total of 24 hours of storage), the bend was confirmed to have recovered by visual inspection and angle measurement.

[0069] In addition, the storage time of 8 hours corresponds to the normal use time in a day, and 24 hours corresponds to the use time when used all day. In addition, the storage temperature of 36°C corresponds to body temperature, and 40°C corresponds to the temperature in midsummer. In addition, the temple cores used in Experiments A to C are different molded products prepared for each experiment.

[0070] Figure 7 : is a graph showing the results of confirming the angle of the bending recovery of each temple core in Experiment A. Figure 7 In the example shown, two temple cores with a glass transition temperature of 45°C (Tg45°C products i and ii) were stored in a thermostat at 13°C and 14°C, respectively, and the bending recovery occurred. It can be said that the bending recovery occurred because the glass transition temperature was 45°C, which was 5°C lower than the 40°C of the thermostat.

[0071] In addition, the two temple cores with a glass transition temperature of 55°C (Tg55°C products i and ii) were stored in a constant temperature machine at 23°C and 25°C, respectively, and some bending recovery occurred. The glass transition temperature is 55°C, while the constant temperature machine is 40°C, and the difference between the two is 15°C, but some bending recovery occurred.

[0072] according to Figure 7In the example shown, two temple cores (Tg65°C products i and ii, Tg75°C products i and ii) with glass transition temperatures of 65°C and 75°C, respectively, were stored in a thermostat at 30°C, and no bending recovery occurred. It can be said that the bending recovery did not occur because the glass transition temperatures were sufficiently high at 65°C and 75°C (the difference between the two was 25°C or more) relative to the experimental temperature of 40°C.

[0073] Figure 8 3 is a diagram showing each temple core in which the bending recovery in Experiment A was visually confirmed. Figure 8 The two temple cores with a glass transition temperature of 45°C have both recovered from the bending and returned to a state close to the initial state (straight line). Figure 7 The results shown show that the bending angles of the temple cores after storage were 13 degrees and 14 degrees.

[0074] Figure 8 The two temple cores with a glass transition temperature of 55°C have both experienced some bending recovery. Figure 7 The results shown in the figure show that the bending angles of the temple cores after storage are 23 degrees and 25 degrees. Figure 8 As shown, some bending recovery was confirmed even under visual observation.

[0075] about Figure 8 The two temple cores with glass transition temperatures of 65°C and 75°C, respectively, did not recover from bending even when visually observed. Therefore, according to this experiment, if the difference between the assumed temperature of the heat load and the glass transition temperature is 15°C, recovery from bending will occur, and if the difference between the two is 25°C, recovery from bending will not occur. Therefore, if the difference between the two is about 20°C, recovery from bending is likely not to occur. According to the above study, a temple core having a glass transition temperature higher than the assumed temperature by more than 20°C is suitable for the temple core of the technology of the present invention. In addition, the assumed temperature refers to the temperature assumed to be the heat load on the glasses when the glasses are normally used.

[0076] Fig. 9 : is a graph showing the results of confirming the angle of the bending recovery of each temple core in Experiment B. Fig. 9 In the example shown, two temple cores with a glass transition temperature of 45°C were stored in a constant temperature machine at 5°C and 9°C, respectively, and the bending recovery occurred. Figure 7 The results shown and Fig. 9 Comparing the results shown in the figure, it can be seen that the bending recovery does not occur linearly as the storage time increases. Figure 7 The results shown in the figure show that the bending angle recovered by 16.5 degrees (bending recovery angle (17+16) / 2) within 8 hours, that is, the recovery exceeded 50%. Fig. 9The results shown show that the recovery is 23 degrees within 24 hours (bending recovery angle (25+21) / 2), which is about 77%.

[0077] In addition, according to Fig. 9 In the example shown, two temple cores with a glass transition temperature of 55°C are stored in a constant temperature machine at 22°C, 20°C, and Figure 7 Compared with the results shown in Figure 2, the bending recovery has further occurred. However, similar to the temple core with a glass transition temperature of 45°C, the bending recovery does not occur linearly as the storage time increases. Figure 7 The results shown in the figure show that the bending angle is restored by 6 degrees within 8 hours (bending angle (7+5) / 2), that is, 20% is restored. Fig. 9 The results shown show that the bending recovery is 9 degrees (bending recovery angle (8+10) / 2) within 24 hours, that is, 30%. In summary, the bending recovery caused by heat load shows a trend of large recovery in the initial period of time when the heat load is applied, and then gradually recovering.

[0078] In addition, according to Fig. 9 In the example shown, two temple cores with glass transition temperatures of 65°C and 75°C, respectively, were stored in a thermostat at 30°C, and no bending recovery occurred. It can be said that although the storage time was longer, the glass transition temperatures were still high enough at 65°C and 75°C (the difference between the two was more than 25°C) relative to the experimental temperature of 40°C, so no bending recovery occurred.

[0079] Fig.10 3 is a diagram showing the cores of each temple in which the bending recovery in Experiment B was visually confirmed. Fig.10 The two temple cores with a glass transition temperature of 45°C have both recovered from the bending and returned to a state close to the initial state (straight line). Fig. 9 The results shown show that the bending angles of the temple cores after storage were 5 degrees and 9 degrees.

[0080] Fig.10 The two temple cores with a glass transition temperature of 55°C have both recovered from bending. Fig. 9 The results shown in the figure show that the bending angles of the temple cores after storage are 22 degrees and 20 degrees. Fig.10 As shown, the bending recovery was confirmed even under visual observation.

[0081] about Fig.10The two temple cores with glass transition temperatures of 65°C and 75°C, respectively, did not recover from bending even under visual observation. Based on Experiment A and Experiment B, according to the above research, it can be said that as long as the temple core has a glass transition temperature at least 20°C higher than the assumed temperature, it will not recover from bending regardless of the storage time, and is suitable for the temple core of the technology of the present invention.

[0082] Fig.11 : is a graph showing the results of confirming the angle of the bending recovery of each temple core in Experiment C. Fig.11 In the example shown, two temple cores with a glass transition temperature of 45°C were stored in a thermostat for 8 hours and 24 hours, and the temperatures were 17°C and 14°C, and 14°C and 11°C, respectively, and the bend recovery occurred. It can be said that the bend recovery occurred because the glass transition temperature was 45°C, which was about 10°C lower than the 36°C of the thermostat.

[0083] In addition, according to Fig.11 In the example shown, two temple cores with a glass transition temperature of 55°C were stored in a constant temperature machine for 8 hours and 24 hours at 30°C and 29°C, respectively, and almost no bending recovery occurred. It is believed that this is because the glass transition temperature is 55°C, which is about 20°C lower than the constant temperature of 36°C, so no bending recovery occurred. This point is also consistent with the above research.

[0084] according to Fig.11 In the example shown, two temple cores with glass transition temperatures of 65°C and 75°C were stored in a constant temperature machine for 8 hours and 24 hours at 30°C, respectively, and no bending recovery occurred. It can be said that the bending recovery did not occur because the glass transition temperatures were sufficiently high at 65°C and 75°C (the difference between the two was about 30°C or more) relative to the experimental temperature of 36°C.

[0085] Fig.12 : is a diagram showing each temple core in which the bending recovery in Experiment C was visually confirmed. Fig.12 The two temple cores shown with a glass transition temperature of 45°C both recovered from bending despite a heat load of 36°C.

[0086] about Fig.12 The two temple cores with a glass transition temperature of 55° C. shown in the figure have almost no bending recovery. Since it is considered that the most common heat load applied when glasses are usually used is 36° C., which is the body temperature, when 36° C. is set as the assumed temperature, the temple core with a glass transition temperature of 55° C. is suitable for the temple core of the present invention.

[0087] about Fig.12The two temple cores with glass transition temperatures of 65°C and 75°C, respectively, did not recover from bending even under visual observation. According to this experiment, the temple cores with glass transition temperatures of 55°C, 65°C, and 75°C did not recover from bending relative to the assumed temperature of 36°C, so temple cores with glass transition temperatures at least about 20°C higher than the assumed temperature are suitable for the temple cores of the present invention.

[0088] <Example>

[0089] According to the results of the heat load test and the 30-degree bending recovery test, it can be said that the following temple core 170 is suitable for the technology of the present invention. First, according to the heat load test, it can be known that the temple core A formed by extrusion has a higher deformation resistance than the temple core B formed by injection molding, so the temple core of the present invention is preferably manufactured by extrusion molding.

[0090] In addition, based on the results of experiments A to C of the 30-degree bending recovery experiment, the glass transition temperature of the temple core 170 can be determined based on the assumed temperature of the heat load. For example, the glass transition temperature of the temple core 170 is preferably within the range of a first temperature set based on a temperature higher than body temperature and a second temperature higher than the first temperature. In this way, the glass transition temperature of the temple core 170 has a clear reference, and the glass transition temperature of the mounted product can be determined.

[0091] In addition, the first temperature of the temple core 170 may be about 55° C., and the second temperature may be about 100° C. For example, Fig.11 The temple core of the experiment C shown in the figure, which has a glass transition temperature of 55°C, hardly recovers from bending at the assumed temperature of 36°C. Therefore, 55°C, which is the lower limit of the glass transition temperature, is a temperature that can be adopted according to the assumed temperature of the heat load. In addition, the upper limit of 100°C is the upper limit of the temperature that can be used as hot water when the temple 160 (the temple core 170) is immersed in hot water to deform in an ordinary household.

[0092] In addition, the first temperature of the temple core 170 may be about 65° C., and the second temperature may be about 75° C. Figure 7 and Fig. 9 The results of Experiments A and B show that even if the assumed temperature of the heat load is 40° C., the bending recovery does not occur as long as the glass transition temperature is at least 65° C. Furthermore, by setting the glass transition temperature of the temple core 170 to 75° C. or less, there is no need to prepare extra high-temperature hot water.

[0093] Alternatively, the glass transition temperature of the temple core 170 may be approximately 75° C. If the assumed temperature of the heat load is 50° C. in consideration of the recent temperature rise, if the glass transition temperature is 65° C., the difference between the two is 15° C. Figure 7 and Fig. 9 The results of Experiment A and Experiment B (assuming that the difference between the product with a temperature of 40°C and a glass transition temperature of 55°C is 15°C) show that bending recovery may occur. However, if the glass transition temperature is 75°C, the difference between the two is 25°C. Figure 7 and Fig. 9 The results of Experiments A and B (the difference between the assumed temperature of 40°C and the glass transition temperature of 65°C is 25°C) shown in the figure show that no bending recovery occurs. In addition, as long as the difference between the assumed temperature and the glass transition temperature is at least 20°C, a shape memory resin with a glass transition temperature of 70°C can be used when the assumed temperature is 50°C.

[0094] In addition, the upper limit of the glass transition temperature of the temple core 170 may be about 90° C. About 90° C. is the temperature of hot water that can be prepared using, for example, a household electric kettle or an electric kettle. Therefore, a shape memory resin having an upper limit of about 90° C. relative to each lower limit of the glass transition temperature may also be used.

[0095] In addition, the glass transition temperature of the temple core 170 may be, for example, about 80° C., about 85° C., etc. The glass transition temperature of the temple core 170 may be set according to the assumed temperature of the heat load.

[0096] In addition, based on the relationship between the assumed temperature of 36°C and the glass transition temperature of 55°C in Experiment C, it is considered that bending recovery is unlikely to occur as long as the difference between the assumed temperature and the glass transition temperature is about 20°C. In this way, when the assumed temperature is 40°C as in Experiments A and B, a shape memory resin with a glass transition temperature of about 60°C can also be used. For example, a shape memory resin with a glass transition temperature of about 60°C as the lower limit and about 75, 80, 85, 90°C or 100°C as the upper limit can also be used.

[0097] Fig.13 This is a graph showing the experimental results of applying a heat load of 70°C for 24 hours to the temple core A and the temple core B with a glass transition temperature of 75°C. Fig.13 In the example shown, the temple core A formed by extrusion and the temple core B formed by injection molding are shown before and after the heat load treatment. Fig.13 As shown, the injection molded temple core B warps due to residual stress, but the extruded temple core A does not show significant deformation.

[0098] Here, annealing refers to a heat treatment that eliminates residual stress in a resin product (resin molded product or resin material) by applying heat, stabilizes dimensional accuracy, or prevents deformation or cracks such as strain of the resin. In the annealing treatment, residual stress is eliminated by heat loading at a high temperature (usually 10°C to 30°C higher than the glass transition temperature for crystalline resins including the shape memory resin of the present invention) for a predetermined time (e.g., 8 hours). Fig.13 The conditions shown are different from those of the annealing treatment, but they are the same in terms of eliminating residual stress. Fig.13 Under the heat load condition of the glass transition temperature shown in FIG. 1 , the injection molded temple core B will also be greatly deformed due to the long-term heat load, and it is believed that it is difficult to eliminate the residual stress when it is manufactured. In contrast, the temple core A after the heat load treatment does not deform significantly, and according to the above Figure 4 and Figure 5 The results show that the temple core A can eliminate the residual stress through the usual annealing treatment, and the temple core A after annealing can be said to be more suitable for the temple core of the technology of the present invention.

[0099] In addition, the temple core 170 may also include: a first portion having a glass transition temperature within a first temperature range; and a second portion having a glass transition temperature within a second temperature range. For example, it is preferable to use a shape memory resin having a first glass transition temperature within the first temperature range to form a prescribed portion of the temple core 170 including the center portion bent as an earrest in the length direction, and use a shape memory resin having a second glass transition temperature within the second temperature range to form portions other than the prescribed portion. In addition, the average temperature of the first temperature range may also be lower than the average temperature of the second temperature range, satisfying the relationship of the first glass transition temperature < the second glass transition temperature.

[0100] In this way, the temple core 170 can be arranged with a portion that is desired to be bent and a portion that is not desired to be bent. For example, if only the portion that is hung on the ear is desired to be bent, the temple 160 is partially immersed in hot water having a temperature that is not less than the first glass transition temperature and not more than the second glass transition temperature. If the entire temple core 170 is desired to be bent to fit the ear, the temple 160 is immersed in hot water having a temperature that is not less than the second glass transition temperature so that the temple core 170 is freely bent. In addition, the temple core 170 may have three or more different glass transition temperatures instead of two.

[0101] In addition, the temple 180 or the temple 160 may be provided with an indicator indicating the position of the temple 160 when immersed in hot water. For example, an indicator is attached to the outer skin of the temple 180 or the temple 160, indicating the appropriate position when the front end of the temple 160 (the end on the opposite side from the front frame 140) is immersed in hot water. The indicator may be any indicator, such as a line, a mark, a color, a pattern, etc., as long as the user can recognize it. In this way, the user can easily understand the position of the temple in hot water.

[0102] In addition, the temple 160 may also be configured to be able to recognize when the temple core 170 reaches a temperature above a threshold. For example, the outer skin of the temple 160 may be coated with a thermochromic paint that changes color at a temperature above the glass transition temperature of the temple core 170, or a thermoplastic tape that changes color at a temperature above the glass transition temperature. In this way, the user can know when to start bending the temple 160 after immersing it in hot water.

[0103] In addition, the temple core 170 may be formed as a straight temple core made of shape memory resin and constituted as one component, and included in the temple 160 included in the glasses and extending along the long side direction of the temple 180 and connected to the temple 180. In this way, the temple core 170 can be manufactured and sold separately.

[0104] Fig.14 1 and 2 are diagrams showing an example of the temple 160 of the eyeglasses 100 before and after partial deformation. Fig.14 The upper part of the spectacles 100 before deformation is shown. The temple 160 including the temple core 170 extends in the long side direction of the temple wire and is connected to the temple wire.

[0105] Fig.14 The lower part of the figure shows the deformed glasses 100. The temple 160 including the temple core 170 is bent so as to fit the ear of the user. For example, the user immerses the temple 160 part in hot water, and wears the glasses 100 when the temple core 170 is considered to have reached a predetermined temperature or above, so that the temple 160 part is deformed to fit the ear of the user.

[0106] Furthermore, by selling the temples 160 of the glasses 100 in a straight state as they were manufactured, ordinary users who do not have special skills can easily adjust the fit according to the size of the face (where to bend) and the shape of the ears (how much to bend) from the initial bending. For example, compared with the prior art where the fit is adjusted from the initial bent temple, the straight temples 160 can easily be bent in the up-down direction to adjust the situation of hanging on the ears, and can be bent in the left-right direction to adjust the fit with the head when the glasses 100 are worn. In addition, the present invention does not exclude the situation of selling the glasses 100 in a bent state. During manufacturing, as long as the straight temple core 170 is arranged in the glasses 100 in a state where the shape is retained or bent, it is covered within the scope of the present invention. That is, as long as the temple core 170 returns to its original straight state when a heat load is applied, it is covered within the scope of the present invention regardless of its shape when sold.

[0107] In addition, in the technology of the present invention, as long as only the temple core 170 is made of shape memory resin, the manufacturing cost is suppressed compared with the prior art that the temple wire and the temple are integrally made of shape memory resin. In addition, since the temple core 170 can be traded separately, it is possible to carry out local repairs and replacements, and the cost of returns can also be reduced. Furthermore, the temple core 170 is preferably in a straight line shape. Since it can be manufactured by extrusion molding, the characteristics of the extrusion molding product with less residual stress can be exerted, and the defective product rate caused by deformation can be reduced. In addition, extrusion molding includes not only the situation that it is initially formed into a straight line, but also the situation that the shape memory resin formed into a plate shape is processed into a straight line by punching or cutting, etc. In addition, the so-called straight line shape can be a roughly straight line shape, as long as it does not deviate from the main purpose of the present invention, such as a shape with a groove from one end to the other end in the long side direction (the cross section perpendicular to the long side direction is a concave shape), or a shape obtained by processing a part of the resin to set a convex part for engagement with the temple 160 after extrusion molding, etc. are all straight lines.

[0108] In addition, there may be an appropriate combination of the relationship between the material of the temple 160 and the glass transition temperature of the temple core 170. The material of the temple 160 may be appropriately selected according to the glass transition temperature of the temple core 170. For example, when the glass transition temperature of the temple core 170 is higher than a specified temperature (e.g., 80° C.), an elastomer with high heat resistance may be selected as the material of the temple 160.

[0109] In addition, the present invention does not exclude the temple core 170 made by injection molding. For example, it is known that the deformation caused by heat load can be suppressed by making the residual stress uniform by injection compression molding. Furthermore, it is considered that the time-dependent deformation of the injection-molded temple core B can also be suppressed by the combination with the material of the temple 160. In addition, although the temple core 160 and the temple core end of the temple 180 can be disassembled, they are preferably fixedly installed to avoid falling off due to heat load.

[0110] The present invention has been described above using various embodiments, but the technical scope of the present invention is not limited to the scope described in the embodiments. It is obvious to the industry that various changes or improvements can be made to the embodiments. It is clear from the claims that forms to which such changes or improvements are made are also included in the technical scope of the present invention.

[0111] [Explanation of Symbols]

[0112] 100: Glasses (glasses)

[0113] 120: Frame

[0114] 140: Front frame

[0115] 142: Zhongliang

[0116] 144: Nose pads

[0117] 146: Lower frame

[0118] 147: Zhuangtou

[0119] 160: temples

[0120] 170: temple core

[0121] 180: Foot silk.

Claims

1. A pair of glasses comprising: Front frame; A pair of heads are arranged at both ends of the front mirror frame; A pair of foot wires, respectively connected to the pair of head wires; and A pair of temples extend along the long side direction of the pair of temples and are connected to the temples, and are linear, and include a linear temple core formed of shape memory resin along the long side direction.

2. The glasses according to claim 1, wherein the glass transition temperature of the temple core is within a range of a first temperature set based on a temperature higher than body temperature and a second temperature higher than the first temperature.

3. The glasses according to claim 2, wherein the first temperature is about 55 degrees and the second temperature is about 100 degrees. The glasses according to claim 3 , wherein the first temperature is about 65 degrees and the second temperature is about 75 degrees.

5. The eyeglasses of claim 4, wherein the glass transition temperature of the temple core is about 75 degrees.

6. Eyeglasses according to any one of claims 1 to 5, wherein the temple core is manufactured by extrusion.

7. The glasses according to claim 1, wherein the temple core comprises: a first portion having a glass transition temperature within a first temperature range; and a second portion having a glass transition temperature within a second temperature range.

8. The glasses according to any one of claims 1 to 5, wherein the temple or the temple is provided with an index indicating the position of the temple when immersed in hot water.

9. Eyeglasses according to any one of claims 1 to 5, wherein the temple is configured to be able to recognize that the temple core has reached a temperature above a threshold value.

10. A temple core, included in a temple included in a pair of glasses and extending along a long side direction of a temple and connected to the temple, formed of a shape memory resin and having a straight line shape.

Citation Information

Cited By

  • Intelligent glasses

    CN120028963A