SiC MOSFET with high saturation current and preparation method thereof
By designing the N zone next to the Pwell zone in the channel region of the SiC MOSFET device, using the external gate voltage to accelerate the hole carriers into the Pwell zone, the problem of insufficient flow capacity of the SiC MOSFET device is solved and a higher saturation current is achieved and lower gate opening voltage requirements improve device performance.
Patent Information
- Application Number
- CN202411380578.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-12-03
AI Technical Summary
In the growth of gate oxide layer of SiC MOSFET devices, the number of interface defects in element C causes increases, affecting device reliability and channel electron mobility, limiting the device's flow capacity, especially at low voltages.
In the trench gate SiC MOSFET device, N zone is designed next to the Pwell zone, and the external gate voltage is used to accelerate the hole carriers into the Pwell zone, increasing the channel width to improve the flow capacity. The specific steps include forming a SiC Drift layer, an N region, a Pwell region, an NP region, and a PP region on the SiC Sub layer, and forming a U-shaped gate oxide layer by high temperature ion annealing and dry oxygen oxidation, filling the Poly layer and forming an isolation dielectric layer.
It improves the throughput capability and saturation current of SiC MOSFET devices, reduces the gate opening voltage requirements, and enhances the performance of the device.
Smart Images

Figure CN119069357A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a SiC MOSFET with high saturation current and a preparation method thereof. Background Art
[0002] In the field of power electronics, voltage-controlled switching devices are popular due to their lower losses. From low- and medium-voltage Si MOSFET devices to medium- and high-voltage Si IGBT devices, their use conditions cover different switching frequencies, different system voltages, and different power levels, and they are used in all walks of life. However, with the continuous development of society, the field of power electronics is also moving towards higher power and more efficient technologies, and increasingly stringent use conditions have put forward more stringent requirements on power switching devices. Si MOSFET and Si IGBT devices have been developed for a long time. As traditional power switching devices, they are limited by the physical properties of Si materials themselves and have almost reached the theoretical performance limit. Therefore, researchers have begun to study newer materials to prepare more advantageous devices.
[0003] As a typical representative of the third-generation wide bandgap semiconductor materials, SiC has a large bandgap width, high critical breakdown electric field, small intrinsic carrier concentration, fast saturation drift velocity, high melting point, and high thermal conductivity. Its many physical performance advantages make SiC-based power devices have great application prospects in high voltage, high temperature, high frequency and other electronic application fields, among which SiC MOSFET is the main product.
[0004] Although SiC MOSFET devices have many advantages over Si MOSFET and Si IGBT devices, they also have problems. In the preparation of SiC MOSFET, the gate oxide layer is usually grown directly by thermal oxidation. Therefore, the C element in SiC will cause the interface state defects in the growth of the gate oxide layer to increase and the quality to deteriorate. In addition to the product reliability problem, the channel electron mobility of the device will also be relatively low, which inhibits the current flow capacity of the device. Therefore, it is usually recommended to use ≥18V when turning on the gate voltage in SiC MOSFET. In addition, there is a limit saturation current in the channel region of MOSFET devices. When the MOSFET device enters the saturation region, it is difficult for the current to continue to increase with the voltage, which also inhibits the current flow capacity of the device. Therefore, how to improve the current flow capacity of SiC MOSFET devices, such as the saturation current capacity, is crucial to improving the performance of the device. Summary of the invention
[0005] The present invention designs an N region next to a vertical channel region in a trench gate SiC MOSFET device, so that when the device gate is turned on to form a channel, the adjacent N region is affected by an external gate voltage, and the internal hole carriers enter the Pwell region to accelerate the formation of the channel, and the channel width as a current path is also increased, thereby improving the current carrying capacity of the SiC MOSFET device, such as the saturation current.
[0006] The technical solution of the present invention is: A method for preparing a SiC MOSFET with high saturation current comprises the following steps: S100, forming a SiC Drift layer on the top surface of the SiC Sub layer by epitaxial deposition, and sequentially forming an N region and a Pwell region in the SiC Drift layer; S200, forming a P region and a NP region in sequence on the top surface of the Pwell region; S300, forming a PP region on the top surface of the NP region by Al ion implantation, and activating the implanted region by high temperature ion annealing; S400, forming spaced trenches on the top surface of the NP region by etching downward; and sequentially forming a gate oxide layer and a Poly layer in the trenches; S500, forming an isolation dielectric layer and an ohmic contact alloy layer in sequence on the top surface of the NP region; S600, forming a front electrode metal layer on the top surface of the device.
[0007] Specifically, the thickness of the SiC Sub layer in step S100 is 100um-450um, and the doping concentration is 1E19cm -2 .
[0008] Specifically, in step S100, the thickness of the SiC Drift layer is 5um-20um, and the doping concentration is 1E15-3E16cm -2 .
[0009] Specifically, in step S100, the bottom depth of the N region is 0.2um-1.6um, and the doping concentration is 1E17-5E18cm -2 .
[0010] Specifically, in step S100, the bottom depth of the Pwell region is 0.5um-2um, and the doping concentration is 1E17-3E18cm -2 .
[0011] Specifically, in step S200, the thickness of the P region is 0.5um-2um, and the doping concentration is 1E17-3E18cm -2 .
[0012] Specifically, in step S200, the bottom depth of the NP region is 0.2um-1.4um, and the doping concentration is 5E17-1E19cm -2 .
[0013] Specifically, in step S300, the bottom depth of the PP region is 0.8um-4um, and the doping concentration is 1E18-1E19cm -2 .
[0014] Specifically, in step S400, the thickness of the gate oxide layer is 40 nm-100 nm.
[0015] A high saturation current SiC MOSFET, comprising a SiC Sub layer, a SiC Drift layer, a P region, an NP region, an ohmic contact alloy layer and a front electrode metal layer arranged in sequence from bottom to top; The SiC Drift layer is provided with: An N region, located in the middle of the SiC Drift layer and extending downward from the top surface of the SiC Drift layer; A Pwell region extending downward from the top surface of the SiC Drift layer and connected to the N region; a bottom surface of the Pwell region (4) is not higher than a bottom surface of the N region; A PP region extends downward from the top surface of the NP region into the N region; the bottom surface of the PP region and the bottom surface of the N region are in the same plane; A gate oxide layer having a U-shaped cross section extending downward from the top surface of the NP region into the SiC Drift layer; A Poly layer, filled in the gate oxide layer, with a top surface flush with the top surface of the gate oxide layer; The top surface of the NP region is provided with an isolation dielectric layer covering the top surfaces of the gate oxide layer and the Poly layer, and the side of the isolation dielectric layer is connected to the ohmic contact alloy layer.
[0016] The bottom of the front electrode metal layer is connected to the ohmic contact alloy layer and the isolation dielectric layer respectively.
[0017] Specifically, the PP region is located in the N region, and is spaced apart from a side of the N region.
[0018] Beneficial effects of the present invention: Due to the presence of C elements in the thermal oxidation growth of the gate oxide layer, SiC MOSFET will form more interface state defects in the gate oxide layer, resulting in poor material quality, reliability risks, and low device channel electron mobility. Therefore, the external gate voltage must be above 18V to achieve better device performance. In the trench gate SiCMOSFET device, the present invention designs an N region in the Pwell region where the channel is formed, so that when the external gate is turned on and pressurized, the N region is affected by the external gate voltage, and the internal hole carriers will enter to help accelerate the formation of the channel, and the channel width as the flow path will also increase, thereby improving the flow capacity of the SiC MOSFET device and the saturation current. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 Schematic diagram of the structure of the trench gate SiC MOSFET of the present invention; Figure 2 is a structural schematic diagram of step S100 of the present invention; Figure 3 is a schematic structural diagram of step S200 of the present invention; Figure 4 is a schematic structural diagram of step S300 of the present invention; Figure 5 is a schematic structural diagram of step S400 of the present invention; Figure 6 is a schematic structural diagram of step S500 of the present invention; Figure 7 is a schematic diagram of the structure of step S600 of the present invention; Figure 8 is a structural schematic diagram of step S800 of the present invention; Fig. 9 is a structural schematic diagram of step S900 of the present invention; Fig.10 is a structural schematic diagram of step S1000 of the present invention; Fig.11 is a structural schematic diagram of step S1100 of the present invention; Fig.12 is a schematic diagram of the structure of step S1200 of the present invention; Fig.13 is a schematic diagram of the structure of step S1300 of the present invention; In the figure, 1 is SiC Sub layer, 2 is SiCDrift layer, 3 is N region, 4 is Pwell region, 5 is P region, 6 is NP region, 7 is PP region, 8 is gate oxide layer, 9 is Poly layer, 10 is isolation dielectric layer, 11 is ohmic contact alloy layer, and 12 is front electrode metal layer. DETAILED DESCRIPTION
[0020] The present invention is described in detail below in conjunction with specific practical cases. Examples of the embodiments are shown in the accompanying drawings, and the schematic implementation methods of the present invention and their descriptions are only used to explain the present invention and are not intended to limit the present invention.
[0021] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0022] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0023] A high saturation current SiC MOSFET comprises the following steps: S100, forming a SiC Drift layer 2 on the top surface of the SiC Sub layer 1 by epitaxial deposition; The thickness of SiC Sub layer 1 in step S100 is 100um-450um, and the doping concentration is 1E19cm -2 , SiC Drift layer 2 thickness is 5um-20um, doping concentration is 1E15-3E16cm -2 .
[0024] S200, forming N regions 3 arranged at intervals on the top surface of the SiC Drift layer 2 by N ion implantation; The bottom depth of N region 3 in step S200 is 0.2um-1.6um, and the doping concentration is 1E17-5E18cm -2 .
[0025] S300, forming a Pwell region 4 on the top surface of the SiC Drift layer 2 by Al ion implantation; The bottom depth of the Pwell region 4 in step S300 is 0.5um-2um, and the doping concentration is 1E17-3E18cm -2 .
[0026] S400, forming a P region 5 on the top surface of the SiC Drift layer 2 by epitaxial deposition; The thickness of the P region 5 in step S400 is 0.5um-2um, and the doping concentration is 1E17-3E18cm -2 .
[0027] S500, forming an NP region 6 on the top surface of the P region 5 by N ion implantation; The bottom depth of the NP region 6 in step S500 is 0.2um-1.4um, and the doping concentration is 5E17-1E19cm -2 .
[0028] S600, forming a PP region 7 on the top surface of the NP region 6 by Al ion implantation; In step S600, the bottom surface depth of the PP region 7 is 0.8um-4um, that is, it coincides with the bottom surface of the N region 3, and the doping concentration is 1E18-1E19cm -2 .
[0029] S700, activating and forming the implanted region by high temperature ion annealing; The high temperature ion annealing conditions in step S700 are a temperature of 1600° C.-1900° C. and a time of 3-5 min.
[0030] S800, forming a plurality of grooves arranged at intervals on the top surface of the NP region 6 by etching downward; In step S800 , the depth of the bottom of the trench from the bottom surface of the Pwell region 4 is 0.2 um-1 um, that is, the bottom surface of the trench is lower than the bottom surface of the Pwell region 4 .
[0031] S900, forming a gate oxide layer 8 in the trench by dry oxygen oxidation; The thickness of the gate oxide layer 8 in step S900 is 40 nm-100 nm.
[0032] S1000, forming a Poly layer 9 inside the trench by depositing polysilicon; S1100, forming an isolation dielectric layer 10 on the top surfaces of the NP region 6 and the Poly layer 9 by oxide deposition; S1200, forming an ohmic contact alloy layer 11 on the top surfaces of the NP region 6 and the PP region 7 by Ni metal sputtering or deposition followed by rapid thermal annealing; The Ni metal thickness in step S1200 is 0.3um-1um.
[0033] S1300, forming a front electrode metal layer 12 on the top of the device by sputtering Ti and AlCu metals; The thickness of the Ti metal in step S1300 is 0.1um-0.6um, and the thickness of the AlCu metal is 2um-5um.
[0034] A high saturation current SiC MOSFET comprises a SiC Sub layer 1, a SiC Drift layer 2, a P region 5, an NP region 6, an ohmic contact alloy layer 11 and a front electrode metal layer 12 arranged in sequence from bottom to top; The SiC Drift layer 2 is provided with: An N region 3, located in the middle of the SiC Drift layer 2, and extending downward from the top surface of the SiC Drift layer 2; A Pwell region 4 extends downward from the top surface of the SiC Drift layer 2 and is connected to the N region 3; a bottom surface of the Pwell region 4 is not higher than a bottom surface of the N region 3; A PP region 7 extends downward from the top surface of the NP region 6 to the N region 3; the bottom surface of the PP region 7 and the bottom surface of the N region 3 are in the same plane; The gate oxide layer 8 has a U-shaped cross section and extends downward from the top surface of the NP region 6 to the SiC Drift layer 2; A Poly layer 9, filled in the gate oxide layer 8, with its top surface flush with the top surface of the gate oxide layer 8; An isolation dielectric layer 10 covering the top surfaces of the gate oxide layer 8 and the Poly layer 9 is disposed on the top surface of the NP region 6 , and a side portion of the isolation dielectric layer 10 is connected to an ohmic contact alloy layer 11 .
[0035] The bottom of the front electrode metal layer 12 is connected to the ohmic contact alloy layer 11 and the isolation dielectric layer 10 respectively.
[0036] The PP region 7 is located in the N region 3 and is spaced apart from the side of the N region 3 .
[0037] A gap is provided between the side of the N region 3 and the gate oxide layer 8 .
[0038] The present invention is Figure 1 The channel region position of the trench gate SiC MOSFET device shown in the figure is designed by designing an N region 3 next to the channel region Pwell, so that when the device gate is turned on to form a channel, the adjacent N region 3 is affected by the external gate voltage, and the internal hole carriers will enter the Pwell region 4 of the channel region to accelerate the formation of the channel, and the channel width as the current path will also increase, thereby improving the current carrying capacity of the SiC MOSFET device, such as the saturation current.
Claims
1. A method for preparing a SiC MOSFET with high saturation current, characterized in that: The steps include: S100, forming a SiC Drift layer (2) on the top surface of the SiC Sub layer (1) by epitaxial deposition, and sequentially forming an N region (3) and a Pwell region (4) in the SiC Drift layer (2); S200, forming a P region (5) and an NP region (6) in sequence on the top surface of the Pwell region (4); S300, forming a PP region (7) on the top surface of the NP region (6) by Al ion implantation, and activating the implanted region by high temperature ion annealing; S400, forming spaced trenches on the top surface of the NP region (6) by etching downward; and sequentially forming a gate oxide layer (8) and a Poly layer (9) in the trenches; S500, forming an isolation dielectric layer (10) and an ohmic contact alloy layer (11) in sequence on the top surface of the NP region (6); S600, forming a front electrode metal layer (12) on the top surface of the device.
2. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: The thickness of the SiC Sub layer (1) in step S100 is 100um-450um, and the doping concentration is 1E19cm -2 .
3. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: In step S100, the thickness of the SiC Drift layer (2) is 5um-20um, and the doping concentration is 1E15-3E16cm -2 .
4. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: In step S100, the bottom depth of the Pwell region (4) is 0.5um-2um, and the doping concentration is 1E17-3E18cm -2 .
5. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: In step S200, the thickness of the P region (5) is 0.5um-2um, and the doping concentration is 1E17-3E18cm -2 .
6. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: In step S200, the bottom depth of the NP region (6) is 0.2um-1.4um, and the doping concentration is 5E17-1E19cm -2 .
7. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: In step S300, the bottom depth of the PP region (7) is 0.8um-4um, and the doping concentration is 1E18-1E19cm -2 .
8. The method for preparing a SiC MOSFET with high saturation current according to claim 1, characterized in that: In step S400, the thickness of the gate oxide layer (8) is 40nm-100nm.
9. A high saturation current SiC MOSFET, characterized in that: The method for preparing a high saturation current SiC MOSFET is prepared by any one of claims 1 to 8, comprising a SiC Sub layer (1), a SiC Drift layer (2), a P region (5), an NP region (6), an ohmic contact alloy layer (11) and a front electrode metal layer (12) arranged in sequence from bottom to top; The SiC Drift layer (2) is provided with: An N region (3) located in the middle of the SiC Drift layer (2) and extending downward from the top surface of the SiC Drift layer (2); A Pwell region (4) extending downward from the top surface of the SiC Drift layer (2) and connected to the N region (3); a bottom surface of the Pwell region (4) is not higher than a bottom surface of the N region (3); A PP region (7) extending downward from the top surface of the NP region (6) into the N region (3); a bottom surface of the PP region (7) and a bottom surface of the N region (3) are in the same plane; A gate oxide layer (8) having a U-shaped cross-section and extending downward from the top surface of the NP region (6) into the SiC Drift layer (2); A Poly layer (9) filled in the gate oxide layer (8), with a top surface flush with the top surface of the gate oxide layer (8); The top surface of the NP region (6) is provided with an isolation dielectric layer (10) covering the top surfaces of the gate oxide layer (8) and the Poly layer (9), and the side of the isolation dielectric layer (10) is connected to the ohmic contact alloy layer (11); The bottom of the front electrode metal layer (12) is respectively connected to the ohmic contact alloy layer (11) and the isolation dielectric layer (10).
10. The SiC MOSFET with high saturation current according to claim 9, characterized in that: The PP region (7) is located in the N region (3) and is spaced apart from the side of the N region (3).