Memory device and method of forming the same
By using a combination of a low dielectric layer and an air gap in the memory device, the problem of increasing parasitic capacitance in the memory device is solved, and the reliability and performance of the device are improved.
Patent Information
- Application Number
- CN202311249883.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-01
- Filing Date
- 2023-09-26
- Publication Date
- 2024-12-03
AI Technical Summary
As the characteristic critical size of the memory device decreases, the parasitic capacitance between the tight elements increases, resulting in a decline in component performance, and a method is needed to reduce the parasitic capacitance without damaging the element.
Using a combination of low-dial constant dielectric layer and air gap, the low-dial constant dielectric layer is located between the bit line and the unit contact, the air gap is located above the low-dial constant dielectric layer and is clamped through multi-layer spacer A memory device structure is formed between the bit line and the unit contact.
The parasitic capacitance between the bit line and the unit contact is effectively reduced, and the reliability and performance of the memory device are improved.
Smart Images

Figure CN119069419A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to memory devices and methods of forming the same, and more particularly to memory devices having air gaps. Background Art
[0002] As the critical dimension (CD) of features in memory devices becomes smaller, the size of the memory devices is also reduced accordingly, thereby increasing the density of components in the devices. However, the reduced distance between closely packed components may easily cause parasitic capacitance that affects the components. Therefore, forming a memory device requires a method of forming an air gap so that the air gap effectively reduces the parasitic capacitance without damaging the components. Summary of the invention
[0003] According to some embodiments of the present disclosure, a memory device includes a bit line on a substrate, a multilayer spacer covering the bit line, and a low-k dielectric layer sandwiched in the multilayer spacer, wherein the top surface of the low-k dielectric layer is lower than the top surface of the bit line. The memory device also includes an air gap sandwiched in the multilayer spacer, wherein the air gap is located above the low-k dielectric layer. The vertical projection of the air gap on the substrate partially overlaps with the vertical projection of the low-k dielectric layer on the substrate. The memory device also includes a cell contact adjacent to the multilayer spacer, wherein the multilayer spacer, the low-k dielectric layer and the air gap are arranged between the bit line and the cell contact.
[0004] In some embodiments, a top surface of the low-k dielectric layer is located between a top surface of the bit line and a top surface of a work function layer in the bit line.
[0005] In some embodiments, a ratio of the height of the low-k dielectric layer to the height of the bit line is equal to or greater than 0.5.
[0006] In some embodiments, the dielectric constant of the low-k dielectric layer is in the range of 2.7 to 3.1.
[0007] In some embodiments, the multi-layer spacer includes a first spacer layer covering the sidewalls and top surface of the bit line, a second spacer layer covering the low-k dielectric layer and the first spacer layer, and a third spacer layer covering the air gap and the second spacer layer.
[0008] In some embodiments, the second spacer layer separates the low-k dielectric layer and the air gap.
[0009] In some embodiments, a sidewall of the first spacer layer is parallel to a sidewall of the third spacer layer. The low-k dielectric layer, the second spacer layer, and the air gap are sandwiched between the sidewall of the first spacer layer and the sidewall of the third spacer layer.
[0010] In some embodiments, the thickness of the second spacer layer is less than the width of the low-k dielectric layer.
[0011] In some embodiments, the width of the air gap is equal to the width of the low-k dielectric layer.
[0012] In some embodiments, a top surface of the air gap is higher than a top surface of the bit line.
[0013] In some embodiments, the first spacer layer, the second spacer layer, and the third spacer layer include the same material.
[0014] In some embodiments, the second spacer layer directly contacts a top surface of the first spacer layer, and the third spacer layer directly contacts a top surface of the second spacer layer.
[0015] In some embodiments, the memory device further includes a contact pad located above the bit line and the multi-layer spacer, wherein the contact pad passes through the multi-layer spacer to be electrically connected to the bit line.
[0016] According to some embodiments of the present disclosure, a method for forming a memory device includes the following steps. A first spacer layer is formed, wherein the first spacer layer covers a bit line on a substrate. A low-k dielectric layer is formed on a sidewall of the first spacer layer, wherein a top surface of the low-k dielectric layer is lower than a top surface of the bit line. A second spacer layer is formed, wherein the second spacer layer covers the low-k dielectric layer and the first spacer layer. A sacrificial layer is formed on the sidewall of the second spacer layer, wherein the sacrificial layer is located above the low-k dielectric layer, and a vertical projection of the sacrificial layer falling on the substrate partially overlaps with a vertical projection of the low-k dielectric layer falling on the substrate. A third spacer layer is formed, wherein the third spacer layer covers the sacrificial layer and the second spacer layer. A cell contact is formed adjacent to the third spacer layer. The sacrificial layer is removed to form an air gap between the second spacer layer and the third spacer layer.
[0017] In some embodiments, the material of the low-k dielectric layer is different from the material of the sacrificial layer.
[0018] In some embodiments, forming the low-k dielectric layer includes forming a low-k dielectric material covering the first spacer layer, and etching the low-k dielectric material to form the low-k dielectric layer. The top surface of the low-k dielectric layer after etching is higher than the top surface of the work function layer in the bit line.
[0019] In some embodiments, forming the second spacer layer comprises conformally forming the second spacer layer on the low-k dielectric layer and the first spacer layer. The second spacer layer covers a non-coplanar outer surface portion of the low-k dielectric layer and a non-coplanar outer surface portion of the second spacer layer covers the first spacer layer.
[0020] In some embodiments, forming the sacrificial layer includes forming a sacrificial material covering the sidewalls of the second spacer layer, forming a mask layer on the top surface of the second spacer layer, and etching the sacrificial material using the mask layer to form the sacrificial layer. The width of the mask layer is greater than the width of the top surface of the second spacer layer. After etching the sacrificial material, the outer side surface of the second spacer layer is exposed.
[0021] In some embodiments, after forming the sacrificial layer, an outer side surface of the sacrificial layer is coplanar with an outer side surface of the second spacer layer.
[0022] In some embodiments, after forming the sacrificial layer, a top surface of the sacrificial layer is coplanar with a top surface of the second spacer layer.
[0023] According to the above-mentioned embodiments, the memory device provided by the present disclosure includes a multi-layer spacer between a bit line and a cell contact, wherein a low-k dielectric layer and an air gap are sandwiched in the multi-layer spacer. During the formation of the air gap, the low-k dielectric layer protects the bit line structure to increase device reliability. The low-k dielectric layer and the air gap reduce the parasitic capacitance between the bit line and the cell contact to improve device performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] When read in conjunction with the accompanying drawings, various aspects of the present disclosure can be best understood from the following detailed description. It should be noted that, in accordance with standard methods in the industry, various features are not drawn to scale. In fact, the size of various features may be arbitrarily increased or reduced for clarity of discussion.
[0025] Figure 1 A flow chart of a method for forming a memory device is shown according to some embodiments of the present disclosure.
[0026] FIG. 2A to FIG. 2O According to some embodiments of the present disclosure, cross-sectional views of a memory device at various intermediate stages of a formation process are depicted. DETAILED DESCRIPTION
[0027] In order to realize the different features of the mentioned subject matter, the following disclosure provides many different embodiments or examples. Specific examples of components, configurations, etc. are described below to simplify the present disclosure. Of course, these are merely examples and are not restrictive. For example, in the following description, forming a first feature on or above a second feature may include an embodiment in which the first feature and the second feature are formed in direct contact, and may also include an embodiment in which an additional feature is formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself represent the relationship between the various embodiments and / or configurations discussed.
[0028] Furthermore, spatially relative terms, such as "below," "beneath," "lower," "above," "upper," and the like, may be used herein to facilitate describing one element or feature's relationship to another element or feature as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein interpreted accordingly.
[0029] The present disclosure provides a memory device, which includes a bit line on a substrate, a multilayer spacer covering the bit line, a low-k dielectric layer and an air gap sandwiched in the multilayer spacer, and a cell contact adjacent to the multilayer spacer. The air gap is located above the low-k dielectric layer, and the vertical projection of the air gap on the substrate partially overlaps with the vertical projection of the low-k dielectric layer on the substrate. During the formation of the air gap, the low-k dielectric layer protects the bit line structure, thereby increasing the reliability of the memory device. In addition, the low-k dielectric layer and the air gap reduce the parasitic capacitance between the bit line and the cell contact, thereby improving the performance of the memory device.
[0030] According to some embodiments of the present disclosure, Figure 1 A flow chart of a method S10 of forming a memory device is shown. FIG. 2A to FIG. 2O The memory device is shown in Figure 1 sectional views of multiple intermediate stages of the forming method S10. Fig.2O The memory device 10 shown in FIG. 1 is used as an example to describe the forming method S10. However, it should be understood by those skilled in the art that Figure 1 and FIG. 2A to FIG. 2O The method shown in FIG. 1 can be used not only to form the memory device 10 , but also to form other memory devices with air gaps within the scope of the present disclosure.
[0031] refer to Figure 1 and Figure 2A The method S10 starts at step S102, where a plurality of bit lines 110 are provided on a substrate 100. The bit lines 110 include a work function layer 112 and a capping layer 114 on the work function layer 112. The work function layer 112 may include a suitable conductive material to provide a read / write function for the bit lines 110. The capping layer 114 separates the work function layer 112 from components subsequently formed on the bit lines 110 to protect the work function layer 112.
[0032] In some embodiments, the work function layer 112 may include a single layer or multiple layers of metal, metal nitride, metal silicide, metal compound, alloy, polysilicon, dielectric material, or a combination thereof. In some embodiments, the capping layer 114 may include a dielectric material, such as silicon oxide, silicon nitride, a combination thereof, or the like.
[0033] refer to Figure 1 and Figure 2B , the method S10 proceeds to step S104, forming a first spacer layer 120 on the bit line 110. Specifically, the first spacer layer 120 is conformally formed on the bit line 110 to cover the top surface and sidewalls of the bit line 110. In subsequent processes, the first spacer layer 120 protects the bit line 110. The first spacer layer 120 may also be formed on the top surface of the substrate 100, so that the first spacer layer 120 continuously covers the substrate 100 and the plurality of bit lines 110.
[0034] In some embodiments, the first spacer layer 120 may include a suitable dielectric material to protect the bit line 110. For example, the first spacer layer 120 may be formed of silicon nitride. In some embodiments, the first spacer layer 120 may be formed by a deposition process, such as chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or the like.
[0035] refer to Figure 1 and Figure 2C to Figure 2D The method S10 proceeds to step S106, where a low-k dielectric layer 135 is formed on the sidewalls of the first spacer layer 120. Specifically, the low-k dielectric material 130 is first formed on the first spacer layer 120. Figure 2C The low-k dielectric material 130 is filled between adjacent bit lines 110 until the low-k dielectric material 130 covers the top surface and sidewalls of the first spacer layer 120. The low-k dielectric material 130 has a dielectric constant lower than 3.9, so that the subsequently formed low-k dielectric layer 135 can reduce parasitic capacitance close to the bit line 110. For example, the dielectric constant of the low-k dielectric material can be in the range of 2.7 to 3.1.
[0036] In some embodiments, the low-k dielectric material 130 may include a dielectric material different from the first spacer layer 120. For example, when the first spacer layer 120 is formed of a nitride, the low-k dielectric material 130 may include an oxide or a carbon-doped oxide, such as SiOCH. In some embodiments, the low-k dielectric material 130 may be formed by a deposition process, such as chemical vapor deposition, plasma enhanced chemical vapor deposition, atomic layer deposition, or the like. The formed low-k dielectric material 130 may have a dielectric structure such as Figure 2CThe top surface of the substrate 100 may be a concave top surface as shown in , or may have a flat surface parallel to the top surface of the substrate 100 , but the present disclosure is not limited thereto.
[0037] Then, if Figure 2D As shown in , the low-k dielectric material 130 is etched to form a low-k dielectric layer 135. The low-k dielectric layer 135 extends along the sidewalls of the first spacer layer 120 in the z direction. The etching process is performed until the top surface of the low-k dielectric layer 135 is lower than the top surface of the bit line 110, but higher than the top surface of the work function layer 112 in the bit line 110. Since the top surface of the low-k dielectric layer 135 is between the top surface of the bit line 110 and the top surface of the work function layer 112, the low-k dielectric layer 135 can protect the work function layer 112 in subsequent processes. Therefore, even if an air gap (e.g., Figure 2N After the air gap 210 is formed in the fabricated memory device 10, the reliability of the fabricated memory device 10 can still be improved.
[0038] In some embodiments, the low-k dielectric layer 135 may have a sufficient height in the z-direction so that the top surface of the low-k dielectric layer 135 is higher than the top surface of the work function layer 112. For example, the ratio of the height of the low-k dielectric layer 135 to the height of the bit line 110 may be equal to or higher than 0.5. In some embodiments, the etching process for forming the low-k dielectric layer 135 may be anisotropic, such as a dry etching process using plasma. The low-k dielectric layer 135 after the etching process may have a thickness of 0.1-1.0mm / s. Figure 2D In other embodiments, the low-k dielectric layer 135 may have a flat top surface parallel to the top surface of the substrate 100 .
[0039] refer to Figure 1 and Figure 2E , the method S10 proceeds to step S108, forming a second spacer layer 140 on the low-k dielectric layer 135 and the first spacer layer 120. Specifically, the second spacer layer 140 is conformally formed so that the second spacer layer 140 continuously covers the low-k dielectric layer 135 and the first spacer layer 120. The second spacer layer 140 may directly contact the top surface and the sidewall of the first spacer layer 120, so that the low-k dielectric layer 135 is sandwiched between the second spacer layer 140 and the first spacer layer 120.
[0040] The thickness of the second spacer layer 140 is less than the width of the low-k dielectric layer 135 in the x-direction, so that the outer surface portion of the second spacer layer 140 covering the low-k dielectric layer 135 and the outer surface portion of the second spacer layer 140 covering the first spacer layer 120 are non-coplanar. In this way, space for forming an air gap above the low-k dielectric layer 135 in subsequent processes can be reserved. If the thickness of the second spacer layer 140 is greater than the width of the low-k dielectric layer 135, the space directly above the low-k dielectric layer 135 may be completely occupied by the second spacer layer 140, and it is difficult to reserve enough space for subsequent formation of the air gap. In addition, the thickness of the second spacer layer 140 above the low-k dielectric layer 135 can be uniform to cover and protect the low-k dielectric layer 135 in subsequent processes.
[0041] In some embodiments, the second spacer layer 140 may extend from above the bit line 110 toward the substrate 100 until the second spacer layer 140 contacts the first spacer layer 120 on the substrate 100. Figure 2E In some other embodiments, the second spacer layer 140 may further extend in the x-direction along the top surface of the substrate 100. In the embodiment where the low-k dielectric layer 135 has a rounded top angle, the conformally formed second spacer layer 140 may also exhibit a rounded top angle corresponding to the low-k dielectric layer 135.
[0042] In some embodiments, the second spacer layer 140 may include a dielectric material similar to the first spacer layer 120 to provide high adhesion between the second spacer layer 140 and the first spacer layer 120. For example, when the first spacer layer 120 is formed of a nitride, the second spacer layer 140 may be formed of the same nitride. In some embodiments, the second spacer layer 140 may be formed by a deposition process similar to the first spacer layer 120, such as atomic layer deposition or the like.
[0043] refer to Figure 1 and Figures 2F to 2H The method S10 proceeds to step S110 to form a sacrificial layer 155 on the sidewalls of the second spacer layer 140 and above the low-k dielectric layer 135. Specifically, the sacrificial material 150 is filled between adjacent bit lines 110 to cover the sidewalls of the second spacer layer 140, such as Figure 2F The sacrificial material 150 may be first formed over the top surface of the second spacer layer 140 and then planarized by, for example, chemical mechanical planarization (CMP) so that the top surface of the sacrificial material 150 is coplanar with the top surface of the second spacer layer 140 .
[0044] In some embodiments, the sacrificial material 150 may include a dielectric material different from the second spacer layer 140. For example, when the second spacer layer 140 is formed of nitride, the sacrificial material 150 may include an oxide. It should be noted that the material of the sacrificial material 150 may also be different from the material of the low-k dielectric layer 135 to provide a higher etching selectivity in subsequent processes. In some examples where the low-k dielectric layer 135 is formed of SiOCH, the sacrificial material 150 may be formed of SiOCH. x In some embodiments, the sacrificial material 150 may be formed by a deposition process such as chemical vapor deposition, plasma enhanced chemical vapor deposition, atomic layer deposition, or the like.
[0045] Then, if Figure 2G As shown in FIG. 1 , a mask layer 160 is formed on the top surfaces of the sacrificial material 150 and the second spacer layer 140. The mask layer 160 may include a photoresist material, so the mask layer 160 may be exposed and developed to cover the top surface of the second spacer layer 140 and expose a portion of the sacrificial material 150. It should be noted that the width of the mask layer 160 in the x-direction is greater than the top surface of the second spacer layer 140. Therefore, the mask layer 160 not only covers the top surface of the second spacer layer 140, but also defines the pattern of the sacrificial layer 155 to be formed.
[0046] Then, if Figure 2H As shown in , the sacrificial material 150 is etched using the mask layer 160 to form the sacrificial layer 155. The etching process stops at the second spacer layer 140 and the first spacer layer 120. In other words, when etching the sacrificial material 150, the second spacer layer 140 and the first spacer layer 120 protect the low-k dielectric layer 135. In some embodiments, the etching process for forming the sacrificial layer 155 can be anisotropic, such as a dry etching process. After forming the sacrificial layer 155, the mask layer 160 can be removed.
[0047] The etched sacrificial layer 155 is located above the low-k dielectric layer 135, and the top surface of the sacrificial layer 155 is coplanar with the top surface of the second spacer layer 140. Since the thickness of the second spacer layer 140 is less than the width of the low-k dielectric layer 135 in the x-direction, the vertical projection of the sacrificial layer 155 on the substrate 100 and the vertical projection of the low-k dielectric layer 135 on the substrate 100 may partially overlap.
[0048] In some embodiments, the sacrificial layer 155 may cover the upper portion of the second spacer layer 140 and expose the outer surface of the lower portion of the second spacer layer 140. For example, the outer surface of the sacrificial layer 155 may be coplanar with the outer surface of the second spacer layer 140, so that the outer surface portion of the second spacer layer 140 covering the low-k dielectric layer 135 is exposed. In embodiments where the outer surface of the sacrificial layer 155 is coplanar with the outer surface of the second spacer layer 140, the width of the sacrificial layer 155 in the x-direction may be equal to the width of the low-k dielectric layer 135 in the x-direction.
[0049] refer to Figure 1 and Fig.2I , the method S10 proceeds to step S112, forming a third spacer layer 170 on the sacrificial layer 155 and the second spacer layer 140. Specifically, the third spacer layer 170 is conformally formed so that the third spacer layer 170 continuously covers the sacrificial layer 155 and the second spacer layer 140. Since the top surface of the sacrificial layer 155 is coplanar with the top surface of the second spacer layer 140, the third spacer layer 170 can directly contact the top surface and sidewall of the second spacer layer 140, thereby sandwiching the sacrificial layer 155 between the third spacer layer 170 and the second spacer layer 140.
[0050] The first spacer layer 120, the second spacer layer 140, and the third spacer layer 170 may be referred to as a multi-layer spacer 175 covering the bit line 110. The low-k dielectric layer 135, the second spacer layer 140, and the sacrificial layer 155 are sandwiched between the first spacer layer 120 and the third spacer layer 170. In some embodiments, the first spacer layer 120, the second spacer layer 140, and the third spacer layer 170 may have the same thickness. In other embodiments, the thicknesses of the plurality of spacer layers of the multi-layer spacer 175 may be different from each other.
[0051] In some embodiments, the third spacer layer 170 may extend from above the bit line 110 toward the substrate 100 until the third spacer layer 170 contacts the first spacer layer 120 on the substrate 100. Fig.2I In some other embodiments, the third spacer layer 170 may further extend in the x-direction along the top surface of the substrate 100. In embodiments where the outer side surface of the sacrificial layer 155 is coplanar with the outer side surface of the second spacer layer 140, the third spacer layer 170 may have straight sidewalls parallel to the sidewalls of the first spacer layer 120.
[0052] In some embodiments, the third spacer layer 170 may include a dielectric material similar to the second spacer layer 140, thereby providing high adhesion between the third spacer layer 170 and the second spacer layer 140. For example, when the second spacer layer 140 is formed of SiN, the third spacer layer 170 may also be formed of SiN. Specifically, the first spacer layer 120, the second spacer layer 140, and the third spacer layer 170 may include the same material. In some embodiments, the third spacer layer 170 may be formed by a deposition process similar to the first spacer layer 120, such as atomic layer deposition or the like.
[0053] refer to Figure 1 and Figure 2J to Figure 2M The method S10 proceeds to step S114 to form a cell contact 200 adjacent to the third spacer layer 170. Specifically, the dielectric layer 180 is first formed on the third spacer layer 170. Figure 2J As shown in . The dielectric layer 180 is filled between the adjacent bit lines 110 until the dielectric layer 180 covers the top surface and sidewalls of the third spacer layer 170. For example, the dielectric layer 180 may include an oxide suitable for chemical vapor deposition or other similar deposition processes. Then, as Figure 2K As shown in FIG. 1 , a mask layer 190 is formed on the top surface of the dielectric layer 180. The mask layer 190 may include a photoresist material so that the mask layer 190 can be exposed and developed to expose a portion of the dielectric layer 180. The portion of the dielectric layer 180 exposed by the mask layer 190 defines a pattern for subsequently forming a cell contact 200.
[0054] like Figure 2L As shown in , the dielectric layer 180 is then etched using the mask layer 190 to form an opening 180p in the dielectric layer 180. The opening 180p extends toward the substrate 100 to expose the sidewalls of the third spacer layer 170. When etching the dielectric layer 180, the material layer sandwiched between the first spacer layer 120 and the third spacer layer 170 is protected, thereby avoiding affecting the structure of the low dielectric constant dielectric layer 135 and the sacrificial layer 155. In some embodiments, the opening 180p can extend into the substrate 100 so that the bottom surface of the opening 180p is lower than the top surface of the substrate 100. In some embodiments, the etching process for forming the opening 180p can be anisotropic, such as a dry etching process. After forming the opening 180p, the mask layer 190 can be removed.
[0055] Then, if Figure 2MAs shown in , a conductive material is filled in the opening 180p to form a cell contact 200. The cell contact 200 is adjacent to the third spacer layer 170, so that the third spacer layer 170 is sandwiched between the sacrificial layer 155 and the cell contact 200. After forming the cell contact 200, the dielectric layer 180 can be removed. In some embodiments, the cell contact 200 may include polysilicon, doped polysilicon, metal, metal silicide, other suitable conductive materials, or a combination of the above. In some embodiments, before forming the cell contact 200, a barrier layer (not shown) may be deposited in the opening 180p, wherein the barrier layer contacts the side surface, the bottom surface, or both of the cell contact 200.
[0056] refer to Figure 1 and Figure 2N , the method S10 proceeds to step S116, removing the sacrificial layer 155 to form an air gap 210 between the second spacer layer 140 and the third spacer layer 170. Specifically, the materials of the first spacer layer 120, the second spacer layer 140, and the third spacer layer 170 are different from the material of the sacrificial layer 155, so the sacrificial layer 155 can be selectively removed by performing an etching process. As a result, when etching the sacrificial layer 155, the low-k dielectric layer 135 between the first spacer layer 120 and the second spacer layer 140 is protected. Furthermore, in the embodiment where the material of the low-k dielectric layer 135 is different from the sacrificial layer 155, there can be a sufficiently high etching selectivity between the materials to selectively etch the sacrificial layer 155.
[0057] After the sacrificial layer 155 is removed, the air gap 210 is formed at the location of the sacrificial layer 155. In other words, the second spacer layer 140 separates the low-k dielectric layer 135 and the air gap 210, and the third spacer layer 170 separates the cell contact 200 and the air gap 210. Since the low-k dielectric layer 135 is not affected when the sacrificial layer 155 is etched, the low-k dielectric layer 135 can protect the first spacer layer 120 and the bit line 110 covered by the low-k dielectric layer 135. As a result, the structure of the bit line 110, especially the side surface of the lower portion of the bit line 110, can be maintained after the air gap 210 is formed.
[0058] The space of the air gap 210 is substantially similar to the structure of the sacrificial layer 155. For example, since the top surface of the sacrificial layer 155 is coplanar with the top surface of the second spacer layer 140, the top surface of the air gap 210 may be higher than the top surface of the bit line 110. In an embodiment where the width of the sacrificial layer 155 in the x-direction is equal to the width of the low-k dielectric layer 135 in the x-direction, the width of the air gap 210 in the x-direction may be equal to the width of the low-k dielectric layer 135.
[0059] According to the above, the memory device 10 is formed. The memory device 10 includes the bit line 110, the cell contact 200, and the multi-layer spacer 175 between the bit line 110 and the cell contact 200. The low-k dielectric layer 135 and the air gap 210 are sandwiched in the multi-layer spacer 175 to reduce the parasitic capacitance between the bit line 110 and the cell contact 200. The air gap 210 is located above the low-k dielectric layer 135, so that the low-k dielectric layer 135 protects the lower part of the bit line 110 during the formation of the air gap 210. The low-k dielectric layer 135 and the multi-layer spacer 175 reserve a space for forming the air gap 210, so that the vertical projection of the air gap 210 falling on the substrate 100 partially overlaps with the vertical projection of the low-k dielectric layer 135 falling on the substrate 100.
[0060] In some embodiments, method S10 may proceed to step S118 to further process memory device 10. For example, Fig.2O A cross-sectional view of the memory device 10 is shown after forming an interlayer dielectric 220 and a contact pad 230 over the bit line 110 and the multi-layer spacer 175. The contact pad 230 is electrically connected to the bit line 110 through the interlayer dielectric 220 and the multi-layer spacer 175 to form a vertical conductive path in the memory device 10. It should be noted that Figure 2N and Fig.2O The memory device 10 in FIG. 1 is simplified to clearly illustrate certain features, and memory devices including additional components are also within the scope of the present disclosure.
[0061] According to the above-described embodiments of the present disclosure, a memory device includes a multi-layer spacer between a bit line and a cell contact. A low-k dielectric layer and an air gap above the low-k dielectric layer are sandwiched in the multi-layer spacer. During the formation of the air gap, the low-k dielectric layer protects the bit line structure, thereby improving the reliability of the memory device. The low-k dielectric layer and the air gap exhibit a low dielectric constant, thereby reducing parasitic capacitance between the bit line and the cell contact.
[0062] The features of some embodiments are summarized above so that those skilled in the art can better understand the viewpoints of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to achieve the same purpose and / or achieve the same advantages as the embodiments described herein. Those skilled in the art should also understand that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and various changes, substitutions and modifications can be made without departing from the spirit and scope of the present disclosure.
[0063]
Explanation of symbols
[0064] 100:Substrate
[0065] 110: Bit line
[0066] 112: Work function layer
[0067] 114: Covering layer
[0068] 120: first spacer layer
[0069] 130: Low dielectric constant dielectric material
[0070] 135: Low dielectric constant dielectric layer
[0071] 140: Second spacer layer
[0072] 150: Sacrificial material
[0073] 155: Sacrificial layer
[0074] 160: Mask layer
[0075] 170: third spacer layer
[0076] 175:Multilayer spacer
[0077] 180: Dielectric layer
[0078] 180p: Open
[0079] 190: Mask layer
[0080] 200: Unit contact
[0081] 210: Air Gap
[0082] 220: Interlayer dielectric
[0083] 230: Contact pad
[0084] S10: Methods
[0085] S102, S104, S106, S108, S110, S112, S114, S116, S118: step x, z: direction.
Claims
1. A memory device, characterized in that: include: A bit line, located on a substrate; A multi-layer spacer covering the bit line; a low-k dielectric layer interposed in the multi-layer spacer, wherein a top surface of the low-k dielectric layer is lower than a top surface of the bit line; an air gap interposed in the multi-layer spacer, wherein the air gap is located above the low-k dielectric layer, and a vertical projection of the air gap on the substrate partially overlaps a vertical projection of the low-k dielectric layer on the substrate; as well as A cell contact is adjacent to the multi-layer spacer, wherein the multi-layer spacer, the low-k dielectric layer and the air gap are disposed between the bit line and the cell contact.
2. The memory device according to claim 1, wherein: The top surface of the low-k dielectric layer is located between the top surface of the bit line and a top surface of a work function layer in the bit line.
3. The memory device according to claim 1, wherein: A ratio of a height of the low-k dielectric layer to a height of the bit line is equal to or higher than 0.
5.
4. The memory device according to claim 1, wherein: The dielectric constant of the low-k dielectric layer is in the range of 2.7 to 3.
1.
5. The memory device according to claim 1, wherein: The multi-layer spacer comprises: a first spacer layer covering the sidewalls and the top surface of the bit line; a second spacer layer covering the low-k dielectric layer and the first spacer layer; and A third spacer layer covers the air gap and the second spacer layer.
6. The memory device according to claim 5, characterized in that The second spacer layer separates the low-k dielectric layer and the air gap.
7. The memory device according to claim 5, wherein: A sidewall of the first spacer layer is parallel to a sidewall of the third spacer layer, and the low-k dielectric layer, the second spacer layer, and the air gap are sandwiched between the sidewall of the first spacer layer and the sidewall of the third spacer layer.
8. The memory device according to claim 5, wherein: The thickness of the second spacer layer is smaller than the width of the low-k dielectric layer.
9. The memory device according to claim 5, wherein: The width of the air gap is equal to the width of the low-k dielectric layer.
10. The memory device according to claim 5, wherein: A top surface of the air gap is higher than the top surface of the bit line.
11. The memory device according to claim 5, wherein: The first spacer layer, the second spacer layer, and the third spacer layer include the same material.
12. The memory device according to claim 5, wherein: The second spacer layer directly contacts a top surface of the first spacer layer, and the third spacer layer directly contacts a top surface of the second spacer layer.
13. The memory device according to claim 1, wherein: Further including: The contact pad is located above the bit line and the multi-layer spacer, wherein the contact pad passes through the multi-layer spacer and is electrically connected to the bit line.
14. A method of forming a memory device, characterized in that: include: forming a first spacer layer, wherein the first spacer layer covers the bit lines on the substrate; forming a low-k dielectric layer on sidewalls of the first spacer layer, wherein a top surface of the low-k dielectric layer is lower than a top surface of the bit line; forming a second spacer layer, wherein the second spacer layer covers the low-k dielectric layer and the first spacer layer; forming a sacrificial layer on the sidewall of the second spacer layer, wherein the sacrificial layer is located above the low-k dielectric layer, and a vertical projection of the sacrificial layer on the substrate partially overlaps with a vertical projection of the low-k dielectric layer on the substrate; forming a third spacer layer, wherein the third spacer layer covers the sacrificial layer and the second spacer layer; forming a cell contact adjacent to the third spacer layer; as well as The sacrificial layer is removed to form an air gap between the second spacer layer and the third spacer layer.
15. The method according to claim 14, characterized in that The material of the low-k dielectric layer is different from the material of the sacrificial layer.
16. The method according to claim 14, characterized in that Forming the low-k dielectric layer includes: forming a low-k dielectric material covering the first spacer layer; and The low-k dielectric material is etched to form the low-k dielectric layer, wherein the top surface of the low-k dielectric layer after etching is higher than the top surface of the work function layer in the bit line.
17. The method according to claim 14, characterized in that Forming the second spacer layer includes conformally forming the second spacer layer on the low-k dielectric layer and the first spacer layer, and the outer surface portion of the second spacer layer covering the low-k dielectric layer is non-coplanar with the outer surface portion of the second spacer layer covering the first spacer layer.
18. The method according to claim 14, characterized in that Forming the sacrificial layer includes: forming a sacrificial material covering the sidewall of the second spacer layer; forming a mask layer on the top surface of the second spacer layer, wherein a width of the mask layer is greater than a width of the top surface of the second spacer layer; and The sacrificial material is etched using the mask layer to form the sacrificial layer, wherein after etching the sacrificial material, an outer surface of the second spacer layer is exposed.
19. The method according to claim 14, characterized in that After forming the sacrificial layer, an outer side surface of the sacrificial layer is coplanar with an outer side surface of the second spacer layer.
20. The method according to claim 14, characterized in that After forming the sacrificial layer, a top surface of the sacrificial layer is coplanar with a top surface of the second spacer layer.