Quantum bit circuit and quantum bit chip
By replacing multiple parallel superconducting tunnel junctions in qubit circuits, the problems of low production yield and large space occupation are solved, and more efficient qubit circuit design is achieved, which improves the accuracy of quantum computing and reliability.
Patent Information
- Application Number
- CN202411194727.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-03
AI Technical Summary
The processing and preparation yield of superconducting tunnel junctions in existing quantum bit circuits is low and takes up a large space, resulting in low yield of qubits and difficult to increase the number of bits.
Superconducting nanowires are used to replace multiple parallel superconducting tunnel junctions as parallel inductors of fluxonium qubits. The resonant frequency is adjusted through the superinductor and capacitance components of the superconducting nanowires, reducing space occupation and improving preparation yield.
The preparation yield of the qubit circuit is improved, the proportional space of the qubit is reduced, and the coherence time and calculation accuracy of fluxonium qubits are improved.
Smart Images

Figure CN119072218A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the field of quantum computing technology, and more specifically, to a quantum bit circuit and a quantum bit chip. Background Art
[0002] Unlike the transmon qubit, whose charge energy is greater than the inductance energy, the charge energy of the fluxonium qubit is much greater than the charge energy (50 times). Therefore, the structure of the fluxonium qubit requires a large inductance device to be connected in parallel. The current mainstream device requires hundreds of small superconducting tunnel junctions to be connected in parallel on a superconducting tunnel junction. The processing and preparation process of superconducting tunnel junctions is relatively complicated, and the yield is not high, which is also a difficulty in the current preparation of superconducting quantum chips. The current mainstream architecture of quantum bits requires more than 100 superconducting tunnel junctions to be connected in parallel to provide inductance, which results in an extremely low processing yield of quantum bits. Moreover, these superconducting tunnel junction arrays occupy a large space, making it difficult to increase the number of bits on the chip. Summary of the invention
[0003] The embodiments of the present application provide a quantum bit circuit and a quantum bit chip to at least solve the problems of low quantum bit yield and large quantum bit space occupation in the quantum bit circuit in the related art.
[0004] According to one embodiment of the present application, a quantum bit circuit is provided, comprising: a superconducting tunnel junction; a superconducting nanowire electrically connected to the superconducting tunnel junction, the superconducting nanowire providing inductance for the superconducting tunnel junction; a capacitor component electrically connected to the superconducting tunnel junction and the superconducting nanowire, and used to adjust the resonant frequency of the quantum bit circuit, the capacitance of the capacitor component having a preset relationship with the resonant frequency.
[0005] In an exemplary embodiment, the types of shapes of the superconducting nanowire include flat spirals and zigzag lines.
[0006] In an exemplary embodiment, the superconducting tunnel junction includes: a Josephson junction.
[0007] In an exemplary embodiment, the inductance of the superconducting nanowire is expressed as: Among them, n s is the density of Cooper pairs of the superconducting nanowire, e is the charge value, m e is the effective mass of the charge carrier, l is the length of the superconducting nanowire, and A is the cross-section of the superconducting nanowire; the complex conductivity of the quantum bit circuit is expressed as: Where n is the load density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of the electron in the material), τ describes the average time interval between two collisions of the carriers, and ω is the frequency of the changing electric field; the real conductivity of the qubit circuit is expressed as: σ0 = ne 2 τ / m, where n is the charge density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of an electron in the material), and τ describes the average time interval between two collisions of the carriers.
[0008] In an exemplary embodiment, the circuit further includes a flux bias line, the superconducting nanowire has an output end and an input end, and a portion of the flux bias line extends in a direction from the output end to the input end to provide magnetic flux for the superconducting nanowire.
[0009] In an exemplary embodiment, the length of the superconducting nanowire per unit area comprises 8 mm to 12 mm, and the unit of the unit area comprises mm2.
[0010] In an exemplary embodiment, the width of the superconducting nanowire in a first direction is comprised between 40 nm and 50 nm, and the first direction is perpendicular to the extension direction of the length of the superconducting nanowire.
[0011] In an exemplary embodiment, in a second direction, the thickness of the superconducting nanowire is 80 nm to 120 nm, and the second direction is perpendicular to the first direction and the extension direction of the length of the superconducting nanowire, respectively, and the first direction is perpendicular to the extension direction of the length of the superconducting nanowire.
[0012] According to another embodiment of the present application, a quantum bit chip is provided, including: the quantum bit circuit described above.
[0013] In an exemplary embodiment, the quantum bit chip further includes: a reading cavity; a microwave transmission line; a cross capacitor having a plurality of connection ends, the connection ends being electrically connected to the quantum bit circuit, the reading cavity and the microwave transmission line, respectively; a bias magnetic flux line located on a side of the quantum bit circuit away from the cross capacitor, the superconducting nanowire of the quantum bit circuit having an output end and an input end, and part of the bias magnetic flux line extending in a direction from the output end to the input end.
[0014] Through this application, since this application uses superconducting nanowires to replace the superconducting tunnel junction array with multiple parallel superconducting tunnel junctions in the quantum bit circuit as the parallel inductor of the fluxonium quantum bit, the low yield of preparing the superconducting tunnel junction is avoided, and the problem of low yield of preparing the quantum bit is caused. The super-inductor of the superconducting nanowire can also reduce the charge noise in the quantum bit circuit and improve the coherence time of the fluxonium quantum bit. The shape and arrangement of the superconducting nanowires have greater flexibility, which can reduce the occupied space of the fluxonium quantum bit. Therefore, the problem of low yield of the quantum bit of the quantum bit circuit and large space occupation of the quantum bit in the related art can be solved, and the yield of the quantum bit circuit is improved, and the occupied space of the quantum bit is reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 is a schematic diagram of the structure of a quantum bit circuit according to an embodiment of the present application;
[0016] Figure 2 is a schematic diagram of the structure of another quantum bit circuit according to an embodiment of the present application;
[0017] Figure 3 is a schematic diagram of a partial structure of a quantum bit chip according to an embodiment of the present application;
[0018] Figure 4 is a schematic diagram of a partial structure of another quantum bit chip according to an embodiment of the present application;
[0019] Figure 5 It is a schematic diagram of a process for preparing a quantum bit circuit on a quantum bit chip according to an embodiment of the present application.
[0020] Among them, the above reference numerals include:
[0021] 10. Superconducting nanowire; 20. Superconducting tunnel junction; 30. Capacitor component; 40. Magnetic flux bias line; 50. Quantum bit chip; 60. Quantum bit circuit; 70. Reading cavity; 80. Microwave transmission line; 90. Cross capacitor; 100. Superconducting nanowire pattern; 110. Substrate; 120. Electron beam exposure glue; 130. Aluminum film connection circuit. DETAILED DESCRIPTION
[0022] The embodiments of the present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0023] It should be noted that the terms "first", "second", etc. in the specification and claims of this application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence.
[0024] In this embodiment, a quantum bit circuit is provided. Figure 1 is a schematic diagram of the structure of a quantum bit circuit according to an embodiment of the present application, such as Figure 1 As shown, the circuit includes: a superconducting tunnel junction 20; a superconducting nanowire 10, which is electrically connected to the superconducting tunnel junction 20, and the superconducting nanowire 10 provides inductance for the superconducting tunnel junction 20; a capacitor component 30, which is electrically connected to the superconducting tunnel junction 20 and the superconducting nanowire 10, and is used to adjust the resonant frequency of the quantum bit circuit, and the capacitance of the capacitor component 30 has a preset relationship with the resonant frequency.
[0025] Through the above-mentioned quantum bit circuit, superconducting nanowires are used to replace the superconducting tunnel junction array with multiple parallel superconducting tunnel junctions in the quantum bit circuit as the parallel inductor of the fluxonium quantum bit, avoiding the low preparation yield of the superconducting tunnel junction, and thus the problem of low preparation yield of the quantum bit. The super-inductor of the superconducting nanowire can also improve the charge noise in the quantum bit circuit and increase the coherence time of the fluxonium quantum bit. The shape and arrangement of the superconducting nanowires have great flexibility, which can reduce the occupied space of the fluxonium quantum bit. The problem of low yield of the quantum bit circuit and large space occupied by the quantum bit is solved, so as to improve the yield of the quantum bit circuit and reduce the occupied space of the quantum bit.
[0026] In the above embodiment, Figure 1 As shown, the capacitor component 30 can adjust the frequency of the qubit to ensure that the qubit can operate at a specific frequency, which is crucial to achieving high-precision quantum operations. In addition, the capacitor component 30 can also affect the coupling strength between the qubit and other components, for example, affecting the coupling between the qubit and the resonant cavity, which is of great significance for reading the state of the qubit and realizing the interaction between the qubits. The design of the qubit circuit involves the fine adjustment of multiple parameters, including the critical current of the superconducting tunnel junction 20, the value of the capacitor component 30, etc. The reasonable design of these parameters can optimize the performance of the qubit and improve the accuracy and reliability of quantum computing. For example, by adjusting the size of the capacitor component 30, the energy level spacing of the qubit can be changed, thereby affecting its response to an external drive, which is crucial to realizing the initialization, manipulation, and reading of the qubit.
[0027] In one alternative, Figure 1 and Figure 2 As shown, the shapes of the superconducting nanowire 10 include a flat spiral and a zigzag line.
[0028] In the above embodiment, the shape of the superconducting nanowire 10 can be Figure 1The broken line type in Figure 2 As shown, the shape of the superconducting nanowire 10 can be Figure 2 The flat spiral line type in the circuit. The zigzag line or flat spiral line type design can increase the length of the superconducting nanowire 10 per unit area, and can improve the value of the kinetic inductance of the superconducting nanowire 10, thereby meeting the parallel inductance required by the fluxonium quantum bit when the quantum bit circuit occupies a reasonable chip space size. Figure 2 The superconducting tunnel junction 20 and the capacitor component 30 in Figure 1 The description is consistent with .
[0029] Compared with the traditional fluxonium quantum bit circuit processing, which requires the preparation of hundreds of superconducting tunnel junctions 20, the micro-nano processing technology has a higher yield in preparing superconducting nanowires 10 with a width of tens of nanometers. Superconducting nanowires 10 with a width of tens of nanometers can be prepared by a stripping process, and their stability and yield far exceed the current preparation process of superconducting tunnel junctions 20.
[0030] In an optional solution, the superconducting tunnel junction includes: a Josephson junction.
[0031] In the above embodiment, the Josephson junction is composed of two superconductors and a barrier layer, and the barrier layer is located between the superconductors.
[0032] In an optional solution, the inductance of the superconducting nanowire is expressed as: Among them, n s is the density of Cooper pairs in the superconducting nanowire, e is the charge value, m e is the effective mass of the charge carrier, l is the length of the superconducting nanowire, and A is the cross-section of the superconducting nanowire. The complex conductivity of the above quantum bit circuit is expressed as: Where n is the load density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of the electron in the material), T describes the average time interval between two collisions of the carriers, and ω is the frequency of the changing electric field; the real conductivity of the above quantum bit circuit is expressed as: σ0 = ne 2 τ / m, where n is the charge density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of an electron in the material), and τ describes the average time interval between two collisions of the carriers.
[0033] In the above embodiment, the motional inductance describes the equivalent inductance of moving charges in a changing electric field, which is equivalent to connecting an inductor in series in the circuit. The conductivity coefficient of the circuit becomes a complex number, and within a finite relaxation time τ (collision time), the complex conductivity of the circuit can be written as:
[0034]
[0035] Here n is the charge density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of the electron in the material), τ describes the average time interval between two collisions of the carriers, and ω is the frequency of the changing electric field. In normal metals, the relaxation time of the carriers is τ≈10 -14 Therefore, for low-frequency electric field ωτ<<1, the imaginary part of conductivity σ can be ignored, and the conductivity becomes a real number, that is, DC (direct current) conductivity σ0=ne 2 τ / m. For light fields with higher frequencies (such as the frequency of visible light 4.2×10 14 ~7.8×10 14 Hz) and materials with longer relaxation times (such as superconducting materials τ→∞), the value of ωτ is relatively large at this time, so the imaginary part of the inductance σ (i.e., the kinetic inductance) makes a greater contribution to the circuit conductivity.
[0036] For superconducting nanowires, the formula for their kinetic inductance can be written as:
[0037]
[0038] Among them, n s is the density of superconducting Cooper pairs, e is the charge value, m e is the effective mass of the charge carriers, l is the length of the superconducting nanowire, and A is the cross-section of the superconducting nanowire.
[0039] In one alternative, Figure 1 As shown, the circuit further includes a magnetic flux bias line 40 . The superconducting nanowire 10 has an output end and an input end. Part of the magnetic flux bias line 40 extends in a direction from the output end to the input end to provide magnetic flux for the superconducting nanowire 10 .
[0040] In the above embodiment, Figure 1 As shown, the flux bias line 40 passes direct current VCC, and the flux bias line 40 can generate a constant magnetic field in the circuit to keep the magnetic flux density at a constant level, thereby improving the performance and stability of the circuit. By applying magnetic flux to the fluxonium quantum bit circuit through the flux bias line 40, the total inductance of the quantum bit circuit and the transition frequency of the fluxonium quantum bit can be changed. The flux bias line 40 is usually made of a special material, such as a magnetic material or ferrite. These materials have good magnetic permeability and can effectively guide and adjust the magnetic flux density, thereby improving the working efficiency and stability of the circuit. By reasonably designing and selecting the material of the flux bias line, the circuit can maintain stable performance under different working conditions, thereby improving the reliability and durability of the circuit.
[0041] In an optional solution, the length of the superconducting nanowire per unit area includes 8 mm to 12 mm, and the unit of the unit area includes mm. 2 .
[0042] In the above embodiment, the length of the superconducting nanowire per unit area is set within the above range, which can achieve the microhenry-level parallel inductance required by the current fluxonium quantum bit circuit. The super inductance of the superconducting nanowire can also suppress the charge noise in the superconducting circuit and increase the coherence time of the fluxonium quantum bit. In addition, the shape and arrangement of the superconducting nanowire have great flexibility, which can reduce the space occupied by the fluxonium quantum bit and form more bits within the preset area. The above unit area is not limited to mm 2 , technical personnel in this field can reasonably select the unit of the above-mentioned unit area according to actual conditions, and this application does not make any specific limitation.
[0043] In an optional solution, the width of the superconducting nanowire in a first direction is 40 nm to 50 nm, and the first direction is perpendicular to the extension direction of the length of the superconducting nanowire.
[0044] In the above embodiment, the width of the superconducting nanowire in a direction perpendicular to the extension direction of the superconducting nanowire can be set to the above range. Those skilled in the art can reasonably select the width of the superconducting nanowire according to actual conditions, and this application does not make any specific limitation.
[0045] In an optional solution, in the second direction, the thickness of the superconducting nanowire is 80nm to 120nm, the second direction is perpendicular to the first direction and the extension direction of the length of the superconducting nanowire, and the first direction is perpendicular to the extension direction of the length of the superconducting nanowire.
[0046] In the above embodiment, in a direction perpendicular to both the extension direction of the superconducting nanowire and the width direction of the superconducting nanowire, the thickness of the superconducting nanowire can be set to the above range. Those skilled in the art can reasonably select the thickness of the superconducting nanowire according to actual conditions, and this application does not make any specific limitation.
[0047] According to another embodiment of the present application, a quantum bit chip is provided. Figure 3 is a schematic diagram of the structure of a quantum bit chip according to an embodiment of the present application, such as Figure 3 As shown, the quantum bit chip 50 includes: the quantum bit circuit 60 mentioned above.
[0048] Since the qubit circuit in the qubit chip of the present application uses superconducting nanowires to replace the superconducting tunnel junction array with multiple parallel superconducting tunnel junctions in the qubit circuit as the parallel inductor of the fluxonium qubit, the problem of low preparation yield of the superconducting tunnel junction and low preparation yield of the qubit is avoided. The super inductor of the superconducting nanowire can also reduce the charge noise in the qubit circuit and improve the coherence time of the fluxonium qubit. The shape and arrangement of the superconducting nanowires are highly flexible, which can reduce the space occupied by the fluxonium qubit. The yield of the qubit chip is improved, and more qubit circuits can be set in a certain area.
[0049] In one alternative, Figure 4 As shown, the quantum bit chip 50 further includes: a reading cavity 70; a microwave transmission line 80; a cross capacitor 90 having a plurality of connection ends, the connection ends being electrically connected to the quantum bit circuit 60, the reading cavity 70 and the microwave transmission line 80 respectively; a magnetic flux bias line 40, located on the side of the quantum bit circuit 60 away from the cross capacitor 90, the superconducting nanowire of the quantum bit circuit 60 having an output end and an input end, and part of the magnetic flux bias line 40 extends in a direction from the output end to the input end.
[0050] In the above embodiment, Figure 4 As shown, microwave transmission line 80 is used to transmit microwave signals to quantum bits and read information from quantum bits. Microwave transmission line 80 can realize control and measurement of quantum bit state by coupling with quantum bits. Cross capacitor 90 can realize coupling between quantum bits. By adjusting the parameters of cross capacitor 90, the interaction between different quantum bits can be controlled, thereby realizing coupling and logic gate operation of quantum bits. Reading cavity 70 can be used to detect the state of quantum bits. When the microwave signal is coupled with the reading cavity, the information of the quantum bit can be read by reading the response of the cavity, realizing the reading and measurement of the quantum bit. The above-mentioned quantum bit chip can also include an adjustable coupler (not shown in the figure), which can improve the efficiency of quantum computing by adjusting the strength of the coupler, thereby speeding up the speed of quantum bit gate operation, and the adjustable coupler can also realize multi-bit gate operation, which is essential for building complex quantum algorithms and simulating complex systems. When quantum gate operation is not required, crosstalk between different quantum bits can be avoided by closing the coupler to ensure the accuracy and stability of quantum computing.
[0051] like Figure 5As shown, the preparation method of preparing a quantum bit circuit on the above-mentioned quantum bit chip includes: first preparing a superconducting nanowire 10, step 1: coating a layer of electron beam exposure glue 120 on the substrate 110; step 2: displaying a superconducting nanowire pattern 100 on the photoresist by electron beam exposure and development; step 3: preparing a superconducting thin film (such as NbN) by electron beam evaporation or sputtering process, and preparing the superconducting nanowire 10 by a stripping process; step 4: then ultraviolet lithography of large-scale aluminum circuits and devices on the prepared chip, including transmission lines, reading cavities, cross capacitors, and Josephson junction area aluminum film connection circuits 130 and flux bias lines 40; step 5: preparing an aluminum / aluminum oxide / molybdenum type tunneling Josephson junction (superconducting tunnel junction 20) by electron beam exposure, completing the preparation of the quantum bit circuit, thereby completing the preparation of the fluxonium quantum bit chip. By applying magnetic flux to the superconducting loop of the fluxonium qubit through biasing magnetic flux lines, its total inductance and the transition frequency of the fluxonium qubit can be changed. Figure 5 The superconducting tunnel junction 20 is only a schematic diagram of its position.
[0052] The above-mentioned quantum bit circuit and quantum bit chip in this application will be specifically described below in conjunction with embodiments.
[0053] Example 1
[0054] The quantum bit circuit includes a superconducting tunnel junction, a superconducting nanowire, a capacitor component and a magnetic flux bias line, wherein the superconducting nanowire is electrically connected to the superconducting tunnel junction, and the superconducting nanowire provides inductance for the superconducting tunnel junction; the capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The superconducting tunnel junction is a Josephson junction; the superconducting nanowire is in the shape of a flat spiral line, with a length of 8nm, a width of 40nm and a thickness of 80nm per unit area.
[0055] Example 2
[0056] The quantum bit circuit includes a superconducting tunnel junction, a superconducting nanowire, a capacitor component and a magnetic flux bias line, wherein the superconducting nanowire is electrically connected to the superconducting tunnel junction, and the superconducting nanowire provides inductance for the superconducting tunnel junction; the capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The superconducting tunnel junction is a Josephson junction; the superconducting nanowire is in the shape of a flat spiral line, with a length of 10nm, a width of 45nm and a thickness of 100nm per unit area.
[0057] Example 3
[0058] The quantum bit circuit includes a superconducting tunnel junction, a superconducting nanowire, a capacitor component and a magnetic flux bias line, wherein the superconducting nanowire is electrically connected to the superconducting tunnel junction, and the superconducting nanowire provides inductance for the superconducting tunnel junction; the capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The superconducting tunnel junction is a Josephson junction; the superconducting nanowire is in the shape of a flat spiral line, with a length of 12nm, a width of 50nm and a thickness of 120nm per unit area.
[0059] Example 4
[0060] The quantum bit circuit includes a superconducting tunnel junction, a superconducting nanowire, a capacitor component and a magnetic flux bias line, wherein the superconducting nanowire is electrically connected to the superconducting tunnel junction, and the superconducting nanowire provides inductance for the superconducting tunnel junction; the capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The superconducting tunnel junction is a Josephson junction; the superconducting nanowire is in the shape of a zigzag line, with a length of 8nm, a width of 40nm, and a thickness of 80nm per unit area.
[0061] Example 5
[0062] The quantum bit circuit includes a superconducting tunnel junction, a superconducting nanowire, a capacitor component and a magnetic flux bias line, wherein the superconducting nanowire is electrically connected to the superconducting tunnel junction, and the superconducting nanowire provides inductance for the superconducting tunnel junction; the capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The superconducting tunnel junction is a Josephson junction; the superconducting nanowire is in the shape of a zigzag line, with a length of 10nm, a width of 45nm, and a thickness of 100nm per unit area.
[0063] Example 6
[0064] The quantum bit circuit includes a superconducting tunnel junction, a superconducting nanowire, a capacitor component and a magnetic flux bias line, wherein the superconducting nanowire is electrically connected to the superconducting tunnel junction, and the superconducting nanowire provides inductance for the superconducting tunnel junction; the capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The superconducting tunnel junction is a Josephson junction; the superconducting nanowire is in the shape of a zigzag line, with a length of 12nm, a width of 50nm, and a thickness of 120nm per unit area.
[0065] The above is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the principles of the present application shall be included in the protection scope of the present application.
Claims
1. A quantum bit circuit, characterized in that: include: Superconducting tunnel junction; a superconducting nanowire, electrically connected to the superconducting tunnel junction, the superconducting nanowire providing inductance for the superconducting tunnel junction; A capacitor component is electrically connected to the superconducting tunnel junction and the superconducting nanowire, and is used to adjust the resonant frequency of the quantum bit circuit. The capacitance of the capacitor component has a preset relationship with the resonant frequency.
2. The quantum bit circuit according to claim 1, characterized in that: The shapes of the superconducting nanowires include flat spirals and zigzag lines.
3. The quantum bit circuit according to claim 1, characterized in that: The superconducting tunnel junction includes: a Josephson junction.
4. The quantum bit circuit according to claim 3, characterized in that: The inductance of the superconducting nanowire is expressed as: Among them, n s is the density of Cooper pairs of the superconducting nanowire, e is the charge value, m e is the effective mass of the charge carriers, l is the length of the superconducting nanowire, and A is the cross-section of the superconducting nanowire; The complex conductivity of the qubit circuit is expressed as: Where n is the charge density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of the electron in the material), τ describes the average time interval between two collisions of the carriers, and ω is the frequency of the changing electric field; The real conductivity of the qubit circuit is expressed as: σ0=ne 2 t / m, Here, n is the charge density in the circuit, e is the elementary charge, m is the carrier mass (the effective mass of an electron in the material), and T describes the average time interval between two collisions of the carriers.
5. The quantum bit circuit according to claim 1, characterized in that: The circuit further includes a magnetic flux bias line, the superconducting nanowire has an output end and an input end, and a portion of the magnetic flux bias line extends in a direction from the output end to the input end, for providing magnetic flux to the superconducting nanowire.
6. The quantum bit circuit according to claim 1, characterized in that: The length of the superconducting nanowire per unit area is 8 mm to 12 mm, and the unit of the unit area is mm. 2 .
7. The quantum bit circuit according to claim 1, characterized in that: The width of the superconducting nanowire in a first direction is 40 nm to 50 nm, and the first direction is perpendicular to an extension direction of the length of the superconducting nanowire.
8. The quantum bit circuit according to claim 1, characterized in that: In the second direction, the thickness of the superconducting nanowire is 80 nm to 120 nm. The second direction is perpendicular to the first direction and the extension direction of the length of the superconducting nanowire. The first direction is perpendicular to the extension direction of the length of the superconducting nanowire.
9. A quantum bit chip, characterized in that: include: The quantum bit circuit according to any one of claims 1 to 8.
10. The quantum bit chip according to claim 9, characterized in that: Also includes: Read cavity; Microwave transmission lines; A cross capacitor having a plurality of connection ends, wherein the connection ends are electrically connected to the quantum bit circuit, the reading cavity and the microwave transmission line respectively; The bias magnetic flux line is located on a side of the quantum bit circuit away from the cross capacitor. The superconducting nanowire of the quantum bit circuit has an output end and an input end. Part of the bias magnetic flux line extends in a direction from the output end to the input end.