Bainite weld and component
By performing special thermal management and surfacing technology on steels with ferrite and bainite structures, the complexity and cost of the thermal conduction process after welding are solved, and efficient repair and performance maintenance on the gas turbine rotor are achieved.
Patent Information
- Application Number
- CN202380033775.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-13
- Filing Date
- 2023-03-30
- Publication Date
- 2024-12-03
AI Technical Summary
The prior art is difficult to simplify and shorten the heat conduction process after welding, resulting in high cost and long-term thermal after-treatment, especially in the case of large gas turbine rotors, affecting the performance and service life of mechanical materials.
By special thermal management of steels with ferrite and bainite structures, including maintaining high temperatures after welding to form bainite structures, reducing the time and cost of traditional heat treatment, while using reasonable materials such as CrMoV steel and MnNiCrMo steel is surfacing.
It achieves the formation of a bainite structure within a reasonable time, extends the service life of the gas turbine rotor, reduces the repair cost and time, and maintains good mechanical properties.
Smart Images

Figure CN119072548A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for welding steel having a bainite structure and to a component. Background Art
[0002] The traditional method used to increase the hardness or strength of steel is quenching and tempering.
[0003] The second and more rare method is bainitization, which was previously known as isothermal tempering (Zwischenstufenvergüten).
[0004] During this heat treatment, the component is austenitized in the same way as in the quenching process, i.e., heat treated at a temperature of 1073K-1323K, depending on the material. The quenching is then carried out in a warm salt bath. The temperature of the warm salt bath depends on the material and is between 533K and 663K. The component remains in the isothermal (isothermal) salt bath until the structural transformation from austenite to bainite (= intermediate phase) is complete. No martensite is formed in this process!
[0005] Depending on the material, the transformation can be completed in a matter of minutes, but sometimes it takes hours.
[0006] The component is then cooled in air.
[0007] The advantage of this method is that it has optimal toughness while maintaining high hardness.
[0008] The bainitic structure has very special properties, such as high impact strength (even at lower temperatures), improved fatigue strength, greater elongation, less quenching deformation, increased section reduction, and better bending properties. Summary of the invention
[0009] It is therefore an object of the present invention to simplify and shorten the heat transfer after welding while maintaining good mechanical properties.
[0010] This object is achieved by a method according to claim 1 and a component according to claim 6 .
[0011] The transfer of bainitization to welding is the subject of the present invention, the purpose of which is to simplify and shorten the heat transfer after welding while maintaining good mechanical properties.
[0012] The dependent claims list further advantageous measures, which can be combined with one another in any way to achieve further advantages.
[0013] The figure shows three curves: the temperature curve for bainitization, the temperature curve for conventional thermal post-treatment (tempering at T>673 K), and the temperature curve according to the invention.
[0014] With the help of the present invention, three different problems can be solved:
[0015] a) For large rotors of turbines, such as gas turbines with an output of at least 200 MW in particular, thermal post-treatment (tempering or stress relief annealing) at 873 K is not possible, since structural conditions (e.g. different thermal expansion of materials and components) may deform or damage the rotor. Furthermore, conventional methods are opposed for safety reasons.
[0016] b) For rotors that can be post-heat treated, e.g. for welds in the bearing area of the rotor, post-heat treatment is usually very complex, time-consuming and expensive, but remains the industry standard because the internal stresses and material properties in the heat-affected zone cannot be achieved otherwise.
[0017] c) The target heat treatment quality of conventional methods (tempering or stress relief annealing) depends on environmental parameters and poses a greater challenge to ensure corresponding (sometimes local) temperatures under construction site conditions.
[0018] If thermal post-treatment is possible, welding repairs will only result in a reduction in the mechanical material properties. In addition, the costs and time required are significantly higher. If thermal post-treatment is not possible, welding repairs with the required material properties cannot be achieved.
[0019] Another solution is to machine the repaired area, wherein this measure can usually only be carried out once on the same rotor for technical safety reasons and the resulting impact on other components in the system.
[0020] The above-mentioned problems can be avoided by special heat management of steels after welding, in particular steels with a ferrite structure and a bainite structure.
[0021] The service life of a damaged rotor can be extended. Alternative methods are:
[0022] 1.) Turn the bearing surface and adjust the bearing:
[0023] Adjustment of the bearing can only be carried out after the cutting process has been completed and therefore lasts longer than the described solution. The duration depends on the logistics / production possibilities of the bearing shells in the specific country. The time difference to restore operational readiness is estimated at at least one to two weeks. Known penalties for breach of contract range from 80,000 to 500,000 euros per day. Assembly costs for both methods (conventional and new) are expected to be equal, as the new method requires additional welding services. For safety reasons and the resulting impact on other components in the system, this method can usually only be carried out once on the same rotor.
[0024] 2.) To replace the damaged bearing part, you need to do the following:
[0025] The gas turbine rotor is disassembled, the parts to be replaced are provided and adjusted, and restacked. Final turning must then be performed to obtain the required bearing clearance tolerances in the stacked state. During this time, assembly workers and machines must be available on site. The overall expense is comparable to the total economic loss.
[0026] 3.) Install and provide new rotor:
[0027] This variant does not affect the time, but is more expensive than any repair method.
[0028] The steel used in the invention is capable of forming a bainitic structure within a technically reasonable time.
[0029] These steels are in particular steels (ie steels) containing nickel (Ni), chromium (Cr), molybdenum (Mo) and vanadium (V).
[0030] Particularly preferred is a material grade of CrMoV steel containing 2.5-4% nickel, in particular steel 26NiCrMoV14-5, 26NiCrMoV14-5 modified, 26NiCrMoV11-5 or 26NiCrMoV11-5 modified, in particular steel according to DIN / EN
[0031] 1.6957 / 26NiCrMoV14-5, 1.6963 / 26NiCrMoV14-5 modified,
[0032] 1.6948 / 26NiCrMoV11-5, 1.6962 / 26NiCrMoV11-5 modified.
[0033] Typically, overlay welding is performed. For the additional material of the overlay welding, a material different from the material of the component to be overlaid is used. Different here means that at least one alloying element is superfluous or missing, or the content of at least one alloying element differs by at least 10%, in particular 20%.
[0034] It is relatively unimportant whether the material to be welded is capable of forming a bainite structure. In particular, the material to be welded is a silicon-containing MnNiCrMo steel.
[0035] In this case, in particular a welding wire for build-up welding is used which is suitable for use under argon shielding gas.
[0036] According to the applicable standards, each welding process must comply with the welding instructions (WPS) and the annealing protocol for the heat treatment. This makes it possible to check whether the method to be patented here is being used. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] The accompanying figures show a number of temperature-time curves. DETAILED DESCRIPTION
[0038] Curve 1 shows a temperature profile for forming a bainitic structure, where the material is heated to an austenitizing temperature of 1073K to 1323K, then cooled and held at a temperature of at least 573K for one to two hours, and then cooled as discussed in the prior art.
[0039] In conventional welding (curve 4), the temperature is as high as 1973K, where the local temperature of the weld is then rapidly cooled and maintained at a temperature well below 573K for one to two hours, then slowly cooled over a few hours, then heated again to a temperature greater than 773K and maintained for several hours, and then cooled again. This is a time-consuming (>40 hours) process.
[0040] In the method according to the invention according to curve 7, temperatures of up to 1973 K are likewise reached during welding, wherein the local temperature of the weld point is then likewise cooled rapidly, but then remains at a temperature greater than 573 K, or generally above the martensite formation temperature, i.e. at least 10 K above this temperature, in particular at least 20 K above this temperature, so that the weld point remains between 623 K and 673 K, in particular until a bainitic structure has been formed.
[0041] The holding time at this temperature may be longer than the first plateau of the commercial thermal post-treatment (curve 4), but the complete thermal post-treatment time is generally reduced by at least 50% since, after specially controlled cooling, the thermal post-treatment is completed according to the invention after this plateau.
[0042] The new thermal management can save the money and time of traditional heat treatment of steels that can form a bainitic structure while achieving the same / improved material properties.
[0043] The additional workload for conventional on-site thermal post-processing is estimated at two to three days for two to three employees per part.
Claims
1. A method for welding components made of steel, in particular with a ferritic structure, in which a build-up weld is carried out, wherein the weld is subsequently cooled and held at a holding temperature above the martensite formation temperature, in particular at least 10 K above the martensite formation temperature, in particular at least 20 K above the martensite formation temperature, for a period of two to ten hours or until a bainite structure has fully formed, and then cooled, in particular in a controlled manner, in particular to room temperature, and in particular the heat treatment is completed thereby.
2. The method according to claim 1, The welding involves welding components made of steel containing nickel (Ni), chromium (Cr), molybdenum (Mo) and vanadium (V), in particular welding components made of steel with a material grade of 2.5-4% NiCrMoV steel, and in particular welding components made of 26NiCrMoV14-5, 26NiCrMoV14-5 modified, 26NiCrMoV11-5 or 26NiCrMoV11-5 modified steel.
3. The method according to any one or both of claims 1 or 2, The holding temperature is at least 573K, in particular at least 623K to 673K, but at most 773K.
4. The method according to any one or more of claims 1, 2 or 3, In this case, a material different from the material of the components to be welded is used as the material for the build-up welding, in particular a silicon-containing MnNiCrMo steel.
5. The method according to any one or more of claims 1, 2, 3 or 4, A welding wire is used for the overlay welding, which is applied in particular under argon shielding gas.
6. A component made of steel having a weld buildup seam made of steel, wherein the component has a bainitic structure at least in the region of the weld buildup seam.
7. The component according to claim 6, The component comprises a steel containing nickel (Ni), chromium (Cr), molybdenum (Mo) and vanadium (V), in particular a steel having the material grade 2.5-4% NiCrMoV steel, in particular 26NiCrMoV14-5, 26NiCrMoV14-5 modified, 26NiCrMoV11-5 or 26NiCrMoV11-5 modified.
8. A component according to either or both of claims 6 or 7, in, The material used for the build-up welding comprises a material different from the material of the components to be welded, in particular comprises a silicon-containing MnNiCrMo steel.