Reactor and preparation method thereof
By setting an isolation reaction layer, thermal insulation layer and nanozirconia coating on the inner wall of the reactor, the problem of insufficient corrosion resistance of the coating in high-temperature and high-pressure environments is solved, the purity of reactants and the life of the reactor are improved, and efficient isolation is achieved Heat and corrosion resistance.
Patent Information
- Application Number
- CN202411239157.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-12-06
AI Technical Summary
In the high temperature and high pressure environment, the corrosion resistance of the existing reactors is insufficient, resulting in a reduced purity of the reactor and a short service life of the reactor.
Three layers of coating structures are arranged on the inner wall of the reactor: isolation reaction layer, thermal insulation layer and nanozirconia coating, which are formed by spraying technology, and are prepared by inner hole supersonic flame spraying, plasma spraying method and air spray gun remelting method respectively. , ensure that the porosity and expansion coefficient of the coating match, improve corrosion resistance and thermal insulation performance.
Effectively prevent reactants from contacting the reactor matrix, improve reactor purity and reactor service life, reduce production costs, and the nano-zirconia coating has corrosion resistance, and the surface is smooth after remelting, without grinding.
Smart Images

Figure CN119075860A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical engineering, and in particular to a reactor and a method for preparing the reactor. Background Art
[0002] Reactors are equipment that realize chemical or biological reaction processes and are widely used in chemical, oil refining, metallurgy, light industry and other industrial sectors. Reactors can provide a suitable chemical reaction environment: such as temperature, pressure, concentration, etc. Reactors can promote full contact between reactants and accelerate the reaction rate; Reactors can control the reaction process and ensure the stability and safety of the reaction.
[0003] A reactor is a device that realizes a chemical reaction or a biological reaction process. The base material of the reactor is austenitic chromium-nickel stainless steel (310S). When the reactor is in a high temperature and high pressure environment or the reactants are corrosive, the metal elements in 310S will be mixed into the reactants, causing the metal content in the reactants to exceed the standard, reducing the purity of the reactants, and also reducing the service life of the reactor. Therefore, in order to improve the high temperature resistance and corrosion resistance of the reactor, the existing reactor sprays a coating on the inner wall of the reactor.
[0004] In the prior art, although the coating of the reactor has certain high temperature resistance and corrosion resistance, the corrosion resistance of the coating is not high and cannot effectively isolate the reactor matrix and reactants under high temperature and high pressure environment, thereby reducing the service life of the reactor and the purity of the reactants. Summary of the invention
[0005] The object of the present invention is to provide a reactor and a method for preparing the reactor, wherein a coating is arranged on the inner wall of the reactor, and the coating can effectively prevent the reactants from contacting with the reactor substrate, so that the reactants have ultra-high purity.
[0006] To achieve this object, the present invention adopts the following technical solutions:
[0007] In one aspect, a reactor is provided, wherein the reactor is provided with a reaction chamber, wherein an inner wall of the reaction chamber is provided with a coating, wherein the coating comprises:
[0008] An isolation reaction layer, which is sprayed on the inner wall of the reaction chamber;
[0009] A heat insulation layer, which is sprayed on the surface of the isolation reaction layer;
[0010] The nano zirconium oxide coating is sprayed on the surface of the thermal insulation layer.
[0011] As a preferred embodiment of the above reactor, the porosity of the isolation reaction layer is less than or equal to 0.2%; and / or the porosity of the heat insulation layer is in the range of 8%-12%; and / or the porosity of the nano zirconium oxide coating is in the range of 2%-5%.
[0012] As a preferred embodiment of the above reactor, the expansion coefficient of the isolation reaction layer is between the expansion coefficient of the inner wall of the reaction chamber and the expansion coefficient of the heat insulation layer.
[0013] As a preferred embodiment of the above reactor, the thickness of the nano zirconium oxide coating ranges from 0.03 mm to 0.06 mm.
[0014] As a preferred embodiment of the above-mentioned reactor, the reactor is composed of a plurality of reactor segments connected in sequence, one of the end faces of adjacent reactor segments is provided with a positioning groove, and the other is provided with a positioning convex edge, the positioning convex edge is embedded in the positioning groove, and the outer edges of adjacent reactor segments are welded and connected.
[0015] As a preferred embodiment of the above reactor, the plurality of reactor sections include an upper cone, an upper tank, a lower cone, a lower feeding cylinder, a lower cylinder and a discharge lower cone connected in sequence;
[0016] The side wall of the upper tank body is provided with a first feeding port, and a first reaction chamber is formed between the upper cone body, the upper tank body and the lower cone body;
[0017] The lower feeding cylinder is provided with a second feeding port, and a second reaction chamber is formed between the lower feeding cylinder, the lower cylinder and the discharge lower cone. The second reaction chamber is connected to the downstream of the first reaction chamber, and the discharge lower cone is provided with a discharge port.
[0018] As a preferred embodiment of the above reactor, the inner walls of the first feeding port and the second feeding port are installed with a heat insulating lining.
[0019] On the other hand, a method for preparing a reactor is provided, which is used to prepare the above reactor, and the preparation method comprises the following steps:
[0020] Step 1: manufacturing a plurality of reactor segments;
[0021] Step 2: spraying the inner wall of each reactor section in sequence to form the isolation reaction layer, the thermal insulation layer and the nano zirconium oxide coating; wherein the spraying step of the nano zirconium oxide coating comprises: preparing a nano zirconium oxide suspension; spraying the nano zirconium oxide suspension on the surface of the thermal insulation layer by an air spray gun; and remelting by a plasma spray gun to form the nano zirconium oxide coating;
[0022] Step 3: Connect multiple reactor segments in sequence.
[0023] As a preferred embodiment of the preparation method of the above reactor, the nano zirconium oxide suspension uses deionized water as solvent, the volume content of zirconium oxide is 15-25%, and the average particle size of zirconium oxide is 50-100 nm.
[0024] As a preferred embodiment of the preparation method of the above reactor, the isolation reaction layer is a nickel-chromium-aluminum-yttrium coating formed by inner hole supersonic flame spraying; and / or the heat insulation layer is a zirconium oxide coating formed by plasma spraying.
[0025] Beneficial effects of the present invention:
[0026] The present invention provides a reactor and a method for preparing the reactor. The reactor is provided with a reaction chamber so that reactants can react in the reaction chamber. A coating is provided on the inner wall of the reaction chamber, and the isolation reaction layer is sprayed on the inner wall of the reaction chamber, which can prevent the reactants from contacting the inner wall of the reaction chamber, thereby preventing the metal elements on the inner wall of the reaction chamber from reacting with the reactants; the heat insulation layer is sprayed on the surface of the isolation reaction layer, which can isolate the high temperature inside the reaction chamber and prevent the temperature of the reactor substrate from being too high, and the heat insulation layer has a high porosity, which can release the stress inside the coating, and its fatigue performance is very good; the nano-zirconia coating is sprayed on the surface of the heat insulation layer, and the particle size of the nano-zirconia is nanometer-level and has an ultra-low porosity, which can prevent the infiltration of the reactants, and further prevent the reactants from contacting the inner wall of the reaction chamber, greatly improving the service life of the reactor and the purity of the reactants; further, the nano-zirconia coating has corrosion resistance, and the surface is smooth after remelting and does not need to be polished, thereby reducing production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 is a schematic diagram of the reactor coating structure provided by an embodiment of the present invention;
[0028] Figure 2 It is a schematic diagram of the structure of a reactor provided in an embodiment of the present invention;
[0029] Figure 3 is a schematic structural diagram of the connection of adjacent reactor segments provided by an embodiment of the present invention;
[0030] Figure 4 is a schematic diagram of the cone structure of the reactor provided by an embodiment of the present invention;
[0031] Figure 5 Schematic diagram of the upper tank structure of the reactor provided by an embodiment of the present invention;
[0032] Figure 6 Schematic diagram of the lower cone structure of the reactor provided by an embodiment of the present invention;
[0033] Figure 7It is a schematic diagram of the structure of the lower feeding cylinder of the reactor provided in an embodiment of the present invention;
[0034] Figure 8 Schematic diagram of the lower cylinder structure of the reactor provided by an embodiment of the present invention;
[0035] Fig. 9 Schematic diagram of the lower cone structure of the reactor provided by an embodiment of the present invention;
[0036] Fig.10 It is a schematic diagram of the structure of the upper cover plate of the reactor provided in an embodiment of the present invention;
[0037] Fig.11 Schematic diagram of the heat insulation lining structure of the reactor provided by an embodiment of the present invention;
[0038] Fig.12 It is a flow chart of a method for preparing a reactor provided in an embodiment of the present invention.
[0039] In the figure:
[0040] 101, isolation reaction layer; 102, heat insulation layer; 103, nano zirconium oxide coating;
[0041] 1. Upper cover plate; 2. Upper cone; 21. Monitoring port; 22. Positioning convex edge; 3. Upper tank body; 31. First feeding port; 32. Reinforcing ribs; 33. Positioning skirt; 34. Positioning groove; 4. Lower cone; 5. Lower feeding cylinder; 51. Second feeding port; 6. Insulating lining; 7. Lower cylinder; 8. Discharging lower cone. DETAILED DESCRIPTION
[0042] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.
[0043] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0044] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0045] In the description of this embodiment, the terms "upper", "lower", "right", etc., directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.
[0046] like Figure 1 and Figure 2 As shown, this embodiment provides a reactor, the reactor is provided with a reaction chamber, and the inner wall of the reaction chamber is provided with a coating, and the coating includes an isolation reaction layer 101, a heat insulation layer 102 and a nano zirconium oxide coating 103. The isolation reaction layer 101 is sprayed on the inner wall of the reaction chamber, which can prevent the reactants from contacting the inner wall of the reaction chamber, thereby preventing the metal elements on the inner wall of the reaction chamber from reacting with the reactants. The heat insulation layer 102 is sprayed on the surface of the isolation reaction layer 101, which can isolate the high temperature inside the reaction chamber and prevent the temperature of the reactor substrate from being too high. The nano zirconium oxide coating 103 is sprayed on the surface of the heat insulation layer 102. The particle size of the nano zirconium oxide is nanometer-level and has an ultra-low porosity, which can prevent the infiltration of the reactants, and further prevent the reactants from contacting the inner wall of the reaction chamber, greatly improving the service life of the reactor and the purity of the reactants; further, the nano zirconium oxide coating 103 has corrosion resistance, and the surface is smooth after remelting and does not need to be polished, which reduces production costs.
[0047] Preferably, the porosity of the isolation reaction layer 101 is less than or equal to 0.2%; and / or the porosity of the heat insulation layer 102 is in the range of 8%-12%; and / or the porosity of the nano zirconium oxide coating 103 is in the range of 2%-5%.
[0048] In this embodiment, the porosity of the isolation reaction layer 101 is less than or equal to 0.2%. The isolation reaction layer 101 can be a nickel-chromium-aluminum-yttrium coating, and nickel-chromium-aluminum-yttrium with a powder particle size in the range of 5-22 μm can be used as a coating. The coating is prepared by an inner hole supersonic flame spraying method, and the porosity of the coating can be less than or equal to 0.2%. The lower porosity of the isolation reaction layer 101 can prevent the reactants in the reactor from penetrating into the reactor matrix material and reacting with the reactor matrix material, prevent the reactants from corroding the inner wall of the reaction chamber, and improve the service life of the reactor. At the same time, it prevents the metal elements in the reactor substrate from entering the reactants, and improves the purity of the reactants. The nickel-chromium-aluminum-yttrium coating itself also has good heat resistance and corrosion resistance.
[0049] The porosity of the thermal insulation layer 102 is in the range of 8%-12%. The thermal insulation layer 102 can be a zirconium oxide coating. Zirconium oxide with a powder particle size in the range of 15-45 μm can be used as a coating, and the coating is prepared by plasma spraying, which can make the porosity of the coating in the range of 8-12%. The zirconium oxide coating has good thermal insulation performance. When the temperature inside the reactor is too high, the zirconium oxide coating can effectively isolate the high temperature inside the reactor, thereby increasing the service life of the reactor. At the same time, the porosity of the zirconium oxide coating is relatively large, which can release the stress inside the coating and effectively prevent thermal fatigue, but the large porosity will cause the reactants to penetrate into the coating and contact the inner wall of the reaction chamber. Therefore, the porosity of the nano zirconium oxide coating 103 is in the range of 2%-5%, and the nano zirconium oxide coating 103 is sprayed on the surface of the thermal insulation layer 102, which further plays a role in preventing the infiltration of the reactants, greatly improving the service life of the reactor and the purity of the reactants.
[0050] Further preferably, the expansion coefficient of the isolation reaction layer 101 is between the expansion coefficient of the inner wall of the reaction chamber and the expansion coefficient of the thermal insulation layer 102. In this embodiment, the expansion coefficient of the isolation reaction layer 101 is between the expansion coefficient of the reactor base material 310S and the expansion coefficient of the thermal insulation layer 102, which can reduce the difference in expansion coefficient between the reactor base material 310S and the thermal insulation layer 102, and can effectively prevent the coating from falling off due to excessive difference in expansion coefficient, thereby increasing the service life.
[0051] Further preferably, the thickness of the nano zirconium oxide coating 103 is in the range of 0.03 mm to 0.06 mm. The nano zirconium oxide coating 103 is relatively thin, which hardly affects the mechanical properties of the coating while being resistant to high temperatures and preventing the infiltration of reactants.
[0052] In the prior art, the coating is usually sprayed on the inner wall of the reactor by a thermal spraying process. Due to the process limitations of thermal spraying, the spraying length of plasma inner hole spraying and supersonic inner hole spraying is generally 1-1.5 meters. If the spraying extension rod is too long, there will be certain unstable factors during the spraying process, resulting in poor quality of the sprayed coating. Generally, when the spraying length exceeds 2 meters, it cannot be sprayed due to mechanical structure limitations. Therefore, it is necessary to segment the reactor and spray in sections. After the final spraying is completed, the reactor sections are welded and connected. However, during the welding process, the welding process will affect the coating in the reactor through the gap between adjacent reactor sections. Since the coating is not weldable, the coating will fall off or crack when it is welded. When the welding area is close to the coating, the coating will also crack or fall off due to local heating.
[0053] To solve the above problems, Figure 2 and Figure 3 As shown, the reactor is formed by splicing a plurality of reactor segments connected in sequence, one of the end faces of the adjacent reactor segments is provided with a positioning groove 34, and the other is provided with a positioning convex edge 22, the positioning convex edge 22 is embedded in the positioning groove 34, and the outer edges of the adjacent reactor segments are welded and connected. The reactor is formed by splicing a plurality of reactor segments connected in sequence, so that each reactor segment can be sprayed separately, which solves the problem that the inner wall of the reactor cannot be completely sprayed with the coating due to the reactor being too long, and improves the coating spraying quality of the inner wall of the reactor. After the reactor segments are sprayed, the positioning convex edges 22 of the adjacent reactor segments are embedded in the positioning groove 34, the adjacent reactor segments are spliced, and finally the outer edges of the adjacent reactor segments are welded and connected. The positioning convex edge 22 is embedded in the positioning groove 34. On the one hand, the convenience and accuracy of assembling adjacent reactor segments are improved, and the subsequent welding between adjacent reactor segments is convenient. On the other hand, the gap between the positioning convex edge 22 and the positioning groove 34 is located at the bottom of the positioning groove 34. The gap and the end face of the adjacent reactor segment are not on the same horizontal plane. The positioning convex edge 22 plays the role of stopping the welding area, thereby achieving effective isolation between the welding area and the inner wall of the reactor segment, so that the coating on the inner wall of the reactor segment will not be affected by welding and cracked or fall off.
[0054] Preferably, the length of each reactor segment does not exceed 1.5 meters, so that each reactor segment can be completely and evenly sprayed with a coating, thereby improving the spraying quality.
[0055] In order to facilitate the splicing of adjacent reactor segments, the inner diameter of the positioning groove 34 is slightly larger than the outer diameter of the positioning convex edge 22, so that a certain gap is left between the upper and lower and side surfaces of the positioning groove 34 and the positioning convex edge 22 after splicing, which is convenient for installation. The gap margin after splicing should be within the range of 0.3-0.4mm. Each reactor segment is spliced by interference connection. The splicing method is as follows: first, the positioning groove 34 of each reactor segment is heated to 150-200°C, and then the positioning convex edge 22 of the reactor segment is embedded into the positioning groove 34, and then the positioning groove 34 is cooled to room temperature. According to the principle of thermal expansion and contraction, the positioning groove 34 will shrink after cooling, thereby eliminating the gap between the positioning groove 34 and the positioning convex edge 22, so that it can achieve interference connection. Then each reactor segment is permanently welded by welding. After spraying and splicing, the inner wall of the reactor can be completely covered with the coating. The reactor manufactured by this method can be used at a temperature as high as 900-1000°C, and the metal content in the reactants is almost zero, which solves the purity problem of high-temperature reactants. The service life is increased by 3-4 times compared with the reactor without coating.
[0056] Preferably, if Figure 2-Figure 9 As shown, the multiple reactor sections include an upper cone 2, an upper tank body 3, a lower cone 4, a lower feeding cylinder 5, a lower cylinder 7 and a discharge lower cone 8 connected in sequence. The side wall of the upper tank body 3 is provided with a first feeding port 31, and a first reaction chamber is formed between the upper cone 2, the upper tank body 3 and the lower cone 4. The lower feeding port cylinder 5 is provided with a second feeding port 51, and a second reaction chamber is formed between the lower feeding cylinder 5, the lower cylinder 7 and the discharge lower cone 8. The second reaction chamber is connected to the downstream of the first reaction chamber, and the discharge lower cone 8 is provided with a discharge port. When in use, the reactant is added to the upper tank body 3 through the first feeding port 31, so that it undergoes a primary reaction in the first reaction chamber. After the primary reaction is completed, another reactant is added to the lower feeding port cylinder 5 through the second feeding port 51, so that it undergoes a secondary reaction in the second reaction chamber. After the reaction is completed, the reactant is discharged from the reactor through the feed port provided on the discharge lower cone 8.
[0057] Preferably, if Figure 2 and Figure 3 As shown, the edges of the connecting parts of adjacent reactor segments form welding grooves, and the welding grooves are configured to be filled with solder. The welding groove can be a ring-shaped structure with a V-shaped cross section, which is arranged on the outside of the connecting parts of adjacent reactor segments. The welding groove can be welded by argon arc welding, and the welding wire can be a heat-resistant stainless steel welding wire. After splicing, the outer edges of the adjacent reactor segments are welded and connected, and the welding grooves are filled with solder, which increases the contact area between the solder and the adjacent reactor segments, improves the welding strength, and at the same time, the welding groove can facilitate the welding between the reactor segments.
[0058] Preferably, an operation port is provided on a side of the upper cone 2 away from the upper tank body 3 , and the provision of the operation port can facilitate spraying of the coating on the upper cone 2 .
[0059] More preferably, if Figure 2 and Fig.10 As shown, the reactor also includes an upper cover plate 1. The upper cover plate 1 can be a cylindrical plate. The upper cover plate 1 can be detachably sealed to the operating port of the upper cone 2, and can be connected by bolts or screws, which is not limited in this embodiment. When connected by bolts or screws, threaded holes are set at the positions corresponding to the upper cover plate 1 and the upper cone 2, and screws or spirals are passed through the threaded holes to fix them. The upper cover plate 1 can block the operating port of the upper cone 2 and seal the reactor.
[0060] Further preferably, a sealing member is provided between the upper cover plate 1 and the operation opening of the upper cone 2. The sealing member is provided between the upper cover plate 1 and the operation opening of the upper cone 2, and a certain pressure is applied to the sealing member by tightening the screws or bolts connecting the upper cover plate 1 and the upper cone 2, so that the sealing member can be fixed between the operation opening of the upper cover plate 1 and the upper cone 2. The sealing member can be made of a flexible material such as rubber or silicone, and this embodiment does not limit this. The sealing member can further improve the sealing performance of the reactor.
[0061] Since the inner diameters of the first feeding port 31 and the second feeding port 51 are relatively small, it is not possible to prepare the coating by spraying.
[0062] To solve the above problems, Figure 2 and Fig.11 As shown, a heat-insulating lining 6 is installed on the inner wall of the first feeding port 31 and the second feeding port 51 to prevent the reactants from contacting the inner wall of the first feeding port 31 and the second feeding port 51. The heat-insulating lining 6 can be a zirconia ceramic lining, and the thickness of the zirconia ceramic lining is 8-10 mm. The heat-insulating lining 6 is interference-connected with the inner wall of the first feeding port 31 and the second feeding port 51. When the first feeding port 31 and the second feeding port 51 are matched with the thermal insulation lining 6, the first feeding port 31 and the second feeding port 51 are first heated to 150-200°C, and then the thermal insulation lining 6 is placed in the feeding port, and then the first feeding port 31 and the second feeding port 51 are cooled to room temperature. According to the principle of thermal expansion and contraction, the first feeding port 31 and the second feeding port 51 will shrink after cooling, thereby eliminating the gap between the thermal insulation lining 6 and the first feeding port 31 and the second feeding port 51, making the fit between the thermal insulation lining 6 and the first feeding port 31 and the second feeding port 51 more firm, and preventing the thermal insulation lining 6 from falling off.
[0063] Preferably, if Figure 2As shown, a positioning skirt 33 is installed on the outer wall of the upper tank body 3, and the side of the positioning skirt 33 close to the lower cone 4 is used to overlap the installation station to fix the reactor. A reinforcing rib 32 is arranged between the side of the positioning skirt 33 away from the lower cone 4 and the upper tank body 3. The reinforcing rib 32 can be in the shape of a long strip, which can improve the strength of the positioning skirt 33. The positioning skirt 33 and the upper tank body 3, and the reinforcing rib 32 and the positioning skirt 33 and the upper tank body 3 can be connected by welding.
[0064] It should be noted that the reinforcing ribs 32 provided in this embodiment can be provided with one, two, three, four, five or more than five. The spacer ring is arranged on the outer wall of the upper tank body 3 and is connected to the side of the positioning skirt 33 away from the lower cone 4. It can be designed according to specific needs and this embodiment does not limit this.
[0065] Preferably, if Figure 2 As shown, monitoring ports 21 are respectively provided on the upper cone 2 and the lower cylinder 7, and a detection device is provided in the monitoring port 21. The detection device can be a temperature sensor or a thermometer to monitor the reaction temperature inside the reactor so as to observe the reaction conditions of the reactants inside the reactor.
[0066] Preferably, the upper cone 2, the upper tank 3, the lower cone 4 and the discharge lower cone 8 are made of curved plates, which facilitates the manufacture of the reactor section.
[0067] Preferably, the lower cylinder 7 is a cylindrical annular cylinder made of a seamless pipe, which can make the strength of the reactor section higher.
[0068] Preferably, if Figure 2 As shown, the lower cylinder 7 of the reactor is manufactured in multiple sections and connected in sequence, which can prevent the lower cylinder 7 from being too long and facilitate the spraying of the lower cylinder 7.
[0069] Further preferably, the lower barrel 7 of the reactor is manufactured in three sections and connected in sequence, so that the length of each reactor section is within the sprayable range, while avoiding too many reactor sections that are difficult to assemble.
[0070] like Fig.12 As shown, this embodiment also provides a method for preparing a reactor, which is used to prepare the above-mentioned reactor. The method for preparing the reactor comprises the following steps:
[0071] Step 1: manufacturing a plurality of reactor segments;
[0072] Step 2: spraying the inner wall of each reactor section in sequence to form an isolation reaction layer 101, a heat insulation layer 102 and a nano zirconium oxide coating 103; wherein the spraying step of the nano zirconium oxide coating 103 comprises: preparing a nano zirconium oxide suspension; spraying the nano zirconium oxide suspension on the surface of the heat insulation layer 102 by using an air spray gun; and remelting by using a plasma spray gun to form the nano zirconium oxide coating 103;
[0073] Preferably, the isolation reaction layer 101 is a nickel-chromium-aluminum-yttrium coating formed by an inner hole supersonic flame spraying method; and / or the heat insulation layer 102 is a zirconium oxide coating formed by a plasma spraying method. In this embodiment, the inner wall of each reactor section is sprayed. During the spraying, the nickel-chromium-aluminum-yttrium coating is first sprayed on the inner wall of each reactor section by an inner hole supersonic flame spraying method; and then the zirconium oxide coating is sprayed on the surface of the nickel-chromium-aluminum-yttrium coating by a plasma spraying method. Finally, the nano zirconium oxide suspension is sprayed on the surface of the zirconium oxide coating by an air spray gun, and then the nano zirconium oxide particles are remelted by a plasma spray gun.
[0074] Further preferably, when spraying the nano zirconium oxide coating 103, the nano zirconium oxide suspension uses deionized water as a solvent, the volume content of zirconium oxide is 15-25%, and the average particle size of zirconium oxide is 50-100 nm.
[0075] Specifically, an air spray gun is used to spray the nano zirconium oxide suspension on the surface of the thermal insulation layer 102. A plasma spray gun is used for remelting to form a nano zirconium oxide coating 103. Nano zirconium oxide can penetrate into the pores of the thermal insulation layer 102. After the pores on the surface of the thermal insulation layer 102 are filled with nano zirconium oxide, the porosity can be reduced to 2-5% after plasma flame sintering, which can prevent the infiltration of reactants. Nano zirconium oxide can also be evenly covered on the surface of the thermal insulation layer 102. After plasma remelting, a dense layer of nano zirconium oxide coating 103 is formed on the surface of the thermal insulation layer 102. The thickness of the nano zirconium oxide coating 103 ranges from 0.03 to 0.06 mm. The porosity of the nano zirconium oxide coating 103 itself is also 2-5%, which can further prevent the infiltration of reactants and greatly improve the purity of the reactants.
[0076] Step 3: Connect multiple reactor segments in sequence.
[0077] Preferably, when connecting, first heat the positioning groove 34 of each reactor segment to 150-200°C, then embed the positioning convex edge 22 of the reactor segment into the positioning groove 34, and then cool the positioning groove 34 to room temperature. According to the principle of thermal expansion and contraction, the positioning groove 34 will shrink after cooling, thereby eliminating the gap between the positioning groove 34 and the positioning convex edge 22, so that it can achieve interference connection, and then weld each reactor segment permanently. After spraying and splicing, the inner wall of the reactor can be completely covered with the coating. The operating temperature of the reactor manufactured by this method can be as high as 900-1000°C, and the metal content in the reactant is almost zero, which solves the problem of poor purity of the reactant in a high temperature environment, and the service life is increased by 3-4 times relative to the reactor without coating.
[0078] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, various obvious changes, readjustments and substitutions can be made without departing from the protection scope of the present invention. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A reactor, It is characterized in that The reactor is provided with a reaction chamber, and the inner wall of the reaction chamber is provided with a coating, and the coating comprises: An isolation reaction layer (101) is sprayed on the inner wall of the reaction chamber; A heat insulation layer (102) sprayed on the surface of the isolation reaction layer (101); A nano zirconium oxide coating (103) is sprayed on the surface of the thermal insulation layer (102).
2. The reactor according to claim 1, It is characterized in that The porosity of the isolation reaction layer (101) is less than or equal to 0.2%; and / or The porosity of the thermal insulation layer (102) is in the range of 8%-12%; and / or The porosity of the nano zirconium oxide coating (103) is in the range of 2%-5%.
3. The reactor according to claim 1, It is characterized in that The expansion coefficient of the isolation reaction layer (101) is between the expansion coefficient of the inner wall of the reaction chamber and the expansion coefficient of the heat insulation layer (102).
4. The reactor according to claim 1, It is characterized in that The thickness of the nano zirconium oxide coating (103) is in the range of 0.03 mm to 0.06 mm.
5. The reactor according to claim 1, It is characterized in that The reactor is formed by splicing a plurality of reactor segments connected in sequence, one of the end faces of adjacent reactor segments is provided with a positioning groove (34), and the other is provided with a positioning convex edge (22), the positioning convex edge (22) is embedded in the positioning groove (34), and the outer edges of adjacent reactor segments are welded and connected.
6. The reactor according to claim 5, It is characterized in that The plurality of reactor sections include an upper cone (2), an upper tank (3), a lower cone (4), a lower feeding cylinder (5), a lower cylinder (7) and a discharge lower cone (8) which are connected in sequence; The side wall of the upper tank body (3) is provided with a first feeding port (31), and a first reaction chamber is formed between the upper cone body (2), the upper tank body (3) and the lower cone body (4); The lower feeding cylinder (5) is provided with a second feeding port (51), and a second reaction chamber is formed between the lower feeding cylinder (5), the lower cylinder (7) and the lower discharge cone (8), the second reaction chamber is connected to the downstream of the first reaction chamber, and the lower discharge cone (8) is provided with a discharge port.
7. The reactor according to claim 6, It is characterized in that The inner walls of the first feeding port (31) and the second feeding port (51) are installed with heat insulating linings (6).
8. A method for preparing a reactor, It is characterized in that For preparing the reactor according to any one of claims 1 to 7, the preparation method of the reactor comprises the following steps: Step 1: manufacturing a plurality of reactor segments; Step 2: spraying the inner wall of each reactor section in sequence to form the isolation reaction layer (101), the heat insulation layer (102) and the nano zirconium oxide coating (103); wherein the spraying step of the nano zirconium oxide coating (103) comprises: preparing a nano zirconium oxide suspension; spraying the nano zirconium oxide suspension on the surface of the heat insulation layer (102) by using an air spray gun; and remelting by using a plasma spray gun to form the nano zirconium oxide coating (103); Step 3: Connect multiple reactor segments in sequence.
9. The method for preparing the reactor according to claim 8, It is characterized in that The nano zirconium oxide suspension uses deionized water as a solvent, the volume content of zirconium oxide is 15-25%, and the average particle size of zirconium oxide is 50-100 nm.
10. The method for preparing the reactor according to claim 8 or 9, It is characterized in that The isolation reaction layer (101) is a nickel-chromium-aluminum-yttrium coating formed by an inner hole supersonic flame spraying method; and / or the heat insulation layer (102) is a zirconium oxide coating formed by a plasma spraying method.