Die for producing drum part and outer rim in same die and using method thereof

By designing a mold structure including upper die core, lower die core, hafu and flow channel, the drum part and outer rim are simultaneously formed, solving the problems of low efficiency and waste of resources in the prior art, and improving production Efficiency and save mold opening cost.

CN119076892APending Publication Date: 2024-12-06ZHEJIANG WANFENG MOTORCYCLE WHEEL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411196155.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The existing molds are inefficient and inadequately utilized in the production of drum sections and outer rims, resulting in waste of resources and high costs.

Method used

Design a mold structure, including an upper mold core, a lower mold core, a hafu, a runner and a cooling mechanism, and achieve simultaneous molding of the drum part and the outer rim through the design of the mold cavity and the runner, and make full use of the mold space by connecting the runner , and optimize the casting process through cooling system.

Benefits of technology

Improve production efficiency, double the cost of mold opening, reduce the occurrence of casting loose defects, and achieve more efficient resource utilization.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119076892A_ABST
    Figure CN119076892A_ABST
Patent Text Reader

Abstract

The invention discloses a die for producing a drum part and an outer rim in the same die and a using method thereof.The die comprises a base, a bottom plate is installed on the upper portion of the base, a lower die core is installed on the upper portion of the bottom plate, an upper die core is arranged above the lower die core, a plurality of halves are arranged on the periphery of the lower die core and the periphery of the upper die core, and an upper die small core is arranged in the middle of the upper die core; a feeding sleeve is installed in the middle of the upper die small core, a first forming cavity is formed among the upper die small core, the upper die core and the lower die core, a sand core is arranged in the first forming cavity, a second forming cavity is formed among the upper die core, the lower die core and the half, a runner is arranged between the first forming cavity and the second forming cavity for communication, and a sprue spreader is arranged in the middle of the lower die core. The drum part and the outer rim can be produced at the same time, and the production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of molds, and more specifically to a mold for producing a drum part and an outer rim in the same mold and a use method thereof. Background Art

[0002] A mold is a tool used to make molded objects. This tool is composed of various parts. Different molds are composed of different parts. It mainly realizes the processing of the shape of the object by changing the physical state of the molded material. Generally, one product corresponds to one mold. Since the outer rim is annular, the mold size is larger, but the part used is less, resulting in the middle part not being fully utilized and wasted. In addition, the efficiency of casting two products separately is low. Summary of the invention

[0003] The purpose of the present invention is to overcome the above-mentioned deficiencies of the prior art and to provide a mold for producing a drum portion and an outer rim in the same mold and a method for using the same mold.

[0004] In order to achieve the above object, the present invention adopts the following technical solution:

[0005] The invention discloses a mold for producing a drum part and an outer rim with the same mold, wherein a plurality of hafu are arranged on the outer peripheries of an upper mold core, a lower mold core and an upper mold core, an upper mold small core is arranged in the middle position of the upper mold core, a feed sleeve is installed in the middle position of the upper mold small core, a molding cavity one is formed between the upper mold small core, the upper mold core and the lower mold core, a sand core is arranged in the molding cavity one, a molding cavity two is formed between the upper mold core, the lower mold core and the hafu, a flow channel is arranged between the molding cavity one and the molding cavity two, and a diverter cone is arranged in the middle position of the lower mold core.

[0006] Furthermore, the flow channel includes flow channel 1 and flow channel 2, flow channel 1 is opened on the upper part of the lower mold core, and flow channel 2 is opened on the sand core.

[0007] Furthermore, the cross-sections of the flow channel 1 and the flow channel 2 are isosceles trapezoids, the width of the flow channel 1 is greater than the height, and the height of the flow channel 2 is greater than the width.

[0008] Furthermore, a clamping pin is connected to the upper part of the lower mold core, and a clamping hole corresponding to the clamping pin is opened on the upper mold core.

[0009] Furthermore, a riser ring is arranged at the upper position of the outer side of the upper mold core, a part of the riser ring is located above the Haver, a riser is opened on the riser ring, and the riser is communicated with the second molding cavity.

[0010] Furthermore, a pressing plate is arranged on the upper part of the upper mold core, a step is arranged on the outer periphery of the feed sleeve, and a part of the pressing plate is pressed on the step.

[0011] Furthermore, it also includes a cooling mechanism, which includes a drum cooling ring, a diverter cone cooling pipe, an outer rim cooling ring and a cooling pipe, and the drum cooling ring, the diverter cone cooling pipe, the outer rim cooling ring and the cooling pipe are connected.

[0012] Furthermore, a groove is provided on the upper part of the Harv, and heat-insulating cotton is installed in the groove. A sealing plate is provided in the groove at a position above the heat-insulating cotton.

[0013] A method for using a mold for producing a drum portion and an outer rim in the same mold, comprising the following steps:

[0014] Cleaning: Use an air gun to blow clean the upper mold core, lower mold core, and Hafu;

[0015] Place the insert: Put the gear sleeve into the heater for baking at a temperature of 530-600℃ for one minute. After baking, take it out and place it on the diverter cone, and place the sand core on the lower mold core;

[0016] Mold closing: several Havers are closed, and the upper mold core moves toward the lower mold core to close, forming molding cavity 1 and molding cavity 2;

[0017] Casting: The aluminum liquid temperature is 695-720℃. The aluminum liquid is poured in from the feed sleeve. The aluminum liquid flows through the molding cavity 1, the runner and the molding cavity 2 in sequence and fills the molding cavity 1, the runner and the molding cavity 2.

[0018] Cooling: Cooling the aluminum liquid in the molding cavity 1 and the molding cavity 2;

[0019] Open the mold and take out the parts: when starting the mold, start the upper mold core, then open the Hafu, and then eject the product.

[0020] Furthermore, a 20-mesh filter is placed at the feed inlet of the feed sleeve.

[0021] The beneficial effect of the present invention is that compared with the conventional mode of separately molding and manufacturing the outer rim and the drum, the outer rim and the drum can be produced at the same time through the mold structure design, doubling the production efficiency and saving the mold manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 A schematic diagram of the structure of a mold in which the drum and the outer rim are produced in the same mold in this embodiment;

[0023] Figure 2 is a top view of the lower mold core in this embodiment;

[0024] Figure 3 is a cross-sectional view of flow channel 1 in this embodiment;

[0025] Figure 4 2 is a cross-sectional view of flow channel 2 in this embodiment.

[0026] Figure numerals: 1. base; 2. bottom plate; 3. lower mold core; 4. Hafu; 5. upper mold core; 6. clamping hole; 7. clamping pin; 8. upper mold small core; 9. feed sleeve; 10. pressure plate; 11. positioning column; 12. riser ring; 13. riser; 14. groove; 15. insulation cotton; 16. sealing plate; 17. molding cavity one; 18. molding cavity two; 19. sand core; 20. runner; 21. drum; 22. outer rim; 23. support plate; 24. diverter cone; 25. gear sleeve; 26. cooling pipe; 27. runner one; 28. runner two; 29. ​​drum cooling ring; 30. diverter cone cooling pipe; 31. outer rim cooling ring; 32. positioning hole. DETAILED DESCRIPTION

[0027] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] like Figure 1-Figure 4 As shown, a mold for producing a drum and an outer rim in the same mold includes a base 1, a bottom plate 2 is installed on the top of the base 1, a lower mold core 3 is installed on the top of the bottom plate 2, a support plate 23 is installed on the bottom of the lower mold core 3 through bolts, a diverter cone 24 is installed on the top of the support plate 23, the lower mold core 3 has an opening in the middle, and the diverter cone 24 is located in the opening of the lower mold core 3.

[0029] An upper mold core 5 is arranged above the lower mold core 3, and an upper mold small core 8 is arranged in the middle position of the upper mold core 5. The outer edge of the upper mold small core 8 is located on the upper mold core 5, and a feed sleeve 9 is installed in the middle position of the upper mold small core 8. A pressure plate 10 is fixedly installed on the upper part of the upper mold core 5 by bolts, and a part of the pressure plate 10 is located above the upper mold small core 8. A step is arranged on the outer periphery of the feed sleeve 9, and the inner edge of the pressure plate 10 is pressed on the step. The upper mold small core 8 and the feed sleeve 9 are fixedly installed in the middle position of the upper mold core 5 by the pressure plate 10.

[0030] Several havers 4 are arranged on the periphery of the lower mold core 3 and the upper mold core 5, and four havers 4 are arranged. The four havers 4 can be closed to form a side mold. A molding cavity 17 is formed between the upper mold core 8, the upper mold core 5 and the lower mold core 3, and a sand core 19 is arranged in the molding cavity 17. A molding cavity 2 18 is formed between the upper mold core 5, the lower mold core 3 and the havers 4, and a flow channel 20 is arranged between the molding cavity 17 and the molding cavity 2 18. The upper end of the diverter cone 24 is located in the molding cavity 17, and the part of the diverter cone 24 located in the molding cavity 17 is installed with a gear sleeve 25.

[0031] The flow channel 20 connects the molding cavity 17 and the molding cavity 2 18, so that the poured aluminum liquid can flow through the molding cavity 17, the flow channel 20 and the molding cavity 2 18 in sequence and fill them, thereby completing the molding of the drum 21 and the outer rim 22 at the same time. Later, the drum 21 and the outer rim 22 can be separated by knocking off the connecting piece formed at the flow channel 20 to obtain two products.

[0032] The mold is provided with molding spaces for the drum portion 21 and the outer rim 22 at the same time, thereby fully utilizing the space of the mold.

[0033] The arrangement of the sand core 19 can optimize the machining allowance of the outer ring of the drum portion 21 and reduce the probability of occurrence of loose defects in casting.

[0034] Furthermore, the flow channel 20 includes flow channel 1 27 and flow channel 2 28, flow channel 1 27 is opened on the upper part of the lower mold core 3, and flow channel 2 28 is opened on the sand core 19. The cross-sections of flow channel 1 27 and flow channel 2 28 are isosceles trapezoids, the width of flow channel 1 27 is greater than the height, and the height of flow channel 2 28 is greater than the width. The width of flow channel 1 27 is the same as the height of flow channel 2 28, and the height of flow channel 1 27 is the same as the width of flow channel 2 28, so that the shape of the connection position can be changed without changing the size of the cross-sectional dimensions, which can facilitate the subsequent removal of the connector formed in the flow channel 20. In particular, for the drum part 21, the knocked connector needs to be on the thin side, so that there is no remaining process flow channel around the drum part after breaking, and it can be directly processed. Therefore, relative to the flow channel 1 27 on the side of the outer rim 22, the flow channel 2 28 needs to be erected to make the thickness of the molded connector relatively thinner.

[0035] Furthermore, a clamping pin 7 is connected to the upper portion of the lower mold core 3, and a clamping hole 6 corresponding to the clamping pin 7 is opened on the upper mold core 5. The positioning between the upper mold core 5 and the lower mold core 3 is achieved through the cooperation of the clamping pin 7 and the clamping hole 6.

[0036] Furthermore, a riser ring 12 is fixedly installed at the upper position of the outer side of the upper mold core 5 by bolts, a part of the riser ring 12 is located above the haveur 4, a riser 13 is opened on the riser ring 12, and the riser 13 is connected to the molding cavity 18. The aluminum liquid can be added to the molding cavity 18 through the riser 13 to play a shrinkage compensation role, so that the outer rim 22 in the molding cavity 18 can be normally formed.

[0037] The mold further includes a cooling mechanism, which includes a drum cooling ring 29, a diverter cone cooling pipe 30, an outer rim cooling ring 31 and a cooling pipe 26. The drum cooling ring 29, the diverter cone cooling pipe 30, the outer rim cooling ring 31 and the cooling pipe 26 are connected. Cooling is achieved by supplying cooling water to the drum cooling ring 29, the diverter cone cooling pipe 30 and the outer rim cooling ring 31 through the cooling pipe 26.

[0038] Furthermore, a groove 14 is provided on the upper part of the Harvest 4, and a heat preservation cotton 15 is installed in the groove 14. A sealing plate 16 is provided in the groove 14 above the heat preservation cotton 15. The heat preservation cotton 15 plays a role in heat preservation, which can enhance the mold temperature at the Harvest 4 and reduce the heat loss of the aluminum liquid.

[0039] A plurality of positioning posts 11 are provided on the upper part of the lower mold core 3, and positioning holes 32 are provided on the lower part of the sand core 19 to match the positioning posts 11. Through the cooperation between the positioning posts 11 and the positioning holes 32, the sand core 19 can be accurately installed on the lower mold core 3, so that the flow channel 1 27 on the lower mold core 3 corresponds to the flow channel 2 28 on the molding cavity 2 18.

[0040] A method for using a mold for producing a drum portion and an outer rim in the same mold, comprising the following steps:

[0041] The upper mold core 5, the lower mold core 3 and the hafu 4 are blown clean by an air gun to ensure that there are no aluminum sheets or other debris in the subsequent molding cavity 17 and the molding cavity 2 18 to affect the molding of the product.

[0042] The gear sleeve 25 is placed in a heater for baking at a temperature of 530-600° C. for one minute. After baking, it is taken out and placed on the diverter cone 24. The sand core 19 is placed on the lower mold core 3 after being dried.

[0043] A plurality of hafu 4 are closed, and the upper mold core 5 moves toward the lower mold core 3 to close the two, and there is no gap at the closing position. A molding cavity 17 and a molding cavity 2 18 are formed between the lower mold core 3, the hafu 4, and the upper mold core 5.

[0044] A 20-mesh filter is placed at the feed port of the feed sleeve 9. The filter is folded into a cone shape with the tip of the cone located at the bottom to filter impurities in the aluminum liquid.

[0045] The aluminum liquid temperature is 695-720℃, and the aluminum liquid is poured in from the feed sleeve 9, and the liquid flow is aligned with the feed sleeve 9, and the feed sleeve 9 does not shake. The aluminum liquid flows through the molding cavity 17, the flow channel 20 and the molding cavity 2 18 in sequence and fills the molding cavity 17, the flow channel 20 and the molding cavity 2 18; the casting time is 8-10 seconds.

[0046] The drum cooling ring 29 , the diverter cone cooling tube 30 and the outer rim cooling ring 31 are opened in sequence to ensure that the drum 21 and the outer rim 22 are solidified in the order.

[0047] When opening the mold, start the upper mold core 5, then open the Hafu 4, and then eject the product. Ensure that the mold is opened smoothly, turn off the cooling system, and use pliers to remove the product from the mold. The clamping position is the product riser.

[0048] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.

Claims

1. A mold for producing a drum and an outer rim in the same mold, characterized in that: The invention comprises a base (1), a bottom plate (2) is installed on the upper part of the base (1), a lower mold core (3) is installed on the upper part of the bottom plate (2), an upper mold core (5) is arranged above the lower mold core (3), a plurality of hafur (4) are arranged on the periphery of the lower mold core (3) and the upper mold core (5), an upper mold small core (8) is arranged in the middle position of the upper mold core (5), a feed sleeve (9) is installed in the middle position of the upper mold small core (8), and the upper mold small core (5) is provided with a plurality of hafur (4) on the periphery of the lower mold core (3) and the upper mold core (5). A molding cavity 1 (17) is formed between the core (8), the upper mold core (5) and the lower mold core (3), a sand core (19) is arranged in the molding cavity 1 (17), a molding cavity 2 (18) is formed between the upper mold core (5), the lower mold core (3) and the hafu (4), a flow channel (20) is arranged between the molding cavity 1 (17) and the molding cavity 2 (18), and a diverter cone (24) is arranged in the middle position of the lower mold core (3).

2. The mold for producing the drum and the outer rim in the same mold as claimed in claim 1, characterized in that: The flow channel (20) comprises a flow channel 1 (27) and a flow channel 2 (28), wherein the flow channel 1 (27) is opened on the upper part of the lower mold core (3), and the flow channel 2 (28) is opened on the sand core (19).

3. The mold for producing the drum and the outer rim in the same mold as claimed in claim 2, characterized in that: The cross-sections of the flow channel 1 (27) and the flow channel 2 (28) are isosceles trapezoids, the width of the flow channel 1 (27) is greater than the height, and the height of the flow channel 2 (28) is greater than the width.

4. The mold for producing the drum and the outer rim in the same mold as claimed in claim 1, characterized in that: The upper part of the lower mold core (3) is connected with a mold pin (7), and the upper mold core (5) is provided with a mold hole (6) corresponding to the mold pin (7).

5. The mold for producing the drum and the outer rim in the same mold as claimed in claim 1, characterized in that: A riser ring (12) is arranged at the upper position of the outer side of the upper mold core (5), a part of the riser ring (12) is located above the haveur (4), a riser (13) is opened on the riser ring (12), and the riser (13) is connected to the second molding cavity (18).

6. The mold for producing the drum and the outer rim in the same mold as claimed in claim 1, characterized in that: A pressing plate (10) is arranged on the upper part of the upper mold core (5), and a step is arranged on the outer periphery of the feed sleeve (9), and a part of the pressing plate (10) is pressed on the step.

7. The mold for producing the drum and the outer rim in the same mold as claimed in claim 1, characterized in that: The invention also comprises a cooling mechanism, wherein the cooling mechanism comprises a drum cooling ring (29), a diverter cone cooling pipe (30), an outer rim cooling ring (31) and a cooling pipe (26); the drum cooling ring (29), the diverter cone cooling pipe (30), the outer rim cooling ring (31) and the cooling pipe (26) are connected.

8. The mold for producing the drum and the outer rim in the same mold as claimed in claim 1, characterized in that: A groove (14) is provided on the upper part of the hafu (4), a heat-insulating cotton (15) is installed in the groove (14), and a sealing plate (16) is provided in the groove (14) at a position above the heat-insulating cotton (15).

9. A method for using a mold for producing a drum portion and an outer rim in the same mold as described in any one of claims 1 to 8, characterized in that: The following steps are involved: Cleaning: Use an air gun to blow clean the upper mold core (5), the lower mold core (3), and the hafu (4); Insert placement: The gear sleeve (25) is placed in a heater for baking at a temperature of 530-600°C for one minute. After baking, it is taken out and placed on the diverter cone (24), and the sand core (19) is placed on the lower mold core (3); Mold closing: a plurality of hafu (4) are closed, and the upper mold core (5) moves toward the lower mold core (3) and closes, thereby forming a molding cavity 1 (17) and a molding cavity 2 (18); Casting: The aluminum liquid has a temperature of 695-720°C. The aluminum liquid is poured in from the feed sleeve (9). The aluminum liquid flows through the molding cavity 1 (17), the flow channel (20) and the molding cavity 2 (18) in sequence and fills the molding cavity 1 (17), the flow channel (20) and the molding cavity 2 (18); Cooling: cooling the aluminum liquid in the molding cavity 1 (17) and the molding cavity 2 (18); Open the mold and take out the product: When starting the mold, move the upper mold core (5) in a step-by-step manner, then open the Hafu (4), and then eject the product.