Anode plate forming method
Through round rolling machine rounding processing and multi-step annealing, welding, sandblasting and grinding, the problem of poor arc of titanium anode plate is solved, high fit rate and stability are achieved, and the production quality of copper foil is improved.
Patent Information
- Application Number
- CN202411458864.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-18
- Publication Date
- 2024-12-06
AI Technical Summary
In the prior art, when the titanium anode plate is pressed and molded through a mold, the arc is poor, resulting in poor fit during subsequent installation, affecting the production quality of copper foil.
The titanium plate is rolled by a round rolling machine. After setting, it is pressed and annealed on the anode support tool, cut, weld, sandblasting and secondary annealing to ensure arc stability and bonding rate.
The high bonding rate and stability of the anode plate are achieved, the production quality of copper foil is improved, the forming process is simplified, and the efficiency is improved.
Smart Images

Figure CN119077300A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of copper electrolysis, and in particular relates to a method for forming an anode plate. Background Art
[0002] Electrolytic copper foil is a copper foil produced by electrolysis process. It is mainly used to manufacture printed circuit boards (PCBs) and lithium-ion batteries. It is widely used in home appliances, communications, computing (3C), new energy and other industries. In the entire process of electrolytic copper foil, electrolytic deposition is a very important step. During the electrolytic deposition process, high-purity electrolytic copper or waste copper wire is used as raw material and dissolved in sulfuric acid to make copper sulfate solution. In the foil machine, the copper sulfate electrolytic solution is pumped from the anode tank to between the anode plate and the cathode roller. When the direct current passes through, the copper ions gradually deposit on the surface of the cathode roller to form a layer of copper foil with uniform thickness. Among them, the anode plate, as an important component of the anode, has a huge impact on the performance of the product. Most of the anode plates in the prior art use precious metal coated titanium anodes. Compared with traditional lead anodes, precious metal coated titanium anodes have the advantages of low overpotential and stable inter-electrode spacing, which not only reduces the cell voltage and power consumption, but also prolongs the life of the electrolyte. In the prior art, titanium anode plates are usually pressed and formed by molds, and then coated after subsequent processing. This molding process has the following disadvantages: During the pressing process, due to the self-stress of the titanium plate, the curvature of the formed titanium plate is poor, that is, the curvature at the opening is small, while the curvature at the bottom is too large, which will cause poor fit during the subsequent installation process, and have an adverse effect on the performance of subsequent products. Therefore, it is urgent to provide a molding method that can ensure the subsequent high fit of the anode plate. Summary of the invention
[0003] In view of the problems existing in the above-mentioned prior art, the present invention provides a method for forming an anode plate. The method has a simple implementation process, good forming effect and high forming efficiency. The method can prepare an anode plate with good stability and high bonding rate, which is beneficial to ensuring the production quality of copper foil.
[0004] In order to solve the above technical problems, the present invention provides an anode plate forming method, comprising the following steps: Step 1: Rolling the plate; The titanium plate is cut into the required size and shape and then placed in a rolling machine, where it is rolled to form a titanium plate with the required curvature; Step 2: Finalize; The rolled titanium plate is pressed and fixed on the anode support fixture by using a pressing plate; Step 3: annealing; The fixed titanium plate and the anode support fixture are placed in an annealing furnace for annealing treatment. The heat preservation time is 2 hours. After cooling in the furnace, they are taken out. Step 4: Cutting; The cooled titanium plate and the anode support fixture are fixed to the boring machine together with the fixing fixture, and the centering and positioning operation is performed, and then the titanium plate is cut by the end mill to cut the titanium plate into the required shape; Step 5: Welding accessories; The titanium screws are fixedly connected to the predetermined positions of the titanium plates by welding; the edge strips are fixedly connected at both ends of the titanium plates in the length direction by welding; Step 6: Sandblasting and polishing; Fix the titanium plate on the sandblasting and grinding tooling, mark the spraying area on the titanium plate, then sandblast the spraying area and make the sandblasting roughness reach the set value, and perform surface grinding after the sandblasting is completed; Step 7: secondary annealing; The titanium plate together with the sandblasting and grinding tooling was placed in a tabletop furnace for annealing treatment, and the heat preservation time was 2 hours. After cooling in the furnace, it was taken out; Step 8: Plastic surgery; Performing plastic treatment on parts of the titanium plate after secondary annealing; Step 9: Inspection; Fix the titanium plate on the testing fixture to check the arc fitting rate of the titanium plate; Step 10: spraying; The precious metal coating is sprayed on the titanium plate that meets the inspection standards to obtain the required anode plate.
[0005] Furthermore, in order to ensure that the titanium plate with the required curvature can be formed quickly and with high quality after the rolling process, in step one, during the rolling process, a bottom template with the required curvature is placed under the titanium plate, and the bottom template is used to ensure that the titanium plate after treatment forms the required curvature.
[0006] As a preference, in step one, the rolling machine is a three-roller rolling machine or a four-roller rolling machine.
[0007] Furthermore, in order to avoid damage to the surface of the titanium plate by the defective roller surface and to effectively ensure the preparation quality of the anode plate, in step one, before placing the titanium plate into the rolling machine, the rolling machine is first cleaned, each roller surface is cleaned, and then each roller surface is checked for defects that may affect the rolling effect. If defects exist, the defective roller is replaced in time.
[0008] Furthermore, in order to ensure the preparation quality of the anode plate, in step 1, each roller surface in the rolling machine is coated with a disposable wrapping film.
[0009] Further, as a preferred embodiment, in step three, the annealing temperature is controlled between 540°C and 560°C. As a preferred embodiment, in step five, the welding operation is performed by laser welding.
[0010] As a preferred embodiment, in step six, a nitrile rubber skin is used to protect the exposed parts of the sandblasting and grinding tooling and the exposed parts of the titanium plate other than the spraying area; the set value is 120μm.
[0011] Furthermore, in order to effectively prevent the titanium plate from being oxidized during the heating and cooling process, in step seven, argon gas is first filled into the titanium plate to form a protective atmosphere before the annealing process.
[0012] Furthermore, in order to accurately and efficiently detect the fitting rate, in step nine, the process of testing the titanium plate arc fitting rate is as follows: S91: Apply red lead powder on titanium plate or on inspection tooling; S92: Use bolts to fix and tighten the titanium plate on the inspection fixture; S93: Remove the bolts and separate the titanium plate and inspection fixture; S94: The fitting rate is calculated based on the ratio of the area of the inspection tooling covered with red lead powder to the area of the titanium plate coated with red lead powder, or based on the ratio of the area of the titanium plate covered with red lead powder to the area of the inspection tooling covered with red lead powder, and the fitting rate is ensured to be not less than 95%.
[0013] In the present invention, firstly, the titanium plate is rolled by a rolling machine, which can facilitate the rapid and high-quality rolling of the titanium plate into a plate of the required curvature, effectively solving the technical problem that the traditional technology uses a pressing method for shaping, which takes a long time and the pressing effect is not ideal. Secondly, the titanium plate with a curvature is pressed tightly on the anode support tooling, and then annealed together, which can effectively eliminate the internal stress of the titanium plate after the curvature is formed, thereby ensuring that the titanium plate can stably maintain a specific shape without deformation during long-term use. On the basis of removing the internal stress, cutting is performed to ensure that the titanium plate after cutting can still maintain the original curvature, solving the technical problem that the cutting process in the traditional technology easily affects the shape of the plate. Furthermore, welding titanium screws at the predetermined position of the titanium plate can facilitate the subsequent assembly with the anode tank. Welding edge strips at both ends of the titanium plate in the length direction can effectively increase the edge strength and durability of the titanium plate. Then, sandblasting and grinding the titanium plate can effectively increase the roughness of the titanium plate surface, thereby helping to improve the adhesion and corrosion resistance of the subsequent electrolysis process. Then, the roughened titanium plate is subjected to secondary annealing to further eliminate internal stress, which is not only conducive to ensuring stability during subsequent use, but also to avoiding deformation of the anode plate during subsequent local shaping, so that the subsequent anode plate can have a good fit rate during use, which can effectively improve the quality of copper foil products. The method has a simple implementation process, good molding effect, and high molding efficiency. It can prepare an anode plate with good stability and high fit rate, which is conducive to ensuring the production quality of copper foil. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 is a flow chart of the present invention; Figure 2 It is a structural schematic diagram of the present invention using a rolling machine to roll a titanium plate; Figure 3 It is a schematic structural diagram of fitting the titanium plate onto the anode support fixture in the present invention.
[0015] In the figure: 1. bottom template, 2. titanium plate, 3. rolling machine, 4. anode plate supporting tooling, 5. pressing plate. DETAILED DESCRIPTION
[0016] The present invention will be further described below in conjunction with the accompanying drawings.
[0017] like Figures 1 to 3 As shown, the present invention provides an anode plate forming method, comprising the following steps: Step 1: Rolling the plate; The titanium plate is cut into a desired size and shape and then placed in a rolling machine 3, where it is rolled to form a titanium plate 2 with a desired curvature; Step 2: Finalize; The rolled titanium plate 2 is pressed and fixed on the anode support fixture 4 by using a pressing plate 5; Step 3: annealing; The fixed titanium plate 2 and the anode support fixture 4 are placed in an annealing furnace for annealing treatment for 2 hours, and then taken out after cooling in the furnace; As a preferred embodiment, the annealing temperature is controlled between 540°C and 560°C; Step 4: Cutting; The cooled titanium plate 2 and the anode support fixture 4 are fixed to the boring machine by using a fixing fixture, and the centering and positioning operation is performed, and then the titanium plate 2 is cut by an end mill to cut the titanium plate 2 into a required shape; Step 5: Welding accessories; The titanium screws are fixedly connected to the predetermined positions of the anode plates by welding so as to facilitate the subsequent assembly with the anode tank; the edge strips are fixedly connected at both ends of the length direction of the anode plates by welding; Step 6: Sandblasting and polishing; The titanium plate 2 is fixed on the sandblasting and grinding tooling, and a spraying area is demarcated on the titanium plate 2, and then the spraying area is sandblasted, and the sandblasting roughness reaches a set value, and the surface is polished after the sandblasting is completed; as a further preferred embodiment, the uniformity of the sandblasting needs to be ensured during the sandblasting process; Step 7: secondary annealing; Put the titanium plate 2 together with the sandblasting and grinding tooling into a desktop furnace for annealing treatment, keep warm for 2 hours, and take it out after cooling in the furnace; As a preferred embodiment, the annealing temperature is controlled between 540°C and 560°C; Step 8: Plastic surgery; Performing shaping treatment on a part of the titanium plate 2 after the secondary annealing treatment; Step 9: Inspection; Fix the titanium plate 2 on the inspection fixture to check the arc fitting rate of the titanium plate 2; Step 10: spraying; A noble metal coating is sprayed on the titanium plate 2 that has passed the inspection to obtain the required anode plate.
[0018] In order to ensure that the titanium plate 2 with the required curvature can be formed quickly and with high quality after the rolling process, in step one, during the rolling process, a bottom template 1 with the required curvature is placed under the titanium plate 2, and the bottom template 1 is used to ensure that the titanium plate 2 after treatment forms the required curvature.
[0019] As a preference, in step 1, the rolling machine 3 is a three-roller rolling machine or a four-roller rolling machine. When a four-roller rolling machine is used, the bottom template 1 is not required during the rolling process.
[0020] In order to prevent the defective roller surface from damaging the surface of the titanium plate and effectively ensure the preparation quality of the anode plate, in step 1, before the titanium plate 2 is placed in the rolling machine 3, the rolling machine 3 is first cleaned, each roller surface is cleaned, and then each roller surface is checked for defects that affect the rolling effect. If there are defects, the defective roller is replaced in time. As a further preferred embodiment, foreign matter and oil on the roller surface are cleaned in the process of cleaning each roller surface.
[0021] In order to ensure the preparation quality of the anode plate, in step 1, each roller surface in the rolling machine 3 is coated with a disposable wrapping film.
[0022] In order to effectively prevent the titanium plate from being oxidized during the heating and cooling process, in step 2, argon gas is first filled into the titanium plate to form a protective atmosphere before the annealing treatment.
[0023] As a preferred embodiment, in step five, the welding operation is performed by laser welding.
[0024] As a preferred embodiment, in step six, a nitrile rubber skin is used to protect the exposed parts of the sandblasting tooling and the exposed parts of the titanium plate 2 outside the spraying area; the set value is 120μm.
[0025] In order to effectively prevent the titanium plate from being oxidized during the heating and cooling process, in step seven, argon gas is first filled into the titanium plate to form a protective atmosphere before the annealing treatment.
[0026] In order to accurately and efficiently detect the bonding rate, in step nine, the process of testing the arc bonding rate of the titanium plate 2 is as follows: S91: coating red lead powder on the titanium plate 2 or on the inspection tool; S92: Use bolts to fix and press the titanium plate 2 onto the inspection fixture; S93: Remove the bolts and separate the titanium plate 2 and the inspection fixture; S94: Calculate the bonding rate according to the ratio of the area of the inspection tooling covered with red lead powder to the area of the titanium plate 2 coated with red lead powder, or according to the ratio of the area of the titanium plate 2 covered with red lead powder to the area of the inspection tooling covered with red lead powder, and ensure that the bonding rate is not less than 95%.
[0027] In the present invention, firstly, the titanium plate is rolled by a rolling machine, which can facilitate the rapid and high-quality rolling of the titanium plate into a plate of the required curvature, effectively solving the technical problem that the traditional technology uses a pressing method for shaping, which takes a long time and the pressing effect is not ideal. Secondly, the titanium plate with a curvature is pressed tightly on the anode support tooling, and then annealed together, which can effectively eliminate the internal stress of the titanium plate after the curvature is formed, thereby ensuring that the titanium plate can stably maintain a specific shape without deformation during long-term use. On the basis of removing the internal stress, cutting is performed to ensure that the titanium plate after cutting can still maintain the original curvature, solving the technical problem that the cutting process in the traditional technology easily affects the shape of the plate. Furthermore, welding titanium screws at the predetermined position of the titanium plate can facilitate the subsequent assembly with the anode tank. Welding edge strips at both ends of the titanium plate in the length direction can effectively increase the edge strength and durability of the titanium plate. Then, sandblasting and grinding the titanium plate can effectively increase the roughness of the titanium plate surface, thereby helping to improve the adhesion and corrosion resistance of the subsequent electrolysis process. Then, the roughened titanium plate is subjected to secondary annealing to further eliminate internal stress, which is not only conducive to ensuring stability during subsequent use, but also to avoiding deformation of the anode plate during subsequent local shaping, so that the subsequent anode plate can have a good fit rate during use, which can effectively improve the quality of copper foil products. The method has a simple implementation process, good molding effect, and high molding efficiency. It can prepare an anode plate with good stability and high fit rate, which is conducive to ensuring the production quality of copper foil.
Claims
1. A method for forming an anode plate, characterized in that: The following steps are involved: Step 1: Rolling the plate; The titanium plate (2) is cut into a desired size and shape and then placed in a rolling machine (3), and the rolling machine (3) is used to roll the titanium plate (2) to form a titanium plate (2) with a desired curvature; Step 2: Finalize; The rolled titanium plate (2) is pressed and fixed on the anode support fixture (4) by using a pressing plate (5); Step 3: annealing; The fixed titanium plate (2) and the anode support fixture (4) are placed together in an annealing furnace for annealing treatment, with a holding time of 2 hours, and then taken out after cooling in the furnace; Step 4: Cutting; The cooled titanium plate (2) and the anode support fixture (4) are fixed together on a boring machine using a fixing fixture, and a centering and positioning operation is performed, and then the titanium plate (2) is cut using an end mill to cut the titanium plate (2) into a desired shape; Step 5: Welding accessories; The titanium screw is fixedly connected to a predetermined position of the titanium plate (2) by welding; and the side strips are fixedly connected at both ends of the titanium plate (2) in the length direction by welding; Step 6: Sandblasting and polishing; Fixing the titanium plate (2) on a sandblasting and grinding tool, demarcating a spraying area on the titanium plate (2), and then sandblasting the spraying area to make the sandblasting roughness reach a set value, and performing surface grinding after the sandblasting is completed; Step 7: secondary annealing; The titanium plate (2) together with the sandblasting and grinding tool is placed in a furnace for annealing treatment, and the heat preservation time is 2 hours. After cooling in the furnace, it is taken out; Step 8: Plastic surgery; Performing shaping treatment on a part of the titanium plate (2) after the secondary annealing treatment; Step 9: Inspection; Fixing the titanium plate (2) on the inspection fixture to inspect the arc fitting rate of the titanium plate (2); Step 10: spraying; A precious metal coating is sprayed on the titanium plate (2) that has passed the test to obtain the required anode plate.
2. The anode plate forming method according to claim 1, characterized in that: In step one, during the rolling process, a bottom template (1) of a desired curvature is placed under the titanium plate (2), and the bottom template (1) is used to ensure that the titanium plate (2) after the treatment forms the desired curvature.
3. The anode plate forming method according to claim 1, characterized in that: In step one, the rolling machine (3) is a three-roller rolling machine or a four-roller rolling machine.
4. The anode plate forming method according to claim 1, characterized in that: In step 1, before placing the titanium plate (2) into the rolling machine (3), the rolling machine (3) is first cleaned to clean the surfaces of each roller, and then the surfaces of each roller are checked to see if there are any defects that may affect the rolling effect. If there are any defects, the defective rollers are replaced in a timely manner.
5. The anode plate forming method according to claim 1, characterized in that: In step one, each roller surface in the rolling machine (3) is coated with a disposable wrapping film.
6. The anode plate forming method according to claim 1, characterized in that: In step three, the annealing temperature is controlled between 540°C and 560°C.
7. The anode plate forming method according to claim 1, characterized in that: In step five, laser welding is used to perform welding operations.
8. The anode plate forming method according to claim 1, characterized in that: In step six, a nitrile rubber sheet is used to protect the exposed parts of the sandblasting tooling and the exposed parts of the titanium plate (2) outside the spraying area; the setting value is 120 μm.
9. The anode plate forming method according to claim 1, characterized in that: In step seven, before the annealing process, argon gas is first filled to form a protective atmosphere.
10. The anode plate forming method according to claim 1, characterized in that: In step nine, the process of inspecting the arc fitting rate of the titanium plate (2) is as follows: S91: Apply red lead powder on titanium plate or on inspection tooling; S92: Use bolts to fix and press the titanium plate 2 onto the inspection fixture; S93: Remove the bolts and separate the titanium plate 2 and the inspection fixture; S94: Calculate the bonding rate according to the ratio of the area of the inspection tooling covered with red lead powder to the area of the titanium plate 2 coated with red lead powder, or according to the ratio of the area of the titanium plate 2 covered with red lead powder to the area of the inspection tooling covered with red lead powder, and ensure that the bonding rate is not less than 95%.
Citation Information
Patent Citations
Process for continuously rolling pipeline without causing pressure head
CN102430894A
Processing device for metal net-shaped sphere and manufacturing method
CN109570801A
Preparation method for electrolytic copper foil anode plates
CN109735879A
Preparation process of titanium polar plate with firmly attached coating
CN113787311A
Titanium material anode tank structure required by electrolytic copper foil and manufacturing process of titanium material anode tank structure