Rapid low-cost manufacturing method for large-size optical mold
Through the grinding and polishing technology combined with MATLAB and robotic arm small grinding head, the high-end surface quality of large-size optical molds is directly achieved, solving the problems of cumbersome and high cost in traditional processes, achieving an efficient and low-cost manufacturing process, and improving the The mold's resistance to wear and scratches.
Patent Information
- Application Number
- CN202411429622.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-14
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-10-14
AI Technical Summary
The traditional large-size optical mold manufacturing method has cumbersome processes, high cost and low efficiency. The nickel-phosphorus modified mold surface has poor wear and scratch resistance, which cannot meet the accuracy and surface quality requirements of high-end optical components.
MATLAB is used for point coordinate extraction and Zenik polynomial fitting, a three-coordinate detection path is designed, and a robotic arm small grinding head is used for grinding and polishing, which directly achieves the required surface shape accuracy and surface roughness, and omits the nickel-phosphorus modification process. Using diamond powder and alumina abrasives of different particle sizes, the surface quality is improved through the coarse and fine polishing stages.
Simplify the manufacturing process, improve manufacturing efficiency, reduce manufacturing costs, extend the service life of the mold, improve the anti-wear and scratch resistance of the mold steel substrate surface, and achieve the surface roughness and surface shape accuracy of high-end optical molds.
Smart Images

Figure CN119077446A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of advanced optical manufacturing technology, and in particular to a method for rapidly and low-cost manufacturing of a large-size optical mold. Background Art
[0002] Large-size optical molds are used to produce a variety of high-precision optical components, such as lenses, prisms, car HUDs, and optical instruments. These components are widely used in consumer electronics, automobiles, medical and communications, and their manufacturing accuracy directly affects the final performance of the product. Large-size high-end optical molds need to achieve extremely high surface roughness and surface accuracy. The traditional manufacturing method is machine tool milling, followed by manual grinding and polishing. This manual grinding and polishing process has a long manufacturing cycle, high cost, and poor process consistency.
[0003] With the advancement of technology, CNC machining (CNC) and electrical discharge machining (EDM) have become the mainstream optical mold manufacturing technologies. However, the above two processing technologies have shortcomings in the manufacturing of large-scale high-end optical molds: CNC machining (CNC) and electrical discharge machining (EDM) equipment investment is large, processing efficiency is low, and the technical level of operators is high. At the same time, the traditional machine tool milling processing is affected by process errors, and the precision and surface quality of the processed molds cannot directly meet the use requirements, and cannot directly achieve the final surface roughness and surface shape accuracy of the optical mold. It is necessary to nickel-phosphorus modify the surface after processing, and then obtain the final surface roughness and surface shape accuracy through single-point diamond turning (SPDT) and manual grinding and polishing. The specific steps include: first, use different numbers of oilstones for rough grinding, and then use multiple types of sandpaper for fine grinding after reaching a certain accuracy, and then use different types of grinding paste and polishing paste for polishing, and finally perform nickel-phosphorus modification after reaching a certain accuracy. The process is cumbersome, the cost is high, the manufacturing efficiency is low, it is highly dependent on manual experience, and the wear and scratch resistance of the nickel-phosphorus modified surface is poor. Summary of the invention
[0004] The present invention aims to solve the technical problems in the prior art and provide a method for rapidly and low-cost manufacturing of large-size optical molds.
[0005] In order to solve the above technical problems, the technical solutions of the present invention are as follows:
[0006] A method for rapidly and cheaply manufacturing a large-size optical mold comprises the following steps:
[0007] Step i: Obtain the processing digital model of the mold;
[0008] MATLAB is used to extract point coordinates, and the Zernike polynomial is used to fit the mold's surface shape. A three-coordinate detection path is generated based on the fitted theoretical surface shape to obtain the mold's surface shape error data. Based on the three-coordinate detection results and the position of the processing optical elements, the processing path of the processing equipment is designed;
[0009] Step ii: grinding;
[0010] Grind the mold steel surface to a roughness of less than 100nm and a surface accuracy PV value of less than 2μm;
[0011] Step iii: polishing;
[0012] First, the rough polishing stage is used to roughly polish the mold steel surface to a roughness of less than 20 nm and no scratches on the surface;
[0013] Then, in the fine polishing stage, the mold steel surface is finely polished to: the roughness is better than 5nm, the surface accuracy PV value is less than 1μm, and there are no scratches on the surface.
[0014] In the above technical solution, in step ii, the air pressure during grinding is 0.15 MPa and the spindle speed is 300 r / min.
[0015] In the above technical solution, in step ii, the grinding pad is polishing leather and the abrasive is 14-18 micron diamond powder.
[0016] In the above technical solution, in step iii, the abrasive in the rough polishing stage is 3 micron aluminum oxide polishing paste.
[0017] In the above technical solution, in step iii, the abrasive in the fine polishing stage is 0.05 micron aluminum oxide polishing paste.
[0018] In the above technical solution, in step iii, the polishing pressure in the rough polishing stage is 0.1 MPa and the rotation speed is 250 r / min.
[0019] In the above technical solution, in step iii, the polishing pressure in the fine polishing stage is 0.06 MPa and the rotation speed is 200 r / min.
[0020] The present invention has the following beneficial effects:
[0021] The invention discloses a fast and low-cost manufacturing method for large-size optical molds. The optical mold with mold steel as the base material is directly processed to the required surface accuracy and surface roughness by a small grinding head of a mechanical arm. The process steps such as surface nickel-phosphorus modification, single-point diamond turning, and manual grinding and polishing are not required, which simplifies the manufacturing process and improves manufacturing efficiency. Compared with the optical surface modified with nickel-phosphorus, the optical surface of the mold steel base has stronger resistance to wear and scratches, which prolongs the service life of the mold and reduces the manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments.
[0023] Figure 1 This is a schematic diagram of the overall structure of the small grinding head robot processing.
[0024] Figure 2 Schematic diagram of the polishing disc.
[0025] Figure 3 Schematic diagram of the high-end optical mold manufacturing process.
[0026] Figure 4 Schematic diagram of the roughness results after grinding.
[0027] Figure 5 Schematic diagram of the roughness results after polishing. DETAILED DESCRIPTION
[0028] The inventive concept of the present invention is:
[0029] The invention discloses a fast and low-cost method for manufacturing large-size optical molds. A small grinding head of a robotic arm is used as a processing tool system to grind and polish the surface of a mold steel roughly formed by CNC processing. The surface shape error is fed back through contour detection. The required accuracy requirement can be directly achieved by replacing different polishing liquids. The nickel-phosphorus modification process is omitted, the manufacturing cost is reduced, and the service life of the mold is increased.
[0030] The fast and low-cost manufacturing method for large-size optical molds of the present invention uses the surface shape error obtained by contour detection as a processing input, and directly processes the mold steel surface to the required surface quality and surface shape accuracy through grinding, rough polishing and fine polishing.
[0031] The large-size optical mold rapid and low-cost manufacturing method of the present invention directly achieves the mirror surface quality and roughness index by polishing the mold steel without nickel-phosphorus surface modification.
[0032] The present invention is described in detail below with reference to the accompanying drawings.
[0033] The system applicable to the large-size optical mold rapid and low-cost manufacturing method of the present invention includes: a six-degree-of-freedom industrial robot, a small grinding head polishing module, a polishing tool, an abrasive and a white light roughness meter. The six-degree-of-freedom robot is low in cost and flexible in operation, and can meet the processing of complex surface molds. Its structure is as follows Figure 1 As shown in the figure, the small grinding head polishing module is integrated at the end of the six-degree-of-freedom industrial robot spindle. The polishing tool is connected to the end of the small grinding head polishing module.
[0034] The polishing tool is divided into three parts, from top to bottom: polishing pad, asphalt layer and base. The base is made of aluminum alloy, the asphalt layer is the polishing asphalt commonly used in processing reflectors, and the polishing pad is made of different types of polishing leather or flannel, such as Figure 2 shown.
[0035] Abrasives include: diamond powder and aluminum oxide abrasives of different particle sizes, which are used for grinding and polishing respectively. White light roughness meter is mainly used to measure the roughness of optical mold surface.
[0036] The large-size optical mold rapid and low-cost manufacturing method of the present invention is as follows: Figure 3 As shown, the following steps are included:
[0037] Step i: Obtain the processing digital model of the mold.
[0038] MATLAB is used to extract point coordinates, and the Zernike polynomials are used to fit the surface shape of the mold. A three-coordinate detection path is generated according to the fitted theoretical surface shape to obtain the surface error data of the mold. Based on the three-coordinate detection results and the position of the processing optical elements, the processing path of the processing equipment is designed.
[0039] Step ii: Grinding.
[0040] The grinding process involves the production of a polishing disc, which is to stick a layer of grinding pad on the asphalt layer of the polishing tool. The grinding pad is made of polishing leather and the abrasive is 14-18 micron diamond powder.
[0041] The entire grinding process includes: coarse grinding stage and fine grinding stage.
[0042] The air pressure in the rough grinding stage was 0.15 MPa and the spindle speed was 300 r / min.
[0043] After the mold steel surface reaches the surface accuracy, fine grinding is carried out. The fine grinding stage also uses an asphalt polishing disc and a grinding pad, the air pressure is also 0.15MPa, and the rotation speed is 300r / min.
[0044] The entire grinding process is repeated until the optical mold surface reaches the accuracy that can be polished. The roughness of the mold steel surface after grinding is less than 100nm, and the surface accuracy PV value is less than 2μm. Figure 4 shown.
[0045] Step iii: Polishing is performed.
[0046] The polishing process is similar to the grinding process, and also uses an asphalt polishing disc, but the difference from the grinding stage is that the polishing pad uses flannel cloth and the abrasive uses aluminum oxide.
[0047] The entire polishing process includes: rough polishing stage and fine polishing stage.
[0048] During the rough polishing stage, the abrasive used was 3 micron aluminum oxide polishing paste, the polishing pressure was 0.1 MPa, and the speed was 250 r / min. After rough polishing, the surface roughness of the mold steel was less than 20 nm, and there were no scratches on the surface, and then fine polishing was performed.
[0049] The fine polishing stage also uses a combination of asphalt polishing disc and flannel cloth, but the abrasive uses a finer 0.05 micron aluminum oxide polishing paste, the polishing pressure is 0.06MPa, and the speed is 200r / min. After fine polishing, the roughness is better than 5nm, the surface accuracy PV value is less than 1μm, and there are no scratches on the surface. Figure 5 As shown, the mold steel surface at this time meets the precision requirements of high-end optical molds, and the mold molding process can be carried out.
[0050] Experiments have shown that the fast and low-cost manufacturing method for large-size optical molds of the present invention is effective and can obtain the surface roughness and surface quality required by the mold.
[0051] The fast and low-cost manufacturing method for large-size optical molds of the present invention is not only limited to the fast and low-cost manufacturing of large-size high-end optical molds, but is also applicable to the high-precision and high-surface quality processing of optical components with other mold steel materials as the base.
[0052] The invention discloses a fast and low-cost manufacturing method for large-size optical molds. The optical mold with mold steel as the base material is directly processed to the required surface accuracy and surface roughness by a small grinding head of a mechanical arm. The process steps such as surface nickel-phosphorus modification, single-point diamond turning, and manual grinding and polishing are not required, which simplifies the manufacturing process and improves manufacturing efficiency. Compared with the optical surface modified with nickel-phosphorus, the optical surface of the mold steel base has stronger resistance to wear and scratches, which prolongs the service life of the mold and reduces the manufacturing cost.
[0053] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the present invention.
Claims
1. A method for rapidly and cheaply manufacturing a large-size optical mold, characterized in that: The following steps are involved: Step i: Obtain the processing digital model of the mold; MATLAB is used to extract point coordinates, and the Zernike polynomial is used to fit the mold surface shape. A three-coordinate detection path is generated based on the fitted theoretical surface shape to obtain the mold surface shape error data. Based on the three-coordinate detection results and the position of the processing optical elements, the processing path of the processing equipment is designed. Step ii: grinding; Grind the mold steel surface to a roughness of less than 100nm and a surface accuracy PV value of less than 2μm; Step iii: polishing; First, the rough polishing stage is used to roughly polish the mold steel surface to a roughness of less than 20 nm and no scratches on the surface; Then, in the fine polishing stage, the mold steel surface is finely polished to: the roughness is better than 5nm, the surface accuracy PV value is less than 1μm, and there are no scratches on the surface.
2. The method for rapid and low-cost manufacturing of large-size optical molds according to claim 1, characterized in that: In step ii, the air pressure during grinding is 0.15 MPa and the spindle speed is 300 r / min.
3. The method for rapid and low-cost manufacturing of large-size optical molds according to claim 1, characterized in that: In step ii, the grinding pad is polishing leather, and the abrasive is 14-18 micron diamond powder.
4. The method for rapid and low-cost manufacturing of large-size optical molds according to claim 1, characterized in that: In step iii, the abrasive in the rough polishing stage is 3 micron aluminum oxide polishing paste.
5. The method for rapid and low-cost manufacturing of large-size optical molds according to claim 1, characterized in that: In step iii, the abrasive used in the fine polishing stage is 0.05 micron aluminum oxide polishing paste.
6. The method for rapid and low-cost manufacturing of large-size optical molds according to claim 1, characterized in that: In step iii, the polishing pressure in the rough polishing stage is 0.1 MPa and the rotation speed is 250 r / min.
7. The method for rapid and low-cost manufacturing of large-size optical molds according to claim 1, characterized in that: In step iii, the polishing pressure in the fine polishing stage is 0.06 MPa and the rotation speed is 200 r / min.
Citation Information
Patent Citations
Method for detecting large-caliber aspheric optical element by utilizing three-coordinate measuring machine
CN101943559A
Tool polishing method
CN104227511A
Large-aperture plane machining method by combining numerical control small tool and annular polishing machine
CN104385064A
System for precise grinding of large-diameter off-axis aspherical mirror
CN105965349A
Combination machining method of complex curved surface
CN106826400A