Tension-adjustable dipping mold and dipping method
By adjusting the fiber tension and resin melt feed flow in the impregnation mold, the problems of fiber impregnation are solved, and uniform coating and stable impregnation between fibers and resins are achieved, and production efficiency and product quality are improved.
Patent Information
- Application Number
- CN202411190543.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-08-28
AI Technical Summary
In the prior art, fiber tension adjustment is not flexible enough during the impregnation process of long fiber reinforced thermoplastic materials, resulting in uneven fiber impregnation and fiber fracture problems, affecting production efficiency and product quality.
Design an impregnated mold with adjustable tension, through the combination of multiple cavity and elliptical cylindrical rollers, adjust the tension of the fibers in the mold and the feed flow of the resin melt to ensure that the fibers are subjected to appropriate tension and sufficient coverage in different areas. , thereby improving the impregnation effect.
It effectively avoids the impregnation effect caused by too little fiber tension and fiber breakage caused by too much tension, achieves uniform coating and stable impregnation between fiber and resin, and improves production efficiency and product quality.
Smart Images

Figure CN119078231A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of composite material molding, and more specifically to a tension-adjustable impregnation mold and an impregnation method. Background Art
[0002] Long fiber reinforced thermoplastic materials (LFT) and prepreg composite tapes are highly valued in the field of lightweight automobiles due to their excellent mechanical properties and cost-effectiveness. The light and high-strength material properties help to ensure the range of energy vehicles and are widely used in battery covers, power battery bottom guards, instrument panel frames, door substrates and other parts. At present, the production process of LFT materials is mainly based on pultrusion technology. The effect of fiber impregnation is greatly affected by the equipment, and uneven fiber impregnation often occurs, which is specifically manifested in particle explosion and excessive single free fiber hairiness.
[0003] Chinese patent CN106903906A discloses a continuous fiber reinforced thermoplastic resin melt impregnation mold and preparation method, which consists of a dispersion roller and a slit roller. The slit roller is rotatable, so the coating angle of the fiber bundle melt impregnation can be changed by the rotation of the slit roller, and the tension of the fiber bundle in the mold can be changed; by combining the dispersion roller and the slit roller, the fibers are fully dispersed and fully impregnated through the slit flow channel. Although the tension of the fiber bundle can be adjusted by the rotation of the slit roller in the above scheme, the above scheme only feeds through one feed port. At a position with greater tension, if faster concentrated feeding is used, uneven impregnation may occur, affecting the impregnation effect of the product; in addition, using faster concentrated feeding will also produce concentrated melt resistance on the fiber, which is prone to fiber breakage and affects production efficiency. Summary of the invention
[0004] The purpose of the present invention is to overcome the deficiencies in the prior art and provide a tension-adjustable impregnation mold and impregnation method, which can not only adjust the fiber tension, but also adjust the feeding flow of the resin melt in different areas according to the tension, thereby effectively improving the product impregnation effect.
[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is:
[0006] Provided is a tension-adjustable impregnation mold, comprising an upper mold plate, a lower mold plate, and a mold cavity formed around the upper mold plate and the lower mold plate, wherein both ends of the mold cavity are respectively provided with a fiber feed port and a discharge port, and the mold cavity comprises a plurality of cavities connected in end-to-end sequence, each cavity is provided with an impregnation roller rotatably adjusting the fiber tension, and each cavity is connected with a melt feed port for feeding a resin melt, wherein the fiber enters from the fiber feed port, bypasses the periphery of each impregnation roller, is impregnated with the resin melt in the cavity, and then is discharged from the discharge port.
[0007] The tension-adjustable impregnation mold of the present invention, the fibers enter from the fiber feed port, bypass the periphery of each impregnation roller, and are impregnated with the resin melt in the cavity before being led out from the discharge port; the resin melt is fed into the cavity from the melt feed port, and impregnates the fibers in the cavity, which is suitable for preparing fiber-reinforced resin composite materials. In the present invention, the impregnation rollers in each cavity can rotate to adjust the tension on the fibers in the cavity, to avoid too small tension, too small contact area between the fibers and the resin melt, resulting in poor impregnation effect, and to avoid excessive tension causing fiber breakage; in addition, in the present invention, each cavity is provided with a melt feed port, and the resin melt is fed from different positions, and the fibers are repeatedly impregnated with multiple feeding stages to achieve better coating of the fibers with the resin melt, and obtain a better impregnation effect.
[0008] Furthermore, the tension generated by the impregnation roller in the first cavity and the tension generated by the impregnation roller in the last cavity are less than the tension generated by any impregnation roller in the middle position; the feeding flow rate of the melt feed port of the first cavity and the feeding flow rate of the melt feed port of the last cavity are greater than the feeding flow rate of the melt feed port of any cavity in the middle position. By setting the tension in a sequence of small, large, and small, the fiber is not easy to break under the action of small tension when entering the mold. After passing through a cavity, when the surface temperature of the fiber rises to a temperature that is easier to be impregnated with the resin melt, the tension is increased to improve the impregnation effect; finally, the cavity at the end stably impregnates the fiber bundle with small tension, and finally obtains a stably impregnated material strip; according to the principle of large tension and small feeding, when the fiber tension in the first cavity and the last cavity is relatively small, a relatively large feeding flow rate is set to help the resin melt fully cover the fiber surface; and when the fiber tension in the cavity in the middle position is large, a correspondingly small feeding flow rate is set to avoid concentrated melt resistance and fiber breakage.
[0009] Furthermore, the tension of the impregnation roller on the fiber in the first cavity is not greater than the tension of the impregnation roller on the fiber in the last cavity, and the feeding flow rate of the melt feed port of the first cavity is not less than the feeding flow rate of the melt feed port of the last cavity. When the fiber in the first cavity enters the mold, it is not easy to break under the action of small tension, and in the last cavity, since the fiber has been partially impregnated with resin melt in the cavity before the last cavity, a smaller feeding flow rate can be used in the last cavity to achieve uniform impregnation.
[0010] Furthermore, the number of the cavities is 2N-1, where N≥2 and N is a positive integer; the tension exerted on the fiber by the impregnation roller in each cavity is recorded as F 1 、F 2 ……F N 、F N+1 ……F 2N-1 , then, F 1 <F 2 <F 3 <…… <FN , F 2N-1 <F 2N-2 <F 2N-3 <…… <F N ; The feeding flow rate in each cavity is recorded as Q 1 , Q 2 ...Q N , Q N+1 ...Q 2N-1 , then, Q 1 >Q 2 >Q 3 >……>Q N , Q 2N-1 >Q 2N-2 >Q 2N-3 >……>Q N From the first cavity to the last cavity, the tension first increases gradually and then decreases gradually, the feeding flow first decreases gradually and then increases gradually, the tension and feeding flow both change gradually, and the changing trends of the tension and feeding flow are opposite, and the two factors cooperate with each other to obtain a better impregnation effect.
[0011] Furthermore, the upper template is provided with a plurality of first corrugated surfaces, the lower template is provided with a plurality of second corrugated surfaces symmetrically arranged with the first corrugated surfaces, the cavity is formed between the first corrugated surface and the second corrugated surface, the minimum distance between the first corrugated surface and the second corrugated surface is D1, the maximum distance between the first corrugated surface and the second corrugated surface is D2, and along the direction from the fiber feed port to the discharge port, the distance between the first corrugated surface and the second corrugated surface gradually increases from D1 to D2, and then gradually decreases from D2 to D1. This cavity with an arc surface makes the continuously accumulated resin melt fed from the melt feed port flow along the arc surface to both ends, increasing the area of fiber impregnation and improving the impregnation effect.
[0012] Furthermore, the impregnation roller is an elliptical roller, the center of the elliptical roller coincides with the center of the cavity, the short axis diameter of the elliptical roller is greater than the minimum distance between the first corrugated surface and the second corrugated surface, the long axis diameter of the elliptical roller is less than the maximum distance between the first corrugated surface and the second corrugated surface, and the fiber in the mold cavity staggers around the lower end surface of the first corrugated surface and the upper surface of the elliptical roller, or staggers around the upper end surface of the second corrugated surface and the lower surface of the elliptical roller. The rotation of the elliptical roller is used to change the impregnation angle of the fiber to adjust the tension of the fiber. The fiber bundle is mainly divided into two parts, one part staggers around the lower end surface of the first corrugated surface and the upper surface of the elliptical roller, and the other part staggers around the upper end surface of the second corrugated surface and the lower surface of the elliptical roller. The fibers will not stagger with each other, thereby helping to improve the impregnation effect.
[0013] Furthermore, the same cavity is connected to be provided with two groups of melt feed ports, the axes of the two melt feed ports of the same cavity coincide, the axes of the melt feed ports pass through the center of the cavity, and the axes of the melt feed ports are perpendicular to the axes of the fiber feed ports. The impregnation process is analyzed by feeding from the melt feed port at the top, part of the resin melt flowing into the top flows onto the fiber surface, part of it is carried by the fiber to the next cavity for impregnation, so as to maximize the contact area between the melt and the fiber, and part of the resin melt passes through the fiber surface and falls to the other fiber surface through the gap, so as to further impregnate the lower fiber.
[0014] Furthermore, it also includes side guards connected to the upper template and the lower template, and the two ends of the impregnation roller are rotatably connected to the side guards through a rotating shaft, and the rotating shaft is connected to a driving motor. The driving motor can be a driving motor with a button, and the impregnation angle of the impregnation roller can be adjusted by pressing the button.
[0015] Furthermore, a controller is included, a flow valve module is provided at the melt feed port, an identification module for identifying the surface morphology of the product is provided at the discharge port, the identification module is connected to the input end of the controller, and the drive motor and the flow valve module are both connected to the output end of the controller. The surface morphology of the product is identified by the identification module, and for products with problems such as side leakage, pelletizing cracks, and excessive glass fiber hair, the impregnation effect is improved by adjusting the tension and feed amount, thereby achieving real-time adjustment of the tension.
[0016] The present invention also provides an impregnation method, comprising the following steps:
[0017] S10. Pulling the fiber so that the fiber enters from the fiber feed port, bypasses the periphery of each impregnation roller, and is led out from the discharge port;
[0018] S20. Feeding a resin melt into each cavity from each melt feed port, the resin melt enters the cavity and impregnates the fiber in the cavity;
[0019] S30. Observe the product morphology of the composite material at the outlet. If the product surface has a bad morphology, proceed to step S40;
[0020] S40. Rotate the impregnation roller to adjust the tension of the fibers in each cavity: first adjust the impregnation roller in the middle position to increase the tension of the fibers in the middle position, and observe the product morphology of the composite material at the outlet; if the product morphology is qualified, the adjustment is terminated; if the product surface still has a bad morphology, gradually increase the tension of the fibers from the middle position to both ends, observe the product morphology of the composite material at the outlet, and terminate the tension adjustment until there is no bad morphology on the surface;
[0021] S50. Adjust the tension of the fibers in each cavity obtained in step S40 to continuously produce fiber-reinforced resin composite materials.
[0022] The impregnation method of the present invention adjusts the tension of the fibers in each cavity when the product has bad morphology such as white leakage, pelletizing explosion, and fiber burrs, gradually increases the tension of the fibers in each cavity from the middle to the two ends, and observes the morphology of the adjusted product in real time. In the present invention, the tension of the fibers in each cavity can be adjusted, effectively avoiding too small tension, too small contact area between the fibers and the resin melt, resulting in poor impregnation effect, and avoiding excessive tension causing fiber breakage; in addition, the resin melt is fed from the melt feed port at different positions, and the fiber is repeatedly impregnated with multiple feeding stages to achieve better coating of the fiber with the resin melt, and a better impregnation effect can be obtained.
[0023] Preferably, step S40 also includes the step of synchronously adjusting the feeding flow rate of each melt feed port: first adjust the middle position cavity to reduce the feeding flow rate of the middle position cavity, and observe the product morphology of the composite material at the discharge port; if the product morphology is qualified, then end the adjustment; if the product surface still has a bad morphology, then gradually reduce the feeding flow rate of the cavity from the middle position to both ends, observe the product morphology of the composite material at the discharge port, until there is no bad morphology on the surface, then end the adjustment of the feeding flow rate. In the present invention, the synchronous adjustment can be to adjust the feeding flow rate of each cavity after each adjustment of the tension of the fibers in the cavity, or it can be to gradually adjust the feeding flow rate of each cavity from the middle to both ends when there is still a bad morphology after adjusting the tension of the fibers in all cavities.
[0024] Compared with the prior art, the present invention has the following beneficial effects:
[0025] The tension-adjustable impregnation mold and impregnation method of the present invention are capable of adjusting the tension on the fibers in each cavity, thereby preventing the tension from being too small, the contact area between the fibers and the resin melt being too small, and resulting in a poor impregnation effect, while also preventing the tension from being too large and resulting in fiber breakage. In addition, each cavity is provided with a melt feed port, and the resin melt is fed from different positions. Multiple stages of feeding are performed to repeatedly impregnate the fibers, thereby achieving better coating of the fibers by the resin melt, and obtaining a better impregnation effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is a schematic structural diagram of the dipping mold with adjustable tension in Example 1;
[0027] Figure 2 It is a schematic structural diagram of the dipping mold with adjustable tension in Example 2;
[0028] Figure 3 It is a schematic diagram of the installation of the dipping roller of the dipping mold with adjustable tension in Example 3;
[0029] Figure 4 This is a control principle diagram of the controller in Example 3;
[0030] In the attached drawings: 1. upper template; 2. lower template; 3. fiber feed port; 4. discharge port; 5. cavity; 6. impregnation roller; 7. melt feed port; 8. first corrugated surface; 9. second corrugated surface; 10. side stop; 11. rotating shaft; 12. identification module; 13. controller; 14. drive motor. DETAILED DESCRIPTION
[0031] The present invention is further described below in conjunction with specific implementation methods. The accompanying drawings are only used for exemplary descriptions and are only schematic diagrams, not actual drawings, and cannot be understood as limiting this patent; in order to better illustrate the embodiments of the present invention, some parts of the accompanying drawings may be omitted, enlarged or reduced, and do not represent the size of the actual product; for those skilled in the art, it is understandable that some well-known structures and their descriptions in the accompanying drawings may be omitted.
[0032] The same or similar numbers in the drawings of the embodiments of the present invention correspond to the same or similar parts; in the description of the present invention, it should be understood that if the terms "upper", "lower", "left", "right" and the like indicate directions or positional relationships based on the directions or positional relationships shown in the drawings, it is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, the terms describing the positional relationship in the drawings are only used for illustrative purposes and cannot be understood as limitations on this patent. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to specific circumstances.
[0033] Embodiment 1
[0034] like Figure 1 The figure shows a first embodiment of a tension-adjustable impregnation mold of the present invention, which is used for preparing fiber-reinforced resin composite materials; the impregnation mold of this embodiment comprises an upper mold plate 1, a lower mold plate 2 and a mold cavity formed around the upper mold plate 1 and the lower mold plate 2, and a fiber feed port 3 and a discharge port 4 are respectively provided at both ends of the mold cavity, and the mold cavity comprises a plurality of cavities 5 which are connected in end-to-end sequence, and each cavity 5 is provided with an impregnation roller 6 which can rotate to adjust the fiber tension, and each cavity 5 is connected with a melt feed port 7 for feeding resin melt, and the fiber enters from the fiber feed port 3, bypasses the outer periphery of each impregnation roller 6, and is discharged from the discharge port 4 after being impregnated with the resin melt in the cavity 5.
[0035] The fibers are pulled by a pulling device so that the fibers enter from the fiber feed port 3, bypass the outer periphery of each impregnation roller 6, and are led out from the discharge port 4. The pulling device provides power for the movement of the fibers. The fibers bypass each impregnation roller 6 by bypassing the upper surface of each impregnation roller 6, bypassing the lower surface of each impregnation roller 6, or bypassing the upper surface and the lower surface of each impregnation roller 6 alternately in sequence. The fibers bypass each impregnation roller 6 by bypassing the upper surface of each impregnation roller 6, or bypassing the lower surface of each impregnation roller 6. When the fibers bypass each impregnation roller 6 by bypassing the upper surface of each impregnation roller 6, or bypassing the lower surface of each impregnation roller 6, a tensioning roller is required to be used to achieve the tensioning of the fibers. The impregnation roller 6 is an elliptical roller, an eccentric roller, a special-shaped roller, etc., and the distance between the center point of the impregnation roller 6 and the contact point between the fiber and the impregnation roller 6 changes during the rotation process. The greater the distance between the center point of the impregnation roller 6 and the contact point between the fiber and the impregnation roller 6, the greater the tension, and the smaller the distance between the center point of the impregnation roller 6 and the contact point between the fiber and the impregnation roller 6, the smaller the tension; the fibers can be specifically glass fibers, carbon fibers, etc., and the resin is a thermoplastic resin.
[0036] When this embodiment is implemented, the fiber enters from the fiber feed port 3, bypasses the outer periphery of each impregnation roller 6, is impregnated with the resin melt in the cavity 5, and then is led out from the discharge port 4; the resin melt is fed into the cavity 5 from the melt feed port 7, and impregnates the fiber in the cavity 5, thereby obtaining a composite material product. The greater the tension, the more dispersed the fiber bundle is into monofilaments, the larger the contact area with the resin melt, and the better the impregnation effect; but if the tension is too large, the greater the resistance of the fiber through the impregnation mold, the fiber is easy to break, and the broken fiber agglomerates to cause greater fiber passing resistance inside the mold, which eventually leads to fiber breakage and inability to produce continuously. When this embodiment is implemented, the impregnation roller 6 in each cavity 5 can be rotated to adjust the tension on the fiber in the cavity 5, so as to avoid too small tension, too small contact area between the fiber and the resin melt, resulting in poor impregnation effect, and at the same time avoid excessive tension causing fiber breakage; in addition, in the present invention, each cavity 5 is provided with a melt feed port 7, and the resin melt is fed from different positions. Multiple stages of feeding and repeated impregnation of the fiber can achieve better coating of the resin melt on the fiber and obtain a better impregnation effect.
[0037] Specifically, the tension generated by the impregnating roller 6 in the first cavity 5 and the tension generated by the impregnating roller 6 in the last cavity 5 on the fiber are less than the tension generated by any impregnating roller 6 in the middle position on the fiber; the feeding flow rate of the melt feed port 7 in the first cavity 5 and the feeding flow rate of the melt feed port 7 in the last cavity 5 are greater than the feeding flow rate of the melt feed port 7 in any cavity 5 in the middle position. In this embodiment, except for the first and last positions, the other positions are called middle positions. When this embodiment is implemented, the tension is set in the order of small, large and small, so that the fiber is not easy to break under the action of small tension when entering the mold. After passing through a cavity 5, when the surface temperature of the fiber rises to a temperature that makes it easier to impregnate with the resin melt, the tension is increased to improve the impregnation effect; finally, the cavity 5 at the end stably impregnates the fiber bundle with small tension, and finally a stably impregnated material strip is obtained; in addition, according to the principle of large tension and small feeding, when the fiber tension in the first cavity 5 and the last cavity 5 is relatively small, a relatively large feeding flow rate is set to help the resin melt to fully cover the fiber surface; and when the fiber tension in the middle cavity 5 is large, a correspondingly smaller feeding flow rate is set to avoid fiber breakage due to concentrated melt resistance.
[0038] Among them, the tension generated by the impregnation roller 6 on the fiber in the first cavity 5 is not greater than the tension generated by the impregnation roller 6 on the fiber in the last cavity 5, and the feeding flow rate of the melt feed port 7 of the first cavity 5 is not less than the feeding flow rate of the melt feed port 7 of the last cavity 5. The temperature of the fiber in the first cavity 5 is relatively low when entering the mold, and it is not easy to break under the action of small tension. In the last cavity 5, the temperature of the fiber rises, and the tension it can withstand is also relatively large. Therefore, the tension generated by the impregnation roller 6 on the fiber in the last cavity 5 can be greater than the tension generated by the impregnation roller 6 on the fiber in the first cavity 5; in the last cavity 5, since the fiber has been impregnated with part of the resin melt in the cavity 5 before the last cavity 5, a smaller feeding flow rate in the last cavity 5 can achieve uniform impregnation.
[0039] In addition, the number of cavities 5 is 2N-1, where N≥2 and N is a positive integer; the tension exerted by the impregnation roller on the fiber in each cavity is recorded as F 1 、F 2 ……F N 、F N+1 ……F 2N-1 , then, F 1 <F 2 <F 3 <…… <F N , F 2N-1 <F 2N-2 <F 2N-3 <…… <F N ; The feeding flow rate in each cavity is recorded as Q 1 , Q 2 ...Q N , Q N+1 ...Q2N-1 , then, Q 1 >Q 2 >Q 3 >……>Q N , Q 2N-1 >Q 2N-2 >Q 2N-3 >……>Q N From the first cavity 5 to the last cavity 5, the tension first gradually increases and then gradually decreases, the feeding flow first gradually decreases and then gradually increases, the tension and feeding flow both gradually change, and the tension and feeding flow have opposite changing trends, and the two factors cooperate with each other to obtain a better impregnation effect.
[0040] Embodiment 2
[0041] like Figure 2 The figure shows a first embodiment of a tension-adjustable impregnation mold of the present invention, wherein the upper mold plate 1 is provided with a plurality of first corrugated surfaces 8, the lower mold plate 2 is provided with a plurality of second corrugated surfaces 9 symmetrically arranged with the first corrugated surfaces 8, the cavity 5 is formed between the first corrugated surfaces 8 and the second corrugated surfaces 9, the minimum distance between the first corrugated surfaces 8 and the second corrugated surfaces 9 is D1, the maximum distance between the first corrugated surfaces 8 and the second corrugated surfaces 9 is D2, and along the direction from the fiber feed port 3 to the discharge port 4, the distance between the first corrugated surface 8 and the second corrugated surface 9 gradually increases from D1 to D2, and then gradually decreases from D2 to D1. When this embodiment is implemented, the cavity 5 is a cavity 5 set on an arc surface, so that the continuously accumulated resin melt fed from the melt feeding port flows along the arc surface to both ends, increasing the area of fiber impregnation and improving the impregnation effect; the fiber feed port 3 is a bell mouth that is large at first and then small, and the discharge port 4 is a bell mouth that is small at first and then large. The fiber enters through the narrowest part between the first corrugated surface 8 and the second corrugated surface 9 at the fiber feed port 3, and the lower end surface of the first corrugated surface 8 and the upper end surface of the second corrugated surface 9 squeeze the fiber, so that the fiber path changes; the bell mouth at the discharge port 4 has a stabilizing buffering effect on the impregnated product, which helps to improve the quality of the impregnated product.
[0042] Among them, the impregnation roller 6 is an elliptical cylinder roller, the center of the elliptical cylinder roller coincides with the center of the cavity 5, the short axis diameter of the elliptical cylinder roller is greater than the minimum distance between the first corrugated surface 8 and the second corrugated surface 9, and the long axis diameter of the elliptical cylinder roller is less than the maximum distance between the first corrugated surface 8 and the second corrugated surface 9. The fiber in the mold cavity staggers around the lower end surface of the first corrugated surface 8 and the upper surface of the elliptical cylinder roller, or staggers around the upper end surface of the second corrugated surface 9 and the lower surface of the elliptical cylinder roller. In this embodiment, the lower end surface of the first corrugated surface 8 and the upper end surface of the second corrugated surface 9 play the role of the tension roller in the first embodiment. Specifically, when this embodiment is implemented, the rotation of the elliptical roller can change the horizontal passing path of the fiber, so as to realize the pressure effect of the first corrugated surface 8, the second corrugated surface 9 and the elliptical roller on the fiber. When the elliptical roller is rotated, the pressure on the fiber can be changed. The expansion degree of the single filaments of the fiber bundle is different, so different impregnation effects can be achieved. In this way, the fiber bundle in this embodiment is divided into two parts: one part is staggered around the lower end surface of the first corrugated surface 8 and the upper surface of the elliptical roller to form a first fiber surface, and the other part is staggered around the upper end surface of the second corrugated surface 9 and the lower surface of the elliptical roller to form a second fiber surface. The fibers in the two fiber surfaces will not be staggered with each other, which can help improve the impregnation effect.
[0043] Since the fiber surface includes the first fiber surface and the second fiber surface, in this embodiment, the same cavity 5 is connected to be provided with two groups of melt feed ports 7, the axes of the two melt feed ports 7 of the same cavity 5 coincide, the axes of the melt feed ports 7 pass through the center of the cavity 5, and the axes of the melt feed ports 7 are perpendicular to the axes of the fiber feed ports 3. Part of the resin melt fed by the multiple melt feed ports 7 at the top flows to the first fiber surface, part of it is carried by the fiber to the next cavity 5 for impregnation, and part of it flows to the impregnation rear end area to maximize the contact area between the melt and the fiber, and part of the resin melt passes through the first fiber surface and falls to the second fiber surface through the gap to impregnate the fibers on the second fiber surface; part of the resin melt fed by the multiple melt feed ports 7 at the bottom flows to the second fiber surface, part of it is carried by the fiber to the next cavity 5 for impregnation, and part of it flows to the impregnation rear end area to maximize the contact area between the melt and the fiber, and part of the resin melt passes through the second fiber surface and flows to the first fiber surface through the gap to impregnate the fibers on the first fiber surface. Thereby, the impregnation area of the fiber by the resin melt can be increased, and the impregnation effect can be improved.
[0044] Embodiment 3
[0045] like Figure 3 to Figure 4The third embodiment of the dipping mold with adjustable tension of the present invention is shown, which further includes side guards 10 connected to the upper mold plate 1 and the lower mold plate 2. Both ends of the dipping roller 6 are rotatably connected to the side guards 10 through a rotating shaft 11, and the rotating shaft 11 is connected to a driving motor 14. The driving motor 14 can be a driving motor 14 with a button, and the dipping angle of the dipping roller 6 can be adjusted by pressing the button. This operation can be adjusted based on the experience of the operator.
[0046] In order to achieve real-time adjustment of tension, the impregnation mold of this embodiment also includes a controller 13, a flow valve module is provided at the melt feed port 7, and an identification module 12 for identifying the surface morphology of the product is provided at the discharge port 4. The identification module 12 is connected to the input end of the controller 13, and the drive motor 14 and the flow valve module are both connected to the output end of the controller 13.
[0047] The recognition module 12 recognizes the surface morphology of the product. For products with problems such as side leakage, pellet bursting, and fiber burrs, the recognition module 12 can specifically use image recognition; if it is recognized that there are bad morphologies such as side leakage, pellet bursting, and fiber burrs, a signal is transmitted to the controller 13, and the controller 13 improves the impregnation effect by adjusting the tension and feed amount, thereby achieving real-time adjustment of the tension. However, it should be noted that no matter how the tension and feed flow are adjusted, the following rules must still be met: The tension generated by the impregnation roller 6 on the fiber in each cavity 5 meets the following rules: F 1 <F 2 <F 3 <…… <F N , F 2N-1 <F 2N-2 <F 2N-3 <…… <F N ; The feeding flow rate in each cavity 5 satisfies the following rules: Q 1 >Q 2 >Q 3 >……>Q N , Q 2N-1 >Q 2N-2 >Q 2N-3 >……>Q N .
[0048] Embodiment 4
[0049] This embodiment is an embodiment of the impregnation method, which is implemented based on the tension-adjustable impregnation mold of any one of the embodiments 1 to 3, and includes the following steps:
[0050] S10. The fibers are pulled so that they enter from the fiber feed port 3, bypass the periphery of each impregnation roller 6, and are led out from the discharge port 4;
[0051] S20. The resin melt is fed into each cavity 5 from each melt feed port 7, and the resin melt enters the cavity 5 and impregnates the fiber in the cavity 5;
[0052] S30. Observe the product morphology of the composite material at the discharge port 4. If the product surface has an undesirable morphology, proceed to step S40; in this embodiment, the undesirable morphology includes white leakage, pelletizing explosion, fiber burr and other morphologies. Of course, other undesirable morphologies can also be set according to actual conditions;
[0053] S40. Rotate the impregnation roller 6 to adjust the tension of the fibers in each cavity 5: first adjust the impregnation roller 6 in the middle position to increase the tension of the fibers in the middle position, and observe the product morphology of the composite material at the discharge port 4; if the product morphology is qualified, the adjustment is terminated; if the product surface still has a bad morphology, gradually increase the tension of the fibers from the middle position to both ends, observe the product morphology of the composite material at the discharge port 4, until there is no bad morphology on the surface, and then end the tension adjustment;
[0054] S50. The tension of the fibers in each cavity 5 is adjusted according to step S40 to continuously produce fiber-reinforced resin composite materials.
[0055] In step S30, the product morphology may be observed by the operator's eyes or by a visual recognition system.
[0056] In step S40, the tension of the fiber is gradually increased from the middle position to both ends. The specific adjustment method is as follows, taking the dipping roller 6 as an odd number (2N-1) dipping rollers 6 and the maximum tension of each dipping roller 6 as T as an example: first adjust the tension of the Nth dipping roller 6, adjust the tension of the Nth dipping roller 6 to the maximum, and observe the product morphology; if the product surface has a bad morphology, increase the tension of the two dipping rollers 6 on both sides of the Nth dipping roller 6, that is, increase the tension of the N-1th dipping roller 6 and the N+1th dipping roller 6, such as increasing it to 0.9T; observe the product morphology, if the product surface has a bad morphology, increase the tension of the N-2th dipping roller 6 and the N+2th dipping roller 6, such as increasing it to 0.8T; adjust in sequence until the product surface has no bad morphology. In the process of adjusting the tension of the dipping roller 6, no matter how it is adjusted, the following rules should be met: F 1 <F 2 <F 3 <…… <F N , F 2N-1 <F 2N-2 <F 2N-3 <…… <F N .
[0057] In step S40, in addition to the tension adjustment, it may also include the step of synchronously adjusting the feeding flow of each melt feed port: first adjust the middle position cavity 5 to reduce the feeding flow of the middle position cavity 5, and observe the product morphology of the composite material at the outlet 4; if the product morphology is qualified, then end the adjustment; if there is still a bad morphology on the product surface, then gradually reduce the feeding flow of the cavity 5 from the middle position to both ends, observe the product morphology of the composite material at the outlet 4, until there is no bad morphology on the surface, then end the feeding flow adjustment. The synchronous adjustment in this embodiment can be to adjust the feeding flow of the cavity 5 after each adjustment of the tension of the fibers in each cavity 5, or it can be to gradually adjust the feeding flow of each cavity 5 from the middle to both ends when there is still a bad morphology after adjusting the tension of the fibers in all cavities 5. Specifically:
[0058] In the process of adjusting the tension, the feeding flow rate of each melt feed port 7 can be adjusted synchronously. However, no matter how the feeding flow rate is adjusted, the feeding flow rate in each cavity 5 should satisfy the following rule: Q 1 >Q 2 >Q 3 >……>Q N , Q 2N-1 >Q 2N-2 >Q 2N-3 >……>Q N , to meet the principle of high tension and low feed. For example, when increasing the tension of a certain impregnation roller 6, the feed flow rate of the cavity 5 can be reduced until the product morphology of the composite material at the outlet 4 is qualified. If the tension of each impregnation roller 6 is adjusted to the upper limit tension of each impregnation roller 6, if the product surface still has a bad morphology, you can consider appropriately increasing the feed flow rate of each melt feed port 7, for example, the feed flow rate of each melt feed port 7 is increased by 5%, as long as the adjusted tension and feed flow rate still meet the above rules.
[0059] When the fiber tension in all cavities is adjusted and there is still a bad morphology, the feeding flow rate of the cavity 5 is gradually reduced from the middle position to both ends, and the product morphology of the composite material at the outlet 4 is observed until there is no bad morphology on the surface, and the adjustment of the feeding flow rate is ended. Regardless of how the feeding flow rate is adjusted, the feeding flow rate in each cavity 5 should meet the following rules: Q 1 >Q 2 >Q 3 >……>Q N , Q 2N-1 >Q 2N-2 >Q 2N-3 >……>Q N , to meet the principle of high tension and small feed.
[0060] After the above steps, the fiber path is changed by adjusting the tension, and the impregnation area of the resin melt on the fiber is increased. Through multi-stage feeding with different proportions and the principle of large tension and small feeding, the excessively concentrated melt resistance is avoided to cause limited breakage. At the same time, the multi-stage feeding is repeated to impregnate the fiber to achieve the melt coating of the fiber, thereby effectively improving the impregnation effect.
[0061] In the specific contents of the above-mentioned specific implementation methods, the various technical features can be combined in any non-contradictory manner. In order to make the description concise, not all possible combinations of the above-mentioned technical features are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0062] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A dipping mold with adjustable tension, It is characterized in that The impregnation mold comprises an upper mold plate (1), a lower mold plate (2) and a mold cavity formed around the upper mold plate (1) and the lower mold plate (2), wherein two ends of the mold cavity are respectively provided with a fiber feed port (3) and a discharge port (4), wherein the mold cavity comprises a plurality of cavities (5) connected in end-to-end sequence, wherein each cavity (5) is provided with an impregnation roller (6) that can be rotated to adjust the fiber tension, and each cavity (5) is connected with a melt feed port (7) for feeding a resin melt, wherein the fiber enters from the fiber feed port (3), bypasses the outer periphery of each impregnation roller (6), is impregnated with the resin melt in the cavity (5), and then is discharged from the discharge port (4).
2. The tension-adjustable impregnation mold according to claim 1, It is characterized in that The tension exerted on the fiber by the impregnation roller (6) in the first cavity (5) and the tension exerted on the fiber by the impregnation roller (6) in the last cavity (5) are smaller than the tension exerted on the fiber by any impregnation roller (6) in the middle position; the feeding flow rate of the melt feed port (7) in the first cavity (5) and the feeding flow rate of the melt feed port (7) in the last cavity (5) are larger than the feeding flow rate of the melt feed port (7) in any cavity (5) in the middle position.
3. The tension-adjustable impregnation mold according to claim 2, It is characterized in that The tension exerted on the fiber by the impregnation roller (6) in the first cavity (5) is not greater than the tension exerted on the fiber by the impregnation roller (6) in the last cavity (5), and the feeding flow rate of the melt feed port (7) in the first cavity (5) is not less than the feeding flow rate of the melt feed port (7) in the last cavity (5).
4. The tension-adjustable impregnation mold according to claim 2, It is characterized in that The number of the cavities (5) is 2N-1, wherein N≥2 and N is a positive integer; the tension exerted on the fiber by the impregnation roller (6) in each cavity (5) is denoted as F 1 、F 2 ……F N 、F N+1 ……F 2N-1 , then, F 1 <F 2 <F 3 <…… <F N , F 2N-1 <F 2N-2 <F 2N-3 <…… <F N The feed flow rate in each cavity (5) is recorded as Q 1 , Q 2 ...Q N , Q N+1 ...Q 2N-1 , then, Q 1 >Q 2 >Q 3 >……>Q N , Q 2N-1 >Q 2N-2 >Q 2N-3 >……>Q N .
5. The tension-adjustable impregnation mold according to claim 1, It is characterized in that The upper template (1) is provided with a plurality of first corrugated surfaces (8), the lower template (2) is provided with a plurality of second corrugated surfaces (9) symmetrically arranged with respect to the first corrugated surfaces (8), the cavity (5) is formed between the first corrugated surfaces (8) and the second corrugated surfaces (9), the minimum distance between the first corrugated surfaces (8) and the second corrugated surfaces (9) is D1, the maximum distance between the first corrugated surfaces (8) and the second corrugated surfaces (9) is D2, and along the direction from the fiber feed port (3) to the discharge port (4), the distance between the first corrugated surfaces (8) and the second corrugated surfaces (9) gradually increases from D1 to D2, and then gradually decreases from D2 to D1.
6. The tension-adjustable impregnation mold according to claim 5, It is characterized in that The impregnation roller (6) is an elliptical roller, the center of which coincides with the center of the cavity (5), the minor axis diameter of the elliptical roller is greater than the minimum distance between the first corrugated surface (8) and the second corrugated surface (9), the major axis diameter of the elliptical roller is less than the maximum distance between the first corrugated surface (8) and the second corrugated surface (9), and the fibers in the mold cavity alternately bypass the lower end surface of the first corrugated surface (8) and the upper surface of the elliptical roller, or alternately bypass the upper end surface of the second corrugated surface (9) and the lower surface of the elliptical roller.
7. The tension-adjustable impregnation mold according to claim 6, It is characterized in that The same cavity (5) is connected to two groups of melt feed ports (7), the axes of the two melt feed ports (7) of the same cavity (5) coincide with each other, the axes of the melt feed ports (7) pass through the center of the cavity (5), and the axes of the melt feed ports (7) are perpendicular to the axes of the fiber feed ports (3).
8. The tension-adjustable impregnation mold according to any one of claims 1 to 7, It is characterized in that It also includes a controller (13) and a driving motor (14) connected to the impregnation roller (6); a flow valve module is provided at the melt feed port (7); an identification module (12) for identifying the surface morphology of the product is provided at the discharge port (4); the identification module (12) is connected to the input end of the controller (13); and the driving motor (14) and the flow valve module are both connected to the output end of the controller (13).
9. A dipping method based on the tension-adjustable dipping mold according to any one of claims 1 to 8, It is characterized in that The following steps are involved: S10. Pulling the fiber so that the fiber enters from the fiber feed port (3), bypasses the periphery of each impregnation roller (6), and is led out from the discharge port (4); S20. Feeding a resin melt into each cavity (5) from each melt feed port (7), the resin melt enters the cavity (5) and impregnates the fiber in the cavity (5); S30. Observe the product morphology of the composite material at the discharge port (4). If the product surface has a poor morphology, proceed to step S40; S40. Rotate the impregnation roller (6) to adjust the tension of the fibers in each cavity (5): first adjust the impregnation roller (6) at the middle position to increase the tension of the fibers at the middle position, and observe the product morphology of the composite material at the outlet (4); if the product morphology is qualified, the adjustment is terminated; if the product surface still has a bad morphology, gradually increase the tension of the fibers from the middle position to both ends, observe the product morphology of the composite material at the outlet (4), until there is no bad morphology on the surface, and then terminate the tension adjustment; S50. The tension of the fibers in each cavity (5) is adjusted according to step S40 to continuously produce fiber-reinforced resin composite materials.
10. A dipping method based on the tension-adjustable dipping mold according to claim 9, It is characterized in that Step S40 also includes the step of synchronously adjusting the feeding flow of each melt feed port (7): firstly adjusting the middle position cavity (5) to reduce the feeding flow of the middle position cavity (5), and observing the product morphology of the composite material at the discharge port (4); if the product morphology is qualified, then the adjustment is terminated; if there is still a bad morphology on the product surface, then the feeding flow of the cavity (5) is gradually reduced from the middle position to both ends, and the product morphology of the composite material at the discharge port (4) is observed until there is no bad morphology on the surface, then the feeding flow adjustment is terminated.
Citation Information
Patent Citations
Continuous long fiber-reinforced thermoplastic resin and its preparation method and molding equipment
CN102729483A
Elliptical dipping device with multiple motion states
CN209616119U
Dipping mold for fiber reinforced composite material
CN223085462U
Apparatus For Manufacturing Fiber Reinforced Composite Material
KR1020160083647A
Bending machine for curved display
KR102494950B1