Composite foam scrubbing agent for oil and gas fields and preparation method of composite foam scrubbing agent
The existing foam discharge agents are solved at high temperature and high mineralization by using a composite foam discharge agent with a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group and a betaine and superhydrophilic quaternary ammonium salt cationic surfactant. The problem of degradation of bubble performance under the condition of degree has achieved efficient bubble discharge effect in oil and gas fields.
Patent Information
- Application Number
- CN202411572966.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-06
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The bubble discharge agent used in existing oil and gas fields has decreased foaming performance under high temperature environment and high mineralization conditions, making it difficult to maintain efficient liquid discharge effect, affecting the wellbore gas production efficiency.
Using polyglycerol alkyl ether anionic surfactant with sulfonic acid groups, a composite spraying agent of betaine and superhydrophilic quaternary ammonium salt cationic surfactant, and octyl chloride and epoxypropane as raw materials Prepolymers are prepared, and surfactants with high synergies and stability are prepared by sulfonation and polyamine linking technology to form a composite bubble discharge agent.
It can maintain high drainage efficiency and foaming under normal temperature and high temperature environments, reduce foam slipping, enhance the foam's liquid-carrying ability, and improve bubble drainage efficiency and stability.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil and gas exploitation, in particular to a composite foaming agent for oil and gas fields and a preparation method thereof. Background Art
[0002] As natural gas wells are mined, formation pressure decays, gas flow rate decreases, and liquid accumulation is likely to occur, shortening the life of the gas well. Foam drainage gas production technology has developed rapidly at home and abroad in recent years. By injecting foam drainage agents into the wellbore, the surface tension of gas and liquid is reduced, and foam is formed under the stirring of the air flow, reducing the relative density of the fluid, so as to achieve the purpose of drainage gas production. In order to promote backflow, chemical additives such as drainage agents and foaming agents are added to the fracturing fluid to reduce the friction between the fracturing fluid and the pipeline and rock formation. At the same time, foam is formed to increase the energy of the formation, making it easier for the bottom liquid to flow back.
[0003] However, during use, the performance of the foaming agent is often greatly affected. On the one hand, after compounding, the surfactants of the drainage aid type will reduce the foaming and foam stabilizing ability of most foaming agents while reducing the surface tension. On the other hand, factors such as the high temperature environment of the formation and the high mineralization of the formation water also seriously affect the foaming performance of the foaming agent. It is an urgent task to develop a foaming agent that can stabilize the foaming efficiency at higher temperatures. Summary of the invention
[0004] The object of the present invention is to provide a composite foaming agent for oil and gas fields and a preparation method thereof, so as to solve the problems existing in the prior art.
[0005] In order to solve the above technical problems, the present invention provides the following technical solutions: a method for preparing a composite foaming agent for oil and gas fields, comprising the following preparation steps: (1) Place a fine powder of potassium hydroxide solid in a four-necked bottle, add octyl chloroglyceryl ether monomer, react in an oil bath at 160°C for 12 hours, add 1% of the reactant mass of deionized water to stop the reaction after the reaction, and wash with deionized water until neutral; remove the lower organic matter, and then precipitate it with petroleum ether, and purify the precipitate at 170°C and reduced pressure for 12 hours to obtain a prepolymer; add the prepolymer into a reactor, heat it to 60-70°C in a water bath, and add sulfuric acid dropwise with a constant pressure dropping funnel at a stirring speed of 60rpm. Add, and continue to keep warm for 4 hours after the addition is completed to obtain a sulfonated prepolymer; pour the sulfonated prepolymer into a beaker, dilute it with deionized water under ice water bath cooling, and neutralize it with powdered sodium hydroxide solid to pH=7, then let it stand for 24 hours, and filter the filtrate; then add anhydrous ethanol dropwise until no sodium sulfate crystals are precipitated, and filter the filtrate; finally, use anhydrous ethanol to precipitate the target product, dry the target product at 100°C for 24 hours, and grind it to obtain a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group; (2) Weigh 10 parts of hexamethylenetetramine and 0.1-0.2 parts of potassium carbonate, and dissolve them in 100 parts of dimethylformamide solvent; then weigh 30-40 parts of epichlorohydrin, and slowly drop them into the solution containing hexamethylenetetramine, and drop half of the epichlorohydrin for 1 hour, and react for 30 minutes under the protection of inert gas and uniform stirring; after the reaction is completed, slowly drop the other half of the epichlorohydrin into the reactor at a temperature of 40°C, and the dropping time is 0.5 hours; after the dropping is completed, continue to stir and react for 3 hours, and then perform reduced pressure distillation to remove Solvent and unreacted products are removed to obtain reactant A; 10 parts of reactant A and 16-24 parts of hexadecyl tertiary amine are respectively dissolved in 100 parts of dimethylformamide solvent, and then the reactant A solution is slowly added dropwise to the hexadecyl tertiary amine solution for 1 hour. After all the additions are completed, the temperature is raised to 60°C, and the reaction is continued for 3 hours, and then the reduced pressure distillation is performed to remove the solvent and unreacted products; then, a mixed solvent of anhydrous ethanol and ethyl acetate is used for crystallization 3 times, and then dried at 60°C for 3 hours to obtain a super hydrophilic quaternary ammonium salt cationic surfactant; (3) Weigh lauryl betaine, polyglycerol alkyl ether anionic surfactant, super hydrophilic quaternary ammonium salt cationic surfactant and water in a mass ratio of 7-8:1:1.2-1.8:30 for later use; first take deionized water, and then add the formulated amount of lauryl betaine, polyglycerol alkyl ether anionic surfactant, and super hydrophilic quaternary ammonium salt cationic surfactant in sequence under stirring, and continue stirring for 20 minutes to obtain a composite foaming agent.
[0006] Furthermore, in step (1), the molar ratio of potassium hydroxide to octyl chloroglyceryl ether monomer is 1:20-40.
[0007] Furthermore, the pressure reduction intensity in step (1) is 1.3 kPa.
[0008] Furthermore, the mass fraction of sulfuric acid in step (1) is 98%.
[0009] Furthermore, in step (1), the molar ratio of the prepolymer to sulfuric acid is 1:3-15.
[0010] Furthermore, in the step (1), the volume ratio of the sulfonated prepolymer to deionized water is 1:5-15.
[0011] Furthermore, the inert gas in step (2) is nitrogen.
[0012] Furthermore, the stirring speed in step (2) is 150 rpm, and the stirring speed in step (3) is 120 rpm.
[0013] Furthermore, the reduced pressure distillation pressure in step (2) is 2.7 kPa.
[0014] A composite foaming agent for oil and gas fields is prepared by the above preparation method.
[0015] Compared with the prior art, the beneficial effects achieved by the present invention are: The present invention forms a composite foaming agent by compounding three active substances, namely, a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group, betaine and a super-hydrophilic quaternary ammonium salt cationic surfactant, so as to achieve the effect of high drainage efficiency at both normal temperature and high temperature.
[0016] Firstly, alkyl chloroglyceryl ether is prepared by using octyl chloroglyceryl ether and epichlorohydrin as raw materials, a prepolymer is prepared by polymerization, and then a polyglycerol alkyl ether with a sulfonic acid group is sulfonated. The sulfonic acid group on the prepolymer is located between the chain segments of polyglycerol, which greatly improves the salt resistance and divalent cation resistance of the foaming agent, and further improves the efficiency of the foaming agent in discharging accumulated liquid as a strong water-absorbing group; and because of the high stability of the polyglycerol alkyl ether itself, it still retains excellent hydrophilicity at high temperature, so that the composite foaming agent has good foaming property and stability in both normal temperature oil and gas fields and high temperature oil and gas fields; and the three active substances of the polyglycerol alkyl ether anionic surfactant with a sulfonic acid group, betaine and super hydrophilic quaternary ammonium salt cationic surfactant are compounded to form a composite foaming agent. The three surfactants have high synergy, can reduce the slippage of foam in the wellbore, enhance the liquid carrying capacity of the foam, avoid the resistance on the wellbore wall after the foam collapses and becomes water, and improve the efficiency of foaming; Secondly, the super hydrophilic quaternary ammonium salt cationic surfactant is homemade. Multiple quaternary ammonium salt molecules are prepared by caged polyamines, alkyl tertiary amines and epichlorohydrin as raw materials and linked on the same long chain. The hydrophilic groups on the quaternary ammonium salt molecules are caged. When multiple quaternary ammonium salt molecules are polymerized together at the same time, the influence of steric hindrance is greatly reduced. The ring is opened during the preparation process, and a part of the hydroxyl groups are retained. The affinity and binding ability of the surfactant to water molecules are greatly improved. The composite foaming agent prepared with this surfactant has very good foaming and drainage efficiency. DETAILED DESCRIPTION
[0017] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0018] In order to more clearly illustrate the method provided by the present invention, the following examples are used to describe in detail the various index testing methods of a composite foaming agent for oil and gas fields prepared in the following examples are as follows: According to GB / T 13173-2008, the foaming agent prepared in the embodiment and the comparative example was subjected to a simulation test at a concentration of 3%, and the simulation device included a Roche foam meter and a constant temperature liquid carrying meter. The test examined the foaming ability, foam stability, liquid carrying rate and high temperature stability of the foaming agent when the simulated formation temperature was 150°C, the simulated formation water was 250g / L, and the foaming ability, foam stability, liquid carrying rate and high temperature stability of the foaming agent were resisted when the condensate oil was 30%. The simulated formation water was prepared as follows: 2 parts of CaCl2, 1.2 parts of MgCl2, 3 parts of Na2SO4, and 19 parts of NaCl were weighed in a beaker, and dissolved and diluted with 100 parts of distilled water.
[0019] Example 1; (1) Place a fine powder of potassium hydroxide solid in a four-necked bottle, add octyl chloroglyceryl ether monomer thereto, the molar ratio of potassium hydroxide to octyl chloroglyceryl ether monomer being 1:20, react at 160°C in an oil bath for 12 hours, add 1% by mass of deionized water to stop the reaction after the reaction, and wash with deionized water until neutral; remove the lower organic matter, precipitate it with petroleum ether, purify the precipitate at 170°C and 1.3 kPa for 12 hours to obtain a prepolymer; add the prepolymer into a reactor, heat it to 60°C in a water bath, and add 98% by mass sulfuric acid using a constant pressure dropping funnel at a stirring speed of 60 rpm. Add dropwise, the molar ratio of prepolymer to sulfuric acid is 1:3, and after the addition is completed, continue to keep warm and react for 4 hours to obtain a sulfonated prepolymer; pour the sulfonated prepolymer into a beaker, dilute it with deionized water under ice water bath cooling conditions, the volume ratio of the sulfonated prepolymer to deionized water is 1:5, and neutralize it with powdered sodium hydroxide solid to pH=7, then let it stand for 24 hours, and filter the filtrate; then add anhydrous ethanol dropwise until no sodium sulfate crystals are precipitated, and filter the filtrate; finally, use anhydrous ethanol to precipitate the target product, dry the target product at 100°C for 24 hours, and grind it to obtain a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group; (2) Weigh 10 parts of hexamethylenetetramine and 0.1 parts of potassium carbonate, and dissolve them in 100 parts of dimethylformamide solvent; then weigh 30 parts of epichlorohydrin, and slowly drop them into the solution containing hexamethylenetetramine, and drop half of the epichlorohydrin for 1 hour, and react for 30 minutes under nitrogen protection and stirring at 150 rpm; after the reaction is completed, slowly drop the other half of the epichlorohydrin into the reactor at a temperature of 40°C, and the dropping time is 0.5 hours; after the dropping is completed, continue to stir at 150 rpm for 3 hours, and then stir at 2.7 kPa. Reducing the pressure to distill and remove the solvent and unreacted products to obtain reactant A; dissolving 10 parts of reactant A and 16 parts of hexadecyl tertiary amine in 100 parts of dimethylformamide solvent respectively, and then slowly dropping the reactant A solution into the hexadecyl tertiary amine solution for 1 hour, and after all the dropping is completed, raising the temperature to 60°C, reacting for 3 hours, and then reducing the pressure to distill and remove the solvent and unreacted products; then using a mixed solvent of anhydrous ethanol and ethyl acetate for crystallization 3 times, and then drying at 60°C for 3 hours to obtain a super hydrophilic quaternary ammonium salt cationic surfactant; (3) Weigh lauryl betaine, polyglycerol alkyl ether anionic surfactant, super hydrophilic quaternary ammonium salt cationic surfactant and water in a mass ratio of 7:1:1.2:30 for later use; first take deionized water, and then add the formulated amount of lauryl betaine, polyglycerol alkyl ether anionic surfactant, and super hydrophilic quaternary ammonium salt cationic surfactant in sequence under stirring at 120 rpm, and continue stirring for 20 minutes to obtain a composite foaming agent.
[0020] Example 2; (1) Place a fine powder of potassium hydroxide solid in a four-necked bottle, add octyl chloroglyceryl ether monomer thereto, the molar ratio of potassium hydroxide to octyl chloroglyceryl ether monomer being 1:30, react at 160°C in an oil bath for 12 hours, add 1% of the mass of the reactants in deionized water to terminate the reaction after the reaction, and wash with deionized water until neutral; remove the lower organic matter, and then precipitate it with petroleum ether, purify the precipitate at 170°C and 1.3 kPa for 12 hours to obtain a prepolymer; add the prepolymer into a reactor, heat it to 65°C in a water bath, and add 98% by mass sulfuric acid using a constant pressure dropping funnel at a stirring speed of 60 rpm. Add dropwise, the molar ratio of prepolymer to sulfuric acid is 1:9, and after the addition is completed, continue to keep warm and react for 4 hours to obtain a sulfonated prepolymer; pour the sulfonated prepolymer into a beaker, dilute it with deionized water under ice water bath cooling conditions, the volume ratio of the sulfonated prepolymer to deionized water is 1:10, and neutralize it with powdered sodium hydroxide solid to pH=7, then let it stand for 24 hours, and filter the filtrate; then add anhydrous ethanol dropwise until no sodium sulfate crystals are precipitated, and filter the filtrate; finally, use anhydrous ethanol to precipitate the target product, dry the target product at 100°C for 24 hours, and grind it to obtain a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group; (2) Weigh 10 parts of hexamethylenetetramine and 0.15 parts of potassium carbonate, and dissolve them in 100 parts of dimethylformamide solvent; then weigh 35 parts of epichlorohydrin, and slowly drop them into the solution containing hexamethylenetetramine, and drop half of the epichlorohydrin for 1 hour, and react for 30 minutes under nitrogen protection and stirring at 150 rpm; after the reaction is completed, slowly drop the other half of the epichlorohydrin into the reactor at a temperature of 40°C, and the dropping time is 0.5 hours; after the dropping is completed, continue to stir at 150 rpm for 3 hours, and then stir at 2.7 kPa. Reducing the pressure to remove the solvent and unreacted products, and obtaining reactant A; dissolving 10 parts of reactant A and 20 parts of hexadecyl tertiary amine in 100 parts of dimethylformamide solvent respectively, and then slowly dropping the reactant A solution into the hexadecyl tertiary amine solution for 1 hour, and after all the dropping is completed, raising the temperature to 60°C, and reacting for 3 hours, and then reducing the pressure to remove the solvent and unreacted products; and then using a mixed solvent of anhydrous ethanol and ethyl acetate for crystallization 3 times, and then drying at 60°C for 3 hours to obtain a super hydrophilic quaternary ammonium salt cationic surfactant; (3) Weigh lauryl betaine, polyglycerol alkyl ether anionic surfactant, super hydrophilic quaternary ammonium salt cationic surfactant and water in a mass ratio of 7.5:1:1.5:30 for later use; first take deionized water, and then add the formulated amount of lauryl betaine, polyglycerol alkyl ether anionic surfactant, and super hydrophilic quaternary ammonium salt cationic surfactant in sequence under stirring at 120 rpm, and continue stirring for 20 minutes to obtain a composite foaming agent.
[0021] Example 3; (1) Place a fine powder of potassium hydroxide solid in a four-necked bottle, add octyl chloroglyceryl ether monomer thereto, the molar ratio of potassium hydroxide to octyl chloroglyceryl ether monomer being 1:40, react at 160°C in an oil bath for 12 hours, add 1% by mass of deionized water to stop the reaction after the reaction, and wash with deionized water until neutral; remove the lower organic matter, and then precipitate it with petroleum ether, purify the precipitate at 170°C and 1.3 kPa for 12 hours to obtain a prepolymer; add the prepolymer into a reactor, heat it to 70°C in a water bath, and add 98% by mass sulfuric acid with a constant pressure dropping funnel at a stirring speed of 60 rpm. Add dropwise, the molar ratio of prepolymer to sulfuric acid is 1:15, and after the addition is completed, continue to keep warm and react for 4 hours to obtain a sulfonated prepolymer; pour the sulfonated prepolymer into a beaker, dilute it with deionized water under ice water bath cooling conditions, the volume ratio of the sulfonated prepolymer to deionized water is 1:15, and neutralize it with powdered sodium hydroxide solid to pH=7, then let it stand for 24 hours, and filter the filtrate; then add anhydrous ethanol dropwise until no sodium sulfate crystals are precipitated, and filter the filtrate; finally, use anhydrous ethanol to precipitate the target product, dry the target product at 100°C for 24 hours, and grind it to obtain a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group; (2) Weigh 10 parts of hexamethylenetetramine and 0.2 parts of potassium carbonate, and dissolve them in 100 parts of dimethylformamide solvent; then weigh 40 parts of epichlorohydrin, and slowly add them dropwise into the solution containing hexamethylenetetramine, and add half of the epichlorohydrin dropwise after 1 hour, and react for 30 minutes under nitrogen protection and stirring at 150 rpm; after the reaction is completed, slowly add the other half of the epichlorohydrin dropwise into the reactor at a temperature of 40°C, and the addition time is 0.5 hours; after the addition is completed, continue to stir at 150 rpm for 3 hours, and then continue to stir at 2.7 kPa. Reducing the pressure to distill and remove the solvent and unreacted products to obtain reactant A; dissolving 10 parts of reactant A and 24 parts of hexadecyl tertiary amine in 100 parts of dimethylformamide solvent respectively, and then slowly dropping the reactant A solution into the hexadecyl tertiary amine solution for 1 hour, and after all the dropping is completed, raising the temperature to 60°C, reacting for 3 hours, and then distilling under reduced pressure to remove the solvent and unreacted products; then crystallizing 3 times using a mixed solvent of anhydrous ethanol and ethyl acetate, and then drying at 60°C for 3 hours to obtain a super hydrophilic quaternary ammonium salt cationic surfactant; (3) Weigh lauryl betaine, polyglycerol alkyl ether anionic surfactant, super hydrophilic quaternary ammonium salt cationic surfactant and water in a mass ratio of 8:1:1.8:30 for later use; first take deionized water, and then add the formulated amount of lauryl betaine, polyglycerol alkyl ether anionic surfactant, and super hydrophilic quaternary ammonium salt cationic surfactant in sequence under stirring at 120 rpm, and continue stirring for 20 minutes to obtain a composite foaming agent.
[0022] Comparative Example 1: The difference between Comparative Example 1 and Example 2 is that step (2) is omitted, and step (3) is changed to: lauryl betaine, polyglycerol alkyl ether anionic surfactant, octadecyl dimethyl hydroxyethyl quaternary ammonium nitrate and water are weighed in a mass ratio of 7.5:1:1.5:30 for later use; deionized water is first taken, and then the formula amount of lauryl betaine, polyglycerol alkyl ether anionic surfactant and octadecyl dimethyl hydroxyethyl quaternary ammonium nitrate are added in sequence under stirring at a speed of 120 rpm, and stirring is continued for 20 minutes to obtain a composite foaming agent; the remaining steps are the same as those of Example 2.
[0023] Comparative Example 2: The difference between Comparative Example 2 and Example 2 is that step (2) is different, and step (2) is changed to: weigh 10 parts of diethylenetriamine and 0.15 parts of potassium carbonate, and dissolve them in 100 parts of dimethylformamide solvent; then weigh 35 parts of epichlorohydrin, slowly add them dropwise into the solution containing diethylenetriamine, add half of the epichlorohydrin dropwise for 1 hour, and react for 30 minutes under nitrogen protection and stirring at 150 rpm; after the reaction is completed, continue to slowly add the other half of the epichlorohydrin dropwise into the reactor at a temperature of 40°C, and the dropping time is 0.5 hours; after the dropping is completed, continue to stir at 150 rpm for 3 hours h, then vacuum distillation at 2.7 kPa to remove the solvent and unreacted products to obtain reactant A; 10 parts of reactant A and 20 parts of hexadecyl tertiary amine were respectively dissolved in 100 parts of dimethylformamide solvent, and then the reactant A solution was slowly added dropwise to the hexadecyl tertiary amine solution for 1 hour. After all the additions were completed, the temperature was raised to 60°C, and the reaction was continued for 3 hours, and then vacuum distillation was carried out to remove the solvent and unreacted products; then crystallization was performed 3 times using a mixed solvent of anhydrous ethanol and ethyl acetate, and then drying was performed at 60°C for 3 hours to obtain a super hydrophilic quaternary ammonium salt cationic surfactant; the remaining steps were the same as in Example 2.
[0024] Comparative Example 3: The difference between Comparative Example 3 and Example 2 is that step (1) is omitted, and step (3) is changed to: lauryl betaine, polyoxyethylene carboxylic acid anionic surfactant, super hydrophilic quaternary ammonium salt cationic surfactant and water are weighed in a mass ratio of 7.5:1:1.5:30 for later use; deionized water is first taken, and then the formula amount of lauryl betaine, polyoxyethylene carboxylic acid anionic surfactant and super hydrophilic quaternary ammonium salt cationic surfactant are added in sequence under stirring at a speed of 120 rpm, and stirring is continued for 20 minutes to obtain a composite foaming agent; the remaining steps are the same as those in Example 2.
[0025] Comparative Example 4: The difference between Comparative Example 4 and Example 2 is that step (1) is omitted, and step (3) is changed to: lauryl betaine, fatty alcohol polyoxyethylene ether, super hydrophilic quaternary ammonium salt cationic surfactant and water are weighed in a mass ratio of 7.5:1:1.5:30 for later use; deionized water is first taken, and then the formula amount of lauryl betaine, fatty alcohol polyoxyethylene ether, and super hydrophilic quaternary ammonium salt cationic surfactant are added in sequence under stirring at a speed of 120 rpm, and stirring is continued for 20 minutes to obtain a composite foaming agent; the remaining steps are the same as those in Example 2.
[0026] Effect example Table 1 below shows the performance analysis results of a composite foaming agent for oil and gas fields using Examples 1 to 3 of the present invention and Comparative Examples 1 to 4.
[0027] Table 1
[0028] From the comparison of the experimental data of foam stability of the embodiment and the comparative example, it can be found that the present invention uses octyl chloroglyceryl ether and epichlorohydrin as raw materials to prepare alkyl chloroglyceryl ether, prepares a prepolymer through polymerization, and then sulfonates it to obtain polyglycerol alkyl ether with sulfonic acid groups, and the sulfonic acid groups thereon are between the segments of polyglycerol, which greatly improves the salt resistance and anti-divalent cation performance of the foaming agent. From the comparison of the experimental data of the liquid carrying capacity of the embodiment and the comparative example, it can be found that the present invention uses sulfonic acid groups as strong water-absorbing groups to further improve the efficiency of the foaming agent in discharging effusion; and the three active substances of polyglycerol alkyl ether anionic surfactant with sulfonic acid groups, betaine and super hydrophilic quaternary ammonium salt cationic surfactant are compounded to form a composite foaming agent, and these three surfactants have high synergy, can reduce the slippage site of foam in the wellbore, enhance the liquid carrying capacity of foam, avoid resistance on the well wall after the foam collapses and becomes water, and improve the efficiency of foaming. The self-made super-hydrophilic quaternary ammonium salt cationic surfactant of the present invention is prepared by using caged polyamine, alkyl tertiary amine and epoxy chloroalkane as raw materials to prepare multiple quaternary ammonium salt molecules linked on the same long chain, and the hydrophilic groups on the quaternary ammonium salt molecules are caged, when multiple quaternary ammonium salt molecules are polymerized together at the same time, the influence brought by steric hindrance is greatly reduced, and a part of hydroxyl groups are retained during the preparation process, which greatly improves the affinity and binding ability of the surfactant to water molecules, and the composite foaming agent prepared by the surfactant has very excellent foaming and drainage efficiency. From the experimental data comparison of the foam stability retention rate at 150°C of the embodiment and the comparative example, it can be found that the present invention still retains excellent hydrophilicity at high temperature because of the high stability of the polyglycerol alkyl ether itself, so that the composite foaming agent has good foaming and stability in both the normal temperature of the oil and gas field and the high temperature environment after operation.
[0029] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered in all respects as exemplary and non-limiting, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations within the meaning and scope of the equivalent elements of the claims be included in the invention. Any marking in a claim should not be considered as limiting the claim to which it relates.
Claims
1. A method for preparing a composite foaming agent for oil and gas fields, characterized in that: The method comprises the following preparation steps: (1) Place finely powdered potassium hydroxide solid in a four-necked flask, add octyl chloroglyceryl ether monomer, and react at 160°C in an oil bath for 12 hours. After the reaction, add 1% deionized water by mass of the reactants to stop the reaction, and wash with deionized water until neutral; remove the organic matter layer, and then precipitate it with petroleum ether. The precipitate is purified at 170°C under reduced pressure for 12 hours to obtain a prepolymer; add the prepolymer into the reactor, heat it to 60-70°C in a water bath, and add sulfuric acid dropwise with a constant pressure dropping funnel at a stirring speed of 60 rpm. Add, and after the addition is completed, continue to keep warm and react for 4 hours to obtain a sulfonated prepolymer; pour the sulfonated prepolymer into a beaker, dilute with deionized water under ice water bath cooling, and neutralize with powdered sodium hydroxide solid to pH = 7, then let it stand for 24 hours, and filter to obtain the filtrate; then add anhydrous ethanol dropwise thereto until no sodium sulfate crystals are precipitated, and filter to obtain the filtrate; finally, precipitate the target product with anhydrous ethanol, dry the target product at 100° C. for 24 hours, and grind to obtain a polyglycerol alkyl ether anionic surfactant with a sulfonic acid group; (2) Weigh 10 parts of hexamethylenetetramine and 0.1-0.2 parts of potassium carbonate, and dissolve them in 100 parts of dimethylformamide solvent; then weigh 30-40 parts of epichlorohydrin, slowly drop them into the solution containing hexamethylenetetramine, add half of the epichlorohydrin dropwise after 1 hour, and react for 30 minutes under the protection of inert gas and uniform stirring; after the reaction is completed, slowly add the other half of the epichlorohydrin dropwise to the reactor at a temperature of 40°C, and the addition time is 0.5 hours; after the addition is completed, continue to stir the reaction for 3 hours, and then perform vacuum distillation to remove Solvent and unreacted products are removed to obtain reactant A; 10 parts of reactant A and 16-24 parts of hexadecyl tertiary amine are respectively dissolved in 100 parts of dimethylformamide solvent, and then reactant A solution is slowly added dropwise to the hexadecyl tertiary amine solution for 1 hour. After all the addition is completed, the temperature is raised to 60°C, and the reaction is continued for 3 hours, and then vacuum distillation is performed to remove the solvent and unreacted products; then crystallization is performed three times using a mixed solvent of anhydrous ethanol and ethyl acetate, and then drying is performed at 60°C for 3 hours to obtain a super hydrophilic quaternary ammonium salt cationic surfactant; (3) Weigh lauryl betaine, polyglycerol alkyl ether anionic surfactant, super hydrophilic quaternary ammonium salt cationic surfactant and water in a mass ratio of 7-8:1:1.2-1.8:30 for later use; first take deionized water, then add the formulated amount of lauryl betaine, polyglycerol alkyl ether anionic surfactant and super hydrophilic quaternary ammonium salt cationic surfactant in sequence under stirring, continue stirring for 20 minutes to obtain a composite foaming agent.
2. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: In the step (1), the molar ratio of potassium hydroxide to octyl chloroglyceryl ether monomer is 1:20-40.
3. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: The pressure reduction intensity in step (1) is 1.3 kPa.
4. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: The mass fraction of sulfuric acid in step (1) is 98%.
5. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: The molar ratio of the prepolymer to the sulfuric acid in the step (1) is 1:3-15.
6. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: In the step (1), the volume ratio of the sulfonated prepolymer to deionized water is 1:5-15.
7. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: The inert gas in step (2) is nitrogen.
8. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: The stirring speed in step (2) is 150 rpm, and the stirring speed in step (3) is 120 rpm.
9. The method for preparing a composite foaming agent for oil and gas fields according to claim 1, characterized in that: The reduced pressure distillation pressure in step (2) is 2.7 kPa.
10. A composite foaming agent for oil and gas fields, characterized in that: Prepared according to any one of claims 1 to 9.
Citation Information
Patent Citations
Foam scrubbing agent for resisting condensate oil and methyl alcohol and preparation method thereof
CN105199702A
Anionic gemini surfactant and preparation method thereof
CN107814755A
Preparation method of polyquaternary ammonium salt surfactant
CN108714398A
Foam drainage agent with resistance to high-content gas condensate and resistance to high mineralization and preparation method of foam drainage agent
CN110819327A