Copper foil substrate with ultrathin copper foil layer and manufacturing method thereof

Through the electroplating forming and hot pressing technology of the roll-shaped copper foil board, an ultra-thin copper foil layer is formed and applied to the substrate, which solves the problem of thickness and bonding of the copper foil layer, realizes cost reduction and circuit refinement, and improves the Product competitiveness.

CN119095283APending Publication Date: 2024-12-06WAN HON ENTERPRISE CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310655201.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-05
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

In the prior art, the copper foil layer is thicker and difficult to etch and is difficult to fit on the substrate, increasing manufacturing costs and reducing product competitiveness.

Method used

A roll-shaped copper foil plate is used to form an ultra-thin copper foil layer by electroplating, roughening and forming a roughened surface, and the copper foil layer is applied to the substrate by hot pressing technology to form an ultra-thin copper foil substrate.

Benefits of technology

Effectively reduce the thickness of the copper foil layer, solve the bonding problem, reduce manufacturing costs, improve the refinement of the line, and enhance market competitiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119095283A_ABST
    Figure CN119095283A_ABST
Patent Text Reader

Abstract

The invention discloses a copper foil substrate with an ultrathin copper foil layer and a manufacturing method thereof, and the manufacturing method comprises the following steps: providing a roll-shaped copper foil plate, the copper foil layer of the roll-shaped copper foil plate is formed by electroplating a seed crystal layer, and the thickness of the copper foil layer is less than or equal to 10 [mu] m; the bundled copper foil plate is cut into a plurality of pieces and leveled to form a plurality of flat copper foil plates; forming a roughened surface on the surface of the copper foil layer of each flat copper foil plate by using a roughening process; providing at least one substrate; adhering and combining the roughened surface of the copper foil layer on each flat copper foil plate on the first surface of each substrate by using a hot pressing technology; the flat copper foil plates are removed from the substrates to form at least one copper foil substrate, the problem that in the prior art, copper foil is not prone to being attached to the substrates is effectively solved, the thickness of the copper foil is reduced, and the market competitiveness of products is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a copper foil substrate and a manufacturing method thereof, in particular to a copper foil substrate with an ultra-thin copper foil layer and a manufacturing method thereof. Background Art

[0002] In recent years, the high functionality of electronic products has increased the frequency of signals. Copper foil substrates (printed circuit boards) that can transmit high-frequency signals without quality degradation are suitable for such high-frequency applications and have therefore received attention from the industry.

[0003] In the prior art, copper foil is adhered to a resin layer by an adhesive to form a substrate, such as a copper-clad laminate disclosed in Taiwan Patent No. 1787480, which includes copper foil, an adhesive layer and a resin layer, wherein the adhesive layer contains one or more selected from the group consisting of polyphenylene ether resin, polyimide resin, olefin resin, liquid crystal polymer, polyester resin, polystyrene resin, hydrocarbon elastomer, benzoxazine resin, active ester resin, cyanate resin, bismaleimide resin, butadiene resin, hydrogenated or non-hydrogenated styrene-butadiene resin, epoxy resin, fluororesin, resin with vinyl group, and copolymers thereof, and is disposed on the surface of the copper foil. However, the adhesive used in the prior art is a special material, which increases the manufacturing cost, and the smooth surface of the copper foil is not easy to be completely attached to the substrate (such as a substrate composed of FR-4 grade glass fiber, FR-5 grade glass fiber, or BT resin material).

[0004] In addition to the above problems, in the prior art, there is also the problem that the thickness of the copper foil is too thick and it is not easy to etch. For example, the content of Taiwan Patent M631636 discloses a copper foil structure, which mainly includes a carrier layer, a peeling layer, a copper foil layer, a roughening layer and an anti-oxidation layer, wherein the thickness of the roughening layer is between 300 μm and 500 μm. Figure 1 It can be clearly seen that the roughened layer (14) is significantly thinner than the copper foil layer (13). Therefore, it can be seen that the thickness of the copper foil layer is at least greater than 300 μm. In terms of modern technology, the copper foil layer in the existing technology is quite thick and difficult to etch, which is not conducive to the refinement of the circuit and reduces the market competitiveness of the product.

[0005] Therefore, a copper foil substrate having an ultra-thin copper foil layer with reduced copper foil thickness and capable of being bonded to a substrate without using an adhesive and a manufacturing method thereof are urgently expected by the current relevant industries. Summary of the invention

[0006] The main purpose of the present invention is to provide a copper foil substrate with an ultra-thin copper foil layer and a manufacturing method thereof, comprising: providing a rolled copper foil plate, wherein the copper foil layer of the rolled copper foil plate is formed by electroplating a seed layer and the thickness of the copper foil layer is less than or equal to 10 μm; cutting the rolled copper foil plate into multiple pieces and flattening them to form multiple flat copper foil plates; forming a roughened surface on the surface of the copper foil layer of each flat copper foil plate by a roughening process; providing at least one substrate; laminating and bonding the roughened surface of the copper foil layer on each flat copper foil plate to the first surface of each substrate by a hot pressing process; removing each flat copper foil plate from each substrate to form at least one copper foil substrate, thereby effectively solving the problem in the prior art that copper foil is not easy to be laminated on the substrate and reducing the thickness of the copper foil.

[0007] To achieve the above-mentioned purpose, the present invention provides a copper foil substrate with an ultra-thin copper foil layer, the copper foil substrate comprising a substrate layer and a first copper foil layer; the substrate layer is formed by using FR-4 grade glass fiber, FR-5 grade glass fiber, or BT (Bismaleimide Triazine) resin material, the substrate layer has a first surface and a second surface opposite to it; the first copper foil layer has a thickness less than or equal to 10 μm and has a roughened surface corresponding to the first surface of the substrate layer, the first copper foil layer is bonded to the first surface of the substrate layer by means of the roughened surface through hot pressing technology to form the copper foil substrate, so as to increase the market competitiveness of the product.

[0008] In a preferred embodiment of the present invention, the thickness of the first copper foil layer is further less than or equal to 5 μm.

[0009] In a preferred embodiment of the present invention, the copper foil substrate further includes a second copper foil layer, which is disposed on the second surface of the substrate layer. The thickness of the second copper foil layer is less than or equal to 10 μm and has a roughened surface corresponding to the second surface of the substrate layer. The second copper foil layer is bonded to the second surface of the substrate layer by means of a hot pressing process through the roughened surface of the second copper foil layer.

[0010] In a preferred embodiment of the present invention, the thickness of the second copper foil layer is further less than or equal to 5 μm.

[0011] The present invention also provides a method for manufacturing a copper foil substrate with an ultra-thin copper foil layer, which comprises the following steps: Step S1: providing a rolled copper foil plate, the rolled copper foil plate comprising a carrier layer, a seed layer (Seed Layer) and a copper foil layer; wherein the seed layer is disposed on a surface of the carrier layer, wherein the copper foil layer is electroplated by the seed layer and the thickness of the copper foil layer is less than or equal to 10 μm; Step S2: cutting the rolled copper foil plate into a plurality of pieces and flattening them to form a plurality of flat copper foil plates, each of which comprises the carrier layer, the seed layer and the copper foil layer; Step S3: forming a roughened surface on the surface of the copper foil layer of each of the flat copper foil plates by a roughening process; Step S4: providing at least one substrate, the at least one substrate having a first surface and an opposite second surface; Step S 5: Using a hot pressing technique to bond the roughened surface of the copper foil layer on each of the flat copper foil boards to the first surface of the at least one substrate; and step S6: removing the seed layer and the carrier layer on each of the flat copper foil boards from the at least one substrate to form at least one copper foil substrate, the at least one substrate is formed as a substrate layer in each of the copper foil substrates, the first surface of the at least one substrate is formed as a first surface of the substrate layer, the second surface of the at least one substrate is formed as a second surface of the substrate layer, and the copper foil layer of each of the flat copper foil boards is formed as a first copper foil layer in the copper foil substrate.

[0012] In a preferred embodiment of the present invention, the roughening process for forming the roughened surface includes plasma surface treatment, sandblasting surface treatment, frosting surface treatment, or chemical etching treatment.

[0013] In a preferred embodiment of the present invention, the thickness of the copper foil layer is further less than or equal to 5 μm.

[0014] In a preferred embodiment of the present invention, after step S6, each of the flat copper foil boards formed by the manufacturing method of steps S1 to S3 described in the manufacturing method of the copper foil substrate is further provided, and the roughened surface of the copper foil layer on each of the flat copper foil boards provided is bonded to the second surface of the substrate layer of the at least one copper foil substrate by hot pressing technology, and then the seed layer and the carrier layer on each of the flat copper foil boards are removed from the second surface of the substrate layer, so that the copper foil layer on each of the flat copper foil boards provided is formed as a second copper foil layer in the at least one copper foil substrate.

[0015] In a preferred embodiment of the present invention, the thickness of the second copper foil layer of the at least one copper foil substrate is further less than or equal to 5 μm. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1It is a side cross-sectional schematic diagram of the copper foil substrate of the present invention.

[0017] Figure 2 It is a perspective schematic diagram of the rolled copper foil sheet of the present invention.

[0018] Figure 3 It is a three-dimensional schematic diagram of cutting the rolled copper foil sheet of the present invention into a plurality of sheets and flattening them to form a plurality of flat copper foil sheets.

[0019] Figure 4 It is a side cross-sectional schematic diagram of the flat copper foil plate of the present invention.

[0020] Figure 5 It is a side cross-sectional schematic diagram of forming a roughened surface on the surface of the flat copper foil plate of the present invention by using a roughening processing technique.

[0021] Figure 6 yes Figure 5 A partial enlarged schematic diagram of .

[0022] Figure 7 It is a schematic diagram of a side cross-section decomposition of laminating and bonding the roughened surface of the copper foil layer on the flat copper foil board of the present invention to the first surface of the substrate by using the hot pressing technique.

[0023] Figure 8 yes Figure 7 Schematic diagram of the combination.

[0024] Fig. 9 Yes Figure 8 A side cross-sectional schematic diagram of the seed layer and the carrier layer on the flat copper foil board being removed from the substrate.

[0025] Fig.10 It is a side cross-sectional schematic diagram of the copper foil substrate of the present invention further having a second copper foil layer.

[0026] Fig.11 It is a schematic diagram of a side cross-section decomposition of laminating and bonding the roughened surface of the copper foil layer on the flat copper foil board of the present invention to the second surface of the copper foil substrate by using a hot pressing technique.

[0027] Fig.12 yes Fig.11 Schematic diagram of the combination.

[0028] Fig.13 Yes Fig.12 A side cross-sectional schematic diagram of the seed layer and the carrier layer on the flat copper foil board being removed from the second surface of the copper foil substrate.

[0029] Explanation of the accompanying drawings: 1-copper foil substrate; 10-substrate layer; 11-first surface; 12-second surface; 20-first copper foil layer; 21-roughened surface; 30-second copper foil layer; 31-roughened surface; 2-rolled copper foil board; 2a-carrier layer; 2b-seed layer; 2c-copper foil layer; 2d-roughened surface; 2e-flat copper foil board; 3-substrate; 3a-first surface; 3b-second surface. DETAILED DESCRIPTION

[0030] With the help of illustrations, the structure and technical features of the present invention are described in detail as follows, wherein each illustration is only used to illustrate the structural relationship and related functions of the present invention, so the size of each element in each illustration is not drawn according to the actual scale and is not used to limit the present invention.

[0031] refer to Figure 1 The present invention provides a copper foil substrate 1 having an ultra-thin copper foil layer. The copper foil substrate 1 includes a substrate layer 10 and a first copper foil layer 20 .

[0032] The substrate layer 10 is made of FR-4 grade glass fiber, FR-5 grade glass fiber, or BT (Bismaleimide Triazine) resin material. The substrate layer 10 has a first surface 11 and an opposite second surface 12. Figure 1 As shown; wherein the FR-4 grade is a code for a flame retardant material grade, FR-4 grade materials have better mechanical properties, dielectric properties, heat resistance and moisture resistance, and are easy to machine, generally composed of glass cloth (Woven glass) and epoxy resin; wherein the FR-5 grade is a code for a flame retardant material grade, FR-5 grade materials have a higher operating temperature and excellent mechanical properties at high temperatures, especially better heat resistance than FR-4 grade materials, generally composed of glass cloth and epoxy resin; wherein the BT resin material is a hard material, the hardness of the substrate made of BT resin material can meet the needs of most semiconductor manufacturers, and BT resin material has a relatively stable material price in the market due to its wide use.

[0033] The first copper foil layer 20 has a thickness less than or equal to 10 μm and has a roughened surface 21 corresponding to the first surface 11 of the substrate layer 10. Figure 1 As shown, the first copper foil layer 20 is bonded to the first surface 11 of the substrate layer 10 through the roughened surface 21 by hot pressing technology to form the copper foil substrate 1; wherein the thickness of the first copper foil layer 20 can be further less than or equal to 5μm but is not limited, so as to increase the refinement of the circuit.

[0034] refer to Fig.10The copper foil substrate 1 further includes a second copper foil layer 30 but is not limited thereto. The second copper foil layer 30 is disposed on the second surface 12 of the substrate layer 10. The thickness of the second copper foil layer 30 is less than or equal to 10 μm and has a roughened surface 31 corresponding to the second surface 12 of the substrate layer 10. The second copper foil layer 30 is bonded to the second surface 12 of the substrate layer 10 by the roughened surface 31 of the second copper foil layer 30 through hot pressing. The thickness of the second copper foil layer 30 can be further less than or equal to 5 μm but is not limited thereto, so as to increase the refinement of the circuit.

[0035] The manufacturing method of the copper foil substrate 1 comprises the following steps:

[0036] Step S1: Provide a bundle of rolled copper foil sheets 2, such as Figure 2 As shown, the rolled copper foil plate 2 includes a carrier layer 2a, a seed layer 2b and a copper foil layer 2c. Figure 4 As shown; wherein the thickness of the carrier layer 2a is further 18μm but not limited; wherein the seed layer 2b is disposed on a surface of the carrier layer 2a; wherein the copper foil layer 2c is formed by electroplating the seed layer 2b and the thickness of the copper foil layer 2c can be less than or equal to 10μm, such as Figure 4 As shown; wherein the thickness of the copper foil layer 2c can be further less than or equal to 5μm but is not limited.

[0037] Step S2: Cut the rolled copper foil sheet 2 into multiple sheets and flatten them to form multiple flat copper foil sheets 2e, such as Figure 3 As shown, each flat copper foil plate 2e includes the carrier layer 2a, the seed layer 2b and the copper foil layer 2c. Figure 4 shown.

[0038] Step S3: Using roughening technology (such as Figure 5 A roughened surface 2d is formed on the surface of the copper foil layer 2c of each flat copper foil plate 2e (as shown in the direction of the arrow A). Figure 6 As shown; the roughening processing technology for forming the roughened surface 2d includes plasma surface treatment, sandblasting surface treatment, frosted surface treatment, or chemical etching treatment but is not limited.

[0039] Step S4: Provide at least one substrate 3, each substrate 3 having a first surface 3a and an opposite second surface 3b, such as Figure 7 shown.

[0040] Step S5: Using a hot pressing technique, the roughened surface 2d of the copper foil layer 2c on each flat copper foil plate 2e is bonded to the first surface 3a of each substrate 3. Figure 7 and Figure 8 shown.

[0041] Step S6: removing the seed layer 2b and the carrier layer 2a on each flat copper foil plate 2e from each substrate 3 to form at least one copper foil substrate 1, such as Fig. 9 As shown, each substrate 3 is formed as a substrate layer 10 in each copper foil substrate 1. Fig. 9 As shown, the first surface 3a of each substrate 3 forms a first surface 11 of each substrate layer 10. Fig. 9 As shown, the second surface 3b of each substrate 3 forms a second surface 12 of each substrate layer 10. Fig. 9 As shown, the copper foil layer 2c of each flat copper foil plate 2e is formed as a first copper foil layer 20 in the copper foil substrate 1. Fig. 9 shown.

[0042] If the copper foil substrate 1 is to be further made into a substrate structure with copper foil on both sides, after step S6, each flat copper foil plate 2e formed by the manufacturing method of steps S1 to S3 described in the manufacturing method of the copper foil substrate 1 is further provided. Figures 3 to 6 As shown, the roughened surface 2d of the copper foil layer 2c on each flat copper foil plate 2e provided separately is attached to the second surface 12 of the substrate layer 10 of each copper foil substrate 1 by using a hot pressing technique, as shown in FIG. Fig.11 and Fig.12 As shown, the seed layer 2b and the carrier layer 2a on each flat copper foil plate 2e are removed from the second surface 12 of the substrate layer 10, as shown in FIG. Fig.13 As shown, the copper foil layer 2c on each flat copper foil plate 2e provided separately is formed into a second copper foil layer 30 in each copper foil substrate 1, as shown in FIG. Fig.13 As shown; wherein the second copper foil layer 30 (such as Fig.10 The thickness of the circuit (as shown) can be less than or equal to 5 μm but is not limited thereto, so as to increase the refinement of the circuit.

[0043] The copper foil substrate 1 of the present invention has the following advantages compared with the existing technology in the field of copper foil substrates:

[0044] (1) The first copper foil layer 20 of the present invention is bonded to the first surface 11 of the substrate layer 10 by the roughened surface 21 through hot pressing technology to form the copper foil substrate 1, that is, the copper foil substrate 1 of the present invention does not use the adhesive used in the prior art (such as the content disclosed in Taiwan Patent No. 1787480) during the formation process, so that the present invention effectively solves the problem that the adhesive used in the prior art is a special material that increases the cost of the manufacturing end, which is conducive to reducing the cost of the manufacturing end. In addition, the present invention also solves the problem that the smooth surface of the copper foil is not easy to completely adhere to the substrate (such as a substrate made of FR-4 grade glass fiber, FR-5 grade glass fiber, or BT resin material), avoiding the occurrence of defective products and reducing the yield and reliability of the product, so as to increase the market competitiveness of the product.

[0045] (2) The thickness of the first copper foil layer 20 of the present invention is less than or equal to 10 μm, that is, the thickness of the copper foil layer used in the present invention is lower than that of the products of the prior art (such as the content disclosed in Taiwan Patent M631636). The present invention effectively solves the problem that the copper foil layer in the prior art is difficult to etch due to its relatively thick thickness, which is not conducive to the refinement of the circuit, thereby increasing the market competitiveness of the product.

[0046] The above description is only a preferred embodiment of the present invention, which is only illustrative rather than restrictive of the present invention. A person skilled in the art will understand that many changes, modifications, and even equivalent changes may be made to the present invention within the spirit and scope defined by the claims of the present invention, but all of these will fall within the scope of protection of the present invention.

Claims

1. A copper foil substrate having an ultra-thin copper foil layer, characterized in that: Include: a substrate layer, which is made of FR-4 grade glass fiber, FR-5 grade glass fiber or BT resin material, and has a first surface and an opposite second surface; and A first copper foil layer, whose thickness is less than or equal to 10 μm and has a roughened surface corresponding to the first surface of the substrate layer. The first copper foil layer is bonded to the first surface of the substrate layer by hot pressing through the roughened surface to form the copper foil substrate.

2. The copper foil substrate according to claim 1, characterized in that The thickness of the first copper foil layer is further less than or equal to 5 μm.

3. The copper foil substrate according to claim 1, wherein: The copper foil substrate further includes a second copper foil layer, which is disposed on the second surface of the substrate layer. The thickness of the second copper foil layer is less than or equal to 10 μm and has a roughened surface corresponding to the second surface of the substrate layer. The second copper foil layer is bonded to the second surface of the substrate layer by means of the roughened surface of the second copper foil layer through hot pressing.

4. The copper foil substrate according to claim 3, characterized in that The thickness of the second copper foil layer is further less than or equal to 5 μm.

5. A method for manufacturing a copper foil substrate having an ultra-thin copper foil layer, characterized in that: It includes the following steps: Step S1: providing a rolled copper foil sheet, the rolled copper foil sheet comprising a carrier layer, a seed layer and a copper foil layer; wherein the seed layer is disposed on a surface of the carrier layer; wherein the copper foil layer is formed by electroplating the seed layer and the thickness of the copper foil layer is less than or equal to 10 μm; Step S2: cutting the rolled copper foil sheet into a plurality of sheets and flattening them to form a plurality of flat copper foil sheets, each of which comprises the carrier layer, the seed layer and the copper foil layer; Step S3: forming a roughened surface on the surface of the copper foil layer of each of the flat copper foil plates by using a roughening process; Step S4: providing at least one substrate, wherein the at least one substrate has a first surface and an opposite second surface; Step S5: bonding the roughened surface of the copper foil layer on each of the flat copper foil plates to the first surface of the at least one substrate by using a hot pressing technique; and Step S6: The seed layer and the carrier layer on each of the flat copper foil plates are removed from the at least one substrate to form at least one copper foil substrate. The at least one substrate is formed as a substrate layer in the at least one copper foil substrate. The first surface of the at least one substrate forms a first surface of the substrate layer. The second surface of the at least one substrate forms a second surface of the substrate layer. The copper foil layer of each of the flat copper foil plates is formed as a first copper foil layer in the copper foil substrate.

6. The manufacturing method according to claim 5, characterized in that: The roughening process for forming the roughened surface includes plasma surface treatment, sandblasting surface treatment, grinding surface treatment or chemical etching treatment.

7. The manufacturing method according to claim 5, characterized in that: The thickness of the copper foil layer is further less than or equal to 5 μm.

8. The manufacturing method according to claim 5, characterized in that: After step S6, each of the flat copper foil boards formed by the manufacturing method of steps S1 to S3 as described in claim 5 is further provided, and the roughened surface of the copper foil layer on each of the flat copper foil boards provided is bonded to the second surface of the substrate layer of the at least one copper foil substrate by using a hot pressing technique, and then the seed layer and the carrier layer on each of the flat copper foil boards are removed from the second surface of the substrate layer, so that the copper foil layer on each of the flat copper foil boards provided is formed as a second copper foil layer in the at least one copper foil substrate.

9. The manufacturing method according to claim 8, characterized in that: The thickness of the second copper foil layer of the at least one copper foil substrate is further less than or equal to 5 μm.