Micro OLED display module manufacturing method, micro OLED display module and display equipment
By using ultrafast laser scanning quantum dot film layers in micro OLED display modules, a quantum dot array with unified parameters is generated, which solves the problem of complex color film preparation and low transmittance, and realizes display of high PPI and high color gamut. Effect, suitable for a variety of usage scenarios.
Patent Information
- Application Number
- CN202310667933.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-06
- Publication Date
- 2024-12-06
AI Technical Summary
The existing micro OLED preparation process based on color films is complex, and the low transmittance of color films limits the use scenarios and display color gamut.
By making a driving substrate on a silicon-based substrate, adding OLED light-emitting devices and quantum dot film layers, and scanning and irradiating the quantum dot film layers with various ultrafast lasers with different energy intensities to generate a quantum dot array with unified parameters, simplifying preparation Process and improve display color gamut.
It realizes the full color of micro OLED, has high PPI, high color gamut, and high luminous efficiency, simplifies the preparation process, improves the display effect, and is suitable for more abundant use scenarios.
Smart Images

Figure CN119095448A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the field of display technology, and in particular to a micro OLED display module manufacturing method, a micro OLED display module and a display device. Background Art
[0002] With the development of science and technology, people use screens in more and more scenarios, and higher requirements are put forward for screens and usage scenarios. There is also a great demand for small-size, high PPI (Pixels Per Inch), and high color gamut display devices. However, due to the current limitations of technological development, microOLED (Organic Light-Emitting Diode) and micro-LED (light-emitting diode) are generally used for high PPI and small size. Among them, micro-LED is too difficult to process and too expensive, so it is not widely used at present. OLED is currently in large-scale commercial use, and the overall process and price can meet the requirements. However, due to the high PPI requirements for micro OLED, it is difficult to achieve full color by ordinary processing methods. The current commercial mass production method of full-color micro OLED is still OLED+color film to achieve full color.
[0003] The existing micro OLED based on color film has a complex preparation process, and the low transmittance of the color film limits the usage scenarios and display color gamut. Summary of the invention
[0004] The embodiments of the present invention provide a micro OLED display module manufacturing method, a micro OLED display module and a display device to solve the technical problems that the preparation process of the existing micro OLED based on color film is complicated and the low transmittance of the color film limits the use scenarios and display color gamut.
[0005] In a first aspect, an embodiment of the present invention provides a method for manufacturing a micro OLED display module, which includes:
[0006] Manufacturing a driving substrate based on a silicon-based substrate;
[0007] Adding an OLED light-emitting device and a first encapsulation layer on the driving substrate in sequence;
[0008] Generating a quantum dot film layer on the first encapsulation layer;
[0009] The quantum dot film layer is scanned and irradiated by ultrafast lasers with different energy intensities, and quantum dots with uniform parameters are generated at the irradiation positions with the same corresponding energy intensities, and the quantum dots form a quantum dot array in the quantum dot film layer;
[0010] A second encapsulation layer is added on the quantum dot film layer.
[0011] The quantum dot array includes quantum dots corresponding to three colors, the quantum dots of the three colors are cyclically distributed in a first direction, and the quantum dots of the same color are continuously distributed in a second direction, and the first direction is perpendicular to the second direction;
[0012] Accordingly, the quantum dot film layer is scanned and irradiated by ultrafast lasers with different energy intensities, and quantum dots with uniform parameters are generated at the irradiation points with the same corresponding energy intensities. The quantum dots form a quantum dot array in the quantum dot film layer, including:
[0013] According to the number of cycles of the quantum dots of three colors in the first direction, the same number of ultrafast laser beams are generated respectively;
[0014] The ultrafast laser beam corresponding to each color is used to continuously scan and irradiate the quantum dot film layer at a uniform speed according to the corresponding distribution position in the second direction, so that quantum dots with uniform parameters are formed when the same ultrafast laser beam is scanned and irradiated.
[0015] The quantum dot array includes quantum dots corresponding to three colors, the quantum dots of the three colors are cyclically distributed in a first direction, and the quantum dots of the same color are distributed one by one in a second direction, and the first direction is perpendicular to the second direction;
[0016] Accordingly, the quantum dot film layer is scanned and irradiated by ultrafast lasers with different energy intensities, and quantum dots with uniform parameters are generated at the irradiation points with the same corresponding energy intensities. The quantum dots form a quantum dot array in the quantum dot film layer, including:
[0017] According to the number of cycles of the quantum dots of three colors in the first direction, the same number of ultrafast laser beams are generated respectively;
[0018] The ultrafast laser beam corresponding to each color is used to scan and irradiate the quantum dot film layer point by point according to the corresponding distribution position in the second direction, so that quantum dots with uniform parameters are formed when the same ultrafast laser beam is used for scanning and irradiation;
[0019] The area between the quantum dots is scanned and irradiated by the fourth ultrafast laser beam, and the quantum dots formed by the scanning and refraction of the fourth ultrafast laser beam are non-visible light quantum dots.
[0020] Wherein, according to the number of cycles of the quantum dots of three colors in the first direction, the same number of ultrafast laser beams are generated respectively, including:
[0021] The original laser beam emitted by the laser is subjected to energy shaping and shape shaping to generate ultrafast laser beams with the same number of cycles as the three colors of quantum dots in the first direction and energy intensities corresponding to the generated three colors of quantum dots.
[0022] Among them, the energy distribution of the ultrafast laser beam is a flat-top energy distribution.
[0023] The shape of the ultrafast laser beam is rectangular.
[0024] Among them, energy shaping and shape shaping are performed by beam shapers.
[0025] Each type of ultrafast laser performs multiple scanning irradiations.
[0026] In a second aspect, an embodiment of the present invention provides a micro OLED display module, which is manufactured by any manufacturing method of the first aspect.
[0027] In a third aspect, an embodiment of the present invention provides a display device, comprising the micro OLED display module of the second aspect.
[0028] In a micro OLED display module manufacturing method, micro OLED display module and display device provided by an embodiment of the present invention, a driving substrate is manufactured based on a silicon-based substrate; an OLED light-emitting device and a first encapsulation layer are sequentially added to the driving substrate; a quantum dot film layer is generated on the first encapsulation layer; the quantum dot film layer is scanned and irradiated by ultrafast lasers with different energy intensities, quantum dots with uniform parameters are generated at the irradiation positions with the same corresponding energy intensities, and the quantum dots form a quantum dot array in the quantum dot film layer; a second encapsulation layer is added on the quantum dot film layer. A quantum dot array is formed by scanning and irradiating the quantum dot film layer with ultrafast lasers with different energy intensities, and the quantum dots in the quantum dot array correspond to pixel points, thereby simplifying the preparation process of micro OLED; using quantum dots to realize the role of pixel points improves the display color gamut and enriches the use scenarios of the prepared micro OLED display module. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Other features, objects and advantages of the present application will become more apparent by reading the detailed description of non-limiting embodiments made with reference to the following drawings:
[0030] Figure 1 is a method flow chart of a method for manufacturing a micro OLED display module provided in an embodiment of the present application;
[0031] Figure 2 is a schematic diagram of the hierarchical structure of the micro OLED display module provided in an embodiment of the present application;
[0032] Figure 3 is a schematic diagram of energy shaping of an original laser beam in an embodiment of the present application;
[0033] Figure 4 is a schematic diagram of shaping the original laser beam in an embodiment of the present application;
[0034] Figure 5 is a schematic diagram of the first scanning irradiation process provided in an embodiment of the present application;
[0035] Figure 6 It is a schematic diagram of the second scanning irradiation process provided in an embodiment of the present application. DETAILED DESCRIPTION
[0036] The present application will be further described in detail below in conjunction with the accompanying drawings and embodiments. It will be appreciated that the specific embodiments described herein are intended to explain the present application, rather than to limit the present application. It should also be noted that, for ease of description, only portions of the present application, rather than all structures, are shown in the accompanying drawings. Based on the embodiments in the present application, all other embodiments obtained by those of ordinary skill in the art without creative work are within the scope of protection of the present application.
[0037] The terms "first", "second", "third" and "fourth" etc. in the specification and claims of the present application and the drawings are used to distinguish different objects, rather than to describe a specific order. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device that includes a series of steps or units is not limited to the listed steps or units, but optionally includes steps or units that are not listed, or optionally includes other steps or units inherent to these processes, methods, products or devices.
[0038] Reference to "embodiments" herein means that a particular feature, result, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments to form optional implementation methods.
[0039] The following describes the various embodiments of the present invention in detail.
[0040] Figure 1A method flow chart of a method for manufacturing a micro OLED display module is provided for an embodiment of the present invention. The micro OLED display module manufacturing method is used to manufacture a micro OLED display module. The prepared micro OLED display module can realize the arrangement of different RGB pixels in a micro area, thereby realizing the full color of the micro OLED display module, and has the characteristics of high PPI, high color gamut, and high luminous efficiency. Please refer to Figure 1 The micro OLED display module manufacturing method in the embodiment of the present invention includes:
[0041] Step S110: manufacturing a driving substrate based on a silicon-based substrate.
[0042] Step S120: adding an OLED light-emitting device and a first encapsulation layer on the driving substrate in sequence.
[0043] Step S110 and step S120 belong to the process of manufacturing the basic functional components of the micro OLED display module. The micro OLED display module to be manufactured in the embodiment of the present invention can be generally regarded as a hierarchical structure. Figure 2 For reference, the top is the light emitting surface, and from bottom to top are the driving substrate 110, the OLED light emitting device 120, the first encapsulation layer 130, the quantum dot film layer 140 and the second encapsulation layer 150. In the embodiment of the present invention, due to the high PPI, the driving substrate is manufactured on the basis of the silicon-based substrate. The driving substrate is used to drive and control the light source of the micro OLED display module. The light source of the micro OLED display module is an OLED light emitting device, such as a blue light emitting layer. The specific preparation method of the OLED light emitting device is in accordance with the current general preparation method, for example, an anode, a hole injection layer, a hole transport layer, a blue light emitting layer (or a blue light auxiliary layer), an electron transport layer, an electron injection layer, a cathode, etc. are prepared on another silicon-based substrate to obtain a layered OLED light emitting device 120, which is attached to the driving substrate 110, and the specific light emitting position is driven and controlled by the driving substrate 110. The first encapsulation layer 130 is set on the OLED light emitting device 120, thereby completing the preparation of the OLED light source and the light source driving part.
[0044] Step S130: generating a quantum dot film layer on the first encapsulation layer.
[0045] Steps S130 to S140 are used to manufacture a pixel array for displaying a picture based on an OLED light source. Compared with the prior art in which a pixel array is often manufactured by using a color film, this solution comprehensively optimizes the manufacturing process of the pixel array.
[0046] The pixel points in the embodiment of the present application are obtained by processing a completely covered film layer, namely, the quantum dot film layer 140. The quantum dot film layer 140 can be formed on the outer side of the first encapsulation layer 130 (ie, Figure 2 A layer of organic material is coated on the first encapsulation layer 130 as a flat layer (if the first encapsulation layer 130 adopts TEF encapsulation, a flat layer is required, but if glass encapsulation is adopted, no flat layer is required), and then the quantum dot film layer 140 is directly coated or inkjet printed on the flat layer. The quantum dot film layer 140 can also be prepared by first coating or inkjet printing on another substrate, and then the substrate with the quantum dot film layer 140 is attached to the first encapsulation layer 130.
[0047] When generating the quantum dot film layer 140, in order to ensure the light conversion efficiency and the uniformity and luminous intensity of the quantum dot film layer 140, the thickness of the quantum dot film layer 140 is set to 50-150nm. The quantum dot film layer 140 can be directly set as a blue light quantum dot film layer, and can be converted into a green light quantum dot film layer or a red light quantum dot film layer in a fixed area in the subsequent ultrafast laser annealing process.
[0048] The quantum dot material is composed of elements of IV, II-VI, IV-VI or III-V, ZnCdSe, CdSe, CdS, CdTe, CuInS, ZnCuInS, PdS, PdSe and one or more of germanium quantum dots, carbon quantum dots and perovskite quantum dots.
[0049] Step S140: Scanning and irradiating the quantum dot film layer with a plurality of ultrafast lasers of different energy intensities, generating quantum dots with uniform parameters at irradiation positions with the same corresponding energy intensities, and the quantum dots form a quantum dot array in the quantum dot film layer.
[0050] In the specific process of forming the quantum dot array, the production process can be further refined according to the distribution of the original laser beam and / or the quantum dots, and even the type of the initially generated quantum dot film layer.
[0051] For example Figure 3As shown, the original laser beam 221 can be energy shaped. The energy distribution of the ultrafast laser directly excited by the general laser satisfies the Gaussian distribution, but the energy distribution of the Gaussian distribution is not uniform. For the annealing of inorganic thin films (component types of the quantum dot film layer 140), the energy is not easy to control, so it is necessary to shape the Gaussian energy distribution into a flat-top energy distribution. The original laser beam 221 with a Gaussian energy distribution can be shaped into an intermediate laser beam 222 with a flat-top energy distribution by a beam shaper 210, so that the energy distribution is uniform within the range of the laser spot, which is conducive to the control of the overall energy during the annealing process, avoiding damage to the underlying OLED light-emitting device due to excessive local energy of the laser spot, and improving the process consistency during manufacturing.
[0052] like Figure 4 As shown, on the basis of energy shaping, the shape of the beam can be further shaped by the beam shaper 210, so that the spot formed by the intermediate laser beam 222 obtained in the vertical irradiation is rectangular and the energy distribution is uniform. Generally speaking, the shape of the laser spot is circular. Since the processing object of the laser annealing in the embodiment of the present application is mainly a whole inorganic thin film, which belongs to surface processing, if it is a circular spot, it will affect the uniformity of the surface processing. Therefore, it is necessary to shape the spot shape, and shape the laser spot shape from circular to rectangular.
[0053] like Figure 4 As shown, for the intermediate laser beam 222 obtained by shaping, a grating 310 can also be added at the same time, so that the rectangular intermediate laser beam 222 can be transformed into multiple ultrafast laser beams 223. The addition of the grating 310 can realize differential scanning of the plane and realize processing of different positions of the quantum dot pixel structure. At the same time, the introduction of the grating can realize surface scanning, greatly improving production efficiency. The energy indicators of the ultrafast laser beam 223 corresponding to different types of pixels are different, but the overall generation principle is the same.
[0054] The quantum dot film layer is scanned and irradiated based on the ultrafast laser beam 223, mainly using the quantum dot film layer under the action of the ultrafast laser to achieve the formation of crystal nuclei and the growth of grains. The size range of quantum dot grains can be controlled by controlling the energy of the laser, and the quantum dot particle size can also be controlled by the number of scans. For example, by increasing the number of scans, low pulse energy, multiple scans can effectively protect the quantum dots from damage while completing annealing. However, due to the limitation of processing speed, the number of repeated scans generally does not exceed 5 times.
[0055] The specific scanning method can be designed according to the type of pixel points and quantum dot film layers.
[0056] For example, each pixel (three types in total, R, G and B) needs to be annealed by the quantum dot film layer. The details can be adjusted according to the arrangement of the pixels, that is, the arrangement of the quantum dots.
[0057] An exemplary arrangement is as follows: Figure 5 As shown, the quantum dot array includes quantum dots corresponding to three colors (red quantum dots 141, green quantum dots 142, and blue quantum dots 143). The quantum dots of the three colors are cyclically distributed in the first direction, and the quantum dots of the same color are continuously distributed in the second direction. The first direction is perpendicular to the second direction. Because the luminous color of quantum dots is actually when irradiated with white light, only the irradiated area emits a certain color of light, so a row or a column of quantum dots of the same type can be continuously distributed.
[0058] Accordingly, a quantum dot array can be formed specifically through step S141 and step S142:
[0059] Step S141: generating the same number of ultrafast laser beams respectively according to the number of cycles of the quantum dots of three colors in the first direction.
[0060] The number of ultrafast laser beams can be the same as the number of cycles, that is, for the same type of pixel points, all scanning irradiation is completed at one time to achieve pixel point generation. In the specific shaping process, the original laser beam emitted by the laser is subjected to energy shaping and shape shaping to generate ultrafast laser beams with the same number of cycles as the three colors of quantum dots in the first direction and energy intensity as the generation of three colors of quantum dots. In fact, it can also be less than the number of cycles, that is, for the same type of pixel points, the generation of pixel points can be completed with a scanning number that is less than the number of rows or columns.
[0061] Step S142: The ultrafast laser beam corresponding to each color is used to continuously scan and irradiate the quantum dot film layer at a uniform speed according to the corresponding distribution position in the second direction, so as to form quantum dots with uniform parameters when the same ultrafast laser beam is used for scanning and irradiation.
[0062] This direction is equivalent to multi-pulse processing, such as Figure 5 As shown, corresponding to the three pixel points, three ultrafast laser beams are generated, namely the first laser beam 223r, the second laser beam 223g and the third laser beam 223b, which respectively scan and irradiate the quantum dot film layer 140 continuously at a uniform speed and polarity, thereby correspondingly forming red quantum dots 141, green quantum dots 142 and blue quantum dots 143 with the same parameters.
[0063] Another exemplary arrangement is as follows: Figure 6As shown, the quantum dot array includes quantum dots corresponding to three colors (red quantum dots 141, green quantum dots 142 and blue quantum dots 143). The quantum dots of the three colors are distributed cyclically in the first direction, and the quantum dots of the same color are distributed one by one in the second direction. The first direction is perpendicular to the second direction. For this distribution method, it is equivalent to that each quantum dot is separated from each other. In the embodiment of the present application, the area between the quantum dots is defined as the separation area 144.
[0064] Accordingly, a quantum dot array can be formed specifically through step S143 and step S145:
[0065] Step S143: Generate the same number of ultrafast laser beams respectively according to the number of cycles of the quantum dots of three colors in the first direction.
[0066] The implementation process of step S143 is substantially the same as that of step S141 and will not be repeated here.
[0067] Step S144: the ultrafast laser beam corresponding to each color is used to scan and irradiate the quantum dot film layer point by point according to the corresponding distribution position in the second direction, so that quantum dots with uniform parameters are formed when the same ultrafast laser beam is used for scanning and irradiation.
[0068] The difference between step S144 and step S142 is that after completing the scanning of one quantum dot, a section is skipped to enter the scanning irradiation of the next quantum dot, thereby forming the separation of each quantum dot.
[0069] Step S145: Scanning and irradiating the area between the quantum dots with the fourth ultrafast laser beam. The quantum dots formed by scanning and refraction of the fourth ultrafast laser beam are non-visible light quantum dots.
[0070] In addition to scanning the quantum dots, the separation area 144 between the quantum dots is also scanned and irradiated by the corresponding ultrafast laser beam, and the fourth type of quantum dots are formed accordingly. The fourth type of quantum dots are non-visible light quantum dots, and non-visible light refers to near-infrared light. This processing method can be regarded as single-pulse processing, which can achieve independent distribution of pixel points and convert the separation area 144 between quantum dots of the same color into non-visible light quantum dots. When actually displayed, the non-visible light quantum dots display near-infrared light, which can effectively relieve eye fatigue, help soothe the eyes, and prevent myopia.
[0071] It should be noted that the above is an exemplary implementation method. In the specific implementation process, the initially set quantum dot layer film may be a film layer that can realize a type of pixel point, such as a blue light quantum dot layer film. At this time, only laser annealing is actually required to form red quantum dots and green quantum dots. The number of ultrafast laser beams mentioned above, the number of scanning irradiation times and positions are adjusted, that is, there is a type of pixel that can generate corresponding quantum dots without laser annealing or with laser annealing, thereby further simplifying the production process.
[0072] Step S150: adding a second encapsulation layer on the quantum dot film layer.
[0073] Since the properties of the OLED light emitting device 120 and the quantum dot film layer 140 are easily degraded when they encounter air or water vapor, special precautions need to be taken against water and oxygen in the overall hierarchical structure, and a first encapsulation layer 130 is provided on the OLED light emitting device 120, and a second encapsulation layer 150 is added on the quantum dot film layer 140. The micro OLED display module manufactured above can be further fully encapsulated by TFE encapsulation or glass encapsulation.
[0074] In general, the size of quantum dot nanoparticles after annealing is controlled by controlling the number of scans or energy, thereby achieving full-color display. Only one quantum dot nanofilm preparation is required, and no photolithography is required to achieve the distribution of quantum dot pixels. It is only necessary to adjust the laser distribution through the grating and cooperate with the blue light OLED pixel definition area to realize the realization of RGB quantum dot pixels. The entire processing process is simple, and only one quantum dot color film preparation is required; full colorization is simple to achieve, and no multiple photolithography is required to form a pixel structure; the processing cost is low, and the required equipment is the equipment currently used for screen preparation, and the processing technology is greatly simplified. The final product of the micro OLED display module has a good display effect, because the laser processing accuracy is high, and through optical path modulation, 2um pixel preparation can be achieved, and the processing accuracy of more than 4000ppi can be achieved. It can meet the needs of near-eye display. After using quantum dots, the color gamut can be effectively improved, and it is better than the current OLED color gamut, greater than 110% NTSC. Due to the high conversion effect of quantum dots, it can reach a high brightness of more than 80%, which is much higher than the conversion effect of color resistance, and can be applied to richer scenes.
[0075] The embodiments of the present application further provide a micro OLED display module manufactured based on the micro OLED display module manufacturing method described above, and a display device including the micro OLED display module, which have the same beneficial effects.
[0076] It should be noted that in the embodiments of the present application, some common technologies in the art are not elaborated in detail. Corresponding traditional technologies, such as laser, can be used when implementing this solution.
[0077] It should also be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, commodity or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, commodity or device. In the absence of more restrictions, the elements defined by the sentence "comprises a ..." do not exclude the existence of other identical elements in the process, method, commodity or device including the elements.
[0078] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A method for manufacturing a micro OLED display module, characterized in that: include: Manufacturing a driving substrate based on a silicon-based substrate; Adding an OLED light-emitting device and a first encapsulation layer on the driving substrate in sequence; generating a quantum dot film layer on the first encapsulation layer; Scanning and irradiating the quantum dot film layer with a plurality of ultrafast lasers of different energy intensities to generate quantum dots with uniform parameters at irradiation positions corresponding to the same energy intensities, wherein the quantum dots form a quantum dot array in the quantum dot film layer; A second encapsulation layer is added on the quantum dot film layer.
2. The method for manufacturing a micro OLED display module according to claim 1, wherein: The quantum dot array includes quantum dots corresponding to three colors, the quantum dots of the three colors are cyclically distributed in a first direction, and the quantum dots of the same color are continuously distributed in a second direction, and the first direction is perpendicular to the second direction; Accordingly, the quantum dot film layer is scanned and irradiated by a plurality of ultrafast lasers with different energy intensities, and quantum dots with uniform parameters are generated at irradiation points with the same corresponding energy intensities, and the quantum dots form a quantum dot array in the quantum dot film layer, including: According to the number of cycles of the three colors of quantum dots in the first direction, the same number of ultrafast laser beams are generated respectively; The ultrafast laser beam corresponding to each color is used to continuously scan and irradiate the quantum dot film layer at a uniform speed according to the corresponding distribution position in the second direction, so that quantum dots with uniform parameters are formed when the same ultrafast laser beam is scanned and irradiated.
3. The method for manufacturing a micro OLED display module according to claim 1, wherein: The quantum dot array includes quantum dots corresponding to three colors, the quantum dots of the three colors are cyclically distributed in a first direction, and the quantum dots of the same color are distributed one by one in a second direction, and the first direction is perpendicular to the second direction; Accordingly, the quantum dot film layer is scanned and irradiated by a plurality of ultrafast lasers with different energy intensities, and quantum dots with uniform parameters are generated at irradiation points with the same corresponding energy intensities, and the quantum dots form a quantum dot array in the quantum dot film layer, including: According to the number of cycles of the three colors of quantum dots in the first direction, the same number of ultrafast laser beams are generated respectively; Scanning and irradiating the quantum dot film layer point by point with an ultrafast laser beam corresponding to each color according to the corresponding distribution position in the second direction, so as to form quantum dots with uniform parameters when the same ultrafast laser beam is scanned and irradiated; The area between the quantum dots is scanned and irradiated by a fourth ultrafast laser beam, and the quantum dots formed by the scanning and refraction of the fourth ultrafast laser beam are non-visible light quantum dots.
4. The method for manufacturing a micro OLED display module according to claim 2 or 3, wherein: The method of generating the same number of ultrafast laser beams according to the number of cycles of the three colors of quantum dots in the first direction comprises: The original laser beam emitted by the laser is subjected to energy shaping and shape shaping to generate ultrafast laser beams with the same number as the number of cycles of the three colors of quantum dots in the first direction and energy intensity corresponding to the generation of the three colors of quantum dots.
5. The method for manufacturing a micro OLED display module according to claim 4, wherein: The energy distribution of the ultrafast laser beam is a flat-top energy distribution.
6. The method for manufacturing a micro OLED display module according to claim 4, wherein: The shape of the ultrafast laser beam is rectangular.
7. The method for manufacturing a micro OLED display module according to claim 4, wherein: The energy shaping and shape shaping are performed by a beam shaper.
8. The method for manufacturing a micro OLED display module according to any one of claims 1 to 3, wherein: Each ultrafast laser performs multiple scanning irradiations.
9. A micro OLED display module, characterized in that: The micro OLED display module is manufactured by the manufacturing method according to any one of claims 1 to 8.
10. A display device, characterized in that: Including the micro OLED display module according to claim 9.