Method for manufacturing wiring structure

By forming a modified region and bonding the conductor layer in the manufacturing of a semiconductor device, the problem of uneven dissolution of the conductor layer is solved, the yield and manufacturing efficiency of the wiring structure are improved, and the integrity of the wiring is ensured.

CN119096349APending Publication Date: 2024-12-06RESONAC CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202280095270.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2022-10-24
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

In the manufacturing of the wiring structure of a semiconductor device, uneven dissolution of the conductor layer leads to a decrease in yield, and some wiring is removed by mistake.

Method used

A modified region is formed on the support substrate, and a conductor layer is formed in an adhesion manner, thereby improving the adhesion between the conductor layer and the support substrate, thereby stably forming the conductor layer, reducing dissolution unevenness, and ensuring the integrity of the wiring.

Benefits of technology

By improving the adhesion between the conductor layer and the support substrate, the yield of the wiring structure is improved, the uneven dissolution problem during the removal of the conductor layer is reduced, and the integrity of the wiring and manufacturing efficiency are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119096349A_ABST
    Figure CN119096349A_ABST
Patent Text Reader

Abstract

The invention discloses a method for manufacturing a wiring structure. This method for manufacturing a wiring structure includes: a step for forming, on a support substrate, a modified region that is exposed on the main surface along the main surface of the support substrate; a step for forming a conductor layer on the main surface so as to be in close contact with the modified region; a step for forming a wiring on the conductor layer; a step for forming an insulating layer on the conductor layer so as to cover the wiring; a step for peeling off the support substrate from the conductor layer; and a step for removing the conductor layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a wiring structure. Background Art

[0002] In a wiring structure for a semiconductor device, an ETS (Embedded Trace Substrate) method is known as a method for forming wiring at a high density (see Patent Documents 1 and 2). In the ETS method, for example, a conductor layer serving as a seed layer is formed on a support substrate, and wiring is formed on the conductor layer by electrolytic plating or the like. Then, an insulating layer is formed to cover the wiring, and the support substrate and the conductor layer are removed.

[0003] Previous technical literature

[0004] Patent Literature

[0005] Patent Document 1: U.S. Patent No. 10622292

[0006] Patent Document 2: U.S. Patent No. 10483196 Summary of the invention

[0007] Technical issues to be solved by the invention

[0008] The conductor layer that functions as a seed layer can be removed by, for example, dissolving it with an etching solution. When removing the conductor layer, the degree of dissolution may be uneven. In this case, for example, excessive dissolution of a portion of the conductor layer may sometimes result in the removal of the wiring formed on the conductor layer. As a result, the yield rate is reduced in the manufacture of the wiring structure.

[0009] An object of the present invention is to provide a method for manufacturing a semiconductor device, which can improve the yield in manufacturing a wiring structure.

[0010] Means for solving technical problems

[0011] One aspect of the present invention relates to a method for manufacturing a wiring structure. The method comprises: forming a modified region on a supporting substrate along a main surface of the supporting substrate and exposed on the main surface; forming a conductor layer on the main surface in a manner closely fitting the modified region; forming wiring on the conductor layer; forming an insulating layer on the conductor layer in a manner covering the wiring; peeling the supporting substrate from the conductor layer; and removing the conductor layer.

[0012] In the manufacturing method, a modified region exposed on the main surface is formed on the support substrate, and a conductor layer is formed on the main surface of the support substrate in a manner that is in close contact with the modified region. In this case, the close contact of the conductor layer with respect to the support substrate is improved by the modified region. Thus, the conductor layer can be stably formed on the support substrate, for example, the conductor layer can be formed thinly. The thinner the conductor layer is, the shorter the time required to remove the conductor layer can be, so the degree of dissolution of the conductor layer is less likely to be uneven. Therefore, when removing the conductor layer, it is possible to suppress the removal of the wiring formed on the conductor layer. Therefore, according to the manufacturing method, the yield rate in the manufacture of the wiring structure can be improved.

[0013] In the method for manufacturing the wiring structure, the modified region may have holes communicating with the main surface. In this case, a portion of the conductor layer enters the holes in the modified region, and the adhesion between the support substrate and the conductor layer is improved by the anchor effect.

[0014] In the method for manufacturing the wiring structure, in the step of forming the modified region, the modified region may be formed by subjecting the support substrate to a plasma treatment. In this case, the modified region can be formed more reliably in the support substrate.

[0015] In the method for manufacturing the wiring structure, the adhesion strength between the conductor layer and the modified region may be 0.1 to 1.0 N / mm. When the adhesion strength between the conductor layer and the modified region is 0.1 N / mm or more, the conductor layer can be formed on the support substrate more stably. When the adhesion strength between the conductor layer and the modified region is 1.0 N / mm or less, the support substrate can be easily peeled off in the step of peeling the support substrate off the conductor layer.

[0016] In the method for manufacturing the wiring structure, the thickness of the modified region may be 50 nm to 500 nm. When the thickness of the modified region is 50 nm or more, sufficient adhesion with the conductor layer can be ensured. When the thickness of the modified region is 500 nm or less, the modified region can be prevented from becoming fragile.

[0017] In the method for manufacturing the wiring structure, the thickness of the conductor layer may be 50 nm to 1 μm. When the thickness of the conductor layer is 50 nm or more, the resistance during power supply can be reduced when the conductor layer is formed by electrolytic plating, so electrolytic plating can be easily performed. When the thickness of the conductor layer is 1 μm or less, the time required to remove the conductor layer can be further shortened.

[0018] In the method for manufacturing the wiring structure, the process of forming the wiring may include: forming a resist on the conductor layer; forming an opening pattern on the resist to expose the conductor layer; filling the opening pattern with a conductive material by electrolytic plating to form the wiring; and removing the resist. In this case, fine wiring can be easily formed.

[0019] In the above-mentioned method for manufacturing a wiring structure, the resist may be formed of a photosensitive material. In this case, a fine pattern can be formed through exposure and development steps.

[0020] In the above-mentioned method for manufacturing a wiring structure, the insulating layer may be formed of a thermosetting resin. In this case, the adhesiveness of the insulating layer to the wiring can be improved.

[0021] In the method for manufacturing the wiring structure, after the step of forming the insulating layer, a series of steps including the step of forming another conductor layer on the insulating layer, the step of forming another wiring on the other conductor layer, and the step of forming another insulating layer so as to cover the other wiring can be performed one or more times to form a plurality of stacked wiring layers. In this case, a wiring structure including multilayered wiring layers can be manufactured.

[0022] Effects of the Invention

[0023] According to an aspect of the present invention, it is possible to improve the yield in manufacturing a semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 middle, Figure 1 (a) and Figure 1 (b) is a cross-sectional view showing a method for manufacturing a wiring structure according to one embodiment.

[0025] Figure 2 middle, Figure 2 (a) and Figure 2 (b) is a cross-sectional view showing a method for manufacturing a wiring structure according to one embodiment.

[0026] Figure 3 middle, Figure 3 (a) and Figure 3 (b) is a cross-sectional view showing a method for manufacturing a wiring structure according to one embodiment.

[0027] Figure 4 middle, Figure 4 (a) and Figure 4 (b) is a cross-sectional view showing a method for manufacturing a wiring structure according to one embodiment.

[0028] Figure 5It is a cross-sectional view showing a method for manufacturing a wiring structure according to an embodiment.

[0029] Figure 6 middle, Figure 6 (a) and Figure 6 (b) is a cross-sectional view showing a method for manufacturing a wiring structure according to a modification example.

[0030] Figure 7 It is a cross-sectional view showing a method of manufacturing a wiring structure according to a modification. DETAILED DESCRIPTION

[0031] Hereinafter, several embodiments of the present invention will be described in detail with reference to the accompanying drawings as needed. In the following description, the same or equivalent parts are marked with the same component symbols, and repeated descriptions are omitted. In addition, as for the positional relationship such as up, down, left, and right, unless otherwise specified, it is based on the positional relationship shown in the accompanying drawings. In addition, the dimensional ratios of the accompanying drawings are not limited to the ratios shown in the drawings.

[0032] In this specification, the numerical range indicated by "~" includes the numerical values ​​before and after "~" as the minimum value and the maximum value, respectively. In the numerical range recorded in stages in this specification, the upper limit value or lower limit value recorded in one numerical range can be replaced by the upper limit value or lower limit value in the numerical range recorded in other stages. Furthermore, in the numerical range recorded in this specification, the upper limit value or lower limit value of the numerical range can be replaced by the value shown in the embodiments.

[0033] refer to Figure 1 to Figure 5 , a wiring structure 1 (reference Figure 6 ) is described below. Figure 1 to Figure 5 2 is a cross-sectional view showing a method for manufacturing the wiring structure 1. The wiring structure 1 can be applied to a semiconductor device. For example, in a semiconductor device, the wiring structure 1 can be used to connect semiconductor chips. The wiring structure 1 is manufactured using, for example, an ETS (Embedded Trace Substrate) method.

[0034] The wiring structure 1 is produced, for example, through the following steps (a) to (f).

[0035] (a) A step of forming, on the supporting substrate 2 , the reformed region 21 along the main surface 2 a of the supporting substrate 2 and exposed on the main surface 2 a .

[0036] (b) A step of forming the conductive layer 3 on the main surface 2 a so as to be in close contact with the reformed region 21 .

[0037] (c) A step of forming the wiring 5 on the conductor layer 3 .

[0038] (d) A step of forming the insulating layer 6 on the conductor layer 3 so as to cover the wiring 5 .

[0039] (e) A step of peeling the supporting substrate 2 from the conductive layer 3 .

[0040] (f) Step of removing the conductor layer 3.

[0041] [Step (a)]

[0042] refer to Figure 1 (a) of step (a) is described. Step (a) is a step of forming a modified region 21 on a supporting substrate 2. In step (a), first, a supporting substrate 2 is prepared. The supporting substrate 2 may be, for example, a silicon plate, a glass plate, a SUS (stainless steel) plate, or a substrate with glass cloth inserted. The supporting substrate 2 is preferably a substrate with high rigidity.

[0043] The thickness of the support substrate 2 can be, for example, 0.2 mm to 2.0 mm. When the thickness of the support substrate 2 is 0.2 mm or more, the operation becomes easy. On the other hand, when the thickness of the support substrate 2 is 2.0 mm or less, the material cost of the wiring structure 1 can be suppressed. The support substrate 2 can be in the form of a wafer or a panel. The size of the support substrate 2 is not limited. The support substrate 2 can be a wafer-shaped substrate with a diameter of 200 mm, 300 mm, or 450 mm, or a rectangular panel-shaped substrate with a side of 300 mm to 700 mm.

[0044] Next, a modified region 21 is formed on the support substrate 2. The modified region 21 is formed along the main surface 2a of the support substrate 2 and exposed on the main surface 2a. The modified region 21 is formed in a layer on the support substrate 2. The thickness of the modified region 21 can be, for example, 50nm to 500nm. The modified region 21 can be formed on the entire surface of the main surface 2a, or on a portion of the main surface 2a. The modified region 21 has pores connected to the main surface 2a. The size of the pores measured by a transmission electron microscope or a scanning electron microscope can be, for example, 50 to 500nm. The size of the pores is not limited. A portion of the conductor layer 3 described later enters the pores of the modified region 21. By the conductor layer 3 entering the pores of the modified region 21, the adhesion between the support substrate 2 and the conductor layer 3 is improved by the anchoring effect. That is, the modified region 21 acts as a bonding layer that is closely bonded to the conductor layer 3.

[0045] The modified region 21 can be formed, for example, by subjecting the support substrate 2 to plasma treatment. The plasma used in the plasma treatment can be, for example, oxygen plasma, argon plasma, nitrogen plasma, helium plasma, or fluorine-containing plasma. As an example, when the support substrate 2 is a silicon plate, a glass plate, or a SUS plate, the modified region 21 can be appropriately formed by using fluorine-containing plasma. The method for forming the modified region 21 is not limited. The modified region 21 can be formed, for example, by using ozone water modification or ultraviolet-ozone modification.

[0046] [Step (b)]

[0047] refer to Figure 1 (b) is used to describe step (b). Step (b) is a step of forming a conductor layer 3 on the main surface 2a in a manner that is in close contact with the modified region 21. The conductor layer 3 is composed of one layer or a plurality of stacked layers. The conductor layer 3 can be formed of, for example, Ti, Ni, NiP, NiB, Co, TaW or CoNiP. The formation method of the conductor layer 3 can be, for example, electroless plating, sputtering or coating. The thickness of the conductor layer 3 can be 50nm to 1μm, or 50nm to 500nm.

[0048] The conductor layer 3 is formed directly on the main surface 2a (modified region 21) of the support substrate 2. The conductor layer 3 formed on the support substrate 2 is in close contact with the modified region 21 as described above. The adhesion strength between the conductor layer 3 and the modified region 21 can be, for example, 0.1 to 1.0 N / mm, or 0.5 to 1.0 N / mm. The adhesion strength is measured by a 90° peel test using Autograph. The peel test conditions are not particularly limited, for example, the peel test piece width is 10 mm, and the peel speed is 10 mm / min.

[0049] [Step (c)]

[0050] refer to Figure 2 and Figure 3 Step (c) is described below. Step (c) is a step of forming wiring 5 on the conductor layer 3. In step (c), first, Figure 2 As shown in (a), a resist 4 is formed on the conductor layer 3. The resist 4 is a resist for forming wiring (circuit). The resist 4 can be formed of a photosensitive material, for example. The photosensitive material can have insulating properties. The resist 4 can be a commercially available resist. As a commercially available resist, a negative film-like photosensitive resist (Showa Denko Materials Co., Ltd., Photec RY-5107UT) can be cited.

[0051] Then, if Figure 2As shown in (b), an opening pattern 41 (resist pattern) is formed on the resist 4. The opening pattern 41 penetrates the resist 4 in the thickness direction of the resist 4. In the opening pattern 41, the conductor layer 3 is exposed. In the case where the resist 4 is formed of a photosensitive material, the opening pattern 41 can be formed by exposing and developing the resist 4. As an example, first, a roll laminator is used to form (film-form) the resist 4. Next, a phototool (Phototool) having a pattern is brought into close contact with the resist 4 and exposed using an exposure machine. Then, the opening pattern 41 is formed, for example, by spraying and developing with an aqueous sodium carbonate solution. A positive photosensitive resist can also be used instead of a negative photosensitive resist. The width of the opening pattern 41 can be, for example, 1μm to 30μm, 3μm to 30μm, or 5μm to 30μm.

[0052] Then, if Figure 3 As shown in (a), the opening pattern 41 is filled with a conductive material to form a wiring 5. The wiring 5 can be formed, for example, by supplying power to the conductor layer 3 and performing electrolytic plating. The electrolytic plating can be, for example, electrolytic copper plating. The thickness of the wiring 5 can be, for example, 1 μm to 10 μm, 3 μm to 15 μm, or 5 μm to 20 μm. Next, as Figure 3 As shown in (b), the resist 4 is peeled off and removed. The resist 4 can be peeled off using a commercially available peeling liquid.

[0053] [Step (d)]

[0054] refer to Figure 4 (a) is used to explain step (d). Step (d) is a step of forming an insulating layer 6 on the conductor layer 3 in a manner covering the wiring 5. The wiring 5 is embedded in the insulating layer 6. The insulating layer 6 can be formed of, for example, a thermosetting resin. The insulating layer 6 can be, for example, a laminated material, glass cloth, or an insulating material containing an inorganic filler.

[0055] The material of the insulating layer 6 can be a liquid or film-like material. From the viewpoint of improving the embedding property of the wiring 5, the material of the insulating layer 6 is preferably a film-like material. When a film-like insulating material is used, the lamination process of the insulating material is preferably a low-temperature process, and the insulating material is preferably a photosensitive insulating film or a thermosetting insulating film that can be laminated at 40°C to 120°C. The insulating film that can be laminated at a temperature of 40°C or above does not become too viscous at room temperature and tends to have good operability. In contrast, the insulating film that can be laminated at a temperature of 120°C or below tends to have less warping after lamination.

[0056] From the viewpoint of suppressing warpage, the thermal expansion coefficient of the insulating layer 6 after curing is preferably 80 ppm / °C or less, and from the viewpoint of obtaining high reliability, it is more preferably 70 ppm / °C or less. From the viewpoint of obtaining stress relaxation of the insulating material and a high-definition pattern, the thermal expansion coefficient of the insulating layer 6 after curing is preferably 20 ppm / °C or more. The thickness of the insulating layer 6 may be 5 μm to 50 μm, or 10 μm to 30 μm.

[0057] [Step (e)]

[0058] refer to Figure 4 (b) is used to explain step (e). Step (e) is a step of peeling the support substrate 2 from the conductor layer 3. The peeling of the support substrate 2 can be performed manually or using a dedicated peeling device. By peeling the support substrate 2, the surface of the conductor layer 3 opposite to the insulating layer 6 is exposed.

[0059] [Step (f)]

[0060] refer to Figure 5 Step (f) is described below. Step (f) is a step of removing the conductor layer 3. The conductor layer 3 is removed, for example, by etching. The etching for removing the conductor layer 3 can be performed using a commercially available etching solution. For example, when the conductor layer 3 is formed of Ti, a Ti etching solution (manufactured by Mitsubishi Gas Chemical Company, Inc., WLC-T) can be used. When the conductor layer 3 is formed of Ni, a Ni etching solution (manufactured by JCU CORPORATION, Ebastrip) can be used. The etching solution can be applied to the surface of the conductor layer 3 opposite to the insulating layer 6. Through the above steps, as shown in FIG. Figure 5 As shown, a wiring structure 1 including the wiring 5 and the insulating layer 6 is manufactured.

[0061] As described above, in the manufacturing method of the wiring structure 1 involved in the present embodiment, the modified region 21 exposed on the main surface 2a is formed on the support substrate 2, and the conductor layer 3 is formed on the main surface 2a of the support substrate 2 in a manner that is in close contact with the modified region 21. In this case, the close contact of the conductor layer 3 with respect to the support substrate 2 is improved by the modified region 21. Thus, the conductor layer 3 can be stably formed on the support substrate 2, for example, the conductor layer 3 can be formed thinly. The thinner the conductor layer 3 is, the shorter the time required to remove the conductor layer 3 can be, so the degree of dissolution of the conductor layer 3 is less likely to be uneven. Therefore, when removing the conductor layer 3, it is possible to suppress the wiring 5 formed on the conductor layer 3 from being removed at the same time. Therefore, according to this manufacturing method, the yield rate in the manufacture of the wiring structure 1 can be improved.

[0062] In the method for manufacturing wiring structure 1 of this embodiment, reformed region 21 has pores communicating with main surface 2a. In this case, part of conductor layer 3 enters the pores of reformed region 21, and adhesion between support substrate 2 and conductor layer 3 is improved by the anchor effect.

[0063] In the method for manufacturing the wiring structure 1 of the present embodiment, in the step (a) of forming the modified region 21, the modified region 21 can be formed by plasma processing the support substrate 2. In this case, the modified region 21 can be formed more reliably in the support substrate 2.

[0064] In the method for manufacturing the wiring structure 1 of the present embodiment, the adhesion strength between the conductor layer 3 and the modified region 21 can be 0.1 to 1.0 N / mm. When the adhesion strength between the conductor layer 3 and the modified region 21 is 0.1 N / mm or more, the conductor layer 3 can be formed more stably on the support substrate 2. When the adhesion strength between the conductor layer 3 and the modified region 21 is 1.0 N / mm or less, the support substrate 2 can be easily peeled off in the step (e) of peeling the support substrate 2 off the conductor layer 3.

[0065] In the manufacturing method of the wiring structure 1 of the present embodiment, the thickness of the modified region 21 can be 50 nm to 500 nm. When the thickness of the modified region 21 is 50 nm or more, sufficient adhesion with the conductor layer 3 can be ensured. When the thickness of the modified region 21 is 500 nm or less, the modified region 21 can be prevented from becoming fragile.

[0066] In the manufacturing method of the wiring structure 1 of the present embodiment, the thickness of the conductor layer 3 can be 50 nm to 1 μm. When the thickness of the conductor layer 3 is 50 nm or more, the resistance during power supply can be reduced when the conductor layer 3 is formed by electrolytic plating, so electrolytic plating can be easily performed. When the thickness of the conductor layer 3 is 1 μm or less, the time required to remove the conductor layer 3 can be further shortened.

[0067] In the manufacturing method of the wiring structure 1 of the present embodiment, the step (c) of forming the wiring 5 may include: a step of forming the resist 4 on the conductor layer 3; a step of forming an opening pattern 41 in which the conductor layer 3 is exposed on the resist 4; a step of filling the opening pattern 41 with a conductive material by electrolytic plating to form the wiring 5; and a step of removing the resist 4. In this case, fine wiring 5 can be easily formed.

[0068] In the method for manufacturing the wiring structure 1 of the present embodiment, the resist 4 may be formed of a photosensitive material. In this case, a fine pattern can be formed through exposure and development steps.

[0069] In the method for manufacturing the wiring structure 1 of the present embodiment, the insulating layer 6 may be formed of a thermosetting resin. In this case, the adhesiveness of the insulating layer 6 to the wiring 5 can be improved.

[0070] As mentioned above, although embodiment of this invention is described in detail, this invention is not limited to the said embodiment.

[0071] refer to Figure 6 and Figure 7 , for the wiring structure 1A according to the modification example (reference Figure 7 ) is described below. Figure 6 and Figure 7 1A is a cross-sectional view showing a method for manufacturing a wiring structure 1A. In the manufacturing method according to the modified example, after the step (d) of forming the insulating layer 6, a step of stacking another wiring layer on the insulating layer 6 is performed one or more times to form a plurality of stacked wiring layers. Specifically, first, as Figure 6 As shown in (a), after the step (d) of forming the insulating layer 6, a conductor layer 7 (seed layer) is formed on the insulating layer 6. The method for forming the conductor layer 7 may be the same as the method for forming the conductor layer 3. Next, a wiring 8 is formed on the conductor layer 7. The method for forming the wiring 8 may be the same as the method for forming the wiring 5.

[0072] Then, if Figure 6 As shown in (b), the exposed portion of the wiring 8 in the conductor layer 7 (the portion not overlapping with the wiring 8) is removed. As a result, the conductor layer 7 remaining on the insulating layer 6 functions as a wiring together with the wiring 5. When the conductor layer 7 is removed by etching, a commercially available etching solution can be used. For example, when the conductor layer 7 is formed of Ti, a Ti etching solution (manufactured by Mitsubishi Gas Chemical Company, Inc., WLC-T) can be used. When the conductor layer 7 is formed of Ni, a Ni etching solution (manufactured by JCU CORPORATION, Ebastrip) can be used.

[0073] Then, if Figure 7 As shown, an insulating layer 9 is formed on the insulating layer 6 in a manner covering the wiring 8 and the conductor layer 7. The wiring 8 and the conductor layer 7 are buried in the insulating layer 9. The method for forming the insulating layer 9 can be the same as the method for forming the insulating layer 6. Through the above series of steps, another wiring layer having wiring and an insulating layer is formed. That is, a wiring structure 1A having a plurality of wiring layers can be obtained. The series of steps for forming the above wiring layers can be implemented multiple times instead of just once. According to the manufacturing method of the wiring structure 1A involved in the modification example, a wiring structure 1A including a multilayered wiring layer can be manufactured.

[0074] Explanation of symbols

[0075] 1. 1A - wiring structure, 2 - supporting substrate, 2a - main surface, 3. 7 - conductor layer, 4 - resist, 5. 8 - wiring, 6. 9 - insulating layer, 21 - modified region, 41 - opening pattern.

Claims

1. A method for manufacturing a wiring structure, comprising: forming, on a supporting substrate, a modified region along a main surface of the supporting substrate and exposed on the main surface; forming a conductive layer on the main surface so as to be in close contact with the modified region; forming wiring on the conductor layer; forming an insulating layer on the conductor layer so as to cover the wiring; a step of peeling the supporting substrate from the conductive layer; and A step of removing the conductor layer.

2. The method for manufacturing a wiring structure according to claim 1, in, The modified region has pores communicating with the main surface.

3. The method for manufacturing a wiring structure according to claim 1 or 2, in, In the step of forming the modified region, the modified region is formed by subjecting the support substrate to a plasma treatment.

4. The method for manufacturing a wiring structure according to any one of claims 1 to 3, in, The adhesion strength between the conductor layer and the modified region is 0.1 N / mm to 1.0 N / mm.

5. The method for manufacturing a wiring structure according to any one of claims 1 to 4, in, The thickness of the modified region is 50nm to 500nm.

6. The method for manufacturing a wiring structure according to any one of claims 1 to 5, in, The conductor layer has a thickness of 50 nm to 1 μm.

7. The method for manufacturing a wiring structure according to any one of claims 1 to 6, in, The process of forming the wiring includes: forming a resist on the conductor layer; forming an opening pattern on the resist to expose the conductor layer; A step of filling the opening pattern with a conductive material by electrolytic plating to form the wiring; and A step of removing the resist.

8. The method for manufacturing a wiring structure according to claim 7, in, The resist is formed of a photosensitive material.

9. The method for manufacturing a wiring structure according to any one of claims 1 to 8, in, The insulating layer is formed of a thermosetting resin.

10. The method for manufacturing a wiring structure according to any one of claims 1 to 9, in, After the step of forming the insulating layer, a series of steps are performed one or more times to form a plurality of stacked wiring layers. The series of steps includes a step of forming another conductive layer on the insulating layer, a step of forming another wiring on the another conductive layer, and a step of forming another insulating layer so as to cover the another wiring.

Citation Information

Patent Citations

  • Embedded trace substrate structure and semiconductor package structure including the same

    US10483196B2

  • High density interconnects in an embedded trace substrate (ETS) comprising a core layer

    US10622292B2