Semiconductor device
By forming a low-concentration impurity layer on the semiconductor substrate and connecting the thick film metal plate with a conductive adhesive, the on-resistance and warping problems of the dual-structure longitudinal MOS transistor are solved, and the strength and adhesion of the chip are improved.
Patent Information
- Application Number
- CN202480002316.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-01-23
- Filing Date
- 2024-01-10
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-01-10
AI Technical Summary
The existing dual-structure longitudinal MOS transistors have shortcomings in terms of on-resistance and strength, especially the warping problem of semiconductor chips is large, which affects the adhesion degree and installation effect.
Using a chip-sized encapsulated semiconductor device mounted facing down, a low-concentration impurity layer is formed on the semiconductor substrate and a conductive adhesive is used to connect the support to the metal layer to form a thick film metal plate to support the semiconductor layer. Reduce on-resistance and reduce warpage.
It effectively reduces the on-resistance of the semiconductor chip, while also improving its strength, reducing the amount of warpage, enhancing the adhesion to the substrate, and improving the stability of high-temperature installation.
Smart Images

Figure CN119096358A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a semiconductor device, and more particularly to a chip size package type semiconductor device. Background Art
[0002] In order to protect the lithium-ion battery from overcharge and / or overdischarge, a vertical MOS transistor with a dual structure capable of controlling bidirectional conduction with one chip is used.
[0003] Prior art literature
[0004] Patent Literature
[0005] Patent Document 1: U.S. Patent No. 4,616,413 Summary of the invention
[0006] Problems to be solved by the invention
[0007] In order to reduce the on-resistance of the dual-structure vertical MOS transistor, the dual-structure vertical MOS transistor (hereinafter, the dual-structure vertical MOS transistor is also referred to as a "semiconductor chip") preferably has a larger area in planar view and a thinner semiconductor substrate. However, in such a structure, the warping of the semiconductor chip becomes larger, and the strength of the semiconductor chip decreases. Patent document 1 discloses a structure in which a printed circuit board is attached to a rigid metal plate via a conductive adhesive.
[0008] Therefore, an object of the present disclosure is to provide a semiconductor device including a vertical MOS transistor with a dual structure capable of improving adhesion in a structure in which a rigid metal plate is bonded via a conductive adhesive.
[0009] Means used to solve problems
[0010] In order to solve the above-mentioned problems, the semiconductor device disclosed in the present invention is a chip-size package type semiconductor device that can be mounted face-down, and is characterized in that it comprises: a semiconductor substrate; a low-concentration impurity layer formed on the surface side of the semiconductor substrate; a first vertical MOS transistor formed in a first region of the semiconductor layer when the semiconductor substrate and the low-concentration impurity layer are used together as a semiconductor layer; a second vertical MOS transistor formed in a second region adjacent to the first region in a planar view of the semiconductor layer; a first source electrode of the first vertical MOS transistor formed on the surface side of the semiconductor layer; and a second vertical MOS transistor formed in a second region adjacent to the first region. The second source electrode of the tube is formed on the surface side of the above-mentioned semiconductor layer; and the support body is formed on the back side of the above-mentioned semiconductor substrate via the conductive adhesive; in the above-mentioned planar observation, the above-mentioned support body is larger in area than the above-mentioned semiconductor layer and contains the above-mentioned semiconductor layer; the thickness of the above-mentioned support body is larger than the thickness of the above-mentioned semiconductor layer; in the cross-section of the above-mentioned semiconductor device including the center of the above-mentioned semiconductor layer and the periphery of the above-mentioned semiconductor layer in the above-mentioned planar observation, when observing the semiconductor chip in the above-mentioned semiconductor device except the above-mentioned support body and the above-mentioned conductive adhesive, the above-mentioned semiconductor chip is a curved shape convex toward the direction away from the above-mentioned support body.
[0011] According to the above-described structure, in the dual-structure vertical MOS transistor, the on-resistance can be reduced and the warping of the semiconductor chip can be alleviated, and the strength of the semiconductor chip can be improved.
[0012] Effects of the Invention
[0013] An object of the present disclosure is to provide a semiconductor device including a dual-structure vertical MOS transistor that reduces the on-resistance of a semiconductor chip and reduces the warping of the semiconductor chip, thereby improving the strength of the semiconductor chip. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a schematic cross-sectional view showing an example of the structure of the semiconductor device according to the first embodiment.
[0015] Figure 2A It is a schematic plan view showing an example of the structure of the semiconductor device according to the first embodiment.
[0016] Figure 2B This is a schematic cross-sectional view showing a main current flowing in the semiconductor device according to the first embodiment.
[0017] Figure 3A It is a schematic plan view showing an example of the structure of the semiconductor device according to the first embodiment.
[0018] Figure 3BThis is a schematic perspective view showing an example of the structure of the semiconductor device according to the first embodiment.
[0019] Figure 4A This is a flowchart showing a part of the manufacturing process of the semiconductor device according to the first embodiment.
[0020] Figure 4B It is a schematic cross-sectional view showing a process of face-down mounting the semiconductor device of the first embodiment.
[0021] Figure 5 It is a schematic cross-sectional view showing an example of the structure of a semiconductor device according to Modification 1 of Embodiment 1.
[0022] Figure 6 This is a drawing showing the size range of the semiconductor chip within which the effect of the semiconductor device of the first embodiment can be obtained.
[0023] Fig. 7A This is a cross-sectional SEM image showing an example of the structure of the semiconductor device according to the first embodiment.
[0024] Figure 7B This is a cross-sectional SEM image showing an example of the structure of the semiconductor device according to the first embodiment.
[0025] Figure 7C This is a cross-sectional SEM image showing an example of the structure of the semiconductor device according to the first embodiment.
[0026] Fig. 8A It is a schematic cross-sectional view showing an example of the structure of a semiconductor device according to a second modification of the first embodiment.
[0027] Figure 8B This is a schematic cross-sectional view showing an example of the structure of a semiconductor device according to Modification 3 of Embodiment 1.
[0028] Fig. 9 It is a schematic cross-sectional view showing an example of the structure of a semiconductor device according to the second embodiment.
[0029] Fig.10 This is a flowchart showing a part of the manufacturing process of the semiconductor device according to the second embodiment.
[0030] Fig.11A It is a schematic cross-sectional view showing an example of the structure of a semiconductor device according to the third embodiment.
[0031] Fig. 11B It is a schematic plan view showing an example of the structure of a processing support body in the semiconductor device according to the third embodiment.
[0032] Fig. 11C It is a schematic plan view showing an example of the structure of a semiconductor device according to the third embodiment. DETAILED DESCRIPTION
[0033] Hereinafter, a specific example of a semiconductor device of a technical solution of the present disclosure is described with reference to the accompanying drawings. The embodiments shown here all represent a specific example of the present disclosure. Therefore, the numerical values, shapes, constituent elements, configurations of constituent elements, and connection forms shown in the following embodiments are taken as examples and are not intended to limit the present disclosure. In addition, each figure is a schematic diagram and is not necessarily a strict illustration. In each figure, the same mark is given to substantially the same structure, and repeated descriptions are omitted or simplified.
[0034] (Implementation Method 1)
[0035] [1. Structure of semiconductor device]
[0036] Figure 1 It is a cross-sectional view showing an example of the structure of a semiconductor device. Figure 2A This is a plan view thereof, and the size and shape of the semiconductor device are examples except that it is rectangular (square or rectangular). In addition, the size, shape and arrangement of the pads are also examples. Figure 2B This is a cross-sectional view schematically showing a main current flowing in a semiconductor device. Figure 1 and Figure 2B It is along Figure 2A The cutting surface when cutting I-I.
[0037] In the present disclosure, the semiconductor device 1 is described assuming that it includes the metal layer 30 , but the semiconductor device 1 is not limited to a structure that necessarily includes the metal layer 30 .
[0038] like Figure 1 and Figure 2B As shown, the semiconductor device 1 includes a semiconductor substrate 32, a metal layer 30, and a low-concentration impurity layer 33 formed on the semiconductor substrate 32. In the present disclosure, the semiconductor substrate 32 and the low-concentration impurity layer 33 are collectively referred to as a semiconductor layer 40.
[0039] The semiconductor substrate 32 is arranged on the back side of the semiconductor layer 40, and is composed of silicon of the first conductivity type containing impurities of the first conductivity type. The low-concentration impurity layer 33 is arranged on the surface side of the semiconductor layer 40, is formed in contact with the semiconductor substrate 32, contains impurities of the first conductivity type at a concentration lower than the concentration of the impurities of the first conductivity type of the semiconductor substrate 32, and is of the first conductivity type. The low-concentration impurity layer 33 can be formed on the semiconductor substrate 32 by, for example, epitaxial growth.
[0040] like Figure 1 and Figure 2AAs shown, the semiconductor device 1 has a first vertical MOS transistor 10 (hereinafter also referred to as "transistor 10") formed in a first region A1 within the semiconductor layer 40 and a second vertical MOS transistor 20 (hereinafter also referred to as "transistor 20") formed in a second region A2 within the semiconductor layer 40.
[0041] Here, if Figure 2A As shown, the first region A1 and the second region A2 are adjacent to each other in a plan view of the semiconductor layer 40, and the semiconductor layer 40 is divided into two equal parts in terms of area. Figure 2A In FIG. 1 , an imaginary boundary line 90 between the first region A1 and the second region A2 is indicated by a dotted line (for ease of understanding, the dotted line indicating the boundary line 90 is extended to the outside of the semiconductor layer 40 and the semiconductor device 1 ). Figure 2A In the figure, the dotted lines representing the first area A1 and the second area A2 are not strictly aligned with the semiconductor layer 40 and the boundary line 90 for ease of understanding, but are slightly left blank and represented on the inside. However, in essence, the outer periphery of the first area A1 and the outer periphery of the second area A2 are aligned with the outer periphery of the semiconductor layer 40 and the boundary line 90.
[0042] The metal layer 30 is formed in contact with the back side of the semiconductor layer 40 (semiconductor substrate 32), and is composed of, for example, silver (Ag) or copper (Cu). In addition, the metal layer 30 may contain trace amounts of elements other than metals mixed as impurities in the manufacturing process of the metal material. In addition, the metal layer 30 may be formed on the entire back side of the semiconductor layer 40 (semiconductor substrate 32). The thickness of the metal layer 30 is preferably 10 [μm] or less, and more preferably 5 [μm] or less. The thickness of the metal layer 30 is, for example, 3 [μm].
[0043] The support body 42 is formed by indirectly contacting the back side of the metal layer 30 via the conductive adhesive 41. Typically, the support body 42 is more than twice the thickness of the semiconductor layer 40, for example, a flat metal plate with a thickness of 200 [μm] uniform in the surface. In the following, the support body 42 is also referred to as a thick film metal plate 42. The thick film metal plate 42 is composed of a metal material mainly composed of copper (Cu). In addition, the conductive adhesive 41 is typically a silver paste.
[0044] like Figure 1 As shown in FIG. 1 , in the present disclosure, the structure in which the support body 42 and the conductive adhesive 41 are removed from the semiconductor device 1 is referred to as a semiconductor chip 2. The semiconductor chip 2 is Figure 1As shown, it is a curved shape that is convex in the direction away from the support body 42. The curved shape is, for example, a shape caused by warping. The warping amount of the semiconductor chip 2 is the difference between the highest position and the lowest position in the Z direction of the upper surface or the lower surface of the semiconductor layer 40, or the lower surface of the metal layer 30 when the semiconductor chip 2 is cross-sectionally viewed. In the case where the warping occurring in the semiconductor chip 2 is a convex warping in the direction away from the support body 42, the highest position is the center of the semiconductor layer 40 in planar observation, and the lowest position is the periphery of the semiconductor layer 40 in planar observation, especially the corner at the periphery.
[0045] In addition, the center of the semiconductor layer 40 in planar observation refers to the intersection of the diagonal lines of the semiconductor layer 40 in planar observation. In addition, the cross-section of the semiconductor device 1 in the present disclosure refers to the situation when the cross section of the semiconductor device 1 is observed with a plane that includes both the center of the semiconductor layer 40 in the semiconductor chip 2 in planar observation and the periphery of the semiconductor layer 40 in the semiconductor chip 2. At this time, the periphery of the semiconductor layer 40 can be any position on the periphery of the semiconductor layer 40.
[0046] like Figure 1 and Figure 2A As shown, a first body region 18 including impurities of a second conductivity type different from the first conductivity type is formed in the first region A1 of the semiconductor layer 40 (low-concentration impurity layer 33). In the first body region 18, a first source region 14 including impurities of the first conductivity type, a first gate conductor 15, and a first gate insulating film 16 are formed.
[0047] The first gate insulating film 16 is formed inside a plurality of first gate trenches 17, and the first gate trenches 17 are formed to a depth that reaches a portion of the low-concentration impurity layer 33 by penetrating the first source region 14 and the first body region 18 from the upper surface of the semiconductor layer 40, and the first gate conductor 15 is formed on the first gate insulating film 16 inside the first gate trenches 17. The first gate conductor 15 is a buried gate electrode buried in the semiconductor layer 40, and is electrically connected to the first gate pad 119.
[0048] The first source electrode 11 is composed of a portion 12 and a portion 13, and the portion 12 is connected to the first source region 14 and the first body region 18 via the portion 13. The portion 12 of the first source electrode 11 is a layer that is joined to the solder during reflow in face-down mounting, and can be composed of a metal material including one or more of nickel, titanium, tungsten, and palladium as a non-limiting example. The surface of the portion 12 can be plated with gold or the like.
[0049] The portion 13 of the first source electrode 11 is a layer connecting the portion 12 and the semiconductor layer 40 , and may be made of a metal material including one or more of aluminum, copper, gold, and silver as a non-limiting example.
[0050] The thickness of the first source electrode 11 is, for example, not less than 2 [μm] and not more than 13 [μm] when the portion 12 and the portion 13 are added together.
[0051] A second body region 28 containing second conductivity type impurities is formed in the second region A2 of the low concentration impurity layer 33. In the second body region 28, a second source region 24 containing first conductivity type impurities, a second gate conductor 25, and a second gate insulating film 26 are formed.
[0052] The second gate insulating film 26 is formed inside a plurality of second gate trenches 27, and the second gate trenches 27 are formed to a depth that reaches a portion of the low-concentration impurity layer 33 by penetrating the second source region 24 and the second body region 28 from the upper surface of the semiconductor layer 40, and the second gate conductor 25 is formed on the second gate insulating film 26 inside the second gate trenches 27. The second gate conductor 25 is a buried gate electrode buried inside the semiconductor layer 40, and is electrically connected to the second gate pad 129.
[0053] The second source electrode 21 is composed of a portion 22 and a portion 23, and the portion 22 is connected to the second source region 24 and the second body region 28 via the portion 23. The portion 22 of the second source electrode 21 is a layer that is joined to the solder during reflow in face-down mounting, and can be composed of a metal material including one or more of nickel, titanium, tungsten, and palladium as a non-limiting example. The surface of the portion 22 can be plated with gold or the like.
[0054] The portion 23 of the second source electrode 21 is a layer connecting the portion 22 and the semiconductor layer 40 , and may be made of a metal material including one or more of aluminum, copper, gold, and silver as a non-limiting example.
[0055] The thickness of the second source electrode 21 is, for example, not less than 2 [μm] and not more than 13 [μm] when the portion 22 and the portion 23 are added together.
[0056] With the above-described structures of the transistors 10 and 20, the semiconductor substrate 32 functions as a common drain region that makes the first drain region of the transistor 10 and the second drain region of the transistor 20 common. In some cases, a portion of the low-concentration impurity layer 33 that is in contact with the semiconductor substrate 32 also functions as a common drain region. In addition, the low-concentration impurity layer 33 is also a drift layer common to the transistors 10 and 20, and is sometimes referred to as the drift layer 33 in this specification.
[0057] The metal layer 30 functions as a common drain electrode that makes the drain electrode of the transistor 10 and the drain electrode of the transistor 20 common. When the support 42 is a thick metal plate, not only the metal layer 30 but also the conductive adhesive 41 and the thick metal plate 42 function as a common drain electrode.
[0058] like Figure 1 As shown, the first body region 18 is covered by an interlayer insulating layer 34 having an opening, and is connected to a portion 13 of the first source electrode 11 connected to the first source region 14 via the opening of the interlayer insulating layer 34. The interlayer insulating layer 34 and the portion 13 of the first source electrode are covered by a passivation layer 35 having an opening, and are connected to a portion 12 connected to the portion 13 of the first source electrode via the opening of the passivation layer 35.
[0059] The second body region 28 is covered by an interlayer insulating layer 34 having an opening, and is connected to the portion 23 of the second source electrode 21 connected to the second source region 24 via the opening of the interlayer insulating layer 34. The interlayer insulating layer 34 and the portion 23 of the second source electrode are covered by a passivation layer 35 having an opening, and are connected to the portion 22 connected to the portion 23 of the second source electrode via the opening of the passivation layer 35.
[0060] Therefore, the plurality of first source pads 111 and the plurality of second source pads 121 refer to regions where the first source electrode 11 and the second source electrode 21 are partially exposed on the surface of the semiconductor device 1, so-called terminal portions. Similarly, the one or more first gate pads 119 and the one or more second gate pads 129 refer to the first gate electrode 19 (on the surface of the semiconductor device 1). Figure 1 , Figure 2A , Figure 2B ) and the second gate electrode 29 (not shown in the figure) Figure 1 , Figure 2A , Figure 2B An area partially exposed on the surface of the semiconductor device 1 (not shown), a so-called terminal portion.
[0061] In addition, in the present disclosure, it is assumed that in a planar observation, only the structure constituting the first vertical MOS transistor 10 is provided in the first region A1, and only the structure constituting the second vertical MOS transistor 20 is provided in the second region A2. In addition, the boundary line 90 can also be understood as an imaginary line along the center position of the interval between the portion 13 of the first source electrode 11 and the portion 23 of the second source electrode 21. In addition, although it has a limited width, it can also be understood as the interval itself (even in the case of this interval, it can be recognized as a line in the appearance at a low magnification or with the naked eye).
[0062] In the semiconductor device 1, for example, the first conductivity type can be set to N type, the second conductivity type can be set to P type, the first source region 14, the second source region 24, the semiconductor substrate 32 and the low-concentration impurity layer 33 are N type semiconductors, and the first body region 18 and the second body region 28 are P type semiconductors.
[0063] In addition, in the semiconductor device 1, for example, the first conductivity type can be set to P type, the second conductivity type can be set to N type, the first source region 14, the second source region 24, the semiconductor substrate 32 and the low-concentration impurity layer 33 are P type semiconductors, and the first body region 18 and the second body region 28 are N type semiconductors.
[0064] [2. Operation of a Dual-Structure Vertical MOS Transistor]
[0065] In the following description, the on-operation of the semiconductor device 1 is described assuming that the transistor 10 and the transistor 20 are so-called N-channel transistors in which the first conductivity type is N-type and the second conductivity type is P-type.
[0066] Figure 3A and Figure 3B The plan view and the perspective view are respectively a rough unit structure of the transistor 10 (or the transistor 20) repeatedly formed in the X direction and the Y direction of the semiconductor device 1. Figure 3A and Figure 3B For ease of understanding, the semiconductor substrate 32, the metal layer 30, the conductive adhesive 41, the thick metal plate 42, the passivation layer 35, the first source electrode 11 (or the second source electrode 21), and the interlayer insulating layer 34 are not shown.
[0067] The structure of the transistor 10 is the same as that of the transistor 20. Therefore, the general unit structure will be described below using the notation of the transistor 10.
[0068] The Y direction is parallel to the upper surface of the semiconductor layer 40 and is the direction in which the first gate trench 17 extends. In addition, the X direction is parallel to the upper surface of the semiconductor layer 40 and is orthogonal to the Y direction. The Z direction is a direction that is orthogonal to both the X direction and the Y direction and indicates the height direction of the semiconductor device. In the present disclosure, there are also cases where the Y direction is indicated as the first direction, the X direction is indicated as the second direction, and the Z direction is indicated as the third direction.
[0069] like Figure 3A and Figure 3BAs shown, the transistor 10 includes a first connecting portion 18a electrically connecting the first body region 18 to the first source electrode 11. The first connecting portion 18a is a region of the first body region 18 where the first source region 14 is not formed, and contains the same second conductivity type impurities as the first body region 18. The first source region 14 and the first connecting portion 18a are alternately and periodically arranged along the Y direction. The transistor 20 is the same.
[0070] In the semiconductor device 1, when a high voltage is applied to the first source electrode 11 and a low voltage is applied to the second source electrode 21, and a voltage higher than a threshold value is applied to the second gate electrode 29 (second gate conductor 25) with reference to the second source electrode 21, a conduction channel is formed near the second gate insulating film 26 in the second body region 28. As a result, a main current flows through the path of the first source electrode 11-first connecting portion 18a-first body region 18-low-concentration impurity layer 33-semiconductor substrate 32-metal layer 30-conductive adhesive 41-thick-film metal plate 42-conductive adhesive 41-metal layer 30-semiconductor substrate 32-low-concentration impurity layer 33-conduction channel formed in the second body region 28-second source region 24-second source electrode 21, and the semiconductor device 1 is turned on. A PN junction exists at the contact surface between the second body region 28 and the low-concentration impurity layer 33 in this conduction path, and functions as a body diode.
[0071] Similarly, in the semiconductor device 1, when a high voltage is applied to the second source electrode 21 and a low voltage is applied to the first source electrode 11, and a voltage higher than a threshold value is applied to the first gate electrode 19 (first gate conductor 15) with reference to the first source electrode 11, a conduction channel is formed near the first gate insulating film 16 in the first body region 18. As a result, a main current flows through the path of the second source electrode 21-second connecting portion 28a-second body region 28-low-concentration impurity layer 33-semiconductor substrate 32-metal layer 30-conductive adhesive 41-thick-film metal plate 42-conductive adhesive 41-metal layer 30-semiconductor substrate 32-low-concentration impurity layer 33-conduction channel formed in the first body region 18-first source region 14-first source electrode 11, and the semiconductor device 1 is turned on. A PN junction exists at the contact surface between the first body region 18 and the low-concentration impurity layer 33 in this conduction path, and functions as a body diode.
[0072] exist Figure 2BSchematically, the bidirectional flow of the main current is indicated by arrows. The main current flows in the horizontal direction (X direction) in each layer of the metal layer 30, the conductive adhesive 41, the thick film metal plate 42 and the semiconductor substrate 32. Since the resistivity of the metal layer 30 and the thick film metal plate 42 is lower than that of other layers, by making the metal layer 30 or the thick film metal plate 42 thicker, the cross-sectional area of the main current path is expanded, and the on-resistance of the semiconductor device 1 can be reduced.
[0073] [3. Method for manufacturing semiconductor device]
[0074] A method for manufacturing the semiconductor device 1 will be described.
[0075] Figure 4A This is a diagram briefly showing a part of the manufacturing process of the semiconductor device 1 according to the present embodiment 1. The structure of each dual-structure vertical MOS transistor to be singulated later is formed in a grid shape on a silicon wafer until step 501 .
[0076] Next, in step 502, the back side of the silicon wafer (corresponding to the semiconductor substrate 32 from the perspective of each dual-structure vertical MOS transistor to be singulated later) is thinned. In the thinning process of step 502, the thickness of the semiconductor layer 40 is preferably controlled to be 15 [μm] or more and 100 [μm] or less, and more preferably controlled to be 15 [μm] or more and 75 [μm] or less.
[0077] Next, in step 503, a metal layer 30 is formed on the back side of the thinned silicon wafer. The metal layer 30 may be a multilayer structure including a plurality of metal layers, for example. The plurality of metal layers may be formed individually by any method including evaporation, sputtering, and plating.
[0078] Next, the silicon wafer is sliced to separate the dual-structure vertical MOS transistors into individual chips in step 504. The individual dual-structure vertical MOS transistors are in a state that can be called semiconductor chips 2 as described above because they are not yet bonded to the thick-film metal plate 42.
[0079] Next, in step 505, a thick metal plate 42 coated with a conductive adhesive 41 such as silver paste is prepared in advance, and the back side of the metal layer 30 of the semiconductor chip 2 is bonded. Usually, the amount of conductive adhesive 41 pushed in is set, for example, between 5 [μm] and 10 [μm], and the thickness of the conductive adhesive 41 after hardening and bonding is calculated to be a target value (for example, 20 [μm] to 60 [μm]), and the conductive adhesive 41 is applied to the surface of the thick metal plate 42.
[0080] The conductive adhesive 41 is used to bond the back side of the metal layer 30 to the thick metal plate 42. Preferably, when the conductive adhesive 41 is observed in a state after being cured and bonded to the thick metal plate 42, the entire back side of the metal layer 30 is completely covered by the conductive adhesive 41.
[0081] For the thick metal plate 42, a structure whose area exceeds that of the semiconductor substrate 32 in plan view is selected, and during bonding, alignment is performed so that a gap is provided with a substantially equal width from the outer periphery of the metal layer 30 to the outer periphery of the closest thick metal plate 42 in plan view. As an example, Figure 2A As shown, the thick metal plate 42 is similar in shape to the semiconductor layer 40. The semiconductor layer 40 and the thick metal plate 42 are similar in shape, which means that the semiconductor layer 40 and the thick metal plate 42 are the same shape in plan view and only differ in area.
[0082] The thick metal plate 42 preferably has a uniform thickness in a plane and is a so-called flat plate without steps or irregularities in macroscopic view for bonding the semiconductor layer 40. In the first embodiment, the thick metal plate 42 is described as a flat plate.
[0083] During bonding, usually, the thick film metal plate 42 with a relatively large area is used as the receiving side, and the semiconductor chip 2 with a relatively small area is aligned. The conductive adhesive 41 can also be exposed from the back side of the metal layer 30 in plan view. The amount of the conductive adhesive 41 exposed can be uniform along the periphery of the semiconductor layer 40 in plan view. Figure 2A , a case where the exposure of the conductive adhesive 41 is uniform is shown as an example.
[0084] In step 505, in order to harden the conductive adhesive 41 such as silver paste, the thick metal plate 42 is subjected to heat treatment at a temperature of about 170[°C] while the semiconductor chip 2 is aligned. The conductive adhesive 41 starts to harden at about 170[°C], and the metal layer 30 is bonded to the thick metal plate 42 to form the semiconductor device 1.
[0085] In addition, during the heat treatment at a high temperature of 170 [°C], the semiconductor chip 2 warps. As described above, the thickness of the semiconductor layer 40 is preferably 15 [μm] or more and 75 [μm] or less, and the thickness of the first source electrode 11 and the second source electrode 21 is 2 [μm] or more and 13 [μm] or less. The thickness of the metal layer 30 is preferably 5 [μm] or less. By appropriately selecting the respective film thicknesses, the direction of the warping of the semiconductor chip 2 at 170 [°C] can be controlled.
[0086] For example, if the thickness of the semiconductor layer 40 is 53 [μm], the thickness of the first source electrode 11 and the second source electrode 21 is 5 [μm], and the thickness of the metal layer 30 is 3 [μm], then at 170 [°C], the semiconductor chip 2 generates a direction away from the thick film metal plate 42 (at Figure 1 The cross-sectional view in the figure shows a convex warp in the +Z direction).
[0087] Figure 4B This is a schematic diagram of a case where the semiconductor device 1 is mounted face down.
[0088] [4. Investigation]
[0089] Hereinafter, effects achieved by the semiconductor device 1 according to the first embodiment will be described.
[0090] In a vertical MOS transistor with a dual structure, in order to reduce the on-resistance when conducting, it is required to make the semiconductor substrate 32 (semiconductor layer 40) thinner and the metal layer 30 thicker. The semiconductor chip 2 with such a structure is prone to warping in the -Z direction at high temperatures. The thinner the semiconductor layer 40 and the thicker the metal layer 30, the greater the warping that occurs at high temperatures.
[0091] In particular, in the case of a dual-structure vertical MOS transistor requiring low on-resistance, it is effective to increase the area of the semiconductor chip 2 in plan view in order to increase the total gate width of the channel. However, if the area is large, the warpage occurring in the semiconductor chip 2 increases significantly.
[0092] When the semiconductor chip 2 is mounted face down on the mounting substrate, it is necessary to perform a reflow process at a temperature of about 240[°C] using a solder material. It is known that if the warpage of the semiconductor chip 2 at 240[°C] exceeds 40[μm], mounting failure is likely to occur regardless of the direction of the warpage, and it is required to suppress the warpage of the semiconductor chip 2 to less than 40[μm].
[0093] The structure of the semiconductor device 1 of the first embodiment is particularly effective for the semiconductor chip 2 having a thin semiconductor layer 40 and a large area as described above. In the semiconductor device 1, the support 42 is made of a thick metal plate and is connected to the metal layer 30 with a conductive adhesive 41. Therefore, even if the metal layer 30 is thin, as long as the thick metal plate 42 is sufficiently thick, the thick metal plate 42 becomes a horizontal conduction path, thereby reducing the conduction resistance of the semiconductor device 1. In addition, in the semiconductor chip 2, by making the metal layer 30 thin, the warping can be reduced.
[0094] Furthermore, since the semiconductor chip 2 is bonded to the thick metal plate 42 at a temperature of approximately 170°C, which is lower than 240°C, the warping of the semiconductor chip 2 can be suppressed to a level that occurs at approximately 170°C. If a material that does not melt again, such as silver paste, is selected as the conductive adhesive 41, the semiconductor chip 2 bonded to the thick metal plate 42 will not be further warped during the reflow process (240°C) when the semiconductor device 1 is mounted face down on the mounting substrate.
[0095] Furthermore, if the thick-film metal plate 42 is sufficiently thick, it can function as a support for the semiconductor chip 2, thereby compensating for the decrease in strength of the semiconductor chip 2 caused by making the semiconductor layer 40 thin.
[0096] Therefore, the thick metal plate 42 of the semiconductor device 1 of the first embodiment has the effect of physically compensating for the thinning of the semiconductor layer 40 and electrically compensating for the thinning of the metal layer 30. As for the metal layer 30, in an extreme sense, it is also possible to not have it. In this case, Figure 5 As in the first modification of the first embodiment shown, the conductive adhesive 41 is directly bonded to the entire surface of the back side of the semiconductor substrate 32 (semiconductor layer 40 ).
[0097] The larger the area of the semiconductor layer 40 in the semiconductor chip 2 when viewed from the plane and the thinner the semiconductor layer 40 is, the more useful the structure of the semiconductor device 1 having the thick film metal plate 42 of the first embodiment is. On the contrary, for a semiconductor chip 2 having a smaller area when viewed from the plane and a thicker semiconductor layer 40, there is little significance in joining the thick film metal plate 42. Therefore, the size (area and thickness) of the semiconductor chip 2 useful for the structure of the semiconductor device 1 having the thick film metal plate 42 of the first embodiment was studied.
[0098] exist Figure 6 , the area and thickness of the semiconductor layer 40 (from the upper surface of the low-concentration impurity layer 33 to the lower surface of the semiconductor substrate 32) required for the on-resistance of the semiconductor chip 2 to be 1 [mΩ] or less, and the amount of warping of the semiconductor chip 2 generated at this time are calculated. Here, 1 [mΩ] is a rough standard, and for battery protection circuits, when large currents are passed, which has been in increasing demand in recent years, a lower on-resistance of, for example, 1 [mΩ] or less is required.
[0099] The horizontal axis represents the area S [mm] of the semiconductor layer 40 when the semiconductor chip 2 is viewed from the plane. 2 ], the left vertical axis is the thickness h [mm] of the semiconductor layer 40 of the semiconductor chip 2. The shape of the semiconductor layer 40 is square. For example, 2.5×2.5 [mm] is equivalent to an area of 6.2 [mm 2], 3.4×3.4[mm] is equivalent to an area of 11.5[mm 2 ]. The thickness of the semiconductor layer 40 when the on-resistance of the semiconductor chip 2 is just 1.00 [mΩ] is plotted by the 0 mark. The thickness of the semiconductor layer 40 when the on-resistance of the semiconductor chip 2 is just 0.75 [mΩ] is plotted by the △ mark. In the semiconductor chip 2 when calculating the thickness of the semiconductor layer 40, it is assumed that the metal layer 30 is made of silver (Ag) and has a thickness of 50 [μm].
[0100] In order to achieve a low on-resistance of 1.00 [mΩ] or less, the semiconductor chip 2 needs to be configured to be suitable for a region below the curve connecting the plots marked with 0. If the area of the semiconductor layer 40 in the semiconductor chip 2 is small when viewed from the plane, the thickness of the semiconductor layer 40 must be thin, while if the area of the semiconductor layer 40 in the semiconductor chip 2 is large when viewed from the plane, the thickness of the semiconductor layer 40 can be increased to a certain extent.
[0101] The line connecting the plots marked with 0 is approximately in the relationship of h = 0.016 × S - 0.042 ( Figure 6 The dashed line in FIG. 1 shows that the accuracy is good when 6.2≤S≤11.5). Therefore, in order to make the on-resistance 1.00 [mΩ] or less, the semiconductor layer 40 of the semiconductor chip 2 is required to be in the relationship of h≤0.016×S-0.042.
[0102] The line connecting the plots marked with △ is approximately in the relationship of h=0.014×S-0.074 ( Figure 6 The dashed line in FIG. 1 shows that the accuracy is good when 6.2≤S≤11.5). Therefore, in order to make the on-resistance 0.75 [mΩ] or less, the semiconductor layer 40 of the semiconductor chip 2 is required to be in the relationship of h≤0.014×S-0.074.
[0103] Figure 6 The vertical axis to the right is the warpage amount [μm] of the semiconductor chip 2 at a high temperature of 240 [℃]. The □ mark plots the warpage amount that occurs when Ag is formed with a thickness of 50 [μm] as the metal layer 30 under the structure (area S and thickness h) of the semiconductor layer 40 of each semiconductor chip 2 represented by the 0 mark. The 50 [μm] thickness of Ag as the metal layer 30 of the semiconductor chip 2 is set to enable comparison with the structure of the semiconductor device 1 of the present embodiment 1 having a thick film metal plate 42. As the material constituting the metal layer 30, Ag with good resistivity is set, and the thickness of 50 [μm] is also selected to be approximately saturated in the contribution to the reduction of the on-resistance.
[0104] In addition, the semiconductor layer 40 is formed into a square shape when viewed from above because even with the same structure (area S and thickness h), the square shape is the one that can reduce the warpage the most. Figure 5 The plot marked with a square in FIG. 1 can be said to indicate the minimum warpage amount in the state of the semiconductor chip 2 that can be electrically compared with the semiconductor device 1 of the first embodiment.
[0105] according to Figure 6 It can be seen that when the on-resistance is required to be 1.00 [mΩ] or less, the area is 6.2 [mm 2 ] or more, the warpage at 240[℃] exceeds 40[μm]. Therefore, in an area of 6.2[mm 2 ] or more, it is difficult to mount the semiconductor chip 2 in its original state, and a countermeasure is needed to reduce the amount of warping.
[0106] Even if the on-resistance is 1.00 [mΩ], the area of the semiconductor chip 2 in plan view is less than 6.2 [mm 2 ], since the warpage is less than 40 [μm], the semiconductor chip 2 can be mounted in its original state. In addition, even if the area of the semiconductor chip 2 in plan view is the same 6.2 [mm 2 ] As long as the on-resistance is higher than 1.00 [mΩ], there is no need to make the thickness of the semiconductor layer 40 excessively thin, so the warpage is less than 40 [μm], and the semiconductor chip 2 can be mounted in its original state.
[0107] Therefore, for a square in plane view with a width of 6.2 [mm 2 When a semiconductor chip 2 with an area of more than ](2.5×2.5[mm]) is required to have an on-resistance of less than 1.00[mΩ], that is, with respect to the semiconductor layer 40 of the semiconductor chip 2, when the relationship h≤0.016×S-0.042 holds, it is preferred to join the thick film metal plate 42 as in the semiconductor device 1 of the present embodiment 1.
[0108] Furthermore, for example, when the on-resistance is required to be 0.75 [mΩ] or less, the thickness of the semiconductor layer 40 needs to be thinner in the semiconductor chip 2. That is, with respect to the semiconductor layer 40 of the semiconductor chip 2, when the relationship of h≤0.014×S-0.074 holds, it is more preferable to bond the thick metal plate 42 as in the semiconductor device 1 of the first embodiment.
[0109] In addition, the semiconductor device 1 of the present embodiment 1 can control the warping of the semiconductor chip 2 at 170 [°C] to be convex in the direction away from the support body 42 (+Z direction) by appropriately selecting the thicknesses of the semiconductor layer 40 (semiconductor substrate 32), the first source electrode 11 and the second source electrode 21, and the metal layer 30.
[0110] like Figure 1 As shown in FIG. 1 , when the thick film metal plate 42 is warped so as to be convex in a direction (+Z direction) away from the back surface of the metal layer 30, the conductive adhesive 41 is squeezed between the metal layer 30 and the thick film metal plate 42. In particular, the end of the metal layer 30 is relatively close to the thick film metal plate 42 (-Z direction) due to the bending of the semiconductor chip 2, and the conductive adhesive 41 is pushed toward the thick film metal plate 42. When the semiconductor chip 2 is bent in such a shape, the effect of improving the closeness of the bonding between the semiconductor chip 2 and the thick film metal plate 42 can be obtained.
[0111] Therefore, for the semiconductor device 1, in the cross-section of the semiconductor device 1, when observing the semiconductor chip 2 other than the thick film metal plate 42 and the conductive adhesive 41 in the semiconductor device 1, the semiconductor chip 2 preferably has a curved shape that is convex in the direction away from the thick film metal plate 42. In other words, it is preferred that the thickness of the conductive adhesive 41 directly below the semiconductor layer 40 at the periphery of the semiconductor layer 40 in planar observation is thinner than the thickness of the conductive adhesive 41 directly below the semiconductor layer 40 at the center of the semiconductor layer 40 in planar observation.
[0112] exist Fig. 7A , Figure 7B , Figure 7C 2 shows a cross-sectional SEM image of the semiconductor device 1 according to the first embodiment when it is mounted face down on a mounting substrate. Figure 7B yes Fig. 7A The enlarged cross-sectional SEM image of the part surrounded by the dotted line is shown in Figure 1. Figure 7C yes Figure 7B The enlarged cross-sectional SEM image of the portion surrounded by the dotted line. Figure 7A to Figure 7C In the semiconductor device 1 shown, the thickness of the semiconductor layer 40 is 53 [μm], the thickness of the first source electrode 11 and the second source electrode 21 is 4 [μm], the thickness of the metal layer 30 is 3 [μm], and the thickness of the thick-film metal plate 42 is 200 [μm].
[0113] Figure 7B and Figure 7C The horizontal line A in FIG. 4 is represented by extending the interface position between the semiconductor layer 40 and the metal layer 30 at the center of the semiconductor layer 40 to the periphery of the semiconductor layer 40. Figure 7CThe horizontal line B in FIG. 4 represents the interface position between the semiconductor layer 40 and the metal layer 30 at the periphery of the semiconductor layer 40. Figure 7C In FIG. 1 , the horizontal line B is located closer to the thick-film metal plate 42 than the horizontal line A (in the −Z direction), and the interval between the horizontal line A and the horizontal line B in the z direction is 2 [μm].
[0114] Therefore, the semiconductor chip 2 is convex and warped in the direction away from the thick film metal plate 42 (+Z direction), and the warping amount is 2 [μm]. The conductive adhesive 41 that joins the semiconductor chip 2 and the thick film metal plate 42 is squeezed between the two and hardened, covering the entire back side of the semiconductor chip 2. For the conductive adhesive 41, no voids or peeling sites are seen, and it can be confirmed that the adhesion is good.
[0115] The inventors have studied and found that if the warpage of the semiconductor chip 2 at 170 [°C] is 2 [μm] or more, the effect of improving the adhesion can be stably obtained. When the warpage is less than 2 [μm], or when the warpage is convex in the opposite direction, the effect of squeezing the conductive adhesive 41 between the semiconductor chip 2 and the thick film metal plate 42 cannot be stably obtained, and there are cases where traces of the conductive adhesive 41 peeling off are seen at the end of the semiconductor device 1.
[0116] The semiconductor chip 2 warps at high temperatures because the first source electrode 11 and the second source electrode 21 are formed on the surface side of the semiconductor layer 40. In addition, when the metal layer 30 is provided on the back side of the semiconductor layer 40, the formation of the metal layer 30 also has an impact. The direction of warping (also referred to as the direction of bending) and the amount of warping (also referred to as the amount of bending) of the semiconductor chip 2 are determined by the relationship between the physical properties such as the linear expansion coefficient and Young's modulus of the semiconductor layer 40, the first source electrode 11 and the second source electrode 21, and the metal layer 30 and their respective thicknesses.
[0117] When the semiconductor chip 2 does not have the metal layer 30 (in Figure 5 In the variation 1 of the present embodiment 1 shown in FIG. 1 , the warping of the semiconductor chip 2 is determined only by the relationship between the semiconductor layer 40 and the first source electrode 11 and the second source electrode 21. Since the linear expansion coefficient is generally large in the case of metals, the direction of the warping that occurs at high temperatures is convex in the +Z direction. The amount of warping is determined by the relative relationship between the thickness of the semiconductor layer 40 and the first source electrode 11 and the second source electrode 21, and the thinner the semiconductor layer 40 is and the thicker the first source electrode 11 and the second source electrode 21 are, the greater the warping is.
[0118] In the case where the semiconductor chip 2 has a metal layer 30, the thickness of the metal layer 30 is mainly determined only by the relationship between the metal layer 30 and the first source electrode 11 and the second source electrode 21. Furthermore, since the linear expansion coefficients of the metal types constituting the first source electrode 11 and the second source electrode 21 and the metal types constituting the metal layer 30 are often close, the direction and amount of warping are determined only by their respective thicknesses in most cases. In the case where the warping is required to be controlled to be convex in the +Z direction, the thickness of the metal layer 30 is preferably thinner than the thickness of the first source electrode 11 and the thickness of the second source electrode 21. This is because, at high temperatures, the thicker the film thickness, the greater the stress caused by expansion, and the curved shape becomes convex in their directions.
[0119] As described above, in order to improve the closeness of the bonding between the metal layer 30 and the thick film metal plate 42, the semiconductor chip 2 is required to be warped in the direction away from the thick film metal plate 42 (+Z direction), but if the warping amount is too large, voids are likely to occur in the conductive adhesive 41 near the center of the semiconductor layer 40 in planar observation. According to the results of the inventor's research, if the warping amount of the semiconductor chip 2 at 170 [℃] is adjusted to 20 [μm] or less, the occurrence of voids can be stably prevented. Therefore, the warping amount of the semiconductor chip 2 at 170 [℃] is preferably 2 [μm] or more and 20 [μm] or less.
[0120] In order to make the semiconductor chip 2 into a curved shape that is convex in the direction away from the thick film metal plate 42 (+Z direction), the thickness of the semiconductor layer 40 in the semiconductor chip 2 is preferably 100 [μm] or less, and more preferably 75 [μm] or less. This is because it is difficult to make the first source electrode 11 and the second source electrode 21 extremely thick and form a film, and the semiconductor chip 2 is easy to bend when the semiconductor layer 40 is thin. In addition, the decrease in the strength of the semiconductor chip 2 caused by the thinning of the semiconductor layer 40 can be compensated by bonding the thick film metal plate 42, so in the present disclosure, the side effects caused by thinning the semiconductor layer 40 can be reduced.
[0121] However, if the thickness of the semiconductor layer 40 is extremely thin, for example, less than 15 [μm], cracks are easily generated in the semiconductor layer 40 (semiconductor substrate 32) during singulation. Therefore, the thickness of the semiconductor layer 40 is preferably 15 [μm] or more and 100 [μm] or less, and more preferably 15 [μm] or more and 75 [μm] or less.
[0122] The thickness of the first source electrode 11 and the thickness of the second source electrode 21 are preferably, for example, not less than 2 [μm] and not more than 13 [μm]. In the case where the semiconductor chip 2 does not include the metal layer 30, if the semiconductor layer 40 is thin, even if the thickness of the first source electrode 11 and the thickness of the second source electrode 21 are 2 [μm] to 5 [μm], the warpage at 170 [°C] can be made to be 2 [μm] or more. However, when the semiconductor layer 40 is thicker, it is preferable to change the thickness of the first source electrode 11 and the thickness of the second source electrode 21 to a thicker direction such as 10 [μm] to 13 [μm].
[0123] If the film thickness structure is as described above, the direction in which the semiconductor chip 2 warps at high temperature can be controlled to be a direction in which the semiconductor chip 2 convexly moves away from the thick film metal plate 42 (+Z direction), and the warping amount can be controlled to be greater than 2 [μm] and less than 20 [μm].
[0124] In addition, as in Figure 1 As schematically shown in FIG. 1 , in the semiconductor device 1 of the first embodiment, the conductive adhesive 41 often forms a substantially triangular chamfer such that a portion of the conductive adhesive 41 is lifted up on the side wall of the semiconductor chip 2. In the semiconductor device 1 of the first embodiment, the conductive adhesive 41 has a substantially triangular chamfer such that a portion of the conductive adhesive 41 is lifted up on the side wall of the semiconductor chip 2. Figure 7A to Figure 7C As shown in FIG. 1 , the semiconductor layer 40 reaches a position close to the upper surface thereof.
[0125] like Figure 7C As shown, if the chamfer angle is defined based on the upper surface of the thick film metal plate 42, the minimum angle in the semiconductor device 1 of the first embodiment is 20 [deg]. Therefore, the conductive adhesive 41 may be exposed from the periphery of the semiconductor layer 40 by a maximum of (h + hp) / tan (20 [deg]) [mm] in planar observation. Here, in planar observation, the total thickness of the metal layer 30 and the conductive adhesive 41 directly below the corner of the semiconductor layer 40 is set to hp [mm]. The corner of the semiconductor layer 40 is specified because it is the part where the conductive adhesive 41 is pushed in the most due to the warping of the semiconductor chip 2. In addition, tan is a tangent function.
[0126] If the area of the thick-film metal plate 42 in plan view is not sufficiently larger than the area of the semiconductor layer 40, the exposure of the conductive adhesive 41 may not be contained in the inside of the thick-film metal plate 42. Therefore, the area of the thick-film metal plate 42 in plan view must be prepared in consideration of the fact that the conductive adhesive 41 is exposed according to the length of the bottom side of the chamfer of the conductive adhesive 41.
[0127] If the shortest length of the closest distance from the periphery of the semiconductor layer 40 to the periphery of the thick-film metal plate 42 in planar observation is L [mm], the thickness of the semiconductor layer 40 is h [mm], and the total thickness of the metal layer 30 and the conductive adhesive 41 directly below the semiconductor layer 40 at the corner of the semiconductor layer 40 in planar observation is hp [mm], then since the chamfer of the conductive adhesive 41 is at least 20 [deg], it is preferred that the relationship L ≥ (h + hp) / tan (20 [deg]) holds. If this relationship holds, the conductive adhesive 41 will not be exposed beyond the periphery of the thick-film metal plate 42 over the entire periphery of the semiconductor layer 40 in planar observation.
[0128] Hereinafter, a modification of the semiconductor device 1 according to the first embodiment will be described.
[0129] exist Fig. 8A , a schematic cross-sectional view of a variation 2 of the semiconductor device 1 of embodiment 1 is shown. In the semiconductor device 1 of variation 2, the support body 42 has a curved shape that is convex in the direction toward the semiconductor chip 2. The so-called curved shape of the support body 42 is, for example, a shape caused by the warping of the support body 42. The so-called warping amount of the support body 42 is the difference between the highest position and the lowest position in the Z direction on the upper surface or the lower surface of the support body 42 when the support body 42 is cross-sectionally viewed. In the case where the warping that occurs in the support body 42 is a convex warping in the direction toward the semiconductor chip 2, the highest position is the center of the support body 42 in planar observation, and the lowest position is the periphery of the support body 42 in planar observation, particularly at the corners of the periphery.
[0130] The direction and amount of warping of the support body 42 can be controlled by adjusting the amount of warping of the semiconductor chip 2 occurring at 170 [°C], the thickness and / or material of the support body 42, the thickness and / or material of the conductive adhesive 41, or the bonding conditions. The easiest way to adjust is to make the thickness of the support body 42 thinner. If the thickness of the support body 42 is made thinner, the amount of warping of the support body 42 at the time when the semiconductor device 1 is completed can be increased, but the rigidity of the semiconductor device 1 is reduced. Therefore, as a reference, it is preferred to design the thickness of the support body 42 so that the amount of warping of the support body 42 is smaller than the amount of warping of the semiconductor chip 2.
[0131] like Fig. 8A As shown, in the semiconductor device 1, when the curvature of the support body 42 is smaller than the curvature of the semiconductor chip 2 and the support body 42 has a curved shape that is convex toward the semiconductor chip 2, the pressure on the conductive adhesive 41 is reduced compared to the case where the support body 42 is not a curved shape, so the length of the conductive adhesive 41 exposed from the semiconductor layer 40 in planar observation can be suppressed.
[0132] exist Figure 8B FIG. 4 is a schematic cross-sectional view of a third variation of the semiconductor device 1 of the first embodiment. In the semiconductor device 1 of the third variation, the support body 42 has a curved shape that is convex in a direction away from the semiconductor chip 2. Figure 8B As shown, in the semiconductor device 1, when the curvature of the support body 42 is smaller than the curvature of the semiconductor chip 2 and the support body 42 has a curved shape that is convex in a direction away from the semiconductor chip 2, compared with the case where the support body 42 is not curved, it is possible to prevent the generation of pores between the semiconductor chip 2 and the conductive adhesive 41 near the center of the semiconductor layer 40 in planar observation.
[0133] (Implementation Method 2)
[0134] Hereinafter, a semiconductor device 100 according to a second embodiment in which a part of the structure of the semiconductor device 1 according to the first embodiment is modified will be described.
[0135] The semiconductor device 100 of the second embodiment is an example of a structure in which the thick metal plate, i.e., the support body 42 of the first embodiment, is changed to an insulating support body 420 , and a support body metal layer 300 is formed on the surface side of the insulating support body 420 , i.e., on the side bonded to the semiconductor chip 2 .
[0136] Here, regarding the semiconductor device 100 of the second embodiment, components similar to those of the semiconductor device 1 of the first embodiment are given the same reference numerals as those already described, and detailed description thereof is omitted, and the description will focus on differences from the semiconductor device 1 .
[0137] [1. Structure of semiconductor device]
[0138] exist Fig. 9 2 shows a schematic cross-sectional view of a semiconductor device 100 according to Embodiment 2. The difference from the semiconductor device 1 according to Embodiment 1 is that the support 42 is changed to an insulating support 420, and a support metal layer 300 is formed on the surface side of the insulating support 420. The support metal layer 300 may cover the entire surface side of the insulating support 420 in a manner that makes the side surface of the insulating support 420 the same as that of the insulating support 420. Alternatively, Fig. 9 As shown, only a portion of the surface side of the insulating support body 420 is covered.
[0139] [2. Method for manufacturing semiconductor device]
[0140] exist Fig.102 briefly shows a part of the manufacturing process of the semiconductor device 100 according to the second embodiment. Steps 501 to 504 are the same as those of the manufacturing process of the semiconductor device 1 according to the first embodiment. Step 506 is a step equivalent to step 505 in the first embodiment.
[0141] In the second embodiment, the semiconductor chip 2 is bonded to the insulating support 420 in step 506. In step 506, the support metal layer 300 is formed on the surface side of the insulating support 420 in advance, and the conductive adhesive 41 is applied to the upper surface of the support metal layer 300. The conductive adhesive 41 is, for example, a silver paste, which is hardened by heating to 170 [° C.], and the semiconductor chip 2 is bonded to the insulating support 420 or the support metal layer 300.
[0142] [3. Investigation]
[0143] In the semiconductor device 100 of this embodiment, since the insulating support 420 is used, the rigidity can be improved compared with the thick metal plate of Embodiment 1. As a raw material with good rigidity, there is a silicon substrate, for example. When a silicon substrate is used as the insulating support 420, the same effect as when a thick metal plate is used in the semiconductor device 1 of Embodiment 1 can be achieved with a thinner size.
[0144] On the other hand, in the semiconductor device 100 of the second embodiment, since the support metal layer 300 is provided on the surface of the insulating support 420, a sufficiently low on-resistance can be achieved using the support metal layer 300 as a conduction path. In particular, the semiconductor device 100 of the second embodiment is practical when the thickness of the support metal layer 300 is greater than the thickness of the first source electrode 11 and the thickness of the second source electrode 21 in the semiconductor chip 2.
[0145] In the semiconductor device 1 of the first embodiment, if the thickness of the metal layer 30 in the semiconductor chip 2 is made larger than the thickness of the first source electrode 11 and the thickness of the second source electrode 21, the direction of the warpage occurring in the semiconductor chip 2 at 170 [° C.] cannot be made convex in the direction away from the support body 42. In contrast, in the semiconductor device 100 of the second embodiment, as long as the thickness of the metal layer 30 in the semiconductor chip 2 is made smaller than the thickness of the first source electrode 11 and the thickness of the second source electrode 21, the direction of the warpage occurring in the semiconductor chip 2 at 170 [° C.] can be made convex in the direction away from the support body 42.
[0146] The support metal layer 300 preferably covers the entire area of the back side of the semiconductor chip 2. Therefore, the support metal layer 300 is provided on the surface side of the insulating support 420 and is formed in an area larger than the semiconductor layer 40 in planar observation. The thickness of the support metal layer 300 is preferably greater than the thickness of the first source electrode 11 and the thickness of the second source electrode 21.
[0147] (Implementation 3)
[0148] Hereinafter, a semiconductor device 200 according to the third embodiment in which a part of the structure is modified from the semiconductor device 1 according to the third embodiment will be described.
[0149] The semiconductor device 200 of the third embodiment is an example of a structure in which the support body 42 of the first embodiment, which is a flat plate having a uniform thickness in the plane of the thick-film metal plate, is changed to a processed support body 430 of the thick-film metal plate having a processed surface.
[0150] Here, regarding the semiconductor device 200 of the third embodiment, the same components as those of the semiconductor device 1 of the first embodiment are given the same reference numerals as those already described, and detailed description thereof is omitted, and the description will focus on the differences from the semiconductor device 1 .
[0151] [1. Structure of semiconductor device]
[0152] exist Fig.11A A schematic cross-sectional view of a semiconductor device 200 according to Embodiment 3 is shown in FIG. Fig. 11B 2 is a schematic plan view of a processing support body 430 according to Embodiment 3. Fig. 11C 2 shows a schematic plan view of the semiconductor device 200 after the semiconductor chip 2 is mounted on the processing support body 430 . The difference is that the support body 42 is changed to the processing support body 430 from the semiconductor device 1 of the first embodiment.
[0153] When only the processing support 430 is observed, the surface of the processing support 430 (the surface bonded to the semiconductor chip 2) is as follows. Fig. 11B As shown, in plan view, the first range includes the center of the processing support body 430 and does not include the outer periphery of the processing support body 430, and the second range surrounds the first range and is the remaining range of the surface of the processing support body 430. Fig.11A and Fig. 11B In FIG. 1 , an imaginary boundary line between the first range and the second range is indicated by a dotted line.
[0154] In the first range, the thickness of the processing support body 430 is constant, but in the second range, a groove-shaped process is performed on a portion of the surface of the processing support body 430, and the thickness of the processing support body 430 is thinner than that in the first range. In the third embodiment, an example is shown in which the thickness of the processing support body 430 is equal to that in the first range near the outer periphery of the processing support body 430 in the second range. However, the thickness of the processing support body 430 in the second range may be constant, or may be a shape that is gradually thinner than the thickness of the processing support body 430 in the first range.
[0155] In the semiconductor device 200, the semiconductor chip 2 is bonded to the surface side of the processing support 430 via the conductive adhesive 41. Fig.11A and Fig. 11C As shown, in plan view, the outer periphery of the semiconductor layer 40 of the semiconductor chip 2 is set to be included in the width of the groove formed in the second range of the processing support body 430. Fig. 11C In the figure, the conductive adhesive 41 which should be visible exposed from the semiconductor chip 2 in plan view is omitted.
[0156] Therefore, in the semiconductor device 200 of the third embodiment, the area of the first range on the surface of the processing support 430 in plan view is smaller than the area of the semiconductor layer 40 of the semiconductor chip 2 , and the semiconductor layer 40 is bonded to cover the entire first range in plan view.
[0157] [2. Investigation]
[0158] By making the above-mentioned structure, the length of the conductive adhesive 41 exposed in the horizontal direction from the semiconductor layer 40 in the plan view can be suppressed. Since the groove-shaped processing is performed in the second range of the processing support 430, the extruded conductive adhesive 41 flows into the groove. Since the extruded conductive adhesive 41 can be accumulated in the groove to a certain extent, the exposed length in the horizontal direction and the height raised to the side of the semiconductor chip 2 can be suppressed by appropriately changing the width and depth of the groove.
[0159] The semiconductor device of one technical solution of the present disclosure is described above based on embodiments 1 to 3 and variations 1 to 3, but the present disclosure is not limited to these embodiments and variations. As long as it does not deviate from the main purpose of the present disclosure, the various forms obtained by implementing various modifications thought of by those skilled in the art to these embodiments, or the forms constructed by combining the constituent elements of different embodiments and variations can also be included in the scope of one or more technical solutions of the present disclosure.
[0160] Industrial Applicability
[0161] A semiconductor device including the vertical MOS transistor of the present invention can be widely used as a device for controlling the conduction state of a current path.
[0162] Description of symbols
[0163] 1, 100, 200 semiconductor devices
[0164] 2Semiconductor Chip
[0165] 10 transistor (1st vertical MOS transistor)
[0166] 11 1st source electrode
[0167] Part 12 and 13
[0168] 141st source region
[0169] 15 1st gate conductor
[0170] 16 1st gate insulating film
[0171] 171st gate trench
[0172] 181st body area
[0173] 18a1st connection area
[0174] 19 1st gate electrode
[0175] 20 transistors (second vertical MOS transistors)
[0176] 21 second source electrode
[0177] Part 22 and 23
[0178] 24 Second source region
[0179] 25 2nd gate conductor
[0180] 26 second gate insulating film
[0181] 27 2nd gate trench
[0182] 28 Second body area
[0183] 28a Second connection area
[0184] 29 second gate electrode
[0185] 30 metal layers
[0186] 32Semiconductor substrate
[0187] 33 Low concentration impurity layer (drift layer)
[0188] 34 Interlayer insulation layer
[0189] 35 Passivation layer
[0190] 40 semiconductor layer
[0191] 41. Conductive adhesive
[0192] 42 Support body (thick film metal plate)
[0193] 300 Support metal layer
[0194] 420 Insulation support
[0195] 430 Processing support
[0196] 90 Boundary Line
[0197] 111 1st source pad
[0198] 119 1st gate pad
[0199] 121 2nd source pad
[0200] 129 2nd gate pad
[0201] A1 Area 1
[0202] A2 Area 2
Claims
1. A semiconductor device, which is a chip size package type semiconductor device capable of face-down mounting, characterized in that: have: Semiconductor substrate; A low-concentration impurity layer formed on the surface side of the semiconductor substrate; a first vertical MOS transistor formed in a first region of the semiconductor layer when the semiconductor substrate and the low-concentration impurity layer are used together as a semiconductor layer; a second vertical MOS transistor formed in a second region adjacent to the first region in a planar view of the semiconductor layer; The first source electrode of the first vertical MOS transistor is formed on the surface side of the semiconductor layer; The second source electrode of the second vertical MOS transistor is formed on the surface side of the semiconductor layer; as well as A support body formed on the back side of the semiconductor substrate via a conductive adhesive; In the above-mentioned planar observation, the above-mentioned support body has a larger area than the above-mentioned semiconductor layer and includes the above-mentioned semiconductor layer; The thickness of the support body is greater than the thickness of the semiconductor layer; In the cross-sectional view of the semiconductor device including the center of the semiconductor layer and the periphery of the semiconductor layer in the planar observation, when observing the semiconductor chip other than the supporting body and the conductive adhesive in the semiconductor device, the semiconductor chip is a curved shape that is convex in a direction away from the supporting body.
2. The semiconductor device according to claim 1, wherein In the above-mentioned plane observation, the above-mentioned semiconductor layer is a square; The thickness of the conductive adhesive directly below the semiconductor layer at the periphery of the semiconductor layer in the planar view is smaller than the thickness of the conductive adhesive directly below the semiconductor layer at the center of the semiconductor layer in the planar view.
3. The semiconductor device according to claim 2, wherein: In the above planar observation, the area of the above semiconductor layer is more than 6.2, the unit is mm 2 ; Assume the area of the semiconductor layer is S, in mm 2 , assuming the thickness of the semiconductor layer is h, in mm, then The relationship h≤0.016×S-0.042 holds true.
4. The semiconductor device according to claim 3, wherein: In the above plan view, the semiconductor layer is 11.5 mm 2 The following area; The relationship h≤0.014×S-0.074 holds true.
5. The semiconductor device according to claim 3, wherein: A metal layer is provided on the back side of the semiconductor substrate and is in contact with the entire back side of the semiconductor substrate; In the above planar observation, let the shortest length of the closest distance from the outer periphery of the above semiconductor layer to the outer periphery of the above support body be L in mm, At the corner of the semiconductor layer in the planar view, the total thickness of the metal layer and the conductive adhesive directly below the semiconductor layer is hp in mm. The relationship of L≥(h+hp) / tan(20deg) holds.
6. The semiconductor device according to claim 3, wherein: The support body is made of metal.
7. The semiconductor device according to claim 3, wherein: A metal layer is provided on the back side of the semiconductor substrate and is in contact with the entire back side of the semiconductor substrate; The thickness of the first source electrode and the thickness of the second source electrode are greater than the thickness of the metal layer.
8. The semiconductor device according to claim 3, wherein: The conductive adhesive is directly bonded to the entire back surface of the semiconductor substrate.
9. The semiconductor device according to claim 1, wherein: A support metal layer is provided on the surface side of the support body, connected to a region having an area larger than that of the semiconductor substrate in the planar view; The thickness of the supporting metal layer is greater than the thickness of the first source electrode and the thickness of the second source electrode; The support body is made of an insulating material.
10. The semiconductor device according to claim 3, wherein: In the above-mentioned planar observation, the surface side of the above-mentioned support body has a first range and a second range, the above-mentioned first range includes the center of the above-mentioned support body and does not include the outer periphery of the above-mentioned support body, and the above-mentioned second range surrounds the above-mentioned first range; In the above cross-sectional view, the height of the first range is constant, and the second range includes a portion lower than the height of the first range; In the above-mentioned planar observation, the area of the above-mentioned first range is smaller than the area of the above-mentioned semiconductor substrate; The semiconductor substrate is provided so as to entirely cover the first region of the support body in the planar view.
11. The semiconductor device according to claim 10, wherein: The second range further includes a portion where the height of the second range is the same as the height of the first range.
12. The semiconductor device according to claim 3, wherein: In the cross-sectional view, the support body is in a curved shape convex toward the semiconductor chip; The amount of curvature of the support body is smaller than the amount of curvature of the semiconductor chip.
13. The semiconductor device according to claim 3, wherein: In the cross-sectional view, the support body is in a curved shape convex in a direction away from the semiconductor chip; The amount of warping of the support body is smaller than the amount of warping of the semiconductor chip.
Citation Information
Patent Citations
Process for manufacturing printed circuits with an individual rigid conductive metallic support
US4616413A
Semiconductor device, semiconductor module, and semiconductor package device
CN109564941A
Semiconductor device
CN110114888A
Semiconductor device and method for manufacturing semiconductor device
CN111630645A
Semiconductor device