Battery assembly method and battery
Through a new battery assembly method, the composite cover plate and battery shell are first welded, and the composite pole and cover plate are then welded, and the current conduction between the electrode ear and the composite pole is achieved through the structure, which solves the welding quality in the traditional method and space occupation issues have improved the space utilization and energy density of the battery.
Patent Information
- Application Number
- CN202411615865.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-13
- Publication Date
- 2025-02-18
AI Technical Summary
In the traditional square shell battery assembly method, the welding quality of the electrode ear and the electrode column is easily affected by high temperature and vibration, resulting in a decrease in product yield. The electrode ear and the electrode ear occupy the inner space of the battery case, limiting the volume and energy of the electrode group. density.
A battery assembly method is adopted, first weld the composite cover plate to the battery shell, then weld the composite pole to the composite cover plate, and finally the electrode ear and the composite pole are turned on, avoiding other welding processes to the electrode ear and the electrode The influence of the quality of the composite pole connection, and the pole ear extends out of the battery case through the penetration structure, eliminating the internal connection and space occupation between the pole ear and the composite pole.
The space utilization and energy density of the battery are improved, the volume of the pole set is increased, and the product quality and power supply capacity are improved.
Smart Images

Figure CN119481308A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of batteries, and in particular to a battery assembly method and a battery. Background Art
[0002] Lithium-ion power battery is a new type of high-energy battery based on the movement of lithium ions between the positive electrode and the negative electrode. When charging, lithium ions are deintercalated from the positive electrode and embedded in the negative electrode through the electrolyte; when discharging, the opposite is true, and lithium ions are deintercalated from the negative electrode back to the positive electrode to form a current for the device to use. Because lithium-ion power batteries have the advantages of high energy, high battery voltage, wide operating temperature range, and long storage life, they are widely used in electric vehicles, energy storage systems, military equipment, etc. With continuous development, lithium-ion power batteries have derived many different types, such as blade batteries, square shell batteries or large cylindrical batteries. Among them, square shell batteries are known for their cubic or rectangular shape and solid metal shell, with high sealing, long life and good safety. With its advantages of high grouping efficiency and large single cell capacity, square shell batteries are highly competitive in the market. Square shell batteries include pole groups with pole ears on the same side, poles, cover plates, upper plastics, lower plastics, welding stations, sealing rings, and battery shells.
[0003] The traditional assembly process of square shell batteries is usually to first install the pole assembly into the battery shell, then weld the pole column to the pole ear of the corresponding polarity, then install the lower plastic and cover plate in sequence, and make a part of the pole column pass through the lower plastic and cover plate and extend out of the battery shell. After the cover plate is assembled, weld the cover plate to the battery shell, and then install the upper plastic, sealing ring and welding platform in sequence on the outer side of the cover plate corresponding to the extended part of the pole column, and complete the welding of the welding platform and the cover plate, as well as the welding of the welding platform and the pole column extending out of the cover plate, thereby completing the assembly of the square shell battery.
[0004] However, for square-shell batteries assembled using this method, on the one hand, it is necessary to complete the welding of the pole ears and pole posts first, and then complete the welding of the cover plate and the battery shell, the welding platform and the cover plate, and the welding platform and the pole posts. As a result, the pole ears and pole posts that have been welded will be affected by adverse factors such as high temperature and vibration during the welding of the cover plate and the battery shell, the welding platform and the cover plate, and the welding platform and the pole posts, thereby reducing the welding quality between the pole posts and the pole ears and reducing the product yield. On the other hand, since this method also requires that the pole posts and the pole ears are connected inside the battery shell, the pole ears and pole posts will occupy a larger space inside the battery shell, limiting the volume of the pole group and resulting in a low energy density. Summary of the invention
[0005] The object of the present invention is to provide a battery assembly method and a battery with high space utilization, good product quality and high energy density.
[0006] To achieve this object, the present invention adopts the following technical solutions:
[0007] On the one hand, a battery assembly method is provided, wherein the battery assembled by the battery assembly method comprises a battery housing, an electrode group, a composite cover plate and a composite electrode column;
[0008] The battery assembly method comprises the following steps:
[0009] S1, the electrode group includes a first surface with an electrode ear, a second surface parallel to the first surface, and a plurality of side surfaces perpendicular to the first surface and the second surface, and an insulating film is coated on the plurality of side surfaces and the outer side of the second surface;
[0010] S2, the composite cover plate is provided with a through structure for the electrode lug to extend, the composite cover plate is installed on the first surface of the electrode group, and the electrode lug is passed through the through structure;
[0011] S3, a first insulating layer for isolating the composite cover plate and the electrode lug is injection-molded on the composite cover plate, and the overlapping area between the insulating film coated on the outside of the electrode group and the first insulating layer is hot-melted to form an electrode group unit;
[0012] S4, the battery housing is a single-side open structure with a cavity, and the electrode group unit is installed in the cavity of the battery housing;
[0013] S5, welding the composite cover plate to the battery housing;
[0014] S6, a receiving groove is further provided on the side of the composite cover plate away from the electrode group, the composite pole is installed in the receiving groove, and the composite pole is welded to the composite cover plate;
[0015] S7, achieving current conduction between the composite pole and the pole lug.
[0016] Optionally, in step S1, the following steps are also included:
[0017] S11, the battery further includes a bottom support plate, and the bottom support plate is pre-heat-fused at a set position of the insulating film;
[0018] S12, covering the insulating film on the plurality of side surfaces and the second surface of the electrode group, and making the bottom support plate cover the second surface of the electrode group.
[0019] Optionally, in step S2, the following steps are also included:
[0020] S21, pre-installing the composite cover plate on the side of the first surface away from the electrode group, and passing the electrode lug through the through structure;
[0021] S22, measuring the distance L1 between the closest points of the composite cover plate and the insulating film, and determining whether L1 satisfies 0.5 mm ≤ L1 ≤ 3 mm, if yes, executing step S3, if no, executing step S23;
[0022] S23, after removing the pre-installed composite cover plate, cutting the insulating film, after the cutting is completed, executing step S21.
[0023] Optionally, a plurality of spaced-apart thermal melting points are provided in the overlapping region between the insulating film and the first insulating layer, and the distance between the boundary of each thermal melting point away from the pole group and the boundary of the overlapping region away from the pole group is L2, and satisfies 0.5mm≤L2≤3mm.
[0024] And / or, the distance between the boundary of each of the thermal melting points facing the electrode group and the boundary of the overlapping area facing the electrode group is L3, and satisfies 0.5mm≤L3≤3mm.
[0025] Optionally, in step S5, the following steps are also included:
[0026] S51, the composite cover plate and the battery housing are pre-welded and positioned at a plurality of first pre-welding points arranged at intervals;
[0027] S52, fully welding the composite cover plate and the battery casing.
[0028] Optionally, the composite cover plate includes a cover plate body and the first insulating layer;
[0029] The receiving groove is provided on the cover body, and the cover body is also provided with a plug-in through hole provided in the receiving groove;
[0030] The first insulating layer is injection molded on the cover body, and includes an upper insulating portion, a lower insulating portion and a plug-in portion. The upper insulating portion is arranged on a side of the cover body away from the pole group and is located in the accommodating groove. The lower insulating portion is arranged on a side of the cover body facing the pole group and is located between the cover body and the pole group. The plug-in portion is inserted in the plug-in through hole and is used to connect the upper insulating portion and the lower insulating portion. The penetrating structure penetrates the upper insulating portion, the plug-in portion and the lower insulating portion.
[0031] Optionally, in step S6, the following steps are also included:
[0032] S61, a mounting groove is further provided on a side of the upper insulating portion away from the cover body, and the battery further comprises a connecting piece, and the connecting piece is installed in the mounting groove;
[0033] S62, bending the portion of the electrode tab extending out of the through structure, and welding the bent electrode tab to the connecting sheet;
[0034] S63, the battery further includes a sealing ring, and the sealing ring is installed in the receiving groove;
[0035] S64, placing the composite pole into the receiving groove, wherein the sealing ring is sandwiched between the composite pole and the composite cover plate;
[0036] S65, welding the composite pole and the composite cover plate.
[0037] Optionally, in step S7, the following steps are also included:
[0038] S71, a connection boss protruding along the side of the connection piece facing the composite pole is provided, and the composite pole is pre-welded and positioned on the connection boss through a plurality of second pre-welding points arranged at intervals;
[0039] S72, fully welding the composite pole and the connecting boss.
[0040] Optionally, in step S65, the following steps are also included:
[0041] S651, the composite pole comprises a pole body, a welding ring and a second insulating layer for realizing an insulating connection between the pole body and the welding ring, the welding ring being pre-welded and positioned in the receiving groove through a plurality of third pre-welding points arranged at intervals;
[0042] S652, fully weld the welding ring in the receiving groove.
[0043] On the other hand, a battery is provided, wherein the battery is assembled using any of the battery assembly methods described above.
[0044] Beneficial effects of the present invention:
[0045] The present invention provides a battery assembly method, which first welds a composite cover plate to a battery shell, then welds a composite pole to a composite cover plate, and finally connects a pole ear to a composite pole to achieve current conduction, thereby avoiding the influence of other welding processes on the connection quality between the pole ear and the composite pole that have already achieved current conduction, and enables the pole ear to extend out of the battery shell through a penetrating structure to achieve current conduction with the composite pole, thereby eliminating the space occupied by the pole ear and the composite pole and the composite pole extending into the battery shell. Therefore, on the one hand, the occupation of the internal space is reduced and the utilization rate of the space is improved, and on the other hand, space is provided for increasing the pole group and the energy density is improved.
[0046] The present invention also provides a battery, which is assembled by applying the above-mentioned battery assembly method, so that the volume of the electrode group can be further increased, thereby improving the energy density of the battery and increasing the power supply capacity of the battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Figure 1 is a flow chart of a battery assembly method provided by the present invention;
[0048] Figure 2 is a structural exploded view of the battery provided by the present invention;
[0049] Figure 3 is a partial front structural cross-sectional view of a battery provided by the present invention;
[0050] Figure 4 is a partial side structural cross-sectional view of a battery provided by the present invention;
[0051] Figure 5 It is a schematic diagram of the distribution of the hot melting points of the first insulating layer and the insulating film in the battery provided by the present invention;
[0052] Figure 6 yes Figure 5 A magnified view of the structure of part A;
[0053] Figure 7 It is a schematic diagram of the distribution of pre-welding points between the composite cover plate and the battery shell in the battery provided by the present invention;
[0054] Figure 8 It is a schematic diagram of the structure of the cover plate body in the battery provided by the present invention;
[0055] Fig. 9 It is a schematic structural diagram of the first insulating layer in the battery provided by the present invention.
[0056] In the figure:
[0057] 1. Battery housing; 11. First pre-welding point;
[0058] 2. pole group; 21. pole ear; 22. first surface; 23. second surface; 24. side surface;
[0059] 3. Composite cover plate; 31. Cover plate body; 311. Accommodating groove; 312. Insertion through hole; 32. First insulating layer; 321. Upper insulating part; 322. Lower insulating part; 323. Insertion part; 324. Mounting groove; 325. Penetration structure; 326. Shaping structure;
[0060] 4. Composite pole; 41. Pole body; 42. Welding ring; 43. Second insulating layer;
[0061] 5. Insulating film; 51. Thermal melting point;
[0062] 6. Bottom support plate;
[0063] 7. Connecting piece; 71. Connecting boss;
[0064] 8. Sealing ring. DETAILED DESCRIPTION
[0065] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.
[0066] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0067] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0068] In the description of this embodiment, the terms "upper", "lower", "right", etc., directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.
[0069] The square shell battery includes a pole group with the pole lugs on the same side, a pole column, a cover plate, an upper plastic, a lower plastic, a welding platform, a sealing ring, and a battery shell. When assembling by the traditional method, on the one hand, it is necessary to complete the welding of the pole lug and the pole column first, and then complete the welding of the cover plate and the battery shell, the welding platform and the cover plate, and the welding platform and the pole column. As a result, the pole lug and the pole column that have been welded will be affected by adverse factors such as high temperature and vibration when the cover plate is welded to the battery shell, the welding platform and the cover plate are welded, and the welding platform and the pole column are welded, thereby reducing the welding quality between the pole column and the pole lug and reducing the product yield. On the other hand, since this method also requires that the pole column and the pole lug be connected inside the battery shell, the pole lug and the pole column will occupy a large space inside the battery shell, limiting the volume of the pole group and having a low energy density.
[0070] Therefore, in order to avoid the connection between the pole and the lug in advance, which may affect the connection quality between the pole and the lug in other subsequent processes, reduce additional space occupation, and improve space utilization and energy density, the present embodiment provides a battery assembly method, and the battery assembled by the battery assembly method includes a battery casing 1, a pole group 2, a composite cover plate 3 and a composite pole 4.
[0071] like Figures 1 to 9 As shown, the battery assembly method includes the following steps:
[0072] S1, the pole group 2 includes a first surface 22 with a pole ear 21, a second surface 23 parallel to the first surface 22, and a plurality of side surfaces 24 perpendicular to the first surface 22 and the second surface 23, and an insulating film 5 is coated outside the plurality of side surfaces 24 and the second surface 23;
[0073] S1, the pole group 2 includes a first surface 22 with a pole ear 21, a second surface 23 parallel to the first surface 22, and a plurality of side surfaces 24 perpendicular to the first surface 22 and the second surface 23, and an insulating film 5 is coated outside the plurality of side surfaces 24 and the second surface 23;
[0074] S2. The composite cover plate 3 is provided with a through structure 325 for the pole ear 21 to extend out. The composite cover plate 3 is installed on the first surface 22 of the pole group 2, and the pole ear 21 passes through the through structure 325.
[0075] S3, a first insulating layer 32 for isolating the composite cover plate 3 and the pole lug 21 is injection molded on the composite cover plate 3, and the overlapping area between the insulating film 5 coated on the outside of the pole group 2 and the first insulating layer 32 is hot-melted to form a pole group unit;
[0076] S4, the battery housing 1 is a single-side open structure with a cavity, and the electrode group unit is installed in the cavity of the battery housing 1;
[0077] S5, welding the composite cover plate 3 to the battery housing 1;
[0078] S6. A receiving groove 311 is further provided on the side of the composite cover plate 3 facing away from the electrode group 2. The composite pole 4 is installed into the receiving groove 311, and the composite pole 4 is welded to the composite cover plate 3.
[0079] S7, achieving current conduction between the composite pole 4 and the pole ear 21.
[0080] By first welding the composite cover plate 3 to the battery shell 1, then welding the composite pole 4 to the composite cover plate 3, and finally connecting the pole ear 21 to the composite pole 4 to achieve current conduction, the influence of other welding processes on the connection quality between the pole ear 21 and the composite pole 4 that have achieved current conduction is avoided, and the pole ear 21 is extended through the through structure 325 to the battery shell 1 and the composite pole 4 to achieve current conduction, eliminating the space occupied by the connection between the pole ear 21 and the composite pole 4 and the composite pole 4 extending into the battery shell 1. On the one hand, the occupation of the internal space is reduced and the utilization rate of the space is improved. On the other hand, space is provided for increasing the pole group 2 and the energy density is improved.
[0081] Alternatively, if Figure 2 As shown, in step S1, the following steps are also included:
[0082] S11, the battery further includes a bottom support plate 6, and the bottom support plate 6 is pre-heat-fused at a set position of the insulating film 5;
[0083] S12 , covering the insulating film 5 on the multiple side surfaces 24 and the second surface 23 of the electrode group 2 , and making the bottom support plate 6 cover the second surface 23 of the electrode group 2 .
[0084] By hot-melting the bottom support plate 6 on the insulating film 5 before coating the insulating film 5, when the insulating film 5 is coated on the electrode group 2, the bottom support plate 6 can cover the second surface 23 of the electrode group 2, so that when the electrode group 2 is put into the shell, the second surface 23 is protected by the bottom support plate 6 to avoid scratches when the electrode group 2 is put into the shell, wherein the area of the bottom support plate 6 is adapted to the area of the second surface 23.
[0085] Alternatively, if Figure 2 , Figure 4 , Figure 5 , Figure 6 As shown, in step S2, the following steps are also included:
[0086] S21, pre-install the composite cover plate 3 on the side of the first surface 22 away from the electrode group 2, and make the electrode ear 21 pass through the through structure 325;
[0087] S22, measuring the distance L1 between the closest points of the composite cover plate 3 and the insulating film 5, and determining whether L1 satisfies 0.5 mm ≤ L1 ≤ 3 mm, if yes, executing step S3, if not, executing step S23;
[0088] S23, after removing the pre-installed composite cover plate 3, the insulating film 5 is trimmed, and after the trimming is completed, step S21 is executed.
[0089] By pre-installing the composite cover plate 3 and determining that the distance dimension L1 between the composite cover plate 3 and the insulating film 5 satisfies the range of 0.5mm≤L1≤3mm, on the one hand, it is possible to avoid the distance dimension L1 between the composite cover plate 3 and the insulating film 5 being too small, which will affect the welding of the composite cover plate 3 and the battery casing 1 and easily cause problems such as welding explosion points. On the other hand, it is possible to avoid the distance dimension L1 between the composite cover plate 3 and the insulating film 5 being too large, which will increase the structural size of the first insulating layer and increase the manufacturing cost.
[0090] In this embodiment, the distance dimension L1 between the cut insulating film 5 and the composite cover plate 3 after assembly can be any value between 0.5 mm and 3 mm or a range between any two values, such as 0.5 mm, 1 mm, 1.5 mm, 2 mm, 2.5 mm, 3 mm, etc.
[0091] Alternatively, if Figure 2 , Figure 4 , Figure 5 , Figure 6 As shown, a plurality of spaced-apart thermal melting points 51 are provided in the overlapping region between the insulating film 5 and the first insulating layer 32, and the distance between the boundary of each thermal melting point 51 away from the pole group 2 and the boundary of the overlapping region away from the pole group 2 is L2, and satisfies 0.5mm≤L2≤3mm.
[0092] By setting a plurality of spaced hot melting points 51, the hot melting between the insulating film 5 and the first insulating layer 32 is achieved, thereby ensuring that the scope of hot melting is wide enough and the firmness of hot melting is ensured. On the other hand, compared with the full hot melting method, the hot melting area is small, thereby shortening the time required for hot melting operation and improving the efficiency of hot melting operation. At the same time, by setting the distance dimension between the boundary of each hot melting point 51 away from the pole group 2 and the boundary of the overlapping area away from the pole group 2 as L2, and limiting the distance dimension L2 between the boundary of each hot melting point 51 away from the pole group 2 and the boundary of the overlapping area away from the pole group 2 to meet 0.5mm≤L2≤3mm, it is ensured that the hot melting point 51 and the boundary of the overlapping area away from the pole group 2 maintain a suitable distance, on the one hand, avoiding the insufficient area that can be operated during hot melting due to too small a distance, and on the other hand, avoiding the loose connection of the area on the side of the hot melting point 51 away from the pole group 2 due to too large a distance.
[0093] In this embodiment, the first insulating layer 32 includes a large end face with a larger area and a small end face with a smaller area, so the area of the overlapping area formed by different end faces and the insulating film 5 is also different, wherein at least three hot melting points 51 arranged at intervals are arranged on the surface with a larger area, and at least one hot melting point 51 is arranged on the surface with a smaller area, wherein the shape of the hot melting point 51 can be freely set according to demand, such as circular, elliptical or polygonal, etc. wherein when there are multiple hot melting points 51, it is necessary to ensure that the multiple hot melting points 51 arranged at intervals are evenly distributed.
[0094] Among them, the distance dimension L2 between the boundary of each thermal melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 can be any value between 0.5mm and 3mm or a range between any two values, such as 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, 3mm, etc.
[0095] Alternatively, if Figure 2 , Figure 4 , Figure 5 , Figure 6 As shown, the distance between the boundary of each thermal melting point 51 facing the electrode group 2 and the boundary of the overlapping area facing the electrode group 2 is L3, and satisfies 0.5 mm≤L3≤3 mm.
[0096] By setting a plurality of spaced hot melting points 51, hot melting between the insulating film 5 and the first insulating layer 32 is achieved, thereby ensuring that the scope of hot melting is wide enough and the firmness of hot melting is ensured, and on the other hand, compared with the full hot melting method, the hot melting operation time is short and the hot melting operation efficiency is high. At the same time, by setting the distance dimension between the boundary of each hot melting point 51 facing the pole group 2 side and the boundary of the overlapping area facing the pole group 2 side as L3, and limiting the distance dimension L3 between the boundary of each hot melting point 51 facing the pole group 2 side and the boundary of the overlapping area facing the pole group 2 side to satisfy 0.5mm≤L3≤3mm, it is ensured that the hot melting point 51 and the boundary of the overlapping area facing the pole group 2 side maintain a suitable distance, on the one hand, avoid too small a distance, resulting in insufficient operable area during hot melting, and on the other hand, avoid too large a distance, resulting in loose connection of the area on the side of the hot melting point 51 facing the pole group 2 side.
[0097] In this embodiment, the first insulating layer 32 includes a large end face with a larger area and a small end face with a smaller area, so the area of the overlapping area formed by different end faces and the insulating film 5 is also different, wherein at least three hot melting points 51 are set on the surface with a larger area, and at least one hot melting point 51 is set on the surface with a smaller area, wherein the shape of the hot melting point 51 can be freely set according to demand, such as circular, elliptical or polygonal, etc. wherein when there are multiple hot melting points 51, it is necessary to ensure that the multiple hot melting points 51 set at intervals are evenly distributed.
[0098] Among them, the distance dimension L3 between the boundary of each thermal melting point 51 toward the pole group 2 side and the boundary of the overlapping area toward the pole group 2 side can be any value between 0.5mm and 3mm or a range between any two values, such as 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, 3mm, etc.
[0099] Alternatively, if Figure 7 As shown, in step S5, the following steps are also included:
[0100] S51, the composite cover plate 3 and the battery housing 1 are pre-welded and positioned at a plurality of first pre-welding points 11 arranged at intervals;
[0101] S52, fully welding the composite cover plate 3 and the battery casing 1.
[0102] By pre-welding the composite cover plate 3 and the battery casing 1 using a plurality of first pre-welding points 11 arranged at intervals, it is ensured that the relative positions of the composite cover plate 3 and the battery casing 1 are positioned before full welding. Even if the initial positioning is incorrect, it is convenient to separate and reposition the two, thereby achieving recycling and reducing the scrap rate of the product.
[0103] In this embodiment, since the composite cover plate 3 includes a large end face with a larger area and a small end face with a smaller area, the area of the overlapping area formed by different end faces and the battery housing 1 is also different, wherein at least three first pre-welding positions 11 are set on the surface with a larger area, preferably five, and at least one first pre-welding position 11 is set on the surface with a smaller area, preferably three, wherein the shape of the first pre-welding position 11 can be freely set according to demand, such as circular, elliptical or polygonal. Wherein, when there are multiple first pre-welding positions 11, it is necessary to ensure that the multiple first pre-welding positions 11 set at intervals are evenly distributed.
[0104] Alternatively, if Figure 2 , Figure 4 , Figure 8 , Fig. 9As shown, the composite cover plate 3 includes a cover plate body 31 and a first insulating layer 32, a receiving groove 311 is opened on the cover plate body 31, and a plug-in through hole 312 is also opened on the cover plate body 31 and is arranged in the receiving groove 311. The first insulating layer 32 is injection molded on the cover plate body 31, and includes an upper insulating portion 321, a lower insulating portion 322 and a plug-in portion 323. The upper insulating portion 321 is arranged on the side of the cover plate body 31 away from the pole group 2 and is located in the receiving groove 311. The lower insulating portion 322 is arranged on the side of the cover plate body 31 facing the pole group 2 and is located between the cover plate body 31 and the pole group 2. The plug-in portion 323 is inserted in the plug-in through hole 312 and is used to connect the upper insulating portion 321 and the lower insulating portion 322. The through structure 325 penetrates the upper insulating portion 321, the plug-in portion 323 and the lower insulating portion 322.
[0105] By setting a first insulating layer 32 composed of an upper insulating part 321, a lower insulating part 322 and an inserting part 323, and making the upper insulating part 321 arranged on the side of the cover body 31 away from the pole group 2, and making the lower insulating part 322 arranged on the side of the cover body 31 facing the pole group 2, making the inserting part 323 inserted in the inserting through hole 312, and making the penetrating structure 325 penetrate the upper insulating part 321, the inserting part 323 and the lower insulating part 322, the first insulating layer 32 is used to achieve insulation protection for both sides of the cover body 31 and the inside of the inserting through hole 312, and isolate the pole ear 21 and the cover body 31, so as to avoid direct contact between the pole ear 21 and the cover body 31 when passing through the cover body 31, resulting in a short circuit, thereby ensuring safety and protection.
[0106] In this embodiment, the cover body 31 is a bare aluminum plate, and the first insulating layer 32 is a plastic part directly molded on the cover body 31 by an injection molding process. Compared with the traditional cover assembly, the separate lower insulating part is eliminated, thereby reducing the number of parts and simplifying the assembly process. In addition, in this embodiment, the upper insulating part 321, the plug-in part 323 and the lower insulating part 322 are an integrated structural part formed simultaneously by an injection molding process. In other embodiments, the upper insulating part 321, the plug-in part 323 and the lower insulating part 322 can also be separately injection molded and then plugged into each other, so that the first insulating layer 32 is a split structural part.
[0107] In this embodiment, in order to verify the influence of the distance dimension L1, the distance dimension L2 and the distance dimension L3 on the quality of the assembled product in the battery assembly method, as shown in Table 1, six groups of embodiments and six groups of comparative examples are provided for verification, wherein the composite cover plate 3 includes a cover plate body 31 and a first insulating layer 32 composed of an upper insulating portion 321, a lower insulating portion 322 and a plug-in portion 323, so the distance dimension L1 between the closest point between the composite cover plate 3 and the insulating film 5 is substantially the distance between the cover plate body 31 and the insulating film 5 away from the electrode group. 2, the distance dimension L2 between the boundary of the hot melting point 51 away from the pole group 2 and the boundary of the overlapping area away from the pole group 2 is essentially the distance between the boundary of the hot melting point 51 away from the pole group 2 and the boundary of the overlapping area of the lower insulating portion 322 away from the pole group 2, and the distance dimension L3 between the boundary of the hot melting point 51 toward the pole group 2 and the boundary of the overlapping area toward the pole group 2 is essentially the distance between the boundary of the hot melting point 51 toward the pole group 2 and the boundary of the overlapping area of the lower insulating portion 322 toward the pole group 2.
[0108] Table 1
[0109]
[0110] In Example 1, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 0.5 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 0.5 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 0.5 mm. At this time, the battery is assembled according to the above data. It is verified that there is no explosion point in the weld around the shell cover. After disassembling the battery, the insulating film 5 is not damaged and does not fall off.
[0111] In Example 2, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 1 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 2 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 2 mm. At this time, the battery is assembled according to the above data, and it is verified that there is no explosion point in the peripheral weld of the shell cover. After disassembling the battery, the insulating film 5 is not damaged and does not fall off.
[0112] In Example 3, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 1.5 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 1 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 3 mm. At this time, the battery is assembled according to the above data, and it is verified that there is no explosion point in the peripheral weld of the shell cover. After disassembling the battery, the insulating film 5 is not damaged and does not fall off.
[0113] In Example 4, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 2 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 3 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 1 mm. At this time, the battery is assembled according to the above data, and it is verified that there is no explosion point in the peripheral weld of the shell cover. After disassembling the battery, the insulating film 5 is not damaged and does not fall off.
[0114] In Example 5, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 2.5 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 1.5 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 2.5 mm. At this time, the battery is assembled according to the above data, and it is verified that there is no explosion point in the peripheral weld of the shell cover. After disassembling the battery, the insulating film 5 is not damaged and does not fall off.
[0115] In Example 6, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 3 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 2.5 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 1.5 mm. At this time, the battery is assembled according to the above data, and it is verified that there is no explosion point in the peripheral weld of the shell cover. After disassembling the battery, the insulating film 5 is not damaged and does not fall off.
[0116] It can be seen from Examples 1 to 6 that when the distance dimension L1 between the composite cover plate 3 and the insulating film 5 satisfies the range of 0.5mm≤L1≤3mm, the distance dimension L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 satisfies the range of 0.5mm≤L2≤3mm, and the distance dimension L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 satisfies the range of 0.5mm≤L3≤3mm, the battery assembled by the battery assembly method has no explosion points in the weld around the shell cover, and after disassembling the battery, the insulating film 5 is not damaged or falls off, and has high product quality.
[0117] In comparative example 1, the distance dimension L1 between the composite cover plate 3 and the insulating film 5 is set to 0.1 mm, the distance dimension L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 1 mm, and the distance dimension L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 1 mm. At this time, the battery assembled according to the above data is verified to have explosion points during welding around the shell cover, and the insulating film 5 melts.
[0118] It can be seen from Comparative Example 1 that when the distance dimension L1 between the composite cover plate 3 and the insulating film 5 is less than the minimum value of 0.5mm≤L1≤3mm, at this time, since the insulating film 5 is close to the cover plate body 31, an explosion point occurs when welding the periphery of the shell cover, and since the insulating film 5 is too close to the welding position, the high temperature generated by the welding causes the insulating film 5 to melt, resulting in poor insulation protection performance of the assembled battery.
[0119] In Comparative Example 2, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 1 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 0.1 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 1 mm. At this time, the battery is assembled according to the above data, and it is verified that the insulating film 5 has fallen off.
[0120] It can be seen from Comparative Example 2 that when the distance dimension L2 between the boundary of the hot melting point 51 away from the side of the electrode group 2 and the boundary of the overlapping area away from the side of the electrode group 2 is less than the minimum value of 0.5mm≤L2≤3mm, since the hot melting point 51 is close to the upper edge of the overlapping area of the lower insulating portion 322, part of the hot melting point exceeds the upper edge of the insulating film 5, resulting in insufficient hot melting area between the insulating film 5 and the lower insulating portion 322, which causes the insulating film 5 to fall off, resulting in poor insulation protection performance of the assembled battery.
[0121] In comparative example 3, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 1 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 1 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 0.1 mm. At this time, the battery is assembled according to the above data, and it is verified that melting through occurs between the insulating film 5 and the lower insulating portion 322, resulting in a short circuit.
[0122] It can be seen from Comparative Example 3 that when the distance dimension L3 between the boundary of the hot melting point 51 toward the side of the electrode group 2 and the boundary of the overlapping area toward the side of the electrode group 2 is less than the minimum value of 0.5mm≤L3≤3mm, since the hot melting point 51 is close to the lower edge of the overlapping area of the lower insulating portion 322, part of the hot melting point 51 exceeds the lower edge of the lower insulating portion 322, resulting in melting through between the insulating film 5 and the lower insulating portion 322, thereby causing a short circuit problem, resulting in poor insulation protection performance of the assembled battery.
[0123] In comparative example 4, the distance L1 between the composite cover plate 3 and the insulating film 5 is set to 4 mm, the distance L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 1 mm, and the distance L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 1 mm. At this time, the battery is assembled according to the above data. It is verified that the lower insulating portion 322 occupies a larger internal space, resulting in the compression of the volume of the electrode group 2, thereby resulting in a lower energy density of the assembled battery.
[0124] It can be seen from Comparative Example 4 that when the distance dimension L1 between the composite cover plate 3 and the insulating film 5 is greater than the maximum value of 0.5mm≤L1≤3mm, at this time, since the insulating film 5 is far away from the cover plate body 31, the lower insulating part 322 occupies a larger internal space. Therefore, in order to complete the assembly, it is necessary to reduce the volume of the electrode group 2, thereby reducing the energy density of the assembled battery, and the power supply capacity is poor, which does not meet the use requirements.
[0125] In comparative example 5, the distance dimension L1 between the composite cover plate 3 and the insulating film 5 is set to 1 mm, the distance dimension L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 4 mm, and the distance dimension L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 1 mm. At this time, the battery is assembled according to the above data. It is verified that the insulating film 5 is located in the area between the hot melting point 51 and the upper edge of the overlapping area of the lower insulating portion 322, and is not tightly connected to the lower insulating portion 322, resulting in flanging of the insulating film 5.
[0126] It can be seen from Comparative Example 5 that when the distance dimension L2 between the boundary of the hot melting point 51 away from the side of the electrode group 2 and the boundary of the overlapping area away from the side of the electrode group 2 is greater than the maximum value of 0.5mm≤L2≤3mm, since the hot melting point 51 is far away from the upper edge of the overlapping area of the lower insulating part 322, the insulating film 5 is located in the area between the hot melting point 51 and the upper edge of the overlapping area of the lower insulating part 322, and is not tightly connected to the lower insulating part 322, resulting in the insulating film 5 being flanging, which does not meet the use requirements.
[0127] In comparative example 6, the distance dimension L1 between the composite cover plate 3 and the insulating film 5 is set to 1 mm, the distance dimension L2 between the boundary of the hot melting point 51 away from the electrode group 2 and the boundary of the overlapping area away from the electrode group 2 is set to 1 mm, and the distance dimension L3 between the boundary of the hot melting point 51 toward the electrode group 2 and the boundary of the overlapping area toward the electrode group 2 is set to 4 mm. At this time, the battery is assembled according to the above data. It is verified that the insulating film 5 is located in the area between the hot melting point 51 and the lower edge of the overlapping area of the lower insulating portion 322, and is not tightly connected to the lower insulating portion 322, and there is a gap between the insulating film 5 and the electrode group 2.
[0128] It can be seen from Comparative Example 6 that when the distance dimension L3 between the boundary of the hot melting point 51 toward the side of the pole group 2 and the boundary of the overlapping area toward the side of the pole group 2 is greater than the maximum value of 0.5mm≤L3≤3mm, since the hot melting point 51 is far away from the lower edge of the overlapping area with the lower insulating portion 322, the insulating film 5 is located in the area between the hot melting point 51 and the lower edge of the overlapping area with the lower insulating portion 322, and is not tightly connected to the lower insulating portion 322, thereby weakening the strength of the insulating film 5 to wrap and converge the pole group 2, resulting in easy generation of gaps between the insulating film 5 and the pole group 2, which does not meet the use requirements.
[0129] Alternatively, if Figure 4 As shown, a shaping structure 326 corresponding to the through structure 325 is provided on the side of the lower insulating portion 322 facing the pole group 2. The shaping structure 326 is a trumpet-shaped structure whose opening gradually decreases in the direction away from the pole group 2. Thus, in step S1, the multiple converged pole ears 21 on the pole group 2 are better supported and fixed, the convergence state of the pole ears 21 is improved, and the problem of short circuit inside the battery due to poor convergence effect of the pole ears 21 is avoided.
[0130] Alternatively, if Figure 2 , Figure 4 , Fig. 9 As shown, in step S6, the following steps are also included:
[0131] S61, a mounting groove 324 is further provided on a side of the upper insulating portion 321 away from the cover body 31, and the battery further includes a connecting piece 7, and the connecting piece 7 is installed in the mounting groove 324;
[0132] S62, bending the portion of the electrode tab 21 extending out of the penetrating structure 325, and welding the bent electrode tab 21 to the connecting piece 7;
[0133] S63, the battery further includes a sealing ring 8, and the sealing ring 8 is installed in the receiving groove 311;
[0134] S64, the composite pole 4 is placed in the receiving groove 311, and the sealing ring 8 is sandwiched between the composite pole 4 and the composite cover plate 3;
[0135] S65, welding the composite pole 4 and the composite cover plate 3.
[0136] By providing the connecting piece 7 and welding the pole lug 21 to the connecting piece 7, the position of the pole lug 21 can be fixed in advance by using the connecting piece 7, thereby ensuring the accuracy of the position of the pole lug 21 during subsequent operations and avoiding the pole lug 21 from moving and affecting the conduction effect of the current between the pole lug 21 and the composite pole 4.
[0137] Among them, the electrode group 2 includes a positive electrode ear and a negative electrode ear located on the same side, so two connecting pieces 7, two sealing rings 8 and two composite poles 4 are correspondingly provided. When assembling the connecting piece 7, the sealing ring 8 and the composite pole 4, the positive electrode ear and the negative electrode ear can be assembled with the connecting piece 7, the sealing ring 8 and the composite pole 4 at the same time, or the connecting piece 7, the sealing ring 8 and the composite pole 4 on the positive electrode ear side can be assembled first, and after the assembly is completed, the connecting piece 7, the sealing ring 8 and the composite pole 4 on the negative electrode ear side can be assembled. In this embodiment, the simultaneous assembly method is adopted to reduce the time required for assembly and improve the efficiency of assembly.
[0138] Alternatively, if Figure 2 , Figure 4 As shown, in step S7, the following steps are also included:
[0139] S71, a connecting boss 71 is provided on one side of the connecting piece 7 facing the composite pole 4 and protrudes along the composite pole 4, and the composite pole 4 is pre-welded and positioned on the connecting boss 71 through a plurality of second pre-welding points arranged at intervals;
[0140] S72, fully welding the composite pole 4 and the connecting boss 71.
[0141] By providing a connecting boss 71 on the side of the connecting piece 7 facing the composite pole 4, it is convenient to weld the connecting piece 7 to the composite pole 4. The size and shape of the connecting boss 71 can be freely set according to demand, and it is sufficient to ensure that there is a sufficient welding area between the connecting boss 71 and the composite pole 4. In this embodiment, the connecting boss 71 is a truncated cone.
[0142] In addition, the composite pole 4 is first pre-welded to the connecting boss 71 through a plurality of second pre-welding points arranged at intervals, so as to ensure that the relative position between the composite pole 4 and the connecting boss 71 is preliminarily positioned before full welding, thereby ensuring the accuracy of the position of the two after welding during full welding, ensuring the welding quality, and even if the initial positioning is incorrect, it is convenient to separate and reposition the two, realize recycling, and reduce the scrap rate of the product.
[0143] Alternatively, if Figure 2 , Figure 4 As shown, in step S65, the following steps are also included:
[0144] S651, the composite pole 4 includes a pole body 41, a welding ring 42 and a second insulating layer 43 for achieving an insulating connection between the pole body 41 and the welding ring 42, and the welding ring 42 is pre-welded and positioned in the receiving groove 311 through a plurality of third pre-welding points arranged at intervals;
[0145] S652 , fully weld the welding ring 42 into the receiving groove 311 .
[0146] First, the welding ring 42 is pre-welded in the receiving groove 311 through a plurality of third pre-welding points arranged at intervals, so as to ensure that the relative position of the welding ring 42 in the receiving groove 311 is positioned before full welding. Even if the initial positioning is wrong, it is convenient to separate and reposition the two, realize recycling, and reduce the scrap rate of the product. The number, size and shape of the third pre-welding points used to realize the pre-welding of the welding ring 42 can be freely set according to actual needs.
[0147] Optionally, in step S62, after the connecting piece 7 is installed in the installation groove 324, the bent pole tab 21 is welded to the side of the connecting piece 7 facing the composite cover plate 3, or the bent pole tab 21 is welded to the side of the connecting piece 7 facing the composite pole 4. In order to adapt to various different working environments, it is convenient to perform welding operations on the bent pole tab 21 and the connecting piece 7. In this embodiment, the bent pole tab 21 is welded to the side of the connecting piece 7 facing the composite pole 4.
[0148] In this embodiment, if Figure 2 As shown, a battery is also provided, which is assembled by the above-mentioned battery assembly method. The battery is assembled by applying the above-mentioned battery assembly method, so that the volume of the electrode group 2 is further increased, thereby improving the energy density of the battery and increasing the power supply capacity of the battery.
[0149] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, various obvious changes, readjustments and substitutions can be made without departing from the protection scope of the present invention. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A battery assembly method, characterized in that: The battery assembled by the battery assembly method comprises a battery shell, an electrode group, a composite cover plate and a composite electrode column; The battery assembly method comprises the following steps: S1, the electrode group includes a first surface with an electrode ear, a second surface parallel to the first surface, and a plurality of side surfaces perpendicular to the first surface and the second surface, and an insulating film is coated on the plurality of side surfaces and the outer side of the second surface; S2, the composite cover plate is provided with a through structure for the pole lug to extend, the composite cover plate is arranged on the first surface of the pole group, and the pole lug is passed through the through structure; S3, a first insulating layer for isolating the composite cover plate and the electrode lug is injection-molded on the composite cover plate, and the overlapping area between the insulating film coated on the outside of the electrode group and the first insulating layer is hot-melted to form an electrode group unit; S4, the battery housing is a single-side open structure with a cavity, and the electrode group unit is installed in the cavity of the battery housing; S5, welding the composite cover plate to the battery housing; S6, a receiving groove is further provided on the side of the composite cover plate away from the electrode group, the composite pole is installed in the receiving groove, and the composite pole is welded to the composite cover plate; S7, achieving current conduction between the composite pole and the pole lug.
2. The battery assembly method according to claim 1, characterized in that: In step S1, the following steps are also included: S11, the battery further includes a bottom support plate, and the bottom support plate is pre-heat-fused at a set position of the insulating film; S12, covering the insulating film on the plurality of side surfaces and the second surface of the electrode group, and making the bottom support plate cover the second surface of the electrode group.
3. The battery assembly method according to claim 2, characterized in that: In step S2, the following steps are also included: S21, pre-installing the composite cover plate on the first surface, and passing the tab through the through structure; S22, measuring the distance L1 between the closest points of the composite cover plate and the insulating film, and determining whether L1 satisfies 0.5 mm ≤ L1 ≤ 3 mm, if yes, executing step S3, if no, executing step S23; S23, after removing the pre-installed composite cover plate, cutting the insulating film, after the cutting is completed, executing step S21.
4. The battery assembly method according to claim 1, characterized in that: A plurality of thermal melting points are arranged at intervals in the overlapping region between the insulating film and the first insulating layer, and the distance between the boundary of each thermal melting point away from the electrode group and the boundary of the overlapping region away from the electrode group is L2, and satisfies 0.5mm≤L2≤3mm; And / or, the distance between the boundary of each of the thermal melting points facing the electrode group and the boundary of the overlapping area facing the electrode group is L3, and satisfies 0.5mm≤L3≤3mm.
5. The battery assembly method according to claim 1, characterized in that: In step S5, the following steps are also included: S51, the composite cover plate and the battery housing are pre-welded and positioned at a plurality of first pre-welding points arranged at intervals; S52, fully welding the composite cover plate and the battery casing.
6. The battery assembly method according to claim 1, characterized in that: The composite cover plate comprises a cover plate body and the first insulating layer; The receiving groove is provided on the cover body, and the cover body is also provided with a plug-in through hole provided in the receiving groove; The first insulating layer is injection molded on the cover body, and includes an upper insulating portion, a lower insulating portion and a plug-in portion. The upper insulating portion is arranged on a side of the cover body away from the pole group and is located in the accommodating groove. The lower insulating portion is arranged on a side of the cover body facing the pole group and is located between the cover body and the pole group. The plug-in portion is inserted in the plug-in through hole and is used to connect the upper insulating portion and the lower insulating portion. The penetrating structure penetrates the upper insulating portion, the plug-in portion and the lower insulating portion.
7. The battery assembly method according to claim 6, characterized in that: In step S6, the following steps are also included: S61, a mounting groove is further provided on a side of the upper insulating portion away from the cover body, and the battery further comprises a connecting piece, and the connecting piece is installed in the mounting groove; S62, bending the portion of the electrode tab extending out of the through structure, and welding the bent electrode tab to the connecting sheet; S63, the battery further includes a sealing ring, and the sealing ring is installed in the receiving groove; S64, placing the composite pole into the receiving groove, wherein the sealing ring is sandwiched between the composite pole and the composite cover plate; S65, welding the composite pole and the composite cover plate.
8. The battery assembly method according to claim 7, characterized in that: In step S7, the following steps are also included: S71, a connection boss protruding along the side of the connection piece facing the composite pole is provided, and the composite pole is pre-welded and positioned on the connection boss through a plurality of second pre-welding points arranged at intervals; S72, fully welding the composite pole and the connecting boss.
9. The battery assembly method according to claim 7, characterized in that: In step S65, the following steps are also included: S651, the composite pole comprises a pole body, a welding ring and a second insulating layer for realizing an insulating connection between the pole body and the welding ring, the welding ring being pre-welded and positioned in the receiving groove through a plurality of third pre-welding points arranged at intervals; S652, fully weld the welding ring in the receiving groove.
10. A battery, characterized in that The battery is assembled using the battery assembly method according to any one of claims 1 to 9.
Citation Information
Patent Citations
Cover plate assembly and battery
CN220672709U