A closed-loop forging longitudinal burr suppression and transfer device and process for steel piston skirts
By setting an annular transverse scrap bin on the outside of the final forging die, the longitudinal burrs are transferred by utilizing plastic flow characteristics, thus solving the problem of burr folding defects in closed forging and achieving efficient production and cost savings.
Patent Information
- Application Number
- CN202611331661.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-31
- Publication Date
- 2026-11-10
AI Technical Summary
In existing closed forging processes, longitudinal burrs cannot be completely avoided, leading to folding defects in the forging matrix. Existing solutions have low material utilization, high mold costs, or unstable production, and subsequent grinding processes increase equipment investment and labor costs.
An annular transverse scrap bin is set on the outside of the final forging die. By utilizing the plastic flow characteristics of the metal during the final forging die extrusion, the longitudinal burrs are redirected and enter the scrap bin. The burrs are then removed through the trimming process to avoid folding defects.
Completely eliminate burr and fold defects, maintain high material utilization, reduce mold and equipment costs, improve production stability, eliminate grinding processes, and shorten production cycle time.
Smart Images

Figure CN123060031A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of hot die forging and precision forging technology, and in particular to a device and process for suppressing and transferring longitudinal burrs in closed-type forging of steel piston skirts. Background Technology
[0002] Steel piston skirts are manufactured using a closed-die hot forging process. Compared to traditional open forging, this process offers significant advantages, including higher material utilization, higher dimensional accuracy of forgings, and lower raw material consumption. It has become the mainstream manufacturing route for large-diameter steel pistons. However, closed forging has inherent defects: during the closed-die forging process at the pre-forging station, high-temperature metal is squeezed outwards along the gap between the upper and lower dies, forming longitudinal burrs perpendicular to the parting surface. These longitudinal burrs cannot be completely avoided. When the pre-forged billet is transferred to the final forging station for closed-die final forging, these longitudinal burrs are pressed into the forging matrix by the upper and lower dies, forming forging fold defects. Folding is a serious fatigue-risk defect, and oxidation and decarburization occur at the fold, making it prone to fatigue cracks during service. Piston skirt forgings are not allowed to have such defects.
[0003] Both of the existing mainstream solutions in the industry have significant shortcomings. Solution one involves designing a trapezoidal material chamber on the forging body at the corresponding die-closing positions of pre-forging and final forging to contain the longitudinal burrs generated during pre-forging. The material chamber is then removed by subsequent machining. However, this requires leaving a large machining allowance on the piston skirt body, reducing material utilization and increasing machining time and tool wear. Solution two involves significantly improving the machining accuracy of the die and strictly controlling the die-closing gap to minimize the longitudinal burrs generated during pre-forging. However, this increases the die manufacturing cost exponentially and places extremely high demands on the guide accuracy of the hot die forging press slide and the rigidity of the equipment. Die wear and thermal expansion during production will cause changes in the die-closing gap, resulting in poor stability in mass production. To eliminate folding defects, existing processes generally add a manual grinding or robotic automatic grinding process after forging, requiring a large investment of manpower or expensive automated grinding machines, resulting in large equipment investment and a longer production cycle.
[0004] Therefore, it is necessary to provide a steel piston skirt closed-type forging longitudinal burr suppression and transfer treatment device to solve the above-mentioned technical problems. Summary of the Invention
[0005] This invention provides a device for suppressing and transferring longitudinal burrs in closed-loop forging of steel piston skirts. It solves the problems of longitudinal burrs generated during pre-forging being pressed into the forging matrix during final forging, forming folding defects; material silo solutions sacrificing material utilization; high-precision mold solutions being costly and having unstable mass production; and subsequent grinding processes increasing equipment investment and cycle time, with the risk of over-grinding.
[0006] To solve the above-mentioned technical problems, the present invention provides a closed-type forging longitudinal burr suppression and transfer treatment device for steel piston skirts, comprising:
[0007] Forging upper die, hot billet, forging lower die, pre-forging upper die, pre-forging lower die ring, pre-forging part, pre-forging lower die core, pre-lower backing plate, final forging upper die, final forging part, final forging lower die ring, final forging lower die core and final lower backing plate;
[0008] The upper forging die and the lower forging die are arranged opposite to each other. The hot billet is placed on the lower forging die, and the upper forging die is used to forge the hot billet.
[0009] The pre-forging upper die is disposed opposite to the pre-forging lower die ring and the pre-forging lower die core. The pre-forging lower die core is disposed on the pre-forging lower pad. The pre-forging upper die cooperates with the pre-forging lower die ring and the pre-forging lower die core to forge the forged billet into a pre-forged part. The sidewall of the pre-forged part has longitudinal burrs.
[0010] The upper forging die, the lower forging die ring, and the lower forging die core are arranged opposite to each other. The lower forging die core is disposed on the lower forging pad. A forging cavity is formed between the upper forging die, the lower forging die ring, and the lower forging die core. An annular transverse scrap bin is provided in the forging cavity. The annular transverse scrap bin is used to accommodate the longitudinal burrs. The upper forging die, the lower forging die ring, and the lower forging die core cooperate to forge the pre-forging part with longitudinal burrs into the forging part in the forging cavity and squeeze the longitudinal burrs into the annular transverse scrap bin.
[0011] Preferably, the width of the annular transverse waste bin is 10mm and the height is 4mm.
[0012] Preferably, the longitudinal burrs are distributed on the outer wall of the pre-forged part forged by the cooperation of the pre-forging upper die, the pre-forging lower die ring, and the pre-forging lower die core.
[0013] Preferably, a trapezoidal material chamber is provided on the side of the final forging upper die facing the final forging lower die ring, and the trapezoidal material chamber is connected to the final forging cavity.
[0014] Preferably, the final forging is trimmed to form a trimmed finished forging, and the longitudinal burrs are completely squeezed into the annular transverse scrap bin during the final forging process, so that no longitudinal burrs remain on the trimmed finished forging.
[0015] Preferably, the interior of the final forging die is provided with a disassembly assembly, which includes a disassembly ring, multiple disassembly blocks, multiple disassembly grooves and multiple bolts. The disassembly ring is disposed inside the final forging die, the multiple disassembly blocks are respectively connected to the surface of the disassembly ring, and the multiple disassembly grooves are respectively opened inside the final forging die.
[0016] Preferably, the plurality of bolts are respectively disposed between the plurality of disassembly blocks and the final forging die.
[0017] This invention also proposes a processing technology for the closed-type forging longitudinal burr suppression and transfer device for steel piston skirts, the steps of which are as follows:
[0018] First, the steel billet is heated to the forging process temperature to obtain a hot billet. The hot billet is placed on the lower upsetting die, and the upper upsetting die moves downward to upset the hot billet, causing the billet to be compressed in the height direction and expanded in the diameter direction.
[0019] After upsetting, the billet is transferred to the pre-forging station and placed on the lower pre-forging die core. The upper pre-forging die moves downward and closes with the lower pre-forging die ring and the lower pre-forging die core to forge the billet into a pre-forged part. Due to the influence of the closed forging die closing gap, a longitudinal burr perpendicular to the parting surface is generated at the die closing position of the upper and lower dies of the pre-forged part. This longitudinal burr is located at the corresponding position on the outer circle of the piston skirt.
[0020] The pre-forging part with longitudinal burrs is transferred to the final forging station and placed on the lower die core of the final forging. The upper die of the final forging moves downward and closes with the lower die ring and the lower die core of the final forging. The final forging die is equipped with an annular transverse scrap bin at the location of the longitudinal burr of the pre-forging part. When the final forging die is closed and squeezed, the longitudinal burrs on the pre-forging part are squeezed by the upper die of the final forging die, and the metal undergoes plastic flow. The longitudinal burrs that were originally perpendicular to the parting surface are forced to change their flow direction and flow radially into the outer annular transverse scrap bin, turning into transverse flash parallel to the parting surface. The piston skirt product body does not receive the burr metal. All the burrs enter the outer scrap bin and will not be pressed into the forging base to cause folding.
[0021] After the final forging is completed, the hot forging with the flash from the transverse scrap bin is transferred to the existing trimming press. The entire annular transverse scrap bin, including the burrs, is removed along with the flash through the trimming die. The scrap is discharged as forging flash waste. The trimmed steel piston skirt forging is directly transferred to the subsequent heat treatment process, without the need for a grinding process to remove burrs and folding defects.
[0022] Compared with related technologies, the steel piston skirt closed forging longitudinal burr suppression and transfer treatment device provided by the present invention has the following beneficial effects:
[0023] This invention provides a closed-loop forging longitudinal burr suppression and transfer device for steel piston skirts. By setting an independent annular transverse scrap bin outside the finished product contour of the final forging die, and utilizing the plastic flow characteristics of metal during final forging die closing and extrusion, the longitudinal burrs generated during pre-forging are forced to change their flow direction, from perpendicular to the parting surface to flowing radially outward along the parting surface. All burrs enter the annular transverse scrap bin and are transformed into ordinary transverse flash, completely isolating the burr metal from the piston skirt finished product body. This completely prevents burrs from being pressed into the base and forming folds, eliminating the fatigue risk of folds at the source. There is no need to reserve a material bin on the forging body, maintaining a high level of material utilization. It eliminates the need for extreme die closing clearance control, reducing die manufacturing costs and equipment precision requirements, and ensuring high stability in mass production. The burr-bearing flash in the scrap bin can be removed through the existing hot-cutting process, eliminating the need for a subsequent specialized grinding process, saving investment in grinding equipment and labor costs, shortening the production cycle, and eliminating the risk of over-grinding. Attached Figure Description
[0024] Figure 1 A schematic diagram of the structure of a first embodiment of a closed-type forging longitudinal burr suppression and transfer treatment device for steel piston skirts provided by the present invention;
[0025] Figure 2 A schematic diagram of the structure of a steel piston skirt pre-forging;
[0026] Figure 3 for Figure 2 The enlarged schematic diagram of part A shown below;
[0027] Figure 4 This is a schematic diagram of the structure of a longitudinal burr;
[0028] Figure 5 This is a cross-sectional view of the final forging die;
[0029] Figure 6 for Figure 5 The enlarged schematic diagram of section B is shown below;
[0030] Figure 7 for Figure 6 The diagram shows the internal structure of the annular transverse waste bin.
[0031] Figure 8 A schematic diagram showing the structure in which longitudinal burrs are squeezed into the transverse scrap bin during the forming of the pre-forged part in the final forging cavity;
[0032] Figure 9 for Figure 8 The enlarged schematic diagram of section C is shown below;
[0033] Figure 10 This is a schematic diagram of the structure of the finished forging after trimming.
[0034] Figure 11This is a schematic diagram of the second embodiment of a closed-type forging longitudinal burr suppression and transfer treatment device for steel piston skirts provided by the present invention.
[0035] The diagram labels are as follows: 1. Upsetting upper die, 2. Hot billet, 3. Upsetting lower die, 4. Pre-forging upper die, 5. Pre-forging lower die ring, 6. Pre-forging part, 7. Pre-forging lower die core, 8. Pre-forging lower backing plate, 9. Longitudinal burr, 10. Final forging upper die, 11. Trapezoidal material bin, 12. Final forging part, 13. Final forging lower die ring, 14. Final forging lower die core, 15. Final lower backing plate, 16. Annular transverse scrap bin.
[0036] 17. Disassembly components, 171. Disassembly ring, 172. Disassembly block, 173. Disassembly groove, 174. Bolt. Detailed Implementation
[0037] The present invention will be further described below with reference to the accompanying drawings and embodiments.
[0038] First Embodiment
[0039] Please refer to the following: Figure 1 , Figure 2 , Figure 3 , Figure 4 and Figure 5 ,in, Figure 1 A schematic diagram of the structure of a first embodiment of a closed-type forging longitudinal burr suppression and transfer treatment device for steel piston skirts provided by the present invention; Figure 2 A schematic diagram of the structure of a steel piston skirt pre-forging; Figure 3 for Figure 2 The enlarged schematic diagram of part A shown below; Figure 4 This is a schematic diagram of the structure of a longitudinal burr; Figure 5 This is a cross-sectional view of the final forging die; Figure 6 for Figure 5 The enlarged schematic diagram of section B is shown below; Figure 7 for Figure 6 The diagram shows the internal structure of the annular transverse waste bin. Figure 8 A schematic diagram showing the structure in which longitudinal burrs are squeezed into the transverse scrap bin during the forming of the pre-forged part in the final forging cavity; Figure 9 for Figure 8 The enlarged schematic diagram of section C is shown below; Figure 10 This is a schematic diagram of the structure of the finished forging after edge trimming. A closed-loop forging longitudinal burr suppression and transfer device for a steel piston skirt includes:
[0040] 1. Forging upper die, 2. Hot billet, 3. Forging lower die, 4. Pre-forging upper die, 5. Pre-forging lower die ring, 6. Pre-forging part, 7. Pre-forging lower die core, 8. Pre-forging lower pad, 10. Final forging upper die, 12. Final forging part, 13. Final forging lower die ring, 14. Final forging lower die core and 15.
[0041] The upper forging die 1 and the lower forging die 3 are arranged opposite to each other. The hot billet 2 is placed on the lower forging die 3. The upper forging die 1 is used to forge the hot billet 2.
[0042] The pre-forging upper die 4 is disposed opposite to the pre-forging lower die ring 5 and the pre-forging lower die core 7. The pre-forging lower die core 7 is disposed on the pre-forging lower pad plate 8. The pre-forging upper die 4 cooperates with the pre-forging lower die ring 5 and the pre-forging lower die core 7 to forge the forged billet into a pre-forged part 6. The sidewall of the pre-forged part 6 is formed with longitudinal burrs 9.
[0043] The upper forging die 10, the lower forging die ring 13, and the lower forging die core 14 are arranged opposite to each other. The lower forging die core 14 is disposed on the lower forging pad 15. A forging cavity is formed between the upper forging die 10, the lower forging die ring 13, and the lower forging die core 14. An annular transverse scrap bin 16 is provided in the forging cavity. The annular transverse scrap bin 16 is used to accommodate the longitudinal burrs 9. The upper forging die 10 cooperates with the lower forging die ring 13 and the lower forging die core 14 to forge the pre-forging part 6 with longitudinal burrs 9 into the forging part 12 in the forging cavity, and to squeeze the longitudinal burrs 9 into the annular transverse scrap bin 16.
[0044] Upsetting upper die 1 is an upper die with a flat downward pressing surface, and upsetting lower die 3 is a lower die with a positioning groove. The hot billet 2 is placed in the positioning groove of the upsetting lower die 3. The upsetting upper die 1 moves downward under the drive of the press, applying pressure to the hot billet 2 to cause it to undergo upsetting deformation, thereby obtaining a flat upsetting billet.
[0045] The upsetting die 1 is used to upset the hot billet 2, compressing the billet in the height direction and expanding it in the diameter direction, so as to provide a billet with a suitable volume and shape for subsequent pre-forging.
[0046] The annular transverse waste bin 16 has a width of 10mm and a height of 4mm.
[0047] The bin width of 10mm and the bin height of 4mm are matched and designed to ensure that burrs can be completely guided into the bin while minimizing the amount of extra material consumed.
[0048] The longitudinal burrs 9 are distributed on the outer wall of the pre-forged part 6 forged by the pre-forging upper die 4, the pre-forging lower die ring 5, and the pre-forging lower die core 7.
[0049] The longitudinal burrs 9 are distributed circumferentially along the side wall of the pre-forging part 6. When the pre-forging part 6 is transferred to the final forging station, the longitudinal burrs 9 enter the final forging cavity together with the pre-forging part 6.
[0050] The upper forging die 10 is provided with a trapezoidal material chamber 11 on the side facing the lower forging die ring 13, and the trapezoidal material chamber 11 is connected to the forging cavity.
[0051] The final forging 12 is trimmed to form a trimmed finished forging. The longitudinal burrs 9 are completely squeezed into the annular transverse scrap bin 16 during the final forging process so that no longitudinal burrs remain on the trimmed finished forging.
[0052] After the final forging is completed, the hot forging with the flash of the transverse scrap bin is transferred to the existing trimming press. The entire annular transverse scrap bin 16 containing burrs is cut off along with the flash by the trimming die. The scrap is discharged as forging flash scrap. The steel piston skirt forging with trimmed edges is directly transferred to the subsequent heat treatment process, and no grinding process is needed to remove burrs and folding defects.
[0053] The processing steps of the closed-type forging longitudinal burr suppression and transfer device for steel piston skirts provided by this invention are as follows:
[0054] First, the steel billet is heated to the forging process temperature to obtain hot billet 2. The hot billet 2 is placed on the upsetting lower die 3. The upsetting upper die 1 moves downward to upset the hot billet 2, so that the billet is compressed in the height direction and expanded in the diameter direction.
[0055] After upsetting, the billet is transferred to the pre-forging station and placed on the pre-forging lower die core 7. The pre-forging upper die 4 moves downward and closes with the pre-forging lower die ring 5 and the pre-forging lower die core 7 to forge the billet into a pre-forged part 6. Due to the influence of the closed forging die closing gap, a longitudinal burr 9 perpendicular to the parting surface is generated at the die closing position of the upper and lower dies of the pre-forged part 6. The longitudinal burr 9 is located at the corresponding position on the outer circle of the piston skirt.
[0056] The pre-forged part 6 with longitudinal burrs 9 is transferred to the final forging station and placed on the final forging lower die core 14. The final forging upper die 10 moves downward and closes with the final forging lower die ring 13 and the final forging lower die core 14. The final forging die is provided with an annular transverse scrap bin 16 at the location of the longitudinal burrs 9 of the pre-forged part 6. When the final forging die is closed and squeezed, the longitudinal burrs 9 on the pre-forged part 6 are squeezed by the final forging upper die 10, and the metal undergoes plastic flow. The longitudinal burrs 9, which were originally perpendicular to the parting surface, are forced to change their flow direction and flow radially into the outer annular transverse scrap bin 16, turning into transverse flash parallel to the parting surface. The piston skirt product body does not receive the burr metal. All the burrs enter the outer scrap bin 16 and will not be pressed into the forging base to cause folding.
[0057] After the final forging is completed, the hot forging with the flash from the transverse scrap bin is transferred to the existing trimming press. The entire annular transverse scrap bin 16, including the flash, is cut off by the trimming die. The scrap is discharged as forging flash waste. The trimmed steel piston skirt forging is directly transferred to the subsequent heat treatment process, and no grinding process is needed to remove burrs and folding defects.
[0058] Compared with related technologies, the steel piston skirt closed forging longitudinal burr suppression and transfer treatment device provided by the present invention has the following beneficial effects:
[0059] This invention provides a closed-loop forging longitudinal burr suppression and transfer device for steel piston skirts. By setting an independent annular transverse scrap bin 16 outside the finished product contour of the final forging die, the device utilizes the plastic flow characteristics of metal during final forging die closing and extrusion to force the longitudinal burrs 9 generated during pre-forging to change their flow direction, from perpendicular to the parting surface to flowing radially outward along the parting surface. All burrs enter the annular transverse scrap bin 16 and are transformed into ordinary transverse flash, completely isolating the burr metal from the piston skirt finished product body. This completely prevents burrs from being pressed into the base and forming folds, eliminating the fatigue risk of folds at the source. It eliminates the need for a pre-reserved material bin on the forging body, maintaining a high level of material utilization. It also eliminates the need for extreme die closing clearance control, reducing die manufacturing costs and equipment precision requirements, resulting in high stability in mass production. The burr-bearing flash can be removed through the existing hot-cutting process, saving on subsequent specialized grinding processes, reducing grinding equipment investment and labor costs, shortening the production cycle, and eliminating the risk of over-grinding.
[0060] Second Embodiment
[0061] Please refer to the following: Figure 11 Based on the first embodiment of this application, which provides a device for suppressing and transferring longitudinal burrs in closed-loop forging of steel piston skirts, the second embodiment of this application proposes another device for suppressing and transferring longitudinal burrs in closed-loop forging of steel piston skirts. The second embodiment is merely a preferred embodiment of the first embodiment, and the implementation of the second embodiment will not affect the separate implementation of the first embodiment.
[0062] Specifically, the second embodiment of this application provides a steel piston skirt closed forging longitudinal burr suppression and transfer treatment device, which differs in that it also includes a disassembly assembly 17. The disassembly assembly 17 is disposed inside the final forging upper die 10. The disassembly assembly 17 includes a disassembly ring 171, a plurality of disassembly blocks 172, a plurality of disassembly grooves 173 and a plurality of bolts 174. The disassembly ring 171 is disposed inside the final forging upper die 10. The plurality of disassembly blocks 172 are respectively connected to the surface of the disassembly ring 171. The plurality of disassembly grooves 173 are respectively opened inside the final forging upper die 10.
[0063] The plurality of bolts 174 are respectively disposed between the plurality of disassembly blocks 172 and the final forging upper die 10.
[0064] The disassembly groove 173 is a groove structure adapted to the disassembly block 172. The bolt 174 passes through the side wall of the final forging upper die 10 and connects to the threaded hole on the disassembly block 172 to fix the disassembly ring 171 inside the final forging upper die 10. The disassembly ring 171 is an annular structure, and its inner wall forms the wall of the annular transverse waste bin 16.
[0065] The working principle of the closed-type forging longitudinal burr suppression and transfer device for steel piston skirt provided by the present invention is as follows:
[0066] When using the disassembly ring 171, first install the disassembly ring 171 with multiple disassembly blocks 172 inside the final forging die 10. At the same time, the multiple disassembly blocks 172 are installed inside the multiple disassembly slots 173 opened inside the final forging die 10. After the disassembly ring 171 is installed, multiple bolts 174 are used to pass through the multiple disassembly blocks 172 and be threaded to the final forging die 10.
[0067] Compared with related technologies, the steel piston skirt closed forging longitudinal burr suppression and transfer treatment device provided by the present invention has the following beneficial effects:
[0068] This invention provides a steel piston skirt closed forging longitudinal burr suppression and transfer treatment device. By setting a disassembly assembly 17 inside the final forging die 10, and utilizing the cooperation of disassembly ring 171, disassembly block 172, disassembly groove 173 and bolt 174, the annular transverse scrap bin 16 area can be disassembled and replaced. This facilitates the replacement of the disassembly ring 171 when the annular transverse scrap bin 16 is worn or deformed after long-term use, without having to replace the entire final forging die 10, thus reducing the die maintenance cost.
[0069] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural or procedural transformations made based on the content of the present invention specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.
Claims
1. A closed-type forging longitudinal burr suppression and transfer treatment device for steel piston skirts, characterized in that, include: Forging upper die, hot billet, forging lower die, pre-forging upper die, pre-forging lower die ring, pre-forging part, pre-forging lower die core, pre-lower backing plate, final forging upper die, final forging part, final forging lower die ring, final forging lower die core and final lower backing plate; The upper forging die and the lower forging die are arranged opposite to each other. The hot billet is placed on the lower forging die, and the upper forging die is used to forge the hot billet. The pre-forging upper die is disposed opposite to the pre-forging lower die ring and the pre-forging lower die core. The pre-forging lower die core is disposed on the pre-forging lower pad. The pre-forging upper die cooperates with the pre-forging lower die ring and the pre-forging lower die core to forge the forged billet into a pre-forged part. The sidewall of the pre-forged part has longitudinal burrs. The upper forging die, the lower forging die ring, and the lower forging die core are arranged opposite to each other. The lower forging die core is disposed on the lower forging pad. A forging cavity is formed between the upper forging die, the lower forging die ring, and the lower forging die core. An annular transverse scrap bin is provided in the forging cavity. The annular transverse scrap bin is used to accommodate the longitudinal burrs. The upper forging die, the lower forging die ring, and the lower forging die core cooperate to forge the pre-forging part with longitudinal burrs into the forging part in the forging cavity and squeeze the longitudinal burrs into the annular transverse scrap bin.
2. The closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 1, characterized in that, The annular transverse waste bin has a width of 10mm and a height of 4mm.
3. The closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 1, characterized in that, The longitudinal burrs are distributed on the outer wall of the pre-forged part forged by the cooperation of the pre-forging upper die, the pre-forging lower die ring, and the pre-forging lower die core.
4. The closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 1, characterized in that, A trapezoidal material chamber is provided on the side of the final forging upper die facing the final forging lower die ring, and the trapezoidal material chamber is connected to the final forging cavity.
5. The closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 1, characterized in that, The final forging is trimmed to form a trimmed finished forging. The longitudinal burrs are completely squeezed into the annular transverse scrap bin during the final forging process so that no longitudinal burrs remain on the trimmed finished forging.
6. The closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 1, characterized in that, The upper die for final forging is provided with a disassembly assembly, which includes a disassembly ring, multiple disassembly blocks, multiple disassembly grooves, and multiple bolts. The disassembly ring is located inside the upper die for final forging, the multiple disassembly blocks are respectively connected to the surface of the disassembly ring, and the multiple disassembly grooves are respectively opened inside the upper die for final forging.
7. The closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 6, characterized in that, The bolts are respectively disposed between the disassembly blocks and the final forging die.
8. The processing technology of the closed-type forging longitudinal burr suppression and transfer device for steel piston skirts according to claim 1, characterized in that, The steps are as follows: First, the steel billet is heated to the forging process temperature to obtain a hot billet. The hot billet is placed on the lower upsetting die, and the upper upsetting die moves downward to upset the hot billet, causing the billet to be compressed in the height direction and expanded in the diameter direction. After upsetting, the billet is transferred to the pre-forging station and placed on the lower pre-forging die core. The upper pre-forging die moves downward and closes with the lower pre-forging die ring and the lower pre-forging die core to forge the billet into a pre-forged part. Due to the influence of the closed forging die closing gap, a longitudinal burr perpendicular to the parting surface is generated at the die closing position of the upper and lower dies of the pre-forged part. This longitudinal burr is located at the corresponding position on the outer circle of the piston skirt. The pre-forging part with longitudinal burrs is transferred to the final forging station and placed on the lower die core of the final forging. The upper die of the final forging moves downward and closes with the lower die ring and the lower die core of the final forging. The final forging die is equipped with an annular transverse scrap bin at the location of the longitudinal burr of the pre-forging part. When the final forging die is closed and squeezed, the longitudinal burrs on the pre-forging part are squeezed by the upper die of the final forging die, and the metal undergoes plastic flow. The longitudinal burrs that were originally perpendicular to the parting surface are forced to change their flow direction and flow radially into the outer annular transverse scrap bin, turning into transverse flash parallel to the parting surface. The piston skirt product body does not receive the burr metal. All the burrs enter the outer scrap bin and will not be pressed into the forging base to cause folding. After the final forging is completed, the hot forging with the flash from the transverse scrap bin is transferred to the existing trimming press. The entire annular transverse scrap bin, including the burrs, is removed along with the flash through the trimming die. The scrap is discharged as forging flash waste. The trimmed steel piston skirt forging is directly transferred to the subsequent heat treatment process, without the need for a grinding process to remove burrs and folding defects.