A method for evaluating the high-temperature erosion capacity of autogenous acid systems and its application.
By simulating the acid-generating behavior of autogenous acid in reservoirs using a hydrothermal reactor and adjusting the mass transfer rate with an interface promoter, the problem of evaluating the high-temperature erosion capacity of autogenous acid systems was solved, enabling the assessment of the erosion performance and deep etching effect of autogenous acid under high-temperature conditions.
Patent Information
- Application Number
- CN202510579658.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-07
- Publication Date
- 2026-11-10
AI Technical Summary
Existing technologies cannot effectively evaluate the erosion capacity of autogenous acid systems under high-temperature conditions, especially in the range of 90–200°C, where there is a lack of methods for evaluating erosion performance.
A hydrothermal reactor was used to simulate the slow acid generation behavior of autogenous acid in the reservoir. The acid generation conversion rate was calculated by weighing the mass reduction of solid carbonate. The mass transfer rate was adjusted by combining an interface promoter, and the high-temperature dissolution capability of the autogenous acid system was evaluated.
It enables accurate evaluation of the dissolution capacity of autogenous acid systems under high-temperature conditions, provides assessment of the deep etching capacity of autogenous acid in reservoirs, and avoids the strong dissolution of wellbore by traditional acid solutions.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of oil and gas field development, specifically relating to an evaluation method and application of the high-temperature dissolution capacity of an autogenous acid system. Background Technology
[0002] Acidizing is one of the key technologies for enhancing oil and gas well production. It increases production by using acid to dissolve acid-soluble minerals, resulting in an acid-rock reaction that forms oil and gas channels. Therefore, the acid-rock reaction dissolution rate is an important indicator for evaluating acid performance.
[0003] In related technologies, such as Q / SHCG 126-2017 "Technical Requirements for Slow-Generating Acids," the determination of dissolution capacity involves measuring the mass change of calcium carbonate particles before and after the reaction in a stoppered plastic container by observing the acid-rock reaction between calcium carbonate particles and the medium, followed by a series of calculations. However, this method is only applicable to lower temperature ranges (typically ≤90℃) and is no longer suitable for evaluating high-temperature dissolution capacity. Therefore, this invention designs an evaluation method for assessing the dissolution capacity of autogenous acid systems under high-temperature conditions (90–200℃), simulating the slow acid generation behavior of autogenous acids in reservoirs and examining its acid generation kinetics. Summary of the Invention
[0004] This invention provides a method for evaluating the high-temperature dissolution capacity of autogenous acid systems, which can evaluate the dissolution capacity of autogenous acids on carbonates in the temperature range of 90 to 200°C.
[0005] One of the objectives of this invention is to provide a method for evaluating the high-temperature erosion capability of an autogenous acid system, which includes the step of heating and reacting components including an autogenous acid system, solid carbonate, and an interface promoter in a hydrothermal reactor, and then evaluating the erosion capability of the autogenous acid system by weighing the amount of mass reduction of the solid carbonate.
[0006] According to the present invention, the method for evaluating the high-temperature dissolution capacity of the self-generating acid system specifically includes the following steps:
[0007] (a) Add solid carbonate, autogenous acid system and interface promoter to a hydrothermal reactor, seal and heat;
[0008] (b) After heating the reaction, the temperature is lowered to room temperature, and the acid conversion rate is calculated from the weight loss of the solid carbonate.
[0009] The evaluation method of this invention is applicable to existing authigenic acid products. Under the high temperature of the reservoir, authigenic acid gradually transforms into free acid, thereby dissolving carbonate reservoirs. The evaluation method used in this invention calculates the amount of free acid (e.g., HCl, HF, organic acids, etc.) generated by calculating the weight loss (dissolution amount) of solid carbonate, and then calculates the acid conversion rate (i.e., the percentage concentration of the authigenic acid mass converted into free acid relative to the initial authigenic acid mass).
[0010] According to an embodiment of the present invention, the hydrothermal reactor can be a commonly used hydrothermal reactor in the prior art, and preferably, the hydrothermal reactor is a hydrothermal reactor with a polytetrafluoroethylene liner.
[0011] According to an embodiment of the present invention, the autogenous acid system comprises solid autogenous acid and water (preferably distilled water), wherein the solid autogenous acid is a commercially available autogenous acid product. The amount of water in the autogenous acid system can be adjusted within a wide range to ensure sufficient hydrolysis of the autogenous acid. Preferably, the mass ratio of solid autogenous acid to water in the autogenous acid system is 1:(2.5~10), for example, any ratio value among 1:2.5, 1:3, 1:3.5, 1:4, 1:4.5, 1:5, 1:5.5, 1:6, 1:6.5, 1:7, 1:7.5, 1:8, 1:8.5, 1:9, 1:9.5, and 1:10, or a ratio value within a range of any two of the above values.
[0012] Carbonate reservoirs are mainly composed of two types of carbonate minerals: calcite (CaCO3) and dolomite (CaMg(CO3)2). To better simulate formation conditions, according to embodiments of the present invention, the solid carbonate can be a commonly used carbonate product in the prior art. Preferably, the solid carbonate is selected from at least one of calcium carbonate, calcite, magnesite, and dolomite.
[0013] According to an embodiment of the present invention, the interface promoter is selected from at least one of C1-C6 haloalkanes and C6-C10 aromatics, preferably from at least one of dichloromethane, trichloromethane, carbon tetrachloride, and m-xylene. Autogenous acid is a water-insoluble solid, and the hydrolysis reaction occurs at the interface between the autogenous acid solid and water, which is relatively slow. The presence of the interface promoter can adjust the mass transfer rate and regulate the acid generation rate to the desired level.
[0014] According to an embodiment of the present invention, the mass ratio of the self-generating acid system to the solid carbonate is (1.5 to 5):1, for example, it can be any mass ratio among 1.5:1, 2:1, 2.5:1, 3:1, 3.5:1, 4:1, 4.5:1, 5:1 or any mass ratio within the range of any two of the above mass ratios; the mass ratio of the self-generating acid system to the interface promoter is (28 to 100):1, for example, it can be any mass ratio among 28:1, 30:1, 35:1, 40:1, 45:1, 50:1, 55:1, 60:1, 65:1, 70:1, 75:1, 80:1, 85:1, 90:1, 100:1 or any mass ratio within the range of any two of the above mass ratios. Preferably, the mass ratio of the self-generating acid system to the solid carbonate is (2.3-3.5):1, and the mass ratio of the self-generating acid system to the interface promoter is (32-85):1.
[0015] According to an embodiment of the present invention, the temperature of the heating reaction is 90 to 200°C, for example, it can be any temperature value of 90, 95, 100, 105, 110, 115, 120, 125, 130, 135, 140, 145, 150, 155, 160, 165, 170, 175, 180, 185, 190, 195, 200°C or a temperature value within a range of any two of the above values; the heating reaction time is 1 to 8 hours, for example, it can be any time value of 1, 1.5, 2, 2.5, 3, 3.5, 4, 4.5, 5, 5.5, 6, 6.5, 7, 7.5, 8 hours or a time value within a range of any two of the above values.
[0016] According to an embodiment of the present invention, step (b) further includes filtering, washing, and drying after cooling to room temperature, wherein the room temperature is 20±5℃, washing is performed multiple times using a commonly used washing solvent (e.g., distilled water), and drying is performed at 105~120℃ for 1~6h.
[0017] According to an embodiment of the present invention, multiple samples can be set at the same temperature and taken out after different heating times, such as heating for 1 hour, 2 hours, 3 hours, 4 hours, 5 hours, 6 hours, 7 hours, and 8 hours respectively. After filtration, washing with distilled water multiple times, and drying, the mass of the remaining solid carbonate is weighed, thereby calculating the amount of solid carbonate dissolved, acid concentration, acid conversion rate, etc. at different times, and thus evaluating the dissolution performance of solid self-generated acid.
[0018] The second objective of this invention is to provide the above-mentioned evaluation method for evaluating the dissolution capacity of autogenous acid systems at different temperatures.
[0019] Traditional hydrochloric acid or terrestrial acid lacks the ability to delay etching, causing strong dissolution in the wellbore and near-wellbore area, making it difficult to achieve effective long-distance etching. In contrast, autogenous acid is neutral or weakly acidic under normal conditions. After being pumped into the reservoir, it slowly generates hydrochloric acid in situ under the high temperature of the reservoir, achieving deep etching. This invention simulates the slow acid generation behavior of autogenous acid in the reservoir using a hydrothermal reactor to investigate its acid generation kinetics. Detailed Implementation
[0020] This invention provides a method for evaluating the high-temperature dissolution capacity of an autogenous acid system. The steps are as follows: Accurately weigh solid carbonate and use multiple hydrothermal reactors with identical polytetrafluoroethylene (PTFE) liners. At t=0, accurately weighed solid carbonate, the autogenous acid system, and an interface promoter are added to each reactor. The PTFE-lined hydrothermal reactor is immediately sealed and placed in a constant-temperature oven at the desired temperature. At set time points, the PTFE-lined hydrothermal reactors are removed and cooled to room temperature. After venting, the reactors are opened, and the remaining solid carbonate mass at different time points is weighed. The dissolution amount of solid carbonate, as well as the acid concentration and acid conversion rate, are calculated according to the formula at the corresponding temperature.
[0021] Taking the sample test at 6 time points under the same temperature as an example, the evaluation method for the high-temperature corrosion resistance of the self-generating acid system can be carried out using the following steps:
[0022] Step 1: Accurately weigh 6 solid carbonate pieces (each piece weighs approximately 15-30g, accurate to 0.0001g).
[0023] Step 2: Take 6 hydrothermal reactors with polytetrafluoroethylene liners of the same specifications, each with a volume of 200mL, and number them 1#, 2#, 3#, 4#, 5#, and 6#.
[0024] Step 3: At t=0, add accurately weighed solid carbonate m1, self-generating acid system and interface promoter respectively, immediately seal the polytetrafluoroethylene-lined hydrothermal reactor and place it in a constant temperature oven.
[0025] Step 4: At t=1h, remove the No. 1 PTFE-lined hydrothermal reactor; at t=2h, remove the No. 2 PTFE-lined hydrothermal reactor; at t=3h, remove the No. 3 PTFE-lined hydrothermal reactor; at t=4h, remove the No. 4 PTFE-lined hydrothermal reactor; at t=5h, remove the No. 5 PTFE-lined hydrothermal reactor; at t=6h, remove the No. 6 PTFE-lined hydrothermal reactor. Allow the reactor to cool to room temperature in the fume hood.
[0026] Step 5: After releasing the gas, open the container and filter the solid carbonate in the acid solution. Wash the inner cavity of the PTFE-lined hydrothermal reactor 2-3 times with distilled water to ensure that all the solids are transferred to the funnel. Then wash the solids on the filter paper 3-4 times with distilled water. Transfer the filter paper with the solids to the oven, dry it, weigh it, and record the mass m2 of the remaining solid carbonate after removing the mass of the filter paper.
[0027] The amount of solid carbonate dissolved (m2-m1) can be obtained by the above method, and then the concentration of acid generated and the acid conversion rate can be calculated.
[0028] The present invention will now be described in detail with reference to specific embodiments. It should be noted that the following embodiments are only used to further illustrate the present invention and should not be construed as limiting the scope of protection of the present invention. Some non-essential improvements and adjustments made by those skilled in the art based on the content of the present invention are still within the scope of protection of the present invention.
[0029] The testing instruments and conditions used in this embodiment are as follows:
[0030] The hydrothermal reactor was purchased from Guangzhou Zhiyan Instrument Co., Ltd.
[0031] The analytical balance was purchased from Mettler Toledo International Trading (Shanghai) Co., Ltd.
[0032] Unless otherwise specified, the raw materials used in the examples and comparative examples are all disclosed in the prior art, such as those that can be directly purchased or prepared according to the preparation methods disclosed in the prior art.
[0033] Calcium carbonate [size (20.0±0.1)mm×(20.0±0.1)mm×(20.0±0.1)mm, content >99%] was purchased from Beijing Huarui Xincheng Technology Co., Ltd.
[0034] The autogenous acid (SFAOR-1) was purchased from Sinopec Petroleum Engineering Technology Research Institute Co., Ltd.
[0035] Example 1
[0036] Step 1: Accurately weigh 6 pieces of solid calcium carbonate (each piece weighs approximately 23-25g, accurate to 0.0001g).
[0037] Step 2: Take 6 hydrothermal reactors with polytetrafluoroethylene liners of the same specifications, each with a volume of 200mL, and number them 1#, 2#, 3#, 4#, 5#, and 6#.
[0038] Step 3: At t=0, add 22.000±0.300g of accurately weighed solid calcium carbonate, 65.000±0.002g of the self-generating acid system (the self-generating acid system contains solid self-generating acid SFAOR-1 and water, of which 10.000±0.100g of solid self-generating acid and 55.000±0.003g of water) and 1.000±0.002g of the interface promoter dichloromethane. Immediately seal the polytetrafluoroethylene-lined hydrothermal reactor and place it in a constant temperature oven at 120±2℃.
[0039] Step 4: At t=1h, remove the No. 1 PTFE-lined hydrothermal reactor; at t=2h, remove the No. 2 PTFE-lined hydrothermal reactor; at t=3h, remove the No. 3 PTFE-lined hydrothermal reactor; at t=4h, remove the No. 4 PTFE-lined hydrothermal reactor; at t=5h, remove the No. 5 PTFE-lined hydrothermal reactor; at t=6h, remove the No. 6 PTFE-lined hydrothermal reactor. Allow the reactor to cool to room temperature in the fume hood.
[0040] Step 5: After releasing the gas, open the container and filter the solid calcium carbonate in the acid solution. Wash the inner cavity of the PTFE-lined hydrothermal reactor 2-3 times with distilled water to ensure that all the solids are transferred to the funnel. Then wash the solids on the filter paper 3-4 times with distilled water. Transfer the filter paper with the solids to the oven and dry it at 105℃ for 4 hours. After drying, take it out and weigh it, and record the mass m2 of the remaining solid calcium carbonate after removing the mass of the filter paper.
[0041] The dissolution rate is calculated using the following formula:
[0042] Dissolution amount = m1 - m2
[0043] Where m1 is the initial mass of solid calcium carbonate, in g; and m2 is the remaining mass of solid calcium carbonate after a period of dissolution, in g.
[0044] Table 1
[0045] 1# 2# 3# 4# 5# 6# <![CDATA[m1,g]]> 22.195 22.117 22.196 22.179 22.069 22.141 <![CDATA[m2,g]]> 21.675 21.391 20.864 20.020 19.173 17.736 Interface promoter, g 1.000 1.000 1.000 1.000 1.000 1.000 t, h 1 2 3 4 5 6 Dissolution amount, g 0.520 0.726 1.332 2.159 2.896 4.405 Acid concentration, % 0.75 1.05 1.91 3.06 4.06 6.04 Acid conversion rate, % 5.14 7.17 13.04 21.24 28.35 43.33
[0046] The concentration of the acid-generating acid is expressed as the percentage of the mass of the acid (SFAOR-1) converted into HCl, and the conversion rate of the acid-generating acid is the percentage of the mass of the acid-generating acid converted into HCl relative to the initial mass of the acid-generating acid.
[0047] Example 2:
[0048] The test procedure of Example 1 was used, except that the reaction temperature was 160°C.
[0049] Table 2
[0050] 1# 2# 3# 4# 5# 6# <![CDATA[m1,g]]> 22.019 22.083 22.160 22.072 22.217 22.118 <![CDATA[m2,g]]> 21.295 20.694 18.929 17.120 14.907 12.826 Interface promoter, g 1.000 1.000 1.000 1.000 1.000 1.000 t, h 1 2 3 4 5 6 Dissolution amount, g 0.724 1.389 3.231 4.952 7.310 9.292 Acid concentration, % 1.05 1.99 4.50 6.74 9.64 11.95 Acid conversion rate, % 7.12 13.65 31.82 48.71 72.05 91.59
[0051] Example 3
[0052] The test procedure of Example 1 was used, except that the reaction temperature was 180°C.
[0053] Table 3
[0054] 1# 2# 3# 4# 5# 6# <![CDATA[m1,g]]> 22.054 22.092 22.103 22.250 22.107 22.088 <![CDATA[m2,g]]> 21.029 20.220 17.287 12.179 12.025 11.954 Interface promoter, g 1.000 1.000 1.000 1.000 1.000 1.000 t, h 1 2 3 4 5 6 Dissolution amount, g 1.025 1.872 4.816 10.071 10.082 10.134 Acid concentration, % 1.47 2.66 6.57 13.04 13.04 13.14 Acid conversion rate, % 10.06 18.42 47.42 99.07 99.08 99.84
[0055] Example 4
[0056] Step 1: Accurately weigh 5 pieces of solid calcium carbonate (each piece weighs approximately 23-25g, accurate to 0.0001g).
[0057] Step 2: Take 5 hydrothermal reactors with polytetrafluoroethylene liners of the same specifications, each with a volume of 200mL, and number them 1#, 2#, 3#, 4#, and 5#.
[0058] Step 3: At t=0, add 22.000±0.300g of accurately weighed solid calcium carbonate, 65.000±0.002g of the self-generating acid system (the self-generating acid system contains solid self-generating acid SFAOR-1 and water, of which 10.000±0.100g of solid self-generating acid and 55.000±0.003g of water) and 1.000±0.002g of the interface promoter chloroform. Immediately seal the polytetrafluoroethylene-lined hydrothermal reactor and place it in a constant temperature oven at 200±2℃.
[0059] Step 4: At t=1h, remove the No. 1 PTFE-lined hydrothermal reactor; at t=2h, remove the No. 2 PTFE-lined hydrothermal reactor; at t=3h, remove the No. 3 PTFE-lined hydrothermal reactor; at t=4h, remove the No. 4 PTFE-lined hydrothermal reactor; at t=5h, remove the No. 5 PTFE-lined hydrothermal reactor. Cool the reactor to room temperature in the fume hood.
[0060] Step 5: After releasing the gas, open the container and filter the solid calcium carbonate in the acid solution. Wash the inner cavity of the PTFE-lined hydrothermal reactor 2-3 times with distilled water to ensure that all the solids are transferred to the funnel. Then wash the solids on the filter paper 3-4 times with distilled water. Transfer the filter paper with the solids to the oven and dry it at 105℃ for 4 hours. After drying, take it out and weigh it, and record the mass m2 of the remaining solid calcium carbonate after removing the mass of the filter paper.
[0061] Table 4
[0062] 1# 2# 3# 4# 5# <![CDATA[m1,g]]> 22.170 22.190 22.050 21.970 22.730 <![CDATA[m2,g]]> 18.940 15.197 10.400 9.191 8.398 Interface promoter, g 1.000 1.000 1.000 1.000 1.000 t, h 1 2 2.5 3 3.5 Dissolution amount, g 3.230 6.993 11.650 12.779 14.332 Acid concentration, % 4.50 9.27 14.54 15.72 17.30 Acid conversion rate, % 22.59 49.09 82.05 89.75 99.99
[0063] Example 5
[0064] The test steps of Example 4 were used, except that the amount of interface promoter added was 0.800g.
[0065] Table 5
[0066] 1# 2# 3# 4# 5# <![CDATA[m1,g]]> 22.015 22.179 22.003 22.081 22.001 <![CDATA[m2,g]]> 18.899 16.006 11.835 10.898 9.711 Interface promoter, g 0.800 0.800 0.800 0.800 0.800 t, h 1 2 2.5 3 3.5 Dissolution amount, g 3.116 6.173 10.168 11.183 12.290 Acid concentration, % 4.351 8.267 12.926 14.036 15.214 Acid conversion rate, % 21.789 43.319 71.609 78.533 85.758
[0067] Example 6
[0068] The test procedure of Example 4 was adopted, except that at t=0, 30.000±0.300g of solid calcium carbonate, 70.000±0.002g of the self-generating acid system (of which, 5.000±0.100g of solid self-generating acid SFAOR-11 and 55.000±0.003g of water) and 1.500±0.002g of interface promoter were added respectively.
[0069] Table 6
[0070] 1# 2# 3# 4# 5# <![CDATA[m1,g]]> 29.975 30.271 30.004 30.128 30.202 <![CDATA[m2,g]]> 26.763 23.148 18.447 17.470 15.957 Interface promoter, g 1.500 1.500 1.500 1.500 1.500 t, h 1 2 2.5 3 3.5 Dissolution amount, g 3.212 7.123 11.557 12.658 14.245 Acid concentration, % 4.475 9.924 16.101 17.635 19.846 Acid conversion rate, % 16.136 35.065 58.608 64.108 71.423
[0071] Example 7
[0072] The test procedure of Example 4 was adopted, except that at t=0, 15.000±0.300g of solid calcium carbonate, 65.000±0.002g of the self-generating acid system (of which, 0.000±0.100g of solid self-generating acid SFAOR-11 and 55.000±0.003g of water) and 2.000±0.002g of interface promoter were added respectively.
[0073] Table 7
[0074] 1# 2# 3# 4# 5# <![CDATA[m1,g]]> 15.265 15.198 15.007 15.032 15.298 <![CDATA[m2,g]]> 12.010 8.201 3.318 2.132 0.997 Interface promoter, g 2.000 2.000 2.000 2.000 2.000 t, h 1 2 2.5 3 3.5 Dissolution amount, g 3.255 6.997 11.689 12.900 14.301 Acid concentration, % 4.54 9.27 14.58 15.85 17.27 Acid conversion rate, % 22.76 49.10 82.32 90.59 99.79
[0075] Comparative Example 1
[0076] The test procedure of Example 4 was adopted, except that at t=0, 30.000±0.300g of solid calcium carbonate, 65.000±0.002g of the self-generating acid system (of which, 10.000±0.100g of solid self-generating acid and 55.000±0.003g of water) and 0.300±0.001g of interface promoter were added respectively.
[0077] Table 8
[0078] 1# 2# 3# 4# 5# <![CDATA[m1,g]]> 21.998 22.073 22.105 22.007 21.862 <![CDATA[m2,g]]> 20.927 19.518 18.403 16.309 13.065 Interface promoter, g 0.300 0.300 0.300 0.300 0.300 t, h 1 2 2.5 3 3.5 Dissolution amount, g 1.071 2.555 3.702 5.698 8.797 Acid concentration, % 1.540 3.596 5.128 7.680 11.382 Acid conversion rate, % 7.489 17.930 26.072 40.014 61.384
[0079] Comparative Example 2
[0080] The test procedure was the same as in Comparative Example 1, except that no interface accelerator was added.
[0081] Table 9
[0082] 1# 2# 3# 4# 5# <![CDATA[m1,g]]> 22.011 22.106 22.097 22.668 22.073 <![CDATA[m2,g]]> 21.091 20.007 19.143 17.903 14.476 t, h 1 2 2.5 3 3.5 Dissolution amount, g 0.920 2.099 2.954 4.765 7.597 Acid concentration, % 1.325 2.973 4.135 6.504 9.984 Acid conversion rate, % 6.433 14.730 20.804 33.462 53.011
[0083] Autogenous acid is a water-insoluble solid that reacts with water to form acid under the action of an interfacial accelerator. The interfacial accelerator regulates the acid-forming rate. Experimental results show that within a certain range, the acid-forming rate increases with increasing interfacial accelerator dosage, reaching a maximum at which point further increases in dosage do not improve the acid-forming rate.
[0084] The experimental results above show that the self-generating acid SFAOR-1 used in this invention, after reacting at 120℃ for 6 hours, 43.33% is converted into hydrochloric acid, with a dissolving effect equivalent to 6.04% hydrochloric acid; after reacting at 160℃ for 6 hours, 91.59% is converted into hydrochloric acid, with a dissolving effect equivalent to 11.95% hydrochloric acid; after reacting at 180℃ for 4 hours, 99.07% is converted into hydrochloric acid, with a dissolving effect equivalent to 13.04% hydrochloric acid; and after reacting at 200℃ for 3.5 hours, 99.99% is converted into hydrochloric acid, with a dissolving effect equivalent to 17.30% hydrochloric acid. Therefore, the applicable temperature and delayed dissolving properties of the self-generating acid can be determined using the evaluation method provided by this invention.
Claims
1. A method for evaluating the high-temperature corrosion resistance of an autogenous acid system, comprising the steps of heating and reacting components including an autogenous acid system, solid carbonate, and an interface promoter, and then evaluating the corrosion resistance of the autogenous acid system by weighing the amount of mass reduction of the solid carbonate.
2. The evaluation method according to claim 1, characterized in that, The evaluation method specifically includes the following steps: (a) Add solid carbonate, autogenous acid system and interface promoter to a hydrothermal reactor, seal and heat; (b) After heating the reaction, the temperature is lowered to room temperature, and the acid conversion rate is calculated from the weight loss of the solid carbonate.
3. The evaluation method according to claim 2, characterized in that, The hydrothermal reactor is a hydrothermal reactor with a polytetrafluoroethylene liner.
4. The evaluation method according to claim 1 or 2, characterized in that, The autogenous acid system comprises solid autogenous acid and water. Preferably, the mass ratio of solid autogenous acid to water in the autogenous acid system is 1:(2.5-10).
5. The evaluation method according to claim 1 or 2, characterized in that, The solid carbonate is selected from at least one of calcium carbonate, calcite, magnesite, and dolomite.
6. The evaluation method according to claim 1 or 2, characterized in that, The interface promoter is selected from at least one of C1-C6 haloalkanes and C6-C10 aromatics, preferably from at least one of dichloromethane, trichloromethane, carbon tetrachloride, and m-xylene.
7. The evaluation method according to claim 1 or 2, characterized in that, The mass ratio of the self-generating acid system to the solid carbonate is (1.5–5):1, preferably (2.3–3.5):1; and / or, The mass ratio of the self-generating acid system to the interface promoter is (28-100):1, preferably (32-85):
1.
8. The evaluation method according to claim 1 or 2, characterized in that, The heating reaction temperature is 90–200°C; and / or, The heating reaction time is 1 to 8 hours.
9. The evaluation method according to claim 2, characterized in that, Step (b) further includes filtering, washing, and drying after cooling to room temperature.
10. An evaluation method according to any one of claims 1 to 9, applied to evaluating the dissolution capacity of an autogenous acid system at different temperatures.