Double-sided electroplating device for composite current collector
By designing a double-sided electroplating device for composite current collectors and using electroplating tanks and heating components to perform double-sided electroplating of magnetron films, the problem that existing technology cannot directly test the performance of composite current collectors has been solved, and true detection of the performance of composite current collectors has been achieved. and efficient analysis of production lines.
Patent Information
- Application Number
- CN202323313790.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-06
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2033-12-06
AI Technical Summary
Existing electroplating experimental equipment cannot directly and truly test the performance of composite current collectors, and the traditional Hull cell experiment can only perform qualitative analysis and cannot reflect the performance of the product.
A composite current collector double-sided electroplating device is designed, including an electroplating tank, a heating component, an anode plate and a cathode. The anode plate is set at both ends of the electroplating tank, and the magnetron film is fixed in the electroplating tank through a fixing component for double-sided electroplating. Combined with optimized designs such as circulation pumps and baffles, it ensures the uniformity of the plating solution and the stable installation of the anode plate.
It realizes direct performance testing and double-sided electroplating of composite current collectors, solves the qualitative analysis problem of traditional experiments, can truly reflect product performance, and ensures solution uniformity through a circulation pump, improving the detection efficiency of the production line.
Smart Images

Figure CN221837127U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of current collectors, and in particular to a composite current collector double-sided electroplating device. Background Art
[0002] At present, under the background of "dual carbon", the new energy industry is developing rapidly, among which composite current collectors based on polymer membranes have received extensive attention and application in the new energy industry. The preparation process of the composite current collector is usually: a layer of metal (aluminum, copper, etc.) material is deposited on a polymer film (such as polypropylene, polyethylene, polyester, polyimide, etc.) by physical vapor deposition (PVD) method, and then a certain thickness of metal layer is deposited by chemical electroplating. The surface metallized film with a certain conductivity is the composite current collector. Compared with traditional current collectors, composite current collectors have the advantages of low cost, light weight and good internal insulation. As the base metal for the positive and negative electrodes of lithium-ion batteries to attach active substances, the performance of the current collector has a huge impact on the performance of lithium batteries. Therefore, it is crucial for the production of current collectors to prepare current collectors through small-scale experimental devices and to detect and regulate their performance.
[0003] However, at present, the performance of the composite current collector in the electroplating stage is mainly judged through the Hull cell experiment in the laboratory. This method can only qualitatively analyze the appearance of the Hull cell and indirectly judge the current collector. On the one hand, this method cannot directly judge the performance of the current collector; on the other hand, since the material of the Hull cell is different from the base material of the current collector, the performance of the two cannot be directly equated. In addition, there are few existing electroplating experimental devices, or only single-sided electroplating of the magnetron film can be performed, which cannot truly reflect the performance of the product. Therefore, it is necessary to develop an experimental device for the electroplating stage of the composite current collector, based on the magnetron film, for the preparation of the composite current collector, and to directly and truly test the performance of the current collector. Utility Model Content
[0004] In order to solve the problems in the above-mentioned background technology, the present application provides a composite current collector double-sided electroplating device.
[0005] The present application provides a composite current collector double-sided electroplating device that adopts the following technical solution:
[0006] A composite current collector double-sided electroplating device comprises an electroplating tank, the electroplating tank is used to hold an electroplating solution; a heating component, the heating component is arranged in the electroplating tank, and is used to heat the electroplating solution; the electroplating component comprises an anode plate and a cathode, the anode plates are two, and are respectively arranged at two ends of the length direction of the electroplating tank, the cathode is a magnetron film, the magnetron film is vertically fixed in the electroplating tank by a fixing component, so that the two sides of the magnetron film in the thickness direction face the two anode plates respectively; during operation, the anode plate is connected to the anode of a rectifier, and the magnetron film is connected to the cathode of the rectifier.
[0007] By adopting the above technical solution, the device can directly perform double-sided electroplating on the magnetron film to prepare a composite current collector, which can help the production line directly analyze the performance of the composite current collector; secondly, it solves the problem that the traditional Hull cell experiment can only perform qualitative analysis.
[0008] Preferably, the electroplating tank is connected to a circulation pipe for circulating the electroplating solution, and the circulation pipe is provided with a circulation pump.
[0009] By adopting the above technical solution, the uniform state of the entire solution is ensured and concentration polarization is prevented.
[0010] Preferably, baffles are respectively provided at both ends of the length direction of the electroplating tank, and the two ends of the baffles in the length direction are respectively connected to the inner side walls on both sides of the width of the electroplating tank, and a slot for inserting the anode plate is formed between the baffle and the wall of the electroplating tank.
[0011] By adopting the above technical solution, the setting of the baffle plate facilitates the rapid installation of the anode plate and the rapid positioning of the anode plate.
[0012] Preferably, one end of the baffle in the length direction is rotatably connected to the inner wall of the electroplating tank, and the inner wall of the electroplating tank is provided with a fixing block for fixing the baffle, and a pin is movably inserted on the fixing block, and the pin is also inserted in the baffle.
[0013] By adopting the above technical solution, the baffle is rotatably arranged, thus preventing the anode plate from being directly inserted from the slot and causing damage to the anode plate; during installation, the baffle can be moved.
[0014] Preferably, the fixing assembly comprises two groups of rubber magnets respectively arranged in the width direction of the electroplating tank, and the inner wall of the electroplating tank is provided with a slot for inserting the rubber magnets; each group of rubber magnets has two rubber magnets, which are magnetically clamped on both sides of the thickness direction of the magnetron film; a conductive sheet is commonly connected between the two groups of rubber magnets.
[0015] By adopting the above technical solution, the disassembly and assembly of the magnetron film is facilitated.
[0016] Preferably, a plurality of grooves are provided on a side of the rubber magnet away from the magnetron film along the length direction of the rubber magnet.
[0017] Preferably, at least one through hole is formed on the anode plate, and one end of the anode plate provided with the through hole faces upward.
[0018] By adopting the above technical solution, the provision of the through holes makes it easier for workers to operate the anode plate.
[0019] In summary, the present application includes at least one of the following beneficial technical effects: the present device can directly perform double-sided electroplating on the magnetron film to prepare a composite current collector, which can help the production line directly analyze the performance of the composite current collector; secondly, it solves the problem that the traditional Hull cell experiment can only perform qualitative analysis. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the overall structure of a composite current collector double-sided electroplating device in an embodiment of the present application.
[0021] Figure 2 yes Figure 1 Enlarged view of part A.
[0022] Figure 3 yes Figure 1 Magnified view of part B.
[0023] Explanation of the reference numerals: 1. electroplating tank; 2. heating component; 3. anode plate; 31. through hole; 4. cathode; 5. fixing component; 51. rubber magnet; 511. groove; 52. card slot; 6. conductive sheet; 7. circulation pipe; 71. circulation pump; 8. baffle; 81. fixing block; 82. latch. DETAILED DESCRIPTION
[0024] The following is combined with Figure 1-3 This application is described in further detail.
[0025] The present application discloses a composite current collector double-sided electroplating device. Figure 1 and Figure 2 , the electroplating device comprises an electroplating tank 1, and the electroplating tank 1 is used to hold an electroplating solution;
[0026] The heating component 2 is a temperature-controlled heating rod, which is arranged in the electroplating tank 1 and is used to heat the electroplating solution;
[0027] The electroplating assembly includes an anode plate 3 and a cathode 4. There are two anode plates 3, which are respectively arranged at the two ends of the length direction of the electroplating tank 1. The cathode 4 is a magnetron film formed by a polymer base film passing through a magnetron metal. The polymer base film can be one or more of polyimide, polypropylene, polyethylene, polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, polypropylene, polyvinyl chloride, polyvinylidene fluoride and polystyrene; the metal is one or more of copper, copper alloy, aluminum, aluminum alloy, nickel, nickel alloy, titanium and silver. The magnetron film in the present application is preferably polybutylene terephthalate with copper layers sputtered on both sides; the magnetron film is vertically fixed on the fixing assembly 5 by the fixing assembly 5. In the electroplating tank 1, the two sides of the magnetron film in the thickness direction are respectively facing the two anode plates 3, and the fixing component 5 includes two groups of rubber magnets 51 respectively arranged in the width direction of the electroplating tank 1, and the inner wall of the electroplating tank 1 is provided with a card slot 52 for inserting the rubber magnet 51; each group of rubber magnets 51 has two, which are clamped on both sides of the magnetron film in the thickness direction by magnetic clamping, and a side of the rubber magnet 51 away from the magnetron film is evenly provided with a plurality of grooves along the length direction of the rubber magnet 51; a conductive sheet 6 is commonly connected between the two groups of rubber magnets 51; during operation, the anode plate 3 is connected to the anode of the rectifier, and the magnetron film is connected to the cathode 4 of the rectifier through the rubber magnet 51 and the conductive sheet 6, and then electroplating is performed.
[0028] Reference Figure 1 The electroplating tank 1 is connected with a circulation pipe 7 for circulating the electroplating solution, and the circulation pipe 7 is provided with a circulation pump 71. The electroplating solution in the electroplating tank 1 is circulated through the circulation pump 71 and the circulation pipe 7 to ensure that the electroplating solution in the electroplating tank 1 is uniform. Secondly, the setting of the circulation pump 71 also has the function of aeration and stirring.
[0029] Reference Figure 1 and Figure 3 Baffles 8 are respectively provided at both ends of the length direction of the electroplating tank 1. Both ends of the length direction of the baffle 8 are respectively connected to the inner side walls on both sides of the width of the electroplating tank 1. A slot for inserting the anode plate 3 is formed between the baffle 8 and the tank wall of the electroplating tank 1. One end of the baffle 8 in the length direction is rotatably connected to the inner side wall of the electroplating tank 1 through a hinge. The inner side wall of the electroplating tank 1 is provided with a fixing block 81 for fixing the baffle 8. A plug 82 is movably inserted on the fixing block 81. The plug 82 is also inserted in the baffle 8 to fix the baffle 8. At least one through hole 31 is provided on the anode plate 3. One end of the anode plate 3 with the through hole 31 faces upward. The setting of the through hole 31 is convenient for the staff to operate the anode plate 3.
[0030] The implementation principle of a double-sided electroplating device for a composite current collector in an embodiment of the present application is as follows: first, the magnetron membrane is clamped with a rubber magnet 51 and placed in a slot 52, and then anode plates 3 and anode plates 3 are respectively placed on the left and right sides of the electroplating tank 1; then, the configured electroplating solution is added to the electroplating tank 1; the circulation pump 71 is turned on, and the anode plates 3 at both ends are respectively connected to the anode of the rectifier, and the conductive sheet 6 on the rubber magnet 51 is connected to the cathode 4 of the rectifier, and the required experimental current is set. After electroplating for a certain period of time, a double-sided electroplated composite current collector can be obtained, and the experiment is ended.
[0031] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A composite current collector double-sided electroplating device, characterized in that: It comprises an electroplating tank (1), wherein the electroplating tank (1) is used to contain an electroplating solution; A heating component (2), wherein the heating component (2) is arranged in the electroplating tank (1) and is used to heat the electroplating solution; The electroplating assembly comprises an anode plate (3) and a cathode (4), wherein two anode plates (3) are provided, respectively disposed at two ends of the length direction of an electroplating tank (1), and the cathode (4) is a magnetron film, which is vertically fixed in the electroplating tank (1) by a fixing assembly (5) so that both sides of the magnetron film in the thickness direction face the two anode plates (3) respectively; during operation, the anode plate (3) is connected to the anode of a rectifier, and the magnetron film is connected to the cathode (4) of the rectifier.
2. A composite current collector double-sided electroplating device according to claim 1, characterized in that: The electroplating tank (1) is connected to a circulation pipe (7) for circulating the electroplating solution, and the circulation pipe (7) is provided with a circulation pump (71).
3. A composite current collector double-sided electroplating device according to claim 1, characterized in that: Baffles (8) are respectively provided at both ends of the length direction of the electroplating tank (1); the two ends of the baffles (8) are respectively connected to the inner side walls on both sides of the width of the electroplating tank (1); and a slot for inserting the anode plate (3) is formed between the baffles (8) and the wall of the electroplating tank (1).
4. A composite current collector double-sided electroplating device according to claim 3, characterized in that: One end of the baffle (8) in the length direction is rotatably connected to the inner wall of the electroplating tank (1); the inner wall of the electroplating tank (1) is provided with a fixing block (81) for fixing the baffle (8); a latch (82) is movably inserted into the fixing block (81); and the latch (82) is simultaneously inserted into the baffle (8).
5. A composite current collector double-sided electroplating device according to claim 1, characterized in that: The fixing assembly (5) comprises two groups of rubber magnets (51) respectively arranged in the width direction of the electroplating tank (1); a slot (52) for inserting the rubber magnets (51) is arranged on the inner wall of the electroplating tank (1); each group of rubber magnets (51) has two rubber magnets (51) which are clamped on both sides of the magnetron film in the thickness direction by magnetic clamping; a conductive sheet (6) is commonly connected between the two groups of rubber magnets (51).
6. A composite current collector double-sided electroplating device according to claim 5, characterized in that: A plurality of grooves (511) are arranged along the length direction of the rubber magnet (51) on one side of the rubber magnet (51) away from the magnetron film.
7. A composite current collector double-sided electroplating device according to claim 1, characterized in that: At least one through hole (31) is provided on the anode plate (3), and one end of the through hole (31) provided on the anode plate (3) faces upward.