Negative electrode of secondary battery, secondary battery, and electronic device
By combining the aluminum material layer and the carbon material layer in the negative electrode of the secondary battery, the problem of separator damage during long-term use of the secondary battery is solved, the conductivity is improved and dendrite formation is suppressed, the service life of the battery is extended and the stability is improved sex.
Patent Information
- Application Number
- CN202420156201.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-22
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2034-01-22
AI Technical Summary
Secondary batteries are prone to side reactions during long-term use, leading to damage to the separator, which in turn leads to internal short circuits. It is difficult to effectively solve this problem with existing technology.
Design a negative electrode for a secondary battery, including a negative electrode conductive case, an aluminum material layer and a carbon material layer. The aluminum material layer is arranged inside the negative electrode conductive case, and the carbon material layer is arranged on the side away from the aluminum material layer. By controlling the material The thickness and mass ratio of the layer improve the conductivity and inhibit the formation of dendrites, thereby protecting the separator.
By improving the conductivity between the carbon material layer and the negative electrode conductive case, the formation of dendrites is suppressed, the service life of the secondary battery is extended, and its reliability and stability during long cycles are improved.
Smart Images

Figure CN221841872U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of batteries, in particular to a negative electrode of a secondary battery, a secondary battery and electronic equipment. Background Art
[0002] A secondary battery (rechargeable battery), also known as a rechargeable battery or storage battery, refers to a battery that can be recharged to activate the active material after being discharged and continue to be used.
[0003] In the related art, during long-term use of secondary batteries such as lithium manganese button batteries, some side reactions are likely to occur inside, which may cause damage to the diaphragm and eventually lead to an internal short circuit of the secondary battery.
[0004] Therefore, the prior art needs to be improved and enhanced. Utility Model Content
[0005] The embodiments of the utility model provide a negative electrode of a secondary battery, a secondary battery and an electronic device, which can improve the technical problem that the diaphragm is easily damaged during the long-term use of the secondary battery.
[0006] In a first aspect, an embodiment of the present utility model provides a negative electrode of a secondary battery, comprising:
[0007] A negative electrode conductive shell;
[0008] an aluminum material layer, the aluminum material layer being disposed inside the negative electrode conductive shell and electrically connected to the negative electrode conductive shell; and
[0009] A carbon material layer is disposed on a side of the aluminum material layer away from the negative electrode conductive shell and is electrically connected to the aluminum material layer.
[0010] In one embodiment, the mass ratio of the carbon material layer to the aluminum material layer is 1:9 to 9:1; and / or
[0011] The thickness of the aluminum material layer is 0.03 to 0.2 mm; and / or
[0012] The thickness of the carbon material layer is 0.05 to 0.35 mm; and / or
[0013] The carbon material layer includes one of carbon foil, hard carbon and soft carbon.
[0014] In one embodiment, the carbon material layer covers a surface of the aluminum material layer that is away from the negative electrode conductive shell.
[0015] In one embodiment, the negative electrode conductive shell includes a negative electrode shell bottom wall and a negative electrode shell ring wall arranged around the negative electrode shell bottom wall, and the aluminum material layer and the carbon material layer are both arranged on the inner side of the negative electrode shell ring wall;
[0016] Wherein, the aluminum material layer covers the bottom wall of the negative electrode shell.
[0017] In a second aspect, an embodiment of the present invention further provides a secondary battery, comprising a negative electrode as described in any one of the above items.
[0018] In one embodiment, the secondary battery further comprises:
[0019] A positive electrode conductive shell, wherein the positive electrode conductive shell has a receiving cavity, and an end edge of the negative electrode conductive shell is disposed in the receiving cavity;
[0020] A positive electrode, the positive electrode is disposed in the accommodating cavity and is electrically connected to the positive electrode conductive shell;
[0021] An electrolyte, the electrolyte is disposed in the accommodating cavity and infiltrates the positive electrode and the carbon material layer respectively;
[0022] a separator, the separator being disposed between the positive electrode and the negative electrode and separating the positive electrode from the negative electrode; and
[0023] A sealing member is at least partially disposed at the opening end edge of the positive electrode conductive shell to seal the gap between the opening end edge of the accommodating cavity and the negative electrode conductive shell.
[0024] In one embodiment, when the negative electrode conductive shell includes a negative electrode shell bottom wall and a negative electrode shell ring wall, at least a portion of the negative electrode shell ring wall is bent and extended outward in a direction away from the negative electrode shell bottom wall, and the diaphragm, the electrolyte and the positive electrode are at least partially arranged on the inner side of the negative electrode shell ring wall.
[0025] In one embodiment, at least one of the separator and the positive electrode is snapped to the seal.
[0026] In one embodiment, the seal comprises:
[0027] A sealing portion, the sealing portion is arranged around the outer circumference of the negative electrode conductive shell;
[0028] a connecting portion connected to an inner side of an end of the sealing portion close to the positive electrode; and
[0029] A clamping portion, the clamping portion is connected to the inner side of the connecting portion, and a clamping groove is formed between the clamping portion and the sealing portion;
[0030] Wherein, the end edge of the negative electrode conductive shell and the end edge of the diaphragm are both clamped in the clamping groove, and the positive electrode is clamped on the inner side wall of the clamping part.
[0031] In a third aspect, an embodiment of the present invention provides an electronic device, comprising the secondary battery as described above.
[0032] Beneficial effects of the embodiments of the utility model:
[0033] In an embodiment of the utility model, the carbon material layer on the inner side of the negative electrode conductive shell can be directed toward or directly contact the diaphragm inside the secondary battery. At this time, the conductivity between the carbon material layer and the negative electrode conductive shell can be improved by the aluminum material layer. At the same time, the carbon material layer can effectively inhibit the generation of dendrites in the aluminum-containing negative electrode during a long cycle. Therefore, the negative electrode provided by the utility model can not only meet the actual demand for having good conductive performance, but also improve the technical problem that the negative electrode is prone to form dendrites and penetrate the diaphragm during a long cycle. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0035] Figure 1 is an exploded view of the negative electrode of the secondary battery provided by an embodiment of the present invention.
[0036] Figure 2 for Figure 1 A cross-sectional view of a first structure of a negative electrode is shown.
[0037] Figure 3 for Figure 1 A cross-sectional view of a second structure of a negative electrode is shown.
[0038] Figure 4 for Figure 1 A cross-sectional view of the third structure of the negative electrode shown.
[0039] Figure 5 A schematic diagram of the structure of a secondary battery provided in an embodiment of the present application.
[0040] Figure 6 Another schematic diagram of the structure of the secondary battery provided in the embodiment of the present application.
[0041] Figure 7 A flow chart of a first method for preparing a negative electrode of a secondary battery provided in an embodiment of the present application.
[0042] Figure 8 A flow chart of a second method for preparing a negative electrode of a secondary battery provided in an embodiment of the present application.
[0043] Fig. 9 A flow chart of a third method for preparing the negative electrode of a secondary battery provided in an embodiment of the present application.
[0044] Fig.10 A flow chart of a fourth method for preparing the negative electrode of a secondary battery provided in an embodiment of the present application.
[0045] The numbers in the figure are:
[0046] 100, negative electrode;
[0047] 11. Negative electrode conductive shell; 111. Negative electrode shell bottom wall; 112. Negative electrode shell ring wall; 12. Aluminum material layer; 13. Carbon material layer;
[0048] 200, positive electrode conductive shell;
[0049] 21. accommodating cavity; 22. bottom wall of positive electrode shell; 23. annular wall of positive electrode shell;
[0050] 300, positive electrode;
[0051] 400, diaphragm;
[0052] 500, seals;
[0053] 51. Sealing part; 52. Connecting part; 53. Clamping part. DETAILED DESCRIPTION
[0054] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the utility model, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application. In addition, it should be understood that the specific implementation methods described herein are only used to illustrate and explain the present application, and are not used to limit the present application. In the present application, unless otherwise stated, the directional words used, such as "upper" and "lower", generally refer to the upper and lower parts of the device in actual use or working state, specifically the drawing direction in the accompanying drawings; and "inside" and "outside" refer to the outline of the device.
[0055] In addition, the "plurality" in the embodiments of the present application refers to two or more than two. In view of this, in the embodiments of the present application, "plurality" can also be understood as "at least two". "At least one" can be understood as one or more, for example, one, two or more. For example, including at least one means including one, two or more, and there is no limit on which ones are included. For example, including at least one of A, B and C, then A, B, C, A and B, A and C, B and C, or A, B and C can be included.
[0056] It should be noted that, in the embodiments of the present application, "and / or" describes the association relationship of the associated objects, indicating that three relationships may exist. For example, A and / or B may represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / ", unless otherwise specified, generally indicates that the associated objects before and after are in an "or" relationship.
[0057] The embodiments of the present application provide a negative electrode of a secondary battery and a preparation method thereof, a secondary battery, and an electronic device, which will be introduced below respectively.
[0058] First, the embodiment of the present application provides a negative electrode of a secondary battery. The secondary battery can be a button battery (also called a button battery) or a cylindrical battery, etc., which is not limited in the embodiment of the present application.
[0059] Please refer to Figure 1 and Figure 2 , Figure 1 is an exploded view of the negative electrode of the secondary battery provided by the embodiment of the utility model, Figure 2 for Figure 1 The negative electrode 100 of the secondary battery may include a negative electrode conductive shell 11, an aluminum material layer 12 and a carbon material layer 13. The aluminum material layer 12 is disposed on the inner side of the negative electrode conductive shell 11 and is electrically connected to the negative electrode conductive shell 11. The carbon material layer 13 is disposed on the side of the aluminum material layer 12 away from the negative electrode conductive shell 11 and is electrically connected to the aluminum material layer 12.
[0060] Therefore, the carbon material layer 13 can be directed toward or directly contact the diaphragm inside the secondary battery, and the aluminum material layer 12 can improve the conductivity between the carbon material layer 13 and the negative electrode conductive shell 11. At the same time, the carbon material layer 13 can effectively inhibit the generation of dendrites in the aluminum-containing negative electrode 100 during a long cycle. Therefore, the negative electrode 100 provided in the embodiment of the present application can not only meet the actual demand for having good conductive properties, but also improve the technical problem that the negative electrode 100 is prone to form dendrites and penetrate the diaphragm during a long cycle.
[0061] In some embodiments, the mass ratio of the carbon material layer 13 to the aluminum material layer 12 is 1:9 to 9:1.
[0062] It can be understood that, taking the button-type secondary battery as an example, the aluminum material layer 12 mainly plays the role of connecting the carbon material layer 13 and the negative electrode conductive shell 11 during the short-term cycle process, and gradually reacts to form an aluminum-lithium alloy during the long-term cycle process, thereby increasing the capacity of the negative electrode 100. Therefore, by controlling the mass ratio of the carbon material layer 13 to the aluminum material layer 12, it is possible to ensure the capacity of the negative electrode 100 in the early or short-term cycle process, and ensure that the carbon material layer 13 can inhibit the formation of dendrites during the long cycle process, thereby ensuring the reliability and stability of the secondary battery during long-term use.
[0063] For example, the mass ratio of the carbon material layer 13 to the aluminum material layer 12 can be 1:9, 1.4:7.6, 2:8, 3:7, 4:6, 4.1:5.9, 5:5, 6:4, 7:3, 7.6:2.4, 8:2 or 9:1, etc., which is not limited to the embodiments of the present application.
[0064] In some embodiments, the thickness of the aluminum material layer 12 may be 0.03-0.2 mm.
[0065] Then, continuing to take the button-type secondary battery as an example, the volume of the battery itself is relatively small. In order to increase the capacity of the battery under a limited volume, the overall thickness of the negative electrode 100 cannot be too large. Based on this, when the overall thickness of the negative electrode 100 is limited, the embodiment of the present application controls the thickness of the aluminum material layer 12 to between 0.03 and 0.2 mm, and the thickness of the carbon material layer 13 can be made thicker, so that the negative electrode 100 can ensure that the negative electrode 100 has sufficient capacity in the early stage or short-term cycle process, and can also ensure that the carbon material layer 13 is sufficient to continuously suppress the formation of dendrites during the long-term cycle process.
[0066] Exemplarily, the thickness of the aluminum material layer 12 can be 0.03 mm, 0.05 mm, 0.06 mm, 0.074 mm, 0.081 mm, 0.099 mm, 0.1 mm, 0.12 mm, 0.137 mm, 0.141 mm, 0.144 mm, 0.15 mm, 0.166 mm, 0.17 mm, 0.184 mm, 0.191 mm or 0.2 mm, etc., which is not limited to the embodiments of the present application.
[0067] In some embodiments, the thickness of the carbon material layer 13 may be greater than the thickness of the aluminum material layer 12 .
[0068] Then, continuing with the button-type secondary battery as an example, the embodiment of the present application can ensure that the carbon material layer 13 has sufficient thickness, thereby ensuring the capacity of the negative electrode 100 in the early or short-term cycle process, and can also ensure that the carbon material layer 13 is sufficient to continuously suppress the formation of dendrites during long-term cycles.
[0069] In some embodiments, the carbon material layer 13 has a thickness of 0.05 to 0.35 mm.
[0070] Then, continuing with the button-type secondary battery as an example, by controlling the thickness of the carbon material layer 13 to be 0.05 to 0.35 mm, it can be ensured that the carbon material layer 13 has sufficient thickness, thereby ensuring the capacity of the negative electrode 100 in the early or short-term cycle process, and at the same time ensuring that the carbon material layer 13 is sufficient to continuously suppress the formation of dendrites during long-term cycles.
[0071] Exemplarily, the thickness of the carbon material layer 13 can be 0.05 mm, 0.06 mm, 0.074 mm, 0.081 mm, 0.099 mm, 0.1 mm, 0.12 mm, 0.137 mm, 0.141 mm, 0.144 mm, 0.15 mm, 0.166 mm, 0.17 mm, 0.184 mm, 0.191 mm, 0.2 mm, 0.214 mm, 0.231 mm, 0.244 mm, 0.25 mm, 0.27 mm, 0.294 mm, 0.3 mm, 0.312 mm, 0.325 mm, 0.341 mm or 0.35 mm, etc., which is not limited to the embodiments of the present application.
[0072] In some embodiments, the carbon material layer 13 includes one of carbon foil, hard carbon and soft carbon. Of course, the carbon material layer 13 may include other types of carbon materials, which is not limited in the embodiments of the present application.
[0073] In some embodiments, the carbon material layer 13 and the aluminum material layer 12 may both be circular, or may both be quasi-circular such as elliptical, etc., which is not limited in the embodiments of the present application. Of course, depending on the form of the secondary battery, the carbon material layer 13 and the aluminum material layer 12 may also be square, triangular, etc., which is not limited in the embodiments of the present application.
[0074] Please refer to Figure 2 and Figure 3 , Figure 3 for Figure 1 In some embodiments, the carbon material layer 13 may cover the surface of the aluminum material layer 12 facing away from the negative electrode conductive shell 11, thereby isolating the aluminum material layer 12 from the separator inside the secondary battery to better inhibit the formation of dendrites.
[0075] In some embodiments, the orthographic projection of the carbon material layer 13 on the plane where the aluminum material layer 12 is located can overlap with the aluminum material layer 12 , so that all parts of the carbon material layer 13 can form a good electrical connection with the negative electrode conductive shell 11 through the aluminum material layer 12 .
[0076] Of course, please continue to refer to Figure 4 , Figure 4 for Figure 1 A cross-sectional view of the third structure of the negative electrode is shown. In some other embodiments, the diameter of the aluminum material layer 12 may be greater than the diameter of the carbon material layer 13, which is not limited in the present embodiment.
[0077] In some embodiments, the negative electrode conductive shell 11 may include a negative electrode shell bottom wall 111 and a negative electrode shell ring wall 112 disposed around the negative electrode shell bottom wall 111. The aluminum material layer 12 and the carbon material layer 13 are both disposed on the inner side of the negative electrode shell ring wall 112.
[0078] In some embodiments, the aluminum material layer 12 covers the bottom wall 111 of the negative electrode shell, so that the aluminum material layer 12 can be made as large as possible to improve the conductivity between the carbon material layer 13 and the negative electrode conductive shell 11, and to improve the capacity of the negative electrode 100 during long cycles.
[0079] It can also be understood that at least one of the negative electrode conductive shell 11 and the carbon material layer 13 can be fixed to the aluminum material layer 12 by pressing.
[0080] Of course, at least one of the carbon material layer 13 and the aluminum material layer 12 may also be connected and fixed to the negative electrode conductive shell 11 by means of clamping or the like, and this embodiment of the present application does not limit this. For example, the inner side of the negative electrode shell ring wall 112 may have a protrusion, and a limiting groove may be formed between the protrusion or the protrusion and the negative electrode shell bottom wall 111 to clamp at least one of the carbon material layer 13 and the aluminum material layer 12.
[0081] The above are some examples of the negative electrode 100 of the secondary battery according to the embodiment of the present application. The secondary battery according to the embodiment of the present application will be described below.
[0082] The secondary battery may include the negative electrode 100 of the secondary battery described above. The secondary battery may be a button cell (also called a button cell) or a cylindrical cell, etc., which is not limited in the embodiment of the present application.
[0083] Please continue to refer to Figure 5 , Figure 5 The secondary battery provided in the embodiment of the present application is a schematic diagram of the structure of the secondary battery. Exemplarily, the secondary battery may further include a positive electrode conductive shell 200, a positive electrode 300, an electrolyte (not shown in the figure) and a separator 400.
[0084] The positive electrode conductive shell 200 has a receiving cavity 21, and the edge of the negative electrode conductive shell 11 is disposed in the receiving cavity 21. The positive electrode 300 is disposed in the receiving cavity 21 and is electrically connected to the positive electrode conductive shell 200. The separator 400 is disposed between the positive electrode 300 and the negative electrode 100, and separates the positive electrode 300 from the negative electrode 100. The electrolyte is disposed in the receiving cavity 21, and infiltrates the positive electrode 300, the separator 400 and the carbon material layer 13 respectively.
[0085] Thus, the secondary battery is connected to an external load device through the positive electrode conductive casing 200 and the negative electrode conductive casing 11 to form a circuit, and the external load device is powered by a chemical reaction inside the secondary battery.
[0086] In some embodiments, the secondary battery may further include a seal 500. The seal 500 is at least partially disposed at the opening edge of the positive electrode conductive shell 200 to seal the gap between the opening edge of the accommodating cavity 21 and the negative electrode conductive shell 11. Thus, the positive electrode conductive shell 200, the negative electrode conductive shell 11 and the seal 500 may form a closed complete shell to achieve sealed isolation between the inside and outside of the secondary battery.
[0087] In some embodiments, the positive electrode conductive shell 200 and the negative electrode conductive shell 11 are further separated by a seal 500 to achieve electrical isolation, so that the seal 500 is reused for electrical isolation between the positive and negative electrodes 100 of the secondary battery to avoid short circuit between the positive and negative electrodes 100 of the secondary battery.
[0088] For example, the sealing member 500 may be a rubber sealing member 500. Of course, the sealing member 500 may also be a sealing member 500 made of other insulating materials, which is not limited in the present embodiment of the application.
[0089] Exemplarily, the positive electrode conductive shell 200 may include a positive electrode shell bottom wall 22 and a positive electrode shell ring wall 23 disposed around the positive electrode shell bottom wall 22. The positive electrode shell bottom wall 22 and the positive electrode shell ring wall 23 are arranged to form a receiving cavity 21. The seal 500 may be partially sandwiched between the positive electrode shell ring wall 23 and the outer peripheral side of the negative electrode conductive shell 11, thereby achieving sealing and electrical isolation between the positive electrode shell ring wall 23 and the negative electrode conductive shell 11. The seal 500 may also be partially disposed between the positive electrode shell bottom wall 22 and the negative electrode conductive shell 11, thereby achieving electrical isolation between the positive electrode shell bottom wall 22 and the negative electrode conductive shell 11.
[0090] In some embodiments, at least a portion of the negative electrode housing ring wall 112 is bent and extended outward in a direction away from the negative electrode housing bottom wall 111. The diaphragm 400, the electrolyte, and the positive electrode 300 are at least partially disposed on the inner side of the negative electrode housing ring wall 112. Thus, the space inside the negative electrode housing ring wall 112 can be increased to increase the capacity of the electrolyte, and a larger positive electrode 300 can be disposed to increase the capacity of the positive electrode 300. In addition, when the volume of the secondary battery is constant, the gap formed between the negative electrode housing ring wall 112 and the positive electrode housing ring wall 23 can be longer and more tortuous, thereby improving the sealing effect between the positive electrode conductive housing 200 and the negative electrode conductive housing 11.
[0091] In some embodiments, one end of the negative electrode casing annular wall 112 away from the negative electrode casing bottom wall 111 is tilted outward.
[0092] Of course, please continue to refer to Figure 6 , Figure 6 Another structural schematic diagram of a secondary battery provided in an embodiment of the present application. The end of the negative electrode casing ring wall 112 away from the negative electrode casing bottom wall 111 may also be perpendicular to the negative electrode casing bottom wall 111, so as to facilitate the buckling of the positive electrode conductive casing 200 to the negative electrode conductive casing 11.
[0093] In some embodiments, one end of the negative electrode casing annular wall 112 away from the negative electrode casing bottom wall 111 is snapped into the sealing member 500 .
[0094] In some embodiments, at least one of the diaphragm 400 and the positive electrode 300 is clamped to the seal 500. For example, the diaphragm 400 may be clamped to the seal 500, and the positive electrode 300 may not be clamped to the seal 500, or the diaphragm 400 may not be clamped to the seal 500, and the positive electrode 300 may be clamped to the seal 500, or both the diaphragm 400 and the positive electrode 300 may be clamped to the seal 500, and the embodiment of the present application is not limited to this.
[0095] Furthermore, the seal 500 can also be reused to fix the diaphragm 400 and / or the positive electrode 300, so that during use, the positive electrode 300 and / or the diaphragm 400 can be prevented from being unique, resulting in damage to the diaphragm 400 by collision, or the diaphragm 400 and / or the positive electrode 300 being displaced and causing poor contact, etc., thereby improving the reliability of the secondary battery.
[0096] In addition, it can also be understood that when the diaphragm 400 and the negative electrode housing ring wall 112 are both clamped to the seal 500, it means that the gap between the diaphragm 400 and the negative electrode housing ring wall 112 is smaller, and the inner side of the corresponding diaphragm 400 will have a larger space. Accordingly, the positive electrode 300 can be at least partially disposed on the inner side of the diaphragm 400. Thereby, the positive electrode 300 can be made larger to further increase the capacity of the positive electrode 300.
[0097] Exemplarily, the seal 500 may include a sealing portion 51, a connecting portion 52, and a clamping portion 53. The sealing portion 51 is arranged around the outer circumference of the negative electrode conductive shell 11. The connecting portion 52 is connected to the inner side of the sealing portion 51 near one end of the positive electrode 300. The clamping portion 53 is connected to the inner side of the connecting portion 52, and a clamping groove is formed between the clamping portion 53 and the sealing portion 51, and the end edge of the negative electrode conductive shell 11 and the end edge of the diaphragm 400 are clamped in the clamping groove.
[0098] In some embodiments, the positive electrode 300 is clamped to the inner wall of the clamping portion 53 .
[0099] It is also understandable that the sealing portion 51 may be a closed annular structure to achieve full circumferential sealing between the positive electrode housing ring wall 23 and the negative electrode housing ring wall 112. Of course, the sealing portion 51 may also be a non-closed annular structure, which is not limited in the present embodiment.
[0100] The connecting portion 52 may be a closed annular structure, or a non-closed annular structure, which is not limited in the embodiment of the present application.
[0101] Of course, in some other implementations, the diaphragm 400 and the positive electrode 300 may not be clamped to the seal 500, and this embodiment of the present application does not limit this.
[0102] In some embodiments, the positive electrode 300 may be made of high nickel, lithium iron phosphate, lithium manganese oxide, rechargeable manganese dioxide, or the like.
[0103] In some embodiments, the diaphragm 400 may be at least one layer, such as one layer, two layers, three layers or four layers, etc. Each layer of the diaphragm 400 may be a polyolefin diaphragm 400 or a glass fiber diaphragm 400, which is not limited in this embodiment of the present application.
[0104] Then, an assembly process of a secondary battery can be as follows:
[0105] First, in an atmosphere with a relative humidity lower than 1%, the aluminum material layer 12 and the carbon material layer 13 are placed in the negative electrode conductive casing 11 .
[0106] Then, the separator 400 is placed in the negative electrode conductive shell 11 . At this time, the electrolyte may be injected into the negative electrode conductive shell 11 to infiltrate the separator 400 and the carbon material layer 13 .
[0107] Next, the positive electrode 300 and the seal 500 are mounted to the negative electrode conductive case 11 so that the electrolyte also infiltrates the positive electrode 300 .
[0108] Finally, the positive electrode conductive shell 200 is buckled onto the negative electrode conductive shell 11 to complete the assembly of the secondary battery.
[0109] The embodiment of the present application also provides an electronic device, which may include the above-mentioned secondary battery. The electronic device may be, but is not limited to, a weight scale, a body fat scale, a nutrition scale, an infrared electronic thermometer, a pulse oximeter, a human body composition analyzer, a mobile power supply, a wireless charger, a fast charger, a car charger, an adapter, a display, a USB (Universal Serial Bus) docking station, a stylus, a true wireless headset, a car central control screen, a car, a smart wearable device, a mobile terminal, and a smart home device. Smart wearable devices include, but are not limited to, smart watches, smart bracelets, and cervical massagers. Mobile terminals include, but are not limited to, smart phones, laptops, tablets, and POS (point of sales terminal). Smart home devices include, but are not limited to, smart sockets, smart rice cookers, smart sweepers, and smart lights.
[0110] The embodiment of the present application also provides a method for preparing a negative electrode of a secondary battery, wherein the specific structure of the negative electrode of the secondary battery can be the same as the negative electrode 100 of the secondary battery described above. Of course, the specific structure of the negative electrode of the secondary battery can also be different from the negative electrode 100 of the secondary battery described above, and the embodiment of the present application does not limit this.
[0111] Please continue to refer to Figure 7 , Figure 7 A flow chart of a first method for preparing a negative electrode of a secondary battery provided in an embodiment of the present application. The preparation method may include the following steps 101 to 102:
[0112] 101. Obtain a negative electrode conductive shell, an aluminum material layer, and a carbon material layer.
[0113] In some embodiments, before obtaining the aluminum material layer, the process may further include preparing an aluminum material, and performing at least one of degreasing, cleaning, and drying the aluminum material to obtain the aluminum material layer.
[0114] 102. Arrange the aluminum material layer on the inner side of the negative electrode conductive shell, and arrange the carbon material layer on the side of the aluminum material layer away from the negative electrode conductive shell.
[0115] Therefore, the aluminum material layer can improve the conductivity between the carbon material layer and the negative electrode conductive shell. At the same time, the carbon material layer can effectively inhibit the generation of dendrites in the aluminum-containing negative electrode during a long cycle. Therefore, the negative electrode provided in the embodiment of the present application can not only meet the actual needs of having good conductive properties, but also improve the technical problem that the negative electrode is prone to form dendrites and penetrate the diaphragm during a long cycle.
[0116] In some embodiments, at least one of the negative electrode conductive shell and the carbon material layer is pressed and fixed with the aluminum material layer by pressing. Alternatively, the aluminum material layer is arranged on the inner side of the negative electrode conductive shell, and the carbon material layer is arranged on the side of the aluminum material layer away from the negative electrode conductive shell, including: pressing and fixing at least one of the negative electrode conductive shell and the carbon material layer with the aluminum material layer by pressing.
[0117] Thereby, at least one of the negative electrode conductive shell and the carbon material layer is more closely attached to the aluminum material layer, so as to further improve the conductivity between the carbon material layer and the negative electrode conductive shell.
[0118] In some embodiments, when at least one of the negative electrode conductive shell and the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature is 25 to 60° C., and / or the pressing pressure is 8 to 35 MPa, and / or the pressing time is 30 to 60 seconds, and / or the pressing environment humidity is less than or equal to 1%.
[0119] It is understandable that when the aluminum material is heated, the aluminum material will become soft or the hardness will decrease. Therefore, pressing the aluminum material layer in an environment between 25 and 60°C can avoid the aluminum material being too hard in a low temperature environment, thereby making the aluminum material layer and the corresponding negative electrode conductive shell and / or carbon material layer pressed more tightly. In addition, for aluminum materials, when the ambient temperature is high, the surface of the aluminum material is prone to produce an oxide layer and turn black, thereby reducing the conductivity of the aluminum material and affecting the appearance of the product, and even causing the aluminum material layer to crack, ultimately reducing the reliability and stability of the secondary battery.
[0120] Illustratively, the ambient temperature for pressing can be 25°C, 29.4°C, 31.1°C, 34.5°C, 36°C, 41°C, 42.4°C, 46.1°C, 49.2°C, 50°C, 51.3°C, 52.4°C, 53.7°C, 54.9°C, 56°C, 57.9°C, 58.9°C, 59.5°C or 60°C, etc., which is not limited to the embodiments of the present application.
[0121] In some embodiments, the pressing environment temperature may be greater than or equal to 45°C.
[0122] It is understandable that the pressing pressure is between 8 and 35 MPa, which means that at least one of the negative electrode conductive shell and the carbon material layer is pressed and fixed to the aluminum material layer by high pressure. Thus, it is possible to avoid the pressing being not in place due to too low a pressing pressure, and to avoid the pressing being too high due to one or more of the negative electrode conductive shell, the aluminum material layer and the carbon material layer being crushed, thereby improving the conductive effect of the negative electrode and making the negative electrode more stable and reliable.
[0123] Illustratively, the pressing pressure may be 8 MPa, 8.4 MPa, 9.7 MPa, 10 MPa, 11 MPa, 13 MPa, 15.5 MPa, 18.1 MPa, 20 MPa, 22.7 MPa, 24.378 MPa, 25 MPa, 28.8 MPa, or 35 MPa, which is not limited in the embodiments of the present application.
[0124] It is understandable that the pressing time is between 30 and 60 seconds, which can not only ensure that the aluminum material layer is pressed in place, but also avoid the reduction of production efficiency due to too long pressing time.
[0125] Exemplarily, the pressing time may be 30 seconds, 32 seconds, 34.7 seconds, 35 seconds, 38 seconds, 43 seconds, 45 seconds, 49.7 seconds, 50 seconds, 51.4 seconds, 53 seconds, 55 seconds, 56.9 seconds, 57 seconds, 58.4 seconds, 59 seconds, 59.7 seconds or 60 seconds, which is not limited to the embodiments of the present application.
[0126] It can also be understood that in actual operation, the pressing environment temperature can be between 25 and 60°C, the pressing pressure can be between 8 and 35 MPa, and the pressing time can be between 30 and 60 seconds, so that the aluminum material layer is in closer contact with the corresponding negative electrode conductive shell and / or carbon material layer.
[0127] Of course, the pressing environment temperature may not be between 25 and 60° C., or the pressing pressure may not be between 8 and 35 MPa, or the pressing time may not be between 30 and 60 seconds, and this embodiment of the present application does not limit this.
[0128] In addition, the humidity of the pressing environment can be less than or equal to 1%, thereby ensuring that water vapor is not easily retained inside the secondary battery during the production process, thereby improving the reliability and stability of the secondary battery.
[0129] A more detailed introduction will be given below.
[0130] Please continue to refer to Figure 8 , Figure 8 A flow chart of a second method for preparing a negative electrode of a secondary battery provided in an embodiment of the present application. The preparation method may include the following steps 201 to 204:
[0131] 201. Obtain a negative electrode conductive shell, an aluminum material layer, and a carbon material layer.
[0132] 202. The negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing to obtain a first intermediate.
[0133] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature is 25-60°C.
[0134] In some embodiments, when the negative electrode conductive casing is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature may be greater than or equal to 45°C.
[0135] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the pressing pressure is 8 to 35 MPa.
[0136] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the pressing time is 30 to 60 seconds.
[0137] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the humidity of the pressing environment is less than or equal to 1%.
[0138] 203. Place the carbon material layer into the first intermediate body and position it on the side of the aluminum material layer facing away from the negative electrode conductive shell.
[0139] 204. The carbon material layer is pressed and fixed to the aluminum material layer by pressing.
[0140] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature is 25-60°C.
[0141] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature may be greater than or equal to 45°C.
[0142] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing pressure is 8 to 35 MPa.
[0143] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing time is 30 to 60 seconds.
[0144] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the humidity of the pressing environment is less than or equal to 1%.
[0145] Of course, in some other embodiments, the carbon material layer may also be fixed to the side of the aluminum material layer away from the negative electrode conductive shell by means of clamping, bonding, etc., and this embodiment of the present application does not limit this.
[0146] Please continue to refer to Fig. 9 , Fig. 9 A flowchart of a third method for preparing a negative electrode of a secondary battery provided in an embodiment of the present application. In some embodiments, the preparation method may include the following steps 301 to 304:
[0147] 301. Obtain a negative electrode conductive shell, an aluminum material layer, and a carbon material layer.
[0148] 302. The carbon material layer is pressed and fixed with the aluminum material layer by pressing to obtain a second intermediate.
[0149] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature is 25-60°C.
[0150] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature may be greater than or equal to 45°C.
[0151] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing pressure is 8 to 35 MPa.
[0152] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the pressing time is 30 to 60 seconds.
[0153] In some embodiments, when the carbon material layer is pressed and fixed to the aluminum material layer by pressing, the humidity of the pressing environment is less than or equal to 1%.
[0154] 303. Place the second intermediate into the negative electrode conductive shell.
[0155] 304. The negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing.
[0156] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature is 25-60°C.
[0157] In some embodiments, when the negative electrode conductive casing is pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature may be greater than or equal to 45°C.
[0158] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the pressing pressure is 8 to 35 MPa.
[0159] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the pressing time is 30 to 60 seconds.
[0160] In some embodiments, when the negative electrode conductive shell is pressed and fixed to the aluminum material layer by pressing, the humidity of the pressing environment is less than or equal to 1%.
[0161] Please continue to refer to Fig.10 , Fig.10 A fourth method for preparing a negative electrode of a secondary battery provided in an embodiment of the present application is a flow chart. In some embodiments, the preparation method may include the following steps 401 to 402:
[0162] 401. Obtain a negative electrode conductive shell, an aluminum material layer, and a carbon material layer.
[0163] 402. Place the aluminum material layer and the carbon material layer in the negative electrode conductive shell in sequence, and press and fix the negative electrode conductive shell and the carbon material layer with the aluminum material layer at the same time.
[0164] In some embodiments, when the negative electrode conductive shell and the carbon material layer are pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature is 25-60°C.
[0165] In some embodiments, when the negative electrode conductive shell and the carbon material layer are pressed and fixed to the aluminum material layer by pressing, the pressing environment temperature may be greater than or equal to 45°C.
[0166] In some embodiments, when the negative electrode conductive shell and the carbon material layer are pressed and fixed to the aluminum material layer by pressing, the pressing pressure is 8 to 35 MPa.
[0167] In some embodiments, in the process of pressing and fixing the negative electrode conductive shell and the carbon material layer to the aluminum material layer by pressing, the pressing time is 30 to 60 seconds.
[0168] In some embodiments, when the negative electrode conductive shell and the carbon material layer are pressed and fixed to the aluminum material layer by pressing, the humidity of the pressing environment is less than or equal to 1%.
[0169] The embodiments of the present application are introduced in detail above. Specific examples are used in this article to illustrate the principles and implementation methods of the present utility model. The description of the above embodiments is only used to help understand the method and core idea of the present utility model. At the same time, for technical personnel in this field, according to the idea of the present utility model, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present utility model.
Claims
1. A negative electrode of a secondary battery, characterized in that: include: A negative electrode conductive shell; an aluminum material layer, the aluminum material layer being disposed on the inner side of the negative electrode conductive shell and being electrically connected to the negative electrode conductive shell; and A carbon material layer is disposed on a side of the aluminum material layer away from the negative electrode conductive shell and is electrically connected to the aluminum material layer.
2. The negative electrode according to claim 1, characterized in that The mass ratio of the carbon material layer to the aluminum material layer is 1:9 to 9:1; and / or The thickness of the aluminum material layer is 0.03 to 0.2 mm; and / or The thickness of the carbon material layer is 0.05 to 0.35 mm; and / or The carbon material layer includes one of carbon foil, hard carbon and soft carbon.
3. The negative electrode according to claim 1, characterized in that The carbon material layer covers a surface of the aluminum material layer that is away from the negative electrode conductive shell.
4. The negative electrode according to claim 1, characterized in that The negative electrode conductive shell comprises a negative electrode shell bottom wall and a negative electrode shell ring wall arranged around the negative electrode shell bottom wall, and the aluminum material layer and the carbon material layer are both arranged on the inner side of the negative electrode shell ring wall; Wherein, the aluminum material layer covers the bottom wall of the negative electrode shell.
5. A secondary battery, characterized in that: The negative electrode comprises the negative electrode as claimed in any one of claims 1 to 4.
6. The secondary battery according to claim 5, characterized in that: The secondary battery further comprises: A positive electrode conductive shell, wherein the positive electrode conductive shell has a receiving cavity, and an end edge of the negative electrode conductive shell is disposed in the receiving cavity; A positive electrode, the positive electrode is disposed in the accommodating cavity and is electrically connected to the positive electrode conductive shell; An electrolyte, the electrolyte is disposed in the accommodating cavity and infiltrates the positive electrode and the carbon material layer respectively; a separator, the separator being disposed between the positive electrode and the negative electrode and separating the positive electrode from the negative electrode; and A sealing member is at least partially disposed at the opening end edge of the positive electrode conductive shell to seal the gap between the opening end edge of the accommodating cavity and the negative electrode conductive shell.
7. The secondary battery according to claim 6, characterized in that: When the negative electrode conductive shell includes a negative electrode shell bottom wall and a negative electrode shell ring wall, at least a portion of the negative electrode shell ring wall is bent and extended outward in a direction away from the negative electrode shell bottom wall, and the diaphragm, the electrolyte and the positive electrode are at least partially arranged on the inner side of the negative electrode shell ring wall.
8. The secondary battery according to claim 6, characterized in that: At least one of the separator and the positive electrode is clamped to the seal.
9. The secondary battery according to claim 8, characterized in that: The sealing element comprises: A sealing portion, the sealing portion is arranged around the outer circumference of the negative electrode conductive shell; a connecting portion connected to an inner side of an end of the sealing portion close to the positive electrode; and A clamping portion, the clamping portion is connected to the inner side of the connecting portion, and a clamping groove is formed between the clamping portion and the sealing portion; Wherein, the end edge of the negative electrode conductive shell and the end edge of the diaphragm are both clamped in the clamping groove, and the positive electrode is clamped on the inner side wall of the clamping part.