Hexagonal socket cold heading die set
Through the multi-stage cold heading process of the internal hexagonal cold heading mold set, the part quality problems caused by insufficient deformation control are solved, and the precise molding of parts and extended mold life are achieved.
Patent Information
- Application Number
- CN202420443777.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-03-08
AI Technical Summary
During the cold heading production process, insufficient deformation control may lead to cracking and fracture problems in parts, affecting product quality and mold life.
Design an internal hexagonal cold heading die set. Through a multi-stage cold heading process, the cutting die and multiple cold heading dies are used to gradually heading the shape to ensure precise alignment and positioning of each step, disperse the deformation, reduce local resistance, and improve molding. Controllability of steps.
It effectively avoids cracking and fracture of parts, improves the mechanical properties of the product and the service life of the mold, ensures the accuracy of the product size and shape, and extends the service life of the mold.
Smart Images

Figure CN221909642U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to a cold heading die set, in particular to a hexagonal cold heading die set. Background Art
[0002] When manufacturing large quantities of fasteners, such as bolts, nuts and other parts, in order to achieve less cutting or even no cutting production, the cold heading production process is usually used. The cold heading production process directly forms the required parts through plastic deformation. Compared with the traditional cutting processing method, it reduces a large amount of waste caused by cutting processing and greatly improves the material utilization rate. Since cold heading is a plastic deformation performed at room temperature, the internal structure of the metal can be optimized. Compared with the cut parts, the parts obtained by cold heading have higher tensile strength and toughness. In addition, the cold heading machine usually adopts a continuous, multi-station automated production mode, which can complete multiple processes sequentially on one device and has high production efficiency. However, during the cold heading process, problems such as inadequate deformation control and cracking and breakage of parts may occur.
[0003] Therefore, the above situation needs to be resolved urgently. Utility Model Content
[0004] Purpose of the utility model: In order to overcome the above shortcomings, the utility model provides a cold heading die set which can accurately control the deformation amount at each stage to ensure the quality of parts, and specifically relates to a hexagonal cold heading die set.
[0005] Technical solution: In order to achieve the above-mentioned purpose, a hexagonal cold heading die set includes a first cold heading die, a second cold heading die, a third cold heading die, and a fourth cold heading die. The utility model is also provided with a cutting die in front of the first cold heading die, and the cutting die cuts the raw material according to the set value to form a blank. The conveying mechanism delivers the blank to the first cold heading die, and the first cold heading die upsets a first pre-upsetting surface at one end of the blank, and at the same time upsets a first pre-upsetting hole coaxial with the blank in the center of the first pre-upsetting surface to form a first pre-upsetting piece. The ejector pushes the first pre-upsetting piece out of the first cold heading die, and the conveying mechanism delivers the first pre-upping piece to the second cold heading die. The second cold heading die forges a first positioning hole coaxial with the first pre-forging piece at one end of the first pre-forging piece away from the first pre-forging surface, the second cold heading die forges a second positioning hole at the center of the first pre-forging hole, and the second cold heading die forms a second pre-forging surface at the position of the first pre-forging surface to form a second pre-forging piece. The ejector pushes the second pre-forging piece out of the second cold heading die, and the conveying mechanism delivers the second pre-forging piece to the third cold heading die. The third cold heading die forges a first step at one end of the second pre-forging surface of the second pre-forging piece, the third cold heading die forges a second pre-forging hole at one end of the second pre-forging piece away from the second positioning hole, and the third cold heading die forges a third positioning hole at the bottom surface of the second pre-forging hole to form a third pre-forging piece. The ejector pin pushes the third pre-forging piece out of the third cold heading die, and the conveying mechanism delivers the third pre-forging piece to the fourth cold heading die. The fourth cold heading die forges the second step on the side of the first step of the third pre-forging piece, and at the same time, the fourth cold heading die forges the hexagon socket at the position of the third positioning hole to form a finished product. The ejector pin pushes the finished product out of the fourth cold heading die, and the processing is completed. In order to ensure that the multi-segment cold heading process is correctly aligned with the previous step, the punch can be accurately positioned to avoid displacement during the forging process, which affects the product quality and the life of the die, the utility model has a hexagon socket cold heading die set with positioning holes on the blank starting from the second cold heading die, ensuring that the cold heading is carried out accurately in each step, guaranteeing product quality, and extending the service life of the die. The utility model discloses a hexagonal cold heading die set that distributes the cold heading process, so that the blank is gradually deformed, and the local deformation resistance in each upsetting process is reduced, so that the subsequent forming steps are easier to carry out, and the cracking and breaking of parts caused by uneven stress distribution caused by one-time forming are avoided. The staged cold heading can more accurately control the size and shape of the final product. And the step-by-step cold heading can help improve the internal organizational structure of the blank, so that the metal grains are continuously distributed along the axial direction, thereby improving the mechanical properties of the final product, such as strength and toughness. At the same time, the staged cold heading can disperse the total deformation to the entire cold heading die set, which can effectively extend the service life of the die and reduce the pressure on the cold heading machine.
[0006] Furthermore, in the above-mentioned hexagonal cold heading die set, the first cold heading die includes a first main die and a first punch. The first main die includes a first main die shell, the interior of the first main die shell is a stepped hole, and the stepped holes are divided into an upper stepped hole of the first main die shell, a middle stepped hole of the first main die shell, and a lower stepped hole of the first main die shell, and the upper stepped hole of the first main die shell, the middle stepped hole of the first main die shell, and the lower stepped hole of the first main die shell are arranged in sequence from top to bottom. The upper stepped hole of the first main die shell is an inverted cone-shaped through hole. The upper stepped hole of the first main die shell is provided with a first upper die core and a first lower die core, and the first upper die core and the first lower die core are arranged in sequence up and down. The cross-section of the first upper die core is a cone adapted to the upper stepped hole of the first main die shell, and the cross-section of the first lower die core is a cone adapted to the upper stepped hole of the first main die shell. The first lower die core and the first upper die core constitute a first die cavity, and the blank is cold headed in the first die cavity. A first core is arranged in the stepped hole in the first main mold shell, and the upper side of the first core is in conflict with the lower side of the first lower mold core. The upper end diameter of the first core is larger than the lower end diameter of the first core to form a first core step. The upper end of the first core is arranged in the stepped hole in the first main mold shell, and the lower end of the first core is arranged in the lower stepped hole of the first main mold shell. The first core step is arranged in the lower stepped hole of the first main mold shell. The lower stepped hole of the first main mold shell is a threaded hole, and a first fastener is arranged in the lower stepped hole of the first main mold shell. The outer side of the first fastener is threaded, and the first fastener is sleeved on the lower end of the first core. The lower stepped hole of the first main mold shell and the first fastener are threadedly connected, and the first fastener squeezes the first core step on the outer side of the first core. The first core fixes the first upper mold core and the first lower mold core in the upper stepped hole of the first main mold shell. A first cushion block is arranged on the lower side of the first fastener, and the first cushion block supports the first fastener. A first ejector rod is passed through the cushion block, and one end of the first ejector rod passes through the first core and is placed in the first mold cavity. The first punch rod is penetrated by the first punch die, and the first punch is provided at the lower end of the first punch rod. The first punch rod and the first punch die are slidably connected, and the first punch rod slides in the first punch die to drive the first punch to cold upset the blank. The blank is upset in the first die cavity, and the upper end of the first push rod is tapered, and the lower end of the blank is squeezed by the upper end of the first push rod to form a first pre-upset hole.
[0007] Furthermore, in the above-mentioned hexagonal cold heading die set, in order to forge the first pre-forging surface, the inner diameter of the first upper die core is greater than the inner diameter of the first lower die core, and the first lower die core is provided with a first molding surface on the upper side, so that the first core sleeve can fix the first upper die core and the first lower die core in the stepped hole on the first main mold shell, the superimposed thickness of the first upper die core and the first lower die core is greater than the depth of the stepped hole on the first main mold shell. The distance from the first core sleeve step to the upper end face of the first core sleeve is greater than the depth of the stepped hole in the first main mold shell.
[0008] Furthermore, in the above-mentioned hexagonal cold heading die set, the second cold heading die includes a second main die and a second punch. The second main die includes a second main mold shell, and the interior of the second main mold shell is a stepped hole. The stepped holes are divided into an upper stepped hole of the second main mold shell, a middle stepped hole of the second main mold shell, and a lower stepped hole of the second main mold shell. The upper stepped hole of the second main mold shell, the middle stepped hole of the second main mold shell, and the lower stepped hole of the second main mold shell are arranged in sequence from top to bottom. The upper stepped hole of the second main mold shell is an inverted cone through hole. A second upper mold core and a second lower mold core are arranged in sequence up and down. The cross section of the second upper mold core is a cone that is adapted to the upper stepped hole of the second main mold shell, and the cross section of the second lower mold core is a cone that is adapted to the upper stepped hole of the second main mold shell. The second upper mold core and the second lower mold core constitute a second mold cavity, and the first pre-forged piece is cold headed in the second mold cavity. A second core is provided in the stepped hole in the second main mold shell. The upper side of the second core is in conflict with the lower side of the second lower mold core. The upper end diameter of the second core is larger than the lower end diameter of the second core to form a second core step. The upper end of the second core is provided in the stepped hole in the second main mold shell, and the lower end of the second core is provided in the lower stepped hole of the second main mold shell. The second core step is provided in the lower stepped hole of the second main mold shell. The lower stepped hole of the second main mold shell is a threaded hole. A second fastener is provided in the lower stepped hole of the second main mold shell. The outer side of the second fastener is threaded. The second fastener is sleeved on the lower end of the second core. The lower stepped hole of the second main mold shell is threadedly connected with the second fastener. The second fastener squeezes the second core step provided on the second core. The second core fixes the second upper mold core and the second lower mold core in the upper stepped hole of the second main mold shell. A second cushion block is provided on the lower side of the second fastener, and the second cushion block supports the second fastener. A second ejector rod is passed through the second cushion block, and one end of the second ejector rod passes through the second core and is placed in the second mold cavity. The second die is penetrated by a second punch rod, and a second punch is provided at the lower end of the second punch rod. The second punch rod slides in the second die, driving the second punch to cold-forge the first pre-forged piece. The first pre-forged piece is upset in the second die cavity. At the same time, a positioning drill is provided at the upper end of the second push rod, and the lower end of the first pre-forged piece is squeezed by the positioning drill to form a second positioning hole. A positioning drill is provided at the lower end of the second punch, and the upper end of the first pre-forged piece is squeezed by the positioning drill at the lower end of the second punch to form a first positioning hole.
[0009] Furthermore, in the above-mentioned hexagonal cold heading die set, in order to forge the second pre-forging surface, the inner diameter of the second upper die core is larger than the inner diameter of the second lower die core, and a second forming surface is provided on the upper side of the second lower die core. In order for the second core set to be able to fix the second upper die core and the second lower die core in the stepped hole on the second main mold shell, the superimposed thickness of the second upper die core and the second lower die core is greater than the depth of the stepped hole on the second main mold shell. The distance from the second core set step to the upper end face of the second core set is greater than the depth of the stepped hole in the second main mold shell.
[0010] Further, in the above-mentioned hexagonal cold heading die set, the third cold heading die includes a third main die and a third punch. The third main die includes a third main die shell, the interior of the third main die shell is a stepped hole, and the stepped holes are divided into an upper stepped hole of the third main die shell, a middle stepped hole of the third main die shell, and a lower stepped hole of the third main die shell, and the upper stepped hole of the third main die shell, the middle stepped hole of the third main die shell, and the lower stepped hole of the third main die shell are arranged in sequence from top to bottom. The upper stepped hole of the third main die shell is an inverted cone through hole. The upper stepped hole of the third main die shell is provided with a third upper die core and a third lower die core, and the third upper die core and the third lower die core are arranged in sequence up and down, and the cross section of the third upper die core is a cone adapted to the upper stepped hole of the third main die shell, and the cross section of the third lower die core is a cone adapted to the upper stepped hole of the third main die shell. The third upper die core and the third lower die core constitute a third die cavity, and the second pre-forged piece is cold headed in the third die cavity. A third core is provided in the stepped hole in the third main mold shell, the upper side of the third core is in conflict with the lower side of the third lower mold core, and the upper end diameter of the third core is greater than the lower end diameter of the third core to form a third core step. The upper end of the third core is provided in the stepped hole in the third main mold shell, and the lower end of the third core is provided in the lower stepped hole of the third main mold shell. The third core step is provided in the lower stepped hole of the third main mold shell. The lower stepped hole of the third main mold shell is a threaded hole, and a third fastener is provided in the lower stepped hole of the third main mold shell. The outer side of the third fastener is threaded, and the third fastener is sleeved on the lower end of the third core. The lower stepped hole of the third main mold shell and the third fastener are threadedly connected, and the third fastener squeezes the third core step provided on the third core, and the third fastener squeezes the third core step provided on the third core, and the third core fixes the third upper mold core and the third lower mold core in the upper stepped hole of the third main mold shell. A third cushion block is provided on the lower side of the third fastener, and the third cushion block supports the third fastener. The third pad is penetrated by a third push rod, and one end of the third push rod passes through the third sleeve and is placed in the third die cavity. The third punch rod is penetrated by a third punch rod, and a third punch is provided at the lower end of the third punch rod. A third guide column is provided on the outer side of the third punch rod. The third punch rod can slide in the guide column, thereby driving the third punch to cold-forge the second pre-forging piece. The second pre-forging piece is forged in the third die cavity, and at the same time, the upper end of the third push rod is conical, and the lower end of the first pre-forging piece is squeezed by the upper end of the third push rod to form a pre-forging surface, and the third punch punches the top end of the second pre-forging piece to form a second pre-forging hole.
[0011] Furthermore, in the above-mentioned hexagonal cold heading die set, in order to reduce the diameter of the lower end of the second pre-forging piece and form the first step, the inner diameter of the third lower die core is smaller than the inner diameter of the third upper die core to form a step. In order for the third core set to be able to fix the third upper die core and the third lower die core in the stepped hole on the third main mold shell, the superimposed thickness of the third upper die core and the third lower die core is greater than the depth of the stepped hole on the third main mold shell. The distance from the third core set step to the upper end face of the third core set is greater than the depth of the stepped hole in the third main mold shell.
[0012] Further, in the above-mentioned hexagonal cold heading die set, the fourth cold heading die includes a fourth main die and a fourth punch. The fourth main die includes a fourth main die shell, the interior of the fourth main die shell is a stepped hole, and the stepped holes are divided into an upper stepped hole of the fourth main die shell, a middle stepped hole of the fourth main die shell, and a lower stepped hole of the fourth main die shell, and the upper stepped hole of the fourth main die shell, the middle stepped hole of the fourth main die shell, and the lower stepped hole of the fourth main die shell are arranged in sequence from top to bottom. The upper stepped hole of the fourth main die shell is an inverted cone through hole. The upper stepped hole of the fourth main die shell is provided with a fourth upper die core and a fourth lower die core, and the fourth upper die core and the fourth lower die core are arranged in sequence up and down, and the cross section of the fourth upper die core is a cone adapted to the upper stepped hole of the fourth main die shell, and the cross section of the fourth lower die core is a cone adapted to the upper stepped hole of the fourth main die shell. The fourth upper die core and the fourth lower die core constitute a fourth die cavity, and the third pre-forged piece is cold headed in the fourth die cavity. A fourth core is provided in the stepped hole in the fourth main mold shell, the upper side of the fourth core is in conflict with the lower side of the fourth lower mold core, and the upper end diameter of the fourth core is greater than the lower end diameter of the fourth core to form a fourth core step. The upper end of the fourth core is provided in the stepped hole in the fourth main mold shell, and the lower end of the fourth core is provided in the lower stepped hole of the fourth main mold shell. The fourth core step is provided in the lower stepped hole of the fourth main mold shell. The lower stepped hole of the fourth main mold shell is a threaded hole, and a fourth fastener is provided in the lower stepped hole of the fourth main mold shell. The outer side of the fourth fastener is threaded, and the fourth fastener is sleeved on the lower end of the fourth core. The lower stepped hole of the fourth main mold shell and the fourth fastener are threadedly connected, and the fourth fastener squeezes the fourth core step provided on the fourth core, and the fourth fastener squeezes the fourth core step provided on the fourth core, and the fourth core fixes the fourth upper mold core and the fourth lower mold core in the upper stepped hole of the fourth main mold shell. A fourth cushion block is provided on the lower side of the fourth fastener, and the fourth cushion block supports the fourth fastener. The fourth pad is provided with a fourth push rod, one end of which passes through the fourth sleeve core and is placed in the fourth die cavity. The fourth punch rod is provided with a fourth punch rod, the lower end of the fourth punch rod is provided with a fourth punch, the outer side of the fourth punch rod is provided with a fourth guide column, the fourth punch rod slides in the fourth punch die through the fourth guide column, and then drives the fourth punch to cold-forge the third pre-forging piece. The fourth punch performs stamping and forming on the top of the third pre-forging piece.
[0013] Furthermore, in the above-mentioned hexagonal cold heading die set, in order to further reduce the diameter of the bottom end of the third pre-forging piece and form a second step, the inner diameter of the fourth lower die core is smaller than the inner diameter of the fourth upper die core to form a step. A fourth inner die core is provided inside the fourth lower die core, the inner diameter of the fourth inner die core is smaller than the inner diameter of the fourth lower die core, and the height of the fourth inner die core is smaller than the height of the fourth lower die core to form a step. In order for the fourth core sleeve to be able to fix the fourth upper die core and the fourth lower die core in the stepped hole on the fourth main mold shell, the superimposed thickness of the fourth upper die core and the fourth lower die core is greater than the depth of the stepped hole on the fourth main mold shell. The distance from the fourth core sleeve step to the upper end face of the third core sleeve is greater than the depth of the stepped hole in the fourth main mold shell.
[0014] Furthermore, in the above-mentioned hexagonal cold heading die set, the upper end of the second pre-forging hole is a tapered hole, and the lower end of the second pre-forging hole is a countersunk hole.
[0015] It can be seen from the above technical scheme that the utility model has the following beneficial effects: the utility model hexagonal cold heading die set distributes the cold heading process, so that the blank is gradually deformed, and the local deformation resistance in each upsetting process is reduced, making the subsequent forming steps easier to carry out, avoiding the cracking and breaking of parts caused by uneven stress distribution caused by one-time forming, and staged cold heading can more accurately control the size and shape of the final product. And cold heading in steps can help improve the internal organizational structure of the blank, so that the metal grains are continuously distributed along the axial direction, thereby improving the mechanical properties of the final product, such as strength and toughness. At the same time, staged cold heading can disperse the total deformation to the entire cold heading die set, which can effectively extend the service life of the die and reduce the pressure on the cold heading machine. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a process diagram of a hexagonal cold heading die set of the utility model;
[0017] Figure 2 This is a die diagram of a hexagonal cold heading die set of the utility model;
[0018] Figure 3 This is a cross-sectional view of the first cold heading die of the utility model;
[0019] Figure 4 This is a cross-sectional view of the second cold heading die of the utility model;
[0020] Figure 5 This is a cross-sectional view of the third cold heading die of the utility model;
[0021] Figure 6 This is a cross-sectional view of the fourth cold heading die of the utility model;
[0022] In the figure: 1, first cold heading die, 100, blank, 110 first pre-heading piece, 111, first pre-heading surface, 112, first pre-heading hole, 120, second pre-heading piece, 123, second pre-heading surface, 130, third pre-heading piece, 131, first step, 132, second pre-heading hole, 133, third positioning hole, 140, finished product, 141, second step, 142, hexagon socket, 2, second cold heading die, 3, third cold heading die, 4, fourth cold heading die, 5, cutting die, 11, main die, 101, first main mold shell, 102, first cushion block, 103, first ejector pin, 12, first punch, 121, first punch rod, 122, first punch, 114, first sleeve core, 1141, first sleeve core step, 115, first upper mold core, 116, first lower mold core, 1161, first molding surface, 117, first mold cavity, 1181, upper stepped hole of first main mold shell, 1182, middle stepped hole of first main mold shell, 1183, lower stepped hole of first main mold shell, 119, first fastener, 21, second main mold, 211, second main mold shell, 212, second cushion block, 213, second ejector pin, 214, second core sleeve, 2141, second core sleeve step, 215, second upper mold core, 216, second lower mold core, 2161, second molding surface, 217, second mold cavity, 2181, upper stepped hole of second main mold shell, 2182, middle stepped hole of second main mold shell, 2183, lower stepped hole of second main mold shell, 219, second fastener, 22, second punch, 221, second punch rod, 222, second punch, 31, third main mold, 311, third main mold shell, 312, third cushion block, 313, third ejector pin, 314, third core sleeve, 3141, third core sleeve step, 315, third upper mold core, 316, third lower mold core, 317, third mold cavity, 3181, upper stepped hole of third main mold shell, 3182, middle stepped hole of third main mold shell, 3183, lower stepped hole of third main mold shell, 319, third fastener, 32, third punch, 321, third punch rod, 3211, third punch, 3212, third guide column, 41, fourth main mold, 411. fourth main mold shell, 412. fourth cushion block, 413. fourth ejector pin, 414. fourth sleeve core, 4141. fourth sleeve core step, 415. fourth upper mold core, 416. fourth lower mold core, 4161. fourth inner mold core, 417. fourth mold cavity, 4181. fourth upper stepped hole of main mold shell, 4182. fourth middle stepped hole of main mold shell, 4183. fourth lower stepped hole of main mold shell, 419. fourth fastener, 42. fourth punch, 421. fourth punch rod, 4211. fourth punch, 4212. fourth guide column. DETAILED DESCRIPTION
[0023] Example 1
[0024] like Figure 1-2The hexagonal cold heading die set shown in the figure comprises a first cold heading die 1, a second cold heading die 2, a third cold heading die 3, and a fourth cold heading die 4. The utility model is further provided with a cutting die 5 in front of the first cold heading die 1, and the cutting die 5 cuts the raw material according to the set value to form a blank 100. The conveying mechanism delivers the blank 100 to the first cold heading die 1, and the first cold heading die 1 forges a first pre-forging surface 111 at one end of the blank 100, and at the same time forges a first pre-forging hole 112 coaxial with the blank 100 at the center of the first pre-forging surface 111, to form a first pre-forging piece 110. The ejector pushes the first pre-forging piece 110 out of the first cold heading die 1, and the conveying mechanism delivers the first pre-forging piece 110 to the second cold heading die 2. The second cold heading die 2 forges a first positioning hole coaxial with the first pre-forging piece 110 at one end of the first pre-forging piece 110 away from the first pre-forging surface 111, and the second cold heading die 2 forges a second positioning hole at the center of the first pre-forging hole 112. The second cold heading die 2 forms a second pre-forging surface 123 at the position of the first pre-forging surface 111, forming a second pre-forging piece 120. The ejector pushes the second pre-forging piece 120 out of the second cold heading die 2, and the conveying mechanism delivers the second pre-forging piece 120 to the third cold heading die 3. The third cold heading die 3 forges a first step 131 at one end of the second pre-forging surface 123 of the second pre-forging piece 120, and the third cold heading die 3 forges a second pre-forging hole 132 at one end of the second pre-forging piece 120 away from the second positioning hole. The upper end of the second pre-forging hole 132 is a tapered hole, and the lower end of the second pre-forging hole 132 is a countersunk hole. The third cold heading die 3 forges a third positioning hole 133 at the bottom surface of the second pre-forging hole 132 to form a third pre-forging piece 130. The ejector pushes the third pre-forging piece 130 out of the third cold heading die 3, and the conveying mechanism delivers the third pre-forging piece 130 to the fourth cold heading die 4. The fourth cold heading die 4 forges a second step 141 on one side of the first step 131 of the third pre-forging piece 130, and at the same time, the fourth cold heading die 4 forges a hexagon socket 142 at the third positioning hole 133 to form a finished product 140. The ejector pushes the finished product out of the fourth cold heading die 4 to complete the processing.
[0025] like Figure 3A hexagonal cold heading die set is shown, and the first cold heading die 1 includes a first main die 11 and a first punch die 12. The first main die 11 includes a first main die shell 101, and the first main die shell 101 has a stepped hole inside. The stepped hole is divided into an upper stepped hole 1181 of the first main die shell, a middle stepped hole 1182 of the first main die shell, and a lower stepped hole 1183 of the first main die shell. The upper stepped hole 1181 of the first main die shell, the middle stepped hole 1182 of the first main die shell, and the lower stepped hole 1183 of the first main die shell are arranged in sequence from top to bottom. The upper stepped hole 1181 of the first main die shell is an inverted cone-shaped through hole. The upper stepped hole 1181 of the first main die shell is provided with a first upper die core 115 and a first lower die core 116, and the first upper die core 115 and the first lower die core 116 are arranged in sequence from top to bottom. The cross section of the first upper mold core 115 is a cone adapted to the upper stepped hole 1181 of the first main mold shell, and the cross section of the first lower mold core 116 is a cone adapted to the upper stepped hole 1181 of the first main mold shell. The first upper mold core 115 and the first lower mold core 116 constitute a first mold cavity 117, and the blank 100 is cold headed in the first mold cavity 117. The first sleeve core 114 is arranged in the stepped hole 1182 in the first main mold shell, and the upper side of the first sleeve core 114 abuts against the lower side of the first lower mold core 116. The upper end diameter of the first sleeve core 114 is larger than the lower end diameter of the first sleeve core 114 to form a first sleeve core step 1141. The upper end of the first sleeve core 114 is arranged in the stepped hole 1182 in the first main mold shell, and the lower end of the first sleeve core 114 is arranged in the lower stepped hole 1183 of the first main mold shell. The first sleeve core step 1141 is arranged in the lower stepped hole 1183 of the first main mold shell. The lower stepped hole 1183 of the first main mold shell is a threaded hole. A first fastener 119 is disposed in the lower stepped hole 1183 of the first main mold shell. The outer side of the first fastener 119 is threaded. The first fastener 119 is sleeved on the lower end of the first core sleeve 114. The lower stepped hole 1183 of the first main mold shell and the first fastener 119 are threadedly connected. The first fastener 119 squeezes the first core sleeve step 1141 on the outer side of the first core sleeve 114. The first core sleeve 114 fixes the first upper mold core 115 and the first lower mold core 116 in the upper stepped hole 1181 of the first main mold shell. A first cushion block 102 is disposed on the lower side of the first fastener 119. The first cushion block 102 supports the first fastener 119. A first ejector rod 103 is passed through the first cushion block 102. One end of the first ejector rod 103 passes through the first core sleeve 114 and is placed in the first mold cavity 117. The first punch rod 121 is penetrated by the first punch rod 121, and the first punch 122 is provided at the lower end of the first punch rod 121. The first punch rod 121 and the first punch die 12 are slidably connected, and the first punch rod 121 slides in the first punch die 12, driving the first punch 122 to cold upset the blank 100. The blank 100 is upset in the first die cavity 117, and at the same time, the upper end of the first push rod 103 is tapered, and the lower end of the blank 100 is squeezed by the upper end of the first push rod 103 to form a first pre-upset hole 112.In order to upset the first pre-upset surface 111, the inner diameter of the first upper mold core 115 is larger than the inner diameter of the first lower mold core 116, and the first lower mold core 116 is provided with a first molding surface 1161 on the upper side. In order for the first core sleeve 114 to fix the first upper mold core 115 and the first lower mold core 116 in the stepped hole 1181 on the first main mold shell, the superimposed thickness of the first upper mold core 115 and the first lower mold core 116 is greater than the depth of the stepped hole 1181 on the first main mold shell. The distance from the first core sleeve step 1141 to the upper end surface of the first core sleeve 114 is greater than the depth of the stepped hole 1182 in the first main mold shell.
[0026] like Figure 4In the illustrated hexagonal cold heading die set, the second cold heading die 2 includes a second main die 21 and a second punch die 22. The second main die 21 includes a second main die shell 211, and the second main die shell 211 has a stepped hole inside, which is divided into an upper stepped hole 2181 of the second main die shell, a middle stepped hole 2182 of the second main die shell, and a lower stepped hole 2183 of the second main die shell. The upper stepped hole 2181 of the second main die shell, the middle stepped hole 2182 of the second main die shell, and the lower stepped hole 2183 of the second main die shell are arranged in sequence from top to bottom. The upper stepped hole 2181 of the second main die shell is an inverted tapered through hole. A second upper mold core 215 and a second lower mold core 216 are arranged in the stepped hole 2181 on the second main mold shell. The second upper mold core 215 and the second lower mold core 216 are arranged in sequence up and down. The cross section of the second upper mold core 215 is a cone adapted to the stepped hole 2181 on the second main mold shell, and the cross section of the second lower mold core 216 is a cone adapted to the stepped hole 2181 on the second main mold shell. The second upper mold core 215 and the second lower mold core 216 form a second mold cavity 217, and the first pre-forging piece 110 is cold-forged in the second mold cavity 217. A second sleeve core 214 is arranged in the stepped hole 2182 in the second main mold shell. The upper side of the second sleeve core 214 abuts against the lower side of the second lower mold core 216. The upper end diameter of the second sleeve core 214 is larger than the lower end diameter of the second sleeve core 214 to form a second sleeve core step 2141. The upper end of the second core sleeve 214 is arranged in the stepped hole 2182 in the second main mold shell, and the lower end of the second core sleeve 214 is arranged in the lower stepped hole 2183 of the second main mold shell. The second core sleeve step 2141 is arranged in the lower stepped hole 2183 of the second main mold shell, and the lower stepped hole 2183 of the second main mold shell is a threaded hole. A second fastener 219 is arranged in the lower stepped hole 2183 of the second main mold shell, and the outer side of the second fastener 219 is threaded. The second fastener 219 is sleeved on the lower end of the second core sleeve 214, and the lower stepped hole 2183 of the second main mold shell and the second fastener 219 are threadedly connected. The second fastener 219 squeezes the second core sleeve step 2141 provided on the second core sleeve 214, and the second core sleeve 214 fixes the second upper mold core 215 and the second lower mold core 216 in the upper stepped hole 2181 of the second main mold shell. A second cushion block 212 is provided at the lower side of the second fastener 219, and the second cushion block 212 supports the second fastener 219. A second push rod 213 is penetrated by the second cushion block 212, and one end of the second push rod 213 passes through the second sleeve core 214 and is placed in the second die cavity 217. A second punch rod 221 is penetrated by the second die 22, and a second punch 222 is provided at the lower end of the second punch rod 221. The second punch rod 221 slides in the second die 22, driving the second punch 222 to cold-forge the first pre-forging piece 110, and the first pre-forging piece 110 is upset in the second die cavity 217. At the same time, a positioning drill is provided at the upper end of the second push rod 213, and the lower end of the first pre-forging piece 110 is squeezed by the positioning drill to form a second positioning hole. A positioning drill is provided at the lower end of the second punch 222, and the upper end of the first pre-forging piece 110 is squeezed by the positioning drill at the lower end of the second punch 222 to form a first positioning hole.In order to upset the second pre-upset surface 123, the inner diameter of the second upper mold core 215 is larger than the inner diameter of the second lower mold core 216, and a second molding surface 2161 is provided on the upper side of the second lower mold core 216. In order for the second core sleeve 214 to fix the second upper mold core 215 and the second lower mold core 216 in the stepped hole 2181 on the second main mold shell, the superimposed thickness of the second upper mold core 215 and the second lower mold core 216 is greater than the depth of the stepped hole 2181 on the second main mold shell. The distance from the second core sleeve step 2141 to the upper end surface of the second core sleeve 214 is greater than the depth of the stepped hole 2182 in the second main mold shell.
[0027] like Figure 5In the illustrated hexagonal cold heading die set, the third cold heading die 3 includes a third main die 31 and a third punch die 32. The third main die 31 includes a third main die shell 311, the interior of the third main die shell 311 is a stepped hole, and the stepped hole is divided into an upper stepped hole 3181 of the third main die shell, a middle stepped hole 3182 of the third main die shell, and a lower stepped hole 3183 of the third main die shell, and the upper stepped hole 3181 of the third main die shell, the middle stepped hole 3182 of the third main die shell, and the lower stepped hole 3183 of the third main die shell are arranged in sequence from top to bottom. The upper stepped hole 3181 of the third main die shell is an inverted tapered through hole. A third upper mold core 315 and a third lower mold core 316 are arranged in the stepped hole 3181 on the third main mold shell. The third upper mold core 315 and the third lower mold core 316 are arranged in sequence up and down. The cross section of the third upper mold core 315 is a cone adapted to the stepped hole 3181 on the third main mold shell. The cross section of the third lower mold core 316 is a cone adapted to the stepped hole 3181 on the third main mold shell. The third upper mold core 315 and the third lower mold core 316 form a third mold cavity 317. The second pre-forging piece 120 is cold-forged in the third mold cavity 317. A third sleeve core 314 is arranged in the stepped hole 3182 in the third main mold shell. The upper side of the third sleeve core 314 abuts against the lower side of the third lower mold core 316. The upper end diameter of the third sleeve core 314 is larger than the lower end diameter of the third sleeve core 314 to form a third sleeve core step 3141. The upper end of the third core 314 is arranged in the stepped hole 3182 in the third main mold shell, and the lower end of the third core 314 is arranged in the lower stepped hole 3183 in the third main mold shell. The third core step 3141 is arranged in the lower stepped hole 3183 in the third main mold shell. The lower stepped hole 3183 in the third main mold shell is a threaded hole, and a third fastener 319 is arranged in the lower stepped hole 3183 in the third main mold shell. The outer side of the third fastener 319 is threaded, and the third fastener 319 is sleeved on the lower end of the third core 314. The lower stepped hole 3183 in the third main mold shell and the third fastener 319 are threadedly connected. The third fastener 319 squeezes the third core step 3141 provided on the third core 314, and the third core 314 fixes the third upper mold core 315 and the third lower mold core 316 in the upper stepped hole 3181 in the third main mold shell. A third cushion block 312 is provided at the lower side of the third fastener 319, and the third cushion block 312 supports the third fastener 319. A third push rod 313 is passed through the third cushion block 312, and one end of the third push rod 313 passes through the third sleeve core 314 and is placed in the third die cavity 317. A third punch rod 321 is passed through the third die 32, and a third punch 3211 is provided at the lower end of the third punch rod 321. A third guide column 3212 is provided on the outer side of the third punch rod 321, and the third punch rod 321 can slide in the third guide column 3212, thereby driving the third punch 3211 to cold-forge the second pre-forging piece 120. The second pre-upsetting piece 120 is upset in the third die cavity 317 , and the upper end of the third push rod 313 is tapered. The lower end of the first pre-upsetting piece 110 is squeezed by the upper end of the third push rod 313 to form a pre-upsetting surface. The third punch 3211 punches the top of the second pre-upsetting piece 120 to form a second pre-upsetting hole 132 .In order to reduce the diameter of the lower end of the second pre-forging piece 120 and form the first step 131, the inner diameter of the third lower mold core 316 is smaller than the inner diameter of the third upper mold core 315 to form a step. In order for the third core sleeve 314 to fix the third upper mold core 315 and the third lower mold core 316 in the stepped hole 3181 on the third main mold shell, the superimposed thickness of the third upper mold core 315 and the third lower mold core 316 is greater than the depth of the stepped hole 3181 on the third main mold shell. The distance from the third core sleeve step 3141 to the upper end surface of the third core sleeve 314 is greater than the depth of the stepped hole 3182 in the third main mold shell.
[0028] like Figure 6In the illustrated hexagonal cold heading die set, the fourth cold heading die 4 includes a fourth main die 41 and a fourth punch die 42. The fourth main die 41 includes a fourth main die shell 411, the interior of the fourth main die shell 411 is a stepped hole, and the stepped hole is divided into a fourth main die shell upper stepped hole 4181, a fourth main die shell middle stepped hole 4182, and a fourth main die shell lower stepped hole 4183. The fourth main die shell upper stepped hole 4181, the fourth main die shell middle stepped hole 4182, and the fourth main die shell lower stepped hole 4183 are arranged sequentially from top to bottom. The fourth main die shell upper stepped hole 4181 is an inverted tapered through hole. A fourth upper mold core 415 and a fourth lower mold core 416 are arranged in the stepped hole 4181 on the fourth main mold shell. The fourth upper mold core 415 and the fourth lower mold core 416 are arranged in sequence up and down. The cross section of the fourth upper mold core 415 is a cone adapted to the stepped hole 4181 on the fourth main mold shell. The cross section of the fourth lower mold core 416 is a cone adapted to the stepped hole 4181 on the fourth main mold shell. The fourth upper mold core 415 and the fourth lower mold core 416 form a fourth mold cavity 417. The third pre-forging piece 130 is cold-forged in the fourth mold cavity 417. A fourth sleeve core 414 is arranged in the stepped hole 4182 in the fourth main mold shell. The upper side of the fourth sleeve core 414 abuts against the lower side of the fourth lower mold core 416. The upper end diameter of the fourth sleeve core 414 is greater than the lower end diameter of the fourth sleeve core 414 to form a fourth sleeve core step 4141. The upper end of the fourth core 414 is arranged in the stepped hole 4182 in the fourth main mold shell, and the lower end of the fourth core 414 is arranged in the lower stepped hole 4183 of the fourth main mold shell. The fourth core step 4141 is arranged in the lower stepped hole 4183 of the fourth main mold shell. The lower stepped hole 4183 of the fourth main mold shell is a threaded hole, and a fourth fastener 419 is arranged in the lower stepped hole 4183 of the fourth main mold shell. The outer side of the fourth fastener 419 is threaded, and the fourth fastener 419 is sleeved on the lower end of the fourth core 414. The lower stepped hole 4183 of the fourth main mold shell and the fourth fastener 419 are threadedly connected. The fourth fastener 419 squeezes the fourth core step 4141 provided on the fourth core 414, and the fourth core 414 fixes the fourth upper mold core 415 and the fourth lower mold core 416 in the upper stepped hole 4181 of the fourth main mold shell. A fourth cushion block 412 is provided at the lower side of the fourth fastener 419, and the fourth cushion block 412 supports the fourth fastener 419. A fourth push rod 413 is passed through the fourth cushion block 412, and one end of the fourth push rod 413 passes through the fourth sleeve core 414 and is placed in the fourth die cavity 417. A fourth punch rod 421 is passed through the fourth die 42, and a fourth punch 4211 is provided at the lower end of the fourth punch rod 421. A fourth guide column 4212 is provided on the outer side of the fourth punch rod 421. The fourth punch rod 421 slides in the fourth die 42 through the fourth guide column 4212, thereby driving the fourth punch 4211 to cold-forge the third pre-forging piece 130. The fourth punch 4211 performs stamping and forming on the top of the third pre-forging piece 130. In order to further reduce the diameter of the bottom end of the third pre-forging piece 130 to form a second step 141, the inner diameter of the fourth lower die core 416 is smaller than the inner diameter of the fourth upper die core 415 to form a step.A fourth inner mold core 4161 is provided inside the fourth lower mold core 416, and the inner diameter of the fourth inner mold core 4161 is smaller than the inner diameter of the fourth lower mold core 416, and the height of the fourth inner mold core 4161 is smaller than the height of the fourth lower mold core 416, forming a step. In order for the fourth core sleeve 414 to fix the fourth upper mold core 415 and the fourth lower mold core 416 in the stepped hole 4181 on the fourth main mold shell, the superimposed thickness of the fourth upper mold core 415 and the fourth lower mold core 416 is greater than the depth of the stepped hole 4181 on the fourth main mold shell. The distance from the fourth core sleeve step 4141 to the upper end surface of the fourth core sleeve 414 is greater than the depth of the stepped hole 4182 in the fourth main mold shell.
[0029] The above embodiments are exemplary, and their purpose is to illustrate the technical concept and features of the utility model so that people familiar with this field can understand the content of the utility model and implement it accordingly, and they cannot be used to limit the protection scope of the utility model. Any equivalent changes or modifications made according to the spirit of the utility model should be included in the protection scope of the utility model.
Claims
1. A hexagonal cold heading die set, Features: The invention comprises a first cold heading die (1), a second cold heading die (2), a third cold heading die (3), and a fourth cold heading die (4); the first cold heading die (1) forges a first pre-forging surface (111) at one end of a blank (100), and simultaneously forges a first pre-forging hole (112) coaxial with the blank (100) at the center of the first pre-forging surface (111), thereby forming a first pre-forging piece (110); the second cold heading die (2) forges a first positioning hole coaxial with the first pre-forging piece (110) at one end of the first pre-forging piece (110) away from the first pre-forging surface (111), the second cold heading die (2) forges a second positioning hole at the center of the first pre-forging hole (112), and the second cold heading die (2) forges a second pre-forging surface (121) at one end of the first pre-forging surface (111). 3), forming a second pre-forging piece (120); the third cold forging die (3) forges a first step (131) at one end of the second pre-forging surface (123) of the second pre-forging piece (120), the third cold forging die (3) forges a second pre-forging hole (132) at one end of the second pre-forging piece (120) away from the second positioning hole, and the third cold forging die (3) forges a third positioning hole (133) at the bottom surface of the second pre-forging hole (132), thereby forming a third pre-forging piece (130); the fourth cold forging die (4) forges a second step (141) at one side of the first step (131) of the third pre-forging piece (130), and at the same time, the fourth cold forging die (4) forges an inner hexagon (142) at the position of the third positioning hole (133), thereby forming a finished product (140).
2. A hexagonal cold heading die set according to claim 1, Features: The first cold heading die (1) comprises a first main die (11) and a first punching die (12); the first main die (11) comprises a first main die shell (101); the first main die shell (101) has a stepped hole inside, the stepped hole is divided into a first main die shell upper stepped hole (1181), a first main die shell middle stepped hole (1182), and a first main die shell lower stepped hole (1183); the first main die shell upper stepped hole (1181), the first main die shell middle stepped hole (1182), and the first main die shell lower stepped hole (1183) are arranged in sequence from top to bottom; the first main die shell upper stepped hole (1181) is an inverted tapered through hole; the first main die shell upper stepped hole (1181) is a ... 1181) is provided with a first upper mold core (115) and a first lower mold core (116), and the first upper mold core (115) and the first lower mold core (116) are arranged in sequence from top to bottom; the cross section of the first upper mold core (115) is a cone that is adapted to the stepped hole (1181) on the first main mold shell, and the cross section of the first lower mold core (116) is a cone that is adapted to the stepped hole (1181) on the first main mold shell. The first upper mold core (115) and the first lower mold core (116) form a first mold cavity (117), and the blank (100) is cold headed in the first mold cavity (117); a first sleeve core (114) is provided in the stepped hole (1182) in the first main mold shell, The upper side of the first sleeve core (114) abuts against the lower side of the first lower mold core (116); the diameter of the upper end of the first sleeve core (114) is larger than the diameter of the lower end of the first sleeve core (114) to form a first sleeve core step (1141); the upper end of the first sleeve core (114) is arranged in the stepped hole (1182) in the first main mold shell; the lower end of the first sleeve core (114) is arranged in the lower stepped hole (1183) of the first main mold shell; the first sleeve core step (1141) is arranged in the lower stepped hole (1183) of the first main mold shell; the lower stepped hole (1183) of the first main mold shell is a threaded hole; a first fastener (119) is arranged in the lower stepped hole (1183) of the first main mold shell; the first fastener (119) 119) is threaded on the outside, the first fastener (119) is sleeved on the lower end of the first core sleeve (114), the lower stepped hole (1183) of the first main mold shell and the first fastener (119) are threadedly connected, and the first fastener (119) squeezes the first core sleeve step (1141) on the outside of the first core sleeve (114); a first cushion block (102) is provided on the lower side of the first fastener (119), and the first cushion block (102) supports the first fastener (119); a first push rod (103) is passed through the first cushion block (102), and one end of the first push rod (103) passes through the first core sleeve (114) and is placed in the first mold cavity (117);The first punching die (12) is provided with a first punch rod (121), a first punch (122) is provided at the lower end of the first punch rod (121), the first punch rod (121) and the first punching die (12) are slidably connected, the first punch rod (121) slides in the first punching die (12), and drives the first punch (122) to perform cold heading on the blank (100).
3. A hexagonal cold heading die set according to claim 2, Features: The inner diameter of the first upper mold core (115) is greater than the inner diameter of the first lower mold core (116); a first molding surface (1161) is provided on the upper side of the first lower mold core (116); the superimposed thickness of the first upper mold core (115) and the first lower mold core (116) is greater than the depth of the stepped hole (1181) on the first main mold shell; and the distance from the first sleeve core step (1141) to the upper end surface of the first sleeve core (114) is greater than the depth of the stepped hole (1182) in the first main mold shell.
4. The hexagonal cold heading die set according to claim 1, Features: The second cold heading die (2) comprises a second main die (21) and a second punch die (22); the second main die (21) comprises a second main die shell (211); the second main die shell (211) has a stepped hole inside, the stepped hole is divided into a second main die shell upper stepped hole (2181), a second main die shell middle stepped hole (2182), and a second main die shell lower stepped hole (2183); the second main die shell upper stepped hole (2181), the second main die shell middle stepped hole (2182), and the second main die shell lower stepped hole (2183) are arranged in sequence from top to bottom; the second main die shell upper stepped hole (2181) is an inverted cone-shaped through hole; the second main die shell upper stepped hole (2181) is provided with a second upper die core (215), a second lower die core (216), and a second lower die core (217). 16), the second upper mold core (215) and the second lower mold core (216) are arranged in sequence from top to bottom, the cross section of the second upper mold core (215) is a cone adapted to the stepped hole (2181) on the second main mold shell, and the cross section of the second lower mold core (216) is a cone adapted to the stepped hole (2181) on the second main mold shell; the second upper mold core (215) and the second lower mold core (216) form a second mold cavity (217), and the first pre-forging piece (110) is cold-forged in the second mold cavity (217); a second sleeve core (214) is arranged in the stepped hole (2182) in the second main mold shell, the upper side of the second sleeve core (214) abuts against the lower side of the second lower mold core (216), and the upper end diameter of the second sleeve core (214) is larger than that of the second sleeve core (214). ) forms a second core step (2141) at the lower end diameter; the upper end of the second core (214) is arranged in the stepped hole (2182) in the second main mold shell; the lower end of the second core (214) is arranged in the lower stepped hole (2183) in the second main mold shell; the second core step (2141) is arranged in the lower stepped hole (2183) in the second main mold shell; the lower stepped hole (2183) in the second main mold shell is a threaded hole; a second fastener (219) is arranged in the lower stepped hole (2183) in the second main mold shell; the outer side of the second fastener (219) is threaded; the second fastener (219) is sleeved on the lower end of the second core (214); the lower stepped hole (2183) in the second main mold shell is threadedly connected to the second fastener (219); the second fastener (219) The second core step (2141) provided on the second core (214) is squeezed by the second fastener (219); a second cushion block (212) is provided on the lower side of the second fastener (219), and the second cushion block (212) supports the second fastener (219); a second push rod (213) is passed through the second cushion block (212), and one end of the second push rod (213) passes through the second core (214) and is placed in the second die cavity (217); a second punch rod (221) is passed through the second die (22), and a second punch (222) is provided at the lower end of the second punch rod (221), and the second punch rod (221) slides in the second die (22) to drive the second punch (222) to cold-forge the first pre-forging piece (110).
5. A hexagonal cold heading die set according to claim 4, Features: The inner diameter of the second upper mold core (215) is greater than the inner diameter of the second lower mold core (216); a second molding surface (2161) is provided on the upper side of the second lower mold core (216); the superimposed thickness of the second upper mold core (215) and the second lower mold core (216) is greater than the depth of the stepped hole (2181) on the second main mold shell; and the distance from the second sleeve core step (2141) to the upper end surface of the second sleeve core (214) is greater than the depth of the stepped hole (2182) in the second main mold shell.
6. A hexagonal cold heading die set according to claim 1, Features: The third cold heading die (3) comprises a third main die (31) and a third punch die (32); the third main die (31) comprises a third main die shell (311); the interior of the third main die shell (311) is a stepped hole, and the stepped hole is divided into an upper stepped hole (3181) of the third main die shell, a middle stepped hole (3182) of the third main die shell, and a lower stepped hole (3183) of the third main die shell; the upper stepped hole (3181) of the third main die shell, the middle stepped hole (3182) of the third main die shell, and the lower stepped hole (3183) of the third main die shell are arranged in sequence from top to bottom; the upper stepped hole (3181) of the third main die shell is an inverted cone-shaped through hole; the upper stepped hole (3181) of the third main die shell is provided with a third upper die core (315), a third lower die core (316), and a third lower die core (317). 16), the third upper mold core (315) and the third lower mold core (316) are arranged in sequence from top to bottom, the cross section of the third upper mold core (315) is a cone adapted to the stepped hole (3181) on the third main mold shell, and the cross section of the third lower mold core (316) is a cone adapted to the stepped hole (3181) on the third main mold shell; the third upper mold core (315) and the third lower mold core (316) form a third mold cavity (317), and the second pre-forging piece (120) is cold-forged in the third mold cavity (317); a third sleeve core (314) is arranged in the stepped hole (3182) in the third main mold shell, the upper side of the third sleeve core (314) abuts against the lower side of the third lower mold core (316), and the upper end diameter of the third sleeve core (314) is larger than the diameter of the third sleeve core (314). ) is formed with a third core step (3141) at the lower end diameter; the upper end of the third core (314) is arranged in the stepped hole (3182) in the third main mold shell; the lower end of the third core (314) is arranged in the lower stepped hole (3183) in the third main mold shell; the lower stepped hole (3183) in the third main mold shell is a threaded hole; a third fastener (319) is arranged in the lower stepped hole (3183) in the third main mold shell; the outer side of the third fastener (319) is threaded; the third fastener (319) is sleeved on the lower end of the third core (314); the lower stepped hole (3183) in the third main mold shell and the third fastener (319) are threadedly connected; the third fastener (319) extrudes the third core step (3141) provided on the third core (314) A third cushion block (312) is provided at the lower side of the third fastener (319), and the third cushion block (312) supports the third fastener (319); a third push rod (313) is passed through the third cushion block (312), and one end of the third push rod (313) passes through the third sleeve core (314) and is placed in the third die cavity (317); a third punch rod (321) is passed through the third die (32), and a third punch (3211) is provided at the lower end of the third punch rod (321), and a third guide column (3212) is provided on the outer side of the third punch rod (321), and the third punch rod (321) can slide in the third guide column (3212), thereby driving the third punch (3211) to cold-forge the second pre-forging piece (120).
7. A hexagonal cold heading die set according to claim 6, Features: The inner diameter of the third lower mold core (316) is smaller than the inner diameter of the third upper mold core (315) to form a step; the superimposed thickness of the third upper mold core (315) and the third lower mold core (316) is greater than the depth of the stepped hole (3181) on the third main mold shell; and the distance from the third sleeve core step (3141) to the upper end surface of the third sleeve core (314) is greater than the depth of the stepped hole (3182) in the third main mold shell.
8. The hexagonal cold heading die set according to claim 1, Features: The fourth cold heading die (4) comprises a fourth main die (41) and a fourth punch die (42); the fourth main die (41) comprises a fourth main die shell (411); the fourth main die shell (411) has a stepped hole inside, the stepped hole is divided into a fourth main die shell upper stepped hole (4181), a fourth main die shell middle stepped hole (4182), and a fourth main die shell lower stepped hole (4183); the fourth main die shell upper stepped hole (4181), the fourth main die shell middle stepped hole (4182), and the fourth main die shell lower stepped hole (4183) are arranged in sequence from top to bottom; the fourth main die shell upper stepped hole (4181) is an inverted tapered through hole; the fourth A fourth upper mold core (415) and a fourth lower mold core (416) are arranged in the stepped hole (4181) on the main mold shell. The fourth upper mold core (415) and the fourth lower mold core (416) are arranged in sequence from top to bottom. The cross section of the fourth upper mold core (415) is a cone that is adapted to the stepped hole (4181) on the fourth main mold shell. The cross section of the fourth lower mold core (416) is a cone that is adapted to the stepped hole (4181) on the fourth main mold shell. The fourth upper mold core (415) and the fourth lower mold core (416) form a fourth mold cavity (417). The third pre-forging piece (130) is cold-forged in the fourth mold cavity (417). The stepped hole ( A fourth sleeve core (414) is provided in the mold body 4182, the upper side of the fourth sleeve core (414) abuts against the lower side of the fourth lower mold core (416), the upper end diameter of the fourth sleeve core (414) is larger than the lower end diameter of the fourth sleeve core (414) to form a fourth sleeve core step (4141), the upper end of the fourth sleeve core (414) is provided in the stepped hole (4182) in the fourth main mold shell, and the lower end of the fourth sleeve core (414) is provided in the lower stepped hole (4183) of the fourth main mold shell; the lower stepped hole (4183) of the fourth main mold shell is a threaded hole, the lower stepped hole (4183) of the fourth main mold shell is provided in the fourth fastener (419), and the outer side of the fourth fastener (419) is The fourth fastener (419) is sleeved on the lower end of the fourth core sleeve (414), the lower stepped hole (4183) of the fourth main mold shell and the fourth fastener (419) are threadedly connected, and the fourth fastener (419) squeezes the fourth core sleeve step (4141) provided on the fourth core sleeve (414); a fourth cushion block (412) is provided on the lower side of the fourth fastener (419), and the fourth cushion block (412) supports the fourth fastener (419); a fourth push rod (413) is passed through the fourth cushion block (412), and one end of the fourth push rod (413) passes through the fourth core sleeve (414) and is placed in the fourth mold cavity (417);The fourth punching die (42) is provided with a fourth punch rod (421), a fourth punch (4211) is provided at the lower end of the fourth punch rod (421), a fourth guide column (4212) is provided on the outer side of the fourth punch rod (421), and the fourth punch rod (421) slides in the fourth punching die (42) via the fourth guide column (4212), thereby driving the fourth punch (4211) to perform cold forging on the third pre-forging piece (130). ; 9. A hexagonal cold heading die set according to claim 8, Features: The inner diameter of the fourth lower mold core (416) is smaller than the inner diameter of the fourth upper mold core (415), forming a step; the fourth lower mold core (416) is provided with a fourth inner mold core (4161) inside, the inner diameter of the fourth inner mold core (4161) is smaller than the inner diameter of the fourth lower mold core (416), and the height of the fourth inner mold core (4161) is smaller than the height of the fourth lower mold core (416), forming a step; the superimposed thickness of the fourth upper mold core (415) and the fourth lower mold core (416) is greater than the depth of the stepped hole (4181) on the fourth main mold shell; the distance from the fourth sleeve core step (4141) to the upper end surface of the fourth sleeve core (414) is greater than the depth of the stepped hole (4182) in the fourth main mold shell.
10. The hexagonal cold heading die set according to claim 1, Features: The upper end of the second pre-upsetting hole (132) is a tapered hole, and the lower end of the second pre-upsetting hole (132) is a countersunk hole.