Cool-feeling anti-sticking polyester fabric
By designing anti-stick grooves, breathable holes and wet dissipation grooves in polyester fabrics, combined with bamboo charcoal yarn and cool yarn, the problem of poor breathability of polyester fabrics after absorbing sweat is solved, and the breathability and comfort of the fabrics are improved Spend.
Patent Information
- Application Number
- CN202420277645.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-05
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-02-05
AI Technical Summary
Polyester fabrics have poor breathability after absorbing sweat, which causes the fabric to stick to the skin to affect the comfort of wearing.
A cool-sensing anti-stick polyester fabric is designed, including the inner layer and the outer layer. The inner layer is equipped with acute triangle anti-stick grooves and breathable holes. The outer layer is equipped with dispersed grooves and breathable holes. The anti-stick dispersed strips are used. Improve stiffness and breathability, reduce the contact area between the inner layer and the skin, and enhance the air exchange rate.
It improves the breathability and quick-drying performance of the fabric, reduces the time the fabric is in wet state, and enhances wear comfort.
Smart Images

Figure CN221913586U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of fabrics, and more specifically, to a cool and anti-sticking polyester fabric. Background Art
[0002] Polyester is a fiber with good elasticity and high strength. Polyester fabric is crisp and has good shape retention. It is a widely used and high-consumption fiber.
[0003] Polyester fabric is woven by warp and weft of polyester composite yarn, and the characteristics of polyester material are used to make daily necessities such as clothing and accessories.
[0004] Summer clothing will continuously absorb sweat from the user's body surface during wearing, especially during exercise or high temperatures. The sweat continuously discharged from the human skin will be absorbed by the fabric, and the pores on the fabric soaked with sweat will be blocked. Polyester fiber, as a chemical fiber, has poor air permeability, which causes a large amount of fabric to accumulate between the skin and the fabric. The fabric will stick to the skin, affecting the comfort of wearing.
[0005] Therefore, new solutions need to be proposed to solve this problem. Utility Model Content
[0006] In view of the shortcomings of the prior art, the utility model aims to provide a cool and anti-sticking polyester fabric.
[0007] The above-mentioned technical purpose of the utility model is achieved through the following technical scheme: the cool and anti-sticking polyester fabric comprises an inner layer and an outer layer fixedly connected to each other, a plurality of anti-sticking grooves are provided on the end surface of the inner layer away from the outer layer, and the cross-sectional shape of the anti-sticking groove is set to an acute triangle, a plurality of air holes 1 are provided on the end surface of the inner layer, and a plurality of anti-sticking and moisture-dissipating strips are fixedly connected to the inner layer, the anti-sticking and moisture-dissipating strips are interspersed in the air hole 1, and a plurality of the anti-sticking and moisture-dissipating strips float on the end surfaces of both sides of the inner layer, and the anti-sticking and moisture-dissipating strips are staggered with the anti-sticking grooves; a plurality of moisture-dissipating grooves are provided on the end surface of the outer layer close to the inner layer, and a plurality of the anti-sticking and moisture-dissipating strips extend into the moisture-dissipating grooves, and a plurality of air holes 2 are provided at the bottom of the moisture-dissipating grooves.
[0008] The utility model is further configured as follows: the stiffness of the anti-sticking and moisture-dissipating strip is greater than the stiffness of the inner layer and the outer layer.
[0009] The utility model is further configured as follows: the anti-sticking and moisture-dissipating strip is configured as bamboo charcoal yarn, and the yarn count of the anti-sticking and moisture-dissipating strip is less than 16S and greater than 12S.
[0010] The utility model is further configured as follows: the warp and weft yarns of the inner layer are configured as cool yarns, and the warp and weft yarns of the outer layer are configured as breathable and moisture-dissipating yarns.
[0011] The utility model is further configured as follows: the inner layer is configured as a mountain twill, and the outer layer is configured as a plain weave.
[0012] The utility model is further configured as follows: the cool yarn is composed of a yarn core and a covering yarn spirally wound on the outside thereof, the yarn core is formed by twisting a plurality of polyester fibers, and the covering yarn is formed by twisting a plurality of jade fibers.
[0013] The utility model is further configured as follows: the breathable and moisture-dissipating yarn is formed by twisting a first strand and a second strand, the first strand is formed by twisting a plurality of ramie fibers, the second strand is formed by twisting a plurality of polyester shaped fibers, and the cross-section of the polyester shaped fibers is configured to be plum blossom-shaped.
[0014] In summary, the utility model has the following beneficial effects: the contact area between the inner layer and the skin is reduced by the anti-sticking grooves provided on the inner layer and the anti-sticking and moisture-dissipating strips floating on the two side end surfaces of the inner layer, and the stability of the inner layer when reducing the contact area with the skin is improved by strengthening the stiffness of the anti-sticking and moisture-dissipating strips, and the air permeability 1 and the air permeability 2 provided on the inner layer and the outer layer respectively are connected to the moisture-dissipating grooves, thereby improving the air exchange rate between the inside and outside air of the fabric, improving the overall air permeability and quick-drying of the fabric, thereby reducing the time that the fabric is in a wet state, reducing the time that the fabric fits the skin, and improving the wearing comfort of the fabric. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the structure of the utility model;
[0016] Figure 2 It is a cross-sectional view of the utility model;
[0017] Figure 3 This is a slice diagram of the cool yarn of the utility model;
[0018] Figure 4 This is a cross-sectional view of the breathable and moisture-dissipating yarn of the utility model.
[0019] In the figure: 1. Outer layer; 101. Moisture dissipation groove; 102. Second ventilation hole; 2. Inner layer; 201. Anti-sticking groove; 202. First ventilation hole; 3. Anti-sticking moisture dissipation strip; 4. Cool yarn; 5. Polyester fiber; 6. Jade fiber; 7. Breathable moisture dissipation yarn; 8. Ramie fiber; 9. Polyester special-shaped fiber. DETAILED DESCRIPTION
[0020] The utility model is described in detail below in conjunction with the accompanying drawings and embodiments.
[0021] Cool and stick-resistant polyester fabric, such as Figure 1 and Figure 2As shown, it comprises an inner layer 2 and an outer layer 1 fixedly connected to each other, a plurality of anti-sticking grooves 201 are provided on the end surface of the inner layer 2 away from the outer layer 1, and the cross-sectional shape of the anti-sticking grooves 201 is set to an acute triangle, a plurality of air holes 202 are provided on the end surface of the inner layer 2, a plurality of anti-sticking and moisture dissipating strips 3 are also fixedly connected to the inner layer 2, the anti-sticking and moisture dissipating strips 3 are inserted in the air holes 202, and a plurality of anti-sticking and moisture dissipating strips 3 float on the end surfaces of both sides of the inner layer 2, and a plurality of moisture dissipating grooves 101 are provided on the end surface of the outer layer 1 close to the inner layer 2, and a plurality of anti-sticking and moisture dissipating strips 3 extend into the moisture dissipating grooves 101. A plurality of air holes 102 are provided at the bottom of the moisture dissipation groove 101, and the air holes on the inner layer 2 are connected to the moisture dissipation groove 101. The air exchange rate between the inside and outside air of the fabric is provided by providing the air holes 1 202 and the air holes 2 102, thereby improving the overall ventilation effect of the fabric. The opening of the anti-sticking groove 201 reduces the contact area between the inner layer 2 and the skin, reduces the contact area between the fabric and the skin when it is in a wet state, and improves the actual comfort of the fabric. The anti-sticking and moisture dissipation strip 3 reduces the contact area between the inner layer 2 and the skin, and improves the overall anti-sticking property of the fabric.
[0022] like Figure 1 , Figure 2 and Figure 3As shown, the warp and weft yarns of the inner layer 2 are set as cool yarns 4, and a number of polyester fibers 5 and jade fibers 6 are respectively put into a twisting machine for twisting to form a yarn core and a covering yarn. The yarn core and the covering yarn are processed by a spindle spinning process, and the covering yarn is spirally wound on the outer side of the yarn core to obtain the cool yarn 4. The high strength and good elasticity of the polyester fiber 5 and the cooling and cooling characteristics of the jade fiber 6 are utilized to ensure that the inner layer 2 has good structural strength, elasticity and cool and refreshing characteristics, and the cool yarn 4 is fed into the jet In the loom, the inner layer 2 with twill lines on the fabric surface continuously forming a peak shape is woven in a orderly and stable manner according to the organization of the mountain-shaped twill organization. The twill with a change in the mountain-shaped pattern can better prevent sticking than the plain weave. The inner layer 2 is rolled up and hot-pressed by a hot press to obtain a plurality of anti-sticking grooves 201, and the cross-sectional shape of the hot-pressing part of the hot press is set to a triangle. When the inner layer 2 is rolled down, the hot-pressed part of the inner layer 2 generates a rebound deformation to form an acute-angled triangle with an oblique cross-section. While reducing the contact area between the inner layer 2 and the skin in this way, the triangular cross-section has the characteristics of structural stability, which improves the overall structural strength of the inner layer 2. A laser punching machine is used to laser punch a plurality of air holes 202 on the end surface of the inner layer 2. The air holes 202 are arranged along the length direction of the anti-sticking groove 201. The anti-sticking and moisture-dispersing strip 3 is set to bamboo charcoal yarn, and the yarn count of the anti-sticking and moisture-dispersing strip 3 is 12S-14S. The anti-sticking and moisture-dispersing strip 3 is impregnated with a fabric stiffening agent. The anti-sticking and moisture-dissipating strip 3 is fixed to the inner layer 2 by glue or sewing with a sewing machine. The stiffness and count of the anti-sticking and moisture-dissipating strip 3 are used to reduce the area of direct contact between the inner layer 2 and the skin, thereby improving the overall anti-sticking effect of the fabric. The air permeability and moisture dissipation characteristics of the bamboo charcoal yarn are used to improve the overall air permeability and moisture dissipation effect of the fabric. The processing and production of the inner layer 2 is now completed.
[0023] like Figure 1 , Figure 2 and Figure 4As shown, the warp and weft yarns of the outer layer 1 are set as breathable and moisture-dissipating yarns 7, and a plurality of ramie fibers 8 and polyester shaped fibers 9 are respectively put into a twisting machine for twisting to form a first strand and a second strand, and the first strand and the second strand are put into the twisting machine for twisting to obtain the breathable and moisture-dissipating yarn 7, wherein the cross section of the polyester shaped fiber 9 is set to a plum blossom shape, which has the characteristics of moisture absorption and quick drying, and the grooves on the surface can increase the specific surface area, which is conducive to the evaporation of water, so that the fabric has the performance of quick drying, and combined with the good moisture absorption and moisture dissipation of the ramie fiber 8, the outer layer 1 can better absorb the sweat absorbed by the inner layer 2 It absorbs moisture and dissipates it to improve the overall moisture dissipation and quick-drying performance of the fabric. The high strength and good elasticity of the polyester fiber 5 are used to ensure that the outer layer 1 has good structural strength and elasticity. The breathable and moisture-dissipating yarn 7 is fed into the air-jet loom, and the outer layer 1 with a strong texture is woven sequentially according to the structure of the plain weave. A hot press is used to hot-press a plurality of moisture-dissipating grooves 101 on one end face of the outer layer 1, and the groove width of the moisture-dissipating groove 101 is greater than the width of the anti-sticking moisture-dissipating strip 3. A laser punching machine is used to laser-punch a plurality of breathable holes 102 at the bottom of the moisture-dissipating groove 101, thereby completing the processing and production of the outer layer 1.
[0024] like Figure 1 and Figure 2 As shown, the end face of the inner layer 2 with the anti-sticking groove 201 is facing downward and laid flat on a workbench, the end face of the outer layer 1 with the moisture-dissipating groove 101 is facing the inner layer 2 and is close to the inner layer 2, the anti-sticking and moisture-dissipating strip 3 is extended into the moisture-dissipating groove 101, and the outer layer 1 is in contact with the inner layer 2, and the inner layer 2 and the outer layer 1 are fixedly connected by sewing with a sewing machine or gluing, thereby completing the processing and production of the cool anti-sticking polyester fabric.
[0025] The above is only a preferred embodiment of the present invention. The protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A cool and anti-sticking polyester fabric, comprising an inner layer (2) and an outer layer (1) fixedly connected to each other, characterized in that: The end surface of the inner layer (2) away from the outer layer (1) is provided with a plurality of anti-sticking grooves (201), the cross-sectional shape of the anti-sticking grooves (201) is set to be an acute triangle, the end surface of the inner layer (2) is provided with a plurality of air holes (202), the inner layer (2) is also fixedly connected with a plurality of anti-sticking and moisture dissipating strips (3), the anti-sticking and moisture dissipating strips (3) are inserted in the air holes (202), a plurality of the anti-sticking and moisture dissipating strips (3) float on the end surfaces of both sides of the inner layer (2), the anti-sticking and moisture dissipating strips (3) and the anti-sticking grooves (201) are arranged alternately, the end surface of the outer layer (1) close to the inner layer (2) is provided with a plurality of moisture dissipating grooves (101), a plurality of the anti-sticking and moisture dissipating strips (3) extend into the moisture dissipating grooves (101), and a plurality of air holes (102) are provided at the bottom of the moisture dissipating grooves (101).
2. The cool and anti-sticking polyester fabric according to claim 1, characterized in that: The stiffness of the anti-sticking and moisture-dissipating strip (3) is greater than the stiffness of the inner layer (2) and the outer layer (1).
3. The cool and anti-sticking polyester fabric according to claim 2, characterized in that: The anti-sticking and moisture-dissipating strip (3) is configured as bamboo charcoal yarn, and the yarn count of the anti-sticking and moisture-dissipating strip (3) is less than 16S and greater than 12S.
4. The cool and stick-resistant polyester fabric according to claim 1, characterized in that: The warp and weft yarns of the inner layer (2) are configured as cool yarns (4), and the warp and weft yarns of the outer layer (1) are configured as breathable and moisture-dissipating yarns (7).
5. The cool and stick-resistant polyester fabric according to claim 1, characterized in that: The inner layer (2) is configured as a mountain twill weave, and the outer layer (1) is configured as a plain weave.
6. The cool and stick-resistant polyester fabric according to claim 4, characterized in that: The cool yarn (4) is composed of a yarn core and a covering yarn spirally wound on the outside thereof, wherein the yarn core is formed by twisting a plurality of polyester fibers (5), and the covering yarn is formed by twisting a plurality of jade fibers (6).
7. The cool and stick-resistant polyester fabric according to claim 4, characterized in that: The breathable and moisture-dissipating yarn (7) is formed by twisting a first strand and a second strand, wherein the first strand is formed by twisting a plurality of ramie fibers (8), and the second strand is formed by twisting a plurality of polyester shaped fibers (9), wherein the cross section of the polyester shaped fibers (9) is arranged to be plum blossom-shaped.