Hard AF film
By introducing a silicon nitride hard layer and an indirect layer into the AF film layer, the problem that the existing AF film is easy to scratch and fall off is solved, and a high hardness and wear-resistant hard AF film is achieved, which is suitable for a variety of glass panels. .
Patent Information
- Application Number
- CN202420242034.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-01
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-02-01
AI Technical Summary
The existing AF film layer lacks hard materials, making the display prone to scratches and falling off after frequent friction.
Silicon nitride is used as the hard layer, and indirect layers are provided above and below it. The hard AF film is formed through magnetron sputtering or evaporation processes to ensure the high hardness and scratch resistance of the film body.
A high-hardness hard AF film is achieved, which can effectively resist scratches, maintain optical performance, is suitable for a variety of glass panels, and significantly improves the wear resistance and waterproof performance of the film layer.
Smart Images

Figure CN221917819U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a protective film, in particular to a hard AF film. Background Art
[0002] Display screens are prone to scratches during use. For example, the glass panels on mobile phones, cars, TVs and other objects rub against sharp objects, causing scratches on the glass panels and affecting the appearance. To this end, R&D personnel coat the surface of the display screen to form an AF film layer, but with the frequent friction between the display screen (glass panels on mobile phones, cars, TVs and other objects) and objects (pockets, fingers), the AF film layer on the glass cover will eventually fall off.
[0003] To prevent the AF film from falling off, SiO 2 or Al 2 O 3 The primer is combined with AF waterproof pills to produce better waterproof and anti-scratch effects. However, this film structure lacks hard materials, and the display screen is prone to scratches. For example, the Chinese patent with application number 2023106464278 discloses a hard film and its preparation method. The technical solution disclosed is to use SiO 2 or Al 2 O 3 The base is laid, and then the AF layer is set on the top, lacking a hard material layer. For example, the Chinese patent with application number 2023102894559 discloses a method for making a super-hard scratch-resistant coating cover plate and a cover plate. The disclosed technical solution uses one of aluminum carbide, chromium carbide, silicon carbide, and niobium carbide as a super-hard scratch-resistant layer on a non-metallic connecting layer. In order to obtain better test results and optical effects, this application has been improved and optimized based on the existing technology, thereby obtaining a better hard film.
[0004] Therefore, those skilled in the art provide a hard AF film to solve the problems raised in the above background technology. Utility Model Content
[0005] The purpose of the utility model is to provide a hard AF film, which can effectively resist scratches and avoid scratches on the display screen by using silicon nitride as a hard layer, so as to solve the problems raised in the above background technology.
[0006] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0007] A hard AF film comprises a substrate and an AF layer arranged opposite to the substrate, wherein a hard layer is stacked between the substrate and the AF layer, and the hard layer is silicon nitride.
[0008] As a further solution of the utility model: an indirect layer is further provided above or below the hard layer.
[0009] As a further solution of the utility model: the indirect layer is a metal or non-metallic coating material;
[0010] If it is a metal coating material, the indirect layer can be AL 2 O 3 ;
[0011] If it is a non-metallic coating material, the indirect layer can be SiO 2 / Si.
[0012] As a further solution of the utility model: the number of stacked layers of silicon nitride is at least 2, and the thickness of the stacked hard layer is ≤3000nm.
[0013] As a further solution of the present invention: the thickness of the indirect layer is ≥2nm.
[0014] As a further solution of the utility model: the hard layer and the indirect layer are both arranged on the substrate by using magnetron sputtering or evaporation process.
[0015] As a further solution of the utility model: the AF layer is deposited on the surface of the hard layer or the indirect layer by evaporating or spraying AF.
[0016] As a further solution of the utility model: the thickness of the indirect layer is less than the thickness of the hard layer.
[0017] Compared with the prior art, the beneficial effects of the utility model are:
[0018] 1. In this application, silicon nitride is used as a hard layer, which has a high hardness characteristic; the overall film hardness is high, the Mohs hardness of the film is ≥6, the nanoindentation is ≥15, and the Vickers hardness is ≥1500;
[0019] 2. Able to maintain the original optical benchmark, haze ≤ 0.18%, B value ≤ 1.2 (CM3600), transmittance 550nm ≥ 89%;
[0020] 3. The membrane has good rubber friction effect and can withstand the following test: rubber friction ≥ 4200 times (load 1kg, ) Water drop angle ≥100°, steel wool friction ≥4200 times (load 1kg, 1*1cm) Water drop angle ≥90°, alkali sweat resistance 24H ≥100°;
[0021] 4. This hard film is suitable for front and rear glass panels of mobile phones, cars, TVs, wearables, cameras, etc. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1It is a schematic diagram of the structure of the hard AF film with an intermediate layer below the hard layer in the utility model.
[0023] Figure 2 It is a schematic diagram of the structure of the hard AF film in which the intermediate layer is above the hard layer in the utility model.
[0024] In the figure: 1, substrate; 2, indirect layer; 3, hard layer; 4, AF layer. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0026] In the present application, the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "vertical", "horizontal", "lateral", "longitudinal" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings. These terms are mainly used to better describe the present application and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific orientation, or to be constructed and operated in a specific orientation.
[0027] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those of ordinary skill in the art, the specific meanings of these terms in this application can be understood according to specific circumstances.
[0028] In addition, the terms "installed", "set", "provided with", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0029] In addition, the terms "first", "second", etc. are mainly used to distinguish different devices, elements or components (the specific types and structures may be the same or different), and are not used to indicate or imply the relative importance and quantity of the indicated devices, elements or components. Unless otherwise specified, "plurality" means two or more.
[0030] As mentioned in the background technology of this application, the inventors have discovered through research that the existing AF film coating method is to use SiO2 or Al2O3 as a base and combine it with AF waterproof pills. Although this coating method produces better waterproof and anti-scratch effects, this film layer structure lacks hard materials and the display screen is prone to scratches.
[0031] In order to solve the above defects, the present application discloses a hard AF film, which uses silicon nitride as a hard layer with a Mohs hardness of ≥6, can effectively resist scratches and avoid scratches on the display screen, thereby effectively solving the above defects.
[0032] The following will describe in detail how the solution of the present application solves the above technical problems in conjunction with the accompanying drawings.
[0033] See also Figure 1-2 As shown, in the embodiment of the utility model, a hard AF film includes a substrate 1 and an AF layer 4 arranged opposite thereto, a hard layer 3 is stacked between the substrate 1 and the AF layer 4, and the hard layer 3 is silicon nitride. Silicon nitride is used as the hard layer 3, which has a higher Mohs hardness and stronger scratch resistance, and the formed film body is not easily scratched during use. Silicon nitride has the advantages of wear resistance and resistance to cold and hot shocks.
[0034] In this embodiment, an indirect layer 2 is further provided above or below the hard layer 3 .
[0035] In this embodiment: the indirect layer 2 is a metal or non-metal coating material;
[0036] If it is a metal coating material, the indirect layer 2 can be AL 2 O 3 ;
[0037] If it is a non-metallic coating material, the indirect layer 2 can be SiO 2 / Si.
[0038] Using metal or non-metallic coating materials as the indirect layer 2 makes the film structure more solid and the AF layer 4 is not easy to fall off during use. 2 and AL 2 O 3 The chemical properties of Si are relatively stable, it does not react with water, and it has high fire resistance, high temperature resistance, small thermal expansion coefficient, corrosion resistance and unique optical properties. Si has a high melting point (1410℃), high hardness, and relatively stable physical properties.
[0039] In this embodiment: the number of stacked silicon nitride layers is at least 2, and the thickness of the hard layer 3 after stacking is ≤3000nm. If the thickness of the hard layer 3 is too small, the hardness and scratch resistance of the final film will be affected. If the thickness is too large, the stress generated on the substrate 1 is too large, affecting the flatness of the substrate 1, resulting in the film being affected. The thickness of the hard layer 3 is preferably 50nm.
[0040] In this embodiment: the thickness of the indirect layer 2 is ≥ 2 nm. In order to keep the film body ultra-thin, the thickness of the indirect layer 2 is preferably 30 nm.
[0041] In this embodiment, the hard layer 3 and the indirect layer 2 are both disposed on the substrate 1 by using a magnetron sputtering or evaporation process.
[0042] In this embodiment, the AF layer 4 is deposited on the surface of the hard layer 3 or the indirect layer 2 by evaporating or spraying AF.
[0043] In this embodiment, the thickness of the indirect layer 2 is smaller than the thickness of the hard layer 3 .
[0044] The working principle of the utility model is: when preparing the hard AF film, if the indirect layer 2 is set between the hard layer 3 and the AF layer 4, the hard layer 3 is formed by sputtering or evaporating silicon nitride on the preset substrate 1 by magnetron sputtering or evaporation process, and then the metal or non-metallic coating material is sputtered or evaporated on the hard layer 3 by magnetron sputtering or evaporation process to form the indirect layer 2. Finally, AF is deposited on the indirect layer 2 by evaporation or spraying to form the AF layer 4.
[0045] If the indirect layer 2 is disposed between the hard layer 3 and the substrate 1, a metal or non-metallic coating material is sputtered or evaporated on the preset substrate 1 by magnetron sputtering or evaporation process to form the indirect layer 2, and then silicon nitride is sputtered or evaporated on the indirect layer 2 by magnetron sputtering or evaporation process to form the hard layer 3. Finally, AF is deposited on the hard layer 3 by evaporation or spraying to form an AF layer 4.
[0046] The finished hard film formed by the above two methods not only has high hardness and good wear resistance, but also can maintain the original optical reference. It is suitable for glass panels such as mobile phone covers, car covers, and TV covers, and has a wide range of applicability.
[0047] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
[0048] What is described above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes within the technical scope disclosed by the present invention according to the technical scheme and the utility model concept of the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A hard AF film, comprising a substrate (1) and an AF layer (4) arranged opposite to the substrate, characterized in that: A hard layer (3) is stacked between the substrate (1) and the AF layer (4), and the hard layer (3) is silicon nitride.
2. A hard AF film according to claim 1, characterized in that: An indirect layer (2) is also provided above or below the hard layer (3).
3. A hard AF film according to claim 2, characterized in that: The indirect layer (2) is a metal or non-metal coating material; If it is a metal coating material, the indirect layer (2) can be Al2O3; If it is a non-metallic coating material, the indirect layer (2) can be SiO2 / Si.
4. A hard AF film according to any one of claims 1 to 3, characterized in that: The number of stacked silicon nitride layers is at least 2, and the thickness of the hard layer (3) after stacking is ≤3000nm.
5. A hard AF film according to claim 2 or 3, characterized in that: The thickness of the indirect layer (2) is ≥2 nm.
6. The hard AF film according to claim 2, characterized in that: The hard layer (3) and the indirect layer (2) are both arranged on the substrate (1) by using a magnetron sputtering or evaporation process.
7. A hard AF film according to claim 2 or 6, characterized in that: The AF layer (4) is deposited on the surface of the hard layer (3) or the indirect layer (2) by evaporating or spraying AF.
8. The hard AF film according to claim 5, characterized in that: The thickness of the indirect layer (2) is smaller than the thickness of the hard layer (3).
Citation Information
Cited By
High-hardness and high-wear-resistance AF film layer, glass product as well as preparation method and application of high-hardness and high-wear-resistance AF film layer
CN120736810A
AF film layer with high hardness and high wear resistance, glass product, preparation method and application
CN120736810B