Self-adhesive coiled material

By using a multi-layer structure of aluminum film, anti-UV fiber braided layer and graphene fireproof layer in the self-adhesive membrane, the problems of insufficient waterproofing, fireproofing and durability of the existing membrane are solved, achieving higher waterproof performance and Longer service life.

CN221917893UActive Publication Date: 2024-10-29HEBEI JIUSHEN WATERPROOF BUILDING MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420409497.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-04
Publication Date
2024-10-29
Estimated Expiration
2034-03-04

AI Technical Summary

Technical Problem

Existing self-adhesive membranes have shortcomings in waterproof performance, fire resistance and durability, especially high-density polyethylene film and PET polyester film have poor aging resistance and poor dimensional stability, aluminum foil has poor friction resistance and puncture resistance, and PET has poor The aluminized film has poor adhesion, and the asphalt membrane absorbs heat and heats up after exposure to light, causing warping and deformation, which affects its service life.

Method used

An aluminum film is used as the surface layer, and warp and weft woven glass fibers are added to enhance the tensile strength and tear resistance. An anti-UV fiber braided layer and a graphene fireproof layer are set under the surface layer. An anti-aging agent is added to the self-adhesive layer, and polyethylene is used. Vinyl or polyester silicone oil isolation film, forming a multi-layer structure to improve waterproof, fireproof and anti-aging properties.

Benefits of technology

It achieves stronger waterproof and fireproof performance, avoids warping and deformation, extends the service life, and improves the overall performance and bonding durability of the membrane.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221917893U_ABST
    Figure CN221917893U_ABST
Patent Text Reader

Abstract

The utility model discloses a self-adhesive coiled material, which relates to the technical field of coiled materials, and comprises a surface layer, a self-adhesive layer and an isolating membrane, and further comprises isolating layers, the isolating layers comprise a first isolating layer and a second isolating layer, the surface layer, the first isolating layer, the second isolating layer, the self-adhesive layer and the isolating membrane are sequentially arranged from top to bottom, the surface layer is an aluminum membrane, a reinforcing layer is arranged in the aluminum membrane, and the reinforcing layer is made of plastic. The reinforcing layer is formed by weaving glass fibers in a warp-weft mode. The coiled material not only has strong waterproof capability, but also is fireproof and sun-resistant, and cannot be warped and deformed when exposed for use, so that the service life is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of coiled materials, in particular to a self-adhesive coiled material. Background Art

[0002] Among the existing waterproof materials, modified asphalt rolls occupy a large market share, but with the increasingly stringent environmental protection requirements, hot-melt rolls are gradually being restricted. Self-adhesive rolls are becoming more and more popular due to their self-adhesion and cold construction. Self-adhesive rolls are mainly used for base surface waterproofing of various buildings. At present, the main covering materials of self-adhesive rolls on the market are high-density polyethylene film, aluminum foil, PET aluminized film, PET polyester film, etc. Among them, high-density polyethylene film and PET polyester film have poor aging resistance and poor dimensional stability; although PE cross film has strong aging resistance, the surface is easy to wrinkle, and aluminum foil has poor friction resistance and puncture resistance. The two layers of PET aluminized film have poor adhesion, and PET film is also easy to break. These defects affect the promotion and application of self-adhesive rolls to varying degrees.

[0003] In addition, most of these types of self-adhesive rolls have poor waterproof performance. At the same time, most of the rolls do not have a fireproof layer and have poor fireproof performance. In addition, the self-adhesive layer of the roll is an asphalt layer. Asphalt rolls absorb heat and heat up significantly after exposure to light. This will not only cause the asphalt layer to slide and flow after the roll is heated and age too quickly, but also cause the bonded roll to be repeatedly pulled under stress due to thermal expansion and contraction, causing warping and deformation, creating water leakage channels, and making the roll unable to be exposed for use. Utility Model Content

[0004] The utility model aims to provide a self-adhesive coiled material which is not only highly waterproof but also fireproof and sun-resistant and will not produce warping and deformation when used exposedly, thereby increasing the service life.

[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0006] A self-adhesive coiled material comprises a surface layer, a self-adhesive layer and an isolation film, and also comprises an isolation layer, wherein the isolation layer comprises a first isolation layer and a second isolation layer, wherein the surface layer, the first isolation layer, the second isolation layer, the self-adhesive layer and the isolation film are arranged in sequence from top to bottom, wherein the surface layer is an aluminum film, wherein a reinforcement layer is arranged in the aluminum film, and wherein the reinforcement layer is woven with glass fiber in the warp and weft.

[0007] Preferably, the first isolation layer is an anti-ultraviolet fiber woven layer.

[0008] Preferably, the second isolation layer is a fireproof layer.

[0009] Preferably, the fireproof layer is a graphene layer.

[0010] Preferably, the surface layer has a thickness of 0.1-0.3 mm, a gram weight of 70-120 g / ㎡, and a tensile force of not less than 600 n / mm.

[0011] Preferably, the self-adhesive layer is a high molecular polymer modified asphalt self-adhesive compound or a self-adhesive rubber asphalt compound.

[0012] Preferably, the self-adhesive layer includes an anti-aging agent.

[0013] Preferably, the isolation membrane is made of polyethylene or polyester silicone oil isolation membrane.

[0014] Preferably, the isolation film is a silicone-coated polyethylene film with a thickness of 35-45 g / ㎡; the total thickness of the surface layer, the self-adhesive layer and the isolation film is 1.5-2.5 mm.

[0015] In the above technical scheme, by setting the surface layer to a thin film made of pure aluminum, it is possible to isolate and reflect part of the light and heat, thereby achieving the effect of lowering the overall temperature of the coil, which can be reduced by about 20-35°C compared with traditional materials, and the aluminum film also has a certain waterproof performance. Further, by adding warp and weft woven glass fiber to the aluminum film, the glass fiber has a high strength, which not only increases the overall tensile strength and tear resistance of the coil, but also makes the covering not brittle, and can resist the wrinkling and warping caused by the material after heating, while avoiding damage to the aluminum film due to wrinkling, warping and deformation, thereby increasing the waterproof performance and service life of the coil.

[0016] Furthermore, a first isolation layer is connected under the surface layer, and the first isolation layer is an anti-UV fiber woven layer. After the aluminum film on the surface isolates and reflects part of the light and heat, the remaining ultraviolet rays are irradiated onto the anti-UV fiber woven layer and blocked by the anti-UV fiber woven layer. Compared with the method of adding ultraviolet absorbers to the coiled material, the anti-UV fiber woven layer will not become invalid over time. While blocking a certain temperature and a certain amount of ultraviolet rays, it reduces the possibility of high-temperature flow of asphalt, thereby increasing its practical value.

[0017] By setting a second isolation layer under the first isolation layer, the second isolation layer is a fireproof layer, and the material of the fireproof layer is graphene. The heat-conducting layer of graphene material can quickly conduct the local heat received by the surface, thereby effectively further dissipating the local high temperature received by the surface layer, and can also make the local heat of the surface layer dissipate faster, which can greatly improve the fireproof performance of the coiled material and reduce the risk of fire. By adding an anti-aging agent to the self-adhesive layer, the self-adhesive asphalt can maintain good low body temperature flexibility after thermal aging, and extend the low service life of the self-adhesive coiled material due to aging after use, and the physical properties are better and the bonding is more durable. The isolation film is made of polyethylene or polyester silicone oil isolation film. When using it, you only need to tear off the isolation film and attach the coiled material to the position where it needs to be used. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the overall structure of the utility model;

[0019] In the figure, 1 is a surface layer; 21 is a first isolation layer; 22 is a second isolation layer; 3 is a self-adhesive layer; and 4 is an isolation film. DETAILED DESCRIPTION

[0020] The utility model is further described below in conjunction with the accompanying drawings:

[0021] like Figure 1 As shown, the utility model includes a surface layer 1, an isolation layer, a self-adhesive layer 3 and an isolation film 4, the isolation layer includes a first isolation layer 21 and a second isolation layer 22, and the surface layer 1, the first isolation layer 21, the second isolation layer 22, the self-adhesive layer 3 and the isolation film 4 are arranged in sequence from top to bottom.

[0022] The thickness of the surface layer 1 for exposed application is 0.1-0.3mm, the gram weight is 70-120g / ㎡, the tensile force is not less than 600n / mm, and the surface layer 1 is an aluminum film, which can isolate and reflect part of the light and heat, thereby reducing the overall temperature of the coil, which can be reduced by about 20-35℃ compared with traditional materials, and the aluminum film also has certain waterproof properties. Further, by adding warp and weft woven glass fiber to the aluminum film, the glass fiber has a high strength, which not only increases the overall tensile strength and tear resistance of the coil, but also makes the covering not brittle, and can resist the wrinkling and warping caused by the heating of the material, while avoiding the damage of the aluminum film caused by wrinkling, warping and deformation, thereby increasing the waterproof performance and service life of the coil.

[0023] The first isolation layer 21 is an anti-UV fiber woven layer. After the aluminum film of the surface layer 1 isolates and reflects part of the light and heat, the remaining ultraviolet rays are irradiated onto the anti-UV fiber woven layer and blocked by the anti-UV fiber woven layer. Compared with the method of adding ultraviolet absorbers to the coiled material, the anti-UV fiber woven layer will not become invalid over time. While blocking a certain temperature and a certain amount of ultraviolet rays, it reduces the possibility of high-temperature flow of asphalt, thereby increasing the practical value. The first isolation layer 21 and the surface layer 1 are connected by a high-viscosity polymer.

[0024] The second insulating layer 22 is a fireproof layer, and the fireproof layer is a graphene layer. The heat-conducting layer made of graphene can quickly conduct the local heat received by the surface, thereby effectively dissipating the local high temperature received by the surface layer 1, and can also make the local heat of the surface layer 1 dissipate heat faster, which can greatly improve the fireproof performance of the coiled material and reduce the risk of fire. The second insulating layer 22 is connected to the first insulating layer 21 by a high-viscosity polymer.

[0025] The self-adhesive layer 3 is a polymer modified asphalt self-adhesive compound or a self-adhesive rubber asphalt compound, and an anti-aging agent is added to the self-adhesive layer 3, which can make the self-adhesive layer 3 maintain good low body temperature flexibility after thermal aging, and extend the service life of the coiled material due to aging after use, and the physical properties are more excellent and the bonding is more durable. The isolation film 4 is made of polyethylene or polyester silicone oil isolation film, and the preferred isolation film 4 is a 35-45g / ㎡ silicone-coated polyethylene film.

[0026] In this embodiment, the total thickness of the surface layer 1, the self-adhesive layer 3 and the isolation film 4 is 1.5-2.5 mm. When in use, the isolation film is torn off and the roll is attached to the position where it is needed. The width of the sunscreen and anti-wrinkle roll can be made into specifications such as 10 cm, 20 cm, 33 cm, 50 cm, 100 cm, etc. according to needs, which is convenient for use.

[0027] This embodiment is only an illustration of the concept and implementation of the utility model, and does not limit it. Under the concept of the utility model, technical solutions that have not been substantially changed are still within the scope of protection.

Claims

1. A self-adhesive coil, comprising a surface layer, a self-adhesive layer and a release film, It is characterized in that It also includes an isolation layer, which includes a first isolation layer and a second isolation layer. The surface layer, the first isolation layer, the second isolation layer, the self-adhesive layer and the isolation film are arranged in sequence from top to bottom. The surface layer is an aluminum film, and a reinforcement layer is arranged in the aluminum film. The reinforcement layer is woven with glass fiber in warp and weft.

2. The self-adhesive coiled material according to claim 1, It is characterized in that The first isolation layer is an anti-ultraviolet fiber braided layer.

3. The self-adhesive coiled material according to claim 2, It is characterized in that The second isolation layer is a fireproof layer.

4. The self-adhesive roll material according to claim 3, It is characterized in that The fireproof layer is a graphene layer.

5. The self-adhesive roll material according to any one of claims 1 to 4, It is characterized in that The surface layer has a thickness of 0.1-0.3 mm, a gram weight of 70-120 g / ㎡, and a tensile force of not less than 600 n / mm.

6. The self-adhesive roll material according to any one of claims 1 to 4, It is characterized in that The self-adhesive layer is a high molecular polymer modified asphalt self-adhesive compound or a self-adhesive rubber asphalt compound.

7. The self-adhesive roll material according to any one of claims 1 to 4, It is characterized in that The isolation film is made of polyethylene or polyester silicone oil isolation film.

8. The self-adhesive roll material according to claim 7, It is characterized in that The isolation film is a silicone-coated polyethylene film with a thickness of 35-45 g / ㎡; the total thickness of the surface layer, the self-adhesive layer and the isolation film is 1.5-2.5 mm.