Multilayer forming coated paper
Through the multi-layer molded coated paper structure, the problems of high cost and poor print quality in the production of handbag paper are solved, the fiber consumption is reduced and the printing effect is improved, and it has broad application prospects.
Patent Information
- Application Number
- CN202420559108.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-21
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-03-21
AI Technical Summary
The existing handbag paper production process has problems such as high cost, high consumption, and average print quality.
It adopts a multi-layer molded coated paper structure, which consists of top coating, middle coating, pre-coating, surface fiber layer, core fiber layer, bottom fiber layer, and back coating from top to bottom. Through specific layer structures and components Cooperate to achieve reduction in fiber consumption and improvement in printing effect.
It reduces the total amount and cost of fiber, improves printing color difference and layering, saves ink consumption, and improves the thickness and stiffness index by adding high-yield and high-bulk mechanical wood pulp, reducing resource consumption.
Smart Images

Figure CN221918779U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of paper, and more specifically to a multi-layer formed coated paper. Background Art
[0002] With the continuous advancement of plastic restriction and the increasing pressure on environmental protection, more and more plastic bags are replaced by paper bags. At present, the existing paper bag packaging materials in China are generally produced by single-layer paper machines. A large amount of bleached chemical pulp is used in the production process. The mechanical strength, packaging uniformity and flatness of the paper are improved through a low-ash production process. The surface is not coated; it is then coated according to actual needs to obtain coated paper bags that meet customer requirements. However, the coated paper bags disclosed in the prior art have the defects of high cost, high consumption and average printing quality. Utility Model Content
[0003] In view of this, the purpose of the utility model is to provide a multi-layer formed coated paper, which can solve the above-mentioned problems of high cost, high consumption and average quality of printed products.
[0004] The utility model provides a multi-layer formed coated paper, which comprises from top to bottom:
[0005] Top coating, middle coating, pre-coating, top fiber layer, core fiber layer, bottom fiber layer, back coating.
[0006] Preferably, the top coating is a coating composed of calcium carbonate, kaolin, adhesive, water repellent, lubricant, and water retaining agent, with a gram weight of 10 g / m 2 ~12g / m 2 .
[0007] Preferably, the middle coating is a coating composed of calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent, with a gram weight of 6 g / m 2 ~8g / m 2 .
[0008] Preferably, the pre-coating layer is a coating composed of calcium carbonate, adhesive, water repellent, lubricant and water retaining agent, with a gram weight of 14 g / m 2 ~16g / m 2 .
[0009] Preferably, the surface fiber layer is a fiber layer formed by coniferous wood pulp and hardwood wood pulp, with a gram weight of 25g / m 2 ~30g / m 2 .
[0010] Preferably, the core fiber layer is a fiber layer formed by mechanical wood pulp, with a gram weight of 140g / m 2 ~150g / m 2 .
[0011] Preferably, the bottom fiber layer is a fiber layer formed by coniferous wood pulp and hardwood wood pulp, with a gram weight of 20g / m 2 ~24g / m 2 .
[0012] Preferably, the back coating is a coating composed of calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent, with a gram weight of 14 g / m 2 ~16g / m 2 .
[0013] Preferably, the weight of the multilayer coated paper is 200 g / m 2 ~300g / m 2 .
[0014] Preferably, it also includes:
[0015] Starch adhesive layer; the starch adhesive layer is respectively arranged between the pre-coating layer and the surface fiber layer, and between the bottom fiber layer and the back coating layer.
[0016] The utility model provides a multi-layer molded coated paper, especially handbag paper, which comprises from top to bottom: a surface coating, a middle coating, a pre-coating, a surface fiber layer, a core fiber layer, a bottom fiber layer, and a back coating. Compared with the prior art, the multi-layer molded coated paper provided by the utility model adopts a specific layer structure with a specific connection relationship to achieve better overall interaction, and realizes three coatings on the surface fiber layer and one coating on the back, which not only reduces the total amount of fiber used and reduces costs, but also has bright color difference and strong layering, and reduces the customer's ink consumption; at the same time, the core layer adds high-yield and high-bulk mechanical wood pulp, which improves the thickness and stiffness index, saves resources, reduces costs, and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 The utility model is a schematic structural diagram of the multi-layer molded coated paper provided by the utility model. DETAILED DESCRIPTION
[0018] The following will be combined with the embodiments of the utility model to clearly and completely describe the technical solution of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0019] The utility model provides a multi-layer formed coated paper, which comprises from top to bottom:
[0020] Top coating, middle coating, pre-coating, top fiber layer, core fiber layer, bottom fiber layer, back coating.
[0021] See also Figure 1 , Figure 1 A schematic structural diagram of a multi-layer molded coated paper provided in an embodiment; wherein 1 is a top coating, 2 is a middle coating, 3 is a pre-coating, 4 is a top fiber layer, 5 is a core fiber layer, 6 is a bottom fiber layer, and 7 is a back coating.
[0022] In the present invention, the top coating mainly improves the surface quality of the paper, improves the glossiness and smoothness, and reduces the ink absorption. It is preferably a coating composed of calcium carbonate, kaolin, adhesive, water repellent, lubricant, and water retaining agent, and the weight is preferably 10g / m 2 ~12g / m 2 . The utility model has no special restrictions on the types and sources of the above-mentioned calcium carbonate, kaolin, adhesive, water repellent, lubricant, and water retaining agent. Conventional types of components and commercial sources for preparing coatings well known to those skilled in the art can be used; at the same time, the method of forming the coating can be a technical solution of coating after mixing the components well known to those skilled in the art. In a preferred embodiment of the utility model, the top coating is dried to 92% to 94% dryness.
[0023] In the present invention, the middle coating mainly reduces the proportion of the fiber layer, reduces the amount of total fiber, and reduces the cost. It is preferably a coating composed of calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent, and the weight is preferably 6g / m 2 ~8g / m 2 . The utility model has no special restrictions on the types and sources of the above-mentioned calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent. Conventional types of components and commercial sources for preparing coatings well known to those skilled in the art can be used; at the same time, the method of forming the coating can be a technical solution of coating after mixing the components well known to those skilled in the art. In a preferred embodiment of the utility model, the middle coating is dried to 93% to 97% dryness.
[0024] In the present invention, the pre-coating layer mainly reduces the proportion of the fiber layer, reduces the amount of total fiber, and reduces the cost. It is preferably a coating composed of calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent, and the weight is preferably 14g / m 2 ~16g / m 2 . The utility model has no special restrictions on the types and sources of the above-mentioned calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent. Conventional types of components and commercial sources for preparing coatings well known to those skilled in the art can be used; at the same time, the method of forming the coating can be a technical solution of coating after mixing the components well known to those skilled in the art. In a preferred embodiment of the utility model, the pre-coating layer is dried to 93% to 97% dryness.
[0025] In the present invention, the surface fiber layer is the supporting layer of the paper, providing strength support, and is preferably a fiber layer formed by coniferous wood pulp and hardwood pulp, and the gram weight is preferably 25g / m 2 ~30g / m 2 The utility model has no special restrictions on the sources of the coniferous wood pulp and the broadleaf wood pulp, and commercial sources or self-made sources known to those skilled in the art can be used; the coniferous wood pulp and the broadleaf wood pulp are preferably bleached wood pulp. At the same time, the fiber layer can be formed by the technical solutions of wood pulp flow, headbox, post-net pressing and drying known to those skilled in the art.
[0026] In the present invention, the core fiber layer is a filling layer, which mainly uses cheap high-yield bleached mechanical wood pulp to increase thickness and reduce costs. It is preferably a fiber layer formed by mechanical wood pulp, and the gram weight is preferably 140g / m 2 ~150g / m 2 The utility model has no special restrictions on the source of the mechanical wood pulp, and a commercial source or a self-made source known to those skilled in the art can be used; the mechanical wood pulp is preferably bleached wood pulp. At the same time, the fiber layer can be formed by the technical solutions of wood pulp flow, headbox, post-net pressing, and drying known to those skilled in the art.
[0027] In the present invention, the bottom fiber layer is a supporting layer of the paper, providing strength support, and is preferably a fiber layer formed by coniferous wood pulp and hardwood pulp, and the gram weight is preferably 20g / m 2 ~24g / m 2 The utility model has no special restrictions on the sources of the coniferous wood pulp and the broadleaf wood pulp, and commercial sources or self-made sources known to those skilled in the art can be used; the coniferous wood pulp and the broadleaf wood pulp are preferably bleached wood pulp. At the same time, the fiber layer can be formed by the technical solutions of wood pulp flow, headbox, post-net pressing and drying known to those skilled in the art.
[0028] In the utility model, the above-mentioned surface fiber layer, core fiber layer and bottom fiber layer are preferably compounded, pressed and dried to form a composite layer of surface fiber layer-core fiber layer-bottom fiber layer with an overall dryness of preferably 93% to 97%, which constitutes the base fiber layer of the original paper as a whole and has a strength supporting function.
[0029] In the present invention, the back coating mainly reduces the proportion of the fiber layer, reduces the amount of total fiber, and reduces the cost. It is preferably a coating composed of calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent, and the weight is preferably 14g / m 2 ~16g / m 2The utility model has no special restrictions on the types and sources of the above-mentioned calcium carbonate, adhesive, water repellent, lubricant, and water retaining agent. Conventional types and commercial sources of components for preparing coatings well known to those skilled in the art can be used; at the same time, the coating can be formed by mixing the components evenly and then applying the components well known to those skilled in the art. In a preferred embodiment of the utility model, the back coating is formed by drying to a dryness of 93% to 97%.
[0030] In the utility model, the above-mentioned coatings can form an integral structure with the fiber layer, which mainly plays the role of reducing the fiber usage, reducing costs, and improving appearance and printing effects.
[0031] In the present invention, the weight of the multi-layer coated paper is preferably 200 g / m 2 ~300g / m 2 .
[0032] In the present utility model, the multi-layer formed coated paper preferably further comprises:
[0033] Starch glue layer.
[0034] In the present invention, the weight of the starch glue layer is preferably 2 g / m 2 ~5g / m 2 .
[0035] In the present invention, the starch adhesive layer is preferably arranged between the pre-coating layer and the surface fiber layer, and between the bottom fiber layer and the back coating layer, respectively; so that the pre-coating layer and the surface fiber layer, and between the bottom fiber layer and the back coating layer have good bonding strength to form an integral structure.
[0036] The multi-layer formed coated paper provided by the utility model has the following beneficial effects:
[0037] (1) Three coatings are applied on the surface fiber layer and one coating is applied on the back side, which not only reduces the total amount of fiber used and reduces costs, but also produces bright color difference and strong layering, saving ink. (2) White cardboard machine is used for production, and high-yield and high-bulk mechanical wood pulp is added to the core layer, which improves the thickness and stiffness index, saves resources and reduces costs. At the same time, the pulping yield of bleached coniferous pulp and bleached broadleaf pulp is about 50%, and the pulping yield of high-yield and high-bulk mechanical wood pulp is 85% to 95%.
[0038] The utility model provides a multi-layer molded coated paper, which includes, from top to bottom: a surface coating, a middle coating, a pre-coating, a surface fiber layer, a core fiber layer, a bottom fiber layer, and a back coating. Compared with the prior art, the multi-layer molded coated paper provided by the utility model adopts a specific layer structure with a specific connection relationship to achieve better overall interaction, and realizes three coatings on the surface fiber layer and one coating on the back, which not only reduces the total amount of fiber used and reduces costs, but also has bright color difference and strong layering, and reduces the customer's ink consumption; at the same time, the core layer adds high-yield and high-bulk mechanical wood pulp, which improves the thickness and stiffness index, saves resources, reduces costs, and has broad application prospects.
[0039] In order to further illustrate the utility model, the following embodiments are described in detail below.
[0040] Example
[0041] See also Figure 1 , Figure 1 A schematic structural diagram of a multi-layer molded coated handbag paper provided in an embodiment; wherein 1 is a top coating, 2 is a middle coating, 3 is a pre-coating, 4 is a top fiber layer, 5 is a core fiber layer, 6 is a bottom fiber layer, and 7 is a back coating.
[0042] The specific preparation steps are as follows:
[0043] The surface fiber layer raw materials are pulped, and the wood pulp components and weight percentages of this layer are 30wt% coniferous pulp and 70wt% hardwood pulp. After surface layer flow conveying, surface layer headbox, and surface wire part, a surface wet fiber layer is obtained.
[0044] The core fiber layer raw material is pulped, the wood pulp component and weight percentage of this layer is 100wt% of mechanical pulp, and it is passed through the core layer flow conveying, the core layer headbox, and the core mesh part to obtain the core wet fiber layer.
[0045] The raw materials for the bottom fiber layer are pulped, and the wood pulp components and weight percentages of this layer are 25wt% coniferous pulp and 75wt% broadleaf pulp. After bottom layer flow conveying, bottom layer headbox and bottom wire part, a bottom wet fiber layer is obtained.
[0046] The three wet fiber layers are compounded, pressed, and dried to obtain a composite layer of a surface fiber layer-core fiber layer-bottom fiber layer with a dryness of 93% to 97%; wherein the surface fiber layer is 27g / m 2 , core fiber layer 145g / m 2 , bottom fiber layer 23g / m 2 .
[0047] The surface glue starch is used to apply glue to the upper and lower surfaces of the above composite layer, and the glue amount on the front side is 4g / m 2 , the amount of glue applied on the back side is 3g / m 2 .
[0048] Then it is dried to a dryness of 93% to 97%, followed by a coating process (the following parts are all parts by weight).
[0049] The pre-coating material calcium carbonate 100 parts, SB butadiene styrene latex 13 parts, water repellent 0.35 parts, lubricant 0.3 parts, water retaining agent 0.55 parts, 500r / min high speed uniform dispersion for 30 minutes, coated on the above front surface adhesive layer, coating amount 15g / m 2 , infrared drying to 93% to 97% dryness to form a pre-coating.
[0050] The raw materials of the middle coating, calcium carbonate 100 parts, SB butadiene styrene latex 13 parts, water repellent 0.35 parts, lubricant 0.3 parts, water retaining agent 0.55 parts, are uniformly dispersed at 500r / min for 30 minutes and applied to the pre-coating layer. The coating amount is 7g / m 2 , infrared drying to 93% to 97% dryness to form a front middle coating.
[0051] The back coating material calcium carbonate 100 parts, SB butadiene styrene latex 13 parts, water repellent 0.35 parts, lubricant 0.3 parts, water retaining agent 0.55 parts, 500r / min high speed uniform dispersion for 30 minutes, coated on the back surface adhesive layer, coating amount 15g / m 2 , infrared drying to 93% to 97% dryness to form a back coating.
[0052] The raw materials of the top coating layer are 80 parts of calcium carbonate, 20 parts of kaolin, 13 parts of SB butadiene rubber latex, 0.4 parts of water repellent, 0.4 parts of lubricant, and 0.2 parts of water retaining agent. Disperse them uniformly at 500r / min for 30 minutes and apply them to the front middle coating layer. The coating amount is 11g / m 2 , infrared drying to 92% to 94% dryness to form a top coating.
[0053] Then it is finished by calender and wound by winder to get 250g / m 2 Multi-layer coated carrier bag paper.
[0054] Comparative Example
[0055] The wood pulp component and the weight percentage are 30wt% of coniferous pulp and 70wt% of broadleaf pulp, and calcium carbonate of 10% of the weight of the wood pulp component is added, and a single layer of wet fiber layer is obtained through flow conveying, headbox, and wire. The single layer of wet fiber layer is pressed and dried to obtain 243g / m 2 Single fiber layer.
[0056] The surface glue starch is applied to the upper and lower surfaces of the above-mentioned single-layer fiber layer, and the amount of glue applied on the front side is 4g / m 2 , the amount of glue applied on the back side is 3g / m 2 .
[0057] Then it is dried to a dryness of 92% to 94%, and then calendered and wound by a paper reel to obtain 250g / m 2 Single-layer uncoated carrier bag paper (conventional carrier bag paper on the market).
[0058] The products of the embodiments and comparative examples were tested for various properties according to the following standards. The results are shown in Table 1.
[0059] Glossiness is tested according to GB / T8941; printing glossiness is tested according to GB / T12032; smoothness is tested according to GB / T456; ink absorption rate is tested according to GB / T12911.
[0060] Table 1 Performance data
[0061] index Example Comparative Example Coniferous pulp dosage, kg / t paper 55.4 268.3 Broadleaf pulp dosage, kg / t paper 144.6 626.0 Mechanical pulp consumption, kg / t paper 580 - Total fiber content, kg / t paper 780 894.3 Glossiness, % 48.6 5.2 Printing gloss, % 89.5 10.2 Smoothness, % 284 30 Ink absorption rate, % 9.6 3.5
[0062] As can be seen from Table 1, the total fiber usage of the embodiment is less, and the usage of high-priced coniferous pulp and broadleaf pulp in the fiber is less; at the same time, the glossiness and printing glossiness are higher (paper and printed products are brighter), the smoothness is better, and the ink absorption rate is lower (printing saves ink).
[0063] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A multi-layered coated paper for handbags, characterized in that: From top to bottom: Top coating, middle coating, pre-coating, top fiber layer, core fiber layer, bottom fiber layer, back coating.
2. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The weight of the top coating is 10 g / m 2 ~12g / m 2 .
3. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The weight of the middle coating is 6 g / m 2 ~8g / m 2 .
4. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The weight of the pre-coating layer is 14 g / m 2 ~16g / m 2 .
5. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The surface fiber layer has a grammage of 25 g / m 2 ~30g / m 2 .
6. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The core fiber layer is a fiber layer formed by mechanical wood pulp, with a gram weight of 140g / m 2 ~150g / m 2 .
7. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The base fiber layer has a grammage of 20 g / m 2 ~24g / m 2 .
8. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The weight of the back coating is 14 g / m 2 ~16g / m 2 .
9. The multi-layered coated carrier bag paper according to claim 1, characterized in that: The weight of the multi-layer coated handbag paper is 200g / m 2 ~300g / m 2 .
10. The multi-layered coated carrier bag paper according to any one of claims 1 to 9, characterized in that: Also includes: Starch glue layer; The starch glue layer is respectively arranged between the pre-coating layer and the surface fiber layer, and between the bottom fiber layer and the back coating layer.