Mask for improving photoetching precision of exposure machine
By adjusting the design of chrome graphic plating and metal frame on the mask plate, reducing the width of the shading area and increasing the width of the light transmission area, the problem of high cost of existing equipment transformation is solved and higher lithography accuracy and production are achieved Margin.
Patent Information
- Application Number
- CN202420013219.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-03
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2034-01-03
AI Technical Summary
When existing exposure machine lithography equipment achieves higher accuracy, it is necessary to replace or modify the equipment, resulting in high costs and it is difficult to improve the lithography accuracy without changing the equipment.
By designing a mask plate that improves the lithography accuracy of the exposure machine, using chrome graphic plating and metal frame, the widths of the shading and light transmission areas are reduced and increased respectively, to achieve the optimization of line width and line distance, and weak exposure is adopted Design method to ensure the improvement of lithography accuracy.
Without changing the equipment, by changing the line width and line distance of the mask plate, the lithography accuracy is improved, the cost is reduced, the process flow is simplified, and the production margin is increased.
Smart Images

Figure CN221960404U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of exposure machine photolithography equipment, in particular to a mask plate for improving the photolithography precision of an exposure machine. Background Art
[0002] The photomask is a fixture used for photolithography of LCD panels. After the photoresist is coated, the traditional projection exposure machine projects the pattern on the mask onto the glass substrate at a 1:1 ratio through the exposure machine, and then forms the photoresist pattern through the development and baking process. With the continuous development of the screen industry, the user experience demand has increased. The higher the screen-to-body ratio, the narrower the frame. The smaller the line width / line spacing of the metal routing in the fanout routing area in the lower frame of the existing display screen, the narrower the frame. When making the panel, the higher the photolithography accuracy of the exposure machine required, the equipment needs to be replaced or the original equipment needs to be modified to achieve higher accuracy requirements, but the modification cost is high.
[0003] For example, the minimum lithography accuracy pitch achieved by the Canon E813 series exposure machine is 6um. The existing technology uses a 1:1 exposure method. If the minimum lithography accuracy is to be 5.5um or less, the margin cannot be achieved with at least 3 exposure dose units (mj / cm 2 ) above, such as Figure 1 As shown in the schematic diagram of the panel structure, the panel 200 includes an AA pixel area 201 and a lower frame 202. The lower frame 202 includes a fanout routing area 2021. If the lower frame 202 of the panel 200 needs to be narrowed, it is necessary to reduce the line and / or space of the fanout routing area 2021 to achieve this. Pitch (period) = line (line width) + space (line spacing). In the prior art, to achieve lower lithography accuracy, it is necessary to modify the equipment, which is costly. Therefore, how to use low cost to improve the lithography accuracy of the exposure machine has become a topic that needs to be studied at present. Summary of the invention
[0004] The technical problem to be solved by the utility model is to provide a method for improving the photolithography accuracy of a product by changing the line width and line spacing of a photolithography mask without modifying the equipment, which is simple, convenient and low-cost.
[0005] The utility model is implemented as follows: a mask for improving the photolithography accuracy of an exposure machine, the mask consisting of a substrate, a coating, a film and a frame, the frame being surrounded below the substrate, the coating and the film being located inside the frame and being sequentially arranged below the substrate, the coating consisting of a plurality of shading areas and light-transmitting areas being alternately arranged in sequence, the width of the shading area being L, the width of the light-transmitting area being D, the metal line width formed after photolithography being l, the metal line spacing being d, wherein Ll=-0.6um, Dd=0.6um.
[0006] Furthermore, the substrate is a quartz substrate.
[0007] Furthermore, the coating is a chromium pattern coating.
[0008] Furthermore, the frame is a metal frame.
[0009] The advantages of the utility model are: the utility model adopts a weak exposure design method of Mask (mask design size) - ADI (line width size after lithography process) = -0.6um to improve the lithography accuracy of the product, and by changing the line and space sizes of the coating, it can ensure that there is a large enough space to improve the lithography accuracy when reducing the pitch of the fanout routing area. It is simple, convenient and low-cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] The present invention will be further described below in conjunction with the embodiments with reference to the accompanying drawings.
[0011] Figure 1 A schematic diagram of the panel structure.
[0012] Figure 2 It is a structural schematic diagram of the mask plate of the utility model.
[0013] Description of the accompanying drawings: panel 200, AA pixel area 201, lower frame 202, fanout wiring area 2021, mask 100, substrate 1, coating 2, shading area 21, light-transmitting area 22, film 3, frame 4. DETAILED DESCRIPTION
[0014] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0015] like Figure 2As shown, the utility model is a mask for improving the photolithography accuracy of an exposure machine. The mask 100 is composed of a substrate 1, a coating 2, a film 3 and a frame 4. The substrate 1 is a quartz substrate, the coating 2 is a chrome pattern coating, and the frame 4 is a metal frame. The frame 4 is surrounded below the substrate 1, the coating 2 and the film 3 are located inside the frame 4, and are sequentially arranged below the substrate 1. The coating 2 is composed of a plurality of light-shielding areas 21 and light-transmitting areas 22 arranged alternately in sequence. The width of the light-shielding area 21 is L, and the width of the light-transmitting area 22 is D. After the photolithography process, a metal line spacing is formed on the fanout wiring area of the panel corresponding to the light-transmitting area 22, and a metal line width is formed in the light-shielding area 21. The metal line width after photolithography is l, and the metal line spacing is d, wherein Ll = -0.6um, Dd = 0.6um. The utility model adopts a weak exposure design method of Mask (mask design size) - ADI (line width size after lithography process) = -0.6um, which reduces the width of the mask shading area 21 and increases the width of the mask transparent area 22 to improve the lithography accuracy.
[0016] In order to achieve a narrow bezel on the mobile phone panel, especially the bottom bezel, the overall height of the panel fanout routing area needs to be reduced. Therefore, the pitch size of the fanout routing area must be reduced, that is, the line and / or space must be reduced. While achieving a smaller bottom bezel, the following must be ensured:
[0017] ① Applied to metal layer (Al Mo or Mo Al Mo structure), etching process line width loss is based on 1um.
[0018] ② The line width after photolithography and etching process is not less than 2um. (The line width below 2um plus process fluctuations can easily cause line breakage and lead to product failure. Controlling the line width to ≥2um can avoid this problem.)
[0019] ③ During the photolithography process, ensure that there is no photoresist residue in the line spacing space and have at least 3 exposure dose units (mj / cm 2 ) to ensure the stability of mass production.
[0020] ④ Based on G6 Canon E813H exposure machine SIB exposure mode / E813T exposure machine high sigma exposure mode.
[0021] At present, if the Canon E813 series exposure machine adopts the 1:1 exposure method, the minimum lithography accuracy pitch (period) achieved is 6um, and the weak exposure design method is used to expand the light transmission area by 0.6um to reduce the diffraction phenomenon of light when passing through the slit of the light transmission area. The light transmission area of the mask is designed to be large enough to ensure that there is no exposure residue problem in the lithography pattern. The reason is that the smaller the light transmission area, the more serious the diffraction phenomenon of light when passing through the slit of the mask, the larger the diffraction angle will be, and the energy finally collected on the surface of the photoresist will be smaller, which may cause photoresist residue. Therefore, when reducing the pitch of the fanout wiring area of the panel, it is necessary to ensure a large enough mask light transmission area to improve the lithography accuracy. When the minimum lithography accuracy pitch (period) to be achieved is less than 6um, the use of weak exposure design mask design can increase the lithography margin of 1-3 exposure dose units. Without changing the lithography equipment, it provides the production feasibility of small pitch and small space models in the fanout wiring area, and improves the production margin in the mass production process. In addition, in the AA area mask compensation part, the loading effect of the line width of each panel partition is different due to the different pitch sizes of the fanout routing area. The line width of the AA pixel area and the line width of the fanout routing area cannot reach the expected specification value at the same time after the photolithography process. Further compensation is required on the mask size of the AA pixel area. The weak exposure design is relatively lower than the 1:1 exposure method, and the required mask compensation is relatively low. Through experimental comparison, it can be seen that when the photolithography accuracy is 5.5um at the same time, the lithography margin of 1:1 exposure is 1, and the mask compensation of the AA area is 0.3um, while the lithography margin of the weak exposure design is 4, and the mask compensation of the AA area is 0.25um.
[0022] The advantages of the utility model are: the utility model adopts a weak exposure design method of Mask (mask design size) - ADI (line width size after lithography process) = -0.6um to improve the lithography accuracy of the product, and by changing the line and space sizes of the coating, it can ensure that there is a large enough space to improve the lithography accuracy when reducing the pitch of the fanout routing area. It is simple, convenient and low-cost.
[0023] Although the specific implementation methods of the present invention are described above, those skilled in the art should understand that the specific embodiments described are only illustrative and are not intended to limit the scope of the present invention. Equivalent modifications and changes made by those skilled in the art in accordance with the spirit of the present invention should be included in the scope of protection of the claims of the present invention.
Claims
1. A mask for improving the photolithography accuracy of an exposure machine, characterized in that: The mask is composed of a substrate, a coating, a film and a frame, the frame is surrounded by the bottom of the substrate, the coating and the film are located inside the frame and are sequentially arranged below the substrate, the coating is composed of a plurality of shading areas and light-transmitting areas alternately arranged in sequence, the width of the shading area is L, the width of the light-transmitting area is D, the metal line width formed after photolithography is l, the metal line spacing is d, wherein Ll=-0.6um, Dd=0.6um.
2. The mask for improving the photolithography accuracy of an exposure machine according to claim 1, characterized in that: The substrate is a quartz substrate.
3. The mask for improving the photolithography accuracy of an exposure machine according to claim 1, characterized in that: The plating layer is a chromium pattern plating layer.
4. The mask for improving the photolithography accuracy of an exposure machine according to claim 1, characterized in that: The frame is a metal frame.