Optical photoresist forming equipment
Through the optical photoresist forming equipment, the photoresist layer is thinned by laser light, which solves the problem that the thickness of the mold photoresist layer is difficult to uniformly reduce, and the uniformity and thickness of the photoresist film is optimized, which supports efficient patterning and chemical etching steps. .
Patent Information
- Application Number
- CN202420529534.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-19
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2034-03-19
AI Technical Summary
The thickness of the existing mold photoresist layer is difficult to shrink evenly, resulting in stagnation of technical research.
An optical photoresist forming equipment is designed, using copper molds, displacement mechanisms, photoresist sprayers and laser emitters to thin the photoresist layer through laser light to form a uniform photoresist film with a thickness of between 0.25 microns and 0.35 microns.
The photoresist layer is uniformly thinned, forming a photoresist film with thin thickness and high uniformity, supporting subsequent patterning and chemical etching steps to form a high-quality imprinted holographic pattern.
Smart Images

Figure CN221983849U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a forming device, in particular to an optical photoresist forming device. Background Art
[0002] Most existing molds have a photoresist layer formed on their outer surface by coating, but the photoresist layer formed by this coating method has its limitations (e.g., the thickness is difficult to be further uniformly reduced), which has led to a stagnation in the relevant technical research in this field. Therefore, the applicant believes that the above defects can be improved, and has devoted himself to research and applied scientific principles, and finally proposed a utility model with a reasonable design and effective improvement of the above defects. Utility Model Content
[0003] The embodiment of the utility model provides an optical photoresist shaping device, which can effectively improve the photoresist shaping limitations of the existing mold.
[0004] The utility model discloses an optical photoresist forming device, which includes: a processing platform for setting a copper mold; a displacement mechanism installed on the processing platform and capable of moving relative to the copper mold; a photoresist sprayer, corresponding to the processing platform, and used to form a photoresist layer with a thickness between 3 microns and 5 microns on the copper mold; and a laser emitter, installed on the displacement mechanism, so as to be able to move relative to the copper mold through the displacement mechanism; wherein the laser emitter can be used to emit laser light back and forth toward the photoresist layer through the displacement mechanism, so that the thickness of the photoresist layer is thinned to between 0.25 microns and 0.35 microns.
[0005] Preferably, the optical photoresist forming equipment further comprises a baking mechanism for curing the photoresist layer formed by the photoresist sprayer.
[0006] Preferably, the photoresist sprayer is mounted on a displacement mechanism so as to be movable relative to the copper mold via the displacement mechanism.
[0007] Preferably, the copper mold is in the shape of a roller, and the processing platform is fixed to both ends of the copper mold and can rotate the copper mold at a constant speed with its center line as the axis.
[0008] Preferably, the laser transmitter can be used to emit laser light with an intensity between 1W and 2W.
[0009] Preferably, the laser transmitter can be used to emit laser light with a wavelength of 405 nanometers.
[0010] The utility model also discloses an optical photoresist forming device, which includes: a processing platform for setting a copper mold; wherein the outer surface of the copper mold is formed with a photoresist layer with a thickness between 3 microns and 5 microns; a displacement mechanism installed on the processing platform and capable of moving relative to the copper mold; and; a laser emitter installed on the displacement mechanism so as to be able to move relative to the copper mold through the displacement mechanism; wherein the laser emitter can be used to emit laser light back and forth toward the photoresist layer through the displacement mechanism, so that the thickness of the photoresist layer is thinned to between 0.25 microns and 0.35 microns.
[0011] Preferably, the copper mold is in the shape of a roller, and the processing platform is fixed to both ends of the copper mold and can rotate the copper mold at a constant speed with its center line as the axis.
[0012] Preferably, the laser transmitter can be used to emit laser light with an intensity between 1W and 2W.
[0013] Preferably, the laser transmitter can be used to emit laser light with a wavelength of 405 nanometers.
[0014] In summary, the optical photoresist forming equipment disclosed in the embodiment of the utility model can implement the thinning of the photoresist layer by optical means (such as: the laser light) so that the outer surface of the copper mold can form the photoresist film with a thickness as thin as the default value and better uniformity.
[0015] In order to further understand the features and technical contents of the present invention, please refer to the following detailed description and drawings of the present invention. However, such description and drawings are only used to illustrate the present invention and are not intended to limit the scope of protection of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 The present invention is a schematic diagram of the steps of the copper mold manufacturing method according to an embodiment of the present invention.
[0017] Figure 2 for Figure 1 Schematic diagram of the preparation steps and photoresist shaping steps.
[0018] Figure 3 for Figure 1 A partial cross-sectional schematic diagram of a photoresist forming step.
[0019] Figure 4 for Figure 3 Schematic cross-sectional view along section line IV-IV.
[0020] Figure 5 for Figure 1 Schematic diagram of the thinning steps.
[0021] Figure 6 for Figure 1 A schematic partial cross-sectional view of the thinning step.
[0022] Figure 7 for Figure 6 Schematic cross-sectional view along section line VII-VII.
[0023] Figure 8 for Figure 1 Schematic diagram of the patterning steps.
[0024] Fig. 9 for Figure 1 Schematic diagram of the copper etching substeps.
[0025] Fig.10 for Figure 1 Schematic diagram of the shaping etching sub-step.
[0026] Fig.11 for Figure 1 Schematic diagram of the layer-building steps. DETAILED DESCRIPTION
[0027] The following is an explanation of the implementation of the "optical photoresist forming device" disclosed in the utility model through specific embodiments. Those skilled in the art can understand the advantages and effects of the utility model from the contents disclosed in this specification. The utility model can be implemented or applied through other different specific embodiments, and the details in this specification can also be modified and changed based on different viewpoints and applications without departing from the concept of the utility model. In addition, the drawings of the utility model are only simple schematic illustrations and are not depicted according to actual dimensions. It is stated in advance. The following implementation methods will further explain the relevant technical contents of the utility model in detail, but the disclosed contents are not intended to limit the scope of protection of the utility model.
[0028] It should be understood that, although the terms "first", "second", "third", etc. may be used herein to describe various components or signals, these components or signals should not be limited by these terms. These terms are mainly used to distinguish one component from another component, or one signal from another signal. In addition, the term "or" used herein may include any one or more combinations of the associated listed items depending on the actual situation.
[0029] See also Figures 1 to 11 As shown, it is an embodiment of the utility model. This embodiment discloses a copper mold manufacturing method S100, which is suitable for forming an imprinted holographic pattern H on the outer surface 11 of a copper mold 1. In other words, any mold manufacturing method not applied to copper molds is different from the copper mold manufacturing method S100 referred to in this embodiment.
[0030] The copper mold manufacturing method S100 in this embodiment sequentially includes or implements a preparation step S110, a photoresist forming step S120, a thinning step S130, a patterning step S140, a chemical etching step S150, and a layer adding step S160. The following will be based on the specific implementation of the above-mentioned multiple steps, but it can also be adjusted and changed according to design requirements. For example, in other embodiments not shown in the present utility model, the copper mold manufacturing method S100 can omit at least one of the preparation step S110 and the layer adding step S160 according to design requirements.
[0031] The preparation step S110: Figure 1 and Figure 2 As shown, an optical photoresist shaping device 100 is provided. The optical photoresist shaping device 100 in this embodiment includes a processing stage 101, a displacement mechanism 102 installed on the processing stage 101, a photoresist sprayer 103 and a laser emitter 104 installed on the displacement mechanism 102, and a baking mechanism 105 installed on the processing stage 101, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the photoresist sprayer 103 and / or the baking mechanism 105 may also be omitted according to design requirements.
[0032] Furthermore, the processing platform 101 is used for setting the copper mold 1, and the copper mold 1 is in the shape of a roller in this embodiment, so the structure adopted by the processing platform 101 is capable of being fixed at both ends of the copper mold 1 and can make the copper mold 1 rotate at a constant speed with its center line as the axis, but it is not limited to this. For example, in other embodiments not shown in the present utility model, the copper mold 1 can also be a flat sheet structure, and the structure of the processing platform 101 is for placing the copper mold 1 thereon.
[0033] The displacement mechanism 102 is installed on the processing stage 101 so as to be movable relative to the copper mold 1, and the photoresist sprayer 103 and the laser emitter 104 are both installed on the displacement mechanism 102 in this embodiment so as to be movable relative to the copper mold 1 through the displacement mechanism 102, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the photoresist sprayer 103 may also be arranged corresponding to the processing stage 101 and not be installed on the displacement mechanism 102.
[0034] It should be noted that the copper mold manufacturing method S100 in this embodiment uses the optical photoresist shaping device 100 to implement the photoresist shaping step S120 and the thinning step S130, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the photoresist shaping step S120 and the thinning step S130 may also be implemented using other photoresist shaping devices having structures different from those of the present embodiment.
[0035] The photoresist forming step S120: Figures 1 to 4 As shown, a photoresist layer 2a with a thickness between 3 microns and 5 microns is formed on the outer surface 11 of the copper mold 1. In the photoresist forming step S120 of this embodiment, the copper mold 1 is rotated at a constant speed by the processing stage 101, and the photoresist sprayer 103 forms the photoresist layer 2a with a uniform thickness on the copper mold 1. Furthermore, the baking mechanism 105 is used to cure the photoresist layer 2a formed by the photoresist sprayer 103 in the photoresist forming step S120.
[0036] The thinning step S130: Figure 1 ,and Figures 5 to 7 As shown, the photoresist layer 2a is irradiated with laser light L back and forth to thin the photoresist layer 2a until the thickness of the photoresist layer 2a is between 0.25 micrometers and 0.35 micrometers, and is defined as a photoresist film 2b. In the thinning step S130 of this embodiment, the copper mold 1 is rotated at a constant speed by the processing stage 101, and the laser emitter 104 can emit the laser light L back and forth toward the photoresist layer 2a through the displacement mechanism 102, so that the thickness of the photoresist layer 2a is thinned to between 0.25 micrometers and 0.35 micrometers, thereby forming the photoresist film 2b.
[0037] The laser emitter 104 can be used to emit the laser light L with a wavelength of 405 nanometers (nm) to effectively thin the photoresist layer 2a. Furthermore, the laser emitter 104 can be used to emit the laser light L with an intensity between 1W and 2W to thin the photoresist layer 2a more quickly.
[0038] Accordingly, the optical photoresist forming device 100 in this embodiment can implement the thinning of the photoresist layer 2a by optical means (such as: the laser light L), so that the outer surface 11 of the copper mold 1 can form the photoresist film 2b with a thickness as thin as a default value and better uniformity, so as to facilitate the implementation of the subsequent patterning step S140 and the chemical etching step S150, and form the imprinted holographic pattern H.
[0039] That is to say, any method or device that does not use laser light to thin the photoresist layer 2 a is different from the copper mold manufacturing method S100 or the optical photoresist shaping device 100 defined in this embodiment.
[0040] The patterning step S140: Figure 1 , Figure 7 ,and Figure 8 As shown, the exposure light passes through interference or mask to form a default holographic pattern layer 2c on the photoresist film 2b. Part of the outer surface 11 of the copper mold 1 is exposed outside the default holographic pattern layer 2c and is defined as a first forming area 111, and the rest of the outer surface 11 of the copper mold 1 is covered by the default holographic pattern layer 2c and is defined as a second forming area 112.
[0041] The chemical etching step S150: Figure 1 ,and Figures 8 to 10 As shown, the outer surface 11 of the copper mold 1 is chemically etched to form the embossed holographic pattern H. The embossed holographic pattern H has a depth between 0.25 microns and 0.35 microns, and the line width and line spacing of the embossed holographic pattern H are not greater than 0.5 microns (μm). In this embodiment, the chemical etching step S150 sequentially includes or implements a copper etching sub-step S151 and a forming etching sub-step S152, and the above two sub-steps are described below respectively.
[0042] The copper etching sub-step S151: Figure 1 , Figure 8 ,and Fig. 9 As shown, the outer surface 11 of the copper mold 1 is chemically etched so that the copper mold 1 is concavely formed with a plurality of grooves 111a in the first forming area 111. The shapes of the plurality of grooves 111a together form an intermediate three-dimensional pattern M.
[0043] The forming etching sub-step S152: Figure 1 , Fig. 9 ,and Fig.10 As shown, the chemical etching is performed from the intermediate three-dimensional pattern M to remove the default holographic pattern layer 2c, and the outer surface 11 of the copper mold 1 is concavely formed with the embossed holographic pattern H, which corresponds to (e.g., is substantially the same as) the intermediate three-dimensional pattern M. Among them, the copper mold 1 has a portion formed by the chemical etching in the second forming area 112, and its appearance corresponds to (e.g., is substantially the same as) the default holographic pattern layer 2c.
[0044] The layer adding step S160: Figure 1 and Fig.11 As shown, a protective layer 3 (such as a chrome plating layer or a fluorine polymer coating) is formed on the copper mold 1, which covers the entire embossed holographic pattern H, so that the protective layer 3 can prevent the copper mold 1 from being oxidized and facilitate the separation of the copper mold 1 from the optical film (not shown in the figure) on which it is rolled.
[0045] [Technical effects of the utility model embodiment]
[0046] In summary, the optical photoresist forming equipment disclosed in the embodiment of the utility model can implement the thinning of the photoresist layer by optical means (such as: the laser light), so that the outer surface of the copper mold can form the photoresist film with a thickness as thin as a default value and better uniformity, which is beneficial to the patterning step and the chemical etching step to form the embossed holographic pattern.
[0047] The contents disclosed above are only preferred feasible embodiments of the present utility model, and are not intended to limit the patent scope of the present utility model. Therefore, all equivalent technical changes made using the contents of the specification and drawings of the present utility model are included in the patent scope of the present utility model.
Claims
1. An optical photoresist forming device, It is characterized in that The optical photoresist forming device comprises: A processing platform for setting a copper mold; A displacement mechanism, mounted on the processing platform and capable of moving relative to the copper mold; a photoresist sprayer, arranged corresponding to the processing stage, for forming a photoresist layer with a thickness between 3 microns and 5 microns on the copper mold; and; A laser emitter is mounted on the displacement mechanism so as to be movable relative to the copper mold through the displacement mechanism; wherein the laser emitter can be used to emit laser light back and forth toward the photoresist layer through the displacement mechanism so that the thickness of the photoresist layer is thinned to between 0.25 microns and 0.35 microns.
2. The optical photoresist forming device according to claim 1, It is characterized in that The optical photoresist forming equipment further comprises a baking mechanism for curing the photoresist layer formed by the photoresist sprayer.
3. The optical photoresist forming device according to claim 1, It is characterized in that The photoresist sprayer is installed on the displacement mechanism so as to be movable relative to the copper mold through the displacement mechanism.
4. The optical photoresist forming device according to claim 1, It is characterized in that The copper mold is in the shape of a roller, and the processing platform is fixed at both ends of the copper mold and can make the copper mold rotate at a constant speed with its center line as the axis.
5. The optical photoresist forming device according to claim 1, It is characterized in that The laser emitter can be used to emit the laser light with an intensity between 1W and 2W.
6. The optical photoresist forming device according to claim 1, It is characterized in that The laser transmitter can be used to emit the laser light with a wavelength of 405 nanometers.
7. An optical photoresist forming device, It is characterized in that The optical photoresist forming device comprises: A processing stage for setting a copper mold; wherein a photoresist layer with a thickness between 3 microns and 5 microns is formed on the outer surface of the copper mold; a displacement mechanism mounted on the processing stage and capable of moving relative to the copper mold; and; A laser emitter is mounted on the displacement mechanism so as to be movable relative to the copper mold through the displacement mechanism; wherein the laser emitter can be used to emit laser light back and forth toward the photoresist layer through the displacement mechanism so that the thickness of the photoresist layer is thinned to between 0.25 microns and 0.35 microns.
8. The optical photoresist forming device according to claim 7, It is characterized in that The copper mold is in the shape of a roller, and the processing platform is fixed at both ends of the copper mold and can make the copper mold rotate at a constant speed with its center line as the axis.
9. The optical photoresist forming device according to claim 7, It is characterized in that The laser emitter can be used to emit the laser light with an intensity between 1W and 2W.
10. The optical photoresist forming device according to claim 9, It is characterized in that The laser transmitter can be used to emit the laser light with a wavelength of 405 nanometers.