Preparation device of fine metal mask plate strip

By using devices such as melting pipes, cooling rollers and conveying mechanisms in FMM manufacturing, the problem of difficult and high cost of extremely thin tiled alloy foils is solved, and efficient and low-cost production of strips below 20μm is achieved, ensuring the product uniformity and quality.

CN221988649UActive Publication Date: 2024-11-12JIANGSU TOPTO MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323377272.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-12
Publication Date
2024-11-12
Estimated Expiration
2033-12-12

AI Technical Summary

Technical Problem

The prior art is difficult to effectively produce extremely thin low-expanded tile alloy foil, which leads to an increase in in-plane wrinkles during the FMM manufacturing process, making the manufacturing difficulty and cost high, and it is impossible to produce FMM below 20 μm.

Method used

The preparation device including a melting pipe, a cooling roller, a conveying mechanism and a winding device is adopted to store alloy melt through the melting pipe and prepare thin strips. The conveying mechanism provides uniform support. The thermometer monitors the temperature in real time and the negative pressure box. and air-cooling devices improve flow rate and continuity, electromagnetic heating and flow meter ensure the stability of the melt.

Benefits of technology

The production of Inwa alloy strips with a thickness of less than 20μm is achieved. The process is simple, efficient and low-cost, ensuring the uniformity and quality of the strips.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221988649U_ABST
    Figure CN221988649U_ABST
Patent Text Reader

Abstract

The utility model provides a preparation device of a fine metal mask strip, and relates to the field of production of invar alloy ultrathin strips. The preparation device comprises a melting pipe, a cooling roller, a conveying mechanism and a winding device, the cooling roller is positioned below the melting pipe, receives the alloy melt flowing out of the melting pipe, cools the alloy melt into a solid and outputs a thin strip; the conveying mechanism is located below the output side of the cooling roller, receives the strip output by the cooling roller and conveys the strip to the downstream. The winding device is used for winding the strip conveyed by the conveying mechanism; the melting pipe comprises a containing section and a discharging section, the containing section is gradually shrunk downwards from a liquid inlet of the containing section, the upper end of the discharging section is connected to a lower opening of the containing section, a rectangular discharging opening is formed in the lower end of the discharging section, the width of the discharging opening is D, the length of the discharging opening is L, D is larger than or equal to 0.2 mm and smaller than or equal to 5 mm, and L is equal to (5-40) * D. The device is suitable for producing invar alloy strips with the thickness being less than 20 microns through a melt-spinning process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the production field of ultra-thin Invar alloy strips, in particular to a preparation device for fine metal mask strips. Background Art

[0002] Flexible AMOLED displays have the advantages of being thin, foldable, and rollable in a variety of forms. Compared with rigid display products, they can provide consumers with a better user experience, and are therefore favored by more and more high-end portable consumer electronics enthusiasts. In the evaporation equipment currently used in OLED mass production lines, FMM (OLED fine metal mask) is mainly used to achieve separate deposition of RGB pixel light-emitting layers. During the production and use of FMM, it will be affected by factors such as gravity, pressure, and magnetism. In addition, it will also produce thermal expansion due to the heat release of the evaporated organic material, as well as creep behavior under stress, which places high demands on the raw materials of FMM. After comprehensive consideration, the raw materials of FMM currently used are mostly extremely thin low-expansion Invar alloy foils.

[0003] In the past, the Invar alloy foil used in the manufacture of FMM was generally formed by rolling or tempering cold rolling. Due to the difficulty of manufacturing, the difficulty of controlling fine structures and gravity factors, the FMM production method is also mostly divided type, and the thinner the raw material foil used, the better. The thickness of the Invar alloy foil is extremely thin and the rigidity is very poor. In the process of processing, it is inevitable that in-plane wrinkles will occur, resulting in an increase in defects in the manufactured FMM. At present, most companies that use etching production cannot produce FMMs below 20μm.

[0004] As the thickness of FMM is required to be thinner, it is becoming increasingly difficult to prepare Invar alloy foil using existing methods, and the cost is greatly increased. To overcome this problem, it is urgent to find a simple, efficient and low-cost way to produce thinner Invar alloy products for manufacturing FMM. Utility Model Content

[0005] In order to solve the above problems existing in the prior art, the utility model provides a preparation device for a fine metal mask strip, the preparation device comprising:

[0006] A melting tube used as a container for receiving alloy melt; and

[0007] A cooling roller, which is located below the melting tube, receives the molten alloy flowing out of the melting tube, cools the molten alloy into a solid and outputs a thin strip; and

[0008] A conveying mechanism, which is located below the output side of the cooling roller and receives the strip output by the cooling roller and conveys it downstream; and

[0009] The winding device is used to convey the strip conveyed by the conveying mechanism into the winding device for winding;

[0010] The molten tube comprises a receiving section and a discharging section. The receiving section gradually contracts downward from its liquid inlet. The upper end of the discharging section is connected to the lower end of the receiving section. The lower end has a rectangular discharging port. The width of the discharging port is D and the length is L, and the conditions are as follows: 0.2 mm ≤ D ≤ 5 mm, and L = (5-40)·D.

[0011] Furthermore, there are two cooling rollers, and one of them is located obliquely above the other;

[0012] An angle γ is formed between a discharging direction of the discharging port of the discharging section and a connecting line direction of the centers of the two cooling rollers, and the angle is 60°≤γ≤90°.

[0013] Furthermore, the conveying mechanism includes a material receiving guide plate and a material receiving pipe, both of which are inclined downward, a vibration motor is arranged in the middle of the material receiving pipe, the upper end of the material receiving guide plate is connected to the output side of the cooling roller, and the lower end is connected to the material receiving pipe.

[0014] Furthermore, a first temperature measuring instrument is provided in the middle of the melting tube;

[0015] There are two cooling rollers, and at least one of them is provided with a second temperature measuring instrument;

[0016] The conveying mechanism is provided with a third temperature measuring instrument.

[0017] Furthermore, a first stop valve is provided at the lower part of the melting tube, and a second stop valve is provided on the conveying mechanism.

[0018] Furthermore, it also includes a box body, the box body is controlled to be negative pressure, the melting tube, cooling roller and conveying mechanism are arranged in the box body, and the liquid inlet of the melting tube is located outside the box body.

[0019] Furthermore, a barometer and an air extraction device are provided on the box.

[0020] Furthermore, it also includes an air cooling device, which is connected to a cold air duct, and the air outlet of the cold air duct extends to the upper end close to the conveying mechanism.

[0021] Furthermore, an electromagnetic heating coil is arranged in the middle of the melting tube; and an electromagnetic flowmeter is arranged in the lower part of the melting tube.

[0022] Furthermore, it also includes a crucible for delivering alloy melt to the melting tube, and the crucible is arranged on an extendable crucible stand.

[0023] The beneficial effects of the utility model are:

[0024] The preparation device of the fine metal mask strip in the utility model is suitable for producing the Invar alloy material used for FMM by the strip-spinning method, and can be used to produce the Invar alloy strip with a thickness of less than 20 μm, and has a simple production process, high efficiency and low cost.

[0025] In addition, other additional aspects and advantages of the present invention will be partially given in the following description, partially become apparent from the following description, or be learned through the practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a structural schematic diagram of the device of the utility model;

[0027] Figure 2 It is a schematic diagram of the structure of the melting tube;

[0028] Figure 3 It is a schematic diagram of the matching angle between the center line of the two cooling rollers and the discharge direction of the molten tube;

[0029] In the figure: 1. box body; 2. crucible; 21. crucible stand; 3. melting tube; 31. electromagnetic heating coil; 32. first thermometer; 33. first stop valve; 34. electromagnetic flowmeter; 301. receiving section; 302. discharging section; 4. cooling roller; 4a. first cooling roller; 4b. second cooling roller; 41. second thermometer; 5. material receiving guide plate; 6. material receiving pipe; 61. third thermometer; 62. vibration motor; 63. second stop valve; 7. winding device; 8. air cooling device; 81. cold air duct; 9. barometer; 10. exhaust device. DETAILED DESCRIPTION

[0030] In order to make the purpose, technical solutions and advantages of the utility model clearer, the utility model will be further described in detail below with reference to the accompanying drawings.

[0031] Reference Figure 1 and Figure 2 As shown in the figure, a device for preparing a fine metal mask strip is provided in this embodiment, and the device comprises a melting tube 3, a cooling roller 4, a conveying mechanism and a winding device 7 which are arranged in sequence, wherein: the melting tube 3 is used as a container for containing alloy melt, and the alloy melt is a raw material melt for preparing Invar alloy. The cooling roller 4 is located below the melting tube 3, and the alloy melt flows out of the melting tube 3 and is cooled into a solid by the cooling roller 4 and outputs a thin Invar alloy strip. The conveying mechanism is located below the output side of the cooling roller 4 (that is, the side where the Invar alloy strip is thrown out), and the strip thrown out from the cooling roller 4 enters the conveying mechanism for transportation. The winding device 7 is arranged downstream of the conveying mechanism, and the strip conveyed by the conveying mechanism is sent to the winding device 7 to complete the winding, and a coil product is obtained.

[0032] In order to obtain an Invar alloy strip with a thickness of less than 20 μm, the structure of the melting tube 3 is designed as follows in this solution. Figure 2 As shown in , the melting tube 3 in this scheme includes a receiving section 301 and a discharging section 302. The upper end of the melting tube 3 has a liquid inlet, which gradually tapers downward from the liquid inlet to form a receiving section 301 with a conical tube structure. The cross section of the discharging section 302 is rectangular, and the equal cross section or cross-sectional area slowly decreases at different positions along its discharging direction. The upper end of the discharging section 302 is connected to the lower end of the receiving section 301, and the lower end of the discharging section 302 has a rectangular discharging port, and the width D of the discharging port is 0.2 to 5 mm. Exemplarily, the width D can be selected as 1 mm, 2 mm, 3 mm or 4 mm, etc., and the length L of the discharging port is 5 to 40 times its width D. The melting tube 3 is suitable for preparing strips of different specifications according to the different specifications of its discharging port.

[0033] The research results show that, combined with the control of the rotation speed of the cooling roller 4 (to control the strip spinning speed), the preparation device using the above-mentioned melting tube 3 structure can produce Invar alloy strips of about 20 to 25 μm or even thinner.

[0034] This preparation device adopts double roller belting, referring to Figure 1 As shown in FIG. 1 , the two cooling rollers 4 are respectively a first cooling roller 4a and a second cooling roller 4b. Figure 3 As shown in the figure, one of the two cooling rollers 4 is located obliquely above the other, that is, the two cooling rollers 4 are arranged obliquely, for example, the center line of the two rollers forms an angle of about 30° with the horizontal plane. The discharge direction of the discharge port of the molten tube 3 and the direction of the line connecting the centers of the two cooling rollers 4 have an angle γ (see the attached figure). Figure 3 ), the γ angle is between 60° and 90°, and for example, the γ angle can be 60°, 70°, 80° or 90°, etc. This design makes it easy to obtain a thin strip with a uniform microstructure.

[0035] Since the thickness of the produced Invar alloy strip is only less than 25 μm, and the strip thrown out from the cooling roller 4 still has a relatively high temperature, if the strip is not well supported during the subsequent conveying process, its thickness uniformity is likely to decrease. To solve this problem, the above-mentioned conveying mechanism in the preparation device preferably uses a vibration mode to convey the Invar alloy strip.

[0036] Specifically, refer to Figure 1As shown in , the above-mentioned conveying mechanism includes a material receiving guide plate 5 and a material receiving pipe 6, both of which are inclined downward, and a vibration motor 62 is arranged in the middle of the material receiving pipe 6. The upper end of the material receiving guide plate 5 is connected to the output side of the cooling roller 4, and the lower end is connected to the material receiving pipe 6. During the operation of the equipment, the strip is thrown out by the cooling roller 4 and enters the material receiving pipe 6 through the material receiving guide plate 5. At this time, the vibration motor 62 provides a small vibration for the material receiving pipe 6, and the strip vibrates in the material receiving pipe 6. In addition, with the influence of the strip's own gravity, the strip can be moved forward at a uniform speed. This conveying mechanism can provide uniform support for the strip while conveying the Invar alloy strip, so that the uniformity and quality of the strip are guaranteed.

[0037] In some embodiments, Figure 1 As shown in the figure, the preparation device is also provided with a first thermometer 32, a second thermometer 41 and a third thermometer 61. The first thermometer 32 is arranged in the middle of the melting tube 3, more specifically, in the lower part of the receiving section 301; the second thermometer 41 is arranged on the cooling roller 4. When a double-roller belt is used, at least one cooling roller 4 is provided with the second thermometer 41, for example, Figure 1 The first cooling roller 4a and the second cooling roller 4b shown in the figure are each provided with a second temperature measuring instrument 41; the third temperature measuring instrument 61 is provided in the conveying mechanism, more specifically, at the rear end of the receiving pipe 6. These temperature measuring instruments are used to control the temperature of the products at each stage in the equipment in real time, so as to respond to abnormal situations in a timely manner.

[0038] For example, when the first thermometer 32 detects that the temperature of the alloy melt in the melting tube 3 is lower than the predetermined value, the melting tube 3 should be heated midway to ensure the stability of the flow state of the alloy melt. When the second thermometer 41 detects that the temperature of the cooling roller 4 is too high, the flow rate of the cooling water in the cooling roller 4 should be accelerated to cool the cooling roller 4 in time. The third thermometer 61 in the receiving tube 6 is used to detect the product temperature, which is generally close to the surface temperature of the cooling roller 4 or the ambient temperature around the receiving tube 6. If the temperature is abnormal, the belt should be stopped immediately.

[0039] like Figure 1 As shown in , the preparation device is also provided with a first stop valve 33 and a second stop valve 63, which are used to pause or terminate the strip-spinning production operation. The first stop valve 33 is located at the lower part of the melting tube 3, specifically, it is arranged on the material discharging section 302; the second stop valve 63 is arranged on the conveying mechanism, specifically, it is arranged in the middle part of the receiving pipe 6. When it is necessary to pause or terminate the strip-spinning, the first stop valve 33 is closed first to stop the outflow of the Invar alloy melt, and after the strip thrown out by the cooling roller 4 completely slides out through the receiving pipe 6, the second stop valve 63 is closed, and the strip is wound up by the winding device 7 to obtain a coil.

[0040] Since the width of the outlet of the melting tube 3 is small, the flow rate and continuity of the feeding will be adversely affected. Figure 1 As shown in the figure, the preparation device is further provided with a box body 1, in which a melting tube 3, a cooling roller 4 and a conveying mechanism are arranged, and a liquid inlet of the melting tube 3 extends out of the box body from the top of the box body 1. The box body 1 is controlled to be negative pressure, and a pressure difference is formed between the liquid inlet and the liquid outlet of the melting tube 3. In this way, when the width of the outlet of the melting tube 3 is small, the flow rate and continuity of the alloy melt outflow are greatly improved, and the output strip is relatively more uniform in its length direction.

[0041] In order to obtain a relatively stable negative pressure environment in the box 1, in some embodiments, Figure 1 As shown in the figure, a barometer 9 and an air extraction device 10 are provided on the box 1. When the equipment is running, the air in the box 1 is extracted through the air extraction device 10 to form a negative pressure environment that meets the requirements, and the barometer 9 is used to monitor the air pressure in the box 1 in real time to ensure that a substantially constant negative pressure environment is maintained in the box 1.

[0042] In some embodiments, the preparation device is further provided with an air cooling device 8, which is connected to a cold air conduit 81, and the air outlet of the cold air conduit 81 extends to the upper end close to the conveying mechanism, that is, the discharge side of the cooling roller 4, to provide cold air cooling and cooling of the strip material thrown out from the cooling roller 4. When the temperature of the cooling roller 4 is too high, the air cooling device 8 should be turned on while starting the cooling water flow rate in the acceleration roller, and the synergistic effect of the two can quickly return the abnormal temperature to a normal level.

[0043] In the above-mentioned embodiment, when the first thermometer 32 detects that the temperature of the alloy melt in the melting tube 3 is lower than the predetermined value, it is necessary to heat the melting tube 3 midway. Therefore, an electromagnetic heating coil 31 is provided in the middle of the melting tube 3 in the preparation device, and the electromagnetic heating coil 31 surrounds the lower part of the receiving section 301. When the temperature of the alloy melt in the receiving section 301 is lower than the normal value, the electromagnetic heating coil 31 is started to heat it midway, so that the temperature of the melt returns to the normal level.

[0044] like Figure 3 As shown in , in the present preparation device, an electromagnetic flowmeter 34 is also provided at the lower part of the melting tube 3, specifically, it is provided on the discharge section 302 of the melting tube 3. The electromagnetic flowmeter 34 is used to monitor the injection speed of the Invar alloy melt in real time. The temperature of the Invar alloy melt can generally reach 1450°C or above, and the electromagnetic flowmeter 34 can complete the work of measuring the flow rate under high temperature environment. It is worth noting that the injection speed of the Invar alloy melt directly affects the quality of the output strip. The electromagnetic flowmeter 34 is used for real-time monitoring, and the flow data can be obtained in time to avoid the occurrence of abnormal situations. When abnormalities occur, timely correction helps to improve product quality.

[0045] like Figure 1 As shown in the figure, the preparation device is further provided with a crucible 2, which is used to deliver the alloy melt to the melting tube 3. The crucible 2 is arranged on a crucible stand 21, and can be rotated on the crucible stand 21 to pour the Invar alloy melt. Preferably, the crucible stand 21 is extendable, and then the Invar alloy melt can be poured at a suitable position according to different melting tubes 3.

[0046] In addition, it is worth mentioning that legs or casters can also be provided at the bottom of the preparation device to facilitate the overall transportation of the equipment.

[0047] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the embodiments of the utility model rather than to limit them. Although the embodiments of the utility model are described in detail with reference to the preferred embodiments, it is obvious that the described embodiments are only part of the embodiments of the utility model, rather than all of the embodiments. Those skilled in the art should understand that the technical solutions of the embodiments of the utility model can still be modified or replaced by equivalents, and these modifications or equivalent replacements cannot make the modified technical solutions deviate from the scope of the technical solutions of the embodiments of the utility model.

Claims

1. A device for preparing a fine metal mask strip, characterized in that: include: A melting tube (3) used as a container for containing alloy melt; as well as A cooling roller (4) is located below the melting tube (3), receives the alloy melt flowing out of the melting tube (3), cools the alloy melt into a solid and outputs a thin strip; and A conveying mechanism, which is located below the output side of the cooling roller (4), receives the strip output by the cooling roller (4) and conveys it downstream; as well as A winding device (7), wherein the strip material conveyed by the conveying mechanism is fed into the winding device (7) to complete winding; The molten tube (3) comprises a receiving section (301) and a discharging section (302), wherein the receiving section (301) gradually contracts downward from its liquid inlet, the upper end of the discharging section (302) is connected to the lower end of the receiving section (301), and the lower end has a rectangular discharging opening, the width of the discharging opening is D, the length is L, and the following conditions are satisfied: 0.2mm≤D≤5mm, L=(5~40)·D.

2. The device for preparing fine metal mask strip according to claim 1, characterized in that: There are two cooling rollers (4), one of which is located obliquely above the other; An angle γ is formed between the discharging direction of the discharging port of the discharging section (302) and the direction of the line connecting the centers of the two cooling rollers (4), and the angle is 60°≤γ≤90°.

3. The device for preparing fine metal mask strip according to claim 1, characterized in that: The conveying mechanism includes a material receiving guide plate (5) and a material receiving pipe (6), both of which are inclined downward, and a vibration motor (62) is arranged in the middle of the material receiving pipe (6). The upper end of the material receiving guide plate (5) is supported on the output side of the cooling roller (4), and the lower end is connected to the material receiving pipe (6).

4. The device for preparing fine metal mask strip according to claim 1, characterized in that: A first temperature measuring instrument (32) is provided in the middle of the melting tube (3); There are two cooling rollers (4), and at least one of them is provided with a second temperature measuring instrument (41); A third temperature measuring instrument (61) is arranged on the conveying mechanism.

5. The device for preparing fine metal mask strip according to claim 1, characterized in that: A first stop valve (33) is provided at the lower part of the melting pipe (3), and a second stop valve (63) is provided on the conveying mechanism.

6. The device for preparing fine metal mask strip according to claim 1, characterized in that: It also includes a box body (1), the box body (1) is controlled to be at negative pressure, the melting tube (3), cooling roller (4) and conveying mechanism are arranged in the box body (1), and the liquid inlet of the melting tube (3) is located outside the box body (1).

7. The device for preparing fine metal mask strip according to claim 6, characterized in that: The box body (1) is provided with a barometer (9) and an air extraction device (10).

8. The device for preparing fine metal mask strip according to claim 1, characterized in that: It also includes an air cooling device (8), the air cooling device (8) is connected to a cold air duct (81), and the air outlet of the cold air duct (81) extends to the upper end close to the conveying mechanism.

9. The device for preparing fine metal mask strip according to claim 1, characterized in that: An electromagnetic heating coil (31) is provided in the middle of the melting tube (3); An electromagnetic flowmeter (34) is provided at the lower part of the melting tube (3).

10. The device for preparing fine metal mask strip according to claim 1, characterized in that: It also includes a crucible (2) for delivering alloy melt to the melting tube (3), and the crucible (2) is arranged on an extendable crucible stand (21).