PEM water electrolyzer bipolar plate and electrolysis cell thereof
By setting up matching grooves and porous titanium mesh support structures of different sizes on the bipolar plate of the electrolytic cell, the problem of membrane electrode damage caused by diffusion layer deformation in conventional electrolytic cell assembly is solved, and a more uniform stress state and higher electrolytic efficiency.
Patent Information
- Application Number
- CN202420055255.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-09
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-01-09
AI Technical Summary
During the assembly process, conventional runner electrolytic cells have a high risk of damage to the membrane electrode due to deformation of the cathode and anode diffusion layer, and are complex in assembly and have high cost.
A PEM water electrolytic cell bipolar plate is designed. By setting up matching grooves of different sizes on the anode and cathode surfaces, diffusion layers are placed to ensure uniform stress during assembly, reduce shear stress, and support the structure through the porous titanium mesh and Positioning holes simplify assembly process.
Reduces the probability of membrane electrode damage, simplifies the assembly process, reduces material costs, and improves electrolytic efficiency and fluid uniformity.
Smart Images

Figure CN222008093U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of electrolytic cells, in particular to a PEM water electrolytic cell bipolar plate and an electrolytic chamber thereof. Background Art
[0002] As the cleanest and most efficient energy source in the 21st century, the development of hydrogen production technology is also the key to the development of the entire hydrogen energy industry. PEM water electrolyzer conforms to the development trend of high voltage and high current density of hydrogen production technology, and has become the most popular hydrogen production technology at present.
[0003] Electrolyzers can be divided into plate-mesh type and flow channel type according to the different composition structures of their electrolytic chambers. Plate-mesh electrolyzers use porous metal mesh as the channel for the fluid, and the bipolar plates only play the role of conductivity and support; flow channel electrolyzers process the flow field on the bipolar plates, taking into account the function of distributing the fluid. In contrast, flow channel electrolyzers usually have more uniform fluid distribution because the flow field can be designed in a targeted manner; at the same time, they have fewer components, lower resistance, and better conductivity. However, conventional flow channel electrolyzers also have certain problems. The biggest one is that the complex structure of the flow field makes the manufacturing cost of the bipolar plate high, which accounts for a high proportion of the cost of the electrolyzer. In addition, there are also problems such as:
[0004] A comb-tooth structure is usually set between the flow channel and the flow field of a conventional channel-type bipolar plate to balance the force on the plate surface. At the same time, the comb-tooth structure can also provide a flow channel for the fluid. A cover sheet is usually attached to the comb-tooth structure to fill the gaps on the surface of the comb-tooth structure, thereby improving the support effect. However, the complex processing features of the comb-tooth structure and the manufacturing cost of the cover sheet itself will increase the manufacturing cost of the channel-type bipolar plate. At the same time, the installation of the cover sheet (usually by gluing) also makes the assembly process of the electrolyzer more complicated.
[0005] The electrolysis chambers of a conventional channel electrolyzer are stacked up and down in the order of bipolar plates, cathode diffusion layers, membrane electrodes, anode diffusion layers, and bipolar plates, and the cathode and anode diffusion layers are of the same size. During the assembly process, the diffusion layer will be compressed and deformed. If the deformation of the cathode and anode is different, the height of the overlapping area of the membrane electrode and the diffusion layer will be offset, and a large shear stress will be generated at the overlapping boundary, increasing the risk of membrane electrode damage. In addition, the conventional structure requires manual alignment of the cathode and anode diffusion layers during assembly. Once misalignment occurs, it will lead to uneven current transmission and greatly reduce the efficiency of hydrogen production. Utility Model Content
[0006] The purpose of the utility model is to provide a PEM water electrolyzer bipolar plate and its electrolysis chamber, so as to solve the technical problem in the prior art that the diffusion layer will be compressed and deformed during the assembly process. If the deformation of the anode and cathode is different, the height of the overlapping area of the membrane electrode and the diffusion layer will be offset, and a large shear stress will be generated at the overlapping boundary position, thereby increasing the risk of membrane electrode damage.
[0007] The utility model discloses a bipolar plate for a PEM water electrolyzer, comprising a plate body, wherein the upper and lower surfaces of the plate body are respectively a cathode surface and an anode surface, an anode matching groove is provided on the anode surface, the outer edge of the anode matching groove surrounds the anode flow field, an anode diffusion layer is provided in the anode matching groove, a cathode matching groove is provided on the cathode surface, the outer edge of the cathode matching groove surrounds the cathode flow field, a cathode diffusion layer is provided in the cathode matching groove, and the size of the anode matching groove is different from that of the cathode matching groove.
[0008] Working principle: When in use, the anode diffusion layer is placed in the anode matching slot, and the cathode diffusion layer is placed in the cathode matching slot. By setting the cathode matching slot and the anode matching slot, and the size of the anode matching slot is different from that of the cathode matching slot, the stress state of the anode and cathode diffusion layers during assembly is changed, so that the maximum deformation is limited, the stress state in the electrolysis chamber becomes controllable, and the membrane electrode can therefore be maintained on the same plane, reducing the probability of damage.
[0009] Furthermore, the anode matching groove is smaller than the cathode matching groove.
[0010] Furthermore, the electrode body is provided with water-oxygen flow openings and hydrogen flow openings which are connected vertically, wherein the water-oxygen flow openings are divided into a water inlet end and a water outlet end.
[0011] At least two water-oxygen flow channels are provided, and the water inlet and the water outlet must each contain at least one. The water flow path formed by the water inlet and the water outlet should cover the entire anode flow field as much as possible to ensure that the water flow is evenly distributed and the reaction is sufficient. (In this embodiment, there are one water inlet and one water outlet for the water-oxygen flow channel, and they are arranged on both sides of the anode flow field in a centrally symmetrical manner with respect to the center of the electrode body).
[0012] Furthermore, the cathode flow field is connected to the hydrogen flow channel opening through the cathode transition zone; the anode flow field is connected to the water oxygen flow channel opening through the anode transition zone.
[0013] Furthermore, the cathode transition zone is flush with the bottom surface of the cathode flow field; the bottom surface of the anode transition zone is flush with the bottom surface of the anode flow field;
[0014] Furthermore, a plurality of support parts are arranged inside the cathode transition region and the anode transition region, and the support parts are used to support the diffusion layer above them to prevent collapse.
[0015] Furthermore, the support part is a porous titanium mesh, which is installed in cooperation with the limiting part to play a guiding and supporting role.
[0016] Furthermore, the plate body is provided with a plurality of positioning holes for assembly positioning, and the positioning holes are provided with wiring parts. The wiring parts are thinner than the plate body and can be used to connect inspection equipment.
[0017] Furthermore, at least two positioning holes are provided and are arranged symmetrically about the center of the electrode body.
[0018] Furthermore, in order to improve the utilization rate of the board surface, the positioning holes are preferably arranged at the four corners, and one or more wiring parts can be arranged.
[0019] Furthermore, the non-overlapping area between the cathode matching groove and the cathode flow field is the cathode bonding area.
[0020] Furthermore, the support portion in the cathode transition region is located in the cathode bonding region.
[0021] Furthermore, the non-overlapping area between the anode matching groove and the anode flow field is the anode bonding area.
[0022] Furthermore, the support portion in the anode transition region is located in the anode bonding region.
[0023] An electrolysis chamber comprises a bipolar plate, a cathode diffusion layer, a membrane electrode and an anode diffusion layer, which are stacked up and down in the order of a bipolar plate body, a cathode diffusion layer, a membrane electrode, an anode diffusion layer and a bipolar plate body, wherein the cathode side of the bipolar plate body faces downward.
[0024] Furthermore, the membrane electrode is composed of a proton exchange membrane coated with a cathode catalyst and an anode catalyst on the upper and lower sides respectively, and the outer edge size of the proton exchange membrane is consistent with that of the bipolar plate.
[0025] Furthermore, the outer edge of the anode diffusion layer is smaller than the outer edge of the anode matching groove and is placed in the groove, and the bipolar plate and the anode diffusion layer are formed into one body at the anode bonding area by gluing; the outer edge of the cathode diffusion layer is slightly smaller than the outer edge of the cathode matching groove and is placed in the groove, and the bipolar plate and the anode diffusion layer are formed into one body at the anode bonding area by gluing.
[0026] The diffusion layer and the matching groove are bonded by glue in the bonding area. The glue used should be chemically stable under working conditions (50°C-80°C, acidic environment) and will not introduce new impurities into the system. UV curing glue or hot melt glue is preferred.
[0027] The depth of the anode-cathode matching groove should be less than the thickness of the anode-cathode diffusion layer. On the one hand, it is beneficial for the diffusion layer to be completely compressed into the matching groove. On the other hand, it is beneficial for the components to have closer contact, thereby reducing resistance and improving electrolysis efficiency.
[0028] Compared with the prior art, the utility model has the following beneficial effects:
[0029] 1. The utility model requires that both input and output fluids need to pass through the transition zone. The porous structure can provide sufficient flow channels. At the same time, the titanium mesh itself has a high strength and can play a supporting role in the transition zone, so that the bipolar plate is evenly stressed. Compared with the conventional comb tooth + cover plate structure, the processing characteristics of the comb tooth structure in the transition zone are simplified, the installation process of the cover plate (usually gluing) is omitted, and the grid structure has a better support effect than the comb tooth structure.
[0030] 2. The electrolyzer usually needs to be connected to inspection equipment during test operation. After the wiring part is combined with the positioning hole, there is no need to set up additional protruding wiring terminals, which can save the material cost of the bipolar plate.
[0031] 3. The number of components that need to be stacked is reduced from 5 to 3, and all 3 components can be positioned and assembled through the positioning holes, without the need for other manual alignment operations, which improves assembly efficiency. During the assembly process, the electrolytic chamber is compressed by the assembly force. When the anode diffusion layer is compressed to the point where the upper surface is flush with the upper surface of the anode matching groove, since the outer edge of the cathode diffusion layer is larger than the anode matching groove, the non-overlapping area of the two will fall on the anode bipolar plate, that is, the cathode diffusion layer is supported by the anode bipolar plate and will not be further compressed toward the anode diffusion layer. In this state, even if the assembly force is further increased, the membrane electrode will always remain in the same plane, and the shear stress it is subjected to will be greatly reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the utility model and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0033] Figure 1 It is a schematic diagram of the cross-sectional structure of the electrolysis chamber of the utility model.
[0034] Figure 2 It is a schematic diagram of the anode surface structure of the pole plate body of the utility model.
[0035] Figure 3 It is a schematic diagram of the cathode surface structure of the pole plate body of the utility model.
[0036] Figure 4 This is an explosion diagram of the electrolysis chamber of the utility model.
[0037] In the above drawings, the meanings of the various marks are: 1-plate body, 2-cathode surface, 3-anode surface, 4-anode matching groove, 5-anode diffusion layer, 6-cathode matching groove, 7-cathode diffusion layer, 8-water-oxygen flow channel outlet, 9-hydrogen flow channel outlet, 10-water inlet, 11-water outlet, 12-cathode flow field, 13-cathode transition zone, 14-anode flow field, 15-anode transition zone, 16-support part, 17-positioning hole, 18-cathode bonding area, 19-anode bonding area, 20-proton exchange membrane, 21-cathode catalyst, 22-anode catalyst, 23-membrane electrode, 24-wiring part. DETAILED DESCRIPTION
[0038] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments.
[0039] Example 1
[0040] The technical solutions adopted in this embodiment are as follows:
[0041] like Figure 1-Figure 4 As shown, a bipolar plate for a PEM water electrolyzer comprises a plate body 1, wherein the upper and lower surfaces of the plate body 1 are respectively a cathode surface 2 and an anode surface 3, wherein the anode surface 3 is provided with an anode matching groove 4, wherein the outer edge of the anode matching groove 4 surrounds an anode flow field 14, wherein an anode diffusion layer 5 is arranged in the anode matching groove 4, wherein a cathode matching groove 6 is provided on the cathode surface 2, wherein the outer edge of the cathode matching groove 6 surrounds a cathode flow field 12, wherein a cathode diffusion layer 7 is arranged in the cathode matching groove 6, and wherein the size of the anode matching groove 4 is different from that of the cathode matching groove 6.
[0042] Working principle: When in use, the anode diffusion layer 5 is placed in the anode matching groove 4, and the cathode diffusion layer 7 is placed in the cathode matching groove 6. By setting the cathode matching groove 6 and the anode matching groove 4, and the size of the anode matching groove 4 is different from that of the cathode matching groove 6, the stress state of the cathode and cathode diffusion layers 5 during assembly is changed, so that the maximum deformation is limited, the stress state in the electrolysis chamber becomes controllable, and the membrane electrode 23 can therefore be maintained on the same plane, and the probability of damage is reduced.
[0043] Example 2
[0044] In this embodiment, as a preferred embodiment of the present utility model, the specific structure is as follows Figure 1-Figure 4As shown, based on the embodiment 1, the following improvement is disclosed: the anode matching groove 4 is smaller than the cathode matching groove 6, and the electrode plate body 1 is provided with a water-oxygen flow channel opening 8 and a hydrogen flow channel opening 9 which are connected vertically, wherein the water-oxygen flow channel opening 8 is divided into a water inlet end 10 and a water outlet end 11.
[0045] At least two water-oxygen flow channel openings 8 are provided, and the water inlet end 10 and the water outlet end 11 must each contain at least one. The water flow path formed by the water inlet end 10 and the water outlet end 11 should cover the entire anode flow field 14 as much as possible to ensure that the water flow is evenly distributed and the reaction is sufficient. (In this embodiment, the water inlet end 10 and the water outlet end 11 of the water-oxygen flow channel opening 8 are each one, and are arranged on both sides of the anode flow field 14 in a centrally symmetrical manner with the center of the electrode body 1).
[0046] The cathode flow field 12 is connected to the hydrogen flow channel opening 9 through the cathode transition zone 13; the anode flow field 14 is connected to the water oxygen flow channel opening 8 through the anode transition zone 15, the cathode transition zone 13 is flush with the bottom surface of the cathode flow field 12; the bottom surface of the anode transition zone 15 is flush with the bottom surface of the anode flow field 14, and several support parts 16 are arranged inside the cathode transition zone 13 and the anode transition zone 15. The support part 16 is used to support the diffusion layer above it to prevent collapse, and the support part 16 is a porous titanium mesh, which is installed in conjunction with the limit part to play a role in guiding and supporting.
[0047] The plate body 1 is provided with a plurality of positioning holes 17 for assembly positioning, and a wiring portion 24 is provided at the positioning holes 17. The wiring portion 24 is thinner than the plate body 1 and can be used to connect inspection equipment. At least two positioning holes 17 are provided, and they are centrally symmetrically arranged with respect to the center of the plate body 1. To improve the utilization rate of the plate surface, the positioning holes 17 are preferably provided at four corners. One or more wiring portions 24 can be provided. The non-overlapping area between the cathode matching groove 6 and the cathode flow field 12 is the cathode bonding area 18, and the support portion 16 in the cathode transition area 13 is located in the cathode bonding area 18. The non-overlapping area between the anode matching groove 4 and the anode flow field 14 is the anode bonding area 19, and the support portion 16 in the anode transition area 15 is located in the anode bonding area 19.
[0048] Example 3
[0049] In this embodiment, as a preferred embodiment of the present utility model, the specific structure is as follows Figure 1-Figure 4As shown, an electrolysis chamber is disclosed, which discloses the following improvements on the basis of embodiment 2, including a plate body 1, a cathode diffusion layer 7, a membrane electrode 23 and an anode diffusion layer 5, which are stacked up and down in the order of the plate body 1, the cathode diffusion layer 7, the membrane electrode 23, the anode diffusion layer 5 and the plate body 1, wherein the cathode surface 2 of the plate body 1 faces downward, the membrane electrode 23 is composed of a proton exchange membrane 20 coated with a cathode catalyst 21 and an anode catalyst 22 on the upper and lower sides respectively, the outer edge size of the proton exchange membrane 20 is consistent with that of the bipolar plate, the outer edge of the anode diffusion layer 5 is smaller than the outer edge of the anode matching groove 4 and is placed in the groove, and the bipolar plate and the anode diffusion layer 5 are formed into one body at the anode bonding area 19 by gluing; the outer edge of the cathode diffusion layer 7 is slightly smaller than the outer edge of the cathode matching groove 6 and is placed in the groove, and the bipolar plate and the anode diffusion layer 5 are formed into one body at the anode bonding area 19 by gluing.
[0050] The diffusion layer and the matching groove are bonded by glue in the bonding area. The glue used should be chemically stable under working conditions (50°C-80°C, acidic environment) and will not introduce new impurities into the system. UV curing glue or hot melt glue is preferred.
[0051] The depth of the cathode and anode matching grooves 4 should be less than the thickness of the cathode and anode diffusion layers 5. On the one hand, this is conducive to the diffusion layer being completely compressed into the matching grooves. On the other hand, it is conducive to closer contact between components, thereby reducing resistance and improving electrolysis efficiency.
[0052] The above are the implementation methods listed in this embodiment, but this embodiment is not limited to the above optional implementation methods. Those skilled in the art can arbitrarily combine the above methods to obtain other various implementation methods. Anyone can derive other various forms of implementation methods under the inspiration of this embodiment. The above specific implementation methods should not be understood as limiting the scope of protection of this embodiment. The scope of protection of this embodiment shall be based on the definition in the claims, and the description can be used to interpret the claims.
Claims
1. A bipolar plate for a PEM water electrolyzer, characterized in that: The invention comprises a plate body (1), wherein the upper and lower surfaces of the plate body (1) are respectively a cathode surface (2) and an anode surface (3); an anode matching groove (4) is provided on the anode surface (3); the outer edge of the anode matching groove (4) surrounds an anode flow field (14); an anode diffusion layer (5) is arranged in the anode matching groove (4); a cathode matching groove (6) is provided on the cathode surface (2); the outer edge of the cathode matching groove (6) surrounds a cathode flow field (12); a cathode diffusion layer (7) is arranged in the cathode matching groove (6); and the size of the anode matching groove (4) is different from that of the cathode matching groove (6).
2. A PEM water electrolyzer bipolar plate according to claim 1, characterized in that: The anode matching groove (4) is smaller than the cathode matching groove (6).
3. A bipolar plate for a PEM water electrolyzer according to claim 1, characterized in that: The electrode body (1) is provided with a water-oxygen flow channel opening (8) and a hydrogen flow channel opening (9) which are connected vertically, wherein the water-oxygen flow channel opening (8) is divided into a water inlet end (10) and a water outlet end (11).
4. A bipolar plate for a PEM water electrolyzer according to claim 3, characterized in that: The cathode flow field (12) is connected to the hydrogen flow channel opening (9) through the cathode transition zone (13); and the anode flow field (14) is connected to the water oxygen flow channel opening (8) through the anode transition zone (15).
5. A bipolar plate for a PEM water electrolyzer according to claim 4, characterized in that: A plurality of support portions (16) are arranged inside the cathode transition region (13) and the anode transition region (15).
6. A bipolar plate for a PEM water electrolyzer according to claim 5, characterized in that: The supporting part (16) is a porous titanium mesh.
7. A bipolar plate for a PEM water electrolyzer according to claim 1, characterized in that: The electrode body (1) is provided with a plurality of positioning holes (17) for assembly positioning, and the positioning holes (17) are provided with wiring portions (24).
8. A bipolar plate for a PEM water electrolyzer according to claim 1, characterized in that: The non-overlapping area between the cathode matching groove (6) and the cathode flow field (12) is the cathode bonding area (18).
9. A bipolar plate for a PEM water electrolyzer according to claim 1, characterized in that: The non-overlapping area between the anode matching groove (4) and the anode flow field (14) is the anode bonding area (19).
10. An electrolysis chamber having a bipolar plate of a PEM water electrolyzer according to any one of claims 1 to 9, characterized in that: It comprises a plate body (1), a cathode diffusion layer (7), a membrane electrode and an anode diffusion layer (5), which are stacked up and down in the order of the plate body (1), the cathode diffusion layer (7), the membrane electrode (23), the anode diffusion layer (5) and the plate body (1), wherein the cathode surface (2) of the plate body (1) faces downward.