Eddy current sensor probe and chemical mechanical polishing equipment
By setting an electromagnetic shielding layer on the base of the eddy current sensor probe and using a probe cover to isolate it, the problem of noise influence during the CMP process is solved, the measurement accuracy is improved, and the service life of the electromagnetic shielding layer is extended, achieving a more accurate wafer film Thick measurements and longer equipment life.
Patent Information
- Application Number
- CN202422242120.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2034-09-13
AI Technical Summary
The complex environment of the CMP process leads to the measurement accuracy of the eddy current sensor being affected by noise, and it is difficult for the prior art to effectively improve the measurement accuracy.
An electromagnetic shielding layer is provided on the base of the eddy current sensor probe to cover the measurement end, and the electromagnetic shielding layer and polishing pad are isolated through the probe cover to reduce noise interference and loss to the electromagnetic shielding layer by replacement of the polishing pad.
It effectively improves the measurement accuracy of the eddy current sensor, and extends the service life of the electromagnetic shielding layer, ensuring more accurate wafer film thickness measurement and longer equipment service life.
Smart Images

Figure CN222021381U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of chemical mechanical polishing, and in particular to an eddy current sensor probe and chemical mechanical polishing equipment. Background Art
[0002] Among the related technologies, Chemical Mechanical Planarization (CMP) technology is the most effective global planarization method today. It uses the synergistic effect of chemical etching and mechanical grinding to effectively balance the local and global flatness of the wafer, and has been widely used in the manufacture of very large-scale integrated circuits.
[0003] During the CMP process, the amount of material removed needs to be precisely controlled. In order to ensure the high requirements of the process environment for the CMP process, eddy current is generally used for non-contact measurement to prevent the measurement process from affecting the CMP process.
[0004] However, the complex environment of the CMP process will generate a lot of noise, which will affect the measurement accuracy of the eddy current sensor. In view of this, the technical problem that needs to be solved in the prior art is how to improve the measurement accuracy of the eddy current sensor used in CMP. Utility Model Content
[0005] In view of this, the present application provides an eddy current sensor probe and a chemical mechanical polishing device to at least partially solve the above problems.
[0006] According to the first aspect of the present application, there is provided an eddy current sensor probe for chemical mechanical polishing equipment, characterized in that the eddy current sensor probe is arranged on the polishing disk of the chemical mechanical polishing equipment and contacts the polishing pad, and the eddy current sensor probe comprises: a probe base, provided with a accommodating space for accommodating the probe body; an electromagnetic shielding layer, arranged on the probe base and at least covering the measuring end of the probe body for shielding noise; and a probe cover, fixedly arranged on the probe base, for isolating the electromagnetic shielding layer from the polishing pad of the chemical mechanical polishing equipment.
[0007] Optionally, in any embodiment of the present application, the thickness of the electromagnetic shielding layer is 50 microns-120 microns.
[0008] Optionally, in any embodiment of the present application, the electromagnetic shielding layer is a conductive film.
[0009] Optionally, in any embodiment of the present application, the accommodating space includes a top wall corresponding to the measuring end side of the probe body, the electromagnetic shielding layer is arranged on the outer surface of the probe base and at least covers the top wall, and the top wall is used to isolate the electromagnetic shielding layer from the probe body.
[0010] Optionally, in any embodiment of the present application, the thickness of the top wall is 120 microns-240 microns, and the thickness of a portion of the probe cover corresponding to the top wall is 120 microns-240 microns.
[0011] Optionally, in any embodiment of the present application, the probe base includes a boss, the shape of the boss matches the accommodating space, and the measuring head of the probe body faces the top of the boss; the electromagnetic shielding layer is arranged on the top surface of the boss, or the electromagnetic shielding layer is arranged on the top surface and side surface of the boss.
[0012] Optionally, in any embodiment of the present application, the side wall of the boss includes a rectangular side wall and a curved side wall. When the electromagnetic shielding layer is arranged on the top surface and the side surface of the boss, the electromagnetic shielding layer covers the surface of the rectangular side wall, and the curved side wall is used to install and position the probe cover.
[0013] Optionally, in any embodiment of the present application, the probe cover includes a groove adapted to the shape of the boss.
[0014] Optionally, in any embodiment of the present application, the probe base is a probe base made of a thermal insulation material, and / or the probe cover is a probe cover made of a thermal insulation material.
[0015] According to the second aspect of the present application, a chemical mechanical polishing device is provided, comprising: a carrying head for holding a wafer and driving the wafer to rotate, a polishing plate covered with a polishing pad, a dresser for dressing the polishing pad, and a liquid supply part for providing a polishing liquid, wherein the polishing plate is provided with an eddy current sensor probe as described above.
[0016] The eddy current sensor performs contactless measurement through an electromagnetic field. The magnetic flux density at its measuring end is the largest and is also most affected by noise. The solution provided in this embodiment can effectively reduce the interference of noise on the measuring end and ensure the measurement accuracy of the eddy current sensor by providing a measuring end that at least covers the probe body on the probe base. In addition, by providing a probe cover, the loss of the electromagnetic shielding layer caused by the replacement process of the polishing pad can be reduced, thereby ensuring a long service life of the electromagnetic shielding layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions in the present application or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present application. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.
[0018] Figure 1 is a schematic diagram of a chemical mechanical polishing device according to an embodiment of the present application;
[0019] Figure 2 is a schematic diagram of a chemical mechanical polishing device provided with an eddy current sensor according to an embodiment of the present application;
[0020] Figure 3 is a schematic diagram of an eddy current sensor probe according to an embodiment of the present application;
[0021] Figure 4 is a schematic diagram of a probe base of an eddy current sensor probe according to an embodiment of the present application;
[0022] Figure 5 is a bottom view of a probe base according to an embodiment of the present application;
[0023] Figure 6 is a top view of another probe base according to an embodiment of the present application;
[0024] Figure 7 is a schematic diagram of a probe body according to an embodiment of the present application;
[0025] Figure 8 It is a schematic diagram of a probe cover according to an embodiment of the present application.
[0026] Description of reference numerals:
[0027] Carrying head 10; polishing pad 21; polishing plate 20; dresser 30; liquid supply part 40; eddy current sensor 50;
[0028] Probe base 51; accommodating space 511; first accommodating cavity 5111; second accommodating cavity 5112; top wall 512; boss 513; rectangular side wall 514; arc-shaped side wall 515; through hole 516;
[0029] Electromagnetic shielding layer 52; probe cover 53; probe body 54; detection coil 541; excitation coil 542. DETAILED DESCRIPTION
[0030] In order to enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in this application will be clearly and completely described below in conjunction with the drawings in this application. Obviously, the described embodiments are only part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field should fall within the scope of protection of this application.
[0031] The wafer edge chipping processing device provided in the present application is described in detail below with reference to the accompanying drawings.
[0032] In this application, Chemical Mechanical Polishing is also referred to as Chemical Mechanical Planarization, and wafer is also referred to as chip, silicon wafer, base sheet or substrate, etc., and their meanings and actual functions are equivalent.
[0033] like Figure 1 As shown, the main components of the chemical mechanical polishing equipment provided by the embodiment of the utility model include a carrier head 10 for holding a wafer w and driving the wafer w to rotate, a polishing disk 20 covered with a polishing pad 21, a dresser 30 for dressing the polishing pad 21, and a liquid supply part 40 for providing a polishing liquid.
[0034] During the chemical mechanical polishing process, the carrier head 10 absorbs the wafer w through negative pressure, and presses the side of the wafer w containing the metal film onto the polishing pad 21, and the carrier head 10 performs a rotational motion and a radial reciprocating motion along the polishing disk 20 so that the surface of the wafer w in contact with the polishing pad 21 is gradually polished, while the polishing disk 20 rotates, and the liquid supply unit 40 sprays the polishing liquid onto the surface of the polishing pad 21. Under the chemical action of the polishing liquid, the relative movement of the carrier head 10 and the polishing disk 20 causes the wafer w to rub against the polishing pad 21 for polishing. During polishing, the dresser 30 is used to dress and activate the surface morphology of the polishing pad 21. The dresser 30 can be used to remove foreign particles remaining on the surface of the polishing pad 21, such as abrasive particles in the polishing liquid and waste materials falling off the surface of the wafer w, and can also be used to flatten the surface deformation of the polishing pad 21 caused by grinding.
[0035] During the chemical mechanical polishing process, the wafer w is pressed onto the polishing pad 21 by the carrier head 20 and reciprocates radially along the polishing disk 10 with the carrier head 20. At the same time, the carrier head 20 and the polishing disk 10 rotate synchronously, so that the surface of the wafer w in contact with the polishing pad 21 is gradually polished away.
[0036] like Figure 2 As shown, the chemical mechanical polishing equipment also includes an eddy current sensor 50 and a control device for online measurement of the film thickness of the wafer w. The eddy current sensor 50 is installed in the polishing plate 20 and is located below the polishing pad 21. The eddy current sensor 50 rotates with the polishing plate 20 to achieve online measurement of the film thickness while polishing. The eddy current sensor 50 is set next to the polishing pad 21, and the wafer w is placed on the polishing pad 21. Therefore, the distance between the eddy current sensor 50 and the wafer w is the thickness of the polishing pad 21.
[0037] During the polishing process, it is necessary to monitor the film thickness change and film thickness value of the wafer w in real time so as to adopt the corresponding polishing process to avoid over-polishing or incomplete polishing. During the polishing process, the metal film thickness on the surface of the wafer is measured online, so as to accurately control the removal rate of the metal film by adjusting the pressure of the carrier head 10 to achieve better global flattening. The eddy current sensor 50 can adopt eddy current detection. The principle of eddy current detection is that when the eddy current sensor 50 scans the wafer w, the metal film layer on the surface of the wafer w will induce eddy currents and change the magnetic field generated by the eddy current sensor 50. When the metal film layer is removed by polishing, the eddy current sensor 50 measures the eddy current changes to measure the film thickness of the metal film layer.
[0038] However, due to the complex environment of the CMP process, the factors affecting the measurement accuracy of the eddy current sensor 50 are also relatively complex. The influencing factors may be, for example: the polishing liquid used in the CMP process may carry ions, which will affect the electromagnetic field when the eddy current sensor is measuring; the coil in the motor used to drive the polishing disc 10 may affect the magnetic field of the eddy current sensor; the polishing disc 10 is made of metal material, and the motor may affect the electric field of the polishing disc 10, indirectly affecting the electromagnetic field of the eddy current sensor.
[0039] The above-mentioned factors may affect the measurement accuracy of the eddy current sensor 50 .
[0040] See also Figure 3-8 In order to improve the measurement accuracy, the utility model provides an eddy current sensor probe for a chemical mechanical polishing device. The eddy current sensor probe is arranged on a polishing disk 20 of the chemical mechanical polishing device and contacts with a polishing pad 21 .
[0041] See also Figure 3 , 4 The eddy current sensor probe includes: a probe base 51, which is provided with a accommodating space 511 for accommodating a probe body 54; an electromagnetic shielding layer 52, which is arranged on the probe base 51 and at least covers the measuring end of the probe body 54 for shielding noise; a probe cover 53, which is fixedly arranged on the probe base 51 and is used to isolate the electromagnetic shielding layer 52 from the polishing pad 21 of the chemical mechanical polishing equipment.
[0042] A transmission line and a PCB board etc. can be connected below the eddy current sensor probe to form a complete eddy current sensor 50 .
[0043] The eddy current sensor performs contactless measurement through the electromagnetic field. The magnetic flux density at its measuring end is the largest and is also most affected by noise. By providing a measuring end that at least covers the probe body 54 on the probe base 51, the interference of noise on the measuring end can be effectively reduced, thereby ensuring the measurement accuracy of the eddy current sensor. In addition, by providing a probe cover 53, the loss of the electromagnetic shielding layer 52 caused by the replacement process of the polishing pad 21 can be reduced, thereby ensuring that the electromagnetic shielding layer 52 has a longer service life.
[0044] The eddy current sensor is a high-precision instrument that uses the principle of electromagnetic induction for non-contact measurement. It generates an electromagnetic field at the measuring end, interacts with the metal layer on the measured wafer, thereby inducing a current, and then measures the thickness of the metal layer of the wafer based on the change in current.
[0045] In practical applications, the measuring end of the eddy current sensor is the part that interacts most directly and sensitively with the object being measured. Since the intensity of the electromagnetic field reaches its maximum in this area and the density of magnetic flux lines is the highest, it is also most susceptible to interference from external environmental noise.
[0046] In order to improve the measurement accuracy and stability of the eddy current sensor, the applicant's staff has taken a variety of measures to reduce the impact of noise. One effective method is to set an electromagnetic shielding layer on the probe base, which can at least cover the measuring end of the probe body 54, thereby providing a more stable electromagnetic environment for the eddy current sensor and reducing the direct interference of external noise on the measuring end.
[0047] In this embodiment, the thickness of the electromagnetic shielding layer 52 is 50 microns to 120 microns. When the thickness of the electromagnetic shielding layer 52 is less than 50 microns, it cannot effectively shield noise. When the thickness of the electromagnetic shielding layer 52 is greater than 120 microns, it will weaken the electromagnetic signal of the eddy current sensor itself. Preferably, the thickness of the electromagnetic shielding layer 52 is 80 microns to 100 microns.
[0048] The electromagnetic shielding layer 52 is a conductive film. A conductive film with a certain thickness can form an equivalent capacitor outside the probe body 54, and use the characteristics of the capacitor's AC resistance to shield the interference signal outside the probe body 54. The conductive film can be a PU conductive film, and the square resistance of the conductive film can be 600-1200 ohms / cm to form a capacitor that can shield the interference signal. Of course, the electromagnetic shielding layer can also be a film of other materials, and the electromagnetic shielding layer can be formed on the probe base by gluing or coating, etc., all within the protection scope of this application.
[0049] See also Figure 4When the electromagnetic shielding layer 52 is specifically set, in order to avoid the electromagnetic shielding layer 52 from directly contacting the probe body 54 and generating new interference signals, the accommodating space 511 includes a top wall 512 on the side corresponding to the measuring end of the probe body 54. The electromagnetic shielding layer 52 is set on the outer surface of the probe base 51 and at least covers the top wall 512. The top wall 512 is used to isolate the electromagnetic shielding layer 52 from the probe body 54.
[0050] Specifically, the thickness of the top wall 512 is 120 microns to 240 microns, and the thickness of the portion of the probe cover 53 corresponding to the top wall 512 is 120 microns to 240 microns. By setting the thickness of the top wall 512 to 120 microns to 240 microns, the electromagnetic shielding layer 52 can be prevented from physically directly contacting the probe body 54, and the shielding effect of the electromagnetic shielding layer 52 can be guaranteed as much as possible.
[0051] In this embodiment, Figure 5 As shown, the probe base 51 may be a cylindrical structure, the opening of the accommodation space 511 is at the bottom of the probe base 51, and after the probe body 54 is placed in the accommodation space 511 from bottom to top, it can be fixed in the probe base 51 through a mounting plate.
[0052] Specifically, Figure 4 , 5 As shown in FIG. 6 , the probe base 51 may include a boss 513, and the shape of the boss 513 matches the accommodating space 511. The accommodating space 511 includes a first accommodating cavity 5111 and a second accommodating cavity 5112 that are connected. The first accommodating cavity is located inside the boss 513 and is used to place the probe body 54. The second accommodating cavity is located below the boss 513 and is used to set a mounting plate for fixing the probe body 54.
[0053] After the probe body 54 is placed in the accommodating space 511 , the probe body 54 is located in the first accommodating cavity inside the boss 513 , and the measuring head of the probe body 54 faces the top of the boss 513 .
[0054] like Figure 7 As shown, the probe body 54 includes a cylindrical body around which a detection coil 541 and an excitation coil 542 are wound. When the probe body 54 is placed in the accommodating space 511 , one end of the cylinder where the detection coil 541 is located is the measuring end, which is located at the top of the accommodating space 511 .
[0055] When the probe base 51 includes the boss 513, the electromagnetic shielding layer 52 can be arranged on the top surface of the boss 513 to at least cover the measuring head of the probe body 54, so as to save costs by minimizing the area of the electromagnetic shielding layer 52. Alternatively, the electromagnetic shielding layer 52 is arranged on the top surface and side surfaces of the boss 513 to enhance the shielding effect.
[0056] In this embodiment, the boss 513 can also be used to fix the probe cover 53. The probe cover 53 may include a groove that matches the shape of the boss 513. Through the cooperation between the boss 513 and the groove, the probe cover 53 can be simply, conveniently and accurately fixed on the probe base 51.
[0057] Furthermore, the first wall of the groove may correspond to the top wall 512 of the probe base 51, and its thickness may be 120 microns to 240 microns. By setting the thickness of the portion of the probe cover 53 corresponding to the top wall 512 to 120 microns to 240 microns, direct contact between the electromagnetic shielding layer 52 and the polishing pad 21 can be avoided, and the loss of the electromagnetic shielding layer 52 caused by the replacement process of the polishing pad 21 can be reduced. At the same time, the distance between the probe body 54 and the wafer above the polishing pad 21 is within a preset range, thereby ensuring the accuracy of measuring the thickness of the metal film on the wafer.
[0058] In addition, the side wall of the boss 513 includes a rectangular side wall 514 and an arcuate side wall 515. When the electromagnetic shielding layer 52 is arranged on the top surface and the side surface of the boss 513, the arcuate side wall 515 can be used to install and position the probe cover 53; the rectangular side wall 514 can be used to set the electromagnetic shielding layer 52, that is, the electromagnetic shielding layer 52 covers the surface of the rectangular side wall 514. Compared with the arcuate side wall 515, the rectangular side wall 514 is more convenient for processing the electromagnetic shielding layer 52, making the process of adding the electromagnetic shielding layer 52 simpler.
[0059] The probe base 51 is a probe base 51 made of a heat insulating material, and / or the probe cover 53 is a probe cover 53 made of a heat insulating material. The heat insulating material may be PEI, PVC, PVDF, etc.
[0060] The probe base 51 and the probe cover 53 are also provided with corresponding through holes for fixing the eddy current sensor probe on the polishing plate 20 .
[0061] To facilitate disassembly, see Figure 8 The side wall of the probe cover 53 may be provided with an annular groove.
[0062] The eddy current sensor probe and chemical mechanical polishing equipment according to the present application have at least the following beneficial effects:
[0063] (1) The eddy current sensor performs contactless measurement through an electromagnetic field. The magnetic flux density at the measuring end is the largest and is also most affected by noise. The solution provided in this embodiment can effectively reduce the interference of noise on the measuring end by providing a measuring end that at least covers the probe body on the probe base, thereby ensuring the measurement accuracy of the eddy current sensor. In addition, by providing a probe cover, the loss of the electromagnetic shielding layer caused by the replacement process of the polishing pad can be reduced, thereby ensuring a long service life of the electromagnetic shielding layer.
[0064] (2) The accommodating space includes a top wall on a side corresponding to the measuring end of the probe body, and the electromagnetic shielding layer is arranged on the outer surface of the probe base and at least covers the top wall, so as to avoid direct contact between the electromagnetic shielding layer and the probe body to generate new interference signals.
[0065] (3) The thickness of the part of the probe cover corresponding to the top wall is 120 μm to 240 μm, which can avoid direct contact between the electromagnetic shielding layer and the polishing pad, reduce the loss of the electromagnetic shielding layer caused by the replacement process of the polishing pad, and at the same time make the distance between the probe body and the wafer above the polishing pad within the preset range, ensuring the accuracy of the measurement of the metal film thickness on the wafer.
[0066] (4) The boss on the probe base includes a rectangular side wall, which is convenient for processing the electromagnetic shielding layer.
[0067] (5) The probe base and / or probe cover are made of heat-insulating material, which can reduce the impact of ambient temperature changes on the measurement results of the eddy current sensor.
[0068] The following is an explanation of the installation and use of the eddy current probe:
[0069] During installation, the probe body 54 can be placed in the accommodation space 511 from bottom to top, and the lower part of the probe body 54 can be fixed to the probe base 51 through the mounting plate.
[0070] Afterwards, the probe cover 53 can be aligned with the probe base 51 , and screws are passed through the through holes of the probe cover 53 and the probe base 51 to fix them on the polishing plate 20 .
[0071] It should be noted that, in this article, relational terms such as first and second are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "comprise a ..." do not exclude the existence of other identical factors in the process, method, article or device including the elements.
[0072] Finally, it should be noted that the above are only preferred embodiments of the present invention, which are only used to illustrate the technical solution of the present invention, and are not used to limit the protection scope of the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.
Claims
1. An eddy current sensor probe for chemical mechanical polishing equipment, characterized in that: The eddy current sensor probe is arranged on a polishing disk of a chemical mechanical polishing device and contacts with a polishing pad. The eddy current sensor probe comprises: The probe base is provided with a receiving space for receiving the probe body; An electromagnetic shielding layer, disposed on the probe base and at least covering the measuring end of the probe body, for shielding noise; The probe cover is fixedly arranged on the probe base and is used to isolate the electromagnetic shielding layer from the polishing pad of the chemical mechanical polishing equipment.
2. The eddy current sensor probe according to claim 1, characterized in that: The thickness of the electromagnetic shielding layer is 50 microns to 120 microns.
3. The eddy current sensor probe according to claim 1, characterized in that: The electromagnetic shielding layer is a conductive film.
4. The eddy current sensor probe according to any one of claims 1 to 3, characterized in that: The accommodating space includes a top wall on one side corresponding to the measuring end of the probe body, the electromagnetic shielding layer is arranged on the outer surface of the probe base and at least covers the top wall, and the top wall is used to isolate the electromagnetic shielding layer from the probe body.
5. The eddy current sensor probe according to claim 4, characterized in that: The thickness of the top wall is 120 microns to 240 microns, and the thickness of the portion of the probe cover corresponding to the top wall is 120 microns to 240 microns.
6. The eddy current sensor probe according to claim 1, characterized in that: The probe base includes a boss, the shape of the boss matches the accommodating space, and the measuring head of the probe body faces the top of the boss; the electromagnetic shielding layer is arranged on the top surface of the boss, or the electromagnetic shielding layer is arranged on the top surface and side surface of the boss.
7. The eddy current sensor probe according to claim 6, characterized in that: The side walls of the boss include rectangular side walls and arc-shaped side walls. When the electromagnetic shielding layer is arranged on the top surface and the side surface of the boss, the electromagnetic shielding layer covers the surface of the rectangular side wall, and the arc-shaped side wall is used to install and position the probe cover.
8. The eddy current sensor probe according to claim 6, characterized in that: The probe cover comprises a groove matched with the shape of the boss.
9. The eddy current sensor probe according to claim 1, characterized in that: The probe base is a probe base made of a heat-insulating material, and / or the probe cover is a probe cover made of a heat-insulating material.
10. A chemical mechanical polishing device, characterized in that: include: A carrier head for holding a wafer and driving the wafer to rotate, a polishing plate covered with a polishing pad, a dresser for dressing the polishing pad, and a liquid supply part for providing polishing liquid, wherein the polishing plate is provided with an eddy current sensor probe as described in any one of claims 1-9.
Citation Information
Cited By
Auxiliary driving device, polishing mechanism for wafer processing and polishing equipment