Anti-bonding system for asphalt reclaimed material production

By adding fine material pipes and electronic weighing bins in the production process of asphalt recycled materials, the problem of small-grained asphalt recycled materials being bonded to the warehouse wall is solved, significantly reducing the amount of materials hanging on the warehouse wall and the labor intensity of workers, and improving production efficiency.

CN222024828UActive Publication Date: 2024-11-19MACHENG YIFA ASPHALT ROAD CONSTRUCTION ENGINEERING CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420377681.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-28
Publication Date
2024-11-19
Estimated Expiration
2034-02-28

AI Technical Summary

Technical Problem

During the production process of asphalt recycled materials, small-grained asphalt recycled materials are easily bonded to the wall of the recycled temporary storage warehouse under heating and extrusion of hot asphalt crude material, resulting in an increase in the wall hanging material of the warehouse, and the labor intensity of workers is high and production Inefficient.

Method used

An anti-bonding system was designed. By adding a fine material pipe at the fine material outlet of the screw conveyor, small particles of asphalt recycled material are sent to the fine material silo, and then the proportion is controlled through the electronic weighing silo and then sent to the mixing cylinder to reduce the The asphalt recycled material bonded to the inner wall of the recycled temporary storage bin.

Benefits of technology

The amount of material hanging on the inner wall of the recycled temporary storage warehouse has been effectively reduced, from 1.5 tons to 200 kilograms, and the cleaning time of workers has been shortened from one day to one hour, which has significantly reduced the labor intensity of workers and improved production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222024828U_ABST
    Figure CN222024828U_ABST
Patent Text Reader

Abstract

The utility model discloses an anti-bonding system for asphalt reclaimed material production, which comprises a settling bin, a screw conveyer, a temporary regeneration storage bin and a fine material bin, asphalt reclaimed materials with various particle sizes are loaded in the settling bin, the screw conveyer is used for conveying the asphalt reclaimed materials in the settling bin to the temporary regeneration storage bin, and the fine material bin is used for conveying the asphalt reclaimed materials in the settling bin to the temporary regeneration storage bin. The regeneration temporary storage bin is provided with a feeding port used for adding hot asphalt coarse materials, a fine material outlet is formed in the side wall of the lower portion of the front end of a discharging port of a machine shell of the spiral conveyor and connected with a fine material pipe, the fine material pipe is communicated with a fine material bin, and weighing bins with electronic scales are arranged at outlets in the lower ends of the regeneration temporary storage bin and the fine material bin. And a discharge port of the weighing bin is connected with a stirring cylinder. According to the utility model, materials attached to the wall of the regeneration temporary storage bin can be greatly reduced, the labor intensity of workers is reduced, and the production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of regeneration of old asphalt mixtures, in particular to an anti-adhesion system for the production of asphalt regeneration materials. Background Art

[0002] Asphalt concrete is widely used in the construction of various highways and roads. Asphalt concrete pavement is affected by various factors such as load-bearing, climate and asphalt performance, which can cause damage to the asphalt pavement. In highway construction and maintenance projects, various materials such as gravel and asphalt in the old asphalt mixture recycled during the renovation and maintenance of asphalt concrete pavement can be recycled, which is also one of the national green environmental protection and resource protection tasks.

[0003] For the recycling of old asphalt mixture, the moisture in the stone can be removed by heating, and the asphalt can be softened and have a certain fluidity. After adding some asphalt recycled materials and mixing with additives and other materials, it can be used as asphalt mixture for constructing asphalt pavement again.

[0004] The current process flow is as follows: asphalt recycled materials of various particle sizes are mixed evenly by rollers and sent to sedimentation bins, and then sent to regeneration temporary storage bins by screw conveyors. At the same time, hot asphalt coarse material is added to the regeneration temporary storage bin, and finally sent to the mixing tank for mixing. After mixing, it is put into use. It is found in use that small particles of asphalt recycled materials themselves have no stickiness, but under the heating and extrusion of hot asphalt coarse material, there will be a lot of small particles of asphalt recycled materials sticking to the walls of the regeneration temporary storage bin. In actual production, a 4-ton regeneration temporary storage bin will have up to 1.5 tons of material hanging on the bin wall after producing more than 1,000 tons, seriously affecting production. Two workers are required to enter the regeneration temporary storage bin for a day of cleaning, which puts a lot of labor intensity on the workers and affects production over a long period of time. Utility Model Content

[0005] In order to solve the shortcomings and deficiencies of the prior art, an anti-adhesion system for asphalt recycled material production is provided, which can significantly reduce the material attached to the wall of the recycled temporary storage bin, reduce the labor intensity of workers, and improve production efficiency.

[0006] In order to achieve the purpose of the utility model, an anti-sticking system for asphalt recycled material production is provided, including a sedimentation bin, a screw conveyor, a regeneration temporary storage bin and a fine material bin, the sedimentation bin is loaded with asphalt recycled material of various particle sizes, the screw conveyor is used to transport the asphalt recycled material in the sedimentation bin to the regeneration temporary storage bin, the regeneration temporary storage bin is provided with a feeding port for adding hot asphalt coarse material, the casing of the screw conveyor is provided with a fine material outlet on the lower side wall at the front end of the discharge port, the fine material outlet is connected with a fine material pipe, and the fine material pipe is connected with the fine material bin, the regeneration temporary storage bin and the fine material bin are both provided with weighing bins with electronic scales at the lower end outlets, and the discharge port of the weighing bin is connected with a stirring cylinder.

[0007] The beneficial effects of the utility model are:

[0008] Compared with the prior art, the utility model provides an anti-adhesion system for the production of asphalt recycled materials. Compared with the existing production of asphalt recycled materials, a fine material bin is added. When the screw conveyor is conveying asphalt recycled materials, small particles of asphalt recycled materials will be squeezed to the inner wall of the casing of the screw conveyor by large particles of asphalt recycled materials. Through the newly added fine material outlet, a large amount of small particles of asphalt recycled materials that would originally adhere to the inner wall of the regeneration temporary storage bin are sent to the fine material bin through the fine material outlet and the fine material pipe, and then through the matching weighing bin to control the mixing ratio, and then sent to the mixing tank.

[0009] After adopting this technical solution, when producing the same 1,000 tons of finished products, the amount of material hanging on the inner wall of the regenerated temporary storage bin has been greatly reduced from 1.5 tons to 200 kilograms. Workers only need 1 hour to do it, which greatly reduces the labor intensity of workers and greatly reduces the equipment downtime, thereby improving efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] The specific implementation of the utility model is further described in detail below with reference to the accompanying drawings, wherein:

[0011] Figure 1 It is a structural schematic diagram of the utility model. DETAILED DESCRIPTION

[0012] like Figure 1As shown, the utility model provides an anti-adhesion system for asphalt recycled material production, including a sedimentation bin, a screw conveyor 1, a regeneration temporary storage bin 2 and a fine material bin 3. The sedimentation bin is loaded with asphalt recycled materials of various particle sizes. The screw conveyor 1 is used to convey the asphalt recycled materials in the sedimentation bin to the regeneration temporary storage bin 2. The regeneration temporary storage bin 2 is provided with a feeding port 4 for adding hot asphalt coarse material. The casing of the screw conveyor 1 is provided with a fine material outlet on the lower side wall of the front end of the discharge port. The fine material outlet is connected to a fine material pipe 5, which is communicated with the fine material bin 3. The regeneration temporary storage bin 2 and the fine material bin 3 are both provided with a weighing bin 6 with an electronic scale at the lower end outlet, and the discharge port of the weighing bin 6 is connected to a stirring cylinder 7.

[0013] The above embodiments are not limited to the technical solutions of the embodiments themselves, and the embodiments can be combined with each other to form new embodiments. The above embodiments are only used to illustrate the technical solutions of the utility model and are not intended to limit them. Any modification or equivalent replacement that does not deviate from the spirit and scope of the utility model shall be included in the scope of the technical solution of the utility model.

Claims

1. An anti-adhesion system for asphalt recycled material production, characterized by: It includes a sedimentation bin, a screw conveyor, a regeneration temporary storage bin and a fine material bin. The sedimentation bin is loaded with asphalt regeneration materials of various particle sizes. The screw conveyor is used to transport the asphalt regeneration materials in the sedimentation bin to the regeneration temporary storage bin. The regeneration temporary storage bin is provided with a feeding port for adding hot asphalt coarse material. The casing of the screw conveyor is provided with a fine material outlet on the lower side wall at the front end of the discharge port. The fine material outlet is connected with a fine material pipe, and the fine material pipe is connected with the fine material bin. The lower end outlets of the regeneration temporary storage bin and the fine material bin are both provided with weighing bins with electronic scales, and the discharge port of the weighing bin is connected with a stirring cylinder.

Citation Information

Cited By

  • Bucket entering method for preventing bonding after dehydration and impurity removal of recycled asphalt pavement waste

    CN120867166A