Preshaping tool for flattened original part of capacitor

By using the stacking structure and jack pressure of aluminum plates and pressure plates in the pre-set tooling of capacitor flattening originals, the problem of excessive film gap in the process of spraying gold first and then setting is solved, avoiding the entry of metal zinc and improving the electrical performance of the capacitor .

CN222028965UActive Publication Date: 2024-11-19NINGBO JIANGBEI GOFRONT HERONG ELECTRIC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202422477488.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-10-14
Publication Date
2024-11-19
Estimated Expiration
2034-10-14

AI Technical Summary

Technical Problem

In the process of spraying gold first and then setting, the film gap is too large due to the unshaping of the original, and metal zinc enters the inside of the component, reducing the insulation performance and affecting the electrical performance of the capacitor.

Method used

The pre-determined tooling for flattening the original parts is used to stack the aluminum plate and the pressure plate. By stacking the aluminum plate and the pressure plate, the jack applies pressure to the flattening original parts to ensure that the film gap is appropriate and metal zinc is avoided from entering.

Benefits of technology

The molding quality of the gold spraying process is improved, and the insulation performance is reduced is avoided and the electrical performance of the capacitor is ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222028965U_ABST
    Figure CN222028965U_ABST
Patent Text Reader

Abstract

The utility model provides a pre-shaping tool for a flattened original part of a capacitor, and relates to the technical field of capacitors. The capacitor flattened original piece pre-shaping tool comprises a base, aluminum plates and a pressing plate, the pressing plate is located above the base, the multiple aluminum plates are stacked between the base and the pressing plate, and the area between the adjacent aluminum plates is used for containing flattened original pieces which are wound. And the pressing plate is used for pressing the flattening original piece under the pressure applied by the jack. Pre-shaping of the flattened element is achieved before the technology of first metal spraying and then shaping is carried out, so that in the process of carrying out the technology of first metal spraying and then shaping, gaps between films wound on the flattened element can be prevented from being too large, metal zinc is prevented from entering the element in the metal spraying process, and then the insulation performance is prevented from being reduced; therefore, the forming quality of the metal spraying and shaping process is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of capacitors, in particular to a capacitor flattening original pre-forming tool. Background Art

[0002] At present, the hot forming of dry flattened components of film capacitors usually adopts the process of first spraying gold and then forming. During the process of first spraying gold and then forming, the flattened original component is not formed before spraying gold, which leads to excessive gaps between films. During the spraying process, metal zinc enters the interior of the component, resulting in a reduction in the inter-electrode gap and reduced insulation performance, thus affecting the electrical performance of the capacitor. Utility Model Content

[0003] The problem solved by the utility model is how to improve the molding quality of the process of first spraying gold and then finalizing the shape.

[0004] In order to solve the above problems, the utility model provides a capacitor flattened component pre-forming tooling, including a base, an aluminum plate and a pressure plate, wherein the pressure plate is located above the base, and multiple aluminum plates are stacked between the base and the pressure plate. The area between adjacent aluminum plates is used to place the wound flattened component, and the pressure plate is used to press down the flattened component under the pressure applied by a jack.

[0005] Optionally, the capacitor flattened component pre-forming tooling further comprises a plurality of guide posts, which are distributed along the circumference of the base and installed between the base and the pressing plate, and the plurality of guide posts are all slidably connected to the pressing plate.

[0006] Optionally, the capacitor flattening component pre-forming tooling also includes a plurality of springs, the plurality of springs correspond one-to-one to the plurality of guide pillars, each of the springs is sleeved on one of the guide pillars, and each of the springs is connected between the base and the pressure plate.

[0007] Optionally, the capacitor flattening component pre-forming tooling also includes a plurality of locking nuts, the plurality of locking nuts correspond one-to-one to the plurality of guide columns, each of the locking nuts is threadedly connected to the corresponding guide column, and each of the locking nuts is located on the side of the pressure plate away from the base.

[0008] Optionally, a placement hole is provided on the pressure plate, and the placement hole is used to place the disassembled locking nut.

[0009] Optionally, the capacitor flattened component pre-forming tool further includes two legs, and the two legs are installed at one end of the base away from the pressing plate.

[0010] Optionally, a handle is provided on the pressing plate.

[0011] Optionally, the capacitor flattened component pre-forming tool further includes an auxiliary alignment tool, and the auxiliary alignment tool is used to align the multiple aluminum plates in the stacking direction.

[0012] Optionally, the guide column is connected to the base via a threaded fastener.

[0013] Optionally, the large surface area of ​​the pressure plate is larger than the large surface area of ​​the aluminum plate.

[0014] Compared with the prior art, the capacitor flattened original pre-forming tooling of the utility model is that a plurality of aluminum plates are stacked between a base and a pressing plate located above the base, and the wound flattened original is placed between adjacent aluminum plates. The adjacent aluminum plates can separate the flattened components to ensure that the flattened components between adjacent layers will not affect each other's deformation. The pressing plate is then used to press down the aluminum plate through a jack, so that the flattened components between adjacent aluminum plates can be flattened and shaped. In this way, the pre-forming of the flattened components is achieved before the implementation of the gold spraying and then shaping process. Therefore, in the process of implementing the gold spraying and then shaping process, it is possible to avoid the gap between the films wrapped around the flattened components being too large, and to avoid the metal zinc from entering the component during the gold spraying process, thereby avoiding the reduction of insulation performance, thereby improving the molding quality of the gold spraying and then shaping process. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a structural schematic diagram of a capacitor flattening component pre-forming tooling in an embodiment of the utility model;

[0016] Figure 2 It is a schematic diagram of the jack in the embodiment of the utility model when it is pressed down.

[0017] Description of reference numerals:

[0018] 1-base; 2-aluminum plate; 3-pressure plate; 31-placement hole; 4-guide column; 5-locking nut; 6-leg; 10-flattened original; 20-jack. DETAILED DESCRIPTION

[0019] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and understandable, the specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0020] In the accompanying drawings, the Z axis represents the vertical position, and the positive direction of the Z axis (that is, the direction in which the arrow of the Z axis points) represents the upper side, and the negative direction of the Z axis (that is, the direction opposite to the positive direction of the Z axis) represents the lower side; in the accompanying drawings, the X axis represents the horizontal position, and the positive direction of the X axis (that is, the direction in which the arrow of the X axis points) represents the right side, and the negative direction of the X axis (that is, the direction opposite to the positive direction of the X axis) represents the left side; in the accompanying drawings, the Y axis represents the front and rear positions, and the positive direction of the Y axis (that is, the direction in which the arrow of the Y axis points) represents the front side, and the negative direction of the Y axis (that is, the direction opposite to the positive direction of the Y axis) represents the rear side. It should also be noted that the aforementioned Z axis, Y axis, and X axis are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation to the present invention.

[0021] It should be noted that the terms "first", "second", etc. in the specification and claims of the present utility model and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the utility model described herein can be implemented in an order other than those illustrated or described herein.

[0022] Traditional film capacitor dry-type flattened components are usually heat-formed by spraying gold first and then forming. During the process of spraying gold first and then forming, since the components are not formed first, the gap between the films is too large. During the spraying process, metal zinc enters the interior of the component, resulting in a reduction in the inter-electrode gap and reduced insulation performance, which affects the electrical performance of the capacitor.

[0023] Among them, heat setting means: due to the heat shrinkage of polypropylene film, the solid film will shrink after being heated to a certain temperature, thereby reducing the film gap in the capacitor element, and the stress in the winding process of the element can be effectively released. The shape of the element is finalized, and it will not change or move due to heat during the subsequent use of the capacitor. Gold spraying means: a layer of metal zinc is evenly attached to the two end faces of the film capacitor, i.e. the two poles, by arc spraying, so that the capacitor end face has the ability to pass large currents, and also provides a carrier for subsequent soldering connection operations to avoid high temperature burns to the film during soldering, thereby avoiding affecting the electrical performance and life of the capacitor.

[0024] Combination Figure 1 and Figure 2 As shown, the utility model provides a capacitor flattened component pre-forming tooling, including a base 1, an aluminum plate 2 and a pressing plate 3, wherein the pressing plate 3 is located above the base 1, and a plurality of aluminum plates 2 are stacked between the base 1 and the pressing plate 3, and an area between adjacent aluminum plates 2 is used for placing a wound flattened component 10, and the pressing plate 3 is used for pressing down the flattened component 10 under the pressure applied by a jack 20.

[0025] It should be noted that the capacitor flattened component pre-forming tooling provided in this embodiment is used before the gold spraying and then shaping process.

[0026] Specifically, the base 1 can be placed on a workbench of the forming process, and the upper end surface of the base 1 is ensured to be a horizontal plane. Multiple aluminum plates 2 are stacked layer by layer on the upper end surface of the base 1, and the flattened original 10 that has been wound (the flattened original 10 is a flattened original 10 that has been wound along the circumference of the flattened original 10) is placed between adjacent aluminum plates 2, and then the pressing plate 3 is stacked on the uppermost aluminum plate 2, so that the multi-layer aluminum plates 2 are located between the pressing plate 3 and the base 1, so as to realize the positioning of the multi-layer aluminum plates 2 and the flattened element 10 between the adjacent aluminum plates 2, and the jack 20 is fixed on the upper end surface of the pressing plate 3, as shown in FIG. Figure 2 As shown, after the telescopic end of the jack 20 abuts against the frame, the pressure of the jack 20 can be maintained at 45MPA, so that the extension of the telescopic end of the jack 20 can be used to apply downward pressure to the pressure plate 3. Under the action of this pressure, the flattened original 10 is flattened, so that the flattened original 10 is pre-shaped before the gold spraying and then shaping process, so as to avoid excessive film gaps on the flattened original 10. After pre-shaping, it can be placed at room temperature for 20 hours for static pressure shaping to release some stress. After the pre-shaping is completed, the pre-shaped flattened original 10 is taken out from between the adjacent aluminum plates 2 in turn, and the taken out multiple flattened elements 10 (such as 10-15) are packaged with plastic steel to be fixed as a whole group, and the gold spraying operation is carried out in groups. After gold spraying, the whole group is not disassembled and placed in an oven for conventional heat setting process. Pay attention to keeping gaps between groups to ensure uniform heating.

[0027] Therefore, in this embodiment, a plurality of aluminum plates 2 are stacked between a base 1 and a pressing plate 3 located above the base 1, and the wound flattened original component 10 is placed in the area between adjacent aluminum plates 2. The adjacent aluminum plates 2 can separate the flattened components 10 to ensure that the flattened components 10 between adjacent layers do not affect each other's deformation. The pressing plate 3 is then used to press down the flattened original component 10 under the pressure applied by the jack 20, so that the flattened components 10 between adjacent aluminum plates 2 can be flattened and shaped. In this way, the pre-shaping of the flattened components 10 is achieved before the implementation of the gold spraying and then shaping process. Therefore, in the process of implementing the gold spraying and then shaping process, it is possible to avoid the gap between the films wound on the flattened components 10 being too large, and to avoid the metal zinc from entering the component during the gold spraying process, thereby avoiding the reduction of insulation performance, thereby improving the molding quality of the gold spraying and then shaping process.

[0028] Optionally, combined Figure 1 As shown, the capacitor flattened component pre-forming tooling also includes a plurality of guide posts 4, which are distributed along the circumference of the base 1 and installed between the base 1 and the pressing plate 3, and the plurality of guide posts 4 are all slidably connected to the pressing plate 3.

[0029] Specifically, there can be four guide columns 4, and the four guide columns 4 are distributed along the circumference of the base 1. Four positioning grooves are also provided on the base 1, and the notches of the positioning grooves are downward. The upper ends of the four guide columns 4 pass through the four positioning grooves from bottom to top and extend from the positioning grooves, and the lower end of any guide column 4 can be installed in the positioning groove by a threaded fastener. The pressure plate 3 is provided with four through holes and is sleeved on the four guide columns 4 through four through holes to slide along the axial direction of the four guide columns 4.

[0030] In this way, multiple guide columns 4 are distributed along the circumference of the base 1 and installed between the base 1 and the pressure plate 3, and the multiple guide columns 4 are all slidably connected to the pressure plate 3. The multiple guide columns 4 can limit the pressure plate 3 horizontally and adjust the position of the pressure plate 3 in the vertical direction, thereby changing the vertical distance between the pressure plate 3 and the base 1, so as to place different layers of aluminum plates 2 between the pressure plate 3 and the base 1 to improve the flexibility of use.

[0031] Optionally, the capacitor flattening component pre-forming tooling also includes multiple springs, the multiple springs correspond to the multiple guide pillars 4 one by one, each spring is sleeved on a guide pillar 4, and each spring is connected between the base 1 and the pressure plate 3.

[0032] Specifically, in combination with the above, the number of springs is four, and the four springs are respectively sleeved on different guide pillars 4, and the two ends of any spring in the axial direction are respectively connected to the base 1 and the pressure plate 3.

[0033] In this way, multiple springs correspond to multiple guide columns 4 one by one, each spring is sleeved on a guide column 4, and each spring is connected between the base 1 and the pressure plate 3. After the jack 20 is removed, the spring can lift the pressure plate 3 to a certain distance, so as to facilitate the removal of the aluminum plate 2 and the flattening element 10 between the pressure plate 3 and the base 1, and prevent the pressure plate 3 from falling vertically and injuring the workers during the removal process.

[0034] Optionally, combined Figure 1 As shown, the capacitor flattening component pre-forming tooling also includes a plurality of locking nuts 5, and the plurality of locking nuts 5 correspond one by one to the plurality of guide columns 4. Each locking nut 5 is threadedly connected to the corresponding guide column 4, and each locking nut 5 is located on the side of the pressure plate away from the base 1.

[0035] Specifically, the number of locking nuts 5 can be four, and the four locking nuts 5 are respectively threadedly connected to different guide posts 4, and the four locking nuts 5 can limit the pressing plate 3 to prevent the spring from pushing the pressing plate 3 away from the guide post 4. In this way, multiple locking nuts 5 are used to correspond to multiple guide posts 4 one by one, each locking nut 5 is threadedly connected to the corresponding guide post 4, and each locking nut 5 is located on the side of the top plate away from the base 1. The locking nuts 5 can limit the pressing plate 3 to prevent the pressing plate 3 from being separated from the guide post 4 under the elastic force of the spring, thereby improving the safety of the pressing plate 3.

[0036] Optionally, combined Figure 1 As shown, a placement hole 31 is provided on the pressure plate 3, and the placement hole 31 is used to place the disassembled locking nut 5.

[0037] Specifically, two placement holes 31 can be provided, and the two placement holes 31 can prevent the disassembled locking nut 5. In this way, the placement holes 31 are provided on the pressing plate 3, and the placement holes 31 are used to place the disassembled locking nut 5. The placement holes 31 can provide a placement position for the locking nut 5, so as to facilitate the storage of the disassembled locking nut 5 and ensure the cleanliness of the workbench.

[0038] Optionally, combined Figure 1 As shown, the capacitor flattened component pre-forming tooling also includes two legs 6, and the two legs 6 are installed at one end of the base 1 away from the pressing plate 3.

[0039] Specifically, the legs 6 can be two vertical plates, which are welded or integrally formed at the lower end of the base 1, so that a certain distance is left between the base 1 and the workbench. In this way, by installing the two legs 6 at one end of the base 1 away from the pressing plate 3, the two legs 6 can support the base 1, so that a certain distance is left between the base 1 and the workbench, so that the fork plate of the forklift can be extended between the base 1 and the workbench, thereby facilitating the transportation of the base 1.

[0040] Optionally, combined Figure 1 As shown, a handle is provided on the pressing plate 3. In this way, the handle can be convenient for holding the pressing plate 3, and the pressing plate 3 can be installed on the guide column 4 by only manually lifting the pressing plate 3.

[0041] Optionally, the capacitor flattened component pre-forming tool further includes an auxiliary alignment tool, which is used to align the multiple aluminum plates 2 in the stacking direction.

[0042] Specifically, the auxiliary alignment tool can be a steel ruler or a long plate. After multiple aluminum plates 2 are stacked on the base 1, the steel ruler or the long plate is used to align the multiple aluminum plates 2 so that the multiple aluminum plates 2 are located on the same central axis.

[0043] In this way, the auxiliary alignment tool is used to align multiple aluminum plates 2 in the stacking direction to prevent the aluminum plates 2 from shifting in the vertical direction, thereby ensuring that the aluminum plates 2 are not overloaded during the pressing process of the pressing plate 3 to ensure the stacking accuracy of the multiple aluminum plates 2.

[0044] Optionally, the guide post 4 is connected to the base 1 via a threaded fastener, so that the connection stability between the guide post 4 and the base 1 can be ensured, and the guide post 4 can be easily disassembled, so that the guide post 4 can be replaced in time.

[0045] Optionally, combined Figure 1 As shown, the large surface area of ​​the pressing plate 3 is larger than the large surface area of ​​the aluminum plate 2.

[0046] Specifically, the large surface of the pressing plate 3 and the large surface of the aluminum plate 2 refer to the sides with the largest areas of the pressing plate 3 and the aluminum plate 2. When in use, the large surface of the pressing plate 3 is in contact with the large surface of the top aluminum plate 2, and it is ensured that the large surface area of ​​the pressing plate 3 is larger than the large surface area of ​​the aluminum plate 2, so that the pressing plate 3 can completely cover the top aluminum plate 2.

[0047] In this way, by making the large surface area of ​​the pressing plate 3 larger than the large surface area of ​​the aluminum plate 2 , it is ensured that the pressing plate 3 can completely cover the uppermost aluminum plate 2 , so as to ensure that the force applied to the aluminum plate 2 is uniform.

[0048] Although the disclosure is as above, the protection scope of the disclosure is not limited thereto. Those skilled in the art may make various changes and modifications without departing from the spirit and scope of the disclosure, and these changes and modifications will fall within the protection scope of the utility model.

Claims

1. A capacitor flattening original pre-forming tool, characterized in that: The invention comprises a base (1), an aluminum plate (2) and a pressing plate (3), wherein the pressing plate (3) is located above the base (1), a plurality of the aluminum plates (2) are stacked between the base (1) and the pressing plate (3), an area between adjacent aluminum plates (2) is used to place a flattened original part (10) that has been wound, and the pressing plate (3) is used to press down the flattened original part (10) under the pressure applied by a jack (20).

2. The capacitor flattening component pre-forming tooling according to claim 1 is characterized in that: It also includes a plurality of guide columns (4), which are distributed along the circumference of the base (1) and installed between the base (1) and the pressure plate (3), and the plurality of guide columns (4) are all slidably connected to the pressure plate (3).

3. The capacitor flattening component pre-forming tool according to claim 2, characterized in that: It also includes a plurality of springs, the plurality of springs corresponding one-to-one to the plurality of guide posts (4), each of the springs being sleeved on one of the guide posts (4), and each of the springs being connected between the base (1) and the pressure plate (3).

4. The capacitor flattening component pre-forming tooling according to claim 2, characterized in that: It also includes a plurality of locking nuts (5), wherein the plurality of locking nuts (5) correspond one-to-one to the plurality of guide posts (4), each of the locking nuts (5) is threadedly connected to the corresponding guide post (4), and each of the locking nuts (5) is located on a side of the pressure plate (3) facing away from the base (1).

5. The capacitor flattening component pre-forming tool according to claim 4, characterized in that: The pressing plate (3) is provided with a placement hole (31), and the placement hole (31) is used to place the disassembled locking nut (5).

6. The capacitor flattening component pre-forming tool according to claim 1, characterized in that: It also comprises two supporting legs (6), wherein the two supporting legs (6) are mounted on an end of the base (1) away from the pressing plate (3).

7. The capacitor flattening component pre-forming tool according to claim 1, characterized in that: The pressing plate (3) is provided with a handle.

8. The capacitor flattened component pre-forming tool according to claim 1, characterized in that: It also includes an auxiliary alignment tool, which is used to align the multiple aluminum plates (2) in the stacking direction.

9. The capacitor flattened component pre-forming tool according to claim 2, characterized in that: The guide column (4) is connected to the base (1) via a threaded fastener.

10. The capacitor flattened component pre-forming tooling according to claim 2, characterized in that: The large surface area of ​​the pressing plate (3) is larger than the large surface area of ​​the aluminum plate (2).