Screw extruder for IXPP film
By introducing dust removal and preheating mechanisms into the screw extruder, the problems of particle adhesion and dust impact are solved, and smoother extrusion molding is achieved and product quality is improved.
Patent Information
- Application Number
- CN202420634938.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-28
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-03-28
AI Technical Summary
When used in existing screw extruders, the particles directly enter the melting section will cause adhesion to the machine arm, affecting use, and excessive dust on the particles during feeding will lead to poor product quality.
A spiral extruder for IXPP film is designed, which includes a dust removal mechanism and a preheating mechanism. The dust removal mechanism removes dust through an air pump and a gas pipe. The preheating mechanism preheats the particles through a heating rod and an air pump, so that the particles enter the melting section. Soften before, avoid adhesion and remove dust through the filter and barrier nets.
Through preheating and dust removal treatment, the particles are ensured not affected by instantaneous high heat when entering the melting stage, improving the smoothness of extrusion molding and product quality.
Smart Images

Figure CN222039520U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of IXPP production, and in particular relates to a screw extruder for IXPP film. Background Art
[0002] Extruder is a type of plastic machinery, which originated in the 18th century. According to the direction of the material flow in the die and the angle between the center line of the screw, the die head can be divided into right-angle die head and bevel die head. The screw extruder relies on the pressure and shear force generated by the rotation of the screw to fully plasticize and evenly mix the material and form it through the die. Plastic extruders can be basically classified into twin-screw extruders, single-screw extruders, and the rare multi-screw extruders and screwless extruders.
[0003] IXPP is irradiated cross-linked polypropylene foam, also known as PPFOAM, which is a new type of environmentally friendly PP foam material. The main raw materials of IXPP are polypropylene resin (PP) and other special fillers, supplemented by auxiliary materials such as foaming agents. After melt mixing and extrusion molding, it is subjected to green and healthy ion radiation cross-linking through irradiation processing technology, and then continuously foamed at high temperature to form a foam product. IXPP foam is a functional polymer foam material that meets international environmental standards. It has good thermal stability (maximum operating temperature can reach 130°C), high toughness, tensile strength, impact strength and other excellent mechanical properties. At this stage, this material is mainly used in automotive soft interior, foam tape, battery insulation and other fields.
[0004] IXPP uses a screw extruder during production. IXPP is in the form of tiny particles before entering the screw extruder, and then it is melted and extruded inside the screw extruder. However, the existing screw extruder has the following disadvantages when used:
[0005] 1. When the screw extruder melts and extrudes the particles, it usually does so in the middle section. Therefore, the particles need to run a certain distance through the extrusion roller in the front section of the screw extruder. However, if the particles directly enter the melting section, some particles will stick to the machine arm due to direct contact with high heat, affecting its use.
[0006] 2. If there is too much dust attached to the particles when the screw extruder is feeding, it will lead to poor product quality. Utility Model Content
[0007] The utility model aims to provide a screw extruder for IXPP film, so as to solve the technical problems that when particles directly enter the melting section, some particles will be adhered to the machine arm due to direct contact with high heat, affecting the use, and if too much dust is attached to the particles during feeding, it will lead to poor product quality, so as to achieve the purpose of solving the problem of particles sticking to the machine arm and processing the dust on the particles during feeding.
[0008] In order to solve the above technical problems, the utility model provides a screw extruder for IXPP film, comprising: an extruder body, a fixed room is provided on the extruder body, a mounting room is installed on the front of the fixed room, a feed hopper is also provided on the top of the fixed room, masterbatch particles will reach the inside of the extruder body through the feed hopper and the fixed room, and in the process of the masterbatch particles falling, a dust removal mechanism located on the back side of the feed hopper will process the dust on the masterbatch particles.
[0009] A preheating mechanism is provided inside the installation room, and the preheating mechanism preheats the masterbatch particles inside the extruder body so that the masterbatch particles are softened in advance.
[0010] Furthermore, a sealing cover plate is provided on the top of the feed hopper, and the sealing cover plate is connected to the feed hopper via a hinge.
[0011] Furthermore, the dust removal mechanism includes a mechanism shell, a first air pump is provided inside the mechanism shell, an air inlet pipe is provided on the left side of the first air pump, an air outlet pipe is provided on the right side of the first air pump, and the first air pump is fixed on the fixed room by a fixing block.
[0012] Furthermore, the preheating mechanism includes a mechanism panel, a plurality of heating rods are provided at the bottom of the mechanism panel, a second air pump is provided on the back side of the plurality of heating rods, an air collecting port is provided between the second air pump and the heating rods, and a connecting pipe is also provided on the back side of the second air pump.
[0013] Furthermore, two air inlet holes are provided on the extruder body and located in the inner section of the fixed room, and the two air inlet holes are connected to each other through a sealing pipe and a connecting pipe.
[0014] Furthermore, an extrusion rod is provided inside the extruder, and a driving motor is provided on the left side of the extrusion rod, and the driving motor can drive the extrusion rod to rotate.
[0015] Furthermore, a barrier net is provided at the front section of the feed hopper, a fixing column is fixedly connected to the bottom of the fixing room, and a filter net is provided at the front of the installation room.
[0016] The beneficial effects of the utility model are:
[0017] 1. Through the design of the preheating mechanism, the preheating mechanism can preheat the masterbatch particles in the front section when they enter the extruder body. During the preheating process, the masterbatch particles will slowly soften due to heat, and then when entering the middle melting section of the extruder, the masterbatch particles will not be instantly subjected to high heat, thereby making the softening extrusion molding process smoother.
[0018] 2. Through the design of the dust removal mechanism, the dust removal mechanism can remove the dust on the masterbatch particles during the falling process of the masterbatch particles, and then the dust attached to the masterbatch particles can be blown out of the device, so that the product quality is better during subsequent extrusion molding.
[0019] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0021] Figure 1 It is a schematic diagram of the main structure of the utility model;
[0022] Figure 2 It is the front view of the internal structure of the fixing room and the installation room of the utility model;
[0023] Figure 3 It is a schematic diagram of the side cross-sectional structure of the dust removal mechanism of the utility model.
[0024] In the figure:
[0025] 1. Extruder body;
[0026] 2. Fixed room;
[0027] 3. Installation room;
[0028] 4. Feed hopper;
[0029] 5. Dust removal mechanism; 51. Mechanism housing; 52. First air pump; 53. Air inlet pipe; 54. Air outlet pipe; 55. Fixed block;
[0030] 6. Preheating mechanism; 61. Mechanism panel; 62. Heating rod; 63. Second air pump; 64. Air collecting port; 65. Connecting pipe;
[0031] 7. Sealing cover plate;
[0032] 8. Air intake hole;
[0033] 9. Seal the pipeline;
[0034] 10. Extrusion rod;
[0035] 11. Driving motor;
[0036] 12. Barrier net;
[0037] 13. Fixed column;
[0038] 14. Filter. DETAILED DESCRIPTION
[0039] In order to make the purpose, technical solution and advantages of the embodiments of the utility model clearer, the technical solution of the utility model will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0040] Example:
[0041] like Figures 1 to 3 As shown, a screw extruder for IXPP film includes an extruder body 1, a fixed room 2 is provided on the extruder body 1, a mounting room 3 is installed on the front of the fixed room 2, and a feed hopper 4 is also provided on the top of the fixed room 2. The masterbatch particles will reach the inside of the extruder body 1 through the feed hopper 4 and the fixed room 2, and in the process of the masterbatch particles falling, the dust removal mechanism 5 located on the back side of the feed hopper 4 will process the dust on the masterbatch particles. A preheating mechanism 6 is provided inside the mounting room 3, and the preheating mechanism 6 will preheat the masterbatch particles located inside the extruder body 1. Preheating can soften the masterbatch particles in advance. The preheating mechanism 6 can preheat the masterbatch particles in the front section when they enter the extruder body 1. During the preheating process, the masterbatch particles will slowly soften due to heat, and then when entering the middle melting section of the extruder, the masterbatch particles will not be instantly subjected to high heat, thereby making the softening extrusion molding process smoother. The dust removal mechanism 5 can remove the dust on the masterbatch particles during their falling process, and then blow the dust attached to the masterbatch particles out of the device, so that the product quality is better during subsequent extrusion molding.
[0042] like Figures 1 to 3As shown, further, a sealing cover plate 7 is provided on the top of the feed hopper 4, and the sealing cover plate 7 is connected to the feed hopper 4 through a hinge. The sealing cover plate 7 can be closed when no feeding is needed, thereby preventing dust from entering the feed hopper 4. The dust removal mechanism 5 includes a mechanism shell 51, and a first air pump 52 is provided inside the mechanism shell 51. An air inlet pipe 53 is provided on the left side of the first air pump 52, and an air outlet pipe 54 is provided on the right side of the first air pump 52. The first air pump 52 is fixed to the fixed room 2 through a fixing block 55. The preheating mechanism 6 includes a mechanism panel 61, and a plurality of heating rods 62 are provided at the bottom of the mechanism panel 61. A second air pump 63 is provided on the back side of the plurality of heating rods 62. An air collecting port 64 is provided between the second air pump 63 and the heating rods 62. A connecting pipe 65 is also provided on the back side of the air pump 63. The heating panel can control the opening and closing of the heating rod 62. The heating rod 62 can heat the surrounding air. Two air inlet holes 8 are provided on the extruder body 1 and located in the inner section of the fixed room 2. The two air inlet holes 8 are connected to the connecting pipe 65 through a sealed pipe 9. The hot air will reach the sealed pipe 9 through the connecting pipe 65, and then enter the extruder body 1 through the air inlet holes 8. An extrusion rod 10 is also provided inside the extruder. A drive motor 11 is provided on the left side of the extrusion rod 10. The drive motor 11 can drive the extrusion rod 10 to rotate. A barrier net 12 is also provided in the front section of the feed hopper 4. A fixed column 13 is also fixedly connected to the bottom of the fixed room 2. A filter net 14 is also provided on the front of the installation room 3.
[0043] To summarize, first, the masterbatch particles will enter the extruder body 1 through the feed hopper 4. During the falling process of the masterbatch particles, the dust removal mechanism 5 will be started first. At this time, the first air pump 52 will be started and the outside air will be sucked in through the air inlet pipe 53, and the inside of the feed hopper 4 will be blown through the air outlet pipe 54, so that the dust on the masterbatch particles can pass through the barrier net 12 to the outside of the device, thereby completing the dust removal work on the outer surface of the masterbatch particles. When the masterbatch particles reach the inside of the extruder body 1, the preheating mechanism 6 will be started at this time, and the heating rod 62 will be started through the mechanism panel 61 to heat the surrounding air. Then the second air pump 63 will be started, and the heated air will be sent through the air collecting port 64 through the connecting pipe 65 and the sealing pipe 9 to the air inlet 8, and then the hot air will be sent to the inside of the extruder body 1 through the air inlet 8, thereby preheating the masterbatch particles located inside the extruder body 1.
[0044] The various devices selected in this application are all universal standard parts or parts known to those skilled in the art, and their structures and principles can be known to those skilled in the art through technical manuals or conventional experimental methods.
[0045] In the description of the embodiments of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0046] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0047] Based on the above ideal embodiments of the utility model, the relevant staff can make various changes and modifications without deviating from the technical concept of the utility model through the above description. The technical scope of the utility model is not limited to the content of the specification, and its technical scope must be determined according to the scope of the claims.
Claims
1. A screw extruder for IXPP film, characterized in that, include: An extruder body (1) is provided with a fixed room (2), a mounting room (3) is installed on the front of the fixed room (2), and a feed hopper (4) is also provided on the top of the fixed room (2). The masterbatch particles will reach the inside of the extruder body (1) through the feed hopper (4) and the fixed room (2), and during the falling process of the masterbatch particles, a dust removal mechanism (5) located on the back side of the feed hopper (4) will process the dust on the masterbatch particles. A preheating mechanism (6) is provided inside the installation room (3), and the preheating mechanism (6) preheats the masterbatch particles inside the extruder body (1), so that the masterbatch particles are softened in advance.
2. A screw extruder for IXPP film according to claim 1, characterized in that, A sealing cover plate (7) is also provided on the top of the feed hopper (4), and the sealing cover plate (7) is connected to the feed hopper (4) via a hinge.
3. A screw extruder for IXPP film as claimed in claim 1, characterized in that: The dust removal mechanism (5) comprises a mechanism housing (51), a first air pump (52) is arranged inside the mechanism housing (51), an air inlet pipe (53) is arranged on the left side of the first air pump (52), an air outlet pipe (54) is arranged on the right side of the first air pump (52), and the first air pump (52) is fixed to the fixed room (2) via a fixing block (55).
4. A screw extruder for IXPP film as claimed in claim 1, characterized in that: The preheating mechanism (6) comprises a mechanism panel (61), a plurality of heating rods (62) are provided at the bottom of the mechanism panel (61), a second air pump (63) is provided on the back side of the plurality of heating rods (62), an air collecting port (64) is provided between the second air pump (63) and the heating rods (62), and a connecting pipe (65) is also provided on the back side of the second air pump (63).
5. A screw extruder for IXPP film as claimed in claim 1 or 4, characterized in that: Two air inlet holes (8) are provided on the extruder body (1) and located in the inner section of the fixed room (2), and the two air inlet holes (8) are connected to each other through a sealing pipe (9) and a connecting pipe (65).
6. A screw extruder for IXPP film as claimed in claim 5, characterized in that: An extrusion rod (10) is also provided inside the extruder, and a driving motor (11) is provided on the left side of the extrusion rod (10), and the driving motor (11) can drive the extrusion rod (10) to rotate.
7. A screw extruder for IXPP film as claimed in claim 1, characterized in that: The front section of the feed hopper (4) is also provided with a barrier net (12), the bottom of the fixed room (2) is also fixedly connected with a fixed column (13), and the front of the installation room (3) is also provided with a filter net (14).