Novel single-mode and multi-mode dual-purpose communication optical fiber
By using a combination of germanium-doped single-mode core, germanium-doped multi-mode core and pure silica cladding in the optical fiber, a light guide structure is formed, which solves the light leakage problem caused by microbending of single-mode fibers and expands the optical fiber. The application scenarios and service life realize mutual updates between single-mode and multi-mode devices.
Patent Information
- Application Number
- CN202420033573.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-08
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-01-08
AI Technical Summary
Existing single-mode and multi-mode fibers have problems with limited transmission rates and light leakage in applications, especially when single-mode fibers are bending, light intensity is easily escaped, resulting in fiber damage.
A new optical fiber consisting of a germanium-doped single-mode core, a germanium-doped multi-mode core and a pure silica cladding is used to form a light guide structure to block light intensity through step-by-step or gradient-type refractive index profile distribution, and combine with MCVD Process preparation increases the microbending resistance and service life of the optical fiber.
It realizes the avoidance of light leakage in single-mode and multi-mode dual-purpose optical fibers, extends the service life of the optical fibers, and supports the mutual update and replacement of equipment, without the need to replace optical fiber wiring, and is suitable for high-speed data transmission and iterative equipment maintenance.
Smart Images

Figure CN222050515U_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of optical fibers, and in particular to a novel single-mode and multi-mode dual-purpose communication optical fiber. Background Art
[0002] There are two major categories of communication optical fibers, single-mode optical fibers and multimode optical fibers.
[0003] The dispersion of multimode fiber includes inter-modal dispersion and intra-modal dispersion. In the transmission of optical fiber digital signals, the input optical pulse is divided into various modes from the fundamental mode to the highest-order mode in the multimode fiber. Each mode carries a part of the pulse power and is recombined into an output optical pulse at the output end. However, due to the different transmission time of each mode in the optical fiber, the time to reach the output end is different, resulting in output pulse broadening, which is inter-modal dispersion. The inter-modal dispersion of multimode fiber with a step-type refractive index profile is very large, which seriously restricts the transmission rate of the optical fiber. Therefore, multimode fiber with a gradient refractive index profile is used to make each order mode have basically the same transmission time in the optical fiber, thereby significantly reducing the inter-modal dispersion and increasing the transmission rate. Intra-modal dispersion means that a single-mode pulse is composed of different wavelength components. Due to the different transmission times of different wavelength components in the optical fiber, the output pulse is broadened. Therefore, intra-modal dispersion can also be called wavelength dispersion. Wavelength dispersion includes material dispersion and waveguide dispersion. Waveguide dispersion plays an important role in single-mode optical fiber, but can be ignored in multimode optical fiber. Therefore, the intra-mode dispersion of multimode optical fiber, or wavelength dispersion, mainly refers to material dispersion. Material dispersion is the pulse broadening caused by the dispersion characteristics of the material: since the refractive index of the optical fiber material (silicon dioxide) is a function of the wavelength in the infrared band, that is, , and the speed of light waves in the medium is , c is the speed of light, so the propagation speed of light waves varies with wavelength, resulting in material dispersion. At a wavelength of 1300nm, the material dispersion is zero, and it is in the low-loss window of the optical fiber, so the operating wavelength of the multimode optical fiber is 850nm and 1300nm. The wavelength dispersion coefficient at a wavelength of 850nm can be calculated from the zero dispersion wavelength λ0 and the zero dispersion slope S0 of the multimode optical fiber. The laser-optimized optical fiber using VCSEL laser as the light source is a multimode optical fiber with a gradient refractive index profile of 50 / 125μm, and the operating wavelength is 850nm.
[0004] The wavelength dispersion of single-mode optical fiber includes the sum of material dispersion and waveguide dispersion. The two have opposite signs and cancel each other out. Zero dispersion is at 1310nm, so the pulse broadening of single-mode optical fiber is very small and can transmit high-speed pulse signals. The fundamental mode HE is transmitted in single-mode optical fiber. 11 model. Summary of the invention
[0005] The main technical problem solved by the present invention is to provide a new type of single-mode and multi-mode dual-purpose communication optical fiber, which can be used as both a single-mode optical fiber and a multi-mode optical fiber, thereby expanding the application scenarios and having a long service life. When the dual-purpose optical fiber of this patent is used as a single-mode optical fiber, no light leakage will occur when the optical fiber is bent.
[0006] In order to solve the above technical problems, a technical solution adopted by the present invention is: to provide a new type of single-mode and multi-mode dual-purpose communication optical fiber, comprising a germanium-doped single-mode fiber core, a germanium-doped multi-mode fiber core and a pure silica cladding arranged concentrically from the inside to the outside, wherein the germanium-doped multi-mode fiber core comprises a step-type refractive index profile distribution or a gradient-type refractive index profile distribution, and the refractive index difference between the germanium-doped multi-mode fiber core and the pure silica cladding is , The refractive index difference between the germanium-doped single-mode fiber core and the germanium-doped silica cladding is , ,in is the refractive index of pure silica cladding, is the refractive index of the germanium-doped multimode fiber core, is the refractive index of the germanium-doped single-mode fiber core.
[0007] In a preferred embodiment of the present invention, the core diameter of the germanium-doped single-mode fiber core is smaller than the core diameter of the germanium-doped multi-mode fiber core.
[0008] In a preferred embodiment of the present invention, the core diameter of the germanium-doped single-mode fiber core is 8.3 μm, the core diameter of the germanium-doped multi-mode fiber core is 50 μm, and the diameter of the pure silica cladding is 125 μm.
[0009] In a preferred embodiment of the present invention, the germanium-doped multimode fiber core and the pure silica cladding form a light-guiding structure to block the light intensity refracted by the germanium-doped single-mode fiber core.
[0010] In order to solve the above technical problems, another technical solution adopted by the present invention is: to provide a novel preparation process of single-mode and multi-mode dual-purpose communication optical fiber, comprising the following steps:
[0011] a. Preform rod production: Place the quartz substrate tube on the glass lathe and rotate it. Use ultra-pure oxygen as carrier gas to enter the quartz substrate tube together with saturated vapor of SiCl4 and GeCl4. The outer wall of the quartz substrate tube is heated by an oxyhydrogen flame at a temperature of 1400-1600℃. The gas phase material in the tube undergoes oxidation reaction at high temperature through heat conduction. The generated oxide forms a deposition layer of porous glass dust on the inner wall of the tube downstream of the high temperature zone. When the high temperature zone of the next wave of oxyhydrogen flame passes through this place, the glass dust is sintered into a uniform transparent glass layer deposited on the inner wall. The oxyhydrogen torch moves slowly from left to right once to form a corresponding deposition layer, and then quickly returns to the original position for the second deposition, and repeats this process until the specified deposition is completed; the quartz substrate tube will serve as the outer cladding part, and the deposition layer will be deposited layer by layer from the cladding to the core. When the deposition is completed, there is still a small hole in the center, and the preform rod enters the burn-out stage. The raw material gas flow is stopped, and the flame temperature rises to about 1800℃ to burn and shrink the quartz tube to form a solid optical fiber preform rod;
[0012] b. Fiber drawing: Insert the fiber preform into the drawing furnace for high-temperature drawing at 2200℃ to form the optical fiber. After the optical fiber is drawn, plastic resin is directly coated on the drawing tower to protect the optical fiber.
[0013] In a preferred embodiment of the present invention, the reaction formula of the oxidation reaction of the gas phase material in the tube at high temperature in step a is: SiCl4+O2→SiO2+2Cl2↑; GeCl4+O2→GeO2+2Cl2↑.
[0014] In a preferred embodiment of the present invention, the chlorine gas generated by the reaction during the deposition process in step a and the gas phase material that has not reacted completely are discharged from the outlet of the quartz substrate tube for waste gas neutralization treatment.
[0015] In a preferred embodiment of the present invention, the refractive index profile in step a is controlled by adjusting the flow rate of the carrier gas of each raw material composition using a mass flow controller.
[0016] In a preferred embodiment of the present invention, in order to reduce the microbending loss of the optical fiber in step b, the coating is usually divided into two layers, the coating diameter is 242±5µm, and the coating is divided into inner and outer layers. The inner coating diameter is 180-190µm, and the inner coating needs to use a coating with a low Young's modulus to improve the anti-microbending performance of the optical fiber, and the Young's modulus of the inner coating is 0.5-2MPa; the outer coating uses a coating with a higher Young's modulus to increase the mechanical and environmental protection performance of the optical fiber, and the Young's modulus of the outer coating should be greater than 600MPa, and UV-curable acrylic resin is used as the coating material.
[0017] The beneficial effect of the present invention is that the novel single-mode and multi-mode dual-purpose communication optical fiber of the present invention, in the single-mode and multi-mode dual-purpose optical fiber, when used as a single-mode jumper, even if the optical fiber is damaged due to micro-bending and the light intensity is refracted out of the cladding, it still falls into its multi-mode fiber core and is blocked by the light-guiding structure of the multi-mode fiber core / cladding interface, so it will not escape from the optical fiber and cause optical fiber leakage.
[0018] The novel single-mode and multi-mode dual-purpose communication optical fiber of the present invention can directly replace the equipment applicable to the novel single-mode and multi-mode dual-purpose communication optical fiber without replacing the optical fiber and rewiring, has a long service life, and is suitable for mutual updating and replacement of single-mode and multi-mode equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work, among which:
[0020] Figure 1 It is a cross-sectional view of the novel single-mode and multi-mode dual-purpose communication optical fiber of the present invention;
[0021] Figure 2 yes Figure 1 A cross-sectional view of
[0022] Figure 3 It is a combined diagram of a multimode fiber core and a single-mode fiber core with a step-index refractive index profile;
[0023] Figure 4 It is a combined diagram of a multimode fiber core with a gradient refractive index profile and a single-mode fiber core;
[0024] Figure 5 It is a graph of the refractive index of silicon dioxide as a function of the doping amount;
[0025] Figure 6 Schematic diagram of the MCVD process;
[0026] The components in the accompanying drawings are marked as follows: 1. germanium-doped single-mode fiber core, 2. germanium-doped multi-mode fiber core, 3. pure silica cladding. DETAILED DESCRIPTION
[0027] The technical scheme in the embodiment of the present invention will be described clearly and completely below. The structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification, so that people familiar with this technology can understand and read them, and are not used to limit the limiting conditions that the present invention can implement, so they have no substantial technical significance. Any modification of the structure, change of the proportional relationship, or adjustment of the size should still fall within the scope that the technical content disclosed by the present invention can cover without affecting the effects that the present invention can produce and the purposes that can be achieved. At the same time, the terms such as "upper", "lower", "left", "right", "middle" and so on quoted in this specification are only for the convenience of narration, and are not used to limit the scope that can be implemented. The change or adjustment of the relative relationship should also be regarded as the scope that the present invention can implement without substantially changing the technical content.
[0028] See also Figure 1 and Figure 2 A new type of single-mode and multi-mode dual-purpose communication optical fiber comprises a germanium-doped single-mode fiber core 1, a germanium-doped multi-mode fiber core 2 and a pure silica cladding 3 which are arranged concentrically from the inside to the outside. The germanium-doped multi-mode fiber core 2 comprises a step-type refractive index profile distribution or a gradient-type refractive index profile distribution, and the refractive index difference between the germanium-doped multi-mode fiber core and the pure silica cladding is , , the refractive index difference between the germanium-doped single-mode core and the germanium-doped silica cladding is , ,in is the refractive index of pure silica cladding, is the refractive index of the germanium-doped multimode fiber core, is the refractive index of the germanium-doped single-mode fiber core.
[0029] The core diameter of the germanium-doped single-mode fiber core 1 is smaller than the core diameter of the germanium-doped multimode fiber core 2. The core diameter of the germanium-doped single-mode fiber core 1 is 8.3 μm, the core diameter of the germanium-doped multimode fiber core 2 is 50 μm, and the diameter of the pure silica cladding 3 is 125 μm.
[0030] When the new single-mode and multi-mode dual-purpose communication optical fiber works as a multi-mode optical fiber, it can be divided into two structures: step refractive index profile distribution and gradient refractive index profile distribution. The gradient refractive index profile curve is parabolic. Figure 3 and Figure 4 From the refractive index profile, it can be seen that there is a small convex refractive index in the center of the multimode optical fiber, which has a slight disturbance to the light field in the center of the multimode optical fiber, but will not affect the transmission of the multimode optical fiber.
[0031] When the new single-mode and multi-mode dual-purpose communication optical fiber works as a single-mode optical fiber, the central core of the optical fiber is 8.3μm, the core / cladding refractive index difference is 0.3%, and when the operating wavelength is 1310nm, the mode field diameter is 8.6-9.2μm; the cut-off wavelength is 1260nm; and the zero dispersion wavelength is 1300-1324nm.
[0032] The germanium-doped multimode fiber core 2 and the pure silica cladding 3 form a light-guiding structure to block the light intensity refracted by the germanium-doped single-mode fiber core 1 .
[0033] The screening stress of the new single-mode and multi-mode dual-purpose communication optical fiber is 100kpsi.
[0034] One of the application scenarios of the new single-mode and multi-mode dual-purpose communication optical fiber: single-mode and multi-mode dual-purpose optical fiber can be used as single-mode patch cord and multi-mode patch cord.
[0035] Usually in single-mode fiber jumpers, due to the process of making the fiber tight cladding, when the take-up tension is too tight or the wiring is uneven, the fiber will be damaged by microbending stress. Because part of the light intensity of the single-mode fiber itself is distributed in the cladding, the fiber damage caused by microbending will cause part of the light intensity to escape from the fiber, resulting in light leakage. In single-mode and multi-mode dual-purpose optical fibers, when used as single-mode jumpers, even if the light intensity of the optical fiber is refracted out of the cladding due to microbending damage, it still falls into its multi-mode core and is blocked by the light-guiding structure of the multi-mode core / cladding interface, so it will not escape from the fiber and cause light leakage.
[0036] New single-mode and multi-mode dual-purpose communication optical fiber application scenario 2: Update and maintenance of data center and other equipment
[0037] Data centers have data transmission equipment and fiber optic cabling. Data transmission equipment includes switches and servers. Currently, there are single-mode or multi-mode devices in the market, and there are single-mode and multi-mode cabling optical fibers. Social progress has led to an increasing demand for data, so the equipment in the computer room is constantly updated and iterated. When data equipment needs to be upgraded, if the single-mode and multi-mode basic equipment needs to be changed, the corresponding cabling optical fiber also needs to be changed. However, if single-mode and multi-mode dual-purpose optical fibers are used, there is no need to replace the cabling optical fiber. The service life of optical fiber is long, usually up to more than 20 years, which is much less than the replacement frequency of equipment, which makes it easier to upgrade and iterate the maintenance of data equipment.
[0038] The third application scenario of the new single-mode and multi-mode dual-purpose communication optical fiber:
[0039] Not only in the data center field, but also in the field of integrated wiring (smart buildings, etc.) and various fiber optic wiring systems, single-mode and multi-mode dual-purpose optical fibers are suitable for the mutual update and replacement of single-mode and multi-mode equipment.
[0040] A novel preparation process for single-mode and multi-mode dual-purpose communication optical fiber comprises the following steps:
[0041] a. Preform rod production: Optical fiber preform rods can be made using the common MCVD process or PCVD process. Here, the MCVD process is described as follows:
[0042] The quartz substrate tube is placed on a glass lathe and rotated. Ultrapure oxygen is used as a carrier gas to enter the quartz substrate tube together with saturated vapor of SiCl4 and GeCl4. The outer wall of the quartz substrate tube is heated by an oxyhydrogen flame at a temperature of 1400-1600°C. The gas phase material in the tube undergoes an oxidation reaction at high temperature through heat conduction. The reaction formula for the oxidation reaction of the gas phase material in the tube at high temperature is: SiCl4+O2→SiO2+2Cl2↑; GeCl4+O2→GeO2+2Cl2↑. The generated oxides such as SiO2 and GeO2 form a deposition layer of porous glass dust on the inner wall of the tube downstream of the air flow in the high temperature zone. When the high temperature zone of the next wave of oxyhydrogen flame passes through this place, the glass dust is sintered into a uniform transparent glass layer deposited on the inner wall. The oxyhydrogen torch moves slowly from left to right once to form a corresponding deposition layer, and then quickly returns to its original position for a second deposition, and repeats this process until the specified deposition is completed.
[0043] The chlorine gas produced by the reaction during the deposition process and the gaseous materials that have not reacted completely are discharged from the outlet of the quartz substrate tube for waste gas neutralization treatment. The quartz substrate tube will serve as the outer cladding part, and the deposition layer will be deposited layer by layer from the cladding to the core. In the matrix of silica, the refractive index can be changed by a small amount of doping, and doping GeO2 helps to increase the refractive index. The refractive index profile is controlled by adjusting the flow rate of the carrier gas composed of each raw material with a mass flow controller (MFC). When the deposition is completed, there is still a small hole in the center, and the preform enters the burn-out stage. The raw material gas flow is stopped, and the flame temperature rises to about 1800°C, and the quartz tube is burned and shrunk to form a solid optical fiber preform.
[0044] In the matrix of silicon dioxide, its refractive index can be changed by a small amount of doping. Figure 5 It shows the refractive index of doped silica as a function of the doping amount. As can be seen from the figure, doping with GeO2 and P2O5 helps to increase the refractive index, while doping with fluorine reduces the refractive index. For example, the refractive index of pure silica as the cladding is 1.458, and the refractive index of the core doped with three percent GeO2 increases to 1.463, which is the refractive index profile of the G.652 matched single-mode optical fiber.
[0045] b. Fiber drawing: Insert the fiber preform into the drawing furnace for high-temperature drawing at 2200℃ to draw the fiber into an optical fiber. The drawing tension is set to 30-45g. The optical fiber formed by these processing parameters is less susceptible to the stress induced by drawing, which is unfavorable to the optical transmission properties of the optical fiber (including waveguide propagation performance). After the optical fiber is drawn, the plastic resin is directly coated on the drawing tower to protect the optical fiber. In order to reduce the microbending loss of the optical fiber, it is usually coated in two layers, with a coating diameter of 242±5µm, and the coating is divided into inner and outer layers. The inner coating diameter is 180-190µm. The inner coating needs to use a low Young's modulus coating to improve the microbending resistance of the optical fiber. The Young's modulus of the inner coating is 0.5-2MPa. The outer coating uses a coating with a higher Young's modulus to increase the mechanical and environmental protection properties of the optical fiber. The Young's modulus of the outer coating should be greater than 600MPa. UV-curable acrylic resin is generally used as the coating material.
[0046] Different from the prior art, the new single-mode and multi-mode dual-purpose communication optical fiber of the present invention can be used as both single-mode optical fiber and multi-mode optical fiber, which expands the application scenarios, has a long service life, and avoids the situation where optical fiber is damaged and part of the light intensity escapes from the optical fiber.
[0047] The present invention and its embodiments are described schematically above, and the description is not restrictive. The drawings show only one embodiment of the present invention, and the actual structure is not limited thereto. Therefore, if a person skilled in the art is inspired by it and designs a structural method and an embodiment similar to the technical solution without creativity without departing from the purpose of the invention, they shall all fall within the protection scope of the present invention.
Claims
1. A new type of single-mode and multi-mode dual-purpose communication optical fiber, characterized in that: The invention comprises a germanium-doped single-mode fiber core, a germanium-doped multimode fiber core and a pure silica cladding arranged concentrically from the inside to the outside, wherein the germanium-doped multimode fiber core comprises a step-type refractive index profile distribution or a gradient-type refractive index profile distribution, and the refractive index difference between the germanium-doped multimode fiber core and the pure silica cladding is , The refractive index difference between the germanium-doped single-mode fiber core and the germanium-doped silica cladding is , ,in is the refractive index of pure silica cladding, is the refractive index of the germanium-doped multimode fiber core, is the refractive index of the germanium-doped single-mode fiber core, the core diameter of the germanium-doped single-mode fiber core is 8.3 μm, the core diameter of the germanium-doped multimode fiber core is 50 μm, and the diameter of the pure silica cladding is 125 μm.
2. The novel single-mode and multi-mode dual-purpose communication optical fiber according to claim 1 is characterized in that: The core diameter of the germanium-doped single-mode fiber core is smaller than the core diameter of the germanium-doped multi-mode fiber core.
3. The novel single-mode and multi-mode dual-purpose communication optical fiber according to claim 1 or 2, characterized in that: The germanium-doped multimode fiber core and the pure silicon dioxide cladding form a light-guiding structure to block the light intensity refracted by the germanium-doped single-mode fiber core.