Local annealing device for screws
By designing a local annealing device for screws, using the combination of a medium-temperature salt bath furnace and a heat dissipation hole insulation layer, the problem of difficult to control and overheating in the prior art is solved, and precise heating and slow cooling of local annealing of screws is achieved. Ensures balanced tissue formation and product functional stability.
Patent Information
- Application Number
- CN202323569882.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-26
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2033-12-26
AI Technical Summary
The existing flame heating, induction heating and lead bath heating methods have problems such as difficulty in precise control of the heating temperature, overheating or overburning, oxidative decarbonization and unbalanced structure formation in local annealing of screws, especially in bending or riveting, which can easily lead to products. Function failed.
Design a local annealing device including upper mold, lower mold and medium temperature salt bath furnace. The screw head heating is realized through heat dissipation holes and heat insulation layer to avoid rapid heating of other parts, and local heating and cooling are used to use the stable heat source of the salt bath furnace to perform local heating and slow cooling. , ensure the formation of balanced tissue.
Accurate heating and slow cooling of local annealing of screws is achieved, overheating and oxidation and decarbonization are avoided, the balanced structure of the product is ensured, and the reliability and safety of bending and riveting are improved.
Smart Images

Figure CN222064603U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of annealing devices, in particular to a local annealing device for screws. Background Art
[0002] Annealing, also known as annealing or high temperature annealing, is a process of heating the product to above Ac1 and Ac3 (phase change to pearlite structure occurs) or below Ac1 (no phase change occurs, stress is eliminated and hardness is reduced), keeping the product warm and then slowly cooling it (air cooling after low temperature annealing). Some heat-treated products usually need to be partially annealed to meet the needs of bending, riveting and reducing hardness. This type of annealing obviously belongs to annealing with phase change. In order to achieve local annealing (tempering), various forms of heating are usually adopted, such as local flame heating, local induction heating and local lead bath heating.
[0003] The methods commonly used to achieve local annealing heating of products are flame heating, induction heating and lead bath heating. Due to many problems, the local annealing process of products is difficult to implement smoothly. Its main disadvantages are:
[0004] (1) The advantage of flame heating is that it is easy to operate and can accurately control the local heating position. The disadvantage is that the heating temperature is difficult to accurately control, and it is difficult to ensure the stable heating temperature required for phase change. The product heating process is prone to overheating or even overburning, especially the oxidation and decarburization of the heated part of the product is serious, the austenitization heating transfer of the structure is insufficient, and the annealing and slow cooling are difficult to achieve, and the balanced structure required for annealing cannot be guaranteed. Its "pseudo-annealing" structure is easy to crack during bending or riveting, resulting in product failure.
[0005] (2) Induction heating is a rapid heating method. Its advantages are simple operation, high production efficiency, and the ability to accurately control the local heating position and heating depth. It has great advantages if used for rapid heating and quenching of the product surface, but it has many problems if used for local annealing of the product. The main problem is that due to the skin effect, the temperature is mainly concentrated on the surface of the local annealing area of the product. It is difficult to achieve uniform heating and heat preservation of the entire annealing area. The degree of austenitization and tissue transfer cannot be fully guaranteed. The heating temperature is difficult to accurately control. Abnormal tissues are easily formed during the heating process. There is a certain degree of oxidation and decarburization. Annealing and slow cooling cannot be achieved, and the balanced tissue required for annealing cannot be obtained. The annealing and softening effect is limited. The area that has been locally annealed by induction heating is very easy to break during bending or riveting.
[0006] (3) Lead bath heating is a common method for local annealing. The process is stable and mature, easy to operate, and easy to accurately control the heating temperature, holding time and local heating position. It can achieve slow cooling of annealing and obtain balanced structure, and generally will not cause overheating or overburning. The disadvantage is that the lead bath heating temperature is relatively low, it is difficult to achieve normal austenitization heating, and the length of the product annealing transition zone is difficult to effectively control. In particular, when heated to above 400°C, a large amount of lead vapor is generated, which is rapidly oxidized to lead oxide in the air, forming smoke and dust that is absorbed by the human body and causes lead poisoning. Lead poisoning can cause significant damage to the human hematopoietic system, central nervous system, renal function, cardiovascular system and reproductive system. It is a process that the state has explicitly ordered to be eliminated.
[0007] Therefore, it is necessary to design a local annealing device for screws, combined with a stable heat source of a medium-temperature salt bath to realize the local heating annealing process of the screws, overcome the shortcomings of flame heating, induction heating and lead bath heating, ensure the needs of the local annealing process of the product, and improve the heat treatment local annealing process methods and safeguards. Utility Model Content
[0008] The purpose of the utility model is to overcome the above technical deficiencies and provide a local annealing device for screws to solve the problem that the local annealing process of the product is difficult to implement smoothly in the prior art using flame heating, induction heating and lead bath heating.
[0009] In order to achieve the above technical purpose, the utility model adopts the following technical solutions:
[0010] The utility model provides a local annealing device for screws, comprising an upper die, a lower die and a salt bath furnace, wherein a heating medium is contained in the salt bath furnace, a heat dissipation hole is provided in the upper die, a first through hole and a second through hole connected to the first through hole are provided in the lower die, an inner wall of the first through hole is provided with a heat insulation layer, when the upper die and the lower die can be fixedly connected via a connecting piece, the central axes of the heat dissipation hole, the first through hole and the second through hole coincide with each other, the screw can be passed through the first through hole and the second through hole, the tail of the screw extends into the heat dissipation hole, the head of the screw extends to the outside of the lower die, contacts with the liquid surface of the heating medium through the lower die, and the heat insulation layer is located above the liquid surface of the heating medium, so as to allow the head of the screw to extend into the heating medium.
[0011] In some embodiments, an annular groove is opened in the lower mold, and the central axis of the annular groove coincides with the central axis of the first through hole and the second through hole, and a water-containing asbestos felt layer is arranged in the annular groove, and the water-containing asbestos felt layer is fixed between the upper mold and the lower mold.
[0012] In some embodiments, the connecting member includes a locking rod and two locking blocks, the locking rod is inserted into the upper mold and the lower mold, and the opposite ends of the locking rod are respectively connected to the two locking blocks to fix the upper mold and the lower mold.
[0013] In some embodiments, the connecting member further includes a hanging ring, which is disposed above the upper mold and fixedly connected to one end of the locking rod.
[0014] In some embodiments, a groove and a first connecting hole connected to the groove are provided in the upper mold, a second connecting hole is opened in the lower mold, the locking rod is sequentially inserted into the first connecting hole, the groove and the second connecting hole, and a temperature-resistant asbestos pad is provided in the groove and is sleeved on the locking rod.
[0015] In some embodiments, a layer of charcoal particles is laid on the liquid surface of the heating medium.
[0016] In some embodiments, the heating medium may be sodium chloride, potassium chloride, barium chloride, sodium cyanide, potassium cyanide, sodium nitrate, or potassium nitrate.
[0017] In some embodiments, the screw has a model of M5x18mm.
[0018] In some embodiments, the upper mold and the lower mold are both made of heat insulation board.
[0019] In some embodiments, the thermal insulation layer is a dry asbestos felt layer.
[0020] Compared with the prior art, the utility model provides a local annealing device for screws, wherein a heat dissipation hole is opened in the upper mold, a first through hole and a second through hole connected to the first through hole are opened in the lower mold, an inner wall of the first through hole is provided with a heat insulation layer, the upper mold and the lower mold can be fixedly connected by a connecting piece, the screw can be inserted into the first through hole and the second through hole, and the tail of the screw extends into the heat dissipation hole, the head of the screw extends to the outside of the lower mold, and contacts with the liquid surface of the heating medium through the lower mold, and the heat insulation layer is located above the liquid surface of the heating medium, so that the head of the screw extends into the heating medium; the head of the screw can be heated, and the rest of the screw is shielded by heating to prevent the rest of the screw from being heated quickly, which effectively gives play to the advantages of stable and controllable salt bath heating, and greatly reduces the disadvantages of excessive and strong salt bath heat radiation, improves the process conditions, and realizes the process requirements of local annealing of the screw, has a simple structure, is easy to operate, and is energy-saving and environmentally friendly. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a structural schematic diagram of a local annealing device for screws provided by the utility model;
[0022] Figure 2It is a cross-sectional view of a local annealing device for screws of the utility model;
[0023] Figure 3 yes Figure 2 A is an enlarged schematic diagram;
[0024] Figure 4 The utility model is a use state diagram of a local annealing device for screws. DETAILED DESCRIPTION
[0025] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.
[0026] See also Figures 1 to 4 The utility model provides a local annealing device for screws. The local annealing device for screws uses the heating medium in the salt bath furnace to heat the local part of the screw, and heats and shields the rest of the screw to prevent the rest of the screw from being heated quickly, thereby realizing the local annealing of the screw. It can better realize the local annealing of the φ3.8mm×4mm part of the head of the screw M5×18mm. The device can also be used for various other products that require local annealing, and has the value of promotion and application.
[0027] In this specific embodiment, a local annealing device for screws includes an upper die 1, a lower die 2 and a salt bath furnace 3, wherein the salt bath furnace 3 contains a heating medium 31, the upper die 1 is provided with a heat dissipation hole 11, the lower die 2 is provided with a first through hole 21, and a second through hole 22 connected to the first through hole 21, the inner wall of the first through hole 21 is provided with a heat insulation layer 23, wherein the heat insulation layer 23 is a dry asbestos felt layer, when the upper die 1 and the lower die 2 can be fixedly connected via a connector 4 The central axes of the heat dissipation hole 11, the first through hole 21 and the second through hole 22 coincide with each other, the screw A can be inserted into the first through hole 21 and the second through hole 22, and the tail of the screw A extends into the heat dissipation hole 11, the head of the screw A extends to the outside of the lower mold 2, and contacts the liquid surface of the heating medium 31 through the lower mold 2, and the heat insulation layer 23 is located above the liquid surface of the heating medium 31, so that the head of the screw extends into the heating medium 31.
[0028] It should be noted that the medium-temperature salt bath is a stable heat source that can accurately control the heating temperature and holding time, can reliably achieve austenitization heating and sufficient tissue transfer of the product, has high heating efficiency, and a stable process. However, the medium-temperature salt bath has high heating power, strong heat radiation, and concentrated heat, making it difficult to achieve local heating of the product. To achieve local annealing of the φ3.8mm×4mm position of the head of the screw (the screw is M5×18mm), a device is required to give full play to the advantages of medium-temperature salt bath heating while overcoming its shortcomings to ensure the smooth implementation of the annealing process. Figure 4 The screw is protected in the local annealing device, with only the head of φ3.8mm×4mm that needs annealing exposed and immersed in the molten heating medium for local heating and heat preservation, and then cooled to about 700℃ with the salt bath and air-cooled out of the furnace to complete the local annealing process and obtain the required balanced structure, in preparation for subsequent bending and riveting. Figure 4 It can also be seen that the rest of the screw is protected from rapid heating.
[0029] In this specific embodiment, with the M5×18mm screw as the center, a large amount of water evaporates through the channel of the heat dissipation hole 11 when heated in the salt bath, taking away the heat of the lower mold 2 near the screw to avoid heat uploading and heating of the part. At the same time, the connection length between the screw and the lower mold 2 is only 5mm, which will achieve heat conduction, while the rest of the screw is wrapped by the heat insulation layer 23 to isolate heat conduction, avoid being heated and reduce the length of the annealing transition zone of the screw.
[0030] Based on the above scheme, when the device falls into the salt bath for heating, dried charcoal particles of 5mm×5mm×5mm can be sprinkled on the liquid surface of the heating medium. These charcoal particles can both deoxygenate the salt bath and isolate the liquid surface to prevent excessive heat from the salt bath from being uploaded.
[0031] In one embodiment, the upper mold 1 and the lower mold 2 are both disc-shaped, and a plurality of heat dissipation holes 11 can be opened in the upper mold 1, and a plurality of first through holes 21 that can correspond to each heat dissipation hole one by one are opened in the lower mold 2, that is, the device can anneal multiple objects simultaneously.
[0032] In this specific embodiment, an annular groove 24 is provided in the lower mold 2, and the central axis of the annular groove 24 coincides with the central axes of the first through hole 21 and the second through hole 22, and a water-containing asbestos felt layer 25 is provided in the annular groove 24, and the water-containing asbestos felt layer 25 is fixed between the upper mold 1 and the lower mold 2.
[0033] Specifically, when the water-containing asbestos felt layer 25 is heated in the salt bath, a large amount of water evaporates through the channels of the heat dissipation holes, taking away the heat of the lower mold 2 near the screw A to avoid heat uploading and heating of this part.
[0034] In this specific embodiment, the connecting member 4 includes a locking rod 41 and two locking blocks 42. The locking rod 41 is inserted into the upper mold 1 and the lower mold 2, and the opposite ends of the locking rod 41 are respectively connected to the two locking blocks 42 to fix the upper mold 1 and the lower mold 2.
[0035] On the basis of the above solution, the connecting member 4 further includes a hanging ring 43 , which is disposed above the upper mold 1 and fixedly connected to one end of the locking rod 41 .
[0036] Specifically, the locking rod 41 is a threaded rod, and the two locking blocks 42 are nuts that can be threadedly connected to the threaded rod. The upper mold 1 and the lower mold 2 are locked and fixed between the two locking blocks, and the two locking blocks 42 are rotated at the same time to facilitate disassembly of the device.
[0037] In this specific embodiment, a first groove and a first connecting hole connected to the first groove are provided in the upper mold 1, a second connecting hole is opened in the lower mold 2, the locking rod 41 is sequentially inserted into the first connecting hole, the first groove and the second connecting hole, and a temperature-resistant asbestos pad 12 is provided in the first groove and is sleeved on the locking rod 41.
[0038] Specifically, a second groove is also provided in the upper mold 1, and the central axis of the second groove coincides with the central axis of the first connecting hole. The inner diameter of the second groove is larger than the inner diameter of the first groove, and the second groove is also provided with a heat-resistant asbestos pad 12, which is fixed between the upper mold 1 and the lower mold.
[0039] In this specific embodiment, the heating medium 31 is sodium chloride. Of course, in other embodiments, the heating medium 31 can also be potassium chloride, barium chloride, sodium cyanide, potassium cyanide, sodium nitrate or potassium nitrate, wherein the upper mold 1 and the lower mold 2 are both made of insulation board.
[0040] The beneficial effects are:
[0041] Compared with the prior art, the utility model provides a local annealing device for screws, wherein a heat dissipation hole is opened in the upper mold, a first through hole and a second through hole connected to the first through hole are opened in the lower mold, an inner wall of the first through hole is provided with a heat insulation layer, the upper mold and the lower mold can be fixedly connected by a connecting piece, the screw can be inserted into the first through hole and the second through hole, and the tail of the screw extends into the heat dissipation hole, the head of the screw extends to the outside of the lower mold, and contacts with the liquid surface of the heating medium through the lower mold, and the heat insulation layer is located above the liquid surface of the heating medium, so that the head of the screw extends into the heating medium; the head of the screw can be heated, and the rest of the screw is shielded by heating to prevent the rest of the screw from being heated quickly, which effectively gives play to the advantages of stable and controllable salt bath heating, and greatly reduces the disadvantages of excessive and strong salt bath heat radiation, improves the process conditions, and realizes the process requirements of local annealing of the screw, has a simple structure, is easy to operate, and is energy-saving and environmentally friendly.
[0042] The specific implementation methods of the utility model described above do not constitute a limitation on the protection scope of the utility model. Any other corresponding changes and modifications made according to the technical concept of the utility model should be included in the protection scope of the claims of the utility model.
Claims
1. A local annealing device for screws, comprising an upper die, a lower die and a salt bath furnace, wherein the salt bath furnace contains a heating medium, the upper die is provided with a heat dissipation hole, the lower die is provided with a first through hole and a second through hole connected to the first through hole, wherein: The inner wall of the first through hole is provided with a heat insulation layer. When the upper mold and the lower mold can be fixedly connected via a connecting piece, the central axes of the heat dissipation hole, the first through hole and the second through hole coincide with each other. The screw can be inserted into the first through hole and the second through hole, and the tail of the screw extends into the heat dissipation hole. The head of the screw extends to the outside of the lower mold and contacts with the liquid surface of the heating medium through the lower mold. The heat insulation layer is located above the liquid surface of the heating medium to allow the head of the screw to extend into the heating medium.
2. A local annealing device for screws according to claim 1, characterized in that: An annular groove is provided in the lower mold, and the central axis of the annular groove coincides with the central axes of the first through hole and the second through hole. A water-containing asbestos felt layer is provided in the annular groove, and the water-containing asbestos felt layer is fixed between the upper mold and the lower mold.
3. A local annealing device for screws according to claim 1, characterized in that: The connecting member includes a locking rod and two locking blocks. The locking rod is inserted into the upper mold and the lower mold, and the opposite ends of the locking rod are respectively connected to the two locking blocks to fix the upper mold and the lower mold.
4. A local annealing device for screws according to claim 3, characterized in that: The connecting member also includes a hanging ring, which is arranged above the upper mold and fixedly connected to one end of the locking rod.
5. A local annealing device for screws according to claim 4, characterized in that: The upper mold is provided with a groove and a first connecting hole connected to the groove, the lower mold is provided with a second connecting hole, the locking rod is sequentially inserted into the first connecting hole, the groove and the second connecting hole, and the groove is provided with a temperature-resistant asbestos pad sleeved on the locking rod.
6. A local annealing device for screws according to claim 1, characterized in that: The liquid surface of the heating medium is paved with a charcoal particle layer.
7. A local annealing device for screws according to claim 1, characterized in that: The heating medium may be sodium chloride, potassium chloride, barium chloride, sodium cyanide, potassium cyanide, sodium nitrate or potassium nitrate.
8. A local annealing device for screws according to claim 1, characterized in that: The model of the screw is M5x18mm.
9. A local annealing device for screws according to claim 1, characterized in that: The upper mold and the lower mold are both made of heat insulation board.
10. A local annealing device for screws according to claim 1, characterized in that: The heat insulation layer is a dry asbestos felt layer.