Middle cylinder structure of hydraulic breaking hammer
By forming a coating with improved wear resistance and hardness on the mounting holes of the cylinder block in the hydraulic breaker, the problem of easy hair pulling in the middle cylinder block during use is solved, extending the service life and improving the equipment performance.
Patent Information
- Application Number
- CN202420538339.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-19
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-03-19
AI Technical Summary
The cylinder block in existing hydraulic breakers is prone to hair removal during use, resulting in a short service life and the traditional low-carbon alloy steel heat treatment process is long and consumes a lot.
In the middle cylinder structure of hydraulic breaker, a coating with improved wear resistance and hardness is formed by using PVD process, spraying process or electroplating process, such as DLC, Ta-C, TiN, CrN, CrAlN, TiAlSi, PN+CrAlN and TiCN Coating to enhance wear resistance and hardness of the inner wall of the mounting hole.
Through the use of the coating, the wear resistance and service life of the middle cylinder are significantly improved, the occurrence of hair pulling is reduced, and the overall performance of the equipment is improved.
Smart Images

Figure CN222065613U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of machinery and relates to a hydraulic breaker, in particular to a middle cylinder structure of a hydraulic breaker. Background Art
[0002] A hydraulic breaker is usually installed on an excavator, loader or power station for use. It has the advantages of large impact force, easy use, good mobility and high efficiency, and is widely used in destructive work such as mountain opening and quarrying. At present, the existing hydraulic breaker generally includes a front cylinder body, a middle cylinder body and a rear cylinder body. A drill rod is arranged in the front cylinder body, and the middle cylinder body is connected to the front cylinder body. A piston is arranged in the middle cylinder body. The piston performs a fixed period of reciprocating motion inside the middle cylinder body. A rear oil chamber is arranged at the rear of the middle cylinder body. In order to prevent the oil in the rear oil chamber from flowing out from the gap between the rear of the middle cylinder body and the piston, a piston sleeve is arranged between the piston and the rear of the middle cylinder body, and sealing rings are arranged on the inner and outer surfaces of the piston sleeve.
[0003] The middle cylinder is generally made of low-carbon alloy steel. The traditional manufacturing process of the middle cylinder is carburizing and quenching, and the carburizing process takes 27 hours, which is a long time. After the middle cylinder made of low-carbon alloy steel undergoes the carburizing and quenching heat treatment process, a hardened layer will form on the inner hole surface of the cylinder. In the actual use of the hydraulic breaker assembled with the middle cylinder, since the hardness of the middle cylinder is close to that of the piston, the middle cylinder is prone to roughening during the reciprocating movement of the piston in the middle cylinder, which affects the service life. Summary of the invention
[0004] The utility model aims to solve the above problems in the prior art and proposes a middle cylinder structure of a hydraulic breaker with good wear resistance and long service life.
[0005] The purpose of the utility model can be achieved through the following technical solutions: a middle cylinder structure of a hydraulic breaker, comprising a middle cylinder body, a mounting hole is provided in the middle of the middle cylinder body and a piston is passed through the mounting hole and the piston can move back and forth axially along the mounting hole, a piston sleeve is fixedly connected to the upper end of the mounting hole and the upper end of the piston passes through the piston sleeve, a rear working chamber is provided at the upper part of the mounting hole, an oil return chamber is provided in the middle part, and a front working chamber is provided at the lower part, and it is characterized in that the inner side wall of the mounting hole has a coating formed by a PVD process, a spraying process or an electroplating process and is used to enhance hardness and improve wear resistance.
[0006] Since the inner wall of the mounting hole has a coating formed by a deposition process for enhancing hardness and improving wear resistance, the strength and wear resistance of the inner wall of the mounting hole are improved, making the inner wall of the mounting hole less prone to tearing and increasing the service life.
[0007] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is DLC material. By setting the DLC (diamond-like carbon) coating, it has a low friction coefficient, high hardness, excellent corrosion resistance and lubricity, and increases the service life.
[0008] In the above-mentioned hydraulic breaker cylinder structure, the main component of the coating is DLC, and the coating is formed on the hole wall of the mounting hole by sputtering and microwave plasma enhanced PVD process. The DLC coating formed by sputtering + microwave plasma enhanced PVD process makes the coating uniform and increases the service life.
[0009] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is molybdenum disulfide, and the coating is formed on the hole wall of the mounting hole by a spraying process. The molybdenum disulfide coating has a low friction coefficient and good wear resistance, thereby increasing the practical life of the cylinder body of the middle cylinder.
[0010] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is Ta-C. By setting the coating of Ta-C (a kind of diamond-like material), it has low friction coefficient, high hardness and good temperature resistance, and has excellent corrosion resistance and lubricity, thereby increasing the service life.
[0011] In the above-mentioned hydraulic breaker cylinder structure, the main component of the coating is Ta-C, and the coating is formed on the hole wall of the mounting hole by arc or sputtering PVD process. The Ta-C coating formed by arc or sputtering deposition process makes the coating uniform and increases the service life.
[0012] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is TiN, and the coating is formed on the hole wall of the mounting hole by arc or sputtering PVD process. The TiN coating has the advantages of good wear resistance and low friction coefficient, which increases the service life of the middle cylinder body.
[0013] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is CrN, and the coating is formed on the hole wall of the mounting hole by arc or sputtering PVD process. The CrN coating has the advantages of good wear resistance and low friction coefficient, high toughness and corrosion resistance, and improves the service life of the middle cylinder body.
[0014] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is CrAlN, and the coating is formed on the hole wall of the mounting hole by using the PVD process of arc deposition. The CrAlN coating has good wear resistance, low friction coefficient, high hardness, good oxidation resistance, and improves the service life of the middle cylinder body.
[0015] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is TiAlSi-based, and the coating is formed on the hole wall of the mounting hole by using the PVD process of arc deposition. The TiAlSi-based coating has good wear resistance, low friction coefficient, good oxidation resistance, and improves the service life of the middle cylinder body.
[0016] In the above-mentioned hydraulic breaker cylinder structure, the main component of the coating is PN+CrAlN, and the coating is formed on the hole wall of the mounting hole by using ion nitridation+arc deposition PVD process. The PN+CrAlN coating has the advantages of good wear resistance and low friction coefficient, which increases the service life of the cylinder body.
[0017] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating is TiCN-based, and the coating is formed on the hole wall of the mounting hole by using the PVD process of ion sputtering + arc deposition. The TiCN-based coating has the advantages of good wear resistance, low friction coefficient, and good impact resistance, which increases the service life of the middle cylinder body.
[0018] In the above-mentioned middle cylinder structure of the hydraulic breaker, the main component of the coating (4) is chromium, and the coating (4) is formed on the hole wall of the mounting hole (1a) by electroplating process.
[0019] Compared with the prior art, the middle cylinder structure of the hydraulic breaker has the following advantages:
[0020] 1. Since the inner wall of the mounting hole is formed with a coating for enhancing hardness and improving wear resistance by PVD process, the coating is evenly distributed, which improves the strength and wear resistance of the inner wall of the mounting hole, makes the inner wall of the mounting hole less likely to be scratched, and increases the service life;
[0021] 2. The DLC coating formed by sputtering + microwave plasma enhanced PVD process has low friction coefficient, high hardness, excellent corrosion resistance and lubricity, and improves service life;
[0022] 3. The CrN coating is formed on the wall of the mounting hole by arc or sputtering PVD process. It has the advantages of good wear resistance and low friction coefficient, high toughness and corrosion resistance, which improves the service life of the cylinder body.
[0023] 4. The TiAlSi-based coating is formed on the wall of the mounting hole by the arc deposition PVD process. It has good wear resistance, low friction coefficient, and good oxidation resistance, which increases the service life of the cylinder block. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a three-dimensional schematic diagram of the middle cylinder structure of the hydraulic breaker.
[0025] Figure 2 It is a cross-sectional schematic diagram of the middle cylinder structure of the hydraulic breaker.
[0026] Figure 3 It is a schematic cross-sectional view of the middle cylinder body of the hydraulic breaker.
[0027] Figure 4 yes Figure 3 A is a partial enlarged schematic diagram of .
[0028] In the figure, 1, middle cylinder body; 1a, mounting hole; 1b, rear working chamber; 1c, oil return chamber; 1d, front working chamber; 2, piston sleeve; 3, piston; 4, coating. DETAILED DESCRIPTION
[0029] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0030] Embodiment 1
[0031] like Figures 1 to 4 As shown, the middle cylinder structure of the hydraulic breaker comprises a middle cylinder body 1, a mounting hole 1a is provided in the middle of the middle cylinder body 1, a piston 3 is passed through the mounting hole 1a and the piston 3 can move axially reciprocatingly along the mounting hole 1a, a piston sleeve 2 is fixedly connected to the upper end of the mounting hole 1a and the upper end of the piston 3 passes through the piston sleeve 2, a rear working chamber 1b is provided at the upper part of the mounting hole 1a, an oil return chamber 1c is provided in the middle part, and a front working chamber 1d is provided at the lower part, the inner side wall of the mounting hole 1a has a coating 4 formed by a PVD process for enhancing hardness and improving wear resistance, the DLC coating 4 is formed on the hole wall of the mounting hole 1a by a sputtering and microwave plasma enhanced PVD process, so that the coating 4 is evenly distributed, has a low friction coefficient, high hardness and high wear resistance, and has excellent corrosion resistance and lubricity, thereby improving the service life.
[0032] PVD process, namely physical vapor deposition (PVD), refers to the technology of vaporizing the surface of the material source (solid or liquid) into gaseous atoms or molecules, or partially ionizing into ions, under vacuum conditions, and depositing a thin film with some special functions on the surface of the substrate through a low-pressure gas (or plasma) process. Physical vapor deposition is one of the main surface treatment technologies. For example, a PVD coating of a metal surface treatment process (application number: 201110390023.4) disclosed in Chinese patent documents; a highly wear-resistant and anti-corrosion PVD coating process (application number: 201810655477.1).
[0033] Embodiment 2
[0034] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is Ta-C, and the coating 4 is formed on the hole wall of the mounting hole 1a by an arc or sputtering PVD process, and has a low friction coefficient, high hardness, and good temperature resistance, and has excellent corrosion resistance and lubricity, thereby increasing the service life.
[0035] Embodiment 3
[0036] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is TiN, and the coating 4 is formed on the hole wall of the mounting hole 1a by an arc or sputtering PVD process, and has the advantages of good wear resistance and a small friction coefficient, thereby increasing the service life of the middle cylinder body 1.
[0037] Embodiment 4
[0038] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is CrN, and the coating 4 is formed on the hole wall of the mounting hole 1a by an arc or sputtering PVD process, and has the advantages of good wear resistance and a small friction coefficient, and has high toughness and corrosion resistance, thereby improving the service life of the middle cylinder body 1.
[0039] Embodiment 5
[0040] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is CrAlN, and the coating 4 is formed on the hole wall of the mounting hole 1a by an arc deposition PVD process, and has good wear resistance, low friction coefficient, high hardness, and good oxidation resistance, thereby improving the service life of the middle cylinder body 1.
[0041] Embodiment 6
[0042] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is TiAlSi-based, and the coating 4 is formed on the hole wall of the mounting hole 1a by an arc deposition PVD process, and has good wear resistance, a small friction coefficient, and good oxidation resistance, thereby increasing the service life of the middle cylinder body 1.
[0043] Embodiment 7
[0044] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is PN+CrAlN, and the coating 4 is formed on the hole wall of the mounting hole 1a by a PVD process of ion nitriding+arc deposition, and has the advantages of good wear resistance and a small friction coefficient, thereby increasing the service life of the middle cylinder body 1.
[0045] Embodiment 8
[0046] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating 4 is TiCN-based, and the coating 4 is formed on the hole wall of the mounting hole 1a by a PVD process of ion sputtering + arc deposition, and has the advantages of good wear resistance, low friction coefficient, and good impact resistance, thereby improving the service life of the middle cylinder body 1.
[0047] Embodiment 9
[0048] The structure and principle of this embodiment are roughly the same as those of the first embodiment, except that the main component of the coating (4) is chromium, and the coating (4) is formed on the hole wall of the mounting hole (1a) by electroplating, and has high hardness and good wear resistance, thereby increasing the service life.
[0049] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
[0050] Although the terms such as middle cylinder body 1, mounting hole 1a, rear working chamber 1b, oil return chamber 1c, front working chamber 1d, piston sleeve 2, piston 3, coating 4 are used more frequently in this article, the possibility of using other terms is not excluded. The use of these terms is only for the purpose of more conveniently describing and explaining the essence of the utility model; interpreting them as any additional restrictions is contrary to the spirit of the utility model.
Claims
1. A middle cylinder structure of a hydraulic breaker, comprising a middle cylinder body (1), wherein a mounting hole (1a) is provided in the middle of the middle cylinder body (1) and the mounting hole (1a) is used to mount a piston (3), wherein: The inner side wall of the mounting hole (1a) has a coating (4) formed by a PVD process, a spraying process or an electroplating process and used to increase hardness and improve wear resistance.
2. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is DLC material, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using sputtering and microwave plasma enhanced PVD process.
3. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is molybdenum disulfide, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using a spraying process.
4. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is Ta-C, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using an arc or sputtering PVD process.
5. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is TiN, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using an arc or sputtering PVD process.
6. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is CrN, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using an arc or sputtering PVD process.
7. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is CrAlN, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using arc deposition PVD.
8. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is TiAlSi-based, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using an arc deposition PVD process.
9. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main components of the coating (4) are PN+CrAlN, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using an ion nitridation+arc PVD process.
10. The middle cylinder structure of the hydraulic breaker according to claim 1, characterized in that: The main component of the coating (4) is chromium, and the coating (4) is formed on the hole wall of the mounting hole (1a) by using an electroplating process.