Nanometer composite film and display screen module

Through the optical coating and electronic heating technology of nanocomposite film, the display differences and low-temperature environment problems in the vehicle display screen are solved, and the color consistency and efficient heating effect are achieved.

CN222070872UActive Publication Date: 2024-11-26AIPTEK TECH (WUJIANG) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420563078.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-22
Publication Date
2024-11-26
Estimated Expiration
2034-03-22

AI Technical Summary

Technical Problem

In multiple vehicle-mounted display screens, due to the different structure, electrical and optical properties of each screen, the display differences are caused. The existing heating methods are inefficient and the anti-EMC/EMI performance is degraded, making it difficult to ensure color consistency and prevent low-temperature environments. Problems of dragging shadows, afterimages, and flower screens.

Method used

Using a nanocomposite film, including a combination of silicon-based nitride, silicon-based oxide, metal oxide and doped metal oxide film layer, the color coordinates of the display screen are adjusted through optical coating, and the doped metal oxide film layer is used. Connect to the electronic control system for heating.

Benefits of technology

The color consistency of multiple screens is achieved without changing the luminous material or color resistance, reducing heating power consumption and avoiding display problems in low-temperature environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222070872U_ABST
    Figure CN222070872U_ABST
Patent Text Reader

Abstract

The utility model provides a nanometer composite film and a display screen module, the provided nanometer composite film comprises at least two different sub-films which are laminated, and each sub-film comprises but is not limited to one or a combination of more of a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer and a doped metal oxide film layer. The provided nano-composite film is plated on one side of a transparent substrate layer of a display screen module in a whole-surface optical coating mode, so that the long-wave green wave band can be effectively reduced, the original yellow-green picture is improved, and the screen color cast is adjusted while the red and blue pictures are not influenced and the short-wave green wave band is not inhibited.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of new materials, and in particular relates to a nano composite film and a display screen module. Background Art

[0002] As the "new four modernizations" of automobiles continue to develop, smart cockpits play an increasingly important role in smart experience. As an important part of the smart cockpit, the in-vehicle display screen is also developing in the direction of "large screen, multi-screen, and connected screen". Among them, "multi-screen" is manifested in an LCD screen in front of the driver, a display screen in the center of the center console, and an entertainment screen at the co-pilot position. However, due to the different performance parameters of the structure, electricity, optics, etc. of each screen itself, it is very easy to cause display differences among multiple screens. In actual production, considering the supply, cost, process, etc., multiple screens are often not from the same manufacturer, which will further increase their display differences. For example, through actual shooting comparison, it is found that some screens have yellow tones, mainly due to the yellowish green screen. Then, by testing the WRGB color coordinates (CIE1931) of multiple screens, it is found by comparing the color coordinate values ​​that the green coordinates of the screen with yellow tones are quite different from those of other screens with non-yellow tones. This result is consistent with the actual shooting comparison result. At this point, the problem of screen color deviation has been found.

[0003] However, in actual situations, each screen has already selected its own RGB color coordinate point (related to material properties) during the design phase, and it cannot be changed. For example, if the screen color coordinates are adjusted, for active light-emitting screens such as organic electroluminescence display (OLED), sub-millimeter light-emitting diode (Mini LED), and micro light-emitting diode display (Micro LED), only the light-emitting material needs to be replaced, which is equivalent to developing a new screen; while for non-self-luminous screens such as LCD, the CF (color resistance) needs to be replaced, which is equivalent to developing a liquid crystal panel, which requires a long cycle and high cost. For the above-mentioned display screens with different principles, their active light-emitting materials or color resistance materials in LCD are mostly organic mixtures, which themselves have a large process fluctuation range. Even if the same material is used, the color consistency cannot be guaranteed to achieve the effect of visually no color difference. In actual situations, there are also differences in materials purchased by different manufacturers. Even if it is the same manufacturer, there will be differences in materials purchased at different times. This is not conducive to controlling the consistency of the display color tones of multiple screens.

[0004] In addition, taking the LCD screen as an example, when it is in a low temperature environment, there will be risks such as streaking, afterimages, and screen noise. The above risks are mostly caused by the slow response of the liquid crystal due to the low temperature, so the heating function of the display screen module is also urgently needed. The existing technology generally heats the LCD backlight iron frame by attaching copper wires to the outer surface, but this heating method requires large heating power consumption and poor heating effect because the heated position is far away from the liquid crystal layer. At the same time, this heating method will also cause the LCD display screen's anti-EMC / EMI performance to decrease. The transparent electrode of the touch screen is a pattern formed by etching, which occupies a small area, and its primary function is also touch, so it is not suitable to use the transparent electrode of the touch screen to heat the screen. Utility Model Content

[0005] In view of the problems existing in the above-mentioned prior art, the main purpose of the present invention is to provide a nano-composite film and a display screen module to solve one or more of the above-mentioned prior art problems.

[0006] The purpose of the utility model is achieved through the following technical solutions:

[0007] The utility model provides a nano composite film, which comprises at least two different sub-films stacked together, each of which comprises but is not limited to: a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a combination of one or more of a doped metal oxide film layer.

[0008] As a further description of the above technical solution, a combination of one or more of the silicon-based nitride (SiNx) film layer, the silicon-based oxide (SiOx) film layer, the metal oxide film layer, and the doped metal oxide film layer is periodically arranged along the stacking direction of the sub-film, thereby constituting the sub-film of the nanocomposite film.

[0009] As a further description of the above technical solution, the nanocomposite film includes 10-40 film layers.

[0010] As a further description of the above technical solution, the nanocomposite film includes 13-39 film layers.

[0011] As a further description of the above technical solution, the nanocomposite film includes 15-20 film layers.

[0012] As a further description of the above technical solution, the metal oxide forming the metal oxide film layer includes but is not limited to one of niobium oxide and titanium oxide.

[0013] As a further description of the above technical solution, the doped metal oxide forming the doped metal oxide film layer includes but is not limited to one of tin-doped indium oxide (ITO), fluorine-doped indium oxide (FTO), and aluminum-doped zinc oxide (AZO).

[0014] As a further description of the above technical solution, the nanocomposite film includes 5 sub-membranes arranged in a stacked manner, and each of the sub-membranes includes but is not limited to: a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a combination of one or more of the doped metal oxide film layers.

[0015] As a further description of the above technical solution, a combination of one or more of the silicon-based nitride (SiNx) film layer, the silicon-based oxide (SiOx) film layer, the metal oxide film layer, and the doped metal oxide film layer is periodically arranged along the stacking direction of the sub-film, thereby constituting 5 sub-films of the nanocomposite film.

[0016] As a further description of the above technical solution, the five sub-films are sequentially as follows along their stacking direction:

[0017] A first sub-film including the silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer and a doped metal oxide film layer;

[0018] A second sub-film including the metal oxide film layer and a doped metal oxide film layer;

[0019] A third sub-film including the metal oxide film layer and a silicon-based nitride (SiNx) film layer;

[0020] a fourth sub-film including the metal oxide film layer and the doped metal oxide film layer; and,

[0021] A fifth sub-film includes a metal oxide film layer and a silicon-based oxide (SiOx) film layer.

[0022] As a further description of the above technical solution, the first sub-film includes 1-3 film layer arrangement periods;

[0023] The second sub-film includes 1-3 film layer arrangement periods;

[0024] The third sub-film includes 1-3 film layer arrangement periods;

[0025] The fourth sub-film includes 2-6 film layer arrangement periods;

[0026] The fifth sub-film includes 1-3 film layer arrangement periods.

[0027] As a further description of the above technical solution, the first sub-film includes 2 film layer arrangement periods;

[0028] The second sub-film includes 1 film layer arrangement period;

[0029] The third sub-film includes 1 film layer arrangement period;

[0030] The fourth sub-film includes 4 film layer arrangement periods;

[0031] The fifth sub-film includes one film layer arrangement period.

[0032] As a further description of the above technical solution, within one film layer arrangement period of the first sub-film,

[0033] The silicon-based nitride (SiNx) film layer has a refractive index of 1.75-1.85 and a thickness of 150nm-300nm;

[0034] The silicon-based oxide (SiOx) film layer has a refractive index of 1.44-1.47 and a thickness of 100nm-300nm;

[0035] The refractive index of the doped metal oxide film layer is between 1.78-1.85 and is not lower than the refractive index of the silicon-based nitride (SiNx) film layer, and the thickness is 20nm-40nm.

[0036] As a further description of the above technical solution, within one film layer arrangement period of the second sub-film,

[0037] The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 150nm-200nm;

[0038] The doped metal oxide film has a refractive index of 1.75-1.85 and a thickness of 30nm-60nm.

[0039] As a further description of the above technical solution, within one film layer arrangement period of the third sub-film,

[0040] The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 50nm-100nm;

[0041] The refractive index of the silicon-based nitride (SiNx) film layer is 1.75-1.85, and the thickness is 150nm-300nm.

[0042] As a further description of the above technical solution, within one film layer arrangement period of the fourth sub-film,

[0043] The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 70nm-150nm;

[0044] The doped metal oxide film has a refractive index of 1.78-1.85 and a thickness of 15nm-50nm.

[0045] As a further description of the above technical solution, within one film layer arrangement period of the fifth sub-film,

[0046] The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 150nm-250nm;

[0047] The silicon-based oxide (SiOx) film layer has a refractive index of 1.44-1.47 and a thickness of 300nm-500nm.

[0048] The utility model also provides a display screen module, which comprises the nano composite film and a transparent substrate layer as described above, wherein the nano composite film is plated on one side of the transparent substrate layer.

[0049] As a further description of the above technical solution, the material forming the transparent base layer includes but is not limited to one of glass or organic glass PC, PMMA, and PET.

[0050] As a further description of the above technical solution, the material forming the transparent substrate layer is glass.

[0051] As a further description of the above technical solution, the refractive index of the transparent substrate layer is 1.46-1.53.

[0052] As a further description of the above technical solution, the refractive index of the transparent substrate layer is 1.49-1.52.

[0053] As a further description of the above technical solution, the display screen module also includes an electric control system, and the one or more sub-films containing the doped metal oxide film layer included in the nano-composite film are electrically connected to the electric control system.

[0054] In summary, the outstanding effects of the utility model are:

[0055] 1. The nanocomposite film provided by the utility model includes at least two different sub-films stacked together, and since each sub-film includes but is not limited to a combination of one or more of a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a doped metal oxide film layer, the refractive index of the sub-film of the nanocomposite film will change periodically. When the display screen module has a screen color deviation due to its green screen being yellowish, the nanocomposite film can be applied to one side of the transparent substrate layer included in the display screen module by optical coating to perform spectral regulation, thereby facilitating the adjustment of the color coordinates of the screen with color deviation to the target color coordinates: for an actively luminous screen, there is no need to replace the luminescent material, and for a non-self-luminous screen, there is no need to replace the CF (color resistance), which is conducive to achieving the effect of color consistency of multiple screens;

[0056] 2. At present, the optical coating technology is mature and the performance of inorganic thin films is stable, which is conducive to ensuring the color coordinate adjustment effect of the nano-composite film on the screen;

[0057] 3. The sub-membrane in the nano-composite film provided by the utility model includes a doped metal oxide film layer, which is made of doped metal oxide. An electric control system can be set to electrically connect with it to heat the screen, thereby replacing the existing method of heating the screen. The required heating power consumption is small and the heating effect is good, which effectively avoids the problems of streaking, afterimage, and screen noise when the display screen is in a low temperature environment. BRIEF DESCRIPTION OF THE DRAWINGS

[0058] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For those skilled in the art, other drawings can be obtained based on these drawings without paying creative work.

[0059] Figure 1 The transmittance spectrum corresponding to one of the film layer arrangements of the nanocomposite film in the embodiment of the utility model;

[0060] Figure 2 The green screen color coordinate fluctuation diagram of screen C with nanocomposite films having different film thicknesses in the embodiment of the utility model corresponding to 5000 calculation simulation tests;

[0061] Figure 3 The trend diagram of the green screen color coordinates of the screen C having the nanocomposite films with different film thicknesses in the embodiment of the utility model corresponding to 5000 calculation simulation tests;

[0062] Figure 4The distribution of discrete data of green screen color coordinates in the CIE1931 xy chromaticity diagram of screen C with nanocomposite films of different film thicknesses in the corresponding 5000 calculation simulation tests in the embodiment of the utility model;

[0063] Figure 5 is a cross-sectional view of a display screen module (without a nanocomposite film) in an application embodiment;

[0064] Figure 6 A cross-sectional view showing that the nanocomposite film in the embodiment of the present invention is disposed between the AR+AF film of the display screen module and the optical cover substrate;

[0065] Figure 7 A cross-sectional view showing a nanocomposite film in an embodiment of the present invention disposed between an optical cover substrate and a second optical adhesive of a display screen module;

[0066] Figure 8 A cross-sectional view showing a nanocomposite film in an embodiment of the present utility model disposed between the second optical adhesive of a display screen module and a touch screen;

[0067] Fig. 9 A cross-sectional view showing a nanocomposite film in an embodiment of the utility model disposed between a touch screen and a first optical adhesive of a display screen module;

[0068] Fig.10 A cross-sectional view showing that the nanocomposite film in the embodiment of the utility model is disposed between the second polarizer and the second transparent substrate of the display screen module;

[0069] Fig.11 A cross-sectional view showing that the nanocomposite film in the embodiment of the utility model is disposed between the second transparent substrate and the RGB color resist of the display screen module;

[0070] Fig.12 A cross-sectional view showing that the nanocomposite film in the embodiment of the utility model is disposed between the liquid crystal layer and the first transparent substrate of the display screen module;

[0071] Fig.13 A cross-sectional view showing that the nanocomposite film in the embodiment of the utility model is disposed between the first transparent substrate and the first polarizer of the display screen module;

[0072] Fig.14 It is a structural schematic diagram of electrically connecting the ITO film layer in the first sub-film of the nano-composite film in the embodiment of the utility model to the electric control system of the display screen module.

[0073] Description of the accompanying drawings:

[0074] 1. Nano-composite film; 2. AR+AF film; 3. Optical cover substrate; 4. Second optical adhesive; 5. Touch screen; 6. First optical adhesive; 7. Second polarizer; 8. Second transparent substrate; 9. RGB color resistance; 10. Liquid crystal layer; 11. First transparent substrate; 12. First polarizer; 13. Backlight module. DETAILED DESCRIPTION

[0075] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0076] In the description of the present utility model, it should be noted that the terms "upper", "middle", "lower", "inner", "outer", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present utility model and simplifying the description, rather than indicating or implying that the device or component referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present utility model. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance. For those of ordinary skill in the art, the specific meanings of the above terms in the present utility model can be understood according to specific circumstances.

[0077] The utility model provides a nano-composite film 1, which comprises at least two different sub-films stacked together, each of which comprises but is not limited to: a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a combination of one or more of a doped metal oxide film layer.

[0078] In the above-mentioned setting method, the nano-composite film 1 includes at least two different sub-films stacked together, and since each of the sub-films includes but is not limited to a combination of one or more of a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a doped metal oxide film layer, the refractive index of the sub-film of the nano-composite film 1 will change periodically. When the display screen module has a screen color deviation due to its yellowish green screen, the nano-composite film 1 can be applied to one side of the transparent substrate layer included in the display screen module by optical coating to perform spectral regulation, so as to adjust the color coordinates of the screen with color deviation to the target color coordinates: for actively luminous screens, there is no need to replace the luminescent material, and for non-self-luminous screens, there is no need to replace the CF (color resistance); both are conducive to achieving the effect of color consistency of multiple screens.

[0079] Specifically, in the utility model, a combination of one or more of the silicon-based nitride (SiNx) film layer, the silicon-based oxide (SiOx) film layer, the metal oxide film layer, and the doped metal oxide film layer is periodically arranged along the stacking direction of the sub-membrane, thereby constituting the sub-membrane of the nano-composite film 1. The multiple film layers are periodically arranged along the stacking direction of the sub-membrane, so that the refractive index of the nano-composite film 1 is periodic and spectral regulation is performed.

[0080] Specifically, in the present invention, the nanocomposite film 1 includes 10-40 film layers. Preferably, the nanocomposite film 1 includes 13-39 film layers. More preferably, the nanocomposite film 1 includes 15-20 film layers.

[0081] Specifically, in the present invention, the metal oxide forming the metal oxide film layer includes but is not limited to one of niobium oxide and titanium oxide.

[0082] Specifically, in the present invention, the doped metal oxide forming the doped metal oxide film layer includes, but is not limited to, one of tin-doped indium oxide (ITO), fluorine-doped indium oxide (FTO), and aluminum-doped zinc oxide (AZO).

[0083] The utility model also provides a display screen module, which comprises the nano-composite film 1 and a transparent substrate layer as described above, wherein the nano-composite film 1 is plated on one side of the transparent substrate layer.

[0084] Specifically, in the present invention, the material forming the transparent base layer includes but is not limited to glass or one of organic glasses PC, PMMA, and PET.

[0085] Specifically, in the present invention, the material forming the transparent base layer is glass, and preferably, its refractive index is 1.46-1.53.

[0086] Specifically, in the present invention, the display screen module further includes an electric control system, and one or more sub-films containing a doped metal oxide film layer included in the nano-composite film 1 are electrically connected to the electric control system.

[0087] A more detailed description will now be given in conjunction with a specific embodiment.

[0088] Specifically, in this embodiment, the nanocomposite film 1 uses glass as the coating substrate, and the refractive index of the glass is more preferably 1.49-1.52. The nanocomposite film 1 includes 5 sub-films, and in the direction gradually away from the coating substrate, the 5 sub-films are the first sub-film, the second sub-film, the third sub-film, the fourth sub-film and the fifth sub-film.

[0089] Specifically, in this embodiment, the five sub-films are divided into four types, wherein the first sub-film includes the silicon-based nitride (SiNx) film layer, the silicon-based oxide (SiOx) film layer and the doped metal oxide film layer, the second sub-film and the fourth sub-film both include the metal oxide film layer and the doped metal oxide film layer, the third sub-film includes the metal oxide film layer and the silicon-based nitride (SiNx) film layer, and the fifth sub-film includes the metal oxide film layer and the silicon-based oxide (SiOx) film layer. The film layers included in each sub-film are periodically arranged in a direction away from the coating substrate.

[0090] Specifically, in this embodiment, the first sub-film includes 1-3 film layer arrangement periods; the second sub-film includes 1-3 film layer arrangement periods; the third sub-film includes 1-3 film layer arrangement periods; the fourth sub-film includes 2-6 film layer arrangement periods; the fifth sub-film includes 1-3 film layer arrangement periods. Preferably, the first sub-film includes 2 film layer arrangement periods; the second sub-film includes 1 film layer arrangement period; the third sub-film includes 1 film layer arrangement period; the fourth sub-film includes 4 film layer arrangement periods; the fifth sub-film includes 1 film layer arrangement period.

[0091] As shown in Table 1 below, specifically, in this embodiment, within one film layer arrangement period of the first sub-film, the refractive index of the silicon-based nitride (SiNx) film layer is preferably 1.75-1.85, and the thickness is preferably 150nm-300nm; the refractive index of the silicon-based oxide (SiOx) film layer is 1.44-1.47, and the thickness is preferably 100nm-300nm; the doped metal oxide film layer is an ITO film layer, and its refractive index is preferably 1.78-1.85, and the thickness is preferably 20nm-40nm. Of course, in other embodiments, the doped metal oxide film layer can also be a FTO film layer, an AZO film layer, etc.

[0092] Specifically, in this embodiment, within a film layer arrangement period of the second sub-film, the metal oxide film layer is a Nb2O5 film layer, and its refractive index is preferably 2.27-2.35, and its thickness is preferably 150nm-200nm; the doped metal oxide film layer is an ITO film layer, and its refractive index is preferably 1.75-1.85, and its thickness is preferably 30nm-60nm. Of course, in other embodiments, the metal oxide film layer can also be selected from other metal oxide film layers, such as a film layer made of titanium oxide, and the doped metal oxide film layer can also be a FTO film layer, an AZO film layer, etc.

[0093] Specifically, in this embodiment, within a film layer arrangement period of the third sub-membrane, the metal oxide film layer is also a Nb2O5 film layer, and its refractive index is preferably 2.27-2.35, and its thickness is preferably 50nm-100nm; the refractive index of the silicon-based nitride (SiNx) film layer is preferably 1.75-1.85, and its thickness is preferably 150nm-300nm.

[0094] Specifically, in this embodiment, within a film layer arrangement period of the fourth sub-membrane, the metal oxide film layer is still a Nb2O5 film layer, whose refractive index is preferably 2.27-2.35, and whose thickness is preferably 70nm-150nm; the doped metal oxide film layer is an ITO film layer, whose refractive index is preferably 1.78-1.85, and whose thickness is preferably 15nm-50nm.

[0095] Specifically, in this embodiment, within one film layer arrangement period of the fifth sub-membrane, the metal oxide film layer is still a Nb2O5 film layer, and its refractive index is preferably 2.27-2.35, and its thickness is preferably 150nm-250nm; the refractive index of the silicon-based oxide (SiOx) film layer is preferably 1.44-1.47, and its thickness is preferably 300nm-500nm.

[0096] Table 1 Structure of the nanocomposite film 1 in the embodiment

[0097]

[0098] Specifically, in this embodiment, three screens from different manufacturers (the screen numbers are A, B, and C, wherein screen A comes from the manufacturer with a product model of, screen B comes from the manufacturer with a product model of, and screen C comes from the manufacturer with a product model of) are selected for power-on. Through actual shooting, it is found that the hue of screen C is yellowish, which is mainly caused by the yellowish green screen. Then, the color coordinates of the screens are tested, and the WRGB color coordinates (CIE1931) of the three screens are obtained as shown in Table 2 below.

[0099] Table 2 WRGB color coordinates (CIE1931) test results of three screens

[0100] Screen Number Wx Wy Rx R Gx Gy Bx By A 0.2879 0.3189 0.6295 0.3384 0.2944 0.6101 0.1420 0.0546 B 0.2881 0.3193 0.6311 0.3402 0.2939 0.6118 0.1416 0.0555 C 0.2896 0.3202 0.6339 0.3370 <![CDATA[ 0.3291 ]]> <![CDATA[ 0.6331 ]]> 0.1416 0.0492

[0101] By comparing the color coordinate values ​​of each screen, it is found that the green color coordinate of screen C is quite different from those of screens A and B, which is consistent with the visual observation results.

[0102] like Figure 1As shown, it is the transmittance spectrum of the nano-composite film 1 described in this embodiment. Through the transmittance spectrum, it can be found that the nano-composite film 1 of this embodiment maintains a transmittance of more than 90% in the wavelength range of 420nm-480nm and 600nm-700nm, and the transmittance changes relatively smoothly with the wavelength. In other words, the nano-composite film 1 of this embodiment will not affect the original blue and red pictures while changing the green hue; and since it has no effect on the red and blue pictures, in this embodiment, the original screen can actually be coated with an optical coating process on the entire surface and the nano-composite film 1 is applied thereon, without the need to perform exposure etching on specific areas of the green pixels of the original screen, thereby reducing the process difficulty, reducing the process cost, and improving the production capacity; and for the green band of the original screen, the central peak is at 520nm, and the transmittance of the nano-composite film 1 of this embodiment at 520nm reaches 92.4%, while not suppressing the short-wave green band, the long-wave green band is reduced, thereby improving the originally yellowish green picture.

[0103] Test results:

[0104] 1. The color coordinate test was performed again on the screen C to which the nanocomposite film 1 of this embodiment was applied (the pixel material of the screen C was not changed), and the green screen coordinates were improved to (Gx: 0.2939, Gy: 0.6172). The difference between the green color coordinates of the screen C and the reference screen (screen A, B) was reduced to within ±0.01, and the screen color deviation was improved well.

[0105] 2. Considering the error fluctuation of the optical coating process, different film thicknesses may be obtained. Therefore, this embodiment uses a computer to perform 5000 simulation calculation experiments to obtain the nanocomposite film 1 composed of film layers with different film thicknesses. Correspondingly, the color coordinate range distribution caused is as follows: Figure 2 As shown: 5000 simulation calculation experiments show that under the action of the nano-composite film 1, the green screen color coordinates of screen C are centered on the mean (Gx: 0.2939, Gy: 0.6172), Gx fluctuates in the range of [0.2835, 0.3041], and Gy fluctuates in the range of [0.608, 0.627], and the fluctuation range of Gx and Gy is only ±0.01.

[0106] Under the effect of the nanocomposite film 1, although the green color coordinates Gx and Gy of the screen C have a variation range of ±0.01, Figure 3 As shown, overall, the change of green color coordinates is concentrated in one area, and is approximately linear in the area. The equation of its trend line is approximately Gy = -0.9167*Gx + 0.8866; the discrete data of the above 5000 experiments and the fitting determination coefficient of the trend line equation R 2=0.9981, which shows that the equation fits the distribution trend of discrete data; Figure 4 As shown, after 5000 simulation calculation tests of thickness fluctuation, the hue of the nanocomposite film 1 is still concentrated in the green area.

[0107] Application Examples

[0108] like Figure 5 As shown, taking the "G+G" form of LCD touch display screen module as an example (those skilled in the art should understand that the "G+G" form of LCD touch display screen is a touch screen 5 made of surface tempered glass + glass GLASS material), the LCD touch display screen module is provided with an AR+AF film 2 (formed as a whole by an AF film layer and an AR film layer), an optical cover substrate 3, a second optical glue 4, a touch screen 5, a first optical glue 6, a second polarizer 7, a second transparent substrate 8, an RGB color resist 9, a liquid crystal layer 10, a first transparent substrate 11, a first polarizer 12 and a backlight module 13 from top to bottom.

[0109] Without improving the original display module materials, Figures 6 to 13 As shown, any of the above-mentioned nanocomposite films 1 with different film thicknesses can be arranged at any of the following positions:

[0110] between the AR+AF film 2 and the optical cover substrate 3 (with the optical cover substrate 3 as the coating substrate layer), between the optical cover substrate 3 and the second optical adhesive 4 (with the optical cover substrate 3 as the coating substrate layer), between the second optical adhesive 4 and the touch screen 5 (with the touch screen 5 as the coating substrate layer), between the touch screen 5 and the first optical adhesive 6 (with the touch screen 5 as the coating substrate layer), between the second polarizer 7 and the second transparent substrate 8 (with the second transparent substrate 8 as the coating substrate layer), between the second transparent substrate 8 and the RGB color resist 9 (with the second transparent substrate 8 as the coating substrate layer), between the liquid crystal layer 10 and the first transparent substrate 11 (with the first transparent substrate 11 as the coating substrate layer), and between the first transparent substrate 11 and the first polarizer 12 (with the first transparent substrate 11 as the coating substrate layer).

[0111] When the display screen module is in a low temperature environment (such as an LCD display screen module), there will be risks such as streaking, afterimages or screen noise. Most of these risks are caused by the low temperature slowing down the response of the liquid crystal. Therefore, the nano-composite film 1 can include one or more sub-films containing a doped metal oxide film layer (such as an ITO film layer), and it can be electrically connected to the electrical control system of the display screen module, so that the screen (liquid crystal layer 10) can be heated, so that the display screen module can still work efficiently in a low temperature environment without the risks of streaking, afterimages, screen noise, etc.

[0112] Among them, the electric control system mainly includes a voltage source V, and a manual switch unit, a temperature measurement and control unit, and a screen drive and signal processing unit electrically connected to the voltage source respectively. The manual switch unit, the temperature measurement and control unit, and the screen drive and signal processing unit can respectively control whether the voltage source V forms an electrical connection with one or more sub-films containing a doped metal oxide film layer of the nano-composite film 1. The temperature measurement and control unit is also electrically connected to the liquid crystal box of the display screen module (composed of two oppositely arranged transparent substrates and a liquid crystal located between the two transparent substrates), and the screen drive and signal processing unit is electrically connected to the driving hardware of the display screen module.

[0113] like Fig.14 As shown, in one embodiment, the nanocomposite film 1 is disposed between the optical cover substrate 3 and the second optical adhesive 4, and the ITO film layer in the first sub-film is electrically connected to the electric control system of the display screen module. When the screen user perceives that the screen has lost picture due to low temperature, he can electrically connect the voltage source V to the sub-film containing the doped metal oxide film layer of the nanocomposite film 1 through the manual operation part of the manual switch unit. Since the sub-film containing the doped metal oxide film layer of the nanocomposite film 1 has resistance, it will heat up and play a role in heating the liquid crystal box to improve the display effect.

[0114] The temperature measurement and control unit includes a temperature measurement module and a temperature control module. The temperature measurement module is used to measure the temperature of the liquid crystal box. When the temperature of the liquid crystal box is determined to be lower than a threshold value (which can be set manually, such as -20°C), it will transmit an electrical signal to the temperature control module. Then the temperature control module will connect the voltage source V to the sub-film containing the doped metal oxide film layer of the nano-composite film 1 and apply voltage to the sub-film, which also plays a role in heating the screen and improving the screen display effect. Of course, after the temperature measurement module determines that the temperature of the liquid crystal box reaches the threshold value, it will transmit another electrical signal to the temperature control module, and then the temperature control module will cut off the electrical connection between the voltage source V and the nano-composite film 1.

[0115] At the same time, the screen driving and signal processing unit includes a screen driving module and a signal processing module. The screen driving module is electrically connected to the driving hardware and signal processing module of the display screen module respectively. When the signal processing module detects from the screen driving module that the corresponding time between frames of the screen is higher than a preset value (for example, 100ms, which can be set according to actual needs), the signal processing module will electrically connect the voltage source V to the nano-composite film 1, so that the voltage V can also be applied to the nano-composite film 1, which also plays a role in heating the screen, thereby increasing the response speed of the liquid crystal and improving the display effect.

[0116] Of course, when connecting specific components, as the position of the nano-composite film 1 changes, the number of sub-membranes it contains and the arrangement period of the film layers in each sub-membrane are different, the connection position of the nano-composite film 1 and the power source V is different. For example, the nano-composite film 1 includes 5 sub-membranes, but one of the sub-membranes contains a doped metal oxide film layer. At this time, only this film layer of the nano-composite film 1 is connected to the voltage source V. When multiple sub-membranes of the nano-composite film 1 contain doped metal oxide film layers, the doped metal oxide film layers contained in multiple sub-membranes can also be set to be connected to the voltage source V. It should be understood that at this time, the doped metal oxide film layers contained in multiple sub-membranes are connected to the voltage source V, and multiple doped metal oxide film layers are connected in parallel. This connection method has a better screen heating effect and is more conducive to providing display protection for the screen in extremely low temperature environments.

[0117] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not limited to the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any changes, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention shall be included in the protection scope of the present invention.

Claims

1. A nanocomposite film, characterized in that: The nanocomposite film includes at least two different sub-films stacked together, each of which includes a combination of one or more of a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a doped metal oxide film layer.

2. The nanocomposite film according to claim 1, characterized in that A combination of one or more of the silicon-based nitride (SiNx) film layer, silicon-based oxide (SiOx) film layer, metal oxide film layer, and doped metal oxide film layer is periodically arranged along the stacking direction of the sub-film, thereby constituting the sub-film of the nanocomposite film.

3. The nanocomposite film according to claim 2, characterized in that The nanocomposite film comprises 10-40 film layers.

4. The nanocomposite film according to claim 3, characterized in that The nanocomposite film comprises 13 to 39 film layers.

5. The nanocomposite film according to claim 4, characterized in that The nanocomposite film comprises 15-20 film layers.

6. The nanocomposite film according to claim 1, characterized in that The metal oxide forming the metal oxide film layer includes one of niobium oxide and titanium oxide.

7. The nanocomposite film according to claim 1, characterized in that The doped metal oxide forming the doped metal oxide film layer includes one of tin-doped indium oxide (ITO), fluorine-doped indium oxide (FTO), and aluminum-doped zinc oxide (AZO).

8. The nanocomposite film according to claim 1, characterized in that The nanocomposite film includes five stacked sub-films, each of which includes a combination of one or more of a silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer, a metal oxide film layer, and a doped metal oxide film layer.

9. The nanocomposite film according to claim 8, characterized in that A combination of one or more of the silicon-based nitride (SiNx) film layer, silicon-based oxide (SiOx) film layer, metal oxide film layer, and doped metal oxide film layer is periodically arranged along the stacking direction of the sub-films, thereby constituting five sub-films of the nanocomposite film.

10. The nanocomposite film according to claim 9, characterized in that The 5 sub-films are arranged in the following order along the stacking direction: A first sub-film including the silicon-based nitride (SiNx) film layer, a silicon-based oxide (SiOx) film layer and a doped metal oxide film layer; A second sub-film including the metal oxide film layer and a doped metal oxide film layer; A third sub-film including the metal oxide film layer and a silicon-based nitride (SiNx) film layer; A fourth sub-film including the metal oxide film layer and the doped metal oxide film layer; as well as, A fifth sub-film includes a metal oxide film layer and a silicon-based oxide (SiOx) film layer.

11. The nanocomposite film according to claim 10, characterized in that The first sub-film includes 1 to 3 film layer arrangement periods; the second sub-film includes 1 to 3 film layer arrangement periods; The third sub-film includes 1-3 film layer arrangement periods; The fourth sub-film includes 2-6 film layer arrangement periods; The fifth sub-film includes 1-3 film layer arrangement periods.

12. The nanocomposite film according to claim 11, characterized in that The first sub-film includes two film layer arrangement periods; The second sub-film includes 1 film layer arrangement period; The third sub-film includes 1 film layer arrangement period; The fourth sub-film includes 4 film layer arrangement periods; The fifth sub-film includes one film layer arrangement period.

13. The nanocomposite film according to claim 12, characterized in that In one film layer arrangement period of the first sub-film, The silicon-based nitride (SiNx) film layer has a refractive index of 1.75-1.85 and a thickness of 150nm-300nm; The silicon-based oxide (SiOx) film layer has a refractive index of 1.44-1.47 and a thickness of 100nm-300nm; The refractive index of the doped metal oxide film layer is between 1.78-1.85 and is not lower than the refractive index of the silicon-based nitride (SiNx) film layer, and the thickness is 20nm-40nm.

14. The nanocomposite film according to claim 12, characterized in that In one film layer arrangement period of the second sub-film, The refractive index of the metal oxide film layer is 2.27-2.35, and the thickness is 150nm-200nm; the refractive index of the doped metal oxide film layer is 1.75-1.85, and the thickness is 30nm-60nm.

15. The nanocomposite film according to claim 12, characterized in that In one film layer arrangement period of the third sub-film, The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 50nm-100nm; The refractive index of the silicon-based nitride (SiNx) film layer is 1.75-1.85, and the thickness is 150nm-300nm.

16. The nanocomposite film according to claim 12, characterized in that In one film layer arrangement period of the fourth sub-film, The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 70nm-150nm; The doped metal oxide film has a refractive index of 1.78-1.85 and a thickness of 15nm-50nm.

17. The nanocomposite film according to claim 12, characterized in that In one film layer arrangement period of the fifth sub-film, The metal oxide film layer has a refractive index of 2.27-2.35 and a thickness of 150nm-250nm; The silicon-based oxide (SiOx) film layer has a refractive index of 1.44-1.47 and a thickness of 300nm-500nm.

18. A display screen module, characterized in that: The display screen module comprises the nanocomposite film according to any one of claims 1 to 17 and a transparent substrate layer, wherein the nanocomposite film is plated on one side of the transparent substrate layer.

19. The display screen module according to claim 18, wherein: The material forming the transparent base layer includes glass or one of organic glasses PC, PMMA and PET.

20. The display screen module according to claim 19, wherein: The material forming the transparent base layer is glass.

21. The display screen module according to claim 20, characterized in that: The refractive index of the transparent substrate layer is 1.46-1.

53.

22. The display screen module according to claim 21, wherein: The refractive index of the transparent substrate layer is 1.49-1.

52.

23. The display screen module according to claim 18, wherein: The display screen module also includes an electric control system, and one or more sub-films containing a doped metal oxide film layer included in the nano-composite film are electrically connected to the electric control system.