Plum-blossom-shaped rod with built-in structure reinforcing function

By designing a plum blossom rod with built-in structural reinforcement function, the problems of insufficient heat dissipation and short service life of the high-frequency welding magnetic rod are solved, and more efficient heat dissipation and cleaning are achieved, and the service life of the equipment is extended.

CN222071657UActive Publication Date: 2024-11-26QINGZHOU YAHUI ELECTROMAGNETIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420713358.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-09
Publication Date
2024-11-26
Estimated Expiration
2034-04-09

AI Technical Summary

Technical Problem

The high-frequency welding magnetic rod has a smooth surface, a small effective heat dissipation area, a simple raw material formula and a low material purity, resulting in a short service life.

Method used

Design plum blossom rods with built-in structural reinforcement function, including welding magnetic rod body, plum blossom block, flowing groove, slide groove, cleaning mechanism, etc., to increase the heat dissipation area and cleaning efficiency, and there are internal heat dissipation holes and reinforcement rings, cleaning rings and sliders Use together.

Benefits of technology

It effectively improves the heat dissipation efficiency and service life of the welding magnetic rod, and extends the service life of the equipment by increasing the heat dissipation area and cleaning efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222071657U_ABST
    Figure CN222071657U_ABST
Patent Text Reader

Abstract

The utility model discloses a plum-blossom-shaped rod with a built-in structure reinforcing function, and relates to the technical field of welding magnetic rods, the plum-blossom-shaped rod comprises a welding magnetic rod body, plum-blossom-shaped blocks are arranged on the surface of the welding magnetic rod body, a plurality of water flowing grooves are formed between the plum-blossom-shaped blocks, sliding grooves are symmetrically formed in the side walls of the plum-blossom-shaped blocks, and the plum-blossom-shaped rod further comprises a cleaning mechanism. An effective heat dissipation effect is achieved by arranging a plum blossom block, the heat dissipation area of materials is increased by designing the surface of the welding magnetic bar body into a plum blossom shape, the surface area of the welding magnetic bar body is increased by more than 100% compared with the surface area of a smooth magnetic bar, and the surface area of the welding magnetic bar body is increased by more than 100%. And the heat dissipation efficiency of the material is effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of welding magnetic rods, in particular to a plum blossom rod with a built-in structural reinforcement function. Background Art

[0002] High-frequency welding magnetic rods are also called welding magnetic cores. The products are round magnetic shapes with different diameters. They are used for high-frequency welding. High-frequency welding is widely used in the production and manufacturing process of seamed steel pipes. The welded steel pipes become welded pipes. High-frequency welding magnetic rods are used as impedances and welded in high-frequency pipe welding machines. Since high-frequency welding has the advantages of wide material, high welding speed, good quality, and low energy consumption, high-frequency welded steel pipes have developed rapidly.

[0003] High-frequency welding magnetic rods are made of ferrite and are indispensable electronic components in high-frequency welding. More than tens of millions of ferrite magnetic rods are consumed each year. With the development of industry, the use of welding pipes is increasing, and more and more ferrite magnetic rods are used. Since the magnetic rods will generate a lot of heat during the welding process, the steel pipes outside the ferrite magnetic rods are always at high temperature. Even with running water cooling, the internal temperature of the ferrite magnetic rods will exceed 100 degrees. At present, domestic round welding rods have a relatively smooth surface, a small effective heat dissipation area, a simple raw material formula, low material purity, many impurities and a short service life.

[0004] Based on this, a plum blossom stick with a built-in structural reinforcement function is now provided, which can eliminate the disadvantages of the existing device. Utility Model Content

[0005] The utility model aims to provide a plum blossom rod with a built-in structural reinforcement function to solve the problems of a welding rod having a relatively smooth surface, a small effective heat dissipation area, a simple raw material formula, low material purity, many impurities and a short service life.

[0006] In order to achieve the above purpose, the utility model provides the following technical solutions:

[0007] A plum blossom rod with built-in structural reinforcement function includes a welded magnetic rod body, a plum blossom block is arranged on the surface of the welded magnetic rod body, a plurality of water flow grooves are arranged between the plum blossom blocks, and the side walls of the plum blossom blocks are symmetrically provided with slide grooves. It also includes a cleaning mechanism, and a cleaning mechanism is slidably arranged in the water flow groove for cleaning dust on the surface of the welded magnetic rod body.

[0008] On the basis of the above technical solutions, the present invention also provides the following optional technical solutions:

[0009] In an optional solution: a plurality of heat dissipation holes are provided inside the welding magnetic rod body.

[0010] In an optional solution: a reinforcement ring is provided inside the welded magnetic rod body.

[0011] In an optional solution: the cross-section of the welding magnetic rod body is plum blossom-shaped.

[0012] In an optional solution: the cleaning mechanism includes a slide groove, a cleaning ring, and a sliding block. The side wall of the plum blossom block is symmetrically provided with a slide groove, a cleaning ring is slidably provided in the slide groove, and a sliding block adapted to the slide groove is provided on the cleaning ring.

[0013] In an optional solution: the side wall of the cleaning ring is provided with a plurality of anti-slip grooves.

[0014] In an optional solution: a limit block is provided at the end of the plum blossom block.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0016] 1. The utility model achieves the effect of effective heat dissipation by arranging the plum blossom block. By designing the surface of the welding magnetic rod body into a plum blossom shape, the heat dissipation area of ​​the material is increased, so that the surface area of ​​the welding magnetic rod body is increased by more than 100% compared with the surface area of ​​the smooth magnetic rod, effectively improving the heat dissipation efficiency of the material.

[0017] 2. The utility model achieves the effect of quickly cleaning the dust on the surface of the welding magnetic rod body by setting a cleaning mechanism. The cleaning ring slides in the slide groove, and the cleaning brush in the cleaning ring is used to quickly clean the dust and impurities on the surface of the welding magnetic rod body, thereby improving work efficiency and extending service life. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the internal structure of the utility model.

[0019] Figure 2 It is a structural schematic diagram of the plum blossom block of the utility model.

[0020] Figure 3 It is a schematic diagram of the overall structure of the utility model.

[0021] Figure 4 It is a structural schematic diagram of the cleaning ring of the utility model.

[0022] Notes on the figure numbers: welded magnetic rod body 100 , heat dissipation hole 101 , reinforcement ring 102 , plum blossom block 200 , water flow groove 201 , slide groove 202 , cleaning ring 300 , anti-slip pattern 301 , slider 302 . DETAILED DESCRIPTION

[0023] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. Example 1

[0024] In one embodiment, Figure 1-Figure 4 As shown, a plum blossom rod with built-in structural reinforcement function includes a welded magnetic rod body 100. The welded magnetic rod body 100 adopts secondary reduction sintering, and no oxide layer is generated on the surface, which can reduce the PCV of the material and improve the BS value of the magnetic rod. The surface of the welded magnetic rod body 100 is provided with a plum blossom block 200, and a plurality of water flow grooves 201 are provided between the plum blossom blocks 200. The side walls of the plum blossom blocks 200 are symmetrically provided with slide grooves 202. The welding magnetic rod body 100 and the plum blossom block 200 are formed by extrusion molding, which can enhance the density of the product and ensure that the internal structure of the material is dense and uniform, with low porosity, good mechanical strength and good heat shock resistance, and can more conveniently meet customer needs, higher molding efficiency, and reduce production costs. It also includes a cleaning mechanism, and a cleaning mechanism for cleaning dust on the surface of the welded magnetic rod body 100 is slidably provided in the water flow groove 201.

[0025] In one embodiment, Figure 1 As shown, the welding magnet bar body 100 is provided with a plurality of heat dissipation holes 101 inside to enhance the heat dissipation effect and also play a role in noise reduction.

[0026] In one embodiment, Figure 1-Figure 2 As shown, a reinforcement ring 102 is provided inside the welding magnet bar body 100 to perform built-in reinforcement to enhance the strength of the welding magnet bar body 100 .

[0027] In one embodiment, Figure 2 As shown, the cross section of the welding magnetic rod body 100 is plum blossom-shaped, which increases the heat dissipation area of ​​the material, so that the surface area of ​​the welding magnetic rod body 100 is increased by more than 100% compared with the surface area of ​​the smooth magnetic rod, effectively improving the heat dissipation efficiency of the material.

[0028] In one embodiment, Figure 3-Figure 4 As shown, the cleaning mechanism includes a slide groove 202, a cleaning ring 300, and a slider 302. The side wall of the plum blossom block 200 is symmetrically provided with a slide groove 202. A cleaning ring 300 is slidably provided in the slide groove 202. The cleaning ring 300 is provided with a slider 302 adapted to the slide groove 202. The cleaning ring 300 slides in the slide groove 202 by means of the slider 302 to quickly clean up dust and impurities on the surface of the welding magnetic rod body 100, thereby improving work efficiency and extending service life. Example 2

[0029] In one embodiment, Figure 3-Figure 4 As shown, the side wall of the cleaning ring 300 is provided with a plurality of anti-skid grooves 301 to prevent skidding.

[0030] In one embodiment, Figure 3-Figure 4As shown, a limit block is provided at the end of the plum blossom block 200 to prevent the cleaning ring 300 from falling.

[0031] In one embodiment, Figure 1-Figure 4 As shown, the welding magnet rod body 100 is made of iron, manganese, zinc and trace elements. A special iron, manganese and zinc ratio is used to control the purity of the material. Trace elements such as copper oxide, cobalt oxide and zirconium oxide are added to the material to make the 100-degree BS of the material reach more than 600mT. At the same time, the Tc of the material can reach more than 300°C, and the Pcv is reduced to 400mw / cm3, which can carry a larger current and better temperature resistance.

[0032] Working principle: When in use, the reinforcement ring 102 is used for built-in reinforcement to strengthen the strength of the welding magnet body 100, and the heat dissipation hole 101 is used to enhance the heat dissipation effect and reduce noise at the same time. The plum blossom block 200 is used to increase the heat dissipation area of ​​the material, so that the surface area of ​​the welding magnet body 100 is increased by more than 100% compared with the surface area of ​​the smooth magnet, which effectively improves the heat dissipation efficiency of the material. After the welding magnet body 100 has been working for a period of time, the operator uses the slider 302 to slide the cleaning ring 300 in the slide groove 202 to quickly clean up the dust and impurities on the surface of the welding magnet body 100, thereby improving work efficiency and extending service life.

[0033] The above is only a specific implementation of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any person skilled in the art who is familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.

Claims

1. A plum blossom bar with a built-in structural reinforcement function, comprising a welded magnetic bar body (100), a plum blossom block (200) is provided on the surface of the welded magnetic bar body (100), a plurality of water flow grooves (201) are provided between the plum blossom blocks (200), and a slide groove (202) is symmetrically provided on the side wall of the plum blossom block (200), characterized in that: It also comprises a cleaning mechanism, wherein a cleaning mechanism for cleaning dust on the surface of the welding magnetic bar body (100) is slidably provided in the water flow groove (201).

2. The plum blossom stick with built-in structural reinforcement function according to claim 1, characterized in that: A plurality of heat dissipation holes (101) are provided inside the welding magnetic bar body (100).

3. The plum blossom stick with built-in structural reinforcement function according to claim 1, characterized in that: A reinforcement ring (102) is provided inside the welded magnetic bar body (100).

4. The plum blossom stick with built-in structural reinforcement function according to claim 1, characterized in that: The cross section of the welding magnetic rod body (100) is plum blossom-shaped.

5. The plum blossom stick with built-in structural reinforcement function according to claim 1, characterized in that: The cleaning mechanism comprises a cleaning ring (300) and a sliding block (302); the cleaning ring (300) is slidably arranged in the sliding groove (202); and the cleaning ring (300) is provided with a sliding block (302) adapted to the sliding groove (202).

6. The plum blossom stick with built-in structural reinforcement function according to claim 5, characterized in that: The side wall of the cleaning ring (300) is provided with a plurality of anti-slip grooves (301).

7. The plum blossom stick with built-in structural reinforcement function according to claim 1, characterized in that: A limiting block is provided at the end of the plum blossom block (200).