Anti-loose pre-coating fastener appearance protection device
Through the magnetic conveyor belt and separation design, the coating and drying of fasteners are handled separately, which solves the problem that fasteners are prone to stick or bump during the anti-loosening coating process, reduces paint consumption and drying time, and improves buckles protection and production efficiency of parts.
Patent Information
- Application Number
- CN202420567160.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-22
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-03-22
AI Technical Summary
In the existing fastener anti-loose coating process, multiple fasteners are easily sticky or damaged due to soaking together, and the amount of sealant in the soaking tank is wasteful.
The magnetic conveyor belt and separation design are adopted, and the fastener is conveyed separately through the magnetic conveyor belt, equipped with a feeding mechanism and a drying mechanism, so that the coating and drying time can be achieved, reducing the coating use and drying time.
It effectively avoids collision damage between fasteners, reduces paint consumption and drying time, and improves the protective effect and production efficiency of fasteners.
Smart Images

Figure CN222077030U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of fastener processing, in particular to an anti-loosening pre-coated fastener appearance protection device. Background Art
[0002] The fasteners will go through the process of processing and drying during the anti-loosening coating process. However, after these processes, the fasteners will become more susceptible to damage, and the appearance will also be easily discolored due to the influence of drying and heating. In order to increase the service life of the fasteners and prevent discoloration, the fasteners will be soaked in a sealant to provide a layer of protection on the surface of the fasteners for easy storage.
[0003] The current fastener protection treatment is a cage-type conveying method, which puts multiple fasteners into a cage and soaks them in a soaking tank, and then dries them. However, this processing method is easy to stick to each other or collide with each other, causing damage, and it is not easy to dry in the cage. In addition, the amount of sealant required in the soaking tank is large, which is easy to cause waste.
[0004] In view of this, a better improvement scheme is proposed to solve the above problems. Utility Model Content
[0005] The main purpose of the utility model is to provide an anti-loosening pre-coated fastener appearance protection device, which is used to solve the problem that when the fasteners are protected, they are easily stuck to each other or collide with each other because they are soaked together, causing damage.
[0006] To achieve the above-mentioned purpose, the utility model provides an anti-loosening pre-coated fastener appearance protection device, which is used for coating and drying on a fastener, and includes:
[0007] A magnetic conveyor belt, the fastener can be adsorbed on the magnetic conveyor belt, and has a conveying path, the fastener can move along the conveying path;
[0008] A material ejection mechanism, which is used to apply a coating to the fastener and is located below the magnetic conveyor belt, and the conveying path passes through the material ejection mechanism;
[0009] a drying mechanism, which is used to dry the fastener, and the conveying path passes through the drying mechanism;
[0010] The fastener can pass through the material ejection mechanism and the drying mechanism in sequence.
[0011] As described above, the anti-loosening pre-coated fastener appearance protection device, wherein the material emitting mechanism comprises:
[0012] An inner flow groove, the inner flow groove can accommodate the coating, the conveying path passes through the inner flow groove, and the opening direction of the inner flow groove faces the magnetic conveyor belt;
[0013] An outer flow slot is located below the inner flow slot, and the opening direction of the outer flow slot is toward the inner flow slot; the outer flow slot is closer to the drying mechanism than the inner flow slot.
[0014] As described above, the anti-loosening pre-coated fastener appearance protection device, wherein the material emitting mechanism comprises:
[0015] A feeding pipe, which is disposed through one side wall of the inner flow channel;
[0016] A recovery pipe is located below the outer flow channel.
[0017] As described above, the anti-loosening pre-coated fastener appearance protection device, wherein the inner flow channel has a coating layer, which is used to apply the coating on the fastener, and the conveying path passes through the coating layer.
[0018] As described above, the anti-loosening pre-coated fastener appearance protection device, wherein the drying mechanism has a drying tunnel, and the conveying path passes through the drying tunnel.
[0019] As described above, the anti-loosening pre-coated fastener appearance protection device, wherein the drying mechanism comprises:
[0020] An air supply mechanism is located below the drying tunnel and comprises:
[0021] An air inlet located on the bottom surface of the air supply mechanism;
[0022] a first gap, which is located at one end of the air supply mechanism connected to the drying tunnel, and the first gap is parallel to the conveying path;
[0023] The drying tunnel also includes:
[0024] an outer shell;
[0025] a second slit formed on the outer shell and corresponding in position to the first slit;
[0026] Two partitions are arranged in the outer shell, and the conveying path passes between the two partitions.
[0027] A bottom plate is connected to the two partition plates at a side away from the magnetic conveyor belt.
[0028] As described above, in the anti-loosening pre-coated fastener appearance protection device, each of the partitions of the drying tunnel includes at least one through hole.
[0029] The anti-loosening pre-coated fastener appearance protection device as mentioned above includes:
[0030] A material unloading mechanism is arranged on the magnetic conveyor belt and passes through the conveying path, and the fastener passes through the material ejection mechanism, the drying mechanism and the material unloading mechanism in sequence.
[0031] As mentioned above, the anti-loosening pre-coated fastener appearance protection device, wherein:
[0032] The unloading mechanism includes a baffle, which is parallel to and close to the magnetic conveyor belt and passes through the conveying path, and also includes:
[0033] A side edge is an oblique edge relative to the conveying path, so the side edge is staggered with the conveying path.
[0034] The advantage of the utility model is that it can coat multiple fasteners individually through the design of the magnetic conveying device, so that the fasteners can be separated and will not collide with each other and cause damage. In addition, because it can coat a single fastener, it is not necessary to prepare a large amount of paint to soak the fastener, which can reduce the consumption of paint. Similarly, because it can dry a single fastener, it can also reduce the required drying time and make the fastener easier to dry. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 It is a three-dimensional schematic diagram of the utility model.
[0036] Figure 2 It is a side view schematic diagram of the utility model.
[0037] Figure 3 It is a three-dimensional schematic diagram of the material ejection mechanism of the utility model.
[0038] Figure 4 It is a cross-sectional schematic diagram of the material ejection mechanism of the utility model.
[0039] Figure 5 It is a three-dimensional schematic diagram of the drying mechanism of the utility model.
[0040] Figure 6 It is a cross-sectional schematic diagram of the drying mechanism of the utility model.
[0041] Figure 7 It is a cross-sectional schematic diagram of the drying mechanism of the utility model.
[0042] In the figure: A, fastener; 10, magnetic conveying device; 11, magnetic conveyor belt; 12, conveying wheel; 20, material ejection mechanism; 21, inner flow trough; 211, coating layer; 22, outer flow trough; 23, feeding pipe; 24, recovery pipe; 30, drying mechanism; 31, air supply mechanism; 311, air inlet; 312, first gap; 32, drying tunnel; 321, outer shell; 3211, second gap; 322, partition; 3221, through hole; 323, bottom plate; 40, unloading mechanism; 41, baffle; 50, collecting trough. DETAILED DESCRIPTION
[0043] Please refer to Figure 1 and Figure 2 The utility model provides an anti-loosening pre-coated fastener appearance protection device, which is used for coating and drying on a fastener A, and has a magnetic conveying device 10, a feeding mechanism 20 and a drying mechanism 30, and can optionally have a feeding mechanism 40. The fastener A can pass through the feeding mechanism 20, the drying mechanism 30 and the feeding mechanism 40 in sequence.
[0044] The magnetic conveying device 10 has a magnetic conveying belt 11, two conveying wheels 12 and a conveying path, and the fastener A can be adsorbed on the magnetic conveying belt 11. In this embodiment, the magnetic conveying belt 11 contains magnets, so that the fastener A can be adsorbed on the magnetic conveying belt 11. The magnetic conveying belt 11 is sleeved on the two conveying wheels 12, one of which is connected to a power mechanism, so that the magnetic conveying belt 11 can transport the fastener A to move. The fastener A moves along the conveying path and passes through the material ejection mechanism 20, the drying mechanism 30 and the unloading mechanism 40 in sequence.
[0045] Please refer to Figure 3 and Figure 4 The ejecting mechanism 20 is used to apply a coating on the fastener A and is located below the magnetic conveyor belt 11, and the conveying path passes through the ejecting mechanism 20. The ejecting mechanism 20 has an inner flow trough 21, an outer flow trough 22, a feeding pipe 23 and a recovery pipe 24.
[0046] The inner flow groove 21 is used to accommodate the paint, and the conveying path passes through the inner flow groove 21, and the opening direction of the inner flow groove 21 faces the magnetic conveyor belt 11. In this embodiment, the inner flow groove 21 has a coating layer 211 that can absorb the paint, such as a sponge or a brush, so that when the fastener A passes through, the paint on the coating layer 211 can be applied to the fastener A.
[0047] The outer flow groove 22 is located below the inner flow groove 21, and the opening direction of the outer flow groove 22 is toward the inner flow groove 21. Specifically, the outer flow groove 22 and the inner flow groove 21 overlap in the vertical direction, and on the conveying path, the outer flow groove 22 protrudes further toward the drying mechanism 30 than the inner flow groove 21. Therefore, when the fastener A passes through the inner flow groove 21, it will pass over the outer flow groove 22, and the excess paint that is not adsorbed on the fastener A can drip into the outer flow groove 22 and be recovered. In this embodiment, the length of the outer flow groove 22 parallel to the conveying path is greater than the length of the inner flow groove 21 parallel to the conveying path. In other embodiments, the length of the outer flow groove 22 parallel to the conveying path may not be limited in this way, as long as the fastener A can pass over the outer flow groove 22 after passing through the inner flow groove 21.
[0048] The feeding pipe 23 is provided through one side wall of the inner flow groove 21, and is used to inject the paint into the inner flow groove 21. The recovery pipe 24 is located below the outer flow groove 22, and is used to recover the paint dripping into the outer flow groove 22. The paint recovered by the recovery pipe 24 can be injected into the inner flow groove 21 through the feeding pipe 23 after being processed, so that the recovered paint can be recycled.
[0049] Please refer to Figures 5 to 7 . The drying mechanism 30 is used to dry the fastener A and is located below the magnetic conveyor belt 11, and the conveying path passes through the drying mechanism 30. The drying mechanism 30 has an air supply mechanism 31 and a drying tunnel 32. The air supply mechanism 31 is located below the magnetic conveyor belt 11, and its width gradually decreases toward the magnetic conveyor belt 11. The air supply mechanism 31 has an air inlet 311 and a first gap 312. The air inlet 311 is located on the bottom surface of the air supply mechanism 31, but is not limited to this. The first gap 312 is parallel to the conveying path and is located at one end close to the magnetic conveyor belt 11, so that the air supply mechanism 31 can supply air to the fastener A located on the magnetic conveyor belt 11.
[0050] The drying tunnel 32 is located between the magnetic conveying device 10 and the air supply mechanism 31, and the conveying path passes through the drying tunnel 32. In this embodiment, the drying tunnel 32 and the magnetic conveyor belt 11 surround the conveying path. The drying tunnel 32 has an outer shell 321, two partitions 322 and a bottom plate 323. The outer shell 321 has a second slit 3211, and the second slit 3211 is located at one end of the outer shell 321 away from the magnetic conveyor belt 11, and corresponds to the first slit 312 in position. Specifically, in this embodiment, the first slit 312 is connected to the second slit 3211. The two partitions 322 are arranged in the outer shell 321, and the conveying path passes between the two partitions 322, and each partition 322 has at least one through hole 3221. The bottom plate 323 connects the two partitions 322 away from the magnetic conveyor belt 11, thereby forming a U-shaped cross section. In other embodiments, the drying tunnel 32 may not have the bottom plate 323 , that is, the two partition plates 322 may be connected at the sides away from the magnetic conveyor belt 11 , thereby forming a V-shaped cross section.
[0051] In this embodiment, when fastener A passes through the drying mechanism 30, the hot air required for drying can sequentially pass through the air inlet 311, the first slit 312, the second slit 3211 and the through hole 3221 on the partition 322, and contact the fastener A for drying. Therefore, the hot air entering from the air inlet 311 can reduce the intensity so that the paint on the fastener A will not be blown away by the hot air. In this embodiment, the drying mechanism 30 dries the paint on the fastener A by blowing air. In other embodiments, the drying mechanism 30 may not have the air supply mechanism 31, and the drying tunnel 32 may be an electric heating tube, using electric heating to dry the paint on the fastener A.
[0052] The unloading mechanism 40 is arranged on the magnetic conveyor belt 11 and passes through the conveying path. In the present embodiment, the unloading mechanism 40 has a baffle 41, which is parallel to and close to the magnetic conveyor belt 11 and passes through the conveying path. Specifically, the baffle 41 can approach the magnetic conveyor belt 11, but does not affect the conveying of the fastener A of the magnetic conveyor belt 11. The baffle 41 has a side. The side of the baffle 41 is a bevel relative to the conveying path, so the side is staggered with the conveying path. When the fastener A contacts the baffle 41, it will be guided by the bevel of the baffle 41, deviate from the conveying path, and leave the magnetic conveyor belt 11. In the present embodiment, the unloading mechanism 40 is connected to a collecting trough 50, and the opening of the collecting trough 50 is located below the baffle 41. After the fastener A leaves the magnetic conveyor belt 11, it will fall into the collecting trough 50 for collection.
[0053] When the fastener A is coated by the utility model, multiple fasteners A can be individually adsorbed on the magnetic conveyor belt 11 and enter the conveying path. Each fastener A can be coated with paint on the fastener A in sequence through the feeding mechanism 20, and then the paint adsorbed on the fastener A is dried by the drying mechanism 30, and finally the fastener A is separated from the magnetic conveyor belt 11 and collected by the unloading mechanism 40, completing the whole fastener A coating process.
[0054] The advantage of the present invention is that the design of the magnetic conveying device 10 can be used to coat multiple fasteners A individually, so that the fasteners A can be separated and will not collide with each other and cause damage. In addition, since a single fastener A can be coated, it is not necessary to prepare a large amount of paint to soak the fastener A, which can reduce the consumption of paint. Similarly, since a single fastener A can be dried, the required drying time can be reduced and the fastener can be dried more easily.
Claims
1. An anti-loosening pre-coated fastener appearance protection device, characterized in that: For coating and drying on a fastener, including: A magnetic conveyor belt, the fastener can be adsorbed on the magnetic conveyor belt, and has a conveying path, the fastener can move along the conveying path; A material ejection mechanism, which is used to apply a coating to the fastener and is located below the magnetic conveyor belt, and the conveying path passes through the material ejection mechanism; a drying mechanism, which is used to dry the fastener, and the conveying path passes through the drying mechanism; The fastener can pass through the material ejection mechanism and the drying mechanism in sequence.
2. The anti-loosening pre-coated fastener appearance protection device according to claim 1, characterized in that: The fraud agencies include: An inner flow groove, the inner flow groove can accommodate the coating, the conveying path passes through the inner flow groove, and the opening direction of the inner flow groove faces the magnetic conveyor belt; An outer flow slot is located below the inner flow slot, and the opening direction of the outer flow slot is toward the inner flow slot; the outer flow slot is closer to the drying mechanism than the inner flow slot.
3. The anti-loosening pre-coated fastener appearance protection device according to claim 2, characterized in that: The fraud agencies include: A feeding pipe, which is disposed through one side wall of the inner flow channel; A recovery pipe is located below the outer flow channel.
4. The anti-loosening pre-coated fastener appearance protection device according to any one of claims 2 or 3, characterized in that: The inner flow channel has a coating layer, which is used to coat the coating on the fastener, and the conveying path passes through the coating layer.
5. The anti-loosening pre-coated fastener appearance protection device according to claim 1, characterized in that: The drying mechanism has a drying tunnel, and the conveying path passes through the drying tunnel.
6. The anti-loosening pre-coated fastener appearance protection device according to claim 5, characterized in that: The drying mechanism comprises: An air supply mechanism, located below the drying tunnel, comprises: An air inlet located on the bottom surface of the air supply mechanism; a first gap, which is located at one end of the air supply mechanism connected to the drying tunnel, and the first gap is parallel to the conveying path; The drying tunnel also includes: an outer shell; a second slit formed on the outer shell and corresponding in position to the first slit; Two partitions are arranged in the outer shell, and the conveying path passes through the two partitions; A bottom plate is connected to the two partition plates at a side away from the magnetic conveyor belt.
7. The anti-loosening pre-coated fastener appearance protection device according to claim 6, characterized in that: Each of the partitions of the drying tunnel has at least one through hole.
8. The anti-loosening pre-coated fastener appearance protection device according to claim 1, characterized in that: include: A material unloading mechanism is arranged on the magnetic conveyor belt and passes through the conveying path, and the fastener passes through the material ejection mechanism, the drying mechanism and the material unloading mechanism in sequence.
9. The anti-loosening pre-coated fastener appearance protection device according to claim 8, characterized in that: The unloading mechanism has a baffle, which is parallel to and close to the magnetic conveyor belt and passes through the conveying path, including: A side edge is an oblique edge relative to the conveying path, whereby the side edge intersects with the conveying path.