Rapid heating breathable polymer foam forming mold
By increasing the ventilation area and structure in the polymer foaming mold, the problem of insufficient ventilation is solved, the rapid penetration and exhaust of gas is achieved, the foaming rate and product quality are improved, and it is suitable for the molding of high-melting polymers.
Patent Information
- Application Number
- CN202420655917.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-01
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-04-01
AI Technical Summary
The insufficient ventilation area of existing polymer foam forming molds leads to poor gas flow, affecting the penetration rate and pressure relief rate of physical foaming agents, resulting in insufficient foaming rate.
A fast heating breathable polymer foaming mold is designed. By setting multiple channels between the upper template and the lower template, the area of gas entering and exiting the mold is increased. The circular pinhole or gas slit structure is adopted to ensure rapid gas flow and Exit, increasing the permeability rate and exhaust rate.
The rapid penetration and exhaust of gas is achieved, the foaming rate and foaming rate are improved, the bubble cells of the product are fine and uniform, which significantly improves the product quality and production efficiency, and can handle high melting point polymers.
Smart Images

Figure CN222079890U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of polymer foaming molding dies, in particular to a fast-heating breathable polymer foaming molding dies. Background Art
[0002] There are three kinds of raw materials for polymer foaming to make available finished products: one is to directly use thermoplastic polymer particles for supercritical fluid foaming molding; the second is to use plastic processing and molding methods to prepare thermoplastic polymer particles into pre-molded embryos for polymer foaming molding, and then use supercritical fluid to foam the pre-molded embryos; the third is to preliminarily foam the thermoplastic polymer particles to become foamed beads; then add the foamed beads to the foaming molding mold, use high-temperature steam to heat or introduce supercritical fluid, and the foamed beads will foam, swell and bond with each other under high pressure and high temperature to make the finished product.
[0003] Existing molding molds are generally composed of an upper mold and a lower mold, but in terms of ventilation, the area for ventilation in and out is often insufficient, resulting in poor gas flow and ventilation. In the theory of polymer foaming, the speed of gas flow in the molding mold directly affects the penetration rate of the physical foaming agent into the polymer, as well as the rate of pressure relief of the physical foaming agent, resulting in insufficient foaming ratio of the polymer. Summary of the invention
[0004] The purpose of the utility model is to overcome the above-mentioned defects in the prior art and provide a fast heating breathable polymer foaming molding mold; to increase the rate at which gas quickly enters the mold and quickly exits the mold, thereby indirectly increasing the penetration rate of super gas into the polymer, so that the mold can be vented quickly, the pressure relief rate is fast, and the pressure relief exhaust foaming rate is increased.
[0005] To achieve the above-mentioned purpose, the utility model provides a fast heating breathable polymer foaming molding mold, including an upper template and a lower template that cooperates with the upper template, and a molding cavity is arranged between the upper template and the lower template; the upper template includes a first support plate and a first breathable plate installed on one side of the first support plate, and the lower template includes a second support plate and a second breathable plate installed on one side of the second support plate; the first breathable plate is provided with a first channel for gas to enter and exit; the second breathable plate is provided with a second channel for gas to enter and exit; the projection area of the first channel accounts for 50~80% of the projection area of the bottom of the first breathable plate; the projection area of the second channel accounts for 50~80% of the projection area of the bottom of the second breathable plate; the gas flows into the molding cavity from the first channel and / or the second channel, and flows out from the first channel and / or the second channel.
[0006] Preferably, the first channel and the second channel are circular pinhole structures, and the circular pinhole structures are evenly distributed on the first air permeable plate and the second air permeable plate.
[0007] Preferably, the first channel and the second channel are air gap structures, and the air gap structures are evenly distributed on the first air permeable plate and the second air permeable plate.
[0008] Preferably, the air gap structure has a plurality of air-permeable grooves for gas to pass through, and the air-permeable grooves are linear and distributed horizontally or vertically; or the air-permeable grooves are at angles to each other; the air-permeable grooves are at an angle of 120°, forming a Y shape; or the air-permeable grooves are perpendicular to each other, forming a square or right-angled shape or a square spiral shape.
[0009] Preferably, the air gap structure has a plurality of air-permeable grooves for gas to pass through, wherein the air-permeable grooves are arc-shaped, and a plurality of arcs are arranged at intervals to present an arc pattern; or the air-permeable grooves are a mixture of arcs and straight lines; or the air-permeable grooves are a mixture of curves and straight lines.
[0010] Preferably, the slit width of the vent groove is between 3-6 mm, and the slit length is between 5-10 mm.
[0011] Preferably, the first support plate is provided with a first cavity connected to the first channel; the second support plate is provided with a second cavity connected to the second channel; the first support plate is provided with a plurality of first reinforcing ribs, and the first cavity is arranged between the first reinforcing ribs; the second support plate is provided with a plurality of second reinforcing ribs, and the second cavity is arranged between the second reinforcing ribs.
[0012] Preferably, the gas is high-temperature steam, and the high-temperature steam is applied to a high-temperature steam-heated foaming bead forming machine to foam and form the thermoplastic polymer particles.
[0013] Compared with the prior art, the beneficial effects of the utility model are:
[0014] 1. In the utility model, the gas can flow into the molding cavity from the first channel and / or the second channel, and flow out from the first channel and / or the second channel; the gas quickly flows into the molding cavity, and quickly penetrates into the polymer, shortening the time for the gas to dissolve into the polymer and increasing the penetration rate; and, because the mold has multiple channels for exhaust, the mold exhausts quickly and the pressure relief rate is fast, thereby increasing the foaming rate, and the exhaust rate is increased by 50%, resulting in a large foaming ratio of the product, fine and uniform foaming holes of the product, greatly improving the quality and production efficiency of the product.
[0015] 2. In the utility model, the projection area of the first channel accounts for 50-80% of the projection area of the bottom of the first air permeable plate; the projection area of the second channel accounts for 50-80% of the projection area of the bottom of the second air permeable plate; by increasing the air permeability areas of the first channel and the second channel, the gas can quickly flow into the molding cavity and can also quickly flow out of the molding cavity, so that the mold is quickly exhausted and the pressure unloading rate is fast, thereby improving the foaming rate, and the exhaust rate is increased by 50%, resulting in a large foaming ratio of the product, fine and uniform foaming holes of the product, greatly improving the quality and production efficiency of the product.
[0016] 3. The utility model increases the air permeability area and improves the gas inflow and outflow speeds, so that a variety of polymer raw materials can be installed inside the molding cavity, and pre-molded embryos, thermoplastic polymer particles or pre-foamed polymer foam beads can be foamed; further, since supercritical fluid is used to directly mold the polymer, and supercritical fluid has a higher temperature and pressure than steam, the mold can also be used to mold some high-melting-point polymers. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0018] Figure 1 It is an exploded schematic diagram of a rapid heating breathable polymer foaming molding mold provided by the utility model;
[0019] Figure 2 yes Figure 1 The enlarged schematic diagram of point A in the middle;
[0020] Figure 3 It is a cross-sectional view of a fast heating breathable polymer foaming molding mold provided by the utility model;
[0021] Figure 4 It is a cross-sectional exploded view of a rapid heating breathable polymer foaming molding die provided by the utility model;
[0022] Figure 5 It is a front view of the first air permeable plate or the second air permeable plate provided by the utility model;
[0023] Figure 6 It is a structural schematic diagram of the first channel or the second channel provided by the utility model;
[0024] Figure 7It is a front view of the V-shaped air gap structure provided by the utility model;
[0025] Figure 8 The utility model provides a plurality of straight lines that are perpendicular to each other and provide an air gap structure;
[0026] Fig. 9 The utility model provides a spiral straight air gap structure;
[0027] Fig.10 The utility model provides an air gap structure in which multiple straight lines are merged together;
[0028] Fig.11 The utility model provides an arc-shaped air gap structure;
[0029] Fig.12 The utility model provides an air gap structure in which a curve and a straight line are connected.
[0030] Included in the figure are:
[0031] 1. Upper template; 2. Lower template; 3. Molding cavity; 12. First air permeable plate; 22. Second air permeable plate; 4. First channel; 5. Second channel; 6. Air gap structure; 13. First cavity; 23. Second cavity; 14. First reinforcing rib; 24. Second reinforcing rib; 61. Air permeable groove. DETAILED DESCRIPTION
[0032] The following will be combined with the drawings in this embodiment of the utility model to clearly and completely describe the technical solution in this embodiment of the utility model. Obviously, the described embodiment is one embodiment of the utility model, not all embodiments of the utility model. Based on this embodiment of the utility model, all other embodiments of the utility model obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model. Embodiment 1
[0033] Please refer to Figures 1 to 12 , this embodiment 1 provides a rapid heating breathable polymer foaming molding mold.
[0034] like Figure 1As shown, the mold includes an upper template 1 and a lower template 2 that cooperates with the upper template 1, and a molding cavity 3 is provided between the upper template 1 and the lower template 2; the upper template 1 includes a first support plate 11 and a first air-permeable plate 12 installed inside the first support plate 11; the first support plate 11 is used to support, limit, install or fix the first air-permeable plate 12; similarly, the lower template 2 includes a second support plate 21 and a second air-permeable plate 22 installed inside the second support plate 21; the second support plate 21 is used to support, limit, install or fix The second air permeable plate 22 is fixed; the first support plate 11 is a female mold that is recessed inwardly, and the second support plate 21 is a male mold that is protruding outwardly, and the second support plate 21 can be inserted into the first support plate 11, that is, the male mold is inserted into the female mold; further, the first support plate 11 and the second support plate 21 are evenly distributed on the sides thereof with a plurality of through holes 55, and a quick locking pin device, a bolt or a positioning rod can be installed inside the through hole 55 to fix the first support plate 11 and the second support plate 21 together, so as to facilitate the subsequent foaming.
[0035] The first air permeable plate 12 and the second air permeable plate 22 are provided with polymers to be foamed, wherein the first air permeable plate 12 is provided with a first channel 4 for gas to enter and exit; the second air permeable plate 22 is provided with a second channel 5 for gas to enter and exit; the gas flows into the molding cavity 3 from the first channel 4 and / or the second channel 5, and flows out from the first channel 4 and / or the second channel 5.
[0036] In a specific embodiment, the gas can flow into the molding cavity 3 from the first channel 4 and the second channel 5 together, and quickly penetrate into the interior of the polymer, thereby reducing the penetration time and increasing the penetration rate; at the same time, during pressure relief, the gas can also flow out from the first channel 4 and the second channel 5 together, accelerating the pressure relief speed, thereby increasing the foaming rate, and increasing the exhaust rate by 50%, resulting in a large foaming ratio of the product, fine and uniform foaming holes of the product, greatly improving the quality and production efficiency of the product.
[0037] In other embodiments, the gas may also flow out of or flow into the first channel 4 or the second channel 5 .
[0038] In order to further speed up the outflow, while ensuring the rigidity of the first air permeable plate 12 and the second air permeable plate 22, the occupied area of the first channel 4 and the second channel 5 is increased as much as possible, so that the gas can quickly enter and flow out; specifically, the projection area of the first channel 4 accounts for 50-80% of the projection area of the bottom of the first air permeable plate 12; the projection area of the second channel 5 accounts for 50-80% of the projection area of the bottom of the second air permeable plate 22; by increasing the air permeability area of the first channel 4 and the second channel 5, the speed of the gas inflow and outflow is increased, so that the pressure relief speed can be accelerated, resulting in a large foaming ratio of the product, fine and uniform foaming holes of the product, and greatly improving the quality and production efficiency of the product.
[0039] Furthermore, in this embodiment, the gas has two forms, the gas is high-temperature steam or supercritical fluid, preferably supercritical fluid, and the supercritical fluid is applied to supercritical fluid foamed products; the supercritical fluid is an existing and common foaming fluid. Since the supercritical fluid technology has the characteristics of cleanliness and environmental protection, the application of supercritical fluid technology to prepare polymer microporous foam products is widely used in the field of shoemaking; in this embodiment, the supercritical fluid is N 2 and CO 2 Mixed gas, N 2 The volume percentage is between 40-90%; the supercritical fluid is filled into the mold by a supercritical fluid delivery system.
[0040] In one embodiment, the first channel 4 and the second channel 5 are circular pinhole structures, that is, a plurality of circular through holes, and the plurality of circular through holes are evenly distributed on the first air permeable plate 12 and the second air permeable plate 22; the circular through holes are easy to manufacture and have low cost.
[0041] In this embodiment, the first channel 4 and the second channel 5 are air gap structures 6 , and the air gap structures 6 are evenly distributed on the first air permeable plate 12 and the second air permeable plate 22 .
[0042] like Figure 7 As shown, the first air permeable plate 12 and the second air permeable plate 22 have a plurality of air gap structures 6, and the air gap structures 6 have a plurality of air permeable grooves 61 for gas to pass through; the air permeable grooves 61 can be linear, with a plurality of linear grooves arranged horizontally or laterally on the support plate; or multiple discontinuous linear grooves; further, in this embodiment, the air permeable grooves 61 can also present a certain angle, for example: the air permeable grooves 61 are composed of two segments of linear grooves presenting an angle of 120°; the air permeable grooves 61 can be independent of each other, such as Figure 8 As shown; they can also be connected to each other, such as Fig. 9 As shown; the ventilation grooves 61 can also be perpendicular to each other, presenting a square or right-angled or square spiral shape.
[0043] Furthermore, Fig.11 As shown; the vent groove 61 may be arc-shaped, with multiple arcs spaced apart to present an arc pattern; it may also be a mixture of arcs and straight lines; as Fig.12 As shown; it can also be a mixture of curves and straight lines.
[0044] like Figure 2 As shown, the air-permeable groove 61 may also be Y-shaped, and the supercritical fluid flows in or out of the Y-shaped groove.
[0045] The vent groove 61 has a gap width of 3-6 mm and a gap length of 5-10 mm.
[0046] like Figure 1 As shown; in order to allow the supercritical fluid to pass through the first support plate 11 and the second support plate 21, the first support plate 11 is provided with a first cavity 13 connected to the first channel 4; the second support plate 21 is provided with a second cavity 23 connected to the second channel 5; specifically, the supercritical fluid flows in from the first cavity 13, flows into the molding cavity 3 through the first channel 4; and can also flow in from the second cavity 23, flows into the molding cavity 3 through the second channel 5.
[0047] Furthermore, in order to improve the supporting capacity and rigidity of the first support plate 11 and the second support plate 21 , a plurality of first reinforcing ribs 14 are provided on the first support plate 11 , and the first holes 13 are arranged between the first reinforcing ribs 14 ; a plurality of second reinforcing ribs 24 are provided on the second support plate 21 , and the second holes 23 are arranged between the second reinforcing ribs 24 .
[0048] Furthermore, by adopting the structure of this embodiment, the supercritical fluid can enter and exit quickly, so the supercritical fluid pressure relief rate inside the molding cavity 3 can reach 100~1000MPa / s; due to the rapid flow of the supercritical fluid, the heating rate can be quickly increased, and the heating time can be further shortened. Specifically, the heating rate inside the molding cavity 3 is 10-20℃ / minute, and the heating time is between 10 and 60 minutes.
[0049] Since supercritical fluid is used to directly mold the polymer, and supercritical fluid has a higher temperature and pressure than steam, the mold can also be used to mold some high melting point polymers. The heating temperature inside the molding cavity 3 is between 80 and 350°C; the pressurization pressure is between 3 and 30 MPa.
[0050] The supercritical fluid can quickly flow into the molding cavity 3 and quickly penetrate into the polymer, and can directly perform supercritical fluid foaming molding on thermoplastic polymer particles; it can also perform foaming molding on pre-molded embryos prepared from thermoplastic polymer particles using plastic processing and molding methods; it can also perform mutual welding molding on pre-foamed polymer foam beads. Specifically, the polymer foam beads are foamed in advance by polymer particles, and the pre-foamed polymer foam beads are blown into the mold, and supercritical fluid is introduced to heat and pressurize them to make the polymer foam beads fuse with each other, and after cooling, a foamed bead molding product with the same shape as the molding cavity 3 is formed.
[0051] In another embodiment, the gas is high-temperature steam, and the high-temperature steam is applied to a high-temperature steam heating foam beads forming machine; used to heat the thermoplastic polymer foam beads, so that the thermoplastic polymer foam beads are compression molded. Embodiment 2
[0052] Please refer to Figures 1 to 12 , this embodiment 2 provides a process method for rapid heating and breathable polymer foaming molding.
[0053] Step S1: Taking the pre-molded embryo as an example, the pre-molded embryo is directly placed into the molding cavity 3; the upper mold plate 1 and the lower mold plate 2 are fixed together by an external quick locking pin device, and placed in a high temperature and high pressure reactor;
[0054] Step S2: introducing a supercritical fluid into the reactor, the supercritical fluid flows into the first cavity 13 and the second cavity 23, and flows into the molding cavity 3 through the first channel 4 and the second channel 5; further, the first channel 4 and the second channel 5 are air gap structures 6, and the supercritical fluid flows into the molding cavity 3 through the air gap structure 6;
[0055] Step S3: Continue to introduce supercritical fluid, heat and pressurize, and the supercritical fluid penetrates into the interior of the pre-molded embryo. After reaching a certain temperature, pressure and time, the high temperature and high pressure reactor is quickly depressurized;
[0056] Step S4: The supercritical fluid quickly flows out through the air gap structure 6. Specifically, the supercritical fluid passes through the air gap structure 6, the first cavity 13 and the second cavity 23 from the molding cavity 3 in sequence; the supercritical fluid is discharged to the outside or to a supercritical fluid collector;
[0057] Step S5: the pre-molded embryo in the molding cavity 3 expands and foams to fill the mold, and after cooling, the mold is opened to obtain a molded product of a polymer molded in-mold foaming.
[0058] The mold has rapid exhaust and high pressure relief rate, the foaming ratio of the foamed product is large, and the foaming holes of the product are fine and uniform. Since the polymer is directly molded by supercritical fluid, which has higher temperature and pressure than steam, the mold can also be used to mold some high-melting-point polymers.
[0059] The above embodiments are preferred implementation modes of the present invention, but the implementation modes of the present invention are not limited by the above embodiments. Any other changes, modifications, substitutions, combinations, and simplifications that do not deviate from the spirit and principle of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.
Claims
1. A rapid heating breathable polymer foaming molding mold, characterized in that: The invention comprises an upper template (1) and a lower template (2) which cooperates with the upper template (1), wherein a molding cavity (3) is arranged between the upper template (1) and the lower template (2); the upper template (1) comprises a first support plate (11) and a first air permeable plate (12) installed on one side of the first support plate (11), and the lower template (2) comprises a second support plate (21) and a second air permeable plate (22) installed on one side of the second support plate (21); a first channel (4) for gas to enter and exit is arranged on the first air permeable plate (12); a second channel (5) for gas to enter and exit is arranged on the second air permeable plate (22); a projection area of the first channel (4) accounts for 50% to 80% of a projection area of the bottom of the first air permeable plate (12); a projection area of the second channel (5) accounts for 50% to 80% of a projection area of the bottom of the second air permeable plate (22); gas flows into the molding cavity (3) from the first channel (4) and / or the second channel (5), and flows out from the first channel (4) and / or the second channel (5).
2. A rapid heating breathable polymer foaming molding mold according to claim 1, characterized in that: The first channel (4) and the second channel (5) are circular pinhole structures, and the circular pinhole structures are evenly distributed on the first air permeable plate (12) and the second air permeable plate (22).
3. A rapid heating breathable polymer foaming molding mold according to claim 1, characterized in that: The first channel (4) and the second channel (5) are air gap structures (6), and the air gap structures (6) are evenly distributed on the first air permeable plate (12) and the second air permeable plate (22).
4. A rapid heating breathable polymer foaming molding mold according to claim 3, characterized in that: The air slot structure (6) has a plurality of air-permeable grooves (61) for gas to pass through, wherein the air-permeable grooves (61) are linear and distributed transversely or longitudinally; or the air-permeable grooves (61) are at an angle to each other; the air-permeable grooves (61) are at an angle of 120°, forming a Y shape; or the air-permeable grooves (61) are perpendicular to each other, forming a square or right-angled shape or a square spiral shape.
5. A rapid heating breathable polymer foaming molding mold according to claim 3, characterized in that: The air slit structure (6) has a plurality of air-permeable grooves (61) for gas to pass through, wherein the air-permeable grooves (61) are arc-shaped, and a plurality of arcs are arranged at intervals to present an arc pattern; or the air-permeable grooves (61) are a mixture of arcs and straight lines; or the air-permeable grooves (61) are a mixture of curves and straight lines.
6. A rapid heating breathable polymer foaming molding die according to claim 4 or 5, characterized in that: The vent groove (61) has a gap width of 3-6 mm and a gap length of 5-10 mm.
7. The rapid heating breathable polymer foaming molding mold according to claim 1, characterized in that: The first support plate (11) is provided with a first cavity (13) connected to the first channel (4); the second support plate (21) is provided with a second cavity (23) connected to the second channel (5); the first support plate (11) is provided with a plurality of first reinforcing ribs (14), the first cavity (13) being arranged between the first reinforcing ribs (14); the second support plate (21) is provided with a plurality of second reinforcing ribs (24), the second cavity (23) being arranged between the second reinforcing ribs (24).
8. The rapid heating breathable polymer foaming molding mold according to claim 1, characterized in that: The gas is high-temperature steam, and the high-temperature steam is applied to a high-temperature steam-heated foaming bead forming machine to foam and form thermoplastic polymer particles.