Exothermic welding sand mold side mold for high-difference rail

By designing aluminothermic welding sand mold side mold adapted to both insert rails and existing rails, the complex operation problem caused by height difference in rail welding was solved, simplifying on-site repair work and improving welding efficiency and post-weld quality.

CN222083228UActive Publication Date: 2024-11-29BEIJING RAILWELD NEW MATERIAL TECH CO LTD +4
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420588765.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-26
Publication Date
2024-11-29
Estimated Expiration
2034-03-26

AI Technical Summary

Technical Problem

In existing technologies, the height difference between the inserted rail and the existing rail during aluminothermic welding of steel rails makes the welding operation complex, relies on manual adjustment of the sand mold side mold, increases the workload and difficulty, and affects the quality of the welded joint.

Method used

A side mold for high-difference rails using aluminothermic welding sand casting is designed, consisting of detachable first and second connecting parts, which are adapted to the insert rail and the existing rail respectively. By designing the top surface of the snap-fit ​​groove to be horizontal, the tread surface of the insert rail and the existing rail are ensured to be at the same level, reducing the amount of on-site grinding and post-weld grinding.

Benefits of technology

It simplifies on-site welding operations, reduces operational difficulty, ensures the quality of welded joints, and improves welding efficiency and finished product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222083228U_ABST
    Figure CN222083228U_ABST
Patent Text Reader

Abstract

The utility model discloses an exothermic welding sand mould side mould for a high difference rail, which comprises a first mounting surface and a second mounting surface, the first mounting surface is provided with a first mounting groove for clamping an insertion rail, the second mounting surface is provided with a second mounting groove for clamping an insertion rail, and the groove top surface of the first mounting groove and the groove top surface of the second mounting groove are positioned on the same horizontal plane. The distances between the groove bottom of the first mounting groove and the horizontal plane are not equal to those between the groove bottom of the second mounting groove and the horizontal plane; the first mounting groove comprises a non-wear rail head step, a non-wear rail lower jaw step and a non-wear rail bottom step, and the non-wear rail head step is attached to a rail head tread of the mounting insertion rail; the second mounting groove comprises an abraded rail head step, an abraded rail lower jaw step and an abraded rail bottom step, and the abraded rail head step is attached to the rail head tread of the rail. According to the exothermic welding sand mold side mold for the high-difference rail, the workload of grinding a sand mold on site and the grinding amount of a welded joint of a welding worker are reduced, the field operation difficulty is reduced, and the quality of the welded joint is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of rail welding, and more specifically to an aluminum thermal welding sand mold side mold for a height difference rail. Background Art

[0002] The working environment of railway sites is complex. In most cases, there are different degrees of height difference between the inserted rail and the existing rail. Rail aluminothermic welding is a casting welding method. Currently, aluminothermic welding materials on the market are limited to standard-sized rails. When actually working on existing lines, operators need to enter the site to temporarily trim the welding materials. When performing insertion welding on existing lines, if there is a height difference between the inserted rail and the existing rail (the top tread of the existing rail is worn, causing the height of the existing rail to decrease), the welding operator will trim the sand mold side mold made according to the on-site rail conditions.

[0003] However, the on-site operation is complicated and there are many uncertain factors. The sand mold side mold repair process is highly dependent on the technical level of the operator. At the least, it will cause the welding materials to be scrapped, and at the worst, it will cause defects such as molten steel leakage and sand inclusion inside the rail head, which directly affects the quality of the joint after welding. On the other hand, the sand mold side mold repair process is time-consuming, which increases the workload of welding operations and the difficulty of on-site operations.

[0004] Therefore, it is necessary to solve the above technical problems. Utility Model Content

[0005] In view of this, the purpose of the utility model is to propose an aluminum thermite welding sand mold side mold for height difference rails, so as to reduce the workload of welding workers in on-site grinding of sand molds and the amount of grinding of joints after welding, reduce the difficulty of on-site operations, and ensure the quality of joints after welding.

[0006] Based on the above purpose, the utility model provides an aluminum thermite welding sand mold side mold for a height difference rail, the aluminum thermite welding sand mold side mold for the height difference rail is composed of two detachable first connecting members and a second connecting member connected to each other, including a first mounting surface and a second mounting surface arranged back to back, the first mounting surface is evenly arranged on the first connecting member and the second connecting member; the second mounting surface is evenly arranged on the first connecting member and the second connecting member, wherein: a first mounting groove for clamping an inserted rail is provided on the first mounting surface, a second mounting groove for clamping an existing rail is provided on the second mounting surface, and the groove top surface of the first mounting groove and the groove top surface of the second mounting groove are in the same horizontal plane, and the distance from the groove bottom of the first mounting groove and the groove bottom of the second mounting groove to the horizontal plane is not equal; the first mounting groove is evenly arranged The first connecting member and the second connecting member are arranged on the second mounting grooves, and the first mounting groove includes a wear-free rail head step, a wear-free rail jaw step and a wear-free rail bottom step. The wear-free rail head step is used to fit and install the rail head tread of the inserted rail, the wear-free rail jaw step is used to fit and install the rail jaw of the inserted rail, and the wear-free rail bottom step is used to fit and install on the rail bottom angle slope of the inserted rail; the second mounting groove includes a worn rail head step, a worn rail jaw step and a worn rail bottom step. The worn rail head step is used to fit and install the rail head tread of the existing rail, the worn rail jaw step is used to fit and install the rail jaw of the existing rail, and the worn rail bottom step is used to fit and install on the rail bottom angle slope of the existing rail.

[0007] Optionally, the first mounting groove is an I-shaped groove that matches the cross-sectional structure of the inserted rail, and the second mounting groove is an I-shaped groove that matches the cross-sectional structure of the existing rail.

[0008] The utility model provides an aluminum thermal welding sand mold side mold for a height difference rail. First, the rail head tread of the inserted rail is fitted on the non-wear rail head step, the rail lower jaw of the inserted rail is fitted on the non-wear rail lower jaw step, and the rail bottom angle inclined surface of the inserted rail is fitted under the non-wear rail bottom step, so that the inserted rail is snap-fitted and installed in the first installation groove; at the same time, the rail head tread of the existing rail is fit on the worn rail head step, the rail lower jaw of the existing rail is fit on the worn rail lower jaw step, and the rail bottom angle inclined surface of the existing rail is fit under the worn rail bottom step, so that the existing rail is snap-fitted and installed in the second installation groove. The utility model provides an aluminum thermite welding sand mold side mold for the height difference rail. When the inserted rail and the existing rail are respectively clamped on the aluminum thermite welding sand mold side mold for the height difference rail, the rail head tread of the inserted rail and the rail head tread of the existing rail are on the same horizontal plane, so that the height difference between the rail bottom of the existing rail and the rail bottom of the inserted rail is the wear amount of the existing rail, and then the subsequent welding operation can be carried out according to the aluminum thermite welding operation instruction manual for the rail, thereby reducing the workload of the welding operator in grinding the sand mold on site and the grinding amount of the joint after welding, reducing the difficulty of on-site operation and ensuring the quality of the joint after welding. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] The preferred embodiments of the present invention will be described in detail below with reference to the accompanying drawings, which will help to understand the purpose and advantages of the present invention, wherein:

[0010] Figure 1 It is a structural schematic diagram of the first connecting member in the side mold of the aluminothermic welding sand mold for the height difference rail according to one embodiment of the utility model;

[0011] Figure 2 It is a schematic diagram of the installation of the aluminothermic welding sand mold side mold for the height difference rail and the existing rail and the insert rail according to one embodiment of the utility model;

[0012] Figure 3 It is a first partial schematic diagram of the installation of the aluminothermic welding sand mold side mold for the height difference rail and the existing rail and the insert rail according to one embodiment of the utility model;

[0013] Figure 4 This is a second partial schematic diagram of the installation of the height difference rail heat welding sand mold side mold with the existing rail and the inserted rail according to one embodiment of the utility model.

[0014] Description of reference numerals:

[0015] 1: second mounting surface; 2: second mounting groove; 3: non-wear rail head step; 4: non-wear rail jaw step; 5: non-wear rail bottom step; 6: worn rail head step; 7: worn rail jaw step; 8: worn rail bottom step; 9: rail head tread of inserted rail; 10: rail jaw of inserted rail; 11: rail bottom angle slope of inserted rail; 12: rail head tread of existing rail; 13: rail jaw of existing rail; 14: rail bottom angle slope of existing rail; 15: first connecting piece; 16: second connecting piece; 17: existing rail; 18: inserted rail. DETAILED DESCRIPTION

[0016] The present invention is described in detail below in conjunction with the embodiments. The same components are denoted by the same reference numerals. It should be noted that the words "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to directions in the drawings, and the words "inner" and "outer" refer to directions toward or away from the geometric center of a specific component, respectively.

[0017] like Figures 1 to 4 As shown, the utility model provides an aluminum thermal welding sand mold side mold for a height difference rail, which is composed of two detachable first connecting members 15 and second connecting members 16 connected to each other, including a first mounting surface and a second mounting surface 1 arranged back to back, the first mounting surface is evenly arranged on the first connecting member 15 and the second connecting member 16, and the second mounting surface 1 is evenly arranged on the first connecting member 15 and the second connecting member 16, wherein: a first mounting groove for clamping an inserted rail 18 is provided on the first mounting surface, a second mounting groove 2 for clamping an existing rail 17 is provided on the second mounting surface 1, and the groove top surface of the first mounting groove and the groove top surface of the second mounting groove 2 are in the same horizontal plane, and the distances from the groove bottom of the first mounting groove and the groove bottom of the second mounting groove 2 to the horizontal plane are not equal; the first mounting groove is evenly arranged in the first On a connecting member 15 and a second connecting member 16, the second mounting groove 2 is evenly arranged on the first connecting member 15 and the second connecting member 16, the first mounting groove includes a wear-free rail head step 3, a wear-free rail jaw step 4 and a wear-free rail bottom step 5, the wear-free rail head step 3 is used to fit and install the rail head tread 9 of the inserted rail, the wear-free rail jaw step 4 is used to fit and install the rail jaw 10 of the inserted rail, and the wear-free rail bottom step 5 is used to fit and install on the rail bottom angle slope 11 of the inserted rail; the second mounting groove 2 includes a worn rail head step 6, a worn rail jaw step 7 and a worn rail bottom step 8, the worn rail head step 6 is used to fit and install the rail head tread 12 of the existing rail, the worn rail jaw step 7 is used to fit and install the rail jaw 13 of the existing rail, and the worn rail bottom step 8 is used to fit and install on the rail bottom angle slope 14 of the existing rail.

[0018] It should be noted that: the structures of the first connecting member 15 and the second connecting member 16 are mirror-symmetrical; the distances from the bottom of the first mounting groove and the bottom of the second mounting groove 2 to the horizontal plane are not equal, and can be 3mm, 6mm, 9mm, etc.; Figure 3 and Figure 4 The height difference between the inserted rail 18 and the existing rail 17 is 6 mm.

[0019] The utility model provides an aluminum thermal welding sand mold side mold for the height difference rail. First, the rail head tread 9 of the inserted rail is fitted on the non-wear rail head step 3, the rail jaw 10 of the inserted rail is fitted on the non-wear rail jaw step 4, and the rail bottom angle slope 11 of the inserted rail is fitted under the non-wear rail bottom step 5, so that the inserted rail 18 is snap-fitted and installed in the first installation groove; at the same time, the rail head tread 12 of the existing rail is fit on the worn rail head step 6, the rail jaw 13 of the existing rail is fit on the worn rail jaw step 7, and the rail bottom angle slope 14 of the existing rail is fit under the worn rail bottom step 8, so that the existing rail 17 is snap-fitted and installed in the second installation groove 2. The utility model provides an aluminum thermite welding sand mold side mold for the height difference rail. When the inserted rail 18 and the existing rail 17 are respectively clamped on the aluminum thermite welding sand mold side mold for the height difference rail, the rail head tread 9 of the inserted rail and the rail head tread 12 of the existing rail are on the same horizontal plane, so that the height difference between the rail bottom of the existing rail 17 and the rail bottom of the inserted rail 18 is the wear amount of the existing rail 17, and then the subsequent welding operation can be carried out according to the aluminum thermite welding operation instruction manual for the rails, thereby reducing the workload of the welding operators for grinding the sand mold on site and the grinding amount of the joint after welding, reducing the difficulty of on-site operation and ensuring the quality of the joint after welding.

[0020] like Figure 1 and Figure 2 As shown, the first mounting groove is an I-shaped groove that matches the cross-sectional structure of the inserted rail 18, and the second mounting groove 2 is an I-shaped groove that matches the cross-sectional structure of the existing rail 17. In this embodiment, the I-shaped first mounting groove that matches the inserted rail 18 and the I-shaped second mounting groove 2 that matches the existing rail 17 can respectively and well clamp and install the inserted rail 18 and the existing rail 17 on the side mold of the aluminum thermite welding sand mold for the height difference rail, thereby improving the convenience of using the side mold of the aluminum thermite welding sand mold for the height difference rail.

[0021] The utility model provides an aluminum thermal welding sand mold side mold for the height difference rail. First, the rail head tread 9 of the inserted rail is fitted on the non-wear rail head step 3, the rail jaw 10 of the inserted rail is fitted on the non-wear rail jaw step 4, and the rail bottom angle slope 11 of the inserted rail is fitted under the non-wear rail bottom step 5, so that the inserted rail 18 is snap-fitted and installed in the first installation groove; at the same time, the rail head tread 12 of the existing rail is fit on the worn rail head step 6, the rail jaw 13 of the existing rail is fit on the worn rail jaw step 7, and the rail bottom angle slope 14 of the existing rail is fit under the worn rail bottom step 8, so that the existing rail 17 is snap-fitted and installed in the second installation groove 2. The utility model provides an aluminum thermite welding sand mold side mold for the height difference rail. When the inserted rail 18 and the existing rail 17 are respectively clamped on the aluminum thermite welding sand mold side mold for the height difference rail, the rail head tread 9 of the inserted rail and the rail head tread 12 of the existing rail are on the same horizontal plane, so that the height difference between the rail bottom of the existing rail 17 and the rail bottom of the inserted rail 18 is the wear amount of the existing rail 17, and then the subsequent welding operation can be carried out according to the aluminum thermite welding operation instruction manual for the rails, thereby reducing the workload of the welding operators for grinding the sand mold on site and the grinding amount of the joint after welding, reducing the difficulty of on-site operation and ensuring the quality of the joint after welding.

[0022] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the various embodiments of the utility model.

Claims

1. A heat-welded sand mold side mold for height difference rail, characterized in that: The aluminothermic welding sand mold side mold for the height difference rail is composed of two detachable first connecting parts and a second connecting part connected together, including a first mounting surface and a second mounting surface arranged back to back, the first mounting surface is evenly arranged on the first connecting part and the second connecting part, and the second mounting surface is evenly arranged on the first connecting part and the second connecting part, wherein: The first mounting surface is provided with a first mounting groove for clamping the inserted rail, and the second mounting surface is provided with a second mounting groove for clamping the existing rail, and the top surface of the first mounting groove and the top surface of the second mounting groove are in the same horizontal plane, and the distances from the bottom of the first mounting groove and the bottom of the second mounting groove to the horizontal plane are not equal; The first mounting groove is evenly arranged on the first connecting member and the second connecting member, the second mounting groove is evenly arranged on the first connecting member and the second connecting member, the first mounting groove comprises a wear-free rail head step, a wear-free rail jaw step and a wear-free rail bottom step, the wear-free rail head step is used to fit and install the rail head tread of the insert rail, the wear-free rail jaw step is used to fit and install the rail jaw of the insert rail, and the wear-free rail bottom step is used to fit and install on the rail bottom angle inclined surface of the insert rail; The second mounting groove comprises a worn rail head step, a worn rail jaw step and a worn rail bottom step, the worn rail head step is used to fit and install the rail head tread of the existing rail, the worn rail jaw step is used to fit and install the rail jaw of the existing rail, and the worn rail bottom step is used to fit and install on the rail bottom angle slope of the existing rail.

2. The aluminothermic welding sand mold side mold for the height difference rail according to claim 1, characterized in that: The first installation groove is an I-shaped groove that matches the cross-sectional structure of the inserted rail, and the second installation groove is an I-shaped groove that matches the cross-sectional structure of the existing rail.