Integrated equipment for preparing lithium iron phosphate

By designing integrated lithium iron phosphate preparation equipment, using thermal convection and waste heat reuse technology, the problems of low efficiency and high cost in the preparation process of lithium iron phosphate in the existing technology are solved, and equipment integration and finished product performance are achieved.

CN222093304UActive Publication Date: 2024-12-03JIANGSU BTR NANO TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420540713.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-20
Publication Date
2024-12-03
Estimated Expiration
2034-03-20

AI Technical Summary

Technical Problem

In the prior art, the lack of integrated equipment in the preparation process of lithium iron phosphate, resulting in separate process steps, low efficiency, complicated equipment, large area occupied, high production costs, and temperature changes and the introduction of pollutants during material transfer affect the performance of the finished product. .

Method used

A lithium iron phosphate integrated equipment including feeding device, drying tower and sintering device is designed, and components such as atomization nozzle, nitrogen delivery pipeline, cyclone separator and heat exchanger are used to realize the reuse of heat convection and waste heat. The uniform drying and sintering of materials reduces manpower and energy consumption and improves production efficiency.

Benefits of technology

It realizes the integration of equipment, energy saving and environmental protection, reduces production costs, improves the capacity and compaction parameters of finished lithium iron phosphate products, shortens the production cycle, and improves the performance of finished products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222093304U_ABST
    Figure CN222093304U_ABST
Patent Text Reader

Abstract

The utility model discloses integrated equipment for preparing lithium iron phosphate, which comprises a feeding device, a drying tower and a sintering device, the feeding device comprises an atomizing nozzle and a second nitrogen conveying pipeline arranged at the top of the atomizing nozzle; a first nitrogen conveying pipeline and a material output pipeline are arranged at the bottom of the drying tower; the feeding device is arranged at the top of the drying tower, and the material output pipeline is sequentially connected with the cyclone separator and the sintering device and is used for collecting waste heat for heating nitrogen. The equipment is integrated, small in size, small in occupied space, convenient to control, low in cost, small in investment and convenient for diversification of product models; the manpower demand and the energy consumption are greatly reduced, and the production efficiency is improved; the performance of a lithium iron phosphate finished product is improved, and the electric capacity and the compaction parameter are improved; and waste heat is recycled, energy is saved, environment is protected, and production cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to powder preparation equipment, in particular to integrated equipment for preparing lithium iron phosphate. Background Art

[0002] As a high-performance secondary green battery, lithium iron phosphate has the advantages of high voltage, high energy density, low self-discharge rate, wide operating temperature range, long cycle life, environmental protection, no memory effect, and high current charge and discharge. At present, the main methods for producing lithium iron phosphate include solid phase method, carbon thermal reduction method, hydrothermal method and liquid phase deposition method. Each process step is carried out separately without integrated equipment. As a result, the preparation process of lithium iron phosphate is long, inefficient, the equipment is complicated, the occupied area is large, the production cost is high, and the transfer of semi-finished materials requires a lot of manpower. At the same time, the temperature change, the introduction of pollutants or the change of form of the material during the transfer process will cause uncertain factors to the subsequent process and affect the performance of the lithium iron phosphate finished product. Utility Model Content

[0003] Purpose of the utility model: The purpose of the utility model is to improve production efficiency, reduce the consumption of manpower and material resources, improve the performance of the finished product, and provide an integrated device for preparing lithium iron phosphate.

[0004] Technical solution: The integrated equipment for preparing lithium iron phosphate described in the utility model includes a feeding device, a drying tower and a sintering device. The feeding device includes an atomizing nozzle and a second nitrogen delivery pipeline placed on the top of the atomizing nozzle; a first nitrogen delivery pipeline and a material output pipeline are provided at the bottom of the drying tower; the feeding device is arranged at the top of the drying tower, and the material output pipeline is connected to the sintering device.

[0005] Furthermore, a cyclone separator is provided between the material output pipeline and the sintering device, and the particle size specification of the product is controlled by adjusting the gas volume of the cyclone separator.

[0006] Furthermore, the first nitrogen delivery pipeline extends into the interior of the drying tower, and a wind cap is provided at the upper end of the pipeline to form heat convection in the drying tower.

[0007] Furthermore, the first nitrogen delivery pipeline is provided with a heating device to heat the nitrogen. The heated nitrogen cooperates with the unheated nitrogen in the feeding device and the waste gas and waste collection pipeline to form stable different temperature zones from top to bottom in the drying tower, which first rise and then fall, to dry and sinter the material once.

[0008] Furthermore, the first nitrogen delivery pipeline is also provided with a heat exchanger at the front end of the heating device. The input end of the heat exchanger is connected to the drying tower and the cyclone separator through the waste gas and waste collection pipeline, and the output end of the heat exchanger is connected to the exhaust fan. The waste heat in the drying tower can be collected for heating the nitrogen, which is environmentally friendly and energy-saving.

[0009] Furthermore, a waste collection device is provided at the output end of the exhaust fan to collect products whose particle sizes do not meet the specifications for recycling and reuse, thereby avoiding waste of raw materials.

[0010] Furthermore, a first temperature sensor is provided on the first nitrogen delivery pipeline near the outer wall of the drying tower, and a second temperature sensor is provided on the material output pipeline near the outer wall of the drying tower, which are used to monitor the temperature changes in the drying tower to ensure the drying of the material and the performance of the primary sintering.

[0011] Beneficial effects: Compared with the prior art, the utility model has the following advantages: 1. Integrated equipment with small size, small space occupation, easy control, low cost, small investment, and convenient for product model diversification; 2. Greatly reduces manpower requirements and energy consumption, and improves production efficiency; 3. Improves the performance of lithium iron phosphate products, and improves both the capacity and compaction parameters; 4. Reuses waste heat, saves energy and protects the environment, and reduces production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 It is a structural schematic diagram of the utility model. DETAILED DESCRIPTION

[0013] The technical solution of the utility model is further described below in conjunction with the accompanying drawings.

[0014] like Figure 1The integrated equipment for preparing lithium iron phosphate shown in the figure comprises a feeding device, a drying tower 7 and a sintering device 12. The feeding device comprises an atomizing nozzle 16 and a second nitrogen delivery pipeline 15 disposed on the top of the atomizing nozzle 16. Nitrogen is delivered to the feeding device through the second nitrogen delivery device 14. A first nitrogen delivery pipeline 4 and a material output pipeline 8 are disposed at the bottom of the drying tower 7. The feeding device is disposed at the top of the drying tower 7. The material output pipeline 5 is connected to a cyclone separator 11. The bottom of the cyclone separator 11 is connected to a sintering device 12. The bottom of the sintering device 12 is connected to a material receiving barrel 13. A heating device 3 is disposed on the first nitrogen delivery pipeline 4. The first nitrogen delivery pipeline 4 extends into the interior of the drying tower 7. A wind cap 6 is disposed at the upper end of the pipeline. A waste gas and waste material collection pipeline 10 is disposed at the top of the cyclone separator 11 and the drying tower 7 to connect to the input end of the heat exchanger 2. The output end of the heat exchanger 2 is connected to an exhaust fan 18 through a waste gas and waste material output pipeline 17. A waste material collection device is disposed at the output end of the exhaust fan 18. A first temperature sensor 5 is disposed on the first nitrogen delivery pipeline 4 near the outer wall of the drying tower 7 , and a second temperature sensor 9 is disposed on the material output pipeline 8 near the outer wall of the drying tower 7 .

[0015] The above-mentioned integrated equipment for preparing lithium iron phosphate is used to mix the lithium source, carbon source and phosphorus source in proportion and evenly mix them through ball milling to form a slurry for use. Open the first nitrogen delivery device 1 and the heating device 3, set the temperature of the heating device 3 to 800°C for heating the nitrogen, open the sintering device 12, and set the sintering temperature to 820°C; open the second nitrogen input device 14, and send the nitrogen into the atomizing nozzle 16 of the feeding device; turn on the exhaust fan 18 and start the heat exchanger 2 at the same time, preheat the equipment for 5 hours to reach a thermal equilibrium state, and the heated nitrogen forms heat convection through the wind cap 6. The heated nitrogen cooperates with the unheated nitrogen in the feeding device and the waste gas and waste collection pipe 10 to form a stable first from top to bottom in the drying tower 7. Different temperature zones are raised and then lowered; the ball-milled slurry is added into the drying tower 7 through the atomizing nozzle 16, the opening of the atomizing nozzle 16 is set to 50, the slurry is dried first and then calcined once after passing through different temperature zones inside the drying tower 7, and then enters the cyclone separator 11 through the material conveying pipe 8 at the bottom, and the products of different particle sizes are screened by adjusting the gas volume of the cyclone separator 11 to enter the sintering device 12 for the second calcination, and the finished products after calcination are collected in the collecting barrel 13, and the materials that do not meet the specifications are collected through the waste collection pipe 10 and the waste collection device at the output end of the exhaust fan 18 for reuse. Sintering the same lithium iron phosphate product through the above-mentioned device saves about 2,000 yuan / ton in electricity, about 300 yuan / ton in nitrogen, and 200 yuan / ton in natural gas. The production cycle is accelerated by 10 hours / ton. The equipment is integrated, small in size, low in failure rate, and high in production efficiency. The sintering is more uniform, and the performance of the lithium iron phosphate product has been improved: 0.1C charging: 163mAh / g, 0.1C discharging: 162mAh / g, compaction parameters: 2.45g / cc.

Claims

1. An integrated device for preparing lithium iron phosphate, comprising a feeding device, a drying tower (7) and a sintering device (12), characterized in that: The feeding device comprises an atomizing nozzle (16) and a second nitrogen delivery pipeline (15) arranged on the top of the atomizing nozzle (16); a first nitrogen delivery pipeline (4) and a material output pipeline (8) are arranged at the bottom of the drying tower (7); the feeding device is arranged at the top of the drying tower (7), and the material output pipeline (8) is connected to the sintering device (12).

2. The integrated equipment for preparing lithium iron phosphate according to claim 1, characterized in that: A cyclone separator (11) is provided between the material output pipeline (8) and the sintering device (12).

3. The integrated equipment for preparing lithium iron phosphate according to claim 1, characterized in that: The first nitrogen delivery pipeline (4) extends into the interior of the drying tower (7), and a wind cap (6) is provided at the upper end of the pipeline.

4. The integrated equipment for preparing lithium iron phosphate according to claim 1, characterized in that: The first nitrogen delivery pipeline (4) is provided with a heating device (3).

5. The integrated equipment for preparing lithium iron phosphate according to claim 3, characterized in that: The first nitrogen delivery pipeline (4) is further provided with a heat exchanger (2) at the front end of the heating device (3); the input end of the heat exchanger (2) is connected to the drying tower (7) and the cyclone separator (11) via the waste gas and waste material collection pipeline (10); and the output end of the heat exchanger (2) is connected to the exhaust fan (18).

6. The integrated equipment for preparing lithium iron phosphate according to claim 5, characterized in that: A waste collection device is provided at the output end of the exhaust fan (18).

7. The integrated equipment for preparing lithium iron phosphate according to claim 1, characterized in that: A first temperature sensor (5) is provided on the first nitrogen delivery pipeline (4) near the outer wall of the drying tower (7), and a second temperature sensor (9) is provided on the material output pipeline (8) near the outer wall of the drying tower (7).